Chemical tempering device for ultra-thin glass of unequal thickness and tempering method thereof

Through the segmented tempering method of chemical tempering device of unequal thickness ultra-thin glass, the 'pleat' problem caused by the different thicknesses of ultra-thin glass in the bending and non-bending areas after chemical tempering is solved, and the high resistance of glass is achieved Impact and excellent bending performance, suitable for electronic product covers.

CN115849690BActive Publication Date: 2024-12-06WUHU DONGXIN PHOTOELECTRIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211440675.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-11-17
Publication Date
2024-12-06
Estimated Expiration
2042-11-17

AI Technical Summary

Technical Problem

After chemical tempering, the different thicknesses of existing ultra-thin glasses in the bending and non-bending zones lead to undulating ‘pleats’ after tempering, affecting the appearance and performance of the product.

Method used

Using a chemical tempering device for unequal thickness ultra-thin glass, the reinforcement of the bending zone and non-bending zone is accurately controlled through structures such as frame, limiting side teeth and guide grooves, and the reinforcement of the bending zone is used for segmented tempering to ensure the non-bending zone. Tempering first and then overall tempering, controlling the expansion rate consistently to avoid 'wrinkle' phenomenon.

Benefits of technology

It effectively suppresses the folding phenomenon in the bending zone after chemical tempering of ultra-thin glass with different thicknesses, improves the impact resistance and bending performance of the glass, and ensures the smooth surface of the finished product, impact resistance and bending strength.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115849690B_ABST
    Figure CN115849690B_ABST
Patent Text Reader

Abstract

The present invention discloses a chemical tempering device for ultra-thin glass of unequal thickness and a tempering method thereof, comprising: a frame body, which can accommodate flexible glass; limiting side teeth, a series of limiting side teeth are provided on the side edges of the frame body, and the limiting side teeth can position the side edges of the flexible glass; a guide groove, which is arranged on both sides of the frame body; a pressure rod, which is slidably installed in the guide groove, and the pressure rod can limit the bending part of the flexible glass, accurately control the bending area and the non-bending area to be separately strengthened, and can effectively suppress the wrinkle phenomenon in the bending area after the ultra-thin glass of unequal thickness is chemically tempered.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of tempered glass, and in particular relates to a chemical tempering device for ultra-thin glass of unequal thickness and a tempering method thereof. Background Art

[0002] With the upgrading of electronic products, people's pursuit of mobile phones and tablets has become thinner and lighter. The emergence of folding screens has attracted widespread attention from all walks of life. The emergence of ultra-thin glass cover plates in the electronic display industry has been paid more and more attention by listed companies. Since 2020, OPPO, Honor, and Huawei have all launched folding screen mobile phones. Among them, OPPO Find N is equipped with UTG ultra-thin flexible glass with a thickness of only 0.03mm. In the second quarter of 2022, 4 UTG cover glass were installed. UTG ultra-thin flexible glass has a small size, thin thickness, high strength, good resilience, and good hand feel. It provides a new direction for foldable computers and scroll displays and is favored by consumers. Ultra-thin glass (UTG) refers to glass with a thickness of less than 100μm and is flexible. Ultra-thin glass after surface processing and edge processing is widely used in various electronic industries due to its advantages such as high impact resistance and bending performance. It has marked a major milestone for the folding display industry and has become an important position in the foldable flexible field after CPI cover plates.

[0003] In the process of realizing the present invention, the inventors found that the prior art has at least the following problems: since the basic thickness of the ultra-thin glass currently under research is 30-100μm, and since the glass is relatively brittle and thin, the non-bending area will also be very thin while ensuring the performance of the bending area, and the impact strength is relatively low. In response to this phenomenon, unequal thickness grooved glass is developed as an ultra-thin glass cover plate, so that the thickness of the non-bending area is thicker than that of the bending area, ensuring the performance of the bending area while ensuring the strength of the non-bending area. However, after chemical tempering treatment, the unequal thickness glass has different thicknesses between the bending area and the non-bending area, and the expansion rate after tempering is different, resulting in wavy "wrinkles" in the bending area after tempering, affecting the appearance and performance of the product. Summary of the invention

[0004] The technical problem to be solved by the present invention is to provide a chemical tempering device and a tempering method for ultra-thin glass of unequal thickness, which can accurately control the bending area and the non-bending area to be strengthened separately, and can effectively suppress the wrinkle phenomenon in the bending area after chemical tempering treatment of ultra-thin glass of unequal thickness.

[0005] In order to solve the above technical problems, the technical solution adopted by the present invention is: a chemical tempering device for ultra-thin glass of unequal thickness, comprising:

[0006] a frame capable of accommodating the flexible glass;

[0007] Limiting side teeth: a series of limiting side teeth are provided on the side of the frame, and the limiting side teeth can position the side of the flexible glass;

[0008] Guide grooves are arranged on both sides of the frame;

[0009] A pressure rod is slidably mounted in the guide groove, and the pressure rod can limit the bending portion of the flexible glass.

[0010] Two rows of limiting side teeth are arranged on one side of the frame, and the two rows of limiting side teeth can be respectively matched with the two ends of the flexible glass.

[0011] The pressure rod can be clamped in the guide groove by a nut.

[0012] The tempering method of the above-mentioned ultra-thin glass chemical tempering device of unequal thickness comprises the following steps:

[0013] 1) heating potassium nitrate until the potassium nitrate is in a molten state;

[0014] 2) Bend the ultra-thin glass of different thicknesses and put them into the railing;

[0015] 3) After preheating the glass and the railing, place them in molten potassium nitrate so that the potassium nitrate liquid level covers the non-bending area and start tempering;

[0016] 4) After tempering is completed, take out, cool and clean;

[0017] 5) After preheating the glass again, put the entire glass into molten potassium nitrate so that the potassium nitrate liquid level submerges the entire glass to start tempering;

[0018] 6) After tempering is completed, take out, cool and clean, and you can get the finished tempered ultra-thin glass of varying thickness.

[0019] In step 3), the tempering time is 43 to 64 minutes; in step 5), the tempering time is 10 to 15 minutes.

[0020] In step 3) and step 5), the melting temperature of potassium nitrate is 370°C to 380°C.

[0021] The thickness of the unequal thickness ultra-thin glass in the bending zone is 30-70 μm, and the thickness of the non-bending zone is 70-200 μm.

[0022] The size of the ultra-thin glass of unequal thickness is between 50*50mm and 300*400mm.

[0023] The tempering temperature of the ultra-thin glass of unequal thickness is 370-420°C.

[0024] After the unequal thickness ultra-thin glass is tempered, the CS of the glass is 600-900MPa and the DOL is 6-9μm; after the unequal thickness ultra-thin glass is tempered, the non-bending area of ​​the glass reaches 380-450mm.

[0025] One of the above technical solutions has the following advantages or beneficial effects. It can precisely control the strengthening of the bending zone and the non-bending zone separately, effectively suppress the wrinkling phenomenon in the bending zone after chemical tempering of ultra-thin glass of unequal thickness, and can correspond to the glass with a thickness of 30-70μm in the bending zone, 70-200μm in the non-bending zone, and a size of 50*50-300*400mm. The tempering temperature is 370-420℃, and the CS (surface compressive stress of the glass) after tempering is 600-900MPa, and the DOL (depth of the stress layer of the glass) is 6-9μm. The non-bending zone can reach 380-450mm, which is significantly improved compared to the 220-260mm UTG pen of equal thickness. It has excellent impact resistance compared to the equal-thickness glass with the same thickness as the bending zone. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is a schematic structural diagram of a chemical tempering device for ultra-thin glass of unequal thickness provided in an embodiment of the present invention;

[0027] Figure 2 for Figure 1 A schematic diagram of the structure of a chemical tempering device for ultra-thin glass of unequal thickness;

[0028] Figure 3 for Figure 1 A schematic diagram of the structure of the glass of the chemical tempering device for ultra-thin glass of unequal thickness;

[0029] Figure 4 for Figure 1 Working principle diagram of chemical tempering device for ultra-thin glass of unequal thickness;

[0030] The marks in the above figures are: 1, frame, 11, guide groove, 12, handle, 2, limiting side teeth, 3, pressure rod, 4, flexible glass. DETAILED DESCRIPTION

[0031] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0032] Embodiment 1

[0033] See also Figure 1-4, a chemical tempering device for ultra-thin glass of unequal thickness, having:

[0034] The frame can accommodate the flexible glass; the limiting side teeth are provided with a series of limiting side teeth on the side of the frame, and the limiting side teeth can locate the side of the flexible glass; two rows of limiting side teeth are provided on one side of the frame, and the two rows of limiting side teeth can respectively match with the two ends of the flexible glass. After the flexible glass is bent, the two ends of the bend are respectively matched with the two rows of limiting side teeth on the side of the frame, so as to achieve the limiting effect, such as Figure 2 shown.

[0035] The guide groove is arranged on both sides of the frame; the pressure rod is slidably installed in the guide groove, and the pressure rod can limit the bending part of the flexible glass. After the flexible glass is limited on the limiting side teeth, the pressure rod is moved to slide in the guide groove, and the bending part of the flexible glass is limited by the pressure rod. The pressure rod can be clamped in the guide groove by a nut. After the limiting is completed, the pressure rod is clamped by the nut. The bending part of the flexible glass is limited by the pressure rod to prevent the glass from floating up during processing in the solution, which affects the processing.

[0036] Before tempering, the glass is bent and placed in a fixed railing so that the horizontal heights of the bending area and the non-groove area are not on the same plane. Then the side line position is controlled so that the tempering liquid level is at the side line position. The non-bending area is tempered first, and then the glass is laid flat and tempered as a whole again. Since the non-bending area is thicker and has a lower expansion rate, the tempering time is controlled by the relationship between the tempering time and the glass thickness during overall tempering so that the expansion rates of the non-bending area and the bending area are consistent, thereby solving the "wrinkle" problem and making the surface of the unequal thickness glass smooth and flat after chemical tempering.

[0037] The main structure of the railing tooling is composed of bottom teeth and limiting side teeth. It can be adjusted in different directions such as front, back, left, right, up and down to adapt to glass of different sizes. Each railing can fix multiple pieces of UTG. The limiting side teeth are made of high-temperature resistant quartz rope. The bottom teeth of the railing are mainly U-shaped, which can limit the position of each piece of ultra-thin glass, adjust the degree of glass bending, and temper glass of different sizes and thicknesses.

[0038] The main process of the present invention includes chemical tempering, which involves placing the glass in a molten potassium nitrate solution to exchange sodium ions in the surface layer of the glass with potassium ions in the molten salt. Due to the volume change after the exchange, the expansion rates of the non-bending area and the bending area are inconsistent, forming apparent "wrinkles". In order to eliminate the "wrinkles", the process flow is as follows: Figure 2As shown, before tempering, the glass is bent and placed in a fixed railing so that the horizontal heights of the bending area and the non-groove area are not on the same plane, and then the side line position is controlled so that the tempering liquid level is at the side line position. The non-bending area is tempered first, and then the glass is laid flat and tempered as a whole again. Since the non-bending area is thicker and has a lower expansion rate, the tempering time is controlled by the relationship between the tempering time and the glass thickness during overall tempering so that the expansion rates of the non-bending area and the bending area are consistent, thereby solving the "wrinkle" problem and making the surface of the unequal thickness glass smooth and flat after chemical tempering.

[0039] The operation is convenient, the processing cycle is short, mass production planning can be realized, the glass edge and surface are processed accordingly, the yield is high, and the finished groove glass has high impact resistance and excellent bending performance, which can meet the current market demand for electronic product cover plates and has good use value. The specific implementation of the present invention is not limited to the above-mentioned method. As long as various non-substantial improvements are made using the method concept and technical solution of the present invention, they are all within the protection scope of the present invention.

[0040] Embodiment 2

[0041] A chemical tempering processing method for an ultra-thin foldable flexible glass cover, taking glass with a thickness of 40 μm in the bending area and 100 μm in the non-bending area as an example, using 99.9% pure potassium nitrate, which is molten when heated to 380°C, and using Figure 2 Fix ultra-thin glass of different thicknesses in accordance with Figure 2 Tempering is performed by tempering. When the glass and the fixture are preheated to 380℃, they are put into molten potassium nitrate, so that the potassium nitrate liquid level is kept level with the limiting side teeth, the non-bending area is immersed, and the tempering is performed for 43 minutes, then taken out, cooled and cleaned. Then the glass is preheated to 380℃ and the entire glass is put into 380℃ molten potassium nitrate for tempering for 15 minutes, taken out, cooled and cleaned, and the finished product of tempered ultra-thin glass of unequal thickness can be obtained. The CS of the overall sample is measured to be 790MPa, the DOL is 9.2μm, the non-bending area is 345mm, and the analog plate thickness is 40μm. After tempering at 380℃ for 15 minutes, the pen is 230mm, which is greatly improved, and there is no appearance defect on the surface of the non-equal thickness area, and the bending performance can meet R1200k.

[0042] Embodiment 3

[0043] A chemical tempering processing method for an ultra-thin foldable flexible glass cover, taking glass with a thickness of 30 μm in the bending area and 200 μm in the non-bending area as an example, using 99.9% pure potassium nitrate, which is molten when heated to 370°C, according to Figure 2Tempering is performed by tempering. When the glass and the fixture are preheated to 380℃, they are put into molten potassium nitrate, so that the potassium nitrate liquid level is kept level with the limiting side teeth, the non-bending area is immersed, and the tempering is performed for 64 minutes, then taken out, cooled and cleaned, and then the glass is preheated to 370℃ and the entire glass is put into 380℃ molten potassium nitrate for tempering for 10 minutes, taken out and cooled, and cleaned to obtain the finished product of tempered ultra-thin glass of unequal thickness. The measured CS is 750MPa, the DOL is 13.2μm, the non-bending area is 420mm, and the analog plate thickness is 30μm. After tempering at 380℃ for 10 minutes, the pen is 210mm, which is greatly improved, and there is no obvious difference between the surface and ultra-thin and equal-thick glass.

[0044] Embodiment 4

[0045] A chemical tempering processing method for an ultra-thin foldable flexible glass cover, taking glass with a thickness of 30 μm in the bending area and 150 μm in the non-bending area as an example, using 99.9% pure potassium nitrate, which is molten when heated to 380°C, according to Figure 2 Tempering is performed by tempering. When the glass and the fixture are preheated to 380℃, they are put into molten potassium nitrate, so that the potassium nitrate liquid level is kept level with the limiting side teeth, the non-bending area is immersed, and the tempering is performed for 55 minutes, then taken out, cooled and cleaned, and then the glass is preheated to 370℃ and the entire glass is put into 380℃ molten potassium nitrate for tempering for 10 minutes, taken out and cooled, and cleaned to obtain the finished product of tempered ultra-thin glass of unequal thickness. The measured CS is 732MPa, the DOL is 11.9μm, the non-bending area is 390mm, and the analog plate thickness is 30μm. After tempering at 380℃ for 10 minutes, the pen is 210mm, which is greatly improved, and there is no obvious difference between the surface and ultra-thin and thick glass.

[0046] It can effectively suppress the wrinkle phenomenon in the bending zone of ultra-thin glass of unequal thickness after chemical tempering treatment. It can correspond to glass with a thickness of 30-70μm in the bending zone, 70-200μm in the non-bending zone, and a size of 50*50-300*400mm. The tempering temperature is 370-420℃, the CS of the tempered glass is 600-900MPa, the DOL is 6-9μm, and the non-bending zone can reach 380-450mm. Compared with the equal-thickness UTG pen of 220-260mm, the performance has been greatly improved. Compared with the equal-thickness glass with the same thickness in the bending zone, it has excellent impact resistance.

[0047] The operation is convenient, the processing cycle is short, mass production planning can be realized, the glass edge and surface are processed accordingly, the yield is high, and the finished groove glass has high impact resistance and excellent bending performance, which can meet the current market demand for electronic product cover plates and has good use value. The specific implementation of the present invention is not limited to the above-mentioned method. As long as various non-substantial improvements are made using the method concept and technical solution of the present invention, they are all within the protection scope of the present invention.

[0048] The quartz bottom teeth and limit side teeth are used to effectively solve the "wrinkle" phenomenon in the bending area of ​​unequal thickness glass. The segmented tempering method can simultaneously ensure the excellent bending ability of the bending area and the excellent impact resistance of the non-bending area. It can effectively control the accuracy and realize the zone tempering.

[0049] It effectively solves the problem of apparent wrinkles on the tempered ultra-thin glass of unequal thickness. The operation is simple, and the finished glass produced has uniform stress value and stress layer, ensuring that the finished glass of unequal thickness has high impact resistance and excellent bending performance. At the same time, it has high transmittance and bending strength, is mass producible, and can effectively solve the problem of low impact strength in the non-bending area, opening up broad horizons for folding screen electronic devices and providing a new possibility for the flexible screen market.

[0050] In the description of the present invention, it is necessary to understand that the terms "coaxial", "bottom", "one end", "top", "middle", "the other end", "upper", "one side", "top", "inside", "front", "center", "both ends" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0051] In the present invention, unless otherwise clearly stipulated and limited, the terms such as "installation", "setting", "connection", "fixation" and "screw-on" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium; it can be the internal connection of two elements or the interaction relationship between two elements. Unless otherwise clearly defined, ordinary technicians in this field can understand the specific meanings of the above terms in the present invention according to the specific circumstances.

[0052] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A tempering method for ultra-thin glass chemical tempering device with unequal thickness, It is characterized in that The tempering device has: a frame capable of accommodating the flexible glass; Limiting side teeth: a series of limiting side teeth are provided on the side of the frame, and the limiting side teeth can position the side of the flexible glass; Guide grooves are arranged on both sides of the frame; A pressure rod, slidably mounted in the guide groove, the pressure rod being capable of limiting the bending portion of the flexible glass; The tempering method of the tempering device includes the following steps: 1) Heat potassium nitrate to a molten state; 2) Bend the ultra-thin glasses of different thicknesses and place them in the tempering device; 3) After preheating the glass and the tempering device, put them into molten potassium nitrate so that the potassium nitrate liquid level submerges the non-bending area and starts tempering; 4) After tempering, take out, cool and clean; 5) Preheat the glass again and put it into molten potassium nitrate so that the potassium nitrate liquid level covers the entire glass to start tempering; 6) After tempering is completed, take it out, cool it, and clean it to get the finished tempered ultra-thin glass of varying thickness.

2. The tempering method of the chemical tempering device for ultra-thin glass of unequal thickness as claimed in claim 1, It is characterized in that Two rows of limiting side teeth are arranged on one side of the frame, and the two rows of limiting side teeth can be respectively matched with the two ends of the flexible glass.

3. The tempering method of the chemical tempering device for ultra-thin glass of unequal thickness as claimed in claim 2, It is characterized in that The pressure rod can be clamped in the guide groove by a nut.

4. The tempering method of the chemical tempering device for ultra-thin glass of unequal thickness as claimed in claim 3, It is characterized in that In step 3), the tempering time is 43~64min; in step 5), the tempering time is 10~15min.

5. The tempering method of the chemical tempering device for ultra-thin glass of unequal thickness as claimed in claim 4, It is characterized in that In step 3) and step 5), the melting temperature of potassium nitrate is 370°C to 380°C.

6. The tempering method of the chemical tempering device for ultra-thin glass of unequal thickness as claimed in claim 5, It is characterized in that The thickness of the unequal thickness ultra-thin glass in the bending zone is 30-70 μm, and the thickness of the non-bending zone is 70-200 μm.

7. The tempering method of the chemical tempering device for ultra-thin glass of unequal thickness as claimed in claim 6, It is characterized in that The size of the ultra-thin glass of unequal thickness is between 50*50 mm and 300*400 mm.

8. The tempering method of the chemical tempering device for ultra-thin glass of unequal thickness as claimed in claim 7, It is characterized in that The tempering temperature of the ultra-thin glass of unequal thickness is 370-420°C.

9. The tempering method of the chemical tempering device for ultra-thin glass of unequal thickness as claimed in claim 8, It is characterized in that After the unequal thickness ultra-thin glass is tempered, the CS of the glass is 600-900MPa and the DOL is 6-9μm; after the unequal thickness ultra-thin glass is tempered, the non-bending area of ​​the glass reaches 380-450mm.