A method for detecting lithium deposition in a battery, a detection device and an electric device thereof
By selecting the appropriate lithium-extraction detection rules based on the operating temperature of the battery, the false alarm problem of lithium-extraction detection of lithium-ion batteries under high charge state, low temperature and large charging rate is solved, and the accuracy and reliability of the detection are improved. This improves battery safety.
Patent Information
- Application Number
- CN202210126061.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-02-10
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2042-02-10
AI Technical Summary
Lithium-ion batteries are prone to lithium-ion extraction under high charge states, low temperatures and large charging ratios, resulting in a decrease in battery cell capacity, an increase in impedance and a decrease in safety. It is difficult to accurately detect the existing technology, resulting in a high false alarm rate.
By determining the operating temperature of the battery, according to the correspondence between the preset temperature and the lithium-extraction detection rules, find out suitable lithium-extraction detection rules and conduct inspections to improve accuracy and reliability.
The false alarm rate of lithium-ion detection is reduced, making the detection results more accurate and reliable, and improving the safety of lithium-ion batteries.
Smart Images

Figure CN116626509B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of batteries, and in particular to a method for detecting lithium deposition in batteries, a detection device thereof and electric equipment. Background Art
[0002] Lithium-ion batteries are prone to lithium plating under high charge state, low temperature and high charge rate. Lithium plating will lead to reduced cell capacity, increased impedance and reduced safety of lithium-ion batteries. Therefore, lithium plating detection of lithium-ion batteries is particularly important. Summary of the invention
[0003] The embodiment of the present invention provides a battery lithium deposition detection method, a detection device and an electric device thereof, which can select appropriate lithium deposition detection rules according to the operating temperature, thereby making the detection result more accurate and reliable and reducing false alarms.
[0004] In a first aspect, an embodiment of the present invention provides a method for detecting lithium deposition in a battery, comprising:
[0005] Determining the current operating temperature of the battery;
[0006] According to the correspondence between the preset temperature and the lithium precipitation detection rule, find out the lithium precipitation detection rule corresponding to the working temperature;
[0007] According to the found lithium deposition detection rule, detect whether lithium deposition occurs in the battery.
[0008] In a second aspect, an embodiment of the present invention provides a battery lithium deposition detection device, comprising:
[0009] A memory for storing program instructions;
[0010] The processor is used to call the program instructions stored in the memory and execute the above-mentioned detection method provided by the embodiment of the present invention according to the obtained program.
[0011] In a third aspect, an embodiment of the present invention provides an electric device, including: a battery, and the above-mentioned detection device provided by the embodiment of the present invention.
[0012] The beneficial effects of the present invention are as follows:
[0013] A battery lithium deposition detection method, a detection device and an electric device provided by an embodiment of the present invention can, when determining the current operating temperature of the battery, find the lithium deposition detection rule corresponding to the operating temperature according to the correspondence between the preset temperature and the lithium deposition detection rule, so that whether lithium deposition occurs in the battery can be detected according to the found lithium deposition detection rule; this process can select a suitable lithium deposition detection rule according to the operating temperature, avoid the problem of inaccurate detection results caused by a single lithium deposition detection rule, reduce the probability of false alarms, make the detection results more accurate and reliable, and thus improve the safety of lithium-ion batteries. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 A flow chart of a method for detecting lithium deposition in a battery provided in an embodiment of the present invention;
[0015] Figure 2 A current schematic diagram provided in an embodiment of the present invention;
[0016] Figure 3 Another current schematic diagram provided in an embodiment of the present invention;
[0017] Figure 4 It is another current schematic diagram provided in an embodiment of the present invention;
[0018] Figure 5 A voltage schematic diagram provided in an embodiment of the present invention;
[0019] Figure 6 Another voltage schematic diagram provided in an embodiment of the present invention;
[0020] Figure 7 This is another voltage schematic diagram provided in an embodiment of the present invention;
[0021] Figure 8 A discharge curve schematic diagram provided in an embodiment of the present invention;
[0022] Fig. 9 Another discharge curve schematic diagram provided in an embodiment of the present invention;
[0023] Fig.10 A schematic diagram of another discharge curve provided in an embodiment of the present invention;
[0024] Fig.11 A schematic structural diagram of a battery lithium deposition detection device provided in an embodiment of the present invention;
[0025] Fig.12 The figure is a schematic diagram of the structure of an electric device provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0026] The following will be combined with the accompanying drawings to describe in detail the specific implementation of a battery lithium deposition detection method, a detection device and an electric device provided by an embodiment of the present invention. It should be noted that the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0027] The embodiment of the present invention provides a method for detecting lithium deposition in a battery, such as Figure 1 As shown, it may include:
[0028] S101, determining the current operating temperature of the battery;
[0029] Among them, the operating temperature can be understood as: the temperature around the battery during the battery charging and discharging process;
[0030] Furthermore, the operating temperature may include: the ambient temperature, and the temperature of adjacent batteries.
[0031] Specifically, the method for determining the current operating temperature of the battery may include:
[0032] When a temperature sensor is provided on the busbar electrically connected to the battery, the operating temperature of the battery is collected through the temperature sensor.
[0033] Of course, in actual situations, the method for determining the current operating temperature of the battery is not limited to the above method, and any other method known to those skilled in the art for the above purpose may also be used, which is not limited here.
[0034] S102, according to the correspondence between the preset temperature and the lithium deposition detection rule, finding the lithium deposition detection rule corresponding to the working temperature;
[0035] Optionally, in the embodiment of the present invention, the corresponding relationship includes:
[0036] The first temperature range corresponds to the first lithium deposition detection rule, the second temperature range corresponds to the first lithium deposition detection rule and the second lithium deposition detection rule, and the third temperature range corresponds to the third lithium deposition detection rule and the fourth lithium deposition detection rule;
[0037] Wherein, the first lithium deposition detection rule includes: based on the current-time curve obtained during the constant voltage charging process of the battery, when the current does not decrease exponentially with the increase of time, and / or the differential result corresponding to the current does not increase exponentially with the increase of time, determining that lithium deposition occurs in the battery;
[0038] The second lithium deposition detection rule includes: based on the voltage-time curve obtained during the static process of the battery after the constant voltage charging process, when the curve shows a first platform and the charging rate used in the constant current charging process is greater than a preset rate, determining that lithium deposition occurs in the battery;
[0039] The third lithium deposition detection rule includes: based on the voltage-time curve obtained during the static process of the battery after the constant voltage charging process, the curve shows a first platform, determining that lithium deposition occurs in the battery;
[0040] The fourth lithium deposition detection rule includes: based on a discharge curve obtained by the battery in the initial stage of discharge, when the curve shows a second platform, determining that lithium deposition occurs in the battery.
[0041] Therefore, when the corresponding lithium deposition detection rule is found through the operating temperature, the detection can be performed according to the found lithium deposition detection rule, so that the most appropriate lithium deposition detection rule is used during the detection to improve the accuracy and reliability of the detection result.
[0042] Optionally, in an embodiment of the present invention, the first temperature range is greater than or equal to 40°C, the second temperature range is greater than or equal to 10°C and less than 40°C, and the third temperature range is less than 10°C.
[0043] That is to say, the first temperature range can be understood as high temperature, the second temperature range can be understood as normal temperature, and the third temperature range can be understood as low temperature.
[0044] The following are detailed descriptions of the four lithium plating detection rules.
[0045] 1. The first lithium deposition detection rule:
[0046] The constant voltage charging process is a depolarization process. As charging progresses, polarization decreases and the current can decrease exponentially. However, if lithium deposition occurs, the current in the constant voltage charging process will no longer decrease exponentially with the increase of time, the curve will bulge, and the differential curve of the current will change and no longer increase exponentially.
[0047] This is due to:
[0048] The elemental lithium precipitated on the surface of the negative electrode will lose electrons and generate lithium ions, which increases the speed of electron transfer. This is reflected in the current as an increase, resulting in a bulge on the current-time curve.
[0049] For example, Figure 2 As shown, Figure (a) is the current-time curve during constant voltage charging at different charging rates when the working temperature is -10°C, and Figure (b) is the differential result-time curve of the current during constant voltage charging at different charging rates when the working temperature is -10°C. It can be seen from the figure that:
[0050] When the operating temperature is -10℃, the curve corresponding to the charging ratio of 2C and the curve corresponding to the charging ratio of 4C in Figure (a) both have bulges (as shown in the dotted circle), that is, they are not decreasing exponentially. The curve corresponding to the charging ratio of 2C and the curve corresponding to the charging ratio of 4C in Figure (b) also do not increase exponentially. Therefore, it can be determined from Figures (a) and (b) that lithium deposition occurs in the battery when the charging ratios are 2C and 4C.
[0051] like Figure 3 As shown, Figure (a) is the current-time curve during constant voltage charging at different charging rates when the working temperature is 25°C, and Figure (b) is the differential result-time curve of the current during constant voltage charging at different charging rates when the working temperature is 25°C. It can be seen from the figure that:
[0052] When the operating temperature is 25℃, the curve corresponding to the charging rate of 1C and the curve corresponding to the charging rate of 2C in Figure (a) both have bulges (as shown in the dotted circle), that is, they are not decreasing exponentially. The curves corresponding to the charging rates of 1C, 2C, 4C and 5C in Figure (b) are not increasing exponentially. Therefore, it can be determined from Figures (a) and (b) that lithium deposition occurs in the battery when the charging rate is greater than 0.5C.
[0053] like Figure 4 As shown, Figure (a) is the current-time curve during constant voltage charging at different charging rates when the working temperature is 45°C, and Figure (b) is the differential result-time curve of the current during constant voltage charging at different charging rates when the working temperature is 45°C. It can be seen from the figure that:
[0054] When the operating temperature is 45℃, the curve corresponding to the charging rate of 4C in Figure (a) bulges (as shown in the dotted circle), that is, it does not decrease exponentially. The curve corresponding to the charging rate of 2C and the curve corresponding to the charging rate of 4C in Figure (b) also do not increase exponentially. Therefore, it can be determined from Figures (a) and (b) that lithium deposition occurs in the battery when the charging rate is greater than 1C.
[0055] Based on the above Figures 2 to 4 The results in Table 1 can be obtained, which shows the characteristics of the curves (including current-time curves and current differential results-time curves) at different temperatures and different charging rates, as well as the actual lithium plating results obtained after disassembling the battery cells in the lithium-ion battery.
[0056] Table 1
[0057]
[0058] From Table 1 we can see that:
[0059] At -10°C, there is a certain difference between the result obtained by analyzing the curve characteristics (recorded as result 1) and the actual disassembly result (recorded as result 2), that is, the consistency between result 1 and result 2 is not very good, so it can be determined that the sensitivity of the lithium precipitation detection method is not high at low temperatures;
[0060] At 25°C and 45°C, the consistency between result 1 and result 2 is good, so it can be determined that the lithium precipitation detection method has high sensitivity and high accuracy at room temperature and high temperature;
[0061] Therefore, the first lithium deposition detection rule is more suitable for lithium deposition detection at room temperature and high temperature.
[0062] 2. The second lithium deposition detection rule and the third lithium deposition detection rule:
[0063] During the static process after the constant voltage charging process is completed, if lithium deposition occurs, a first platform will appear in the voltage-time curve, and the greater the charging rate, the more obvious the first platform will be.
[0064] This is due to:
[0065] The elemental lithium precipitated on the surface of the negative electrode will lose electrons and generate lithium ions (i.e., lithium extraction reaction). These lithium ions can be embedded in the negative electrode, causing the potential of the negative electrode to decrease. When reflected in the voltage, the voltage increases during the static process, resulting in the first platform appearing on the voltage-time curve.
[0066] For example, Figure 5 As shown in the figure, this figure is the voltage-time curve during the static process after the constant voltage charging process at different charging rates when the working temperature is -10℃. It can be seen from the figure that:
[0067] When the operating temperature is -10℃, the curves corresponding to the charging rates of 0.5C, 1C, 2C and 4C all show the first platform (as shown in the dotted circle), so it can be determined that lithium deposition occurs in the battery when the charging rates are 0.5C, 1C, 2C and 4C.
[0068] like Figure 6 As shown in the figure, this figure is the voltage-time curve during the static process after the constant voltage charging process at different charging rates when the working temperature is 25°C. It can be seen from the figure that:
[0069] When the operating temperature is 25°C, the curve corresponding to the charging rate of 5C shows the first platform (as shown in the dotted circle), so it can be determined that lithium deposition occurs in the battery when the charging rate is 5C.
[0070] like Figure 7As shown in the figure, this figure is the voltage-time curve during the static process after the constant voltage charging process at different charging rates when the working temperature is 45°C. It can be seen from the figure that:
[0071] When the operating temperature is 45°C, the curves corresponding to the charging rates of 1C, 2C and 4C do not show the first platform, so it can be determined that when the charging rates are 1C, 2C and 4C, the battery does not experience lithium deposition.
[0072] Based on the above Figures 5 to 7 The results in Table 2 can be obtained, which shows the curve characteristics at different temperatures and different charging rates, as well as the actual lithium precipitation results obtained after disassembling the battery cells in the lithium-ion battery.
[0073] Table 2
[0074]
[0075] From Table 2 we can see that:
[0076] At -10°C, the result obtained by analyzing the curve characteristics (recorded as result 1) is consistent with the actual disassembly result (recorded as result 2), so it can be determined that the lithium precipitation detection method has high sensitivity and high accuracy at low temperatures;
[0077] At 45°C, the consistency between Result 1 and Result 2 is poor, so it can be determined that the sensitivity of the lithium precipitation detection method is low at high temperatures;
[0078] At 25°C, when the charge rate is greater than 4C, the consistency between results 1 and 2 is good;
[0079] Therefore, the third lithium deposition detection rule is more suitable for lithium deposition detection at low temperatures, and the second lithium deposition detection rule is more suitable for lithium deposition detection at room temperature and with a larger charging rate.
[0080] It should be noted that the reason why the curve does not show the first platform at a low charge rate of 25°C and 45°C may be:
[0081] During the constant voltage charging process, the lithium extraction reaction has been completed, and during the static process, there is only a diffusion process, so the voltage does not rise, and thus the first platform does not appear.
[0082] 3. The fourth lithium deposition detection rule:
[0083] In the initial stage of the discharge process, if lithium plating occurs, a second platform will appear in the voltage-state of charge curve, and the greater the charge rate, the more obvious the second platform will be.
[0084] This is due to:
[0085] When the negative electrode is made of graphite material, in the initial stage of the discharge process, the lithium extraction reaction will precede the extraction of lithium ions in the graphite, resulting in a second platform on the discharge curve.
[0086] For example, Figure 8 As shown in the figure, this figure shows the discharge curve at different charging rates when the operating temperature is -10°C, where 0.1C corresponds to the charging cut-off current. It can be seen from the figure that:
[0087] When the operating temperature is -10℃, the curves corresponding to the charging rates of 0.5C, 1C, 2C and 4C all show a second platform (as shown in the dotted circle), so it can be determined that lithium deposition occurs in the battery when the charging rates are 0.5C, 1C, 2C and 4C.
[0088] like Fig. 9 As shown in the figure, this figure shows the discharge curve at different charging rates when the operating temperature is 25°C, where 0.1C corresponds to the charging cut-off current. It can be seen from the figure that:
[0089] When the operating temperature is 25℃, the curves corresponding to the charging rates of 0.5C, 1C, 2C and 4C do not show the second platform, so it can be determined that when the charging rates are 0.5C, 1C, 2C and 4C, the battery does not experience lithium deposition.
[0090] like Fig.10 As shown in the figure, this figure shows the discharge curve at different charging rates when the operating temperature is 45°C, where 0.1C corresponds to the charging cut-off current. It can be seen from the figure that:
[0091] When the operating temperature is 45°C, the curves corresponding to the charging rates of 1C, 2C and 4C do not show the second platform, so it can be determined that when the charging rates are 1C, 2C and 4C, the battery does not experience lithium deposition.
[0092] Based on the above Figures 8 to 10 The results in Table 3 can be obtained, which shows the curve characteristics at different temperatures and different charging rates, as well as the actual lithium precipitation results obtained after disassembling the battery cells in the lithium-ion battery.
[0093] From Table 3 we can see that:
[0094] At -10°C, the result obtained by analyzing the curve characteristics (recorded as result 1) is consistent with the actual disassembly result (recorded as result 2), so it can be determined that the lithium precipitation detection method has high sensitivity and high accuracy at low temperatures;
[0095] At 25℃ and 45℃, the consistency between Result 1 and Result 2 is poor, so it can be determined that the sensitivity of the lithium precipitation detection method is low at room temperature and high temperature;
[0096] Therefore, the fourth lithium deposition detection rule is more suitable for lithium deposition detection at low temperatures.
[0097] Table 3
[0098]
[0099] Optionally, in an embodiment of the present invention, according to the correspondence between the preset temperature and the lithium deposition detection rule, finding out the lithium deposition detection rule corresponding to the operating temperature specifically includes:
[0100] Determine the temperature range corresponding to the operating temperature;
[0101] The lithium deposition detection rule corresponding to the determined temperature range is found from the corresponding relationship.
[0102] For example, if the operating temperature is 25°C, the corresponding temperature range can be determined to be the second temperature range, that is, corresponding to normal temperature. At this time, the first lithium deposition detection rule and the second lithium deposition detection rule can be selected, and based on the first lithium deposition detection rule and the second lithium deposition detection rule, it is detected whether the battery has lithium deposition.
[0103] In this way, the lithium precipitation detection rule corresponding to the operating temperature can be determined according to the corresponding relationship, thereby improving the accuracy and reliability of the detection result.
[0104] Optionally, in the embodiment of the present invention, for the fourth lithium deposition detection rule, the initial discharge stage may be a stage where the state of charge of the battery is not greater than 20%.
[0105] In this way, it is convenient to detect whether lithium deposition occurs in the battery by observing the voltage variation characteristics during the discharge process when the battery is in a low charge state.
[0106] In actual process, the battery charging process may include: constant current charging process and constant voltage charging process;
[0107] Among them, the constant current charging process can be understood as: charging with a set current (i.e., charging rate), during which the current remains constant, and the voltage increases with the increase of charging time until the voltage reaches the set cut-off voltage, and the constant current charging process ends;
[0108] The constant voltage charging process can be understood as: charging at the cut-off voltage, during which the charging voltage clock is kept at the cut-off voltage, and the current decreases as the charging time increases until it reaches the cut-off charging rate, and the charging is terminated.
[0109] Optionally, in an embodiment of the present invention, for the second lithium plating detection rule, the starting voltage of the first platform is less than the cut-off voltage, and the difference between the starting voltage of the first platform and the voltage during constant voltage charging (ie, the cut-off voltage) is less than 0.5V.
[0110] This shows that the first platform appears in the high-pressure stage.
[0111] In addition, it should be noted that during the static process, the battery is not discharged, and the voltage gradually decreases due to the existence of the battery voltage drop; if the first platform appears, it is very likely that the voltage increases to a certain extent due to the lithium extraction reaction of the elemental lithium precipitated on the surface of the negative electrode, changing the original decreasing trend and thus achieving the first platform.
[0112] S103. Detect whether lithium deposition occurs in the battery according to the found lithium deposition detection rule.
[0113] Optionally, in an embodiment of the present invention, detecting whether lithium deposition occurs in the battery according to the found lithium deposition detection rule specifically includes:
[0114] When the operating temperature is within the first temperature range, whether lithium deposition occurs in the battery is detected according to the first lithium deposition detection rule.
[0115] That is to say, when the operating temperature is in the first temperature range, the lithium deposition detection rule found is the first lithium deposition detection rule. At this time, whether lithium deposition occurs in the battery can be detected according to the first lithium deposition detection rule; since the first lithium deposition detection rule is more accurate in the first temperature range, the detection result is also more accurate and reliable.
[0116] Optionally, in an embodiment of the present invention, detecting whether lithium deposition occurs in the battery according to the found lithium deposition detection rule specifically includes:
[0117] When the operating temperature is within the second temperature range, when lithium deposition is detected in the battery according to the first lithium deposition detection rule and / or the second lithium deposition detection rule, it is determined that lithium deposition occurs in the battery;
[0118] According to the lithium plating detection rules found, detect whether lithium plating occurs in the battery, including:
[0119] When the operating temperature is within the third temperature range, when lithium deposition is detected in the battery according to the third lithium deposition detection rule and / or the fourth lithium deposition detection rule, it is determined that lithium deposition occurs in the battery.
[0120] That is to say, when the operating temperature is in the second temperature range, the lithium deposition detection rules found include: the first lithium deposition detection rule and the second lithium deposition detection rule. At this time, whether lithium deposition occurs in the battery can be detected according to the first lithium deposition detection rule and / or the second lithium deposition detection rule; since the first lithium deposition detection rule and the second lithium deposition detection rule are more accurate in the second temperature range, the detection results are also more accurate and reliable.
[0121] Similarly, when the operating temperature is in the third temperature range, the lithium deposition detection rules found include: the third lithium deposition detection rule and the fourth lithium deposition detection rule. At this time, whether lithium deposition occurs in the battery can be detected according to the third lithium deposition detection rule and / or the fourth lithium deposition detection rule; since the third lithium deposition detection rule and the fourth lithium deposition detection rule are more accurate in the third temperature range, the detection results are also more accurate and reliable.
[0122] Moreover, taking the operating temperature being in the second temperature range as an example, since the lithium deposition detection rules found include: a first lithium deposition detection rule and a second lithium deposition detection rule, in specific implementation, a first detection may be performed according to the first lithium deposition detection rule, and then a second detection may be performed using the second lithium deposition detection rule, and the accuracy of the first detection result may be verified by the result of the second detection;
[0123] If the two results are inconsistent, it may be that the lower degree of lithium deposition causes a deviation in the test result (i.e. the first or second time). At this time, it can be determined that the battery has lithium deposition. If the two results are consistent, it means that there is no error in the test result and the test result is accurate.
[0124] In this way, through the two test results, it is possible to detect whether the battery has lithium plating from multiple angles, so as to reduce the detection error and improve the accuracy of the test results.
[0125] Based on this, the above technical solution can achieve the following technical effects:
[0126] When determining the current operating temperature of the battery, the lithium deposition detection rule corresponding to the operating temperature can be found according to the correspondence between the preset temperature and the lithium deposition detection rule, so that whether lithium deposition occurs in the battery can be detected according to the found lithium deposition detection rule; this process can select appropriate lithium deposition detection rules according to the operating temperature, avoid the problem of inaccurate detection results caused by a single lithium deposition detection rule, reduce the probability of false alarms, make the detection results more accurate and reliable, and thus improve the safety of lithium-ion batteries.
[0127] Based on the same inventive concept, an embodiment of the present invention provides a battery lithium deposition detection device. The implementation principle of the detection device is similar to the implementation principle of the aforementioned detection method. The specific implementation of the detection device can refer to the specific embodiment of the aforementioned detection method, and the repeated parts will not be repeated.
[0128] Specifically, an embodiment of the present invention provides a battery lithium deposition detection device, such as Fig.11 As shown, it may include:
[0129] Memory 1101, used for storing program instructions;
[0130] The processor 1102 is used to call the program instructions stored in the memory 1101 and execute the above-mentioned detection method provided in the embodiment of the present invention according to the obtained program.
[0131] Based on the same inventive concept, an embodiment of the present invention provides an electric device, such as Fig.12 As shown, it includes: a battery 1201, and the above-mentioned detection device 1202 provided by the embodiment of the present invention.
[0132] Optionally, in an embodiment of the present invention, if Fig.12 As shown, the electric device may further include: a battery management system m1, and the detection device 1202 is located in the battery management system m1.
[0133] That is to say, a certain module in the battery management system can realize the function of the detection device.
[0134] In this way, the detection device can be integrated into the battery management system, thereby improving the integration of the battery management system and simplifying the structure of the electric device.
[0135] Alternatively, an existing module in the battery management system can be reused as a detection device to avoid increasing the structural complexity of the battery management system. Thus, accurate lithium plating detection can be achieved based on the original structure, providing guidance for subsequent safety measures.
[0136] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A method for detecting battery lithium deposition, characterized in that: include: Determining the current operating temperature of the battery; According to the correspondence between the preset temperature and the lithium precipitation detection rule, find out the lithium precipitation detection rule corresponding to the working temperature; According to the found lithium deposition detection rule, detecting whether lithium deposition occurs in the battery; The corresponding relationship includes: The first temperature range corresponds to the first lithium deposition detection rule, the second temperature range corresponds to the first lithium deposition detection rule and the second lithium deposition detection rule, and the third temperature range corresponds to the third lithium deposition detection rule and the fourth lithium deposition detection rule; the first temperature range is greater than or equal to 40°C, the second temperature range is greater than or equal to 10°C and less than 40°C, and the third temperature range is less than 10°C; Wherein, the first lithium deposition detection rule comprises: based on the current-time curve obtained during the constant voltage charging process of the battery, when the current does not decrease exponentially with the increase of time, and / or the differential result corresponding to the current does not increase exponentially with the increase of the time, determining that lithium deposition occurs in the battery; The second lithium deposition detection rule includes: based on a voltage-time curve obtained during the static process of the battery after the constant voltage charging process, when the curve shows a first platform and the charging rate used in the constant current charging process is greater than a preset rate, determining that lithium deposition occurs in the battery; The third lithium deposition detection rule comprises: based on a voltage-time curve obtained during a static state of the battery after the constant voltage charging process, the curve shows the first platform, and it is determined that lithium deposition occurs in the battery; The fourth lithium deposition detection rule includes: based on a discharge curve obtained by the battery in an initial discharge stage, when the curve shows a second platform, determining that lithium deposition occurs in the battery.
2. The detection method according to claim 1, characterized in that According to the found lithium deposition detection rule, detecting whether lithium deposition occurs in the battery specifically includes: When the operating temperature is within the first temperature range, whether lithium deposition occurs in the battery is detected according to the first lithium deposition detection rule.
3. The detection method according to claim 1, characterized in that According to the found lithium deposition detection rule, detecting whether lithium deposition occurs in the battery specifically includes: When the operating temperature is within the second temperature range, when lithium deposition is detected in the battery according to the first lithium deposition detection rule and / or the second lithium deposition detection rule, determining that lithium deposition occurs in the battery; According to the found lithium deposition detection rule, detecting whether lithium deposition occurs in the battery specifically includes: When the operating temperature is within the third temperature range, when lithium deposition is detected in the battery according to the third lithium deposition detection rule and / or the fourth lithium deposition detection rule, it is determined that lithium deposition occurs in the battery.
4. The detection method according to claim 1, characterized in that According to the correspondence between the preset temperature and the lithium precipitation detection rule, the lithium precipitation detection rule corresponding to the working temperature is found, specifically including: Determine the temperature range corresponding to the operating temperature; The lithium deposition detection rule corresponding to the determined temperature range is found from the corresponding relationship.
5. The detection method according to any one of claims 1 to 4, characterized in that: The difference between the starting voltage of the first platform and the voltage during the constant voltage charging process is less than 0.5V.
6. The detection method according to any one of claims 1 to 4, characterized in that: The initial discharge stage is a stage where the state of charge of the battery is not greater than 20%.
7. A battery lithium deposition detection device, characterized in that: include: A memory for storing program instructions; A processor is used to call the program instructions stored in the memory and execute the detection method according to any one of claims 1 to 6 according to the obtained program.
8. An electric device, characterized in that: include: A battery, and a detection device as claimed in claim 7.
Citation Information
Cited By
Dendritic crystal in-situ quantitative detection system and detection method based on battery internal distributed micro-area capacitance detection