A process for hydrodesiliconization of high-silicon naphtha
By separating naphtha into light and heavy components and using a combined process of hydrogenating deolefins with organic matter containing hydroxyl or carboxyl groups and silicon capture catalysts, the problem of difficulty in removing stable silicon compounds in high-silica naphtha has been successfully solved, and heavy-duty processing has been achieved. The feed to the whole or ethylene cracking unit reaches the standard, which improves the processing efficiency and economic benefits.
Patent Information
- Application Number
- CN202210408712.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2021-10-31
- Filing Date
- 2022-04-19
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2042-04-19
AI Technical Summary
It is difficult to effectively remove stable silicon compounds, such as alkyl silanes, silanols or silicon ethers, from naphtha with high silicon content using existing technology, resulting in substandard feeds to reforming or ethylene cracking units, affecting the stability of the units. run.
The feed oil is separated into light components and heavy components. Organic matter containing hydroxyl and/or carboxyl groups is added to the light component. Through the action of hydrogenation deolefinization catalyst and silicon capture catalyst, the deolefinization and desiliconization reactions are carried out respectively, and the recombination is carried out. Hydrodesulfurization and denitrification reactions are carried out separately to achieve efficient silicon removal.
It achieves the effective removal of silicon compounds that are difficult to remove from high-silica naphtha, meets the feed requirements of reforming or ethylene cracking units, and improves the processing efficiency and economic benefits of the unit.
Smart Images

Figure CN116064111B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of clean oil refining, and in particular relates to a process for hydrogenating and desiliconizing naphtha. Background Art
[0002] With the overcapacity of my country's fuel oil market, reducing diesel and producing more chemical raw materials are the general direction of adjusting the structure of refining products. Naphtha from different sources can be used as raw materials for ethylene cracking, reforming pre-hydrogenation and other units after hydrofining to remove or partially remove impurities such as silicon, olefins, sulfur, and nitrogen. The requirements for the feed of the reforming unit are relatively strict, usually requiring low sulfur (<0.5ppm), low nitrogen (<0.5ppm), and low impurity content (<0.5ppm); for the impurity content in the ethylene cracking raw material, especially the silicon content <0.1ppm. Among them, the impurity silicon in naphtha is easily deposited on the catalyst, covering the active metal and blocking the pores, causing the catalyst to deactivate, and it cannot be removed by the method of burning regeneration, which directly affects the long-term operation of the unit. Therefore, desiliconization treatment is often carried out to avoid poisoning and deactivation of the refined catalyst. Research has found that naphtha from different sources contains complex types of silicon compounds, including cyclosiloxanes, siloxanes, silanes, etc. Among them, cyclosiloxanes are easier to remove, while siloxanes and silanes are more difficult to remove. The silicon content in some naphtha is as high as 300~1000ppm. It is difficult to remove silicon with current technology to meet the requirements of reforming or ethylene cracking unit feed.
[0003] CN200710012085.5 discloses a method for hydrofining silicon-containing fraction oil. In this method, silicon-containing fraction oil raw material and hydrogen are passed through at least two hydrofining catalyst beds under hydrofining conditions, and the silicon-containing fraction oil first passes through a hydrogenation catalyst bed with silicon-capturing function, and then passes through a conventional hydrofining catalyst bed; wherein the hydrogenation catalyst with silicon-capturing function has a large pore volume and specific surface area and a relatively low metal content. The silicon compound targeted by this method comes from the defoamer added in the coking unit, which has a low silicon content and is mainly cyclosiloxane compounds that are easy to remove.
[0004] CN200810113398.4 discloses a method for hydrofining inferior gasoline. In this method, gasoline raw oil is contacted with a hydrogenation protective agent under low temperature conditions for reaction, and the reaction effluent is mixed with circulating oil and then contacted with a hydrogenation desiliconizing agent and a hydrofining catalyst in sequence under high temperature conditions for reaction, and the reaction product is cooled and separated to obtain hydrogen-rich gas and refined gasoline fractions, and part of the refined gasoline fractions are returned to the outlet of the first hydrogenation reaction zone as circulating oil. This method is mainly used to treat coked gasoline with high sulfur, high nitrogen and high olefin content, and to alleviate coking and the deactivation rate of the refining catalyst at the bottom of the reactor.
[0005] At present, the research on desiliconization of oil products mainly focuses on relatively easy-to-remove cyclosiloxane compounds, with a general silicon content of <100ppm. With the development of crude oil extraction technology, it has been found in recent years that some naphtha contains higher levels of silicon compounds, and the siloxanes and silanes in them are difficult to effectively remove using existing technologies, which directly affects the smooth operation of the device and the subsequent oil processing process. Summary of the invention
[0006] The analysis results of high-silicon naphtha show that the silicon compounds therein are mainly alkylsilane, silanol or silyl ether silicon-containing compounds. After the raw oil products are treated according to the desiliconization methods and processes of the prior art, the silicon content is still very high, and it is difficult to make the silicon content meet the standards even by adjusting the process operating conditions. In addition, the study found that these silicon compounds are mainly present in the light fraction of the oil products. Based on the above research results, the present invention provides a desiliconization process method for high-silicon naphtha, which can effectively remove high-content difficult-to-remove silicon compounds and impurities such as olefins, sulfur, and nitrogen in the oil products, and provide qualified raw materials for reforming or ethylene cracking devices.
[0007] The process method for hydrodesiliconation of high-silicon naphtha of the present invention comprises the following contents: separating crude oil to obtain light components and heavy components; wherein the light components and at least one organic matter containing hydroxyl and / or carboxyl groups enter into a first reactor, the first reactor is filled with at least one hydrodeolefination catalyst, the effluent of the first reactor enters into a second reactor, the second reactor is filled with at least one silicon capture catalyst; the heavy components enter into a third reactor, the third reactor is filled with at least one hydrogenation catalyst, and hydrodesulfurization and hydrodenitrogenation reactions are carried out; when the sulfur and nitrogen content in the effluent of the second reactor meets the standard, the effluent of the third reactor is directly mixed and used as feed for a reforming or ethylene cracking device; when the sulfur and nitrogen content in the effluent of the second reactor does not meet the standard, the effluent of the third reactor is firstly entered into the third reactor for reaction, and the effluent of the third reactor is used as feed for a reforming or ethylene cracking device.
[0008] In the process of the present invention, the raw oil is at least one of straight-run naphtha, coking naphtha, hydrogenated reformed naphtha, jet fuel, gasoline and light diesel; the silicon content of the raw oil is 1-3000 μg / g, and the raw oil with a high silicon content needs to be desiliconized for several cycles to meet the standard, and the raw oil with a silicon content of 5-700 μg / g is preferably treated.
[0009] Furthermore, according to the properties of the crude oil, a silicon trap can be selectively loaded in the upper bed layer at the entrance of the third reactor, and the easily removable silicon compounds such as cyclosiloxanes and silanes in the heavy component can be treated by conventional desiliconization methods using existing technology to avoid poisoning of the catalyst in the third reactor. That is, there is at least one silicon-containing compound other than cyclic siloxane compounds and silane compounds in the crude oil. Among them, the cyclic siloxane compound is a cyclic silicon-oxygen bond (-Si-O-) n , n≥3 as the main chain of organic silicon compounds, such as those having the general formula (H 2 SiO) n , n≥3, or a compound in which H in the general formula is replaced by an alkyl group, a halogen, etc.; the silane compound is a compound having Si n H 2n+2 , an organosilicon compound of the general formula: n≥1.
[0010] Furthermore, the silicon-containing compound in the feedstock oil includes but is not limited to at least one of alkylsilane, silanol or silane ether silicon-containing compounds.
[0011] Furthermore, as a specific embodiment, the silicon-containing compounds in the crude oil include but are not limited to at least one of tetramethylsilane, triethylsilane, tetraethylsilane, tetrapropylsilane, trimethylsilanol, dimethoxydimethylsilane, diethoxydimethylsilane, hexamethyldisiloxane, dimethyloctylchlorosilane, octamethyltrisiloxane and n-octyltriethoxysilane.
[0012] The above silicon compounds are more stable than epoxysilane compounds or silane compounds. It is difficult to remove them to meet the requirements using the existing desiliconization conditions and silicon trapping catalysts. The present invention adopts a method of adding organic matter containing hydroxyl and / or carboxyl groups. The inventors found that organic matter containing hydroxyl and / or carboxyl groups helps to remove the above stable silicon compounds. The specific principle may be that the hydroxyl and carboxyl groups in the organic matter help to break the Si-O or Si-C bonds, exposing Si atoms, and then being removed by the silicon trapping agent.
[0013] During the above process, the crude oil is separated into light components and heavy components, the distillation range of the light component is <110°C, and the ratio of silicon content to total silicon content is >98%; after the crude oil is cut, most of the silicon that is difficult to remove exists in the light component, and the heavy component is directly desulfurized and denitrified, which is beneficial to reduce the difficulty of processing and improve the processing efficiency of the device. The mass content of the organic matter containing hydroxyl and / or carboxyl groups in the light component is 0.01-5wt%, preferably 0.5-3.5wt%, and more preferably 1-2.5wt%; the inventors found that after the effluent of the first reactor was cut, most of the silicon that was difficult to remove existed in the light component, so cutting was adopted first and then desiliconization was carried out on the light component, while the heavy component was directly desulfurized and denitrified, which was beneficial to reduce the difficulty of processing and save the process.
[0014] Further, the organic matter containing hydroxyl and / or carboxyl groups is alcohol or organic acid, and more preferably C1-C10 alcohol and / or acid, more preferably C2-C8 alcohol and / or acid; most preferably C2-C6 alcohol and / or acid. Wherein, the alcohol and / or acid includes monohydric alcohol, dihydric alcohol, trihydric alcohol, monobasic acid, dibasic acid and tribasic acid; as a more specific embodiment, the organic matter containing hydroxyl and / or carboxyl groups is selected from at least one of ethanol, ethylene glycol, propanol, propylene glycol, glycerol, butanol, butanediol, butanetriol, pentanol, acetic acid, oxalic acid, tartaric acid, succinic acid, glycolic acid and citric acid.
[0015] Furthermore, the process conditions of the first reactor are: reaction pressure 1-4 MPa, hydrogen-to-oil volume ratio 80-200, volume space velocity 2-8 h -1 The reaction temperature is 40-150° C., preferably 40-100° C., and most preferably 50-80° C. The reaction conditions in the first reactor are controlled so that the olefin removal rate is 95-100%.
[0016] Furthermore, the process conditions of the second reactor are: reaction pressure 1-4 MPa, hydrogen-oil volume ratio 100:1-200:1, volume space velocity 2-8 h -1 , the reaction temperature is 250~400℃, preferably 260~380℃.
[0017] Furthermore, when the silicon content in the effluent of the second reactor is high and does not meet the standard, it is circulated to the second reactor for hydrodesiliconization again. Specifically, when the silicon content in the effluent of the second reactor is ≥1ppm, it is circulated to the inlet of the second reactor for further hydrodesiliconization until the silicon content in the effluent of the second reactor is <1ppm.
[0018] Furthermore, the process conditions in the third reactor are: reaction pressure 2-6 MPa, hydrogen-oil volume ratio 100:1-500:1, volume space velocity 1-5 h -1 , the reaction temperature is 200~400℃, preferably 220~360℃.
[0019] Furthermore, the active metal of the hydrodeolefination catalyst is a metal of Group VIII, and the content of the reduced metal of Group VIII is 5% to 30%, preferably 10% to 20%, based on the weight of the hydrodeolefination catalyst; the carrier is alumina or additive-modified alumina, and the additive is one or more of Mo, B, P, Mg, Zr or Si, and the additive is 1% to 15%, preferably 2% to 8%, in terms of oxide, based on the weight of the carrier. The preparation method of the catalyst is well known in the art, and one or more of the impregnation method, the coextrusion method, and the coprecipitation method can be used. Under the catalyst and process conditions of the first reactor, the hydrodeolefination reaction is mainly carried out, which can prevent olefin polymerization and coking. Under these conditions, the silicon-containing compounds that are difficult to remove in the light component will not affect the catalyst in the first reactor.
[0020] Furthermore, the active metal of the silicon capture catalyst loaded in the second reactor is a metal oxide of Group VIB or / and a metal oxide of Group VIII, the carrier is alumina or additive-modified alumina, and the content of the metal oxide of Group VIB is 5% to 30%, preferably 5% to 15%, and the content of the metal oxide of Group VIII is 1% to 15%, preferably 2% to 6%, based on the weight of the silicon capture catalyst; the specific surface area is 100 to 500 m 2 / g, preferably 300~500m 2 / g, the pore volume is 0.3~1.2mL / g, preferably 0.4~0.8mL / g. The preparation method of the catalyst is well known in the art, and one or more of the following methods can be used: impregnation method, co-extrusion method, and co-precipitation method. Under the process conditions of the second reactor, the organic matter containing hydroxyl and / or carboxyl groups is used as an auxiliary agent, and under the action of the silicon capture catalyst, the silicon-containing compound in the raw material can be removed.
[0021] Further, the hydrogenation catalyst loaded in the third reactor is a catalyst with desulfurization and denitrification activity, the active metal is a metal oxide of Group VIB or / and a metal oxide of Group VIII, based on the weight of the hydrogenation catalyst, the content of the metal oxide of Group VIB is 5% to 30%, preferably 15% to 25%, and the content of the metal oxide of Group VIII is 1% to 15%, preferably 3% to 8%; the carrier is alumina or additive-modified alumina, the additive is one or more of B, P, Mg, Zr or Si, based on the weight of the carrier, the additive is 3% to 15% in terms of oxide, preferably 3% to 10%. The preparation method of the catalyst is well known in the art, and one or more of the impregnation method, the co-extrusion method, and the co-precipitation method can be used. Under the catalyst and process conditions of the third reactor, hydrodesulfurization and hydrodenitrogenation reactions are mainly carried out. According to the silicon content in the heavy components at the inlet of the third reactor, the hydrogenation catalyst and the silicon-trapping catalyst are optionally loaded in the third reactor in a graded manner, and the silicon-trapping catalyst is in the upper bed layer to ensure the removal of silicon-containing compounds to protect the hydrogenation catalyst. The volume ratio of the silicon-trapping catalyst to the hydrogenation catalyst is 1:9~1:1.
[0022] The process method of the present invention aims at the problem that the silicon content in the raw oil does not meet the standard. It adopts a process different from the conventional desiliconization treatment process, and separates the light and heavy components and then undergoes a process route of deolefination and desiliconization, desulfurization and denitrogenation. This route can simply and efficiently remove stable silicon compounds to obtain qualified reforming or ethylene cracking raw materials. Specifically, since the stable silicon compounds in the raw oil are mainly present in the light fraction, the present invention first separates the light and heavy components; wherein the light component undergoes a hydrogenation deolefination reaction under mild conditions in the first reactor to avoid coking of the catalyst in the second reactor, and then enters the second reactor to undergo a desiliconization reaction under the action of an organic alcohol or / and an organic acid and a silicon-capturing catalyst; the heavy component undergoes a hydrogenation desulfurization and denitrogenation reaction in the third reactor; and the effluents of the second reactor and the third reactor are mixed and used as feed for the reforming or ethylene cracking device. The process method of the present invention can solve the problem faced by enterprises that the high silicon content of naphtha raw materials cannot meet the feed requirements of the reforming or ethylene devices, and create considerable economic benefits for the enterprises. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 . Schematic diagram of the device for producing reforming feed or ethylene cracking feed used in the examples.
[0024] In the figure: 1-raw oil, 2-separator, 3-light component, 4-heavy component, 5-hydrogen, 6-first reactor, 7-effluent from the first reactor, 8-second reactor, 9-effluent from the second reactor, 10-third reactor, 11-effluent from the third reactor. DETAILED DESCRIPTION
[0025] The following non-limiting embodiments may enable a person skilled in the art to more fully understand the present invention, but are not intended to limit the present invention in any way.
[0026] The composition of the catalyst provided by the present invention can be characterized by combining inductively coupled plasma ICP and XRF energy spectrum to characterize the total content of the VIB group metal and the total content of the VIII group metal in the catalyst. The specific surface area and pore volume of the catalyst provided by the present invention are analyzed by nitrogen physical adsorption. The silicon content and type in the raw oil and the product of the present invention are analyzed by ICP and nuclear magnetic resonance, wherein the silicon content in the raw oil and the product is analyzed by ICP, and the type of silicon in the raw oil and the product is analyzed by nuclear magnetic resonance 29Si MASNMR.
[0027] In Example 1, a silicon capture catalyst was prepared:
[0028] Example 1
[0029] An equal volume of a solution containing nickel salt and molybdenum salt was impregnated into an alumina carrier, then dried at 110°C for 3 h in an air atmosphere, and calcined at 350°C for 3 h to obtain a silicon-trapping catalyst C-1.
[0030] The weight percentages of the components in the silicon trapping catalyst C-1 are: 13.5% molybdenum oxide, 4.3% nickel oxide, and the rest aluminum oxide. The catalyst properties are shown in Table 1.
[0031] In Example 2, a hydrogenation catalyst was prepared:
[0032] Example 2
[0033] An equal volume of a solution containing nickel salt and molybdenum salt was impregnated into an alumina carrier, then dried at 110°C for 3 h in an air atmosphere, and calcined at 350°C for 3 h to obtain a hydrogenation catalyst C-2.
[0034] The weight percentages of the components in the hydrogenation catalyst C-2 are: 24.1% molybdenum oxide, 5.4% nickel oxide, and the remainder aluminum oxide. The catalyst properties are shown in Table 1.
[0035] In Example 3, a hydrodeolefination catalyst was prepared:
[0036] Example 3
[0037] An equal volume of a nickel salt-containing solution was impregnated into an alumina carrier, then dried at 110°C for 3 h in an air atmosphere, calcined at 350°C for 3 h, and then reduced in hydrogen at 450°C for 1 h to obtain a hydrodeolefination catalyst C-3.
[0038] The weight percentages of the components in the hydrodeolefination catalyst C-3 are as follows: 14.7% of metallic nickel and the rest of aluminum oxide. The catalyst properties are shown in Table 1.
[0039] Table 1
[0040]
[0041] by Figure 1 The implementation process of the process for producing reforming feed and ethylene cracking raw material of the present invention is described as follows: the raw oil 1 (naphtha) enters the separator 2 for separation to obtain a light component 3 and a heavy component 4; the light component 3 and hydrogen 5 enter the first reactor 6 under certain temperature and pressure conditions, and undergo a hydrodeolefination reaction in the first reactor 6 to obtain a first reactor effluent 7. The first reactor effluent 7 enters the second reactor 8 for a desiliconization reaction to obtain a second reactor effluent 9; the heavy component 4 enters the third reactor 10 for a hydrodesulfurization and hydrodenitrogenation reaction to obtain a third reactor effluent 11; the second reactor effluent 9 and the third reactor effluent 11 are mixed.
[0042] The feedstock oil is separated into light components 3 and heavy components 4 by separator 2. The first reactor 6 mainly undergoes a hydrodeolefination reaction to generate a light component with low olefin content, namely, the first reactor effluent 7. The second reactor 8 mainly undergoes a silicon capture reaction to remove silicon-containing compounds in the light component 7 to generate a second reactor effluent 9 with low silicon content. The third reactor 10 mainly undergoes hydrodesulfurization and hydrodenitrogenation reactions to generate a third reactor effluent 11 with low sulfur and low nitrogen content. The second reactor effluent 9 and the third reactor effluent 11 are mixed to obtain a qualified feed for the reforming or ethylene cracking unit.
[0043] Example 4
[0044] exist Figure 1 In the reaction device, a catalyst bed is set in the first reactor, the second reactor and the third reactor. The first reactor is filled with the Ni-based hydrodeolefination catalyst C-3 prepared in Example 3, the second reactor is filled with the Ni-Mo type silicon capture catalyst C-1 prepared in Example 1, and the third reaction zone is filled with the Ni-Mo type hydrogenation catalyst C-2 prepared in Example 2. The C-1 and C-2 catalysts are first subjected to an ex-situ sulfurization treatment, and the sulfurization conditions are: temperature of 340°C, hydrogen partial pressure of 3.0MPa, hydrogen-to-oil ratio of 500:1, volume space velocity of 2.0h -1 , the curing agent is 10%H 2 S / H 2 During the reaction process, the temperature of the reaction bed of each reactor is stable and controllable.
[0045] 1.0wt% oxalic acid was added to the light component 3, and the naphtha was provided by a refinery of Sinopec. The silicon content in the raw oil was 463μg / g, the sulfur content was 2757µg / g, and the nitrogen content was 346µg / g. The types of silicon in the raw oil were tetramethylsilane, dimethoxydimethylsilane, and triethylsilane according to nuclear magnetic resonance analysis. The final distillation point of the light component was 109°C, the silicon content was 457µg / g, the sulfur content was 109µg / g, and the nitrogen content was 22µg / g (in order to reflect the content changes of each element in the light and heavy components, the silicon content, sulfur content and nitrogen content were calculated based on the weight of the naphtha raw material). The reaction process conditions and results are shown in Table 2.
[0046] Example 5
[0047] The reaction apparatus, catalyst and sulfurization process used are the same as those in Example 4.
[0048] 1.5wt% ethanol was added to the light component 3, and the naphtha was provided by a refinery of Sinopec. The silicon content in the raw oil was 463μg / g, the sulfur content was 2757µg / g, and the nitrogen content was 346µg / g. The types of silicon in the raw oil were tetramethylsilane, dimethoxydimethylsilane, and triethylsilane according to nuclear magnetic resonance analysis. The final distillation point of the light component was 109°C, the silicon content was 457µg / g, the sulfur content was 109µg / g, and the nitrogen content was 22µg / g (in order to reflect the changes in the content of each element in the light and heavy components, the silicon content, sulfur content, and nitrogen content were calculated based on the weight of the naphtha raw material). The reaction process conditions and results are shown in Table 2.
[0049] Example 6
[0050] The reaction apparatus, catalyst and sulfurization process used are the same as those in Example 4.
[0051] 1.0wt% butanediol was added to the light component 3, and the naphtha was provided by a refinery of Sinopec. The silicon content in the raw oil was 463μg / g, the sulfur content was 2757µg / g, and the nitrogen content was 346µg / g. The types of silicon in the raw oil were tetramethylsilane, dimethoxydimethylsilane, and triethylsilane according to nuclear magnetic resonance analysis. The final distillation point of the light component was 109°C, the silicon content was 457µg / g, the sulfur content was 109µg / g, and the nitrogen content was 22µg / g (in order to reflect the changes in the content of each element in the light and heavy components, the silicon content, sulfur content, and nitrogen content were calculated based on the weight of the naphtha raw material). The reaction process conditions and results are shown in Table 2.
[0052] Example 7
[0053] The reaction apparatus, catalyst and sulfurization process used are the same as those in Example 4.
[0054] 1.0wt% malonic acid was added to the light component 3. The naphtha was provided by a refinery of Sinopec. The silicon content in the raw oil was 463μg / g, the sulfur content was 2757µg / g, and the nitrogen content was 346µg / g. The types of silicon in the raw oil were tetramethylsilane, dimethoxydimethylsilane, and triethylsilane according to nuclear magnetic resonance analysis. The final distillation point of the light component was 109°C, the silicon content was 457µg / g, the sulfur content was 109µg / g, and the nitrogen content was 22µg / g (in order to reflect the changes in the content of each element in the light and heavy components, the silicon content, sulfur content, and nitrogen content were calculated based on the weight of the naphtha raw material). The reaction process conditions and results are shown in Table 2.
[0055] Comparative Example 1
[0056] The reaction apparatus, catalyst and sulfurization process used are the same as those in Example 4.
[0057] No organic acid or organic alcohol is added to the light component 3. The naphtha is provided by a refinery of Sinopec. The silicon content in the raw oil is 463μg / g, the sulfur content is 2757µg / g, and the nitrogen content is 346µg / g. The types of silicon in the raw oil are tetramethylsilane, dimethoxydimethylsilane, and triethylsilane according to nuclear magnetic resonance analysis. The final distillation point of the light component is 109°C, the silicon content is 457µg / g, the sulfur content is 109µg / g, and the nitrogen content is 22µg / g (in order to reflect the content changes of each element in the light and heavy components, the silicon content, sulfur content and nitrogen content are calculated based on the weight of the naphtha raw material). The reaction process conditions and results are shown in Table 2.
[0058] Comparative Example 2
[0059] This comparative example uses three hydrogenation reactors, and a catalyst bed is set in the first hydrogenation reactor, the second hydrogenation reactor, and the third hydrogenation reactor. The first hydrogenation reactor is filled with the olefin hydrogenation catalyst C-3 prepared in Example 3, the second hydrogenation reactor is filled with the silicon capture catalyst C-1 prepared in Example 1, and the third hydrogenation reactor is filled with the first hydrogenation catalyst C-2 prepared in Example 2. The C-1 and C-2 catalysts are first subjected to an ex-situ sulfurization treatment, and the sulfurization conditions are: temperature 320°C, hydrogen partial pressure 3.0MPa, hydrogen-to-oil ratio 500:1, volume space velocity 2.0h -1 , the curing agent is 10%H 2 S / H 2 During the reaction process, the temperature of the reaction bed of each reactor is stable and controllable.
[0060] The naphtha was provided by a refinery of Sinopec. The silicon content in the raw oil was 463μg / g, the sulfur content was 2757μg / g, and the nitrogen content was 346μg / g. The types of silicon in the raw oil were tetramethylsilane, dimethoxydimethylsilane, and triethylsilane according to nuclear magnetic resonance analysis. The reaction process conditions and results are shown in Table 2.
[0061] Table 2
[0062]
[0063] The evaluation results in Table 2 indicate that the process for producing reforming feed or ethylene cracking feed of the present invention can effectively remove silicon from crude oil which is difficult to remove by conventional methods.
Claims
1. A process for hydrodesiliconization of high-silicon naphtha, comprising the following contents: The crude oil is separated into a light component and a heavy component, wherein the distillation range of the light component is less than 110° C. The light component and at least one organic matter containing hydroxyl and / or carboxyl groups enter into a first reactor, wherein at least one hydrodeolefination catalyst is loaded in the first reactor, and the effluent of the first reactor enters into a second reactor, wherein at least one silicon capture catalyst is loaded in the second reactor; The heavy component enters the third reactor, in which at least one hydrogenation catalyst is loaded, and hydrodesulfurization and hydrodenitrogenation reactions are carried out; when the sulfur and nitrogen content in the effluent of the second reactor meets the standard, it is directly mixed with the effluent of the third reactor and used as the feed of the reforming or ethylene cracking device; when the sulfur and nitrogen content in the effluent of the second reactor does not meet the standard, it first enters the third reactor for reaction, and then the effluent of the third reactor is used as the feed of the reforming or ethylene cracking device; The silicon-containing compound in the feedstock oil is selected from at least one of tetramethylsilane, triethylsilane, tetraethylsilane, tetrapropylsilane, trimethylsilanol, dimethoxydimethylsilane, diethoxydimethylsilane, hexamethyldisiloxane, dimethyloctylchlorosilane, octamethyltrisiloxane and n-octyltriethoxysilane; the organic matter containing hydroxyl and / or carboxyl groups is selected from at least one of ethanol, ethylene glycol, propanol, propylene glycol, glycerol, butanol, butanediol, butanetriol, amyl alcohol, acetic acid, oxalic acid, tartaric acid, succinic acid, glycolic acid and citric acid; the mass content of the organic matter containing hydroxyl and / or carboxyl groups in the light component is 0.01-5wt%; The active metal of the silicon capture catalyst loaded in the second reactor is a metal oxide of Group VIB or / and a metal oxide of Group VIII, the carrier is alumina or additive-modified alumina, and the content of the metal oxide of Group VIB is 5% to 30% and the content of the metal oxide of Group VIII is 1% to 15% based on the weight of the silicon capture catalyst; the specific surface area is 100 to 500 m 2 / g, and the pore volume is 0.3~1.2mL / g.
2. The process according to claim 1, characterized in that: The silicon content of the raw oil is 1-3000 μg / g.
3. The process according to claim 1, characterized in that: According to the properties of the crude oil, a silicon scavenger is loaded in the upper bed layer at the inlet of the third reactor to remove silicon from the heavy components.
4. The process according to claim 1, characterized in that: The mass content of the organic matter containing hydroxyl and / or carboxyl groups in the light component is 0.5-3.5wt%.
5. The process according to claim 4, characterized in that: The mass content of the organic matter containing hydroxyl and / or carboxyl groups in the light component is 1-2.5wt%.
6. The process according to claim 1, characterized in that: The process conditions of the first reactor are: reaction pressure 1~4MPa, hydrogen-oil volume ratio 80~200, volume space velocity 2~8h -1 , reaction temperature 40~150℃, control the reaction conditions in the first reactor so that the olefin removal rate is 95~100%.
7. The process according to claim 1, characterized in that: The process conditions of the second reactor are: reaction pressure 1~4MPa, hydrogen oil volume ratio 100:1~200:1, volume space velocity 2~8h -1 , reaction temperature 250~400℃.
8. The process according to claim 1, characterized in that: When the silicon content in the effluent of the second reactor is ≥1 ppm, it is recycled to the inlet of the second reactor for re-feeding for further hydrodesiliconization until the silicon content in the effluent of the second reactor is <1 ppm.
9. The process according to claim 1, characterized in that: The process conditions in the third reactor are: reaction pressure 2-6 MPa, hydrogen-to-oil volume ratio 100:1-500:1, volume space velocity 1-5 h -1 , reaction temperature 200~400℃.
10. The process according to claim 1, characterized in that: The active metal of the hydrodeolefination catalyst is a Group VIII metal, and the content of the reduced Group VIII metal is 5% to 30% based on the weight of the hydrodeolefination catalyst; the carrier is alumina or additive-modified alumina, and the additive is one or more of Mo, B, P, Mg, Zr or Si, and the additive is 1% to 15% in terms of oxide based on the weight of the carrier.
11. The process according to claim 1, characterized in that: The active metal of the hydrogenation catalyst loaded in the third reactor is a metal oxide of Group VIB and / or a metal oxide of Group VIII, and the content of the metal oxide of Group VIB is 5% to 30% and the content of the metal oxide of Group VIII is 1% to 15% based on the weight of the hydrogenation catalyst; the carrier is alumina or alumina modified with an additive, and the additive is one or more of B, P, Mg, Zr or Si, and the additive is 3% to 15% in terms of oxide based on the weight of the carrier.