An active agent for promoting crop growth and its preparation method and application
By using active agents with core-shell structures in the soil, heavy metals are cured and plant regulators are gradually released, the problems of solidification and crop growth of heavy metal-contaminated soil are solved, and soil fertility improvement and pollution prevention are achieved.
Patent Information
- Application Number
- CN202211435317.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-16
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2042-11-16
AI Technical Summary
Heavy metals polluted soil are difficult to degrade, causing heavy metals to enter the human body through the biological chain. The existing governance methods have problems such as incomplete governance and secondary pollution, which affect crop growth and soil fertility.
The substrate is made of natural zeolite particles and polyvinyl butyral, and combined with plant active agent and modified curing agent, the plant regulator and metal ion chelating agent are coated with the sustained release membrane layer to form a core-shell structure and cure it. Heavy metals and gradually release plant regulators to promote crop growth.
Effectively cure heavy metals in the soil to prevent recontamination, and stay in the soil for a long time as a water retention agent and soil plate preservation agent to enhance soil fertility, and gradually release plant regulators through a sustained release mechanism to promote crop growth and increase yield.
Smart Images

Figure CN115735911B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of soil improvement, and in particular to an active agent for promoting crop growth, and a preparation method and application thereof. Background Art
[0002] The content of the background technology is intended to increase the understanding of the present invention through some basic technical knowledge related to the present invention. Therefore, the following information does not necessarily constitute the knowledge known to those skilled in the art.
[0003] Heavy metal pollution is one of the main types of soil pollution. Soil heavy metal pollution refers to the pollution caused by human activities, which causes the content of trace metal elements in the soil to exceed the background value. At present, the pollutants facing my country's soil mainly include inorganic pollutants (such as cyanide, heavy metals, etc.), pesticides and polycyclic aromatic hydrocarbons, among which the sources of heavy metals mainly include sewage irrigation, mining pollution, atmospheric deposition, etc. Although the soil has a certain self-purification ability, the heavy metals that pollute the soil can generally only undergo morphological transformation and migration and are difficult to degrade. In this case, these heavy metals are easily absorbed by the human body through the "soil → plant → human body" food chain and are enriched in the human body, and are not easy to detect, which brings great potential harm to human health.
[0004] However, many methods for treating heavy metal-contaminated soil are not thorough enough and are prone to secondary pollution. In addition, for some relatively poor and heavy metal-contaminated lands, simply treating heavy metal pollution cannot guarantee the healthy growth of crops, but often leads to poor growth and low crop yields. Therefore, it is necessary to further study and explore the treatment and restoration technology of poor and heavy metal-contaminated soil to promote crop growth. Summary of the invention
[0005] The main purpose of the present invention is to provide an active agent for promoting crop growth and its preparation method and application, which can not only effectively fix heavy metals in the soil, but also release plant regulators into the soil for a longer period of time. To achieve the above invention purpose, the present invention discloses the following technical solutions:
[0006] First, the present invention discloses an active agent for promoting crop growth, which includes a matrix and a plant active agent and a modified curing agent distributed in the matrix. The matrix is a granular material formed by natural zeolite particles and polyvinyl butyral; the plant active agent includes natural zeolite particles containing a plant regulator and a slow-release film layer coated on the surface of the natural zeolite particles; the modified curing agent includes natural zeolite particles containing a metal ion chelating agent and a slow-release film layer coated on the surface of the natural zeolite particles, and the plant active agent and the modified curing agent are cured in the matrix.
[0007] Furthermore, the particle size of the natural zeolite particles in the matrix is 400-500 meshes; the particle size of the natural zeolite particles in the plant active agent and the modified curing agent is 100-250 meshes.
[0008] Furthermore, the plant regulator includes at least one of 2,4-dichlorophenoxyacetic acid, sodium nitrophenolate, succinamic acid, chlormequat, sodium naphthylacetate, potassium indolebutyrate, etc., and may also be any other suitable plant regulator. Plant regulators play an important role in regulating the growth, development and metabolism of crops and promote crop growth.
[0009] Furthermore, the metal ion chelating agent includes at least one of citric acid, tartaric acid, sodium gluconate, dithiocarbamate (such as sodium salt, potassium salt, etc.), etc., which can chelate and solidify the heavy metal ions entering the matrix to avoid easy transfer and re-contamination.
[0010] Furthermore, the raw materials of the slow-release membrane include 10 to 17 parts by weight of membrane material, 2 to 3.1 parts by weight of graphite powder, and 0.4 to 0.65 parts by weight of polyvinyl alcohol. The membrane material includes any one of microcrystalline wax, paraffin wax, etc. The slow-release membrane of the present invention can not only effectively prolong the release time of the plant regulator and chelating agent, but also has good mixing properties.
[0011] Secondly, the present invention discloses a method for preparing the active agent for promoting crop growth, comprising the following steps:
[0012] (1) The natural zeolite particles are immersed in the plant regulator solution, and then the natural zeolite particles are taken out and dried to obtain plant regulator modified zeolite particles for later use.
[0013] (2) The sustained-release film is heated and melted, and then sprayed on the surface of the plant regulator modified zeolite particles to form a coating layer, and after cooling, a sustained-release film is formed, and the plant active agent is obtained for standby use.
[0014] (3) The natural zeolite particles are immersed in the metal ion chelating agent solution, and then the natural zeolite particles are taken out and dried to obtain chelating agent modified zeolite particles for later use.
[0015] (4) The raw material of the sustained-release film is heated and melted, and then sprayed on the surface of the chelating agent-modified zeolite particles to form a coating layer, and after cooling, a sustained-release film is formed, thereby obtaining the modified curing agent for standby use.
[0016] (5) Natural zeolite particles, an ethanol solution containing polyvinyl butyral, the plant active agent, and a modified curing agent are mixed and granulated, and then the obtained granules are dried to obtain the active agent for promoting crop growth.
[0017] Furthermore, in step (1), the material-liquid ratio of the natural zeolite particles to the plant regulator solution is 1:10 to 25. The plant regulator solution is an aqueous solution of the plant regulator, and optionally, the mass concentration of the plant regulator solution is 3 to 5%.
[0018] Furthermore, in step (1), the immersion time is 20 to 40 minutes, so that the plant regulator solution can fully enter the pores of the natural zeolite particles. The drying temperature is 50 to 65° C., and the drying time is 50 to 70 minutes.
[0019] Furthermore, in step (2), the ratio of the raw material of the sustained-release film to the plant regulator modified zeolite particles is 10-17 parts by weight: 35-50 parts by weight. Optionally, the temperature of the heating and melting in step (2) is 75-85° C., and the molten liquid formed after the raw material of the sustained-release film is heated is sprayed and coated on the surface of the plant regulator modified zeolite particles, so as to form a sustained-release film with good lubricity.
[0020] Furthermore, in step (3), the material-liquid ratio of the natural zeolite particles to the metal ion chelating agent solution is 1:12-18, and the metal ion chelating agent solution is a metal ion chelating agent aqueous solution. Optionally, the mass concentration of the metal ion chelating agent solution is 10-20%.
[0021] Furthermore, in step (3), the immersion time is 20 to 35 minutes, so that the plant regulator solution can fully enter the pores of the natural zeolite particles. The drying temperature is 55 to 75° C., and the drying time is 60 to 80 minutes.
[0022] Furthermore, in step (4), the ratio of the raw material of the sustained-release film to the chelating agent modified zeolite particles is 10-13 parts by weight: 30-44 parts by weight. Optionally, the temperature of the heating and melting in step (4) is 75-85°C, and the molten liquid formed after the raw material of the sustained-release film is heated is sprayed and coated on the surface of the chelating agent modified zeolite particles, so as to form a sustained-release film with good lubricity.
[0023] Furthermore, in step (5), the ratio of the natural zeolite particles, the ethanol solution containing polyvinyl butyral, the plant active agent, and the modified curing agent is 85-93 parts by weight: 14-19 parts by weight: 22-25 parts by weight: 30-36 parts by weight, and the ethanol solution containing polyvinyl butyral is a mixed solution formed by polyvinyl butyral and ethanol. Optionally, the mass concentration of the ethanol solution containing polyvinyl butyral is 4-5%.
[0024] Furthermore, in step (5), the particle size of the particles is 10-15 mm, wherein the particle size of the active agent for promoting crop growth and the chelating agent modified zeolite particles is 1-2 mm. Optionally, the drying temperature is 50-65° C. and the drying time is 60-65 min.
[0025] Thirdly, the present invention discloses the application of the active agent for promoting crop growth or the active agent obtained by the preparation method in the fields of agriculture, forestry, environmental engineering, etc.
[0026] Compared with the prior art, the beneficial effects achieved by the present invention are as follows: the crop growth promoting agent of the present invention adopts a core-shell structure composed of a matrix and a plant active agent and a modified curing agent distributed in the matrix, which has the functions of curing heavy metals in the soil and improving sudden impoverishment. The matrix formed by curing the crop growth promoting agent with natural zeolite particles and polyvinyl butyral can effectively absorb and enrich heavy metal ions in the contaminated soil by using the pores in the zeolite particles, thereby reducing the heavy metal ions in the soil. At the same time, the matrix formed by curing the polyvinyl butyral and natural zeolite particles also has good stability, preventing pulverization in the soil, so that the matrix of the present invention can remain in the soil for a long time as a water-retaining agent and an anti-soil compaction agent, thereby improving soil fertility.
[0027] Furthermore, the active agent for promoting crop growth of the present invention is coated with a plant active agent with slow-release properties in the matrix, wherein the plant regulator contained therein realizes the first slow release under the action of the slow-release membrane, and enters the matrix after the slow release. Its adsorption effect can further reduce the release of the plant regulator into the soil, and coupled with the filling effect of the microparticles formed by the chelating agent adsorbed in the matrix, the plant regulator can be gradually released into the soil more slowly. Since the plant regulator can play a good role in promoting plant growth, metabolism, etc. at a low concentration, the active agent for promoting crop growth of the present invention can release the plant regulator into the soil more effectively to meet the needs of plant growth.
[0028] Furthermore, the active agent for promoting crop growth of the present invention is coated with a modified curing agent with slow-release performance in the matrix, wherein the metal ion chelating agent contained therein is released into the matrix, so that the heavy metal ions adsorbed in the matrix are further solidified, and the heavy metal ions are prevented from easily migrating with rainwater and causing secondary pollution. The slow-release film on the surface of the modified curing agent gradually releases the metal ion chelating agent, and the adsorption effect of the matrix helps to keep the metal ion chelating agent in the matrix as much as possible, so as to avoid the metal ion chelating agent entering the soil after rapid release and failing to solidify the heavy metal ions in the matrix.
[0029] In addition, the sustained-release film coated with the plant active agent and the modified curing agent of the present invention uses paraffin wax or microcrystalline wax and other film materials, graphite powder and polyvinyl alcohol as raw materials, and the obtained coated film layer not only has good sustained-release performance, but also the sustained-release film formed by the paraffin wax or microcrystalline wax has good stability and can exist in the soil for a long time, which is convenient for the long-term sustained-release of the plant regulator and the chelating agent. The graphite powder mixed in the sustained-release film can make the plant active agent and the modified curing agent have good mixing properties, which is convenient for more uniform mixing with the matrix on the one hand, and helps to reduce the wear of the sustained-release film during the granulation process on the other hand. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. The embodiments of the present invention are described in detail below in conjunction with the accompanying drawings, wherein:
[0031] Figure 1 This is a diagram showing the effects of commercially available natural zeolite particles used in the following examples of the present invention. DETAILED DESCRIPTION
[0032] The present invention will be further described below in conjunction with specific examples. It should be understood that these examples are only used to illustrate the present invention and are not intended to limit the scope of the present invention. The experimental methods in the following examples without specifying specific conditions are usually carried out under conventional conditions or under conditions recommended by the manufacturer.
[0033] Unless otherwise defined, all professional and scientific terms used in the present invention have the same meanings as those familiar to those skilled in the art. The reagents or raw materials used in the present invention can be purchased through conventional channels. If there are no special instructions, the reagents or raw materials used in the present invention are used in a conventional manner in the art or in accordance with the product instructions. In addition, any method and material similar or equivalent to the described content can be applied to the method of the present invention.
[0034] In the following examples, the natural zeolite particles are commercially available products (refer to Figure 1 ) After further crushing treatment in the present invention, different particle sizes need to be obtained after sieving. The polyvinyl butyral is a commercially available product, CAS No.: 63148-65-2, Tianjin Baima Technology Co., Ltd.
[0035] Example 1
[0036] A method for preparing an active agent for promoting crop growth comprises the following steps:
[0037] (1) A prepared plant regulator (composed of 2,4-dichlorophenoxyacetic acid, chlormequat chloride, succinamide, and potassium indolebutyrate in a mass ratio of 4:7:3.5:5.5) was added into water and stirred for 5 minutes to form a plant regulator solution with a mass concentration of 4.5%.
[0038] (2) Mix the natural zeolite particles with a particle size of 100-150 mesh with the plant regulator solution at a solid-liquid ratio of 1:15, and then immerse for 30 minutes (stirring every 5 minutes). After completion, filter out the natural zeolite particles, drain the water, and then place them in an oven at 60° C. and dry them for 55 minutes to obtain plant regulator modified zeolite particles.
[0039] (3) Mix microcrystalline wax, graphite powder and polyvinyl alcohol 1788 powder in a mass ratio of 15:2.5:0.6, place in a coating machine and heat to 80°C to melt to form a coating liquid, and at the same time add the plant regulator modified zeolite particles into the coating machine (rotation speed 80r / min), the mass ratio of the coating liquid to the plant regulator modified zeolite particles is 13:40. Then spray the melted sustained-release film on the surface of the rolling plant regulator modified zeolite particles to form a coating layer, stop heating after the coating liquid is sprayed, and continue to rotate the coating machine for 5 minutes before discharging the material, and after cooling, obtain a plant active agent with a particle size of 1 to 2 mm.
[0040] (4) Natural zeolite particles were mixed with a 16% by mass aqueous solution of a metal ion chelating agent (wherein the mass ratio of citric acid, tartaric acid, and sodium gluconate was 1:1.5:1.2) at a solid-liquid ratio of 1:15 and then immersed for 30 minutes. After completion, the natural zeolite particles were filtered out and drained, and then placed in an oven and dried at 75° C. for 60 minutes to obtain chelating agent modified zeolite particles.
[0041] (5) Mix microcrystalline wax, graphite powder and polyvinyl alcohol 1788 powder in a mass ratio of 15:2.5:0.6, place in a coating machine and heat to 80°C to melt to form a coating liquid, and at the same time add the chelating agent modified zeolite particles into the coating machine (rotation speed 80r / min), the mass ratio of the coating liquid to the chelating agent modified zeolite particles is 11:35. Then spray the melted sustained-release film on the surface of the rolling chelating agent modified zeolite particles to form a coating layer, stop heating after the coating liquid is sprayed, and continue to rotate the coating machine for 5 minutes before discharging the material, and obtain a modified curing agent with a particle size of 1 to 2 mm after cooling.
[0042] (6) Add polyvinyl butyral to ethanol and stir evenly to obtain a polyvinyl butyral alcohol solution with a mass concentration of 5%. Mix natural zeolite particles with a particle size of 400 to 500 meshes, the polyvinyl butyral alcohol solution prepared in this embodiment, a plant active agent, and a modified curing agent in a mass ratio of 90:16:23:35 and granulate. After completion, place the obtained granules in an oven at 60°C and dry for 65 minutes to obtain an active agent for promoting crop growth with a particle size of 12 to 15 mm.
[0043] Example 2
[0044] A method for preparing an active agent for promoting crop growth comprises the following steps:
[0045] (1) A prepared plant regulator (composed of 2,4-dichlorophenoxyacetic acid, succinamic acid, sodium nitrophenolate, and potassium indolebutyrate in a mass ratio of 4:3.5:7:4) was added into water and stirred for 5 minutes to form a plant regulator solution with a mass concentration of 3.0%.
[0046] (2) Mix the natural zeolite particles with a particle size of 200-250 mesh with the plant regulator solution at a solid-liquid ratio of 1:25, and then immerse for 20 minutes (stirring every 5 minutes). After completion, filter out the natural zeolite particles, drain the water, and then place them in an oven at 60° C. and dry them for 55 minutes to obtain plant regulator modified zeolite particles.
[0047] (3) Mix microcrystalline wax, graphite powder and polyvinyl alcohol 2488 powder in a mass ratio of 10:2:0.4, place in a coating machine and heat to 75°C to melt to form a coating liquid, and at the same time add the plant regulator modified zeolite particles into the coating machine (rotation speed 80r / min), the mass ratio of the coating liquid to the plant regulator modified zeolite particles is 17:50. Then spray the melted sustained-release film on the surface of the rolling plant regulator modified zeolite particles to form a coating layer, stop heating after the coating liquid is sprayed, and continue to rotate the coating machine for 6 minutes before discharging, and after cooling, obtain a plant active agent with a particle size of 1 to 2 mm.
[0048] (4) Natural zeolite particles are mixed with a 20% by mass aqueous solution of a metal ion chelating agent (wherein the mass ratio of citric acid, tartaric acid, and sodium dithiocarbamate is 1:1.5:0.8) at a solid-liquid ratio of 1:12 and then immersed for 20 minutes. After completion, the natural zeolite particles are filtered out and drained, and then placed in an oven and dried at 60°C for 75 minutes to obtain chelating agent modified zeolite particles.
[0049] (5) Mix microcrystalline wax, graphite powder and polyvinyl alcohol 2488 powder in a mass ratio of 10:2:0.4, place in a coating machine and heat to 75°C to melt to form a coating liquid, and at the same time add the chelating agent modified zeolite particles into the coating machine (rotation speed 80r / min), the mass ratio of the coating liquid to the chelating agent modified zeolite particles is 13:44. Then spray the melted sustained-release film on the surface of the rolling chelating agent modified zeolite particles to form a coating layer, stop heating after the coating liquid is sprayed, and continue to rotate the coating machine for 5 minutes before discharging the material, and obtain a modified curing agent with a particle size of 1 to 2 mm after cooling.
[0050] (6) Add polyvinyl butyral to ethanol and stir evenly to obtain a polyvinyl butyral alcohol solution with a mass concentration of 4%. Mix natural zeolite particles with a particle size of 400 to 500 mesh, the polyvinyl butyral alcohol solution prepared in this embodiment, a plant active agent, and a modified curing agent in a mass ratio of 85:14:22:30 and granulate. After completion, place the obtained granules in an oven at 65°C and dry for 60 minutes to obtain an active agent for promoting crop growth with a particle size of 10 to 12 mm.
[0051] Example 3
[0052] A method for preparing an active agent for promoting crop growth comprises the following steps:
[0053] (1) A prepared plant regulator (composed of 2,4-dichlorophenoxyacetic acid, chlormequat chloride, sodium nitrophenolate, and potassium indolebutyrate in a mass ratio of 4:2.6:7:4) was added into water and stirred for 5 minutes to form a plant regulator solution with a mass concentration of 5.0%.
[0054] (2) Mix the natural zeolite particles with a particle size of 150-200 meshes with the plant regulator solution at a solid-liquid ratio of 1:10, and then immerse for 40 minutes (stirring every 8 minutes). After completion, filter out the natural zeolite particles, drain the water, and then place them in an oven at 65°C for 50 minutes to obtain plant regulator modified zeolite particles.
[0055] (3) Paraffin wax, graphite powder and polyvinyl alcohol 1788 powder are mixed in a mass ratio of 17:3.1:0.65, placed in a coating machine and heated to 85°C to melt to form a coating liquid, and the plant regulator modified zeolite particles are added to the coating machine (rotation speed 70r / min), and the mass ratio of the coating liquid to the plant regulator modified zeolite particles is 10:35. Then the melted sustained-release film is sprayed on the surface of the rolling plant regulator modified zeolite particles to form a coating layer. After the coating liquid is sprayed, the heating is stopped, and the coating machine continues to rotate for 5 minutes before discharging the material. After cooling, the plant active agent with a particle size between 1 and 2 mm is obtained.
[0056] (4) Natural zeolite particles are mixed with a 10% by mass aqueous solution of a metal ion chelating agent (wherein the mass ratio of tartaric acid, sodium gluconate, and sodium dithiocarbamate is 1.5:1.2:0.8) at a solid-liquid ratio of 1:18 and then immersed for 35 minutes. After completion, the natural zeolite particles are filtered out and drained, and then placed in an oven and dried at 55°C for 80 minutes to obtain chelating agent modified zeolite particles.
[0057] (5) Paraffin wax, graphite powder and polyvinyl alcohol 1788 powder are mixed in a mass ratio of 17:3.1:0.65, placed in a coating machine and heated to 85°C to melt to form a coating liquid, and the chelating agent modified zeolite particles are added to the coating machine (rotation speed 70r / min), and the mass ratio of the coating liquid to the chelating agent modified zeolite particles is 10:33. Then the melted sustained-release film is sprayed on the surface of the rolling chelating agent modified zeolite particles to form a coating layer. After the coating liquid is sprayed, the heating is stopped, and the coating machine continues to rotate for 5 minutes before discharging the material. After cooling, a modified curing agent with a particle size between 1 and 2 mm is obtained.
[0058] (6) Add polyvinyl butyral to ethanol and stir evenly to obtain a polyvinyl butyral alcohol solution with a mass concentration of 5%. Natural zeolite particles with a particle size of 400 to 450 mesh, the polyvinyl butyral alcohol solution prepared in this embodiment, a plant active agent, and a modified curing agent are mixed in a mass ratio of 93:19:25:36 and granulated. After completion, the obtained granules are placed in an oven at 50°C and dried for 65 minutes to obtain a crop growth promoting active agent with a particle size of 12 to 14 mm.
[0059] Example 4
[0060] A method for preparing an active agent for promoting crop growth comprises the following steps:
[0061] (1) A prepared plant regulator (composed of 2,4-dichlorophenoxyacetic acid, chlormequat chloride, succinamide, and potassium indolebutyrate in a mass ratio of 4:7:3.5:5.5) was added into water and stirred for 5 minutes to form a plant regulator solution with a mass concentration of 4.5%.
[0062] (2) Mix the natural zeolite particles with a particle size of 100-150 mesh with the plant regulator solution at a solid-liquid ratio of 1:15, and then immerse for 30 minutes (stirring every 5 minutes). After completion, filter out the natural zeolite particles, drain the water, and then place them in an oven at 60° C. and dry them for 55 minutes to obtain plant regulator modified zeolite particles.
[0063] (3) Mix microcrystalline wax, graphite powder and polyvinyl alcohol 1788 powder in a mass ratio of 15:2.5:0.6, place in a coating machine and heat to 80°C to melt to form a coating liquid, and at the same time add the plant regulator modified zeolite particles into the coating machine (rotation speed 80r / min), the mass ratio of the coating liquid to the plant regulator modified zeolite particles is 13:40. Then spray the melted sustained-release film on the surface of the rolling plant regulator modified zeolite particles to form a coating layer, stop heating after the coating liquid is sprayed, and continue to rotate the coating machine for 5 minutes before discharging the material, and after cooling, obtain a plant active agent with a particle size of 1 to 2 mm.
[0064] (4) Natural zeolite particles were mixed with clean water at a material-liquid ratio of 1:15 and then immersed for 30 minutes. After the mixture was immersed, the natural zeolite particles were filtered out and the water was drained. The mixture was then placed in an oven and dried at 75° C. for 60 minutes to obtain dry zeolite particles.
[0065] (5) Add polyvinyl butyral to ethanol and stir evenly to obtain a polyvinyl butyral alcohol solution with a mass concentration of 5%. Natural zeolite particles with a particle size of 400 to 500 mesh, the polyvinyl butyral alcohol solution prepared in this embodiment, a plant active agent, and dry zeolite particles are mixed in a mass ratio of 90:16:23:35 and granulated. After completion, the obtained granules are placed in an oven and dried at 60°C for 65 minutes to obtain a crop growth promoting active agent with a particle size of 12 to 15 mm.
[0066] Example 5
[0067] A method for preparing an active agent for promoting crop growth comprises the following steps:
[0068] (1) A prepared plant regulator (composed of 2,4-dichlorophenoxyacetic acid, chlormequat chloride, succinamide, and potassium indolebutyrate in a mass ratio of 4:7:3.5:5.5) was added into water and stirred for 5 minutes to form a plant regulator solution with a mass concentration of 4.5%.
[0069] (2) Mix the natural zeolite particles with a particle size of 100-150 mesh with the plant regulator solution at a solid-liquid ratio of 1:15, and then immerse for 30 minutes (stirring every 5 minutes). After completion, filter out the natural zeolite particles, drain the water, and then place them in an oven at 60° C. and dry them for 55 minutes to obtain plant regulator modified zeolite particles.
[0070] (3) Mix the microcrystalline wax and polyvinyl alcohol 1788 powder in a mass ratio of 15:0.6, place in a coating machine and heat to 80°C to melt to form a coating liquid, and at the same time add the plant regulator modified zeolite particles into the coating machine (rotation speed 80r / min), the mass ratio of the coating liquid to the plant regulator modified zeolite particles is 13:40. Then spray the melted sustained-release film on the surface of the rolling plant regulator modified zeolite particles to form a coating layer, stop heating after the coating liquid is sprayed, and continue to rotate the coating machine for 5 minutes before discharging the material, and obtain a plant active agent with a particle size of 1 to 2 mm after cooling.
[0071] (4) Natural zeolite particles were mixed with a 16% by mass aqueous solution of a metal ion chelating agent (wherein the mass ratio of citric acid, tartaric acid, and sodium gluconate was 1:1.5:1.2) at a solid-liquid ratio of 1:15 and then immersed for 30 minutes. After completion, the natural zeolite particles were filtered out and drained, and then placed in an oven and dried at 75° C. for 60 minutes to obtain chelating agent modified zeolite particles.
[0072] (5) Mix the microcrystalline wax and polyvinyl alcohol 1788 powder in a mass ratio of 15:0.6, place in a coating machine and heat to 80°C to melt to form a coating liquid, and at the same time add the chelating agent modified zeolite particles into the coating machine (rotation speed 80r / min), the mass ratio of the coating liquid to the chelating agent modified zeolite particles is 11:35. Then spray the melted sustained-release film on the surface of the rolling chelating agent modified zeolite particles to form a coating layer, stop heating after the coating liquid is sprayed, and continue to rotate the coating machine for 5 minutes before discharging the material, and obtain a modified curing agent with a particle size of 1 to 2 mm after cooling.
[0073] (6) Add polyvinyl butyral to ethanol and stir evenly to obtain a polyvinyl butyral alcohol solution with a mass concentration of 5%. Mix natural zeolite particles with a particle size of 400 to 500 meshes, the polyvinyl butyral alcohol solution prepared in this embodiment, a plant active agent, and a modified curing agent in a mass ratio of 90:16:23:35 and granulate. After completion, place the obtained granules in an oven at 60°C and dry for 65 minutes to obtain an active agent for promoting crop growth with a particle size of 12 to 15 mm.
[0074] Example 6
[0075] A method for preparing an active agent for promoting crop growth comprises the following steps:
[0076] (1) A prepared plant regulator (composed of 2,4-dichlorophenoxyacetic acid, succinamic acid, sodium nitrophenolate, and potassium indolebutyrate in a mass ratio of 4:3.5:7:4) was added into water and stirred for 5 minutes to form a plant regulator solution with a mass concentration of 3.0%.
[0077] (2) Mix the natural zeolite particles with a particle size of 200-250 mesh with the plant regulator solution at a solid-liquid ratio of 1:25, and then immerse for 20 minutes (stirring every 5 minutes). After completion, filter out the natural zeolite particles, drain the water, and then place them in an oven at 60° C. and dry them for 55 minutes to obtain plant regulator modified zeolite particles.
[0078] (3) Mix microcrystalline wax, graphite powder and polyvinyl alcohol 2488 powder in a mass ratio of 10:2:0.4, place in a coating machine and heat to 75°C to melt to form a coating liquid, and at the same time add the plant regulator modified zeolite particles into the coating machine (rotation speed 80r / min), the mass ratio of the coating liquid to the plant regulator modified zeolite particles is 17:50. Then spray the melted sustained-release film on the surface of the rolling plant regulator modified zeolite particles to form a coating layer, stop heating after the coating liquid is sprayed, and continue to rotate the coating machine for 6 minutes before discharging, and after cooling, obtain a plant active agent with a particle size of 1 to 2 mm.
[0079] (4) Natural zeolite particles are mixed with a 20% by mass aqueous solution of a metal ion chelating agent (wherein the mass ratio of citric acid, tartaric acid, and sodium dithiocarbamate is 1:1.5:0.8) at a solid-liquid ratio of 1:12 and then immersed for 20 minutes. After completion, the natural zeolite particles are filtered out and drained, and then placed in an oven and dried at 60°C for 75 minutes to obtain chelating agent modified zeolite particles.
[0080] (5) Add polyvinyl butyral to ethanol and stir evenly to obtain a polyvinyl butyral alcohol solution with a mass concentration of 4%. Natural zeolite particles with a particle size of 400 to 500 mesh, the polyvinyl butyral alcohol solution prepared in this embodiment, a plant active agent, and a chelating agent modified zeolite particles are mixed in a mass ratio of 85:14:22:30 and granulated. After completion, the obtained granules are placed in an oven and dried at 65°C for 60 minutes to obtain a crop growth promoting active agent with a particle size of 10 to 12 mm.
[0081] Example 7
[0082] A method for preparing an active agent for promoting crop growth comprises the following steps:
[0083] (1) A prepared plant regulator (composed of 2,4-dichlorophenoxyacetic acid, chlormequat chloride, sodium nitrophenolate, and potassium indolebutyrate in a mass ratio of 4:2.6:7:4) was added into water and stirred for 5 minutes to form a plant regulator solution with a mass concentration of 5.0%.
[0084] (2) Mix the natural zeolite particles with a particle size of 150-200 meshes with the plant regulator solution at a solid-liquid ratio of 1:10, and then immerse for 40 minutes (stirring every 8 minutes). After completion, filter out the natural zeolite particles, drain the water, and then place them in an oven at 65°C for 50 minutes to obtain plant regulator modified zeolite particles.
[0085] (3) Paraffin wax, graphite powder and polyvinyl alcohol 1788 powder are mixed in a mass ratio of 17:3.1:0.65, placed in a coating machine and heated to 85°C to melt to form a coating liquid, and the plant regulator modified zeolite particles are added to the coating machine (rotation speed 70r / min), and the mass ratio of the coating liquid to the plant regulator modified zeolite particles is 10:35. Then the melted sustained-release film is sprayed on the surface of the rolling plant regulator modified zeolite particles to form a coating layer. After the coating liquid is sprayed, the heating is stopped, and the coating machine continues to rotate for 5 minutes before discharging the material. After cooling, the active agent for promoting crop growth with a particle size of 1 to 2 mm is obtained.
[0086] The crop growth promoting active agent prepared in the above-mentioned embodiments was tested for its removal effect on heavy metal ions in the soil and its promoting effect on wheat crop yield. Wherein: the test method for the removal effect of heavy metal ions is: dissolve the fly ash from garbage incineration in water and leach it for 24 hours, irrigate the obtained leaching solution containing heavy metal ions (Pb, Cd, Hg, Cr, As, etc.) into the test soil, and then test the concentration of total heavy metal ions in the soil, which is recorded as A1. Then, the crop growth promoting active agent is applied to the soil irrigated with the leaching solution, and the application amount is 800kg / mu. After two weeks, the concentration of total heavy metal ions in the soil is tested again, which is recorded as B1, and the removal rate of heavy metal ions is calculated as C1=(A1-B1) / A1. At the same time, when the wheat has grown for 2 months, the above-mentioned leachate is poured into the soil again to test the concentration of total heavy metal ions in the soil, recorded as A2. Two weeks later, the concentration of total heavy metal ions in the soil is tested again, recorded as B2, and the removal rate of heavy metal ions is calculated as C2 = (A2-B2) / A2. Finally, after the wheat is mature and harvested, the yield growth rate of wheat corresponding to each embodiment is calculated relative to the blank group. No active agent for promoting crop growth is added to the blank group. The results are shown in the following table. It can be seen that the active agent for promoting crop growth prepared in each embodiment has a certain improvement in the removal effect of heavy metal ions in the soil and the yield of wheat crops, and the improvement effect of Examples 1 to 3 is more obvious.
[0087]
[0088] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A method for preparing an active agent for promoting crop growth, It is characterized in that The steps include: (1) soaking natural zeolite particles with a particle size of 100 to 250 meshes in a plant regulator aqueous solution, then taking out the natural zeolite particles and drying them to obtain plant regulator modified zeolite particles for standby use; the mass concentration of the plant regulator aqueous solution is 3 to 5%, and the plant regulator includes: at least one of 2,4-dichlorophenoxyacetic acid, sodium nitrophenolate, succinamic acid, chlormequat, sodium naphthylacetate, and potassium indolebutyrate; the material-liquid ratio of the natural zeolite particles to the plant regulator aqueous solution is 1:10 to 25; (2) heating the raw material of the slow-release film to 75-85° C. to melt and then spraying the melt on the surface of the plant regulator modified zeolite particles to form a coating layer, and cooling to form a slow-release film, thereby obtaining the plant active agent for standby use; the ratio of the raw material of the slow-release film to the plant regulator modified zeolite particles is 10-17 parts by weight: 35-50 parts by weight; the raw material of the slow-release film includes 10-17 parts by weight of film material, 2-3.1 parts by weight of graphite powder, and 0.4-0.65 parts by weight of polyvinyl alcohol; the film material includes any one of microcrystalline wax and paraffin wax; (3) soaking the natural zeolite particles in an aqueous solution of a metal ion chelating agent having a mass concentration of 10 to 20%, then taking out the natural zeolite particles and drying them to obtain chelating agent-modified zeolite particles for later use; the metal ion chelating agent includes at least one of citric acid, tartaric acid, sodium gluconate, and dithiocarbamate; the material-liquid ratio of the natural zeolite particles to the aqueous solution of the metal ion chelating agent is 1:12 to 18; (4) heating the raw material of the sustained-release membrane to 75-85° C. to melt and then spraying it on the surface of the chelating agent modified zeolite particles to form a coating layer, and cooling to form a sustained-release membrane, thereby obtaining the modified curing agent for standby use; the ratio of the raw material of the sustained-release membrane to the chelating agent modified zeolite particles is 10-13 parts by weight: 30-44 parts by weight; the raw material of the sustained-release membrane includes 10-17 parts by weight of membrane material, 2-3.1 parts by weight of graphite powder, and 0.4-0.65 parts by weight of polyvinyl alcohol; the membrane material includes any one of microcrystalline wax and paraffin wax; (5) Natural zeolite particles of 400 to 500 mesh, an ethanol solution containing polyvinyl butyral, the plant active agent, and a modified curing agent are mixed in a ratio of 85 to 93 parts by weight: 14 to 19 parts by weight: 22 to 25 parts by weight: 30 to 36 parts by weight, and then granulated, and then the obtained granules are dried to obtain the active agent for promoting crop growth; the ethanol solution containing polyvinyl butyral is a mixed solution of polyvinyl butyral and ethanol with a mass concentration of 4 to 5%.
2. The method for preparing the active agent for promoting crop growth according to claim 1, It is characterized in that In step (1), the immersion time is 20 to 40 minutes; the drying temperature is 50 to 65° C., and the drying time is 50 to 70 minutes.
3. The method for preparing the active agent for promoting crop growth according to claim 1, It is characterized in that In step (3), the immersion time is 20 to 35 minutes; the drying temperature is 55 to 75° C., and the drying time is 60 to 80 minutes.
4. The method for preparing the active agent for promoting crop growth according to claim 1, It is characterized in that In step (5), the particle size of the particulate matter is 10 to 15 mm, wherein the particle size of the active agent for promoting crop growth and the chelating agent modified zeolite particles is 1 to 2 mm.
5. The method for preparing the active agent for promoting crop growth according to claim 1, It is characterized in that In step (5), the drying temperature is 50-65° C. and the drying time is 60-65 min.
6. Use of the crop growth promoting agent obtained by the preparation method according to any one of claims 1 to 5 in any field of agriculture, forestry and environmental engineering.