A preparation method and application of a composite ZnO / ZnS nanoarray film
ZnO nanoarray films were grown by simple vapor deposition and liquid phase methods, and complex ZnO/ZnS nanoarray films were prepared by in-situ vulcanization, which solved the problems of complex preparation process and poor responsiveness of existing ZnO films, and achieved room temperature Highly sensitive hydrogen sulfide gas detection, suitable for industrial production and gas sensor applications.
Patent Information
- Application Number
- CN202211320815.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-10-26
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2042-10-26
AI Technical Summary
The existing ZnO thin film preparation process is complex and costly, and has poor responsiveness to hydrogen sulfide gas at low temperatures, making it difficult to achieve industrial production and efficient gas monitoring.
A simple vapor evaporation method was used to grow the ZnO seed crystal layer, and then a nanoarray film was grown on the ZnO seed crystal through a liquid phase method, and a complex ZnO/ZnS nanoarray film was prepared by an in-situ vulcanization method to achieve firm bonding with the base material. .
It achieves simplification of the preparation process, reduction of energy consumption and high-sensitivity detection of hydrogen sulfide gas at room temperature. It is suitable for array applications of gas sensors and has high selectivity and rapid response.
Smart Images

Figure CN115595565B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of semiconductor technology, and in particular to a preparation method of a composite ZnO / ZnS nanometer array film and its application. Background Art
[0002] The deteriorating ecological environment has given rise to an urgent need for efficient and real-time monitoring of gases. Although gas sensors have been widely used to detect various toxic, harmful, explosive and volatile substances, with the increasing development of science and technology, gas sensors are also constantly developing in the direction of thin film, nanometer and array. Room temperature detection is a prerequisite for achieving thin film and array development.
[0003] At present, there are many preparation technologies for ZnO thin films. Traditional vapor phase growth methods such as magnetron sputtering have complex processes, expensive equipment and high costs. Array thin films prepared by liquid phase growth methods mostly grow a ZnO seed layer first, and then prepare thin films by chemical methods. The physical method is used to prepare the ZnO seed layer, which can obtain a seed layer with good crystallinity and stable adhesion to the substrate surface, such as preparing zinc oxide nanorod arrays on a silicon substrate by magnetron sputtering; ZnO seeds are prepared on a conductive glass substrate by magnetron sputtering. Compared with the magnetron sputtering method, considering the complexity and cost of the process, more researchers use the sol-gel method to prepare the ZnO seed layer, and then use the hydrothermal method or liquid phase deposition method to grow the thin film. However, the seed layer prepared by the sol-gel method has a low degree of bonding with the substrate, and most of them require more than three immersion film-forming processes. The process is relatively complicated and the structure of the seed layer is difficult to control. Therefore, seeking a simple and controllable preparation process is the basis for achieving industrialization. At the same time, the traditional single ZnO gas-sensitive film has poor responsiveness to hydrogen sulfide gas at low temperatures and is easily corroded by hydrogen sulfide gas. Therefore, a preparation method of a composite ZnO / ZnS nanoarray film and its application are urgently needed to solve the above problems. Summary of the invention
[0004] The technical problem to be solved by the present invention is to overcome the above technical problems and provide a method for preparing a composite ZnO / ZnS nanoarray film with simple preparation process, reasonable design, low energy consumption and room temperature sensitivity and its application.
[0005] In order to solve the above technical problems, the technical solution provided by the present invention is: a method for preparing a multiphase ZnO / ZnS nanoarray film, comprising the following steps:
[0006] S1: growing a ZnO seed layer on the surface of the interdigital electrode by simple vapor deposition using crystalline zinc acetate;
[0007] S2: Using crystalline zinc nitrate and 1,2-dimethylimidazole as reaction raw materials, ethanol and water as solvents, a ZnO nanoarray film is grown on ZnO seed crystals by a liquid phase method. The film is uniform and dense.
[0008] S3: ZnO nanoarray thin film is vertically grown on the interdigitated electrode substrate. The thickness of the nanoarray thin film is 50-100 nm and is firmly bonded to the substrate material.
[0009] S4: The interdigitated electrodes are subjected to in-situ sulfidation treatment using a sodium sulfide solution to prepare a ZnO / ZnS nanoarray film.
[0010] As an improvement, the interdigital electrodes in S1 are silicon-based electrodes or ceramic-based electrodes, and the line width and line spacing of the interdigital electrodes are both 20-30 microns.
[0011] As an improvement, the interdigital electrodes in S1 are cleaned with acetone and ethanol before use, and then dried for standby use.
[0012] As an improvement, the simple vapor phase evaporation method in S1 is to place a certain amount of crystalline zinc acetate powder in a quartz tube with a diameter of 1 cm and a height of 5 cm, and suspend a forked electrode 1-2 cm above the powder to ensure that the surface of the forked electrode is facing downward and parallel to the powder surface. The temperature of the bottom of the quartz tube is controlled at 200-220°C by a heating electric furnace, and the zinc acetate is heated to evaporate and deposited on the surface of the forked electrode above it. The evaporation time is controlled at 3-5 minutes. The forked electrode is placed in a muffle furnace and heated at 300-350°C for 1 hour to obtain a ZnO seed layer.
[0013] As an improvement, the molar ratio of crystalline zinc nitrate to 1,2-dimethylimidazole in S2 is 1:1-2.
[0014] As an improvement, the steps of the liquid phase method in S2 are: dissolving crystalline zinc nitrate and 1,2-dimethylimidazole in a mixture of ethanol and water in a ratio of 1:4, stirring for 20-30 minutes to fully mix them to obtain a mixed solution; suspending the interdigital electrode with ZnO seeds in the mixed solution for immersion growth for 12-24 hours, then taking it out and rinsing it with ethanol; placing the interdigital electrode in a muffle furnace, heating it at 400-450°C for 1 hour, and obtaining a ZnO nanoarray film.
[0015] As an improvement, the in-situ sulfurization reaction in S4 is to suspend the ZnO nanoarray film in a sodium sulfide solution, the concentration of the sodium sulfide aqueous solution is 0.3 mol / L, the sulfurization temperature is 60-70°C, the sulfurization time is 3-5 minutes, and the obtained interdigitated electrode is washed with deionized water and dried in a forced air drying oven at 80-90°C for 1-2 hours to obtain a ZnO / ZnS nanoarray film.
[0016] An application of a composite ZnO / ZnS nanoarray film is to install the ZnO / ZnS nanoarray film prepared by the above preparation method on the fixed pin of the electrode to obtain a thin film ZnO / ZnS room temperature H2S gas sensitive sensor.
[0017] After adopting the above structure, the present invention has the following advantages:
[0018] 1. The present invention adopts a simple vapor deposition method to directly prepare the ZnO seed layer, so that the size of the ZnO nanocrystal seed is controllable, the operability is strong, the reproducibility is good, the preparation process is simple, and it is suitable for large-scale and industrial production;
[0019] 2. The present invention uses an in-situ sulfurization method to realize the application of ZnO / ZnS nanoarray film in room temperature hydrogen sulfide gas detection and leakage alarm. It has high safety in use and is suitable for array applications of gas sensors.
[0020] The above summary is for illustrative purposes only and is not intended to be limiting in any way. In addition to the illustrative aspects, embodiments and features described above, further aspects, embodiments and features of the present invention will be readily apparent by reference to the accompanying drawings and the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 This is a SEM picture of a ZnS / ZnO nanoarray film obtained in a method for preparing a composite ZnO / ZnS nanoarray film of the present invention.
[0022] Figure 2 This is an XRD diagram of the ZnS / ZnO nanoarray film obtained in Example 1 of a method for preparing a composite ZnO / ZnS nanoarray film of the present invention.
[0023] Figure 3 This is a room temperature resistance response recovery curve of the ZnS / ZnO nanoarray thin film gas sensor obtained in Example 2 of the preparation method of a composite ZnO / ZnS nanoarray thin film of the present invention to 10 ppm hydrogen sulfide gas.
[0024] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or technical descriptions will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work. DETAILED DESCRIPTION
[0025] In the following, only some exemplary embodiments are briefly described. As those skilled in the art will appreciate, the described embodiments may be modified in various ways without departing from the spirit or scope of the present invention. Therefore, the drawings and descriptions are considered to be exemplary and non-restrictive in nature.
[0026] The embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0027] Combination Figure 1-Figure 3 The simple vapor deposition method evaporates and deposits crystalline zinc acetate into a film at a temperature of 180-200°C. By controlling the heating temperature, the position of the interdigital electrodes and the deposition time, the thickness and grain size of the ZnO seed layer can be controlled. Moreover, the film formed by the simple vapor deposition method is firmly bonded to the surface of the interdigital electrodes, which effectively reduces the lattice mismatch between the later sheet zinc oxide array and the surface of the interdigital electrodes. The use of crystalline zinc nitrate and 1,2-dimethylimidazole to prepare ZnO flake crystals is to obtain a surface that is highly sensitive to hydrogen sulfide. At the same time, the in-situ sulfidation method is also used to obtain a surface that is highly sensitive to hydrogen sulfide. The gas sensor obtained by the above preparation method has a sensitivity of more than 3 to 10ppm hydrogen sulfide gas at room temperature, and a response time of less than 20s. Under the same test conditions, the responsiveness of the gas sensor to 100ppm ethanol, formaldehyde, ammonia and methane gases is very low. Therefore, the gas sensor has a high selectivity to hydrogen sulfide gas.
[0028] Embodiment 1
[0029] Weigh 0.5 g of crystalline zinc acetate powder and place it in a quartz tube with a diameter of 1 cm and a height of 5 cm. Hang an interdigital electrode 1 cm above the powder. The interdigital electrode is a silicon-based electrode with a line width and a line spacing of 20 μm. Before use, the interdigital electrode is cleaned with acetone and ethanol respectively to ensure that the surface of the interdigital electrode is facing downward and parallel to the powder surface. Use a heating electric furnace to control the temperature of the bottom of the quartz tube to 220°C. Heat to evaporate zinc acetate. The evaporation time is controlled within 3 minutes. Then place the interdigital electrode in a muffle furnace and heat at 300°C for 1 hour. Zinc acetate is decomposed to obtain a ZnO seed layer. Crystalline zinc nitrate and 1,2-dimethylimidazole are weighed according to a molar ratio of 1:1 and dissolved in a mixture of ethanol and water. The ratio of ethanol to water is 1:4. Stir for 20 After 30 minutes, the mixed solution was obtained. The interdigital electrode with ZnO seeds was suspended in the mixed solution and immersed in the growth for 24 hours. It was then taken out and rinsed with ethanol, and then placed in a muffle furnace and heated at 400°C for 1 hour to obtain a ZnO nanoarray film. The ZnO nanoarray film was suspended in a sodium sulfide solution for in-situ sulfidation reaction. The concentration of the sodium sulfide aqueous solution was 0.3 mol / L, the sulfidation temperature was 60°C, and the sulfidation time was 5 minutes. The obtained interdigital electrode was washed with deionized water and dried in a blast drying oven at 80°C for 1 hour to obtain a ZnO / ZnS nanoarray film. The ZnO / ZnS nanoarray film was installed on the fixed pin of the electrode to obtain a thin film ZnO / ZnS gas sensitive sensor for detecting H2S gas at room temperature. After testing, its sensitivity to 10ppm hydrogen sulfide gas at room temperature can reach more than 5, the response time is less than 20s, and the selectivity for hydrogen sulfide gas is very high.
[0030] Embodiment 2
[0031] On the basis of Example 1, the temperature of the bottom of the quartz tube was changed to 200°C, the evaporation time was changed to 5 minutes, and the other preparation processes remained unchanged. The resulting ZnS / ZnO gas sensor had a sensitivity of more than 6 to 10ppm hydrogen sulfide gas at room temperature, a response time of less than 20s, and a high selectivity to hydrogen sulfide gas.
[0032] Embodiment 3
[0033] On the basis of Example 1, the molar ratio of liquid phase crystallized zinc nitrate and 1,2-dimethylimidazole was changed to 1:2, and the other preparation processes remained unchanged. The obtained ZnS / ZnO gas sensor had a sensitivity of more than 7.2 to 10ppm hydrogen sulfide gas at room temperature, a response time of less than 20s, and high selectivity to hydrogen sulfide gas.
[0034] Embodiment 4
[0035] On the basis of Example 1, the immersion growth time of the interdigital electrode with ZnO seed crystals suspended in the mixed solution is changed to 12 hours, and the other preparation processes remain unchanged. The resulting ZnS / ZnO gas sensor has a sensitivity of more than 3.5 to 10ppm hydrogen sulfide gas at room temperature, a response time of less than 20s, and a high selectivity to hydrogen sulfide gas.
[0036] Embodiment 5
[0037] On the basis of Example 1, the immersion growth time of the interdigital electrode with ZnO seed crystals suspended in the mixed solution was changed to 18 hours, and the other preparation processes remained unchanged. The resulting ZnS / ZnO gas sensor had a sensitivity of more than 4.4 to 10ppm hydrogen sulfide gas at room temperature, a response time of less than 20s, and a high selectivity to hydrogen sulfide gas.
[0038] Embodiment 6
[0039] On the basis of Example 1, the sintering temperature of the ZnO nanoarray film was changed to 450°C, and other preparation processes remained unchanged. The resulting ZnS / ZnO gas sensor had a sensitivity of more than 5 to 10ppm hydrogen sulfide gas at room temperature, a response time of less than 20s, and high selectivity to hydrogen sulfide gas.
[0040] Embodiment 7
[0041] On the basis of Example 1, the sulfurization time was changed to 3 minutes, and other preparation processes remained unchanged. The obtained ZnS / ZnO gas sensor had a sensitivity of more than 3.5 to 10ppm hydrogen sulfide gas at room temperature, a response time of less than 20s, and a high selectivity to hydrogen sulfide gas.
[0042] The present invention and its implementation methods are described above, but such description is not restrictive. The drawings show only one implementation method of the present invention, and the actual implementation method is not limited thereto. In short, if ordinary technicians in the field are inspired by it and design structural methods and implementation methods similar to the technical solution without creative design without departing from the purpose of the invention, they should all fall within the protection scope of the present invention.
Claims
1. A method for preparing a multiphase ZnO / ZnS nanoarray film, characterized in that: The following steps are involved: S1: growing a ZnO seed layer on the surface of the interdigital electrode by simple vapor deposition using crystalline zinc acetate; S2: Using crystalline zinc nitrate and 1,2-dimethylimidazole as reaction raw materials, and ethanol and water as solvents, a ZnO nanoarray film is grown on a ZnO seed crystal by a liquid phase method; the ZnO nanoarray film sheet is vertically grown on the interdigitated electrode substrate, the thickness of the nanoarray film sheet is 50-100nm, and it is firmly bonded to the substrate material; S3: In-situ sulfidation treatment of the interdigitated electrodes was performed using a sodium sulfide solution to prepare a ZnO / ZnS nanoarray film; The molar ratio of crystalline zinc nitrate to 1,2-dimethylimidazole in S2 is 1:1-2; The steps of the liquid phase method in S2 are: dissolving crystalline zinc nitrate and 1,2-dimethylimidazole in a mixture of ethanol and water in a ratio of 1:4, stirring for 20-30 minutes to fully mix them to obtain a mixed solution; suspending an interdigital electrode with ZnO seed crystals in the mixed solution for immersion growth for 12-24 hours, then taking it out and rinsing it with ethanol; placing the interdigital electrode in a muffle furnace, heating it at 400-450°C for 1 hour, and obtaining a ZnO nanoarray film.
2. The method for preparing a multiphase ZnO / ZnS nanoarray thin film according to claim 1, characterized in that: The interdigital electrodes in S1 are silicon-based electrodes or ceramic-based electrodes, and the line width and line spacing of the interdigital electrodes are both 20-30 microns.
3. The method for preparing a multiphase ZnO / ZnS nanoarray thin film according to claim 1, characterized in that: The interdigital electrodes in S1 are cleaned with acetone and ethanol before use, and then dried for later use.
4. The method for preparing a multiphase ZnO / ZnS nanoarray thin film according to claim 1, characterized in that: The simple vapor deposition method in S1 is to place a certain amount of crystalline zinc acetate powder in a quartz tube with a diameter of 1 cm and a height of 5 cm, suspend and place an interdigital electrode 1-2 cm above the powder, ensure that the surface of the interdigital electrode is facing downward and parallel to the powder surface, use a heating electric furnace to control the temperature of the bottom of the quartz tube to 200-220°C, heat to evaporate the zinc acetate, and deposit it on the surface of the interdigital electrode above it, the evaporation time is controlled to be 3-5 minutes, place the interdigital electrode in a muffle furnace, and heat it at 300-350°C for 1 hour to obtain a ZnO seed layer.
5. The method for preparing a multiphase ZnO / ZnS nanoarray thin film according to claim 1, characterized in that: The in-situ sulfurization reaction in S3 is to suspend the ZnO nanoarray film in a sodium sulfide solution, the concentration of the sodium sulfide aqueous solution is 0.3 mol / L, the sulfurization temperature is 60-70°C, the sulfurization time is 3-5 minutes, and the obtained interdigitated electrode is washed with deionized water and dried in a forced air drying oven at 80-90°C for 1-2 hours to obtain a ZnO / ZnS nanoarray film.
6. An application of a multiphase ZnO / ZnS nanoarray film, characterized in that: The ZnO / ZnS nanoarray film prepared by the preparation method described in any one of claims 1 to 5 is installed on the fixed pins of the electrode to obtain a thin film ZnO / ZnS gas sensor for detecting H2S gas at room temperature.