MEMS sensors and their fabrication methods, electronic devices

By setting an insulating layer in the MEMS sensor to cover the bottom and side walls of the trench, the short circuit problem caused by particles during chip cutting was solved, improving the electrical performance stability and product yield.

CN115557460BActive Publication Date: 2026-11-10SEMICON MFG ELECTRONICS (SHAOXING) CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202211034169.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-08-26
Publication Date
2026-11-10
Estimated Expiration
2042-08-26

AI Technical Summary

Technical Problem

MEMS sensors are prone to short circuits during chip cutting due to particles falling into the trenches, affecting electrical performance stability and product yield.

Method used

An insulating layer is placed in the MEMS sensor to cover the bottom and side walls of the trench to prevent particles from falling in and avoid short circuits.

Benefits of technology

This improves the electrical performance stability and product yield of MEMS sensors, ensuring electrical performance stability and increasing product qualification rate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115557460B_ABST
    Figure CN115557460B_ABST
Patent Text Reader

Abstract

This invention relates to a MEMS sensor, its fabrication method, and an electronic device. A MEMS sensor includes: a first wafer; a second wafer disposed opposite to the first wafer; a bonding structure disposed between the first and second wafers; the bonding structure having a bonding surface; and an insulating layer covering at least a portion of the side surface of the bonding structure to insulate the bonding surface of the bonding structure from the external environment. The MEMS sensor provided in this application, through the provision of the insulating layer, effectively prevents moisture from the external environment from eroding the bonding surface and entering the MEMS sensor, thereby better protecting the electrical performance of the MEMS sensor and improving its reliability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor technology, and in particular to a MEMS sensor, its fabrication method, and an electronic device. Background Technology

[0002] MEMS (Micro Electro Mechanical System) sensors are a new type of sensor manufactured using microelectronics and micromachining technologies. Commonly used MEMS sensors include pressure sensors, inertial sensors, microphones, light sensors, catalytic sensors, and more. With continuous improvement and development of manufacturing technologies, MEMS sensors have been widely used in fields such as smartphones, fitness trackers, printers, automobiles, drones, and VR / AR devices.

[0003] Typically, a MEMS sensor includes a first wafer, a second wafer, and a functional layer disposed between the first and second wafers. The functional layer has exposed pads to facilitate electrical connection to external circuitry. However, MEMS sensors are prone to high failure rates due to substandard electrical performance testing. Summary of the Invention

[0004] In view of the above, this application provides a MEMS sensor and its fabrication method, as well as an electronic device, to solve at least one problem existing in the background art.

[0005] To achieve the above objectives, the technical solution of this application is implemented as follows:

[0006] In a first aspect, this embodiment provides a MEMS sensor, which includes:

[0007] First wafer;

[0008] The second wafer is disposed opposite to the first wafer;

[0009] A functional layer is disposed on the first wafer; the functional layer includes a first region covered by the second wafer and a second region surrounding the first region; the second region of the functional layer is provided with a plurality of pads; the functional layer is provided with trenches corresponding to the pads; and

[0010] An insulating layer covers the bottom and sidewalls of the trench.

[0011] Optionally, the insulating layer also covers the side surface of the pad.

[0012] Optionally, it further includes a bonding structure; the bonding structure is disposed between the functional layer and the second wafer; the bonding structure has a bonding surface; the insulating isolation layer also covers at least a portion of the side surface of the bonding structure to insulate the bonding surface of the bonding structure from the external environment.

[0013] Optionally, the insulating layer completely covers the outer surface of the bonding structure and extends to cover at least a portion of the second wafer;

[0014] And / or, the insulating isolation layer completely covers the outer surface of the bonded structure and extends to cover at least part of the functional layer.

[0015] Optionally, the surface of the second wafer opposite to the first wafer is the first surface, and the insulating layer further covers at least partially the first surface of the second wafer.

[0016] Secondly, this embodiment provides an electronic device that includes the MEMS sensor provided in this application.

[0017] Thirdly, this embodiment provides a method for fabricating a MEMS sensor, which includes the following steps:

[0018] A preliminary MEMS sensor body is provided; the preliminary MEMS sensor body includes a first wafer, a second wafer, and a functional layer; the functional layer is provided with trenches;

[0019] An insulating and protective full-coverage layer is formed on the MEMS sensor substrate before the slicing process;

[0020] The insulating isolation layer is patterned to at least expose the pads on the second wafer and at least cover the bottom and sidewalls of the trench, forming an insulating isolation layer.

[0021] Optionally, forming an insulating and protective full-coverage layer on the initial MEMS sensor body before the slicing process includes:

[0022] An insulating material is coated onto the MEMS sensor substrate.

[0023] Optionally, the patterning of the insulating isolation full-coverage layer to at least expose the pads on the second wafer and at least cover the bottom and sidewalls of the trench to form an insulating isolation layer includes:

[0024] Photoresist is coated onto the insulating and protective full-coverage layer and then exposed and developed.

[0025] High-temperature curing is used to form the insulating layer.

[0026] Optionally, the insulating isolation layer formed by patterning the insulating isolation full cover layer also covers the side surface of the pad.

[0027] Optionally, the MEMS sensor substrate further includes a bonding structure; the bonding structure is disposed between the functional layer and the second wafer; the bonding structure has a bonding surface;

[0028] The insulating layer formed by patterning the insulating isolation full-coverage layer also covers at least a portion of the side surfaces of the bonding structure to insulate the bonding surfaces of the bonding structure from the external environment.

[0029] Optionally, the insulating isolation layer formed by patterning the insulating isolation full-coverage layer completely covers the outer surface of the bonding structure and extends to cover at least a portion of the second wafer;

[0030] And / or, the insulating isolation layer formed by patterning the insulating isolation full-coverage layer completely covers the outer surface of the bonding structure and extends to cover at least part of the functional layer.

[0031] Optionally, the surface of the second wafer opposite to the first wafer is the first surface; the insulating isolation layer formed by patterning the insulating isolation full-coverage layer also at least partially covers the first surface of the second wafer.

[0032] The MEMS sensor provided in this application embodiment covers the bottom and side walls of the trench with an insulating isolation layer, thereby avoiding short circuits caused by particles that may fall into the trench during subsequent chip cutting processes. This better ensures the stability of the electrical performance of the MEMS sensor and improves the product yield of the MEMS sensor.

[0033] The electronic device provided in this application, in its MEMS sensor, covers the bottom and side walls of the trench with an insulating isolation layer, thereby preventing particles that may be generated during subsequent chip cutting processes from falling into the trench and thus avoiding short circuits. This better ensures the stability of the electrical performance of the MEMS sensor and improves the product yield of the MEMS sensor.

[0034] The MEMS sensor fabrication method provided in this application covers the bottom and sidewalls of the trench with an insulating layer, thereby preventing particles that may be generated during subsequent chip dicing processes from falling into the trench and thus avoiding short circuits. This better ensures the stability of the electrical performance of the MEMS sensor and improves the product yield of the MEMS sensor.

[0035] Additional aspects and advantages of this application will be set forth in part in the description which follows, and in part will be obvious from the description, or may be learned by practice of this application. Attached Figure Description

[0036] The accompanying drawings, which are included to provide a further understanding of this application and form part of this application, illustrate exemplary embodiments and are used to explain this application, but do not constitute an undue limitation of this application. In the drawings:

[0037] Figure 1 This is a schematic cross-sectional view of the structure of a MEMS sensor provided in an embodiment of this application;

[0038] Figure 2 for Figure 1 Top view;

[0039] Figure 3 This is a schematic cross-sectional view of the structure of a MEMS sensor provided in another embodiment of this application;

[0040] Figure 4 This is a schematic cross-sectional view of the structure of a MEMS sensor provided in another embodiment of this application;

[0041] Figure 5 This is a schematic cross-sectional view of the structure of a MEMS sensor provided in another embodiment of this application;

[0042] Figure 6 This is a schematic cross-sectional view of the structure of a MEMS sensor provided in another embodiment of this application;

[0043] Figure 7 This is a schematic cross-sectional view of the structure of a MEMS sensor provided in another embodiment of this application;

[0044] Figure 8 for Figure 7 Top view;

[0045] Figure 9 This is a schematic cross-sectional view of the structure of a MEMS sensor provided in another embodiment of this application;

[0046] Figure 10 This is a schematic cross-sectional view of the structure of a MEMS sensor provided in another embodiment of this application;

[0047] Figure 11 This is a schematic flowchart illustrating a method for fabricating a MEMS sensor according to an embodiment of this application.

[0048] Figure 12 for Figure 11 A detailed flowchart of step S03 is shown below;

[0049] Figures 13a to 13c for Figure 9 The diagram shows a cross-sectional view of the MEMS sensor during its fabrication process.

[0050] Explanation of reference numerals in the attached figures

[0051] 100 / 200 / 300 / 400 / 500 / 600 / 700 / 800, MEMS sensor; 110, First wafer; 111, Functional layer; 111a, First region; 111b, Second region; 112, Trench; 113, Pad; 130, Second wafer; 131, First surface; 150, Bonding structure; 151, Bonding surface; 152, First bonding metal; 154, Second bonding metal; 156, Barrier; 170, Insulating layer; 171, Patterned region; 01, Second surface; 02, Full insulating layer; 03, First opening; 04, Second opening; 05, Third opening; 06, Cut track; 101, Sacrificial material layer; 102, Interface material layer. Detailed Implementation

[0052] Exemplary embodiments of the present application will now be described in more detail with reference to the accompanying drawings. While exemplary embodiments of the present application are shown in the drawings, it should be understood that the present application may be implemented in various forms and should not be limited to the specific embodiments set forth herein. Rather, these embodiments are provided to enable a more thorough understanding of the present application and to fully convey the scope of the disclosure of the present application to those skilled in the art.

[0053] In the following description, numerous specific details are set forth in order to provide a more thorough understanding of this application. However, it will be apparent to those skilled in the art that this application can be practiced without one or more of these details. In other instances, to avoid confusion with this application, some technical features well-known in the art have not been described; that is, not all features of actual embodiments are described herein, nor are well-known functions and structures described in detail.

[0054] In the accompanying drawings, for clarity, the dimensions of layers, areas, and elements, as well as their relative dimensions, may be exaggerated. The same reference numerals denote the same elements throughout.

[0055] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, components, areas, layers, and / or portions, these elements, components, areas, layers, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, area, layer, or portion from another element, component, area, layer, or portion. Therefore, without departing from the teachings of this application, the first element, component, area, layer, or portion discussed below may be referred to as a second element, component, area, layer, or portion. And the discussion of a second element, component, area, layer, or portion does not imply that the first element, component, area, layer, or portion necessarily exists in this application.

[0056] Spatial relation terms such as “below,” “under,” “below,” “under,” “above,” “above,” etc., are used herein for convenience of description to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms are intended to also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, then the element or feature described as “below,” “under,” or “below” other elements or features will be oriented “above” other elements or features. Therefore, the exemplary terms “below” and “under” can include both above and below orientations. The device may be otherwise oriented (rotated 90 degrees or otherwise) and the spatial descriptive terms used herein will be interpreted accordingly.

[0057] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the scope of this application. When used herein, the singular forms “a,” “an,” and “the” are also intended to include the plural forms unless the context clearly indicates otherwise. It should also be understood that the terms “comprising” and / or “including,” when used in this specification, identify the presence of the stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups. When used herein, the term “and / or” includes any and all combinations of the associated listed items.

[0058] To fully understand this application, detailed steps and structures will be presented in the following description to illustrate the technical solution of this application. Preferred embodiments of this application are described in detail below; however, in addition to these detailed descriptions, this application may have other implementation methods.

[0059] like Figure 1 and Figure 2 As shown, an embodiment of this application provides a MEMS sensor 100, including a first wafer 110, a second wafer 130, a functional layer 111 disposed on the first wafer 110, and an insulating isolation layer 170. The functional layer 111 includes a first region 111a covered by the second wafer 130 and a second region 111b surrounding the first region 111a. The second region 111b of the functional layer 111 is provided with a plurality of pads 113; the functional layer 111 is provided with trenches 112 corresponding to the pads 113; the insulating isolation layer 170 covers the bottom wall and sidewalls of the trenches 112.

[0060] It is understood that the trenches 112 and pads 113 are configured in a one-to-one correspondence. Furthermore, in this embodiment, the trenches 112 surround the pads 113. It is understood that in other feasible embodiments, the trenches are not limited to surrounding the pads; they may also be located only on one side of the pads, as long as they effectively separate the pads from other cables.

[0061] The MEMS sensor 100 undergoes a chip dicing process during its fabrication. The inventors discovered that particles generated during chip dicing can easily fall into the trench 112, potentially causing short circuits, damaging the electrical performance of the MEMS sensor 100, and even rendering it a defective product, thus reducing its yield. In this embodiment, an insulating layer 170 covers the bottom and sidewalls of the trench 112. Even if particles fall into the trench 112 during chip dicing, short circuits are prevented. This avoids short circuits caused by particles falling into the trench 112 during subsequent chip dicing processes, better ensuring the stability of the MEMS sensor 100's electrical performance and improving its product yield.

[0062] Optionally, see Figure 1 The insulating layer 170 fills the trench 112 completely, thereby preventing particles from falling into the trench 112.

[0063] Understandable Figure 2The shape, arrangement, and position of the pads are only shown schematically. It is understood that in other feasible embodiments, the shape, arrangement, and position of the pads can be set as needed, according to conventional choices in the art, and will not be elaborated here.

[0064] Optionally, the insulating layer 170 is a polyimide layer. Of course, it is understood that the insulating layer 170 is not limited to polyimide material, as long as it can achieve the aforementioned insulating effect and does not affect the performance of the MEMS sensor.

[0065] Optionally, the material of the first wafer 110 may be silicon, germanium, silicon-germanium, silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, or indium antimonide, etc., or it may be silicon-on-insulator (SOI) or germanium-on-insulator (GOI), or it may be other materials, such as GaAs, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP, or GaInAsP, etc., or it may be a combination of the above materials.

[0066] Similarly, optionally, the material of the second wafer 130 can be silicon, germanium, silicon-germanium, silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, or indium antimonide, etc., or it can be silicon-on-insulator (SOI) or germanium-on-insulator (GOI), or it can be other materials, such as GaAs, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP, or GaInAsP, etc., or it can be a combination of the above materials. Of course, in a unified MEMS sensor, the materials of the first wafer 110 and the second wafer 130 can be the same or different.

[0067] In this embodiment, the MEMS sensor 100 further includes a sacrificial material layer 101 and an interface material layer 102 sequentially disposed on the first wafer, with the interface material layer 102 disposed between the sacrificial material layer 101 and the functional layer 111. The interface material layer 102 may include one of silicon oxide, silicon nitride, and silicon oxynitride.

[0068] This application only schematically illustrates the structures of the sacrificial material layer 101, the interface material layer 102, and the functional layer 111. Specifically, those skilled in the art can use conventional techniques as needed to configure them, which will not be elaborated here.

[0069] like Figure 3 As shown, another embodiment of the MEMS sensor 200 provided in this application differs from the MEMS sensor 100 in that the insulating isolation layer 170 also covers the side surface of the pad 113. This better prevents short circuits in the pad 113 that might occur when particles fall into the trench 112.

[0070] like Figure 4 As shown, the MEMS sensor 300 provided in one embodiment of this application differs from the MEMS sensor 100 in that it further includes a bonding structure 150. The bonding structure 150 is disposed between the functional layer 111 and the second wafer 130. The bonding structure 150 has a bonding surface 151. An insulating isolation layer 170 covers the side surface of the bonding structure 150 to insulate the bonding surface 151 of the bonding structure 150 from the external environment.

[0071] Understandably, based on common knowledge in the art, in addition to being disposed on the first wafer 110 and the second wafer 130, the projection of the bonding structure 150 on the first wafer 110 completely falls on the first wafer 110, and the projection of the bonding structure 150 on the second wafer 130 also completely falls on the second wafer 130. Furthermore, the bonding structure 150 is provided for the packaging of MEMS sensors; generally, while the bonding structure 150 is disposed between the first wafer 110 and the second wafer 130, it is also located at the edge of the first wafer 110 and the second wafer 130.

[0072] By setting the insulating isolation layer 170, the bonding surface 151 of the bonding structure 150 is insulated from the external environment, which can effectively prevent water vapor in the external environment from eroding the bonding surface 151 and entering the MEMS sensor, thereby better protecting the electrical performance of the MEMS sensor and improving the reliability of the MEMS sensor.

[0073] In this embodiment, the insulating layer 170 is directly attached to the bonding structure 150. It is understood that in other feasible embodiments, the insulating layer may also have a gap with the bonding structure, covering at least a portion of the side surface of the bonding structure, thereby insulating the bonding surface of the bonding structure from the external environment.

[0074] Of course, it is understandable that the bonding structure 150 is ring-shaped.

[0075] In this embodiment, the bonding structure 150 includes a first bonding metal 152 disposed on a first wafer 110, a second bonding metal 154 disposed on a second wafer 130, and baffles 156 disposed on the inner and outer sides of the first bonding metal 152. The surface where the first bonding metal 152 and the second bonding metal 154 are joined is the bonding surface 151. In this embodiment, the baffle 156 is located on the bottom side of the second bonding metal 154, and the baffle 156 and the second bonding metal 154 are in approximately contact. Therefore, in this embodiment, the insulating isolation layer 170 only needs to cover part of the side surface of the bonding structure 150, covering the area where the baffle 156 and the second bonding metal 154 are joined. Further, specifically, in this embodiment, the insulating isolation layer 170 covers part of the baffle 156 and extends to the second bonding metal 154, thus enclosing the area between the baffle 156 and the second bonding metal 154. It should be noted that the insulating isolation layer 170 can also cover part of the side surface of the bonding structure 150 by filling the gap between the barrier wall 156 and the second bonding metal 154.

[0076] Thus, by covering the gap between the barrier 156 and the second bonding metal 154 with the insulating isolation layer 170, the bonding surface 151 is isolated from the external environment, thereby preventing moisture from the external environment from corroding the bonding surface 151 and entering the MEMS sensor. This effectively avoids the influence of moisture in the external environment on the electrical performance of the MEMS sensor and improves the reliability of the MEMS sensor.

[0077] Optionally, the bonding metal material includes germanium. It is understood that, in other feasible embodiments, the specific structure of the bonding structure is not limited to this, and is not limited to metal bonding; bonding between the first and second wafers can also be achieved through adhesives or the like.

[0078] Optionally, the material of the barrier 156 is silicon oxide. It is understood that, in other feasible embodiments, the material of the barrier 156 is not limited to silicon oxide, but may be other materials conventionally chosen in the art.

[0079] Of course, the material of the barrier 156 is not limited to a single material such as silicon dioxide; it can also be formed from multiple materials. For example, the barrier includes a main body portion disposed on the surface of the functional layer and a metal layer covering the upper and side surfaces of the main body portion. During metal bonding, the barrier can prevent molten fluid from flowing into the central region and can also be used to control the degree of reaction, avoiding insufficient or excessive reaction. Due to the protection of the metal layer, the barrier is less susceptible to damage from the cavity release process before bonding, resulting in better quality and facilitating the formation of a stable bonding structure, thus improving the quality of the bonding structure and the performance of the sensor. The metal protective layer can be formed together with the bonding metal, requiring no additional processes and simplifying the process.

[0080] like Figure 5 As shown, another embodiment of the MEMS sensor 400 provided in this application differs from the MEMS sensor 300 in that the outer barrier 156 in the bonding structure is located outside the second bonding metal, rather than at the bottom, i.e., the second wafer 130. Thus, the top surface of the barrier 156 is directly opposite to the second wafer 130. The insulating layer 170 achieves insulation isolation between the bonding surface 151 and the external environment by wrapping the area where the barrier 156 connects to the second wafer 130. Similarly, if there is a gap between the barrier 156 and the second wafer 130, the insulating layer 170 can also achieve insulation isolation between the bonding surface 151 and the external environment by filling the gap.

[0081] like Figure 6 As shown, another embodiment of this application provides a MEMS sensor 500, which differs from the MEMS sensor 300 in that the insulating isolation layer 170 completely covers the outer surface of the bonding structure 150 and extends to cover a portion of the second wafer 130. This more effectively severs all possible channels on the bonding structure 150 that could lead to communication between the bonding surface 151 and the external environment.

[0082] In this application, the functional layer refers to the layer structure in a MEMS sensor that realizes electrical functions through metal layers, such as a capacitor layer. The specific layer can be selected based on the type of MEMS sensor and conventional design practices in this field, and will not be elaborated further here.

[0083] like Figure 7 and Figure 8 As shown, another embodiment of this application provides a MEMS sensor 600, which differs from the MEMS sensor 500 in that the surface of the second wafer 130 opposite to the first wafer 110 is a first surface 131, and the insulating isolation layer 170 at least partially covers the first surface 131 of the second wafer 130; the insulating isolation layer 170 includes a patterned region 171 covering the first surface 131 of the second wafer 130. The patterned region 171 enhances the aesthetic appeal of the MEMS sensor 400, or the patterned shape represents information such as the model number of the MEMS sensor 400, thereby facilitating the identification of the MEMS sensor 400.

[0084] Of course, it is understood that in other feasible embodiments, the specific shape of the patterned region 171 can be defined as needed, which will not be elaborated here.

[0085] Of course, in this embodiment, the insulating isolation layer 170 also covers the side surface of the second wafer 130, thereby more effectively cutting off all channels that may appear on the bonding structure 150 that would cause the bonding surface 151 to communicate with the external environment.

[0086] like Figure 9 As shown, another embodiment of this application provides a MEMS sensor 700, which differs from the MEMS sensor 600 in that the insulating isolation layer 170 also covers the side surface of the pad 113. This better prevents short circuits in the pad 113 that might occur when particles fall into the trench 112.

[0087] like Figure 10 As shown, another embodiment of this application provides a MEMS sensor 800, which differs from the MEMS sensor 300 in that the bonding structure 150 only includes a first bonding metal 152 and a second bonding metal 154, without any blocking walls. The insulating isolation layer 170 directly covers the outer surfaces of the first bonding metal 152 and the second bonding metal 154. Of course, in other feasible embodiments, the insulating isolation layer is not limited to completely covering the outer surfaces of the first bonding metal and the second bonding metal; it can cover the bonding surface between the first bonding metal and the second bonding metal.

[0088] One embodiment of this application also provides an electronic device, which includes the MEMS sensor provided in this application.

[0089] In the aforementioned electronic device, the MEMS sensor has an insulating layer covering the bottom and sidewalls of the trench. This prevents particles that may fall into the trench during subsequent chip cutting processes, thus avoiding short circuits and ensuring the stability of the electrical performance of the MEMS sensor, thereby improving the product yield of the MEMS sensor.

[0090] One embodiment of this application also provides a method for fabricating the MEMS sensor provided in this application, see [link to relevant documentation]. Figure 11 The steps include:

[0091] SO1. A preliminary MEMS sensor body is provided; the preliminary MEMS sensor body includes a first wafer, a second wafer, and a functional layer; the functional layer is provided with a plurality of pads and a plurality of trenches corresponding to the pads;

[0092] SO2, before the slicing process, forms an insulating and protective full-coverage layer on the MEMS sensor substrate;

[0093] SO3, pattern the insulating isolation full-coverage layer to at least expose the pads on the second wafer, forming an insulating isolation layer that at least covers the bottom and sidewalls of the trench.

[0094] The above-mentioned MEMS sensor fabrication method covers the bottom and side walls of the trench with an insulating isolation layer, thereby preventing particles that may be generated during subsequent chip dicing processes from falling into the trench and thus avoiding short circuits. This better ensures the stability of the electrical performance of the MEMS sensor and improves the product yield of the MEMS sensor.

[0095] It is understood that the functional layer is disposed on the first wafer; the functional layer includes a first region covered by the second wafer and a second region surrounding the first region; a plurality of pads are disposed on the second region of the functional layer. For ease of description, the surface of the MEMS sensor prototype on which the second wafer is disposed is defined as the second surface. In step S02, an insulating isolation full-coverage layer is formed on the second surface of the MEMS sensor prototype.

[0096] It should be noted that the second surface refers to the surface of the MEMS sensor body located on the corresponding side, including the surface of the second wafer that is away from the first wafer, and the surface of the functional layer that is away from the first wafer and is not covered by the second wafer.

[0097] It is understandable that the above steps are only used to form an insulating layer. In the fabrication method of forming a MEMS sensor, after step S03, there is also a step of obtaining several MEMS sensors by chip dicing.

[0098] It is understandable that the initial MEMS sensor provided in step SO1 has already completed the following steps;

[0099] a. Bonding of the first wafer and the second wafer;

[0100] b. Grinding and thinning the back side of the first wafer;

[0101] c. Patterning of the second wafer.

[0102] Optionally, step S02 includes:

[0103] An insulating material is coated onto the MEMS sensor substrate.

[0104] It is understood that, in other feasible embodiments, the method of forming the insulating and protective full-coverage layer is not limited to coating. Alternatively, a suitable method can be selected based on the material chosen for the insulating and protective full-coverage layer, without affecting the performance and use of the MEMS sensor.

[0105] Optionally, see Figure 12 Step S03 includes:

[0106] S031. Coat the insulating and protective full-coverage layer with photoresist and expose and develop it.

[0107] S032. High-temperature curing to form the insulating layer.

[0108] In step S031, exposure and development are performed to form an opening. The specific opening configuration is determined based on the design structure of the insulating layer.

[0109] Optionally, in step S032, the high-temperature curing temperature is 350℃-450℃. Of course, in other feasible embodiments, the high-temperature curing temperature is not limited to this, as long as the curing purpose is achieved and the performance and structure of other structures are not affected.

[0110] Optionally, in step S03, the insulating isolation layer formed by patterning the insulating isolation full-coverage layer also covers the side surface of the pad.

[0111] Optionally, in step S03, the MEMS sensor prototype further includes a bonding structure; the bonding structure is disposed between the functional layer and the second wafer; the bonding structure has a bonding surface;

[0112] The insulating layer formed by patterning the insulating isolation full-coverage layer also covers at least a portion of the side surfaces of the bonding structure to insulate the bonding surfaces of the bonding structure from the external environment.

[0113] Optionally, in step S03, the insulating isolation layer formed by patterning the insulating isolation full-coverage layer completely covers the outer surface of the bonding structure and extends to cover at least a portion of the second wafer;

[0114] And / or, the insulating isolation layer formed by patterning the insulating isolation full-coverage layer completely covers the outer surface of the bonding structure and extends to cover at least part of the functional layer.

[0115] Optionally, in step S03, the surface of the second wafer opposite to the first wafer is the first surface; the insulating isolation layer formed by patterning the insulating isolation full-coverage layer also at least partially covers the first surface of the second wafer.

[0116] To better understand the fabrication methods of MEMS sensors, the following section uses MEMS sensor 700 as an example to briefly describe its fabrication process.

[0117] Specifically, the fabrication process of the MEMS sensor 700 includes the following steps:

[0118] S01, Provide the initial MEMS sensor body; see [link / reference] Figure 13aThe MEMS sensor prototype includes a first wafer 110, a second wafer 130, a functional layer 111, and a bonding structure 150; the first wafer 110 and the second wafer 130 are disposed opposite to each other; the bonding structure 150 is disposed between the functional layer 111 and the second wafer 130; the bonding structure 150 has a bonding surface 151; the surface of the MEMS sensor prototype with the second wafer 130 is a second surface 01;

[0119] S02. An insulating material is coated on the second surface of the MEMS sensor substrate to form an insulating and isolation full-coverage layer O2. (See also...) Figure 13b ;

[0120] S031. Photoresist is coated on the insulating and protective full-coverage layer 02 and then exposed and developed.

[0121] The purpose of step S031 is to remove portions of the insulating cover layer that affect electrical connections by forming openings. (See also...) Figure 13c Specifically, the openings include a first opening 03 corresponding to the pad 113, a second opening 04 corresponding to the cut track 06, and a third opening 05 formed to form a patterned area.

[0122] It is understandable that the dicing track corresponding to the second opening is the dicing track used during chip cutting, located on the first wafer 110.

[0123] S032. High-temperature curing to form the insulating layer 170.

[0124] It should be noted that the MEMS sensor embodiments and the MEMS sensor fabrication method embodiments provided in this application belong to the same concept; the technical features in the technical solutions described in each embodiment can be arbitrarily combined without conflict. However, it should be further noted that the combination of technical features of the MEMS sensor provided in the embodiments of this application can already solve the technical problems to be solved by this application; therefore, the MEMS sensor provided in the embodiments of this application is not limited to the MEMS sensor fabrication method provided in the embodiments of this application, and any MEMS sensor that can be fabricated by the MEMS sensor fabrication method provided in the embodiments of this application is within the scope of protection of this application.

[0125] It should be understood that the above embodiments are exemplary and are not intended to encompass all possible implementations included in the claims. Various modifications and changes can be made to the above embodiments without departing from the scope of this disclosure. Similarly, the various technical features of the above embodiments can be arbitrarily combined to form other embodiments of the present invention that may not be explicitly described. Therefore, the above embodiments only illustrate several implementations of the present invention and do not limit the scope of protection of this patent.

Claims

1. A MEMS sensor, characterized in that, include: First wafer; The second wafer is disposed opposite to the first wafer; The functional layer is disposed on the first wafer; The functional layer includes a first region covered by the second wafer and a second region surrounding the first region and not covered by the second wafer; the second region of the functional layer is provided with a plurality of pads; the functional layer is provided with trenches corresponding to the pads; and An insulating layer covers the bottom and sidewalls of the trench.

2. The MEMS sensor according to claim 1, characterized in that, The insulating layer also covers the side surface of the pad.

3. The MEMS sensor according to claim 1, characterized in that, It also includes a bonding structure; the bonding structure is disposed between the functional layer and the second wafer; the bonding structure has a bonding surface; the insulating isolation layer also covers at least a portion of the side surface of the bonding structure to insulate the bonding surface of the bonding structure from the external environment.

4. The MEMS sensor according to claim 3, characterized in that, The insulating layer completely covers the outer surface of the bonding structure and extends to cover at least a portion of the second wafer; And / or, the insulating isolation layer completely covers the outer surface of the bonded structure and extends to cover at least part of the functional layer.

5. The MEMS sensor according to claim 1, characterized in that, The surface of the second wafer opposite to that of the first wafer is the first surface, and the insulating layer also at least partially covers the first surface of the second wafer.

6. An electronic device, characterized in that, Includes the MEMS sensor described in any one of claims 1-5.

7. A method for fabricating a MEMS sensor, characterized in that, Including the following steps: A preliminary MEMS sensor body is provided; the preliminary MEMS sensor body includes a first wafer, a second wafer, and a functional layer; the functional layer includes a first region covered by the second wafer, and a second region surrounding the first region and not covered by the second wafer; the second region of the functional layer is provided with a plurality of pads and a plurality of trenches corresponding to the pads; An insulating and protective full-coverage layer is formed on the MEMS sensor prototype before the slicing process; The insulating isolation layer is patterned to at least expose the pads and at least cover the bottom and sidewalls of the trench, forming an insulating isolation layer.

8. The method for fabricating a MEMS sensor according to claim 7, characterized in that, The process of forming an insulating and protective full-coverage layer on the initial MEMS sensor body before the slicing process includes: An insulating material is coated onto the MEMS sensor substrate.

9. The method for fabricating a MEMS sensor according to claim 7, characterized in that, The patterning of the insulating isolation full-coverage layer to at least expose the pads and at least cover the bottom and sidewalls of the trench to form an insulating isolation layer includes: Photoresist is coated onto the insulating and protective full-coverage layer and then exposed and developed. High-temperature curing is used to form the insulating layer.

10. The method for fabricating a MEMS sensor according to any one of claims 7-9, characterized in that, The insulating isolation layer, formed by patterning the insulating isolation full-coverage layer, also covers the side surface of the pad.

11. The method for fabricating a MEMS sensor according to any one of claims 7-9, characterized in that, The MEMS sensor substrate further includes a bonding structure; the bonding structure is disposed between the functional layer and the second wafer; the bonding structure has a bonding surface. The insulating layer formed by patterning the insulating isolation full-coverage layer also covers at least a portion of the side surfaces of the bonding structure to insulate the bonding surfaces of the bonding structure from the external environment.

12. The method for fabricating a MEMS sensor according to claim 11, characterized in that, The insulating isolation layer, formed by patterning the insulating isolation full-coverage layer, completely covers the outer surface of the bonding structure and extends to cover at least a portion of the second wafer; And / or, the insulating isolation layer formed by patterning the insulating isolation full-coverage layer completely covers the outer surface of the bonding structure and extends to cover at least part of the functional layer.

13. The method for fabricating a MEMS sensor according to any one of claims 7-9, characterized in that, The surface of the second wafer opposite to that of the first wafer is the first surface; the insulating isolation layer formed by patterning the insulating isolation full-coverage layer also at least partially covers the first surface of the second wafer.

Citation Information

Patent Citations

  • Component with a via and method for producing it

    CN103038156A

  • MEMS sensor and forming method thereof

    CN111439721A