A continuous crystallization method for cannabidiol
Through continuous crystallization method and solid content gradient control, the problem of difficulty in improving yield and purity in the purification process of cannabidiol is solved, and high efficiency, high yield and high purity production of cannabidiol crystals is achieved, which is suitable for industrial applications.
Patent Information
- Application Number
- CN202310386520.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-12
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2043-04-12
AI Technical Summary
In the existing cannabidiol extraction methods, the crystallization purification process is inefficient and it is difficult to simultaneously improve the yield and purity of cannabidiol, especially when impurities of similar properties exist.
The continuous crystallization method is adopted to concentrate the crystallization liquid during the first, second and third-level crystallization process, control the solid content within a specific gradient range, combine non-polar solvents and optimize the cooling and crystallization temperature gradient to achieve cannabidiol crystals high yield and high purity.
It significantly improves the yield and purity of cannabidiol crystals, with the highest yield up to 85%, and the crystal purity can reach more than 99%, making it suitable for large-scale industrial production.
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of crystallization purification, and in particular to a continuous crystallization method of cannabidiol. Background Art
[0002] Cannabidiol (CBD) is a pure natural substance extracted from industrial hemp, which can inhibit brain excitement and the occurrence of epilepsy; it has analgesic, analgesic and anti-inflammatory effects; it has anti-proliferation and pro-apoptosis effects, and interferes with tumor angiogenesis and cancer cell migration, adhesion, invasion and metastasis; it can reduce the duration of anxiety and help sleep, and is widely used in the medicinal field. The main ingredients in industrial hemp flowers and leaves include tetrahydrocannabinol (THC), cannabidiol (CBD), cannabinol (CBN), cannabidivarin (CBDV), cannabidiolic acid (CBDA) and tetrahydrocannabinolic acid (THCA), and the properties of these substances are relatively similar. How to effectively separate cannabidiol from other components in hemp and improve the yield and purity of cannabidiol are the key to the development of the cannabidiol industry.
[0003] At present, the commonly used cannabidiol extraction method is mainly an organic solvent extraction method, which uses ethanol to extract the raw material and use it as a chromatography elution medium, which not only improves the purity of cannabidiol in the finished product, but also removes a certain amount of psychotoxic component tetrahydrocannabinol, thereby improving the safety of the product. However, the content of cannabidiol in the extract obtained is still low, and further separation and purification is required. At present, there are few studies on the crystallization and purification of cannabidiol, and the existing methods mostly use a single solvent to repeat multiple crystallizations, which is time-consuming and laborious. There is currently no report on the crystallization of cannabidiol using a continuous crystallization method. Summary of the invention
[0004] The present invention provides a continuous crystallization method of cannabidiol.
[0005] In the existing continuous crystallization method, if cooling crystallization is adopted, since the filtrate of crystallization at each level should be in a supersaturated state in theory, the influence of the solid content of crystallization at each level on the crystallization effect is usually seldom paid attention to. The present invention finds that in the continuous crystallization process of cannabidiol, in the subsequent cooling crystallization processes such as secondary and tertiary, the solid content of the crystallization feed liquid will have a significant impact on the purity and yield of cannabidiol crystals, and, because the hemp raw material contains tetrahydrocannabinol (THC), cannabinol (CBN), cannabidiol (CBDV), cannabidiol acid (CBDA) and tetrahydrocannabinol acid (THCA) and other impurity components similar to cannabidiol in nature, it is not simply to increase the solid content of crystallization at each level to simultaneously achieve the high yield and high purity of cannabidiol crystals, in many cases, increasing the solid content can improve the crystallization yield of cannabidiol, but its crystal purity is significantly reduced. In further research, the present invention concentrates the crystallization liquid at each level to control the solid content at a certain gradient level, thereby achieving a significant improvement in the purity of the crystals while ensuring a high yield of cannabidiol crystals.
[0006] Specifically, the present invention provides the following technical solutions:
[0007] The present invention provides a continuous crystallization method of cannabidiol, the method comprising: sequentially subjecting a crystallization raw material containing cannabidiol to primary crystallization, secondary crystallization and tertiary crystallization;
[0008] The secondary crystallization and the tertiary crystallization include: concentrating the filtrate and the crystal washing liquid obtained from the previous crystallization and then cooling and crystallizing them,
[0009] Among them, the solid content concentrated in the tertiary crystallization is increased by 5% to 10% compared with the solid content concentrated in the secondary crystallization.
[0010] The present invention finds that in the continuous crystallization process of cooling crystallization, controlling the solid content of the tertiary crystallization and the secondary crystallization within the above-mentioned lifting gradient range is very beneficial for simultaneously improving the yield of continuous crystallization and the purity of the cannabidiol crystals obtained.
[0011] The above-mentioned percentage increase in solid content is the ratio of the difference between the solid content concentrated in the tertiary crystallization and the solid content concentrated in the secondary crystallization to the solid content concentrated in the secondary crystallization.
[0012] Further preferably, the solid content concentrated in the tertiary crystallization is increased by 5% to 8% compared with the solid content concentrated in the secondary crystallization.
[0013] In the above method, the filtrate refers to the liquid portion obtained by solid-liquid separation of crystals and liquid after the cooling crystallization is completed, and the crystal washing liquid refers to the liquid portion of the crystal washing flow recovered in the process of washing the crystals with a solvent.
[0014] In the above method, the cannabidiol crystals are separated in time after each level of crystallization, so that the crystal nucleation and production are separated, and the number, particle size and particle size distribution of the crystals are effectively controlled.
[0015] Specifically, in the secondary crystallization, the solid content is concentrated to 50-59%. In the tertiary crystallization, the solid content is concentrated to 54-62%.
[0016] Under the condition of satisfying the above-mentioned solid content increase gradient, controlling the solid content of secondary crystallization and tertiary crystallization within the above-mentioned range is more conducive to simultaneously ensuring the yield of continuous crystallization and the purity of the cannabidiol crystals obtained.
[0017] In the above-mentioned continuous crystallization method, the crystallization raw material containing cannabidiol is mixed with the crystallization solvent and filtered before primary crystallization, wherein the mass volume ratio of the crystallization raw material containing cannabidiol and the crystallization solvent (kg:L) is 1:1.35~1:1.5.
[0018] In the primary crystallization process, controlling the material-liquid ratio within the above range is more conducive to improving the crystallization yield and the purity of the cannabidiol crystals obtained.
[0019] On the basis of the above-mentioned solid content control, the present invention further significantly improves the yield of continuous crystallization and the purity of the cannabidiol crystals obtained by optimizing the temperature gradient setting of cooling crystallization in each stage of crystallization.
[0020] Preferably, in the primary crystallization, the starting temperature of the cooling crystallization is 20-24°C, and the end temperature of the cooling crystallization is 14-18°C;
[0021] In the secondary crystallization, the starting temperature of the cooling crystallization is 14°C to 18°C; the end temperature of the cooling crystallization is -5°C to -2°C;
[0022] In the three-stage crystallization, the starting temperature of the cooling crystallization is -5°C to -2°C; the terminal temperature of the cooling crystallization is -18°C to -22°C.
[0023] Controlling the starting and ending temperatures of each stage of cooling crystallization within the above range is more conducive to simultaneously improving the yield of continuous crystallization and the purity of the cannabidiol crystals obtained.
[0024] Preferably, the cooling rate of the cooling crystallization is 1°C / h to 6°C / h. The cooling rates of the above-mentioned cooling crystallization at each level can be controlled within the range of 1°C / h to 6°C / h.
[0025] Further preferably, the cooling rate of the cooling crystallization is 2°C / h~6°C / h.
[0026] In the above continuous crystallization method, the crystallization solvent is a non-polar solvent.
[0027] Preferably, the non-polar solvent is one or more selected from n-hexane, n-heptane and petroleum ether.
[0028] More preferably, the non-polar solvent is n-hexane.
[0029] The present invention finds that, compared with polar solvents such as alcohols or mixed crystallization solvents consisting of non-polar and polar solvents, the use of non-polar solvents as crystallization solvents is more conducive to improving the crystallization yield and the purity of the cannabidiol crystals obtained in the continuous crystallization method.
[0030] In the above-mentioned continuous crystallization method, the cooling crystallization includes: adding seed crystals under the starting temperature condition of cooling crystallization, growing the crystals for 0.5 to 2 hours, and then starting to cool down to the end temperature.
[0031] If the temperature of the crystallization liquid is not within the starting temperature range of the cooling crystallization, the liquid is rapidly heated or cooled to the starting temperature of the cooling crystallization. After adding the seed crystal, the crystal is first grown and then cooled at the above cooling rate until the terminal temperature is reached.
[0032] Preferably, the crystal growing time is 1 to 2 hours.
[0033] Preferably, the added amount (mass) of the seed crystals is 0.1% to 2% of the mass of the crystalline raw material containing cannabidiol, and more preferably 1% to 2%.
[0034] In the present invention, the crystalline raw material containing cannabidiol is preferably cannabidiol extract. Cannabidiol extract refers to an extract obtained by extraction, separation and purification using industrial hemp as raw material.
[0035] Preferably, the content of cannabidiol in the crystalline raw material containing cannabidiol is greater than 70%, more preferably greater than 80%.
[0036] In the above continuous crystallization method, after the cooling crystallization is completed, the obtained crystals are washed; the solvent used for washing the crystals is a non-polar solvent.
[0037] Preferably, the non-polar solvent is one or more selected from n-hexane, n-heptane and petroleum ether.
[0038] Preferably, the temperature of the solvent used for washing the crystals is 0°C to -5°C.
[0039] After the cooling crystallization is completed, the crystals and the feed liquid are separated into solid and liquid, and the separated crystals are washed. The optional solid-liquid separation method includes centrifugal separation.
[0040] In some embodiments of the present invention, the continuous crystallization method comprises the following steps:
[0041] (1) dissolving cannabidiol extract in a non-polar solvent at a solid-liquid ratio of 1:1.35 to 1:1.5, and filtering to obtain a crystallization liquid;
[0042] (2) Add the crystallization liquid of step (1) to the first-stage crystallizer, raise or lower the temperature to 20-24°C, add seed crystals, and grow the crystals for 1-2 hours; then lower the temperature to 14-18°C at a rate of 1°C / h-6°C / h, filter with a centrifuge, wash the crystals with a non-polar solvent, add the filtrate and the washing liquid to the second-stage crystallizer, concentrate to a solid content of 50-59%, control the temperature of the second-stage crystallizer to 14-18 ...°C / h-6°C / h is cooled to -2~-5℃, filtered by a centrifuge, and then washed with a non-polar solvent. The filtrate and the crystal washing liquid are added to the third-stage crystallizer and concentrated to a solid content of 54~62%. The temperature of the third-stage crystallizer is controlled at -2~-5℃, seed crystals are added, and the crystals are cultured for 1~2h; then the temperature is cooled to -18~-22℃, filtered by a centrifuge, and then washed with a non-polar solvent. Among them, the concentrated solid content in the tertiary crystallization is increased by 5%-10% compared with the concentrated solid content in the secondary crystallization.
[0043] In the above method, the primary crystallizer, the secondary crystallizer and the tertiary crystallizer are connected in series. Stirring is performed during the cooling crystallization process, and the rotation speed is 45-90r / min.
[0044] The present invention also provides cannabidiol crystals prepared by the continuous crystallization method of cannabidiol described above.
[0045] The above-mentioned cannabidiol crystals include cannabidiol crystals obtained by primary crystallization, the cannabidiol content of which can reach more than 99%, cannabidiol crystals obtained by secondary crystallization, the cannabidiol content of which can reach more than 98%, and cannabidiol crystals obtained by tertiary crystallization, the cannabidiol content of which can reach more than 90%.
[0046] The beneficial effects of the present invention are as follows: the continuous crystallization method provided by the present invention significantly improves the yield and purity of cannabidiol crystals, the total yield of cannabidiol can reach up to 85% and the crystal purity is high, wherein the cannabidiol content of the cannabidiol crystals obtained by the primary crystallization can reach more than 99%, the cannabidiol content of the cannabidiol crystals obtained by the secondary crystallization can reach more than 98%, and the cannabidiol content of the cannabidiol crystals obtained by the tertiary crystallization can reach more than 90%, and cannabidiol crystals of different qualities can be obtained to meet different needs, thereby realizing the continuous, efficient, high-content and high-yield production of cannabidiol crystals, which is suitable for industrial large-scale production. DETAILED DESCRIPTION
[0047] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be described clearly and completely below. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Example 1
[0048] This embodiment provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0049] Take 20kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 27L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 24°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1h, cool it to 14°C at 2°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0050] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after the crystals are separated by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 50%, the temperature is raised or lowered to 14°C, and then 1% of the mass of the extract is added as seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -2°C at 2°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0051] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after filtering and separating the crystals by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 54%, the temperature is raised or lowered to -2°C, 1% of the mass of the extract is added with seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -20°C at 2°C / h, and the crystals and the filtrate are separated by centrifuge filtering.
[0052] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0053] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this embodiment were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 99.48%, and the cannabidiol yield was 45%. The cannabidiol content in the crystals obtained by the second stage crystallization was 98.56%, and the cannabidiol yield was 18%. The cannabidiol content in the crystals obtained by the third stage crystallization was 92.40%, and the cannabidiol yield was 5%. Example 2
[0054] This embodiment provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0055] Take 20kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 27L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 24°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1h, cool it to 14°C at 2°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0056] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after separating the crystals by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 52%, the temperature is raised or lowered to 14°C, and then 1% of the mass of the extract is added as seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -2°C at 2°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0057] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after filtering and separating the crystals by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 56%, the temperature is raised or lowered to -2°C, 1% of the mass of the extract is added with seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -20°C at 2°C / h, and the crystals and the filtrate are separated by centrifuge filtering.
[0058] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0059] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this embodiment were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 99.53%, and the cannabidiol yield was 45%. The cannabidiol content in the crystals obtained by the second stage crystallization was 98.61%, and the cannabidiol yield was 21%. The cannabidiol content in the crystals obtained by the third stage crystallization was 91.80%, and the cannabidiol yield was 7%. Example 3
[0060] This embodiment provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0061] Take 20kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 27L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 24°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1h, cool it to 14°C at 2°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0062] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after the crystals are separated by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 55%, the temperature is raised or lowered to 14°C, and then 1% of the mass of the extract is added as seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -2°C at 2°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0063] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after the crystals are separated by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, and the mother liquor and the crystal washing liquid are concentrated to a solid content of 58%. The temperature is raised or lowered to -2°C, and 1% of the extract mass of seed crystals is added, and the crystals are grown for 1 hour, and the temperature is lowered to -20°C at 2°C / h, and the crystals and filtrate are separated by centrifuge filtration.
[0064] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0065] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this embodiment were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 99.46%, and the cannabidiol yield was 45%. The cannabidiol content in the crystals obtained by the second stage crystallization was 98.56%, and the cannabidiol yield was 23%. The cannabidiol content in the crystals obtained by the third stage crystallization was 91.65%, and the cannabidiol yield was 9%. Example 4
[0066] This embodiment provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0067] Take 20kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 27L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 24°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1h, cool it to 14°C at 2°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0068] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after separating the crystals by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 57%, the temperature is raised or lowered to 14°C, and then 1% of the mass of the extract is added as seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -2°C at 2°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0069] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after filtering and separating the crystals by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 60%, the temperature is raised or lowered to -2°C, and seed crystals of 1% by weight of the extract are added, the crystals are grown for 1 hour, the temperature is lowered to -20°C at 2°C / h, and the crystals and the filtrate are separated by centrifuge filtering.
[0070] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0071] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this embodiment were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 99.49%, and the cannabidiol yield was 45%. The cannabidiol content in the crystals obtained by the second stage crystallization was 98.34%, and the cannabidiol yield was 25%. The cannabidiol content in the crystals obtained by the third stage crystallization was 90%, and the cannabidiol yield was 10%. Example 5
[0072] This embodiment provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0073] Take 20kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 27L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 24°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1h, cool it to 14°C at 2°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0074] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after separating the crystals by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 59%, the temperature is raised or lowered to 14°C, and then 1% of the mass of the extract is added as seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -2°C at 2°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0075] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after filtering and separating the crystals by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 62%, the temperature is raised or lowered to -2°C, 1% of the mass of the extract is added with seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -20°C at 2°C / h, and the crystals and the filtrate are separated by centrifuge filtering.
[0076] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0077] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this embodiment were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 99.32%, and the cannabidiol yield was 45%. The cannabidiol content in the crystals obtained by the second stage crystallization was 98.76%, and the cannabidiol yield was 24%. The cannabidiol content in the crystals obtained by the third stage crystallization was 90.20%, and the cannabidiol yield was 12%. Example 6
[0078] This embodiment provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0079] Take 20kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 30L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 24°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1h, cool it to 14°C at 2°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0080] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after separating the crystals by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 57%, the temperature is raised or lowered to 14°C, and then 1% of the mass of the extract seed is added, the crystals are grown for 1 hour, the temperature is lowered to -2°C at 2°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0081] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after filtering and separating the crystals by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 60%, the temperature is raised or lowered to -2°C, and seed crystals of 1% by weight of the extract are added, the crystals are grown for 1 hour, the temperature is lowered to -20°C at 2°C / h, and the crystals and the filtrate are separated by centrifuge filtering.
[0082] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0083] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this embodiment were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 99.58%, and the cannabidiol yield was 39%. The cannabidiol content in the crystals obtained by the second stage crystallization was 99.16%, and the cannabidiol yield was 20%. The cannabidiol content in the crystals obtained by the third stage crystallization was 91.30%, and the cannabidiol yield was 12%. Example 7
[0084] This embodiment provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0085] Take 20 kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 27 L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 24°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1 hour, cool to 14°C at 6°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0086] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after separating the crystals by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 57%, the temperature is raised or lowered to 14°C, and then 1% of the mass of the extract is added as seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -2°C at 6°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0087] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after filtering and separating the crystals by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 60%, the temperature is raised or lowered to -2°C, 1% of the mass of the extract is added with seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -20°C at 6°C / h, and the crystals and the filtrate are separated by centrifuge filtering.
[0088] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0089] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this embodiment were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 99.28%, and the cannabidiol yield was 45%. The cannabidiol content in the crystals obtained by the second stage crystallization was 98.06%, and the cannabidiol yield was 23%. The cannabidiol content in the crystals obtained by the third stage crystallization was 90.70%, and the cannabidiol yield was 15%. Example 8
[0090] This embodiment provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0091] Take 20 kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 27 L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 20°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1 hour, cool it to 18°C at 6°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0092] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after separating the crystals by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 57%, the temperature is raised or lowered to 18°C, and then 1% of the mass of the extract is added as seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -5°C at 6°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0093] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after filtering and separating the crystals by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 60%, the temperature is raised or lowered to -5°C, 1% of the mass of the extract is added with seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -22°C at 6°C / h, and the crystals and the filtrate are separated by centrifuge filtering.
[0094] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0095] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this embodiment were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 99.58%, and the cannabidiol yield was 38%. The cannabidiol content in the crystals obtained by the second stage crystallization was 97.56%, and the cannabidiol yield was 33%. The cannabidiol content in the crystals obtained by the third stage crystallization was 88.70%, and the cannabidiol yield was 10%. Comparative Example 1
[0096] This comparative example provides a method for crystallizing cannabidiol, and the steps are as follows:
[0097] Take 20 kg of cannabidiol extract (containing 80% cannabidiol), heat the extract until it is fluid, pour it into 27 L of n-hexane solvent, stir, and then filter. The filtrate obtained by cooling and crystallizing, with a starting temperature of 24 ° C and a cooling rate of 2 ° C / h. Cool to -2 ° C, filter and separate the crystals and filtrate using a centrifuge, wash the crystals with -2 ° C n-hexane solvent, and dry.
[0098] The purity and yield of the crystals obtained by the cannabidiol crystallization method of this comparative example were tested and calculated, and the results showed that the content of cannabidiol in the obtained crystals was 98.50%, and the yield of cannabidiol was 65%. Comparative Example 2
[0099] This comparative example provides a method for crystallizing cannabidiol, and the steps are as follows:
[0100] Take 20 kg of cannabidiol extract (containing 80% cannabidiol), heat the extract until it is fluid, pour it into 27 L of n-hexane solvent, stir, and then filter. The filtrate obtained by filtration begins to cool and crystallize. The starting temperature is 24 ° C, the cooling rate is 2 ° C / h, and it is cooled to -20 ° C. The crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2 ° C n-hexane solvent and dried.
[0101] The purity and yield of the crystals obtained by the cannabidiol crystallization method of this comparative example were tested and calculated, and the results showed that the cannabidiol content in the obtained crystals was 95.20%, and the cannabidiol yield was 75%. Comparative Example 3
[0102] This comparative example provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0103] Take 20kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 27L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 24°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1h, cool it to 14°C at 2°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0104] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after the crystals are separated by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 50%, the temperature is raised or lowered to 14°C, and then 1% of the mass of the extract is added as seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -2°C at 2°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0105] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after filtering and separating the crystals by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 62%, the temperature is raised or lowered to -2°C, 1% of the mass of the extract is added with seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -20°C at 2°C / h, and the crystals and the filtrate are separated by centrifuge filtering.
[0106] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0107] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this comparative example were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 99.48%, and the cannabidiol yield was 45%. The cannabidiol content in the crystals obtained by the second stage crystallization was 98.06%, and the cannabidiol yield was 18%. The cannabidiol content in the crystals obtained by the third stage crystallization was 87.20%, and the cannabidiol yield was 10%. Comparative Example 4
[0108] This comparative example provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0109] Take 20kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 27L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 24°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1h, cool it to 14°C at 2°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0110] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after the crystals are separated by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 50%, the temperature is raised or lowered to 14°C, and then 1% of the mass of the extract is added as seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -2°C at 2°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0111] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after filtering and separating the crystals by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 52%, the temperature is raised or lowered to -2°C, and seed crystals of 1% by weight of the extract are added, the crystals are grown for 1 hour, the temperature is lowered to -20°C at 2°C / h, and the crystals and the filtrate are separated by centrifuge filtering.
[0112] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0113] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this comparative example were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 99.48%, and the cannabidiol yield was 45%. The cannabidiol content in the crystals obtained by the second stage crystallization was 98.06%, and the cannabidiol yield was 18%. The cannabidiol content in the crystals obtained by the third stage crystallization was 92.10%, and the cannabidiol yield was 2%. Comparative Example 5
[0114] This comparative example provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0115] Take 20kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 27L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 24°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1h, cool it to 14°C at 2°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0116] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after separating the crystals by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 64%, the temperature is raised or lowered to 14°C, and then 1% of the mass of the extract is added as seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -2°C at 2°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0117] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after filtering and separating the crystals by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 68%, the temperature is raised or lowered to -2°C, and seed crystals of 1% by weight of the extract are added, the crystals are grown for 1 hour, the temperature is lowered to -20°C at 2°C / h, and the crystals and the filtrate are separated by centrifuge filtering.
[0118] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0119] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this comparative example were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 99.48%, and the cannabidiol yield was 45%. The cannabidiol content in the crystals obtained by the second stage crystallization was 97.50%, and the cannabidiol yield was 30%. The cannabidiol content in the crystals obtained by the third stage crystallization was 85.30%, and the cannabidiol yield was 5%. Comparative Example 6
[0120] This comparative example provides a continuous crystallization method of cannabidiol, and the steps are as follows:
[0121] Take 20 kg of cannabidiol extract (with a cannabidiol content of 80%), heat the extract until it is fluid, pour it into 27 L of n-hexane solvent, stir, and then filter. Place the filtrate obtained by filtration in a primary crystallizer, heat or cool it to 24°C to start cooling crystallization, add 1% of the extract mass of seed crystals, grow the crystals for 1 hour, cool it to 8°C at 2°C / h, filter and separate the crystals and the filtrate using a centrifuge, and wash the crystals with -2°C n-hexane solvent.
[0122] The mother liquor obtained from the first-stage crystallization (i.e., the filtrate obtained after the crystals are separated by centrifuge filtration in the first-stage crystallization) and the crystal washing liquid are added to the second-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 57%, the temperature is raised or lowered to 8°C, and then 1% of the mass of the extract is added as seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -8°C at 2°C / h, the crystals and the filtrate are separated by centrifuge filtration, and the crystals are washed with -2°C n-hexane solvent.
[0123] The mother liquor obtained from the secondary crystallization (i.e., the filtrate obtained after filtering and separating the crystals by centrifuge in the secondary crystallization) and the crystal washing liquid are added to the third-stage crystallizer, the mother liquor and the crystal washing liquid are concentrated to a solid content of 60%, the temperature is raised or lowered to -8°C, 1% of the mass of the extract is added with seed crystals, the crystals are grown for 1 hour, the temperature is lowered to -20°C at 2°C / h, and the crystals and the filtrate are separated by centrifuge filtering.
[0124] The crystals obtained from the first and second stage crystallizers are dried at 45°C. The crystals obtained from the third stage crystallizer can be incorporated into the next batch for crystallization, or can be used for other desired purposes after being dried at 45°C.
[0125] The purity and yield of the crystals obtained by the continuous crystallization method of cannabidiol in this comparative example were tested and calculated. The results showed that the cannabidiol content in the crystals obtained by the first stage crystallization was 98.78%, and the cannabidiol yield was 55%. The cannabidiol content in the crystals obtained by the second stage crystallization was 95.50%, and the cannabidiol yield was 20%. The cannabidiol content in the crystals obtained by the third stage crystallization was 83.30%, and the cannabidiol yield was 5%.
[0126] In summary, in the cannabidiol crystals obtained by the continuous crystallization method of each embodiment, the cannabidiol content of the crystals obtained by the primary crystallization can reach more than 99%, the cannabidiol content of the crystals obtained by the secondary crystallization can reach more than 98%, and the highest yield can reach 85%. It can be seen that the cannabidiol continuous crystallization method of the present invention can greatly improve the quality and yield of the crystals, and can obtain cannabidiol crystals of different specifications, meet different needs, and are suitable for industrial large-scale production.
[0127] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A continuous crystallization method for cannabidiol, characterized in that: The method comprises: sequentially subjecting a crystalline raw material containing cannabidiol to primary crystallization, secondary crystallization and tertiary crystallization; The secondary crystallization and the tertiary crystallization include: concentrating the filtrate and the crystal washing liquid obtained from the previous crystallization and then cooling and crystallizing them, Among them, the solid content concentrated in the tertiary crystallization is increased by 5% to 10% compared with the solid content concentrated in the secondary crystallization; In the secondary crystallization, the solid content is concentrated to 50-59%; In the tertiary crystallization, the solid content is concentrated to 54-62%.
2. The continuous crystallization method according to claim 1, characterized in that The crystallization raw material containing cannabidiol is mixed with the crystallization solvent and filtered before primary crystallization, wherein the mass volume ratio of the crystallization raw material containing cannabidiol to the crystallization solvent (kg:L) is 1:1.35 to 1:1.
5.
3. The continuous crystallization method according to claim 1 or 2, characterized in that In the primary crystallization, the starting temperature of the cooling crystallization is 20-24°C, and the end temperature of the cooling crystallization is 14-18°C; In the secondary crystallization, the starting temperature of the cooling crystallization is 14°C to 18°C; the end temperature of the cooling crystallization is -5°C to -2°C; In the three-stage crystallization, the starting temperature of the cooling crystallization is -5°C to -2°C; the terminal temperature of the cooling crystallization is -18°C to -22°C.
4. The continuous crystallization method according to claim 3, characterized in that The cooling rate of the cooling crystallization is 1°C / h to 6°C / h.
5. The continuous crystallization method according to claim 2, characterized in that The crystallization solvent is a non-polar solvent.
6. The continuous crystallization method according to claim 5, characterized in that The non-polar solvent is one or more selected from n-hexane, n-heptane and petroleum ether.
7. The continuous crystallization method according to any one of claims 1, 2, 4 to 6, characterized in that: The cooling crystallization comprises: adding seed crystals under the starting temperature condition of cooling crystallization, growing the crystals for 0.5 to 2 hours, and then starting to cool down until the end temperature.
8. The continuous crystallization method according to claim 7, characterized in that The amount of the seed crystal added is 0.1% to 2% of the mass of the crystalline raw material containing cannabidiol.
9. The continuous crystallization method according to any one of claims 1, 2, 4 to 6, and 8, characterized in that: After the cooling crystallization is completed, the obtained crystals are washed; The solvent used for washing the crystal is a non-polar solvent.
10. The continuous crystallization method according to claim 9, characterized in that The non-polar solvent is one or more selected from n-hexane, n-heptane and petroleum ether.
11. The continuous crystallization method according to claim 10, characterized in that The temperature of the solvent used for the crystal washing is 0°C to -5°C.
Citation Information
Patent Citations
Method of extracting high-purity cannabidiol from industrial hemp
CN110304994A
Preparation method of high-quality cannabidiol crystal
CN113402365A
Method for preparing ultra-pure cannabidiol monomer
CN114539032A
Method for purifying and extracting cannabidiol and application
CN115260005A
Continuous crystallization of cannabinoids in a stirred-tank reactor