A kind of agent suitable for treating fluorine-containing wastewater in semiconductor industry

By using inorganic dispersion suspension formulas of calcium compounds and phosphates in fluorine-containing wastewater treatment, the high cost and precipitation problems in the treatment process of the semiconductor industry are solved, and the formulation and treatment efficiency are simplified, and energy consumption and management difficulties are reduced.

CN116177702BActive Publication Date: 2024-11-08明金阳
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202211692753.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-12-28
Publication Date
2024-11-08
Estimated Expiration
2042-12-28

AI Technical Summary

Technical Problem

The prior art has high costs, precipitation and scale problems when dealing with fluorine-containing wastewater in the semiconductor industry, and the preparation cycle is long and the method is complex, making it difficult to achieve industrial production.

Method used

Using an inorganic dispersion suspension formula containing calcium compounds, tripolyphosphates, polyaluminum chloride, phosphates and hexamer metaphosphates, avoid precipitation and scaling by uniformly distributing calcium oxide or calcium hydroxide, and simplifying preparation process.

Benefits of technology

It has achieved the reduction of energy consumption, the reduction of high-cost drug dosage, the improvement of fluorine-containing wastewater treatment capacity, the reduction of treatment costs, and the improvement of treatment effect and product stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116177702B_ABST
    Figure CN116177702B_ABST
Patent Text Reader

Abstract

The present invention belongs to the field of wastewater treatment technology, and in particular to a medicament suitable for the treatment of fluorine-containing wastewater in the semiconductor industry, which comprises the following components by weight percentage: calcium compound: 1%-50%; tripolyphosphate: 0.1%-10%; polyaluminium chloride: 1%-10%; phosphate: 1%-7%; hexapolyphosphate: 0.1%-10%; the remainder is water. Relative to the prior art, the present invention adopts a new inorganic dispersed suspension formula to prepare a suspended liquid on the basis of fully considering the advantages and disadvantages of using lime and calcium chloride. The formula is to enable calcium oxide and / or calcium hydroxide to be evenly distributed in an aqueous solution with extremely small particles without precipitation in a fluorine-containing wastewater treatment system without changing the existing process system, thereby completely solving the problem of precipitation and scaling caused by the use of lime and calcium chloride. Due to the use of calcium oxide and / or calcium hydroxide, the use of sodium hydroxide in the process treatment process is avoided, and from the perspective of operation, the cost of the medicament is greatly reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of wastewater treatment, and in particular relates to a medicament suitable for treating fluorine-containing wastewater in the semiconductor industry. Background Art

[0002] Companies that produce semiconductor chips and finished products use a large amount of chemical reagents such as hydrochloric acid, sulfuric acid, hydrofluoric acid, phosphoric acid, ammonia water, ammonium fluoride, etc. in the production process. The semiconductor production process is complex, with more than 300 process steps, and a variety of chemical reagents and special gases are used at the same time. The main production processes include: silicon wafer cleaning, oxidation / diffusion, chemical vapor deposition (CVD), photolithography, degumming, dry etching (DE), wet etching (WE), ion implantation, metallization (sputtering PVD, electroplating copper), chemical mechanical polishing CMP, and testing. Silicon wafers are cleaned with hydrofluoric acid, ammonium fluoride and high-purity water in the cleaning, etching stage, and cleaning system CDS processes, which is the source of fluoride-containing wastewater.

[0003] There are many methods for treating fluoride-containing wastewater, such as adsorption, freezing, ion exchange resin defluorination, activated carbon defluorination, ultrafiltration, and electrodialysis. These methods have rarely been promoted and applied, mainly because of their high cost and low defluorination rate. At present, the most practical treatment measures are based on chemical precipitation and coagulation precipitation.

[0004] At present, the semiconductor industry generally uses calcium salt precipitation to treat fluoride-containing wastewater, that is, adding lime or CaCl2 solution to the wastewater to remove fluoride ions and calcium ions by forming CaF2 precipitation. This process has the advantages of simple method and convenient treatment, but it has the disadvantages of difficult to meet the standards for the treated effluent, slow sedimentation of sludge and difficulty in dehydration. At the same time, the CaF2 content in the sludge is high, which is a dangerous solid pollutant and the treatment cost is extremely high.

[0005] Faced with the above shortcomings, many companies are considering using lime emulsion instead of CaCl2 solution to treat fluoride-containing wastewater. This process has the advantages of low cost, good treatment effect, easy dehydration, etc., but it also has the disadvantages of large dosage, easy precipitation, easy scaling, high energy consumption, etc. Therefore, it is impossible to achieve accurate dosing in actual use, which brings great difficulties to process management.

[0006] Patent No. CN201810111347.1 (A lime suspension suitable for fluoride-containing wastewater treatment and its preparation method) and Patent No. ZL 201810271997.2 (A treatment liquid for phosphorus-containing wastewater and its preparation method) both use a combination of inorganic and organic agents to solve the various problems caused by the above two agents, but there are still some shortcomings: (1) The preparation cycle is long and it is difficult to achieve industrial production; (2) The preparation method is complicated and the quality of the suspension is unstable.

[0007] Therefore, the present invention aims to provide a reagent suitable for treating fluorine-containing wastewater in the semiconductor industry, which can meet the requirements of industrial production while also overcoming the above two problems. Not only is the method simple, the preparation cycle is short, and only one formula is needed to solve all the above problems. This has a great promoting effect on reducing energy consumption, reducing the amount of high-cost reagents, scientifically improving the treatment capacity of fluorine-containing wastewater, and further reducing the cost of fluorine-containing wastewater treatment. Summary of the invention

[0008] The purpose of the present invention is to provide a reagent suitable for treating fluorine-containing wastewater in the semiconductor industry in view of the shortcomings of the prior art, which can meet the requirements of industrial production while also overcoming the above two problems. Not only is the method simple and the preparation cycle short, but only one formula is needed to solve all the above problems. This has a great promoting effect on reducing energy consumption, reducing the amount of high-cost reagents, scientifically improving the treatment capacity of fluorine-containing wastewater, and further reducing the cost of fluorine-containing wastewater treatment.

[0009] In order to achieve the above object, the present invention adopts the following technical solution:

[0010] A reagent suitable for treating fluorine-containing wastewater in the semiconductor industry, comprising the following components by weight percentage:

[0011] Calcium compounds: 1%-50%;

[0012] Tripolyphosphate: 0.1%-10%;

[0013] Polyaluminium chloride: 1%-10%;

[0014] Phosphate: 1%-7%;

[0015] Hexamethaphosphate: 0.1%-10%;

[0016] The balance is water.

[0017] As an improvement of the agent suitable for treating fluorine-containing wastewater in the semiconductor industry of the present invention, the calcium compound is CaO and / or calcium hydroxide.

[0018] As an improvement of the agent suitable for treating fluoride-containing wastewater in the semiconductor industry of the present invention, the tripolyphosphate is sodium tripolyphosphate and / or potassium tripolyphosphate.

[0019] As an improvement of the agent suitable for treating fluorine-containing wastewater in the semiconductor industry of the present invention, the phosphate is sodium phosphate and / or potassium phosphate.

[0020] As an improvement of the agent suitable for treating fluorine-containing wastewater in the semiconductor industry of the present invention, the hexametaphosphate is sodium hexametaphosphate and / or potassium hexametaphosphate.

[0021] Compared with the prior art, the present invention adopts a new inorganic dispersion suspension formula to prepare the suspension liquid on the basis of fully considering the advantages and disadvantages of using lime and calcium chloride. This formula can make calcium oxide and / or calcium hydroxide evenly distributed in the aqueous solution in the form of extremely small particles without precipitation in the fluorine-containing wastewater treatment system without changing the existing process system, thereby completely solving the precipitation and scaling problems caused by the use of lime and calcium chloride. Since calcium oxide and / or calcium hydroxide are used, the use of sodium hydroxide in the process is avoided, which greatly reduces the cost of the agent from the perspective of operation. Moreover, the raw materials used in the preparation method disclosed in the present invention are simple and easy to obtain, the cost is extremely low, and it is very easy to promote.

[0022] In short, the invention has a simple formula, convenient operation, and can completely solve the problems of high cost, precipitation and scaling.

[0023] Among them, gelatin and other organic substances are not used in the formula of the present invention, so that the whole formula is inorganic, hexamethylmetaphosphate is easy to dissolve, and the solubility of the solution is greatly improved, thereby greatly shortening the preparation time; the polyaluminium chloride of the above ratio is a flocculent after dissolution, which is more conducive to the stability of the suspension, and it is the key to the medicine made by the whole formula to be a suspended liquid. The reasonable preparation of the above substances avoids the increase of processing costs and management difficulties of traditional medicines; and the formula raw materials are simple and easy to obtain, low in price, which reduces energy consumption and equipment maintenance costs, and improves the treatment capacity of fluoride-containing wastewater. In short, the advantages of the present invention are: simple and easy to obtain raw materials, low price, simple method, short preparation cycle, stable quality, significant effect and easy to promote.

[0024] As an improvement of the agent suitable for treating fluorine-containing wastewater in the semiconductor industry, the preparation method thereof comprises at least the following steps:

[0025] The first step is to prepare the ingredients: prepare the raw materials according to the weight ratio;

[0026] The second step is mixing: all the raw materials are mixed evenly according to the proportion, and water is added at the same time to just dissolve all the materials;

[0027] The third step is dilution: add the remaining water to the mixed materials and dilute them to the concentration required on site.

[0028] That is, in the method of the present invention, a new type of inorganic dispersion suspension formula is used to prepare the suspension liquid, and the liquid of the present invention is prepared through the steps of material preparation, mixing and dilution. Calcium oxide and / or calcium hydroxide are uniformly distributed in the aqueous solution in the form of extremely small particles without precipitation, thereby completely solving the problems of increased cost, precipitation, scaling, etc. caused by the use of lime and calcium chloride. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1It is a physical picture of the medicine just prepared in Example 1 and Comparative Example 1 of the present invention.

[0030] Figure 2 It is a physical picture of the medicine of Example 1 and Comparative Example 1 of the present invention after being left to stand for two weeks. DETAILED DESCRIPTION

[0031] The following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0032] Example 1

[0033] On October 6-20, 2022, a suspension was prepared according to the method and steps of the present invention.

[0034] Specifically, in the first step, take 20% CaO, 0.2% sodium tripolyphosphate, 3% polyaluminium chloride, 3% sodium phosphate, 0.1% sodium hexametaphosphate, and the balance water.

[0035] Step 2: Prepare the raw materials: prepare the raw materials according to the weight ratio of the above formula;

[0036] Step 3: Mixing: Mix all the raw materials evenly according to the above proportions, and add water at the same time to dissolve all the materials; Concentration dilution: Add clean water to dilute the dissolved materials to a concentration of 30%. The total preparation time is about 15 minutes.

[0037] The prepared pharmaceutical preparations are Figure 1 As shown in the right figure, it can be seen that it is a uniformly dispersed suspension liquid. After standing for two weeks, the material is still evenly distributed, the solution has very little stratification, and no precipitation occurs. Figure 2 As shown in the right figure.

[0038] Comparative Example 1

[0039] Take 30% CaO and add it to 70% water to get traditional lime water, which can be seen to have begun to precipitate. Figure 1 As shown in the left figure, after standing for two weeks, it can be seen that the sedimentation and stratification are very obvious, such as Figure 2 As shown in the right figure.

[0040] Example 2

[0041] From October 10 to 24, 2022, a suspension was prepared according to the method and steps of the present invention.

[0042] Specifically, in the first step, take 20% CaO, 0.2% potassium tripolyphosphate, 3% polyaluminium chloride, 3% potassium phosphate, 0.1% potassium hexametaphosphate, and the balance water.

[0043] Step 2: Prepare the raw materials: prepare the raw materials according to the weight ratio of the above formula;

[0044] Step 3: Mixing: Mix all the raw materials evenly according to the above proportions, and add water at the same time to dissolve all the materials; Concentration dilution: Add clean water to dilute the dissolved materials to a concentration of 30%. The total preparation time is about 15 minutes.

[0045] After standing for two weeks, the material was still evenly distributed, the solution showed very little stratification, and no precipitation occurred.

[0046] Example 3

[0047] From October 12 to 26, 2022, a suspension was prepared according to the method and steps of the present invention.

[0048] Specifically, in the first step, take 30% CaO, 0.5% potassium tripolyphosphate, 5% polyaluminium chloride, 5% potassium phosphate, 0.5% potassium hexametaphosphate, and the balance water.

[0049] Step 2: Prepare the raw materials: prepare the raw materials according to the weight ratio of the above formula;

[0050] Step 3: Mixing: Mix all the raw materials evenly according to the above proportions, and add water at the same time to dissolve all the materials; Concentration dilution: Add clean water to dilute the dissolved materials to a concentration of 30%. The total preparation time is about 15 minutes.

[0051] After standing for two weeks, the material was still evenly distributed, the solution showed very little stratification, and no precipitation occurred.

[0052] Example 4

[0053] From October 12 to 26, 2022, a suspension was prepared according to the method and steps of the present invention.

[0054] Specifically, in the first step, take 30% CaO, 0.5% sodium tripolyphosphate, 5% polyaluminium chloride, 5% sodium phosphate, 0.5% sodium hexametaphosphate, and the balance water.

[0055] Step 2: Prepare the raw materials: prepare the raw materials according to the weight ratio of the above formula;

[0056] Step 3: Mixing: Mix all the raw materials evenly according to the above proportions, and add water at the same time to dissolve all the materials; Concentration dilution: Add clean water to dilute the dissolved materials to a concentration of 30%. The total preparation time is about 15 minutes.

[0057] After standing for two weeks, the material was still evenly distributed, the solution showed very little stratification, and no precipitation occurred.

[0058] Example 5

[0059] From October 14 to 28, 2022, a suspension was prepared according to the method and steps of the present invention.

[0060] Specifically, in the first step, take 40% CaO, 1% sodium tripolyphosphate, 4% polyaluminium chloride, 4% sodium phosphate, 3% sodium hexametaphosphate, and the balance water.

[0061] Step 2: Prepare the raw materials: prepare the raw materials according to the weight ratio of the above formula;

[0062] Step 3: Mixing: Mix all the raw materials evenly according to the above proportions, and add water at the same time to dissolve all the materials; Concentration dilution: Add clean water to dilute the dissolved materials to a concentration of 30%. The total preparation time is about 15 minutes.

[0063] After standing for two weeks, the material was still evenly distributed, the solution showed very little stratification, and no precipitation occurred.

[0064] Example 6

[0065] From October 14 to 28, 2022, a suspension was prepared according to the method and steps of the present invention.

[0066] Specifically, in the first step, take 35% CaO, 5% sodium tripolyphosphate, 8% polyaluminium chloride, 7% sodium phosphate, 5% sodium hexametaphosphate, and the balance water.

[0067] Step 2: Prepare the raw materials: prepare the raw materials according to the weight ratio of the above formula;

[0068] Step 3: Mixing: Mix all the raw materials evenly according to the above proportions, and add water at the same time to dissolve all the materials; Concentration dilution: Add clean water to dilute the dissolved materials to a concentration of 30%. The total preparation time is about 15 minutes.

[0069] After standing for two weeks, the material was still evenly distributed, the solution showed very little stratification, and no precipitation occurred.

[0070] Example 7

[0071] From October 14 to 28, 2022, a suspension was prepared according to the method and steps of the present invention.

[0072] Specifically, in the first step, take 25% calcium hydroxide, 8% sodium tripolyphosphate, 6% polyaluminium chloride, 2% sodium phosphate, 6% sodium hexametaphosphate, and the balance water.

[0073] Step 2: Prepare the raw materials: prepare the raw materials according to the weight ratio of the above formula;

[0074] Step 3: Mixing: Mix all the raw materials evenly according to the above proportions, and add water at the same time to dissolve all the materials; Concentration dilution: Add clean water to dilute the dissolved materials to a concentration of 30%. The total preparation time is about 15 minutes.

[0075] After standing for two weeks, the material was still evenly distributed, the solution showed very little stratification, and no precipitation occurred.

[0076] Example 8

[0077] From October 16 to 30, 2022, a suspension was prepared according to the method and steps of the present invention.

[0078] Specifically, in the first step, take 45% calcium hydroxide, 2% sodium tripolyphosphate, 4% polyaluminium chloride, 3.5% sodium phosphate, 3.5% sodium hexametaphosphate, and the balance water.

[0079] Step 2: Prepare the raw materials: prepare the raw materials according to the weight ratio of the above formula;

[0080] Step 3: Mixing: Mix all the raw materials evenly according to the above proportions, and add water at the same time to dissolve all the materials; Concentration dilution: Add clean water to dilute the dissolved materials to a concentration of 30%. The total preparation time is about 15 minutes.

[0081] After standing for two weeks, the material was still evenly distributed, the solution showed very little stratification, and no precipitation occurred.

[0082] Example 9

[0083] From October 16 to 30, 2022, a suspension was prepared according to the method and steps of the present invention.

[0084] Specifically, in the first step, take 15% calcium hydroxide, 3.5% sodium tripolyphosphate, 4.5% polyaluminium chloride, 2.5% sodium phosphate, 2.5% sodium hexametaphosphate, and the balance water.

[0085] Step 2: Prepare the raw materials: prepare the raw materials according to the weight ratio of the above formula;

[0086] Step 3: Mixing: Mix all the raw materials evenly according to the above proportions, and add water at the same time to dissolve all the materials; Concentration dilution: Add clean water to dilute the dissolved materials to a concentration of 30%. The total preparation time is about 15 minutes.

[0087] After standing for two weeks, the material was still evenly distributed, the solution showed very little stratification, and no precipitation occurred.

[0088] Example 10

[0089] From October 17 to 31, 2022, a suspension was prepared according to the method and steps of the present invention.

[0090] Specifically, in the first step, take 35% calcium hydroxide, 5.5% sodium tripolyphosphate, 5.5% polyaluminium chloride, 4.5% sodium phosphate, 3.5% sodium hexametaphosphate, and the balance water.

[0091] Step 2: Prepare the raw materials: prepare the raw materials according to the weight ratio of the above formula;

[0092] Step 3: Mixing: Mix all the raw materials evenly according to the above proportions, and add water at the same time to dissolve all the materials; Concentration dilution: Add clean water to dilute the dissolved materials to a concentration of 30%. The total preparation time is about 15 minutes.

[0093] After standing for two weeks, the material was still evenly distributed, the solution showed very little stratification, and no precipitation occurred.

[0094] According to the disclosure and teaching of the above description, those skilled in the art to which the present invention belongs may also make changes and modifications to the above embodiments. Therefore, the present invention is not limited to the specific embodiments disclosed and described above, and some modifications and changes to the present invention should also fall within the scope of protection of the claims of the present invention. In addition, although some specific terms are used in this specification, these terms are only for the convenience of description and do not constitute any limitation to the present invention.

Claims

1. A reagent suitable for treating fluorine-containing wastewater in the semiconductor industry, characterized in that: In terms of weight percentage, it contains the following components: Calcium compounds: 1%-50%; Tripolyphosphate: 0.1%-10%; Polyaluminium chloride: 1%-10%; Phosphate: 1%-7%; Hexamethaphosphate: 0.1%-10%; The balance is water; The preparation method thereof comprises at least the following steps: The first step is to prepare the ingredients: prepare the raw materials according to the weight ratio; The second step is mixing: all the raw materials are mixed evenly according to the proportion, and water is added at the same time to just dissolve all the materials; The third step is dilution: add the remaining water to the mixed materials and dilute them to the concentration required on site.

2. The agent for treating fluorine-containing wastewater in the semiconductor industry according to claim 1, characterized in that: The calcium compound is CaO and / or calcium hydroxide.

3. The agent for treating fluorine-containing wastewater in the semiconductor industry according to claim 1, characterized in that: The tripolyphosphate is sodium tripolyphosphate and / or potassium tripolyphosphate.

4. The agent for treating fluorine-containing wastewater in the semiconductor industry according to claim 1, characterized in that: The phosphate is sodium phosphate and / or potassium phosphate.

5. The agent for treating fluorine-containing wastewater in the semiconductor industry according to claim 1, characterized in that: The hexametaphosphate is sodium hexametaphosphate and / or potassium hexametaphosphate.