Display panel and method for manufacturing the same

By depositing and etching the organic light-emitting layer and cathode layer on the array substrate, and using the patterned photoresist layer as an anti-etching layer to replace the fine metal mask, the problem of high production cost of the display panel is solved and the cost is reduced. and quality improvement.

CN116887616BActive Publication Date: 2024-10-29CHUZHOU HKC OPTOELECTRONICS TECH CO LTD +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202310851010.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-07-11
Publication Date
2024-10-29
Estimated Expiration
2043-07-11

AI Technical Summary

Technical Problem

The production cost of conventional display panels is higher, mainly due to the high cost of using fine metal masks.

Method used

The pixel openings on the array substrate are used to deposit and etch the organic light-emitting layer and cathode layer. The patterned photoresist layer is used as an anti-etching layer to replace the fine metal mask, which reduces the preparation cost and improves the etching process. During the process, the organic light-emitting layer is protected by the deposited cathode layer to avoid damage.

Benefits of technology

It significantly reduces the preparation cost of the display panel, improves the production quality and reliability, avoids damage to the organic light-emitting layer during the patterning process of the next layer, and ensures the quality of the display panel.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116887616B_ABST
    Figure CN116887616B_ABST
Patent Text Reader

Abstract

The present application discloses a display panel and a method for preparing the same, and belongs to the field of display technology. The method for preparing the display panel includes: providing an array substrate, etching the first organic light-emitting layer and the first cathode layer sequentially deposited on the array substrate to obtain a graphic first organic light-emitting layer and a graphic first cathode stacked together; then sequentially depositing the second organic light-emitting layer and the second cathode layer, and during the etching process, protecting the graphic first organic light-emitting layer by the graphic first cathode to obtain a graphic second organic light-emitting layer and a graphic second cathode, and then using the same method to obtain a graphic third organic light-emitting layer and a graphic third cathode, and depositing an auxiliary electrode to connect the graphic first cathode, the graphic second cathode and the graphic third cathode to obtain a display panel. The present application solves the technical problem of the high cost of preparing conventional display panels.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of display technology, and in particular to a display panel and a method for preparing the same. Background Art

[0002] In recent years, organic light emitting diode (OLED) display panels have been widely used in the display field due to their advantages such as self-luminescence, wide viewing angle, fast response, low power consumption and flexible display. Conventional display panels are mostly prepared by evaporation process, that is, using fine metal mask (FMM) to evaporate organic materials into each pixel unit of the pixel area of ​​OLED backplane, so as to form the required organic light emitting material layer on the OLED backplane; however, the cost of FMM is high, which leads to high production cost of display panels.

[0003] The above contents are only used to assist in understanding the technical solution of the present application and do not constitute an admission that the above contents are prior art. Summary of the invention

[0004] The main purpose of the present application is to provide a display panel and a method for preparing the same, aiming to solve the technical problem of high production cost of conventional display panels.

[0005] To achieve the above object, the present application provides a method for preparing a display panel, the method comprising the following steps:

[0006] Providing an array substrate, forming a pixel definition layer and a pixel anode layer on the array substrate; wherein the pixel definition layer has a plurality of pixel openings, the anodes of the pixel anode layer expose the pixel openings, and the plurality of pixel openings include a first opening, a second opening, and a third opening;

[0007] Depositing a first organic light-emitting layer and a first cathode layer on the array substrate in sequence, forming a first photoresist layer on the first cathode layer, and patterning the first photoresist layer to obtain a first mask pattern located above the first opening;

[0008] Using the first mask pattern as an anti-etching layer, etching the first organic light-emitting layer and the first cathode layer to obtain a patterned first organic light-emitting layer and a patterned first cathode layer stacked together;

[0009] Removing the first mask pattern, depositing a second organic light-emitting layer and a second cathode layer on the array substrate in sequence, forming a second photoresist layer on the second cathode layer, and patterning the second photoresist layer to obtain a second mask pattern located above the second opening;

[0010] Using the second mask pattern as an anti-etching layer, etching the second organic light-emitting layer and the second cathode layer to obtain a patterned second organic light-emitting layer and a patterned second cathode layer stacked together;

[0011] Removing the second mask pattern, depositing a third organic light-emitting layer and a third cathode layer on the array substrate in sequence, forming a third photoresist layer on the third cathode layer, and patterning the third photoresist layer to obtain a third mask pattern located above the third opening;

[0012] Using the third mask pattern as an anti-etching layer, etching the third organic light-emitting layer and the third cathode layer to obtain a patterned third organic light-emitting layer and a patterned third cathode layer stacked together;

[0013] The third mask pattern is removed, and an auxiliary electrode is deposited on the array substrate to connect the patterned first cathode, the patterned second cathode and the patterned third cathode to obtain a display panel.

[0014] Optionally, the thickness of the first cathode layer is 150-300 nm, the thickness of the second cathode layer is 100-250 nm, and the thickness of the third cathode layer is 50-200 nm.

[0015] Optionally, the step of depositing an auxiliary electrode on the array substrate includes:

[0016] A fine metal mask is arranged on the array substrate to deposit the auxiliary electrode in a non-opening area on the array substrate, wherein the non-opening area is an area on the array substrate except the first opening, the second opening and the third opening.

[0017] Optionally, the step of depositing an auxiliary electrode on the array substrate further includes:

[0018] The auxiliary electrode is deposited as a whole layer on the array substrate.

[0019] Optionally, the auxiliary electrode comprises: one or more of silver, aluminum, magnesium-aluminum alloy, indium tin oxide and indium zinc oxide, and has a thickness of 200-400 nm.

[0020] Optionally, the first cathode layer, the second cathode layer and the third cathode layer include one or more of silver, aluminum, magnesium-aluminum alloy, indium tin oxide and indium zinc oxide.

[0021] Optionally, the deposition process of the first organic light-emitting layer, the second organic light-emitting layer and the third organic light-emitting layer is an evaporation process.

[0022] Optionally, a deposition process of the first cathode, the second cathode and the third cathode is an evaporation process or a magnetron sputtering process.

[0023] The present application also provides a display panel, which is manufactured by the above-mentioned display panel manufacturing method.

[0024] The present application discloses a display panel and a preparation method thereof, wherein an array substrate is provided, a pixel definition layer and a pixel anode layer are formed on the array substrate; wherein the pixel definition layer has a plurality of pixel openings, the anode of the pixel anode layer is exposed to the pixel opening, and the plurality of pixel openings include a first opening, a second opening, and a third opening; then a first organic light-emitting layer and a first cathode layer are sequentially deposited on the array substrate, a first photoresist layer is formed on the first cathode layer, and the first photoresist layer is patterned to obtain a first mask pattern located above the first opening; and the first mask pattern is used as an anti-etching layer to etch the first organic light-emitting layer and the first cathode layer to obtain The method comprises the following steps: first, a patterned first organic light-emitting layer and a patterned first cathode layer are stacked together; an etching process is used to replace a fine metal mask required in a conventional display panel preparation process, thereby greatly reducing the preparation cost of the display panel; then, the first mask pattern is removed, a second organic light-emitting layer and a second cathode layer are sequentially deposited on the array substrate, a second photoresist layer is formed on the second cathode layer, and the second photoresist layer is patterned to obtain a second mask pattern located above the second opening; then, the second mask pattern is used as an anti-etching layer to etch the second organic light-emitting layer and the second cathode layer to obtain a patterned second organic light-emitting layer stacked together. and a patterned second cathode; since a patterned first cathode is deposited on the patterned first organic light-emitting layer, the patterned first organic light-emitting layer can be well protected from damage during the etching of the second organic light-emitting layer and the second cathode layer, so as to ensure the quality of the prepared display panel; then the second mask pattern is removed, a third organic light-emitting layer and a third cathode layer are sequentially deposited on the array substrate, a third photoresist layer is formed on the third cathode layer, and the third photoresist layer is patterned to obtain a third mask pattern located above the third opening; then the third organic light-emitting layer and the third cathode layer are etched using the third mask pattern as an anti-etching layer , so as to obtain a patterned third organic light-emitting layer and a patterned third cathode stacked together; since a patterned first cathode is deposited on the patterned first organic light-emitting layer, and a patterned second cathode is deposited on the patterned second organic light-emitting layer, the patterned first organic light-emitting layer and the patterned second organic light-emitting layer can be well protected from damage during the etching process of the third organic light-emitting layer and the third cathode layer, so as to ensure the quality of the prepared display panel; then the third mask pattern is removed, and an auxiliary electrode is deposited on the array substrate, so that the patterned first cathode, the patterned second cathode and the patterned third cathode are connected to obtain a display panel. The display panel is prepared by replacing the conventional fine metal mask with an etching process, which greatly reduces the cost of the preparation process of the display panel, and in the etching process, the cathode deposited on the organic light-emitting layer provides protection for the organic light-emitting layer, so as to avoid the patterned organic light-emitting layer on the array substrate from being damaged during the patterning process of the next organic light-emitting layer, thereby improving the production quality and reliability of the prepared display panel. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 A schematic diagram of a process for preparing a display panel according to an embodiment of the present application;

[0026] Figure 2 This is a schematic structural diagram of an array substrate according to an embodiment of the present application;

[0027] Figure 3 for Figure 1 A schematic diagram of the structure of an intermediate device obtained in step S20;

[0028] Figure 4 for Figure 1 A schematic structural diagram of another intermediate device obtained in step S20;

[0029] Figure 5 for Figure 1 A schematic diagram of the structure of an intermediate device obtained in step S30;

[0030] Figure 6 for Figure 1 A schematic diagram of the structure of an intermediate device obtained in step S40;

[0031] Figure 7 for Figure 1 A schematic structural diagram of another intermediate device obtained in step S40;

[0032] Figure 8 for Figure 1 A schematic structural diagram of another intermediate device obtained in step S40;

[0033] Fig. 9 for Figure 1 A schematic diagram of the structure of an intermediate device obtained in step S50;

[0034] Fig.10 for Figure 1 A schematic diagram of the structure of an intermediate device obtained in step S60;

[0035] Fig.11 for Figure 1 A schematic structural diagram of another intermediate device obtained in step S60;

[0036] Fig.12 for Figure 1 A schematic structural diagram of another intermediate device obtained in step S60;

[0037] Fig.13 for Figure 1 A schematic diagram of the structure of an intermediate device obtained in step S70;

[0038] Fig.14 for Figure 1A schematic diagram of the structure of an intermediate device obtained in step S80;

[0039] Fig.15 A schematic diagram of the structure of a display panel according to an embodiment of the present application;

[0040] Fig.16 FIG. 4 is another schematic diagram of the structure of the display panel according to the embodiment of the present application.

[0041] Description of Figure Numbers:

[0042]

[0043]

[0044] The realization of the purpose, functional features and advantages of this application will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0045] In order to make the purpose, technical scheme and advantages of the embodiments of the present application clearer, the technical scheme in the embodiments of the present application will be described clearly and completely below. If the specific conditions are not specified in the embodiments, they are carried out according to the conventional conditions or the conditions recommended by the manufacturer. If the manufacturer is not specified for the reagents or instruments used, they are all conventional products that can be purchased commercially.

[0046] In addition, the meaning of "and / or" appearing in the full text includes three parallel solutions. Taking "A and / or B" as an example, it includes solution A, solution B, or a solution that satisfies both A and B. In addition, the technical solutions between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in this field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such a combination of technical solutions does not exist and is not within the scope of protection required by this application. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.

[0047] A first aspect of the present application provides a method for preparing a display panel, referring to Figure 1 , the preparation method comprises the following steps:

[0048] Step S10, providing an array substrate 100, forming a pixel definition layer 110 and a pixel anode layer 120 on the array substrate 100; wherein the pixel definition layer 110 has a plurality of pixel openings 130, the anode of the pixel anode layer 120 exposes the pixel openings 130, and the plurality of pixel openings 130 include a first opening 131, a second opening 132 and a third opening 133;

[0049] Reference Figure 2, providing an array substrate 100, on which a pixel definition layer 110 and a pixel anode layer 120 are formed, the pixel definition layer 110 can be a patterned pixel definition layer 110, that is, the pixel definition layer 110 has a plurality of pixel openings 130, so that the anode of the pixel anode layer 120 is exposed in each of the pixel openings 130; the plurality of pixel openings 130 include a first opening 131, a second opening 132 and a third opening 133.

[0050] In a feasible implementation, the array substrate 100 includes one or more of a low-temperature polysilicon substrate, a low-temperature polycrystalline oxide substrate, and a metal oxide substrate.

[0051] Exemplarily, the array substrate 100 is a thin film transistor backplane (Thin Film Transistor, TFT).

[0052] In another feasible implementation, the pixel anode layer 120 includes: one or more of silver, aluminum, silver oxide, aluminum oxide, indium tin oxide and indium zinc oxide, and has a thickness of 50-200 nm.

[0053] Exemplarily, the pixel anode layer 120 is a stacked structure, which may be two layers, three layers or more layers; the top and bottom layers of the pixel anode layer 120 are metal oxides, and the middle layer is a single metal.

[0054] Exemplarily, the pixel anode layer 120 is electrically connected to the array substrate 100 .

[0055] Step S20, sequentially depositing a first organic light-emitting layer 210 and a first cathode layer 220 on the array substrate 100, forming a first photoresist layer on the first cathode layer 220, and patterning the first photoresist layer to obtain a first mask pattern 230 located above the first opening 131;

[0056] A first organic light emitting layer 210 is deposited on the array substrate 100, and then a first cathode layer 220 is deposited on the first organic light emitting layer 210 (see Figure 3 ), and then coating a photoresist on the first cathode layer 220 to form a first photoresist layer, and patterning the first photoresist layer to obtain a first mask pattern 230 located above the first opening 131 (refer to Figure 4 ); The organic light-emitting layer and cathode are patterned by etching, so there is no need to use a fine metal mask, which reduces the process cost of display panel preparation.

[0057] Exemplarily, the thickness of the first organic light emitting layer 210 is 100-300 nm.

[0058] Exemplarily, the first organic light-emitting layer 210 is any one of a red organic light-emitting layer, a green organic light-emitting layer and a blue organic light-emitting layer.

[0059] For example, the first organic light-emitting layer 210 , the second organic light-emitting layer 310 , and the third organic light-emitting layer 410 in the present application may include: one or more of a hole injection layer, a hole transport layer, a light-emitting layer, and an electron transport layer.

[0060] In a feasible implementation manner, the first cathode layer 220 includes: one or more of silver, aluminum, magnesium-aluminum alloy, indium tin oxide and indium zinc oxide; the thickness of the first cathode layer 220 is 150-300 nm.

[0061] In another feasible embodiment, the deposition process of the first organic light-emitting layer 210 is an evaporation process, and the deposition process of the first cathode layer 220 is an evaporation process or a magnetron sputtering process.

[0062] Exemplarily, the first photoresist layer is a positive photoresist, such as a diazonaphthoquinone phenolic resin photoresist.

[0063] Step S30, using the first mask pattern 230 as an anti-etching layer, etching the first organic light-emitting layer 210 and the first cathode layer 220 to obtain a patterned first organic light-emitting layer 211 and a patterned first cathode 221 stacked together;

[0064] The first organic light-emitting layer 210 and the first cathode layer 220 are etched using the first mask pattern 230 as an anti-etching layer to achieve patterning of the first organic light-emitting layer 210 and the first cathode layer 220, thereby obtaining a patterned first organic light-emitting layer 211 and a patterned first cathode layer 221 stacked together (refer to Figure 5 ).

[0065] Exemplarily, gas is used to perform plasma treatment on portions of the first organic light-emitting layer 210 and the first cathode layer 220 located outside the first mask pattern 230 to achieve patterning of the first organic light-emitting layer 210 and the first cathode layer 220, wherein the gas contains at least one of O2, N2O, CF4, and Ar.

[0066] Step S40, removing the first mask pattern 230, depositing a second organic light-emitting layer 310 and a second cathode layer 320 on the array substrate 100 in sequence, forming a second photoresist layer on the second cathode layer 320, and patterning the second photoresist layer to obtain a second mask pattern 330 located above the second opening 132;

[0067] The first mask pattern 230 is removed (see Figure 6), and then continue to deposit the second organic light-emitting layer 310 on the array substrate 100, and deposit the second cathode layer 320 on the second organic light-emitting layer 310 (refer to Figure 7 ); then coating a photoresist on the second cathode layer 320 to form a second photoresist layer; and patterning the second photoresist layer to obtain a second mask pattern 330 located above the second opening 132 (refer to Figure 8 ).

[0068] In one feasible implementation, the thickness of the second organic light-emitting layer 310 is 100-300 nm; the second organic light-emitting layer 310 is any one of a red organic light-emitting layer, a green organic light-emitting layer and a blue organic light-emitting layer, and has a different color from the first organic light-emitting layer 210 .

[0069] In another feasible implementation, the second cathode layer 320 includes: one or more of silver, aluminum, magnesium-aluminum alloy, indium tin oxide and indium zinc oxide, and has a thickness of 100-250 nm.

[0070] In another feasible implementation, the deposition process of the second organic light-emitting layer 310 is an evaporation process, and the deposition process of the second cathode layer 320 is an evaporation process or a magnetron sputtering process.

[0071] Exemplarily, the second photoresist layer is a positive photoresist, such as a diazonaphthoquinone phenolic resin photoresist.

[0072] Step S50, using the second mask pattern 330 as an anti-etching layer, etching the second organic light-emitting layer 310 and the second cathode layer 320 to obtain a patterned second organic light-emitting layer 311 and a patterned second cathode 321 stacked together;

[0073] The second organic light-emitting layer 310 and the second cathode layer 320 are etched with the second mask pattern 330 as an anti-etching layer to pattern the second organic light-emitting layer 310 and the second cathode layer 320, thereby obtaining a patterned second organic light-emitting layer 311 and a patterned second cathode layer 321 stacked together (refer to Fig. 9 ). A patterned first cathode 221 is deposited on the patterned first organic light-emitting layer 211. Therefore, when the second organic light-emitting layer 310 and the second cathode layer 320 are etched, the patterned first cathode 221 can be used to provide protection for the patterned first organic light-emitting layer 211 to avoid damage to the patterned first organic light-emitting layer 211. In addition, by setting the thickness of the first cathode layer 220 to 150-300 nm, the influence of etching on the first cathode layer 220 is reduced with a larger thickness, thereby improving the reliability of the prepared display panel.

[0074] Step S60, removing the second mask pattern 330, depositing a third organic light-emitting layer 410 and a third cathode layer 420 on the array substrate 100 in sequence, forming a third photoresist layer on the third cathode layer 420, and patterning the third photoresist layer to obtain a third mask pattern 430 located above the third opening 133;

[0075] The second mask pattern 33032 is removed (refer to Fig.10 ), and then the third organic light emitting layer 410 is further deposited on the array substrate 100, and then the third cathode layer 420 is deposited on the third organic light emitting layer 410 (refer to Fig.11 ); coating a photoresist on the third cathode layer 420 to form a third photoresist layer; and then patterning the third photoresist layer to obtain a third mask pattern 430 located above the third opening 133 (refer to Fig.12 ).

[0076] In one feasible embodiment, the thickness of the third organic light-emitting layer 410 is 100-300 nm; the third organic light-emitting layer 410 is any one of a red organic light-emitting layer, a green organic light-emitting layer and a blue organic light-emitting layer, and has a different color from the first organic light-emitting layer 210 and the second organic light-emitting layer 310 .

[0077] In another feasible implementation, the third cathode layer 420 includes: one or more of silver, aluminum, magnesium-aluminum alloy, indium tin oxide and indium zinc oxide, and has a thickness of 50-200 nm.

[0078] In another feasible implementation manner, the deposition process of the third organic light-emitting layer 410 is an evaporation process, and the deposition process of the third cathode layer 420 is an evaporation process or a magnetron sputtering process.

[0079] Exemplarily, the third photoresist layer is a positive photoresist; for example, a diazonaphthoquinone phenolic resin photoresist.

[0080] Step S70, using the third mask pattern 430 as an anti-etching layer, etching the third organic light-emitting layer 410 and the third cathode layer 420 to obtain a patterned third organic light-emitting layer 411 and a patterned third cathode 421 stacked together;

[0081] The third organic light-emitting layer 410 and the third cathode layer 420 are etched using the third mask pattern 430 as an anti-etching layer to achieve patterning of the third organic light-emitting layer 410 and the third cathode layer 420 to obtain a patterned third organic light-emitting layer 411 and a patterned third cathode 421 (refer to Fig.13). On the patterned first organic light-emitting layer 211 and the patterned second organic light-emitting layer 311, a patterned first cathode 221 and a patterned second cathode 321 are deposited respectively. Therefore, when etching the third organic light-emitting layer 410 and the third cathode layer 420, the patterned first cathode 221 and the patterned second cathode 321 can be used to provide protection for the patterned first organic light-emitting layer 211 and the patterned second organic light-emitting layer 311, respectively, to avoid damage to the patterned first organic light-emitting layer 211 and the patterned second organic light-emitting layer 311. In addition, by setting the thickness of the first cathode layer 220 to 150-300nm and the thickness of the second cathode layer 320 to 100-250nm, the effect of etching on the first cathode layer 220 and the second cathode layer 320 is reduced with a larger thickness, so that the thicknesses of the patterned first cathode 221, the patterned second cathode 321 and the patterned third cathode 421 obtained after etching are approximately equal, thereby improving the reliability of the prepared display panel.

[0082] Step S80 , removing the third mask pattern 430 , and depositing an auxiliary electrode 500 on the array substrate 100 , so as to connect the patterned first cathode 221 , the patterned second cathode 321 , and the patterned third cathode 421 , to obtain a display panel.

[0083] The third mask pattern 430 is removed (refer to Fig.14 ), and depositing an auxiliary electrode 500 on the array substrate 100 to connect the patterned first cathode 221, the patterned second cathode 321 and the patterned third cathode 421, thereby manufacturing a display panel.

[0084] Exemplarily, the deposition process of the auxiliary electrode 500 is an evaporation process or a magnetron sputtering process.

[0085] In a feasible implementation manner, the auxiliary electrode 500 includes: one or more of silver, aluminum, magnesium-aluminum alloy, indium tin oxide and indium zinc oxide, and has a thickness of 200-400 nm.

[0086] In another feasible implementation manner, step S80, the step of depositing the auxiliary electrode 500 on the array substrate 100 includes:

[0087] Step S81, setting a fine metal mask on the array substrate 100 so that the auxiliary electrode 500 is deposited in a non-opening area on the array substrate 100, wherein the non-opening area is an area on the array substrate 100 except the first opening 131, the second opening 132 and the third opening 133.

[0088] A fine metal mask is set on the array substrate 100, and the auxiliary electrode 500 is deposited, so that the non-opening area on the array substrate 100 is deposited with the auxiliary electrode 500 (refer to Fig.15 ), wherein the non-opening area is an area on the array substrate 100 except the first opening 131, the second opening 132 and the third opening 133, that is, an area without an organic light-emitting layer.

[0089] In this embodiment, although a fine metal mask is used, the fine metal mask is only used once in the entire process of preparing the display panel, so compared with the conventional display panel preparation method, the preparation cost can still be reduced.

[0090] In another feasible implementation manner, step S80, the step of depositing the auxiliary electrode 500 on the array substrate 100 includes:

[0091] Step S82 , depositing the auxiliary electrode 500 as a whole layer on the array substrate 100 .

[0092] The auxiliary electrode 500 is deposited as a whole layer on the array substrate 100 , so that an auxiliary electrode 500 layer is formed on the array substrate 100 .

[0093] In this embodiment, an array substrate 100 is provided, and a pixel definition layer 110 and a pixel anode layer 120 are formed on the array substrate 100; wherein the pixel definition layer 110 has a plurality of pixel openings 130, and the anode of the pixel anode layer 120 is exposed in the pixel openings 130, and the plurality of pixel openings 130 include a first opening 131, a second opening 132, and a third opening 133; then, a first organic light emitting layer 210 and a first cathode layer 220 are sequentially deposited on the array substrate 100, a first photoresist layer is formed on the first cathode layer 220, and the first photoresist layer is patterned to obtain a first mask pattern 230 located above the first opening 131; and the first mask pattern 230 is used as an anti-etching layer to form a first organic light emitting layer 210 and a first cathode layer 220. The organic light-emitting layer 210 and the first cathode layer 220 are etched to obtain a patterned first organic light-emitting layer 211 and a patterned first cathode 221 stacked together; the etching process is used to replace the fine metal mask required in the conventional display panel preparation process, which greatly reduces the preparation cost of the display panel; then the first mask pattern 230 is removed, and the second organic light-emitting layer 310 and the second cathode layer 320 are sequentially deposited on the array substrate 100, a second photoresist layer is formed on the second cathode layer 320, and the second photoresist layer is patterned to obtain a second mask pattern 330 located above the second opening 132; then the second mask pattern 330 is used as an anti-etching layer to The second organic light-emitting layer 310 and the second cathode layer 320 are etched to obtain a patterned second organic light-emitting layer 311 and a patterned second cathode 321 stacked together; since the patterned first cathode 221 is deposited on the patterned first organic light-emitting layer 211, the patterned first organic light-emitting layer 211 can be well protected from being damaged during the etching of the second organic light-emitting layer 310 and the second cathode layer 320, so as to ensure the quality of the prepared display panel; then the second mask pattern 330 is removed, and the third organic light-emitting layer 410 and the third cathode layer 420 are sequentially deposited on the array substrate 100, a third photoresist layer is formed on the third cathode layer 420, and the third photoresist layer is patterned to obtain a third organic light-emitting layer 410 located at the third opening 1 33; then, using the third mask pattern 430 as an anti-etching layer, the third organic light-emitting layer 410 and the third cathode layer 420 are etched to obtain a patterned third organic light-emitting layer 411 and a patterned third cathode 421 stacked together; since the patterned first cathode 221 is deposited on the patterned first organic light-emitting layer 211, and the patterned second cathode 321 is deposited on the patterned second organic light-emitting layer 311, therefore, in the process of etching the third organic light-emitting layer 410 and the third cathode layer 420, the patterned first organic light-emitting layer 211 and the patterned second organic light-emitting layer 311 can be well protected from being damaged, so as to ensure the quality of the prepared display panel;Then, the third mask pattern 430 is removed, and the auxiliary electrode 500 is deposited on the array substrate 100 to connect the patterned first cathode 221, the patterned second cathode 321 and the patterned third cathode 421 to obtain a display panel. The display panel is prepared by replacing the conventional fine metal mask with an etching process, which greatly reduces the manufacturing process cost of the display panel. In addition, during the etching process, the cathode deposited on the organic light-emitting layer provides protection for the organic light-emitting layer, thereby preventing the patterned organic light-emitting layer on the array substrate 100 from being damaged during the next organic light-emitting layer patterning process, thereby improving the production quality and reliability of the prepared display panel. ;

[0094] The above are only preferred embodiments of the present application, and do not limit the scope of the present application. For those skilled in the art, the present application may have various changes and modifications. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the scope of patent protection of the present application.

Claims

1. A method for preparing a display panel, characterized in that: The preparation method comprises the following steps: Providing an array substrate, forming a pixel definition layer and a pixel anode layer on the array substrate; wherein the pixel definition layer has a plurality of pixel openings, the anodes of the pixel anode layer expose the pixel openings, and the plurality of pixel openings include a first opening, a second opening, and a third opening; Depositing a first organic light-emitting layer and a first cathode layer on the array substrate in sequence, forming a first photoresist layer on the first cathode layer, and patterning the first photoresist layer to obtain a first mask pattern located above the first opening, wherein the thickness of the first cathode layer is 150-300 nm; Using the first mask pattern as an anti-etching layer, etching the first organic light-emitting layer and the first cathode layer to obtain a patterned first organic light-emitting layer and a patterned first cathode layer stacked together; Removing the first mask pattern, depositing a second organic light-emitting layer and a second cathode layer on the array substrate in sequence, forming a second photoresist layer on the second cathode layer, and patterning the second photoresist layer to obtain a second mask pattern located above the second opening, wherein the thickness of the second cathode layer is 100-250 nm; Using the second mask pattern as an anti-etching layer, etching the second organic light-emitting layer and the second cathode layer to obtain a patterned second organic light-emitting layer and a patterned second cathode layer stacked together; removing the second mask pattern, depositing a third organic light-emitting layer and a third cathode layer on the array substrate in sequence, forming a third photoresist layer on the third cathode layer, and patterning the third photoresist layer to obtain a third mask pattern located above the third opening, wherein the thickness of the third cathode layer is 50-200 nm; Using the third mask pattern as an anti-etching layer, etching the third organic light-emitting layer and the third cathode layer to obtain a patterned third organic light-emitting layer and a patterned third cathode layer stacked together; The third mask pattern is removed, and an auxiliary electrode is deposited on the array substrate to connect the patterned first cathode, the patterned second cathode and the patterned third cathode to obtain a display panel.

2. The method for preparing a display panel according to claim 1, wherein: The step of depositing an auxiliary electrode on the array substrate comprises: A fine metal mask is arranged on the array substrate to deposit the auxiliary electrode in a non-opening area on the array substrate, wherein the non-opening area is an area on the array substrate except the first opening, the second opening and the third opening.

3. The method for preparing a display panel according to claim 1, wherein: The step of depositing an auxiliary electrode on the array substrate further includes: The auxiliary electrode is deposited as a whole layer on the array substrate.

4. The method for preparing a display panel according to claim 1, wherein: The first organic light-emitting layer, the second organic light-emitting layer and the third organic light-emitting layer are organic light-emitting layers of different colors, and the colors include red, green and blue.

5. The method for preparing a display panel according to claim 1, wherein: The first cathode layer, the second cathode layer and the third cathode layer include: one or more of silver, aluminum, magnesium aluminum alloy, indium tin oxide and indium zinc oxide.

6. The method for preparing a display panel according to claim 1, wherein: The auxiliary electrode comprises: one or more of silver, aluminum, magnesium-aluminum alloy, indium tin oxide and indium zinc oxide, and has a thickness of 200-400 nm.

7. The method for preparing a display panel according to claim 1, wherein: The deposition process of the first organic light-emitting layer, the second organic light-emitting layer and the third organic light-emitting layer is an evaporation process.

8. The method for preparing a display panel according to claim 1, wherein: The deposition process of the first cathode, the second cathode and the third cathode is an evaporation process or a magnetron sputtering process.

9. A display panel, characterized in that: The display panel is manufactured by the method according to any one of claims 1 to 8.

Citation Information

Patent Citations

  • Manufacturing method for array substrate, array substrate, display panel and display device

    CN109742125A