Double-sided polishing cloth repair process

By adopting a multi-step cloth repair process and an optimized emery wheel speed scheme in the double-sided polishing process, the problems of flatness deterioration caused by polishing cloth wear and easy wear of the emery wheel are solved, ensuring the stability and efficiency of the polishing process.

CN115609480BActive Publication Date: 2024-10-29ZHEJIANG LISHUI ZHONGXIN WAFER SEMICONDUCTOR MATERIALS CO LTD +1
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
CN202211229492.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-10-08
Publication Date
2024-10-29
Estimated Expiration
2042-10-08

AI Technical Summary

Technical Problem

In the existing double-sided polishing process, the flatness of the polishing cloth will deteriorate and the polishing efficiency will decrease due to wear during the processing, and the emery wheel is easy to wear, affecting the stability of the process.

Method used

A double-sided polishing cloth repair process is adopted. By testing the initial polishing cloth thickness, using an emery wheel to press the cloth, and adjusting the cloth repair program and grinding wheel speed according to the removal amount to ensure the smoothness of the polishing cloth and the removal amount, including Multiple dressing steps and optimized procedures to extend the life of the emery wheel.

Benefits of technology

It achieves the stability and flatness of the polishing process, extends the service life of the emery wheel, and avoids the decrease in polishing efficiency and the increase in silicon wafer scratches.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115609480B_ABST
    Figure CN115609480B_ABST
Patent Text Reader

Abstract

The present invention relates to a double-sided polishing cloth repairing process, belonging to the technical field of silicon wafer processing technology, including the following operating steps: the first step: testing the initial polishing cloth thickness N. The second step: then using a diamond grinding wheel A to repair the cloth and pressing it, and then using a cloth repairing program to repair the cloth. Cloth repairing program: in the first stage, grinding wheel speed: upper disk speed = 0.5-2:1, grinding wheel speed: lower disk speed = 2-10:-1 (negative value indicates the opposite direction of travel); in the second stage, grinding wheel speed: upper disk speed = 2-10:-1, grinding wheel speed: lower disk speed = 0.5-2:1. The third step: testing the polishing cloth thickness M after the cloth repairing, and obtaining the removal amount by N-M. The fourth step: when the thickness removal amount is less than 20-120 μm, using diamond grinding wheel A to press the cloth repairing again. The fifth step: when the thickness removal amount reaches 20-120 μm, using a grinding wheel to press the cloth repairing, the cloth repairing is completed after the cloth repairing removal amount reaches 10-30 μm. It has the characteristics of ensuring stable polishing and stable flatness. The problem of easy wear of diamond grinding wheels is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of silicon wafer processing technology, and in particular to a double-sided polishing cloth repairing process. Background Art

[0002] Double-sided polishing requires that polishing cloths be attached to the upper and lower plates of the machine, and then the silicon wafers be rotated and processed in the presence of polishing liquid to achieve high flatness of the silicon wafers.

[0003] After the polishing cloth is attached, it is usually necessary to "trim the cloth" to remove a certain surface layer. The purpose is to trim the uneven cloth surface to be sufficiently flat and uniform, so that the cloth state that meets the flatness requirements can be processed.

[0004] The first case is to put on a new cloth to repair the cloth. Repairing the cloth will make the surface flatness of the polishing cloth uniform, mainly to reduce the scratches on the silicon wafer caused by the uneven surface of the new cloth. At the same time, the flatness of the cloth can ensure the stability of the flatness parameters of the silicon wafer during processing. In order to achieve process repeatability, general processing companies will quantify the removal thickness of the new cloth, such as starting processing after removing 20 to 150 microns.

[0005] The second situation is to repair the cloth during the processing. As the processing amount increases, the surface microscopic state of the polishing cloth gradually becomes smooth (flat). The smooth surface state of the polishing cloth will lead to a decrease in the removal rate of the silicon wafer, that is, a decrease in the polishing efficiency. If no treatment is done, the flatness will eventually deteriorate and scratches will increase. At this time, the cloth also needs to be repaired. Summary of the invention

[0006] The present invention mainly solves the deficiencies in the prior art and provides a double-sided polishing cloth repairing process, which has the characteristics of ensuring stable polishing and stable flatness, and solves the problem of easy wear of diamond grinding wheels.

[0007] The above technical problems of the present invention are mainly solved by the following technical solutions:

[0008] A double-sided polishing cloth repair process includes the following steps:

[0009] Step 1: Test the initial polishing cloth thickness N.

[0010] Step 2: Then use diamond grinding wheel A to perform cloth repair and pressing, the cloth repair pressure is 100-200DaN, and then use the cloth repair procedure to repair the cloth.

[0011] Cloth repair procedure: In the first stage, grinding wheel speed: upper plate speed = 0.5~2:1, grinding wheel speed: lower plate speed = 2~10:-1 (negative value means the moving direction is opposite); in the second stage, grinding wheel speed: upper plate speed = 2~10:-1, grinding wheel speed: lower plate speed = 0.5~2:1.

[0012] Step 3: Test the polishing cloth thickness M after repairing, and get the removal amount through NM.

[0013] Step 4: When the thickness removal is less than 20-120 μm, use diamond grinding wheel A to press the repair cloth again.

[0014] Step 5: When the thickness removal reaches 20-120μm, use the grinding wheel to press the repair cloth. The repair is completed when the thickness removal reaches 10-30μm.

[0015] Preferably, the diamond wheel A can fix the diamond grit by electroplating or sintering, the mesh size of the diamond grit can be 60-200 meshes, and the number of pieces is 3 or 4; the diamond wheel B can fix the diamond grit by electroplating or sintering, the mesh size of the diamond grit can be 100-200 meshes, and the number of pieces is 3 or 4.

[0016] Preferably, when the number of the diamond grinding wheels A and B is 3, diamond grinding wheels have diamond grit on both sides; when the number of the diamond grinding wheels A and B is 4, diamond grinding wheels have diamond grit on one side or both sides.

[0017] Preferably, when the thickness removal amount is less than 40-90 μm, the grinding wheel A is repaired again using the optimal procedure; the optimal procedure: in the first stage, the grinding wheel speed: the upper disk speed = 2-10:-1, the grinding wheel speed: the lower disk speed = 4-8:1; in the second stage, the grinding wheel speed: the upper disk speed = 2-8:1, the grinding wheel speed: the lower disk speed = 2-10:-1.

[0018] Preferably, when the diamond grinding wheels A and B are being repaired, water or polishing liquid during processing flows out of the pipeline of the upper plate, with a flow rate of 4 to 12 L / min and a temperature of 16 to 30°C.

[0019] The present invention can achieve the following effects:

[0020] The invention provides a double-sided polishing cloth repairing process, which has the characteristics of ensuring stable polishing and stable flatness compared with the prior art, and solves the problem of easy wear of diamond grinding wheels. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 It is a schematic side view of the double-sided polishing structure of the present invention. DETAILED DESCRIPTION

[0022] The technical solution of the invention is further specifically described below through embodiments and in conjunction with the accompanying drawings.

[0023] Example: Figure 1 As shown, a double-sided polishing cloth repair process includes the following steps:

[0024] Step 1: Test the initial polishing cloth thickness N.

[0025] Step 2: Then use diamond grinding wheel A to perform cloth repair and pressing, the cloth repair pressure is 100-200DaN, and then use the cloth repair procedure to repair the cloth.

[0026] Cloth repair procedure: In the first stage, grinding wheel speed: upper plate speed = 0.5~2:1, grinding wheel speed: lower plate speed = 2~10:-1 (negative value means the moving direction is opposite); in the second stage, grinding wheel speed: upper plate speed = 2~10:-1, grinding wheel speed: lower plate speed = 0.5~2:1.

[0027] Step 3: Test the polishing cloth thickness M after repairing, and get the removal amount through NM.

[0028] Step 4: When the thickness removal is less than 20-120 μm, use diamond grinding wheel A to press the repair cloth again.

[0029] When the thickness removal amount is less than 40-90 μm, the grinding wheel A is dressed again using the optimal procedure; the optimal procedure: in the first stage, the grinding wheel speed: the upper disc speed = 2-10:-1, the grinding wheel speed: the lower disc speed = 4-8:1; in the second stage, the grinding wheel speed: the upper disc speed = 2-8:1, the grinding wheel speed: the lower disc speed = 2-10:-1.

[0030] Step 5: When the thickness removal reaches 20-120μm, use grinding wheel B to press the repair cloth. The repair is completed when the thickness removal reaches 10-30μm.

[0031] When the emery wheels A and B are being repaired, water or polishing liquid during processing flows out of the pipe of the upper plate, with a flow rate of 4 to 12 L / min and a temperature of 16 to 30°C.

[0032] The diamond grinding wheel A can be fixed with diamond grit by electroplating or sintering, the mesh of diamond grit can be 60-200 mesh, and the number of diamond grit is 3 or 4; the diamond grinding wheel B can be fixed with diamond grit by electroplating or sintering, the mesh of diamond grit can be 100-200 mesh, and the number of diamond grit is 3 or 4. When the number of diamond grinding wheels A and B is 3, diamond grit is present on both sides of the diamond grinding wheel; when the number of diamond grinding wheels A and B is 4, diamond grit is present on one or both sides of the diamond grinding wheel.

[0033] In summary, the double-sided polishing cloth repair process has the characteristics of ensuring stable polishing and stable flatness, and solves the problem of easy wear of the diamond grinding wheel.

[0034] The above description is only a specific embodiment of the present invention, but the structural features of the present invention are not limited thereto. Any changes or modifications made by any technician in the field of the present invention are included in the patent scope of the present invention.

Claims

1. A double-sided polishing cloth repair process, characterized in that The steps are as follows: Step 1: Test the initial polishing cloth thickness N; Step 2: Then use the diamond wheel A to perform cloth repair and pressing, the cloth repair pressure is 100-200DaN, and then use the cloth repair procedure to repair the cloth; the diamond wheel A fixes the diamond by electroplating or sintering, the mesh number of the diamond is 60-200 mesh, and the number of pieces is 3 or 4; Repairing procedure: In the first stage, grinding wheel speed: upper plate speed = 0.5~2:1, grinding wheel speed: lower plate speed = 2~10:-1; in the second stage, grinding wheel speed: upper plate speed = 2~10:-1, grinding wheel speed: lower plate speed = 0.5~2:1; negative values ​​indicate the opposite direction of travel; Step 3: Test the polishing cloth thickness M after repairing, and get the removal amount through NM; Step 4: When the thickness removal is less than 20 μm, use diamond grinding wheel A to press the repair cloth again; Step 5: When the thickness removal amount is between 20 and 120 μm, use the diamond wheel B to press the repair cloth. When the repair cloth removal amount is between 10 and 30 μm, the repair cloth is completed. The diamond wheel B fixes the diamond by electroplating or sintering. The mesh number of the diamond is 100 to 200, and the number of pieces is 3 or 4.

2. The double-sided polishing cloth repairing process according to claim 1, characterized in that: When the number of the emery grinding wheels A and B is 3, emery grinding wheels have emery grinding on both sides; when the number of the emery grinding wheels A and B is 4, emery grinding wheels have emery grinding on one side or both sides.

3. The double-sided polishing cloth repairing process according to claim 1, characterized in that: When the emery wheels A and B are being repaired, water or polishing liquid during processing flows out of the pipe of the upper plate, with a flow rate of 4 to 12 L / min and a temperature of 16 to 30°C.

Citation Information

Patent Citations

  • Finishing process of polishing cloth for double-sided polishing

    CN103817600A

  • Rough polishing process for ceramic product

    CN109648404A

  • Polishing cloth finishing loose pulley

    CN211332766U

  • Repairing disc of ceramic grinding and polishing equipment

    CN211517156U

  • Disc surface correction clamp for double-sided polishing of optical parts

    CN214723416U