A cold film biodegradable film production extruder

By using fan-shaped hole screening and personalized preheating technology in the feed barrel of the extruder, the problem of uneven preheating temperature caused by inconsistent particle sizes of the material is solved, and the extrusion effect and biodegradation of the extruder are improved. membrane quality.

CN117103489BActive Publication Date: 2024-10-29JIANGSU SHANHAITIAN ENVIRONMENTAL PROTECTION TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202311299131.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-10-09
Publication Date
2024-10-29
Estimated Expiration
2043-10-09

AI Technical Summary

Technical Problem

In the production of biodegradable films by existing extruders, the preheating temperature is uneven due to inconsistent particle sizes of the materials, resulting in excessive heating of some materials to form burnt materials, which reduces the extrusion effect and film quality.

Method used

A cold film type biodegradable film production extruder is designed, which uses fan-shaped holes in the feed barrel to screen materials of different particle sizes, and uses temperature sensors and heating wires to achieve personalized preheating of materials of different particle sizes, which avoids The difference in melting time improves the preheating effect.

Benefits of technology

It effectively avoids overheating of materials, improves the extrusion effect of the extruder and the quality of the finished biodegradable film, and enhances the control of the amount of materials put in.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117103489B_ABST
    Figure CN117103489B_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of extruders, in particular to an extruder for producing cold film type biodegradable films, comprising a machine body, wherein the machine body comprises a control unit, a drive unit, a temperature control unit, a mixing unit and a feeding unit; the control unit is used to control the operation of the machine body, the drive unit is used to drive the machine body, and the mixing unit is used to mix and melt different materials; materials with large particle sizes are screened by fan-shaped holes and fall between a No. 1 plate and an inner wall of a feeding barrel, and materials with small particle sizes and materials with large particle sizes are blocked by the No. 1 plate on both sides of the No. 1 plate, so that the preheating temperature of the materials with large particle sizes is higher than that of the materials with small particle sizes, so that the purpose of preheating different particle sizes at different temperatures is achieved, so that the melting time difference of the materials after entering the mixing unit is too long, which may cause coking, and the preheating effect of the materials is improved, so as to improve the extrusion effect of the extruder, and further improve the quality of the finished product of the biodegradable film.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of extruders, in particular to an extruder for producing cold film type biodegradable films. Background Art

[0002] Extruder is an important machine for plastic production. The production of most plastic products can be achieved by extrusion molding, such as its application in the production of biodegradable films. Biodegradable films refer to a type of plastic film that can be degraded by microorganisms under natural environmental conditions. After microorganisms such as bacteria, fungi and actinomycetes erode plastic films, the polymer components are hydrolyzed, ionized or protonated due to cell growth, causing mechanical damage and splitting into oligomer fragments. The enzymes secreted by fungi or bacteria decompose or oxidize water-soluble polymers into water-soluble fragments, generating new small molecule compounds until they are finally decomposed into C02 and H20.

[0003] When producing biodegradable film, the material is extruded through an extruder, and then the material is made into a film using a die head, and then the film is cooled and cut to form a cold film type biodegradable film. In the production process of cold film type biodegradable film, the required materials are first put into the extruder through a feed barrel according to the ratio, and then the extruder heats and mixes the internal materials, and the biodegradable film is produced by the film-forming device of the extruder die head.

[0004] Although the prior art includes a stage of preheating the materials put in, there is no strict regulation on the particle size of the materials put in, resulting in different particle sizes of the materials put into the extruder and different preheating temperatures. In the process of heating and melting the materials in the extruder, the materials with small particle sizes melt first, while the materials with large particle sizes take longer to melt than the materials with small particle sizes due to their larger volume. Therefore, the materials with small particle sizes have been melted into rubber in the extruder, while the materials with large particle sizes are still in granular form. In the process of continuing heating and mixing, after the materials with large particle sizes melt, part of the rubber-like materials may be burnt to form charred materials due to overheating, and intermittent char spots or even char blocks may appear during the extrusion process of the extruder, reducing the extrusion effect of the extruder, resulting in a part of the biodegradable film produced by the film-forming device being in a charred state, and these charred areas may lead to a decrease in the quality of the biodegradable film. Summary of the invention

[0005] In order to make up for the deficiencies of the prior art and solve the above-mentioned technical problems, the present invention provides an extruder for producing cold film type biodegradable films.

[0006] The technical solution adopted by the present invention to solve the technical problem is as follows: the present invention proposes an extruder for producing cold film type biodegradable film, comprising a machine body, the machine body comprising a control unit, a drive unit, a temperature control unit, a mixing unit and a feeding unit; the control unit is used to control the operation of the machine body, the drive unit is used to drive the machine body, the mixing unit is used to mix and melt different materials; the temperature control unit is used to control the temperature; the feeding unit is used to store and put materials into the mixing unit; the feeding unit comprises:

[0007] A feed barrel, the feed barrel is evenly installed on the top of the machine body, and the feed barrel is connected to the mixing unit; a temperature sensor is arranged inside the feed barrel; a No. 1 cavity is opened in the inner wall of the feed barrel, and a heating wire is coiled in the No. 1 cavity;

[0008] No. 1 pipe, the No. 1 pipe is rotatably connected to the center position of the feed barrel, and a disc is fixedly connected to the No. 1 pipe near the top of the feed barrel; fan-shaped holes are evenly opened on the disc; feed ports are evenly opened on the No. 1 pipe, and the feed ports are located between the disc and the top of the feed barrel, and a No. 1 block is fixedly connected to the No. 1 pipe below the feed port;

[0009] A baffle, the baffle is arranged near the bottom of the feed barrel, and one end of the No. 1 pipe is rotatably connected to the baffle; a No. 1 groove is provided on the baffle, and a stopper is slidably connected in the No. 1 groove; a No. 2 groove is provided inside the baffle near the No. 1 pipe, and one end of the stopper extends into the No. 2 groove; a push plate is hingedly connected to the No. 1 pipe at the position in the No. 2 groove, and the push plate swings in one direction;

[0010] A No. 1 plate, the No. 1 plate is fixedly connected to the top of the baffle plate, and the No. 1 plate is located between the disc and the baffle plate, and the No. 1 plate is in a barrel shape;

[0011] A No. 1 driving member is installed near the center of the top of the feed barrel, and the No. 1 driving member is used to drive a No. 1 pipe.

[0012] Preferably, the cross section of the disc is arc-shaped, and the surface of the disc is smooth; a lever is fixedly connected to the inner wall of the feed barrel, and the bottom of the lever is close to the top of the disc.

[0013] Preferably, the lever is arranged in a conical spiral shape, and a rubber block is arranged at the bottom of the lever, and the rubber block is close to the top of the disc.

[0014] Preferably, a heat-insulating material is provided in the first cavity, and the feed barrel is made of a metal with high thermal conductivity, and the feed barrel is in contact with the mixing unit.

[0015] Preferably, a No. 1 rod is evenly fixedly connected to the bottom of the disc, and the No. 1 rod is respectively located on the inner and outer sides of the No. 1 plate.

[0016] Preferably, the No. 1 rod is composed of the No. 2 rod and the No. 3 rod, and the cross section of the No. 1 rod is U-shaped; the No. 2 rod and the No. 3 rod are respectively closely attached to the surface of the No. 1 plate which is adjacent to each other.

[0017] Preferably, the second rod and the third rod are arranged in an arc shape, and the same-facing side of the second rod and the third rod are both serrated, and the serrated tooth tips of the second rod and the third rod face the disc.

[0018] Preferably, a guide plate is fixedly connected to one side of the No. 2 rod, and the guide plate is arranged obliquely.

[0019] Preferably, a No. 1 cover is fixedly connected to the top of the feed barrel, and the top cross-section of the No. 1 cover is arc-shaped, and the top of the No. 1 tube passes through the No. 1 cover; a support rod is fixedly connected to the top of the feed barrel, and an electric telescopic rod is fixedly connected to the top of the support rod; a sealing plate is slidably connected to the No. 1 tube near the top, and the sealing plate is connected to the telescopic end of the electric telescopic rod.

[0020] Preferably, the baffle is slidably connected to the inner wall of the feed barrel, and a weighing sensor is provided on the inner wall of the feed barrel near the bottom of the baffle.

[0021] The beneficial effects of the present invention are as follows:

[0022] 1. In the extruder for producing cold film type biodegradable film of the present invention, materials with large particle sizes are screened by fan-shaped holes and fall between the No. 1 plate and the inner wall of the feed barrel, and materials with small particle sizes and materials with large particle sizes are blocked by the No. 1 plate on the inner and outer sides of the No. 1 plate, so that the preheating temperature of materials with large particle sizes is higher than that of materials with small particle sizes, so as to achieve the purpose of preheating at different temperatures for different particle sizes, avoid the possibility of coking caused by the melting time difference of the materials after entering the mixing unit being too long, and improve the preheating effect of the materials, thereby improving the extrusion effect of the extruder, and further improving the quality of the finished biodegradable film.

[0023] The present invention provides an extruder for producing cold film type biodegradable films. When the push plate is reversed, the push plate does not swing. The push plate contacts one end of the stopper extending into the No. 2 groove and drives the stopper to slide along the No. 1 groove and the No. 2 groove, so that the stopper is retracted into the No. 1 groove. At this time, the stopper no longer blocks the material. The material on the baffle passes through the No. 1 groove and passes through the baffle, and falls from the bottom of the feed barrel into the mixing unit for heating and mixing. While the material is heated, the material feeding amount can be controlled, thereby improving the degree of control over the material feeding amount, thereby improving the convenience of using the extruder. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] The present invention will be further described below in conjunction with the accompanying drawings.

[0025] Figure 1 is a stereogram of the present invention;

[0026] Figure 2 It is a schematic diagram of the structure of the present invention;

[0027] Figure 3 yes Figure 2 A partial enlarged view of the middle A;

[0028] Figure 4 yes Figure 2 A partial enlarged view of point B in the middle;

[0029] Figure 5 is a top view of the disc in the present invention;

[0030] Figure 6 is a top view of the baffle in the present invention;

[0031] Figure 7 is a cross-sectional view of the baffle in the present invention in a top-down direction;

[0032] Figure 8 is a stereogram of the No. 1 pipe in the present invention;

[0033] Fig. 9 is a three-dimensional diagram of a No. 1 rod in the present invention;

[0034] In the figure: body 1, control unit 11, drive unit 12, temperature control unit 13, mixing unit 14, feeding unit 15, feeding barrel 2, temperature sensor 21, No. 1 cavity 22, heating wire 23, No. 1 tube 3, feeding port 31, No. 1 block 32, No. 1 driving member 33, disc 4, fan-shaped hole 41, lever 42, rubber block 43, No. 1 rod 44, No. 2 rod 45, No. 3 rod 46, guide plate 47, baffle 5, No. 1 slot 51, block 52, No. 2 slot 53, push plate 54, No. 1 plate 55, No. 1 cover 6, support rod 61, electric telescopic rod 62, sealing plate 63, weighing sensor 7. DETAILED DESCRIPTION

[0035] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0036] Embodiment 1:

[0037] Although the prior art has a stage of preheating the material to be put in, there is no strict regulation on the particle size of the material put in, resulting in different particle sizes of the material put into the extruder, and different preheating temperatures. In the process of heating and melting the material in the extruder, the material with a small particle size melts first, while the material with a large particle size takes longer to melt than the material with a small particle size due to its large volume. Therefore, the small particle size has been melted into a rubber material in the extruder, while the large particle size material is still in a granular state. In the process of continuing heating and mixing, after the large particle size material is melted, part of the rubber material may be burnt to form a coke material due to overheating. In the process of extrusion by the extruder, intermittent coke spots or even coke blocks appear, which reduces the extrusion effect of the extruder and causes a part of the biodegradable film produced by the film forming device to be in a coked state. These coked areas may cause the quality of the biodegradable film to decrease.

[0038] In order to effectively solve the above problems, as shown in the accompanying drawings of the specification Figure 1-9 As shown, an extruder for producing cold film type biodegradable film includes a body 1, which includes a control unit 11, a drive unit 12, a temperature control unit 13, a mixing unit 14 and a feeding unit 15; the control unit 11 is used to control the operation of the body 1, the drive unit 12 is used to drive the body 1, and the mixing unit 14 is used to mix and melt different materials; the temperature control unit 13 is used to control the temperature; the feeding unit 15 is used to store and put materials into the mixing unit 14; the control unit 11 is a conventional control component in the field, and the control unit 11 controls the drive unit 12, the temperature control unit 13, the mixing unit 14 and The feeding units 15 work in coordination with each other; the driving unit 12 is a conventional driving transmission device in the art, and the driving unit 12 drives and transmits the mixing unit 14; the temperature control unit 13 is a conventional temperature control component in the art, and the temperature control unit 13 controls the temperature inside the mixing unit 14 and the feeding barrel 2; the mixing unit 14 is a conventional mixing component in the art, and the mixing unit 14 heats, melts, mixes and extrude the materials fed through the feeding unit 15 into the extruder; the feeding unit 15 feeds the required materials into the mixing unit 14 at each stage of the mixing process; the feeding unit 15 includes:

[0039] The feed barrel 2 is evenly mounted on the top of the machine body 1, and the feed barrel 2 is connected to the mixing unit 14; a temperature sensor 21 is arranged inside the feed barrel 2, and the temperature sensor 21 is of a high temperature resistant type; a cavity No. 1 22 is opened in the inner wall of the feed barrel 2, and a heating wire 23 is coiled in the cavity No. 1 22; the heating wire 23 is connected to the temperature control unit 13, and the control unit 11 controls the heating wire 23 to work through the temperature control unit 13;

[0040] No. 1 pipe 3, No. 1 pipe 3 is rotatably connected to the center position of the feed barrel 2, and a disc 4 is fixedly connected to the part of the No. 1 pipe 3 near the top of the feed barrel 2; fan-shaped holes 41 are evenly opened on the disc 4, and the fan-shaped holes 41 expand toward the inner wall of the feed barrel 2 with the No. 1 pipe 3 as the starting point to form a fan shape; a feed port 31 is evenly opened on the No. 1 pipe 3, and the feed port 31 is located between the disc 4 and the top of the feed barrel 2, and a No. 1 block 32 is fixedly connected to the No. 1 pipe 3 below the feed port 31; the top of the No. 1 pipe 3 passes through the top of the feed barrel 2 and is exposed;

[0041] The baffle 5 is arranged near the bottom of the feed barrel 2, and one end of the No. 1 pipe 3 is rotatably connected to the baffle 5; a No. 1 groove 51 is provided on the baffle 5, and a stopper 52 is slidably connected in the No. 1 groove 51, and a return spring is provided between the No. 1 groove 51 and the stopper 52; a No. 2 groove 53 is provided inside the baffle 5 near the No. 1 pipe 3, and one end of the stopper 52 extends into the No. 2 groove 53; a push plate 54 is hingedly connected to the No. 1 pipe 3 at the position in the No. 2 groove 53, and the push plate 54 swings in one direction;

[0042] The first plate 55 is fixedly connected to the top of the baffle 5 and is located between the disc 4 and the baffle 5. The first plate 55 is in the shape of a barrel;

[0043] A No. 1 driving member 33 is installed near the center of the top of the feed barrel 2, and the No. 1 driving member 33 is used to drive the No. 1 pipe 3; the No. 1 driving member 33 is a conventional driving component, such as a motor, and the motor drives the No. 1 pipe through a belt, so that the No. 1 driving member 33 drives the No. 1 pipe 3 to rotate;

[0044] Specific work flow: the worker starts the extruder through the control unit 11 to preheat the mixing unit 14 in the machine body 1. After the temperature of the mixing unit 14 reaches the required temperature for mixing, the worker controls the temperature control unit 13 through the control unit 11 to make the heating wire 23 heat the feed barrel 2. After the temperature sensor 21 detects that the internal temperature of the feed barrel 2 reaches the material preheating temperature, and the preheating temperature in the feed barrel 2 is lower than the mixing temperature in the mixing unit 14, the feed barrel 2 preheats the material in an environment lower than the mixing temperature. When feeding is required, the heated material enters the mixing unit 14, which can shorten the heating time of the material in the mixing unit 14 and increase the extrusion efficiency. When feeding is not required, the heating barrel heats the material and stores it at a constant temperature, thereby improving the convenience of the extruder production process.

[0045] The worker will pour the material into the end of the No. 1 tube 3 exposed from the top of the feed barrel 2 according to the specified ratio of the biodegradable film. After entering the No. 1 tube 3, the material falls to the No. 1 block 32 until the material is blocked by the No. 1 block 32 inside the No. 1 tube 3 between the top inner wall of the feed barrel 2 and the disc 4. Then the material flows through the feed port 31 and is scattered on the disc 4 near the No. 1 tube 3; the No. 1 tube 3 rotates forward to drive the disc 4 to rotate, and the disc 4 drives the material to move. During the rotation of the material, it is affected by the centrifugal force and rolls on the disc 4 toward the side wall of the feed barrel 2; in the process of the material contacting the top of the disc 4 and rolling toward the side wall of the feed barrel 2, the material is continuously screened by the fan-shaped holes 41, and the material with a small particle size falls through the fan-shaped holes 41 into the area between the No. 1 plate 55 and the No. 1 tube 3, and the material with a large particle size passes through the fan-shaped holes 41. Screening, falling between the No. 1 plate 55 and the inner wall of the feed barrel 2, the materials with small particle size and the materials with large particle size are blocked by the No. 1 plate 55 on the inner and outer sides of the No. 1 plate 55, because when the feed barrel 2 is heated or kept at a constant temperature, since the heating wire 23 is coiled in the No. 1 cavity 22 in the feed barrel 2, the feed barrel 2 is preheated first, and then the inside of the feed barrel 2 and the No. 1 tube 3 are preheated, and the temperature of the inner wall of the feed barrel 2 is higher than the temperature inside the feed barrel 2, so that the preheating temperature of the material with large particle size is higher than the preheating temperature of the material with small particle size, so as to achieve the purpose of preheating at different temperatures for different particle sizes, avoid the melting time difference of the material after entering the mixing unit 14 is too long, causing the possibility of coking, improve the preheating effect of the material, thereby improving the extrusion effect of the extruder, and then improving the quality of the finished product of the biodegradable film;

[0046] After the materials are screened by the fan-shaped holes 41, they fall on the baffles 5 on the inner and outer sides of the No. 1 plate 55, and the baffles 5 block the screened materials and store them in the feed barrel 2; when adding materials is needed, the No. 1 driving member 33 is controlled to drive the No. 1 tube 3 to reverse the set angle, and the No. 1 tube 3 reverses and drives the push plate 54 to rotate around the axis of the No. 1 tube 3. Since the push plate 54 is a unidirectional swing setting, when the push plate 54 reverses, the push plate 54 will not swing. The push plate 54 contacts one end of the stopper 52 extending into the No. 2 groove 53 and drives the stopper 52 to slide along the No. 1 groove 51 and the No. 2 groove 53, so that the stopper 52 retracts into the No. 1 groove 51. At this time, the stopper 52 no longer blocks the materials, and the materials on the baffle 5 pass through the No. 1 groove 51 through the baffle 5, and fall from the bottom of the feed barrel 2 into the mixing unit 14 for heating and mixing. While heating the materials, the amount of materials fed can be controlled, thereby improving the degree of control over the amount of materials fed, thereby improving the convenience of using the extruder;

[0047] When no material is needed, the No. 1 driving member 33 is controlled to drive the No. 1 tube 3 to continue to rotate forward, and the No. 1 tube 3 drives the push plate 54 to rotate forward. At this time, the block 52 is affected by the reset spring to extend out of the No. 1 slot 51 for reset, thereby blocking and storing the material on the baffle 5. When the push plate 54 contacts the block 52 during rotation, the push plate 54 is squeezed by the block 52 and swings until it passes over the block 52. Then the push plate 54 is reset again, so that the No. 1 tube 3 will not affect the storage effect of the block 52 when it rotates forward, and the No. 1 tube 3 can also keep the material on the disc 4 Screening action improves the screening efficiency, thereby improving the screening efficiency of the feed barrel 2, and maintaining the continuous operation of the extruder from screening to preheating and then to heating and mixing, thereby improving the extrusion efficiency of the extruder.

[0048] Embodiment 2:

[0049] Based on the first embodiment, as shown in the accompanying drawings of the specification Figure 3 , Figure 5 and Figure 8 As shown, the cross section of the disc 4 is arc-shaped, and the surface of the disc 4 is smooth; a lever 42 is fixedly connected to the inner wall of the feed barrel 2, and the bottom of the lever 42 is close to the top of the disc 4;

[0050] The lever 42 is arranged in a conical spiral shape, and a rubber block 43 is arranged at the bottom of the lever 42, and the rubber block 43 is close to the top of the disc 4;

[0051] Specific working process: by setting the cross section of the disc 4 to be arc-shaped, the middle part of the disc 4 is far away from the baffle 5, and the outer circular end of the disc 4 is close to the baffle 5, so that the disc 4 is shaped like a pot cover; when the material flows to the part of the disc 4 close to the No. 1 pipe 3, the material slides down along the surface of the disc 4 toward the inner wall of the feed barrel 2 under the influence of gravity, and cooperates with the effect of the smooth treatment of the surface of the disc 4 to reduce the friction force generated by the material sliding up and down the disc 4, promote the material to slide down on the surface of the disc 4, increase the movement effect of the material on the surface of the disc 4, and make the material with a large particle size slide more quickly to the part of the fan-shaped hole 41 away from the No. 1 pipe 3, screened and dropped, thereby improving the screening efficiency of the material, shortening the time for the material to fall inside the feed barrel 2 for preheating, thereby improving the preheating effect of the material, thereby improving the extrusion effect of the extruder;

[0052] By setting a lever 42, and the lever 42 is in a conical spiral shape, the lever 42 can be close to the top of the disc 4; when the disc 4 rotates, the lever 42 is stationary, and the material on the disc 4 contacts the lever 42 during the sliding process, and slides down along the surface of the lever 42, guiding the material on the disc 4 to slide or roll downward in circles around the No. 1 tube 3, further increasing the movement effect of the material on the surface of the disc 4, shortening the time for the material to fall into the feed barrel 2 for preheating, thereby improving the preheating effect of the material, thereby improving the extrusion effect of the extruder;

[0053] In addition, if the material moves too fast on the disc 4, the material with a small particle size is engulfed by the material with a large particle size, and the fan-shaped hole 41 is close to the inner wall of the feed barrel 2, causing the material with a small particle size to be closer to or in contact with the inner wall of the feed barrel 2, and softening or over-preheating occurs due to the high preheating temperature; therefore, the lever 42 can also block the material that has just flowed to the surface of the disc 4, so that the material is fully screened by the fan-shaped hole 41 from the part close to the No. 1 pipe 3 to the part far away from the No. 1 pipe 3, thereby improving the screening effect, thereby improving the preheating effect of the material, and thus improving the extrusion effect of the extruder;

[0054] By providing the rubber block 43, when the disc 4 drives the material to rotate, the lever 42 contacts and pushes the material to move through the rubber block 43, so that the lever 42 and the material are in flexible contact, thereby preventing the lever 42 from crushing the material, resulting in a large amount of debris in the material, and affecting the material preheating effect.

[0055] Embodiment three:

[0056] Based on the second embodiment, as shown in the accompanying drawings of the specification Figure 4 As shown, the first cavity 22 is provided with a heat-insulating material, and the feed barrel 2 is made of a metal with high thermal conductivity, and the feed barrel 2 is in contact with the mixing unit 14;

[0057] Specific work flow: by setting the thermal insulation material, the thermal insulation material is selected from polyurethane foam, because the thermal conductivity of polyurethane itself is relatively low, so whether it is used outdoors or indoors, it can play a good thermal insulation role. The temperature in the environment will not spread, and the external high temperature will not be conducted in; after the heating wire 23 heats the feed barrel 2, the thermal insulation material in the No. 1 cavity 22 insulates the feed barrel 2, allowing the feed barrel 2 to heat up faster, and prolong its preheating temperature state, reducing the additional energy consumption of the heating wire 23; by setting the feed barrel 2 material to have high thermal conductivity Metal, such as silver-nickel alloy, has a higher thermal conductivity than copper, so that the feed barrel 2 can transfer heat faster. Since the feed barrel 2 is in contact with the mixing unit 14, the temperature control unit 13 can heat the feed barrel 2 synchronously while heating the mixing unit 14. Since the feed barrel 2 is exposed to the air, it loses heat faster than the mixing unit 14. The temperature of the feed barrel 2 is lower than the temperature in the mixing unit 14, so that in a colder environment where the heating wire 23 is not needed, the additional energy consumption of the heating wire 23 is further reduced, thereby increasing the practicality of the extruder.

[0058] In addition, when installing the feed barrel 2, a cooling water pipe can be wound around the outer wall of the feed barrel 2, and the feed barrel 2 with too high a temperature can be cooled by a circulating cooler to avoid the preheating temperature of the feed barrel 2 being too high, which affects the preheating effect of the material.

[0059] Embodiment 4:

[0060] Based on the third embodiment, as shown in the accompanying drawings of the specification Figure 3 , Figure 4 , Figure 6 , Figure 8 and Fig. 9 As shown, the bottom of the disc 4 is evenly fixed with a No. 1 rod 44, and the No. 1 rod 44 is located at both the inner and outer sides of the No. 1 plate 55;

[0061] The first rod 44 is composed of the second rod 45 and the third rod 46, and the cross section of the first rod 44 is U-shaped; the second rod 45 and the third rod 46 are respectively closely attached to the surface of the first plate 55;

[0062] The second rod 45 and the third rod 46 are arranged in an arc shape, and the same side of the second rod 45 and the third rod 46 is serrated, and the serrated tips of the second rod 45 and the third rod 46 face the disc 4;

[0063] A guide plate 47 is fixedly connected to one side of the second rod 45, and the guide plate 47 is inclined;

[0064] Specific working process: No. 1 pipe 3 drives disc 4 to rotate, and disc 4 drives rod 44 to rotate in feed barrel 2 with No. 1 pipe 3 as the center. Rod 44 contacts materials stored on baffle 5 during rotation, and turns these materials over, changing the area between materials, and turning over part of the materials that were originally far away from the inner wall of feed barrel 2 to approach the inner wall of feed barrel 2, so that materials with large particle sizes are heated evenly, and materials with small particle sizes are heated evenly, thereby improving the preheating effect of materials, thereby improving the extrusion effect of the extruder;

[0065] When installing the feed barrel 2, workers can increase or decrease the number of installed plates 55 according to needs. For example, when the number of plates 55 is one, the number of rods 44 is two, and the two rods 44 are located on the inner and outer sides of the barrel-shaped plate 55, respectively, to turn over materials of different particle sizes on the inner and outer sides of the plate 55; when the number of plates 55 is two, the number of rods 44 is three, the first rod 44 is located between the feed barrel 2 and the plate 55, the second rod 44 is located between adjacent plates 55, and the third rod 44 is located between the plate 55 and the tube 3. By increasing the number of plates 55, the particle size of the material can be screened more finely, and in combination with the rods 44, the preheating effect of the material can be further improved.

[0066] When the number of plates 55 is one and the number of rods 44 is two, the rotation of rod 44 drives rod 45 and rod 46 to rotate. Since the cross section of rod 44 is U-shaped, rod 45 located on the outside of plate 55 scrapes the inner wall of feed barrel 2, and rod 46 located on the outside of plate 55 scrapes the outer surface of plate 55; rod 45 located on the inside of plate 55 scrapes the inner surface of plate 55, and rod 46 located on the inside of plate 55 scrapes the surface of tube 3. Through the scraping of rod 45 and rod 46, the materials that are partially close to the inner wall of feed barrel 2, the inner and outer surfaces of plate 55 and the surface of tube 3 are regularly turned over, so that the materials in each area are evenly heated while avoiding the possibility of adhesion between the materials and the surfaces of these components, which affects the smoothness of feeding and discharging of the feed barrel 2.

[0067] Furthermore, because when it is necessary to replace materials or replace biodegradable films with different quality parameters, workers need to thoroughly clean the extruder to ensure that the quality will not be affected by material residues, and the depth of the feed barrel 2 in the conventional field is large, which is inconvenient for workers to clean; the second rod 45 and the third rod 46 scrape the inner wall of the feed barrel 2, the inner and outer surfaces of the first plate 55 and the surface of the first tube 3 to scrape away material dust or a small amount of debris that may adhere to the surface of these parts, thereby improving the cleanliness of the feed barrel 2, facilitating workers to clean the extruder when changing materials, reducing the cleaning work of the extruder, and improving the convenience of using the extruder;

[0068] Because the arc curvature of the inner wall of the feed barrel 2, the inner and outer surfaces of the No. 1 plate 55 and the surface of the No. 1 tube 3 are different, by setting the No. 2 rod 45 and the No. 3 rod 46 to be arc-shaped, and the arc curvature of each No. 2 rod 45 and the No. 3 rod 46 is different, each No. 2 rod 45 and the No. 3 rod 46 can be more closely fitted to the inner wall of the feed barrel 2, the inner and outer surfaces of the No. 1 plate 55 and the surface of the No. 1 tube 3 corresponding to each other, so that the No. 2 rod 45 and the No. 3 rod 46 can more effectively scrape impurities on the surfaces of these parts, further improving the cleanliness of the inside of the feed barrel 2;

[0069] In addition, the second rod 45 and the third rod 46 can also be arranged at an angle. When the second rod 45 and the third rod 46 scrape and clean these surfaces, impurities are scraped into the gap of the serrated portion on the second rod 45. Since the tooth tips in the serrated portion on the second rod 45 face the top of the disc 4, the impurities are retained in the serrated portion on the second rod 45, thereby avoiding the possibility of impurities in the serrated portion on the second rod 45 falling, thereby improving the cleanliness of the feed barrel 2.

[0070] By setting a guide plate 47, and with the guide plate 47 tilted toward between the No. 2 rod 45 and the No. 3 rod 46, the rotation of the No. 2 rod 45 drives the guide plate 47 to rotate. After part of the material is flipped over the No. 2 rod 45, it contacts the guide plate 47. The guide plate 47 guides the flipped material to the area between the No. 2 rod 45 and the No. 3 rod 46, increasing the flipping area of ​​the material by the No. 1 rod 44, improving the flipping effect of the material during the storage preheating process, thereby improving the preheating effect of the material, thereby improving the extrusion effect of the extruder.

[0071] Embodiment five:

[0072] Based on the fourth embodiment, as shown in the accompanying drawings of the specification Figure 1-Figure 4 As shown, a No. 1 cover 6 is fixedly connected to the top of the feed barrel 2, and the top cross-section of the No. 1 cover 6 is arc-shaped, and the top of the No. 1 tube 3 passes through the No. 1 cover 6; a support rod 61 is fixedly connected to the top of the feed barrel 2, and an electric telescopic rod 62 is fixedly connected to the top of the support rod 61, and the electric telescopic rod 62 is a conventional telescopic drive device; a sealing plate 63 is slidably connected to the No. 1 tube 3 near the top position, and the sealing plate 63 is connected to the telescopic end of the electric telescopic rod 62;

[0073] The baffle plate 5 is slidably connected to the inner wall of the feed barrel 2, and a weighing sensor 7 is arranged on the inner wall of the feed barrel 2 near the bottom of the baffle plate 5;

[0074] Specific working process: when adding materials, workers tear open the bagged materials. If workers are asked to add materials to the No. 1 tube 3, it will cause trouble for the workers during the use of the extruder; by setting the No. 1 cover 6, and the top of the No. 1 tube 3 is in contact with the top surface of the No. 1 cover 6, the top of the No. 1 tube 3 is exposed; workers only need to pour the materials into the No. 1 cover 6, and when adding materials is needed, the control unit 11 controls the electric telescopic rod 62 to retract, and the electric telescopic rod 62 drives the sealing plate 63 to move out of the No. 1 tube 3, opens the top of the No. 1 tube 3, and the materials in the No. 1 cover 6 slide into the No. 1 tube 3 along the surface of the No. 1 cover 6, and the feeding is completed; when no feeding is needed, the electric telescopic rod 62 extends and drives the sealing plate 63 to re-enter the No. 1 tube 3, and the top of the No. 1 tube 3 is blocked, so as to complete the blocking of the materials from entering the No. 1 tube 3, so that the materials can be added in an arbitrarily controlled manner, and the workers are convenient for feeding, thereby improving the convenience of using the extruder;

[0075] In addition, by setting a weighing sensor 7, and connecting the weighing sensor 7 to the control unit 11, when the material is stored on the inner wall of the feed barrel 2, the weighing sensor 7 weighs the material in the feed barrel 2 through the baffle 5, and keeps the feed barrel 2 preheated with a specified amount of material; when a specified amount of material needs to be added, the No. 1 pipe 3 is reversed, and the No. 1 slot 51 is opened through the block 52 to add material. The weighing sensor 7 monitors the weight of the remaining material on the baffle 5 in real time, and the weight of the material added to the mixing unit 14 is the weight lost on the baffle 5. Material weight; when the weighing sensor 7 detects that the set addition amount is reached, the control unit 11 controls the No. 1 tube 3 to continue to rotate forward and stops adding material, and the control unit 11 controls the electric telescopic rod 62 to retract, open the top of the No. 1 tube 3, and replenish the material inside the feed barrel 2 until the weighing sensor 7 monitors that the material on the baffle 5 reaches the storage value, then the electric telescopic rod 62 is controlled to retract to close the No. 1 tube 3, thereby realizing the functions of automatic feeding, preheating and replenishing of the feed barrel 2, further improving the convenience of using the extruder.

[0076] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. An extruder for producing cold film type biodegradable film, comprising a machine body (1), wherein the machine body (1) comprises a control unit (11), a drive unit (12), a temperature control unit (13), a mixing unit (14) and a feeding unit (15); the control unit (11) is used to control the operation of the machine body (1), the drive unit (12) is used to drive the machine body (1), the mixing unit (14) is used to mix and melt different materials; the temperature control unit (13) is used to control the temperature; the feeding unit (15) is used to store and feed materials into the mixing unit (14); characterized in that The feeding unit (15) comprises: A feed barrel (2), the feed barrel (2) being evenly mounted on the top of the machine body (1), and the feed barrel (2) being connected to the mixing unit (14); a temperature sensor (21) is arranged inside the feed barrel (2); a first cavity (22) is provided in the inner wall of the feed barrel (2), and a heating wire (23) is coiled inside the first cavity (22); A No. 1 pipe (3), the No. 1 pipe (3) is rotatably connected to the center position of the feed barrel (2), and a disc (4) is fixedly connected to the No. 1 pipe (3) near the top of the feed barrel (2); fan-shaped holes (41) are evenly opened on the disc (4), and the fan-shaped holes (41) expand toward the inner wall of the feed barrel (2) with the No. 1 pipe (3) as the starting point to form a fan shape; a feed port (31) is evenly opened on the No. 1 pipe (3), and the feed port (31) is located between the disc (4) and the top of the feed barrel (2), and a No. 1 block (32) is fixedly connected to the No. 1 pipe (3) below the feed port (31); A baffle (5), the baffle (5) is arranged near the bottom of the feed barrel (2), and one end of the No. 1 pipe (3) is rotatably connected to the baffle (5); a No. 1 groove (51) is provided on the baffle (5), and a stopper (52) is slidably connected in the No. 1 groove (51); a No. 2 groove (53) is provided inside the baffle (5) near the No. 1 pipe (3), and one end of the stopper (52) extends into the No. 2 groove (53); a push plate (54) is hingedly connected to the No. 1 pipe (3) in the No. 2 groove (53), and the push plate (54) swings in one direction; A first plate (55), the first plate (55) is fixedly connected to the top of the baffle (5), and the first plate (55) is located between the disc (4) and the baffle (5), and the first plate (55) is in the shape of a cylinder; A No. 1 driving member (33), wherein the No. 1 driving member (33) is installed near the center of the top of the feed barrel (2), and the No. 1 driving member (33) is used to drive the No. 1 pipe (3); The cross section of the disk (4) is arc-shaped, and the surface of the disk (4) is smooth; a lever (42) is fixedly connected to the inner wall of the feed barrel (2), and the bottom of the lever (42) is close to the top of the disk (4); the lever (42) is arranged in a conical spiral shape, and a rubber block (43) is arranged at the bottom of the lever (42), and the rubber block (43) is close to the top of the disk (4).

2. The extruder for producing cold film type biodegradable film according to claim 1, characterized in that: The first cavity (22) is provided with a heat-insulating material, and the material of the feed barrel (2) is a metal with high thermal conductivity, and the feed barrel (2) is in contact with the mixing unit (14).

3. The extruder for producing cold film type biodegradable film according to claim 1, characterized in that: The bottom of the disc (4) is evenly fixedly connected to a No. 1 rod (44), and the No. 1 rod (44) is located at both inner and outer sides of the No. 1 plate (55).

4. The extruder for producing cold film type biodegradable film according to claim 3, characterized in that: The first rod (44) is composed of a second rod (45) and a third rod (46), and the cross section of the first rod (44) is U-shaped; the second rod (45) and the third rod (46) are respectively closely attached to the surface of the first plate (55) adjacent to each other.

5. The extruder for producing cold film type biodegradable film according to claim 4, characterized in that: The second rod (45) and the third rod (46) are arranged in an arc shape, and the same side of the second rod (45) and the third rod (46) is serrated, and the serrated tooth tips of the second rod (45) and the third rod (46) face the disc (4).

6. The extruder for producing cold film type biodegradable film according to claim 4, characterized in that: A guide plate (47) is fixedly connected to one side of the second rod (45), and the guide plate (47) is arranged obliquely.

7. The extruder for producing cold film biodegradable film according to claim 1, characterized in that: The top of the feed barrel (2) is fixedly connected to a No. 1 cover (6), and the top cross-section of the No. 1 cover (6) is arc-shaped, and the top of the No. 1 tube (3) passes through the No. 1 cover (6); the top of the feed barrel (2) is fixedly connected to a support rod (61), and the top of the support rod (61) is fixedly connected to an electric telescopic rod (62); a sealing plate (63) is slidably connected to the inside of the No. 1 tube (3) near the top, and the sealing plate (63) is connected to the telescopic end of the electric telescopic rod (62).

8. The extruder for producing cold film biodegradable film according to claim 1, characterized in that: The baffle (5) is slidably connected to the inner wall of the feed barrel (2), and a weighing sensor (7) is provided on the inner wall of the feed barrel (2) near the bottom of the baffle (5).

Citation Information

Patent Citations

  • High-speed hot mixer for PVC plastic film production

    CN110919888A

  • Raw material adding device for producing PPR pipe fitting

    CN111136889A