A multi-layer mesh spraying concrete reinforcement method for old house renovation
By adopting multi-layer web spraying concrete reinforcement method in old house buildings, and using layer-by-layer steel mesh and dry jetting technology, the problem of insufficient wall bearing capacity in the existing technology is solved, and the building bearing capacity is effectively improved and The effect of extending the life of the building.
Patent Information
- Application Number
- CN202211523607.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-11-30
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2042-11-30
AI Technical Summary
In the prior art, sprayed concrete on the wall can only protect the surface of the wall and cannot effectively improve the bearing capacity of the wall, resulting in poor building life extension.
The multi-layer hanging net spray concrete reinforcement method is adopted. By installing anchor bars on the original wall and installing steel mesh layer by layer, each layer of steel mesh is alternately installed with the concrete layer, and the stability and bearing capacity of the concrete layer are ensured by dry jet technology.
The construction method of spraying concrete with multi-layer steel mesh on the wall is realized, so that the sprayed concrete can form a new wall that can improve the bearing capacity of the original wall, and at the same time, the problem of disturbing the concrete sprayed after the installation of the subsequent steel mesh is avoided. .
Smart Images

Figure CN115773014B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of construction measures for existing buildings, in particular to a multi-layer mesh spraying reinforcement method for old house reconstruction. Background Art
[0002] With the accelerating pace of urbanization and the rapid growth of urban populations, housing is becoming increasingly scarce. For various reasons, the functionality and durability of existing buildings are no longer sufficient to meet people's living needs. Furthermore, some older buildings (such as sites of major historical events or former residences of celebrities) and even ancient structures possess significant cultural and historical value and need to be used for a longer period without altering their appearance. This means finding ways to extend the lifespan of these buildings, which have already reached the end of their useful life.
[0003] Therefore, strengthening and renovating existing buildings has become an inevitable research topic in the current construction industry, and conducting research on structural reinforcement and renovation in housing construction projects has very important practical significance.
[0004] In the existing technology, the reinforcement and reconstruction of existing buildings mainly fall into the following categories:
[0005] 1. Add steel structure on the basis of existing buildings. The added steel structure includes steel beams, steel columns, steel purlins, etc.
[0006] This method is highly versatile and can be used for various types of existing buildings. It works well on beams, columns, roofs and other structures in the original building, but is not as effective on walls and has a significant impact on the building's appearance.
[0007] 2. Add prestressed cables to the existing building to apply restraint in a specific direction.
[0008] This method has a relatively narrow scope of application and is specifically suitable for load-bearing masonry structures, such as masonry walls or masonry columns. It can greatly improve the seismic resistance of the building while having little impact on the appearance of the building.
[0009] 3. Place the wall next to the existing building and cast a layer of reinforced concrete (either on one side or both sides) to thicken the original wall.
[0010] This method can effectively reinforce the building walls, improve their stability and bearing capacity, and has little impact on the building's appearance. However, due to the large space required for construction (the thickness of the reinforced concrete wall cannot be too thin, otherwise the steel cage will be difficult to tie, and the wall formwork, formwork support system, and the foundation of the newly added wall also require space), in many cases it will interfere with the original structure and cannot be constructed.
[0011] 4. Hang a mesh and spray concrete on the walls of existing buildings.
[0012] This method is similar to pouring a layer of reinforced concrete against the wall of an existing building, but it requires minimal construction space, and the new structure and construction equipment will not interfere with the existing structure. However, the sprayed concrete layer cannot be too thick, otherwise it will not only easily flow and deform but also crack when solidified (because there is only one layer of mesh and the sprayed concrete cannot be vibrated). This will not form a new wall capable of bearing vertical loads, and it mainly serves to protect the original wall surface, with little reinforcement effect.
[0013] When constructing on slopes (such as hillsides and dams), there is a construction method that uses multi-layer mesh spraying concrete. This method allows for the spraying of very thick concrete. This method is mentioned in the article "Analysis of the Causes of Leakage and Anti-seepage Remediation Measures for the Shichengzi Arch Dam". However, this method has many problems when applied to walls:
[0014] Concrete sprayed on walls has extremely poor fluidity (otherwise it wouldn't stick), and it can't flow freely to fill gaps. Furthermore, the wall is covered with steel mesh, not wire mesh (otherwise it would be easily deformed, but the mesh would block the concrete). If multiple layers of mesh were used, they would significantly block the sprayed concrete, leaving large hollows. While a single layer of mesh could overcome this blockage through oblique spraying during construction, multiple layers of mesh are not feasible. Therefore, spraying concrete with multiple layers of mesh is not feasible.
[0015] The inventor solved this problem and successfully used the multi-layer mesh spraying method to complete the single-story multi-functional hall reinforcement project in the Haigang District No. 3 Middle School project. Summary of the Invention
[0016] The invention provides a multi-layer mesh-hanging concrete spraying reinforcement method for old house reconstruction.
[0017] The technical problem to be solved is that hanging a mesh and spraying concrete on the wall can only protect the wall surface, but cannot effectively improve the wall's bearing capacity and has a poor effect on extending the life of the building.
[0018] In order to solve the above technical problems, the present invention adopts the following technical solutions: a multi-layer mesh spraying reinforcement method for old house renovation, comprising the following steps:
[0019] Step 1: Clean the surface of the original wall;
[0020] Step 2: Evenly install anchor bars for fixing the steel mesh on the original wall;
[0021] Step 3: Install steel mesh on the anchor bar layer by layer, spraying a layer of concrete after each layer of steel mesh is installed;
[0022] Among the steel meshes, the first one installed is called the primary mesh and is fixedly connected to the anchor bars. The last one installed is called the final mesh, and the remaining meshes are called middle meshes. Top keels are anchored horizontally on the tops of the middle and final meshes. Both ends of the top keels are mounted on a temporary swing support structure so that neither the middle nor the final meshes are in contact with the anchor bars.
[0023] Each time concrete is sprayed, it must be done after the previous layer of concrete has completely set.
[0024] Furthermore, a limiting rod fixedly connected to the anchor bar is vertically provided on the anchor bar, and the limiting rod corresponds to each layer of steel mesh in sequence starting from the original wall and is used to block the horizontal steel bars in the steel mesh;
[0025] After each layer of steel mesh is installed in step 3, the distance between the steel mesh and the original wall, as well as the distance between each layer of steel mesh, is controlled by a distance controller; the distance controller is a steel bar bent into a spoon shape, the spoon body portion is a right-angled U-shape, and the leg of the right-angled U-shape away from the spoon handle is longer than the leg close to the spoon handle;
[0026] The primary net and the middle net are uniformly recorded as non-net. The outer surface of the concrete layer sprayed after each non-net is installed is flush with the non-net, and the concrete layer sprayed after the final net is installed will wrap the final net.
[0027] Furthermore, in step 3, the following method is used to control the distance between the initial mesh and the original wall:
[0028] After the primary net is installed, insert the spoon body of the distance controller between the primary net and the original wall, so that the primary net is pushed onto the corresponding limit rod, and the handle of the distance controller is stuck on the limit rod corresponding to the primary net, and then fix the primary net to the anchor bar by tying or welding;
[0029] In step 3, the spacing between two adjacent layers of steel mesh is controlled in the following way:
[0030] After the steel mesh is installed, insert the spoon body of the distance controller between the limit rod corresponding to the steel mesh installed last time and the steel mesh installed this time, so that the steel mesh installed this time is pushed onto the corresponding limit rod, and the spoon handle of the distance controller is stuck on the limit rod corresponding to the steel mesh installed this time.
[0031] Furthermore, a foundation groove along the wall is opened at the bottom of the wall surface on the side of the original wall to be reinforced, and the width of the foundation groove along the wall is not less than the total thickness of the concrete layer sprayed directly above it. The bottom of the steel mesh and the concrete layer extends downward to the bottom of the foundation groove, and after step three, the foundation groove along the wall is filled with concrete and smoothed.
[0032] Furthermore, the original door and window openings of the original wall are also blocked with door and window hole molds for forming new door and window openings with straight yin and yang corner lines in the sprayed concrete layer. The door and window hole molds are cylinders or hollow boxes with a cross-section consistent with the original door and window openings, and are inserted into the original door and window openings before step three; the steel mesh is provided with avoidance openings for the door and window hole molds to extend out.
[0033] Furthermore, both ends of the keel extend outside the steel mesh, and the swing support structure is a telescopic support rod supported by construction workers.
[0034] Furthermore, if a single-sided wall is reinforced, the anchor bars are chemically planted bars; if a double-sided wall is reinforced, the anchor bars are S-shaped through-wall bars.
[0035] Furthermore, the installation process of the chemical anchoring is as follows: line positioning → drilling → hole washing → glue injection → anchoring → curing and maintenance → pull-out test.
[0036] Furthermore, step one includes the following sub-steps:
[0037] Step 1.1. Remove the original wall surface layer to the original structural base layer;
[0038] Step 1.2. After removing the surface layer of the original wall, measure the verticality and surface flatness of the original wall. If any areas do not meet the design requirements, repair them.
[0039] Step 1.3. Sweep away dust from the original wall surface, then spray water to clean the original wall.
[0040] Furthermore, in step three, the concrete layer is sprayed using a dry spraying method.
[0041] Compared with the prior art, the multi-layer mesh spraying reinforcement method for old house renovation of the present invention has the following beneficial effects:
[0042] In the present invention, the steel mesh is not installed in place at one time before installation, but a layer of mesh is hung and concrete is sprayed one by one, thereby solving the problem of hollowing in the concrete caused by hanging multiple layers of mesh on the wall; and the steel mesh other than the initial mesh (the initial mesh can be in contact with the anchor bars) is suspended and not in contact with the anchor bars when hanging the mesh, and the spacing is subsequently controlled by the distance controller to open each layer of steel mesh, thereby avoiding the disturbance of the previously sprayed concrete perpendicular to the anchor bar direction when installing the subsequent steel mesh (there is no need to hang it on the anchor bar, and the previously sprayed concrete will not be knocked down due to the shaking of the anchor bar); the above two aspects are combined to realize the construction method of hanging multiple layers of steel mesh on the wall and spraying concrete, so that the sprayed concrete can form a new wall that can improve the bearing capacity of the original wall like formwork casting, and at the same time is not subject to the many restrictions of formwork casting. BRIEF DESCRIPTION OF THE DRAWINGS
[0043] Figure 1This is a schematic diagram of a building structure in a multi-layer mesh spraying reinforcement method for old house renovation according to the present invention, in which the first layer of steel mesh (first mesh) is currently being installed;
[0044] Figure 2 This is a schematic diagram of how to use the distance controller. This figure is a top view.
[0045] Figure 3 This is a structural diagram of a steel mesh with a keel;
[0046] Among them, 1-original wall, 2-anchor bar, 21-limit rod, 3-steel mesh, 31-top keel, 4-distance controller, 5-foundation groove along the wall. DETAILED DESCRIPTION
[0047] like Figure 1 As shown, a multi-layer mesh spraying reinforcement method for old house renovation includes the following steps
[0048] Step 1: Clean the surface of the original wall 1;
[0049] Step 2: Evenly install anchor bars 2 for fixing the steel mesh 3 on the original wall 1;
[0050] Step 3: Install the steel mesh 3 on the anchor bar 2 layer by layer, spraying a layer of concrete each time a layer of steel mesh 3 is installed;
[0051] Among the steel meshes 3, the first steel mesh 3 installed is recorded as the primary mesh and is fixedly connected to the anchor bar 2. The last steel mesh 3 installed is recorded as the final mesh. The remaining steel meshes 3 are recorded as the middle mesh. Top keels 31 are horizontally anchored on the top of the middle mesh and the final mesh. The ends of the top keels 31 are erected on a temporary swing support structure so that the middle mesh and the final mesh are not in contact with the anchor bar 2.
[0052] Here, the bottom of the middle and last nets is a little higher than the first net, so that the grid does not contact the anchor bar 2 when the lower end touches the ground. Of course, the middle and last nets can be suspended. And the keel 31 is selected from steel pipes in this embodiment and is welded to the steel mesh 3.
[0053] A swing support structure provides support but does not restrict horizontal displacement, facilitating subsequent adjustment of the mesh spacing. A swing support structure can be constructed using a swing column. If this is not available, a rigid pole erected on the construction site can also be used for manual support. (When adjusting the mesh spacing, do not secure the pole underneath; instead, manually support it. After adjustment, secure it with a brick, sandbag, or other heavy object.) A temporary setup is one that will be removed after the concrete has completely solidified.
[0054] When installing the middle and end meshes, they are first placed in the air, and then the anchor bars 2 are passed through the grid on the steel mesh 3, and then the spacing between them and the previously installed steel mesh 3 is adjusted.
[0055] Each time you spray concrete, it should be done after the previous layer of concrete has completely set to avoid dragging down the previously sprayed concrete. Note that if you spray again one hour after the previous layer of concrete has completely set, you should first spray water to wet the surface of the previous layer of concrete. If the surface of the previous layer of concrete becomes contaminated during this interval, it should be cleaned.
[0056] A limiting rod 21 is vertically provided on the anchor bar 2 and fixedly connected to the anchor bar 2. The limiting rod 21 corresponds to each layer of steel mesh 3 in sequence starting from the original wall 1 and is used to block the horizontal steel bars in the steel mesh 3;
[0057] After each layer of steel mesh 3 is installed in step three, the distance between the steel mesh 3 and the original wall 1 and the distance between each layer of steel mesh 3 are controlled by the distance controller 4; the distance controller 4 is a steel bar bent into a spoon shape, and the spoon body part is a right-angled U-shape, and the leg of the right-angled U-shape away from the spoon handle is longer than the leg close to the spoon handle; thereby preventing the distance controller 4 from falling off after installation.
[0058] Here, the spoon body acts as a compression spring, which supports the steel mesh 3 installed later. At the same time, it does not cause disturbance to the anchor bar 2 in the direction perpendicular to the anchor bar 2 as would be caused by tying or welding. The longer legs of the spoon handle and the spoon body prevent it from falling after installation.
[0059] This shape of rebar can be bent directly from a single rebar without any connections, making it very low-cost and capable of rapid mass production. High precision is not possible when bending rebar on a construction site, so the distance controller 4 should be made from low-carbon rebar (thick wire) with a diameter of approximately 5 mm. The scoop should be slightly larger than the space it will be inserted into, allowing it to deform and hold the distance controller in place.
[0060] The primary net and the middle net are uniformly recorded as non-net. The outer surface of the concrete layer sprayed after each non-net is installed is flush with the non-net, and the concrete layer sprayed after the final net is installed will wrap the final net.
[0061] like Figure 2 As shown, in step 3, the spacing between two adjacent layers of steel mesh 3 is controlled in the following manner:
[0062] After the steel mesh 3 is installed, the spoon body of the distance controller 4 is inserted between the limit rod 21 corresponding to the steel mesh 3 installed last time and the steel mesh 3 installed this time, so that the steel mesh 3 installed this time is pushed onto the corresponding limit rod 21, and the spoon handle of the distance controller 4 is stuck on the limit rod 21 corresponding to the steel mesh 3 installed this time.
[0063] Here, please note that the distance controller 4 is extended from the mesh of the steel mesh 3 to the space between the two layers of steel mesh 3 during installation. Be careful not to hit the anchor bar 2 during installation. When using, the spoon handle should be on the outside. Otherwise, the spoon handle will interfere with the upper layer of concrete. See Figure 2 .
[0064] The control method of the distance between the initial mesh and the original wall 1 is the same as Figure 2 The details are as follows:
[0065] After the primary net is installed, the spoon body of the distance controller 4 is inserted between the primary net and the original wall 1, so that the primary net is pushed onto the corresponding limit rod 21, and the spoon handle of the distance controller 4 is stuck on the limit rod 21 corresponding to the primary net, and then the primary net is fixedly connected to the anchor bar 2 by binding or welding.
[0066] Here, the distance controller 4 is not necessary for the primary net, and it is also OK to directly pull the primary net to the corresponding limit rod 21 and fix it. But here, if there is a distance controller 4, it can play a temporary fixing role, and one hand can be freed up for subsequent tying or welding.
[0067] A wall foundation groove 5 is opened at the bottom of the wall surface on the side to be reinforced of the original wall 1. The width of the wall foundation groove 5 is not less than the total thickness of the concrete layer sprayed directly above it. The bottom of the steel mesh 3 and the concrete layer extends downward to the bottom of the foundation groove. After step three, the wall foundation groove 5 is filled with concrete and smoothed.
[0068] The multiple layers of steel mesh 3 here effectively form a steel cage, which, together with the sprayed concrete, forms a new wall. This new wall, however, cannot be fully supported by anchor bars 2, so a simple foundation is provided. The depth of the foundation trench 5 should not exceed half the depth of the original wall 1 foundation; typically, half a meter is sufficient. If the original wall 1 foundation is very shallow, temporary support may be provided on one side of the trench 5 during construction, using diagonal braces or other tools.
[0069] If the original wall 1 is on the second floor or higher, then it is only necessary to chisel out the steel bars on the floor surface along the wall foundation groove 5, and then install the steel mesh 3 so that the steel mesh 3 and the steel bars of the floor intersect.
[0070] The original door and window openings of the original wall 1 are also blocked with door and window hole molds for forming new door and window openings with straight yin and yang corner lines in the sprayed concrete layer. The door and window hole molds are cylinders or hollow boxes with a cross-section consistent with the original door and window openings, and are inserted into the original door and window openings before step three; a relief opening is opened on the steel mesh 3 for the door and window hole molds to extend out.
[0071] The concrete sprayed here may affect the appearance of the door and window openings, so door and window opening molds need to be set up.
[0072] like Figure 3 As shown, both ends of the keel 31 extend beyond the steel mesh 3, and the swing support structure is a telescopic support rod supported by the construction worker. The telescopic support rod facilitates height adjustment, allowing the anchor bar 2 to smoothly pass through the grid of the steel mesh 3 without contacting the steel mesh 3. If the construction worker holds it by hand, the length adjustment and the swinging of the support rod as required (the telescopic support rod needs to be swung to adjust the spacing of the steel mesh 3) can be performed by the same person. If the steel mesh 3 here is very heavy, a small pit should be dug in the base surface of the telescopic support rod to prevent the bottom of the telescopic support rod from slipping.
[0073] If a single wall is reinforced, the anchor bar 2 is a chemically planted bar; if a double wall is reinforced, the anchor bar 2 is an S-shaped through-wall bar. These are two commonly used anchor bars 2 in the prior art and can be used directly in this embodiment without further modification.
[0074] The installation process of chemical anchoring is: marking line for positioning → drilling → hole washing → glue injection → anchoring → curing and maintenance → pull-out test.
[0075] Note that anchor bar 2 needs to be thoroughly polished and rust-free. To clean the hole, use a brush with an extension rod, extend it to the bottom of the hole, and repeatedly pump it back and forth to remove dust and debris. Then, use compressed air to blow out any loose dust inside the hole. Afterward, scrub the inside of the hole with cotton wool dipped in alcohol or acetone. Avoid scrubbing with water, as alcohol and acetone evaporate easily, while water does not. Scrubbing with water will prevent the hole from drying quickly.
[0076] Step 1 includes the following sub-steps:
[0077] Step 1.1. Remove the surface layer of the original wall 1 to the original structural base, that is, expose the original masonry or concrete of the wall 1.
[0078] Step 1.2. After removing the surface layer of the original wall 1, measure the verticality and surface flatness of the original wall 1. If any areas do not meet the design requirements, repair them. Mortar or concrete with glue can be used for this repair.
[0079] Step 1.3. Sweep away dust from the surface of the original wall 1, and then clean the original wall 1 with water.
[0080] In step three, dry spraying is used to spray the concrete layer. Even if the previous layer of concrete has initially set, the subsequent sprayed concrete, if highly fluid, can still flow over the previous layer and cause damage. Therefore, dry spraying is required, as it allows for very low moisture content in the concrete (dry spraying uses dry material, which is then mixed with water mist at the nozzle. Low moisture content does not affect spraying. With wet spraying, low moisture content in the concrete prevents spraying).
[0081] The embodiments described above are merely descriptions of preferred implementations of the present invention and are not intended to limit the scope of the present invention. Without departing from the spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should fall within the scope of protection determined by the claims of the present invention.
Claims
1. A multi-layer mesh spraying reinforcement method for old house reconstruction, characterized in that: The following steps are included Step 1: Clean the surface of the original wall (1); Step 2: evenly installing anchor bars (2) for fixing the steel mesh (3) on the original wall (1); Step 3: installing the steel mesh (3) on the anchor bar (2) layer by layer, spraying a layer of concrete after each layer of the steel mesh (3) is installed; Among the steel meshes (3), the first steel mesh (3) installed is recorded as the primary mesh and is fixedly connected to the anchor bar (2), the last steel mesh (3) installed is recorded as the final mesh, and the remaining steel meshes (3) are recorded as the middle mesh; the top of the middle mesh and the final mesh is horizontally anchored with a keel (31), and the two ends of the keel (31) are erected on a temporarily set swing support structure so that the middle mesh and the final mesh are not in contact with the anchor bar (2); Each time concrete is sprayed, it must be done after the previous layer of concrete has finally set; A limiting rod (21) fixedly connected to the anchor bar (2) is vertically arranged on the anchor bar (2), and the limiting rod (21) corresponds to each layer of the steel mesh (3) in sequence starting from the original wall (1) and is used to block the horizontal steel bars in the steel mesh (3); After each layer of steel mesh (3) is installed in step 3, the distance between the steel mesh (3) and the original wall (1) and the distance between each layer of steel mesh (3) are controlled by a distance controller (4); the distance controller (4) is a steel bar bent into a spoon shape, the spoon body portion is a right-angled U-shape, and the right-angled U-shape has a leg away from the spoon handle that is longer than the leg close to the spoon handle; The primary net and the middle net are uniformly recorded as non-net-covered. The outer surface of the concrete layer sprayed after each non-net-covered net is installed is flush with the non-net-covered net, and the concrete layer sprayed after the final net is installed will wrap the final net inside. In step 3, the distance between the initial mesh and the original wall (1) is controlled by: After the primary net is installed, the spoon body of the distance controller (4) is inserted between the primary net and the original wall (1), so that the primary net is pushed onto the corresponding limit rod (21), and the spoon handle of the distance controller (4) is clamped on the limit rod (21) corresponding to the primary net, and then the primary net is fixedly connected to the anchor bar (2) by tying or welding; In step 3, the spacing between two adjacent layers of steel mesh (3) is controlled in the following manner: After the steel mesh (3) is installed, the spoon body of the distance controller (4) is inserted between the limit rod (21) corresponding to the steel mesh (3) installed last time and the steel mesh (3) installed this time, so that the steel mesh (3) installed this time is pushed onto the corresponding limit rod (21), and the spoon handle of the distance controller (4) is stuck on the limit rod (21) corresponding to the steel mesh (3) installed this time.
2. A multi-layer mesh spraying concrete reinforcement method for old house reconstruction according to claim 1, characterized in that: A wall foundation groove (5) is provided at the bottom of the wall surface on one side of the original wall (1) to be reinforced. The width of the wall foundation groove (5) is not less than the total thickness of the concrete layer sprayed directly above it. The bottom of the steel mesh (3) and the concrete layer extends downward to the bottom of the foundation groove. After step three, the wall foundation groove (5) is filled with concrete and smoothed.
3. The multi-layer mesh spraying concrete reinforcement method for old house reconstruction according to claim 1 is characterized in that: The original door and window openings of the original wall (1) are also blocked with door and window opening molds for forming new door and window openings with straight yin and yang angle lines in the sprayed concrete layer. The door and window opening molds are cylinders or hollow boxes with a cross section consistent with the original door and window openings, and are inserted into the original door and window openings before step three. The steel mesh (3) is provided with avoidance openings for the door and window opening molds to extend out.
4. The multi-layer mesh spraying concrete reinforcement method for old house reconstruction according to claim 1 is characterized in that: Both ends of the keel (31) extend outside the steel mesh (3), and the swing support structure is a telescopic support rod supported by construction workers.
5. The multi-layer mesh spraying concrete reinforcement method for old house reconstruction according to claim 1 is characterized in that: If a single-sided wall is reinforced, the anchor bar (2) is a chemically embedded bar; if a double-sided wall is reinforced, the anchor bar (2) is an S-shaped through-wall bar.
6. A multi-layer mesh spraying concrete reinforcement method for old house reconstruction according to claim 5, characterized in that: The installation process of the chemical anchor bar is as follows: marking line for positioning → drilling → hole washing → glue injection → anchor bar implantation → curing and maintenance → pull-out test.
7. The multi-layer mesh spraying concrete reinforcement method for old house reconstruction according to claim 1 is characterized in that: Step 1 includes the following sub-steps: Step 1.
1. Remove the original wall (1) surface layer to the original structural base; Step 1.
2. After removing the surface layer of the original wall (1), measure the verticality and surface flatness of the original wall (1). If there are any areas that do not meet the design requirements, repair them; Step 1.
3. Sweep away the dust on the surface of the original wall (1), and then spray water to clean the original wall (1).
8. The multi-layer mesh spraying concrete reinforcement method for old house reconstruction according to claim 1 is characterized in that: In step three, the concrete layer is sprayed by dry spraying.
Citation Information
Patent Citations
Construction method for reinforcing treatment of bonding layer of sprayed concrete and brick wall
CN107288364A
Construction method for repairing ancient building wall face
CN110528906A