Piezoelectric sensors, their driving methods and tactile feedback devices

By applying a driving signal consisting of a superposition of DC and AC voltages to the second electrode layer of the piezoelectric sensor, the internal stress of the piezoelectric thin film layer is overcome, solving the problem of insufficient vibration displacement of piezoelectric sensors in the prior art. This achieves greater vibration displacement and performance improvement, making it suitable for tactile feedback devices.

CN117203600BActive Publication Date: 2026-11-10BOE TECHNOLOGY GROUP CO LTD +1
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202280000636.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-03-31
Publication Date
2026-11-10
Estimated Expiration
2042-03-31

AI Technical Summary

Technical Problem

Existing piezoelectric sensors cannot function effectively when a symmetrical sinusoidal signal with its center at 0V is applied, resulting in unresolved internal stress in the piezoelectric thin film layer, which affects vibration displacement and performance.

Method used

By applying a grounding signal to the first electrode layer and a driving signal consisting of a superposition of DC and AC voltages to the second electrode layer, the piezoelectric thin film layer is deformed by the alternating electric field to generate force, thereby overcoming internal stress and improving vibration displacement.

Benefits of technology

It enhances the vibration displacement and performance of piezoelectric sensors, ensuring that the piezoelectric thin film layer has a large vibration amplitude under drive, making it suitable for tactile feedback devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117203600B_ABST
    Figure CN117203600B_ABST
Patent Text Reader

Abstract

This disclosure provides a piezoelectric sensor, its driving method, and a tactile feedback device. The piezoelectric sensor includes a substrate, and a first electrode layer, a piezoelectric thin film layer, and a second electrode layer located on the substrate. The first electrode layer is grounded, and the second electrode layer is coupled to a driving signal terminal. The driving method includes loading a grounding signal onto the first electrode layer and loading a driving signal consisting of a superposition of a DC voltage and an AC voltage onto the second electrode layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure relates to the field of haptic feedback technology, and in particular to a piezoelectric sensor, its driving method, and a haptic feedback device. Background Technology

[0002] Haptics is a key area of ​​technological development today. Specifically, haptic feedback enables interaction between a device and the human body through touch. Haptic feedback can be divided into two categories: vibration feedback and haptic reproduction technology.

[0003] Surface tactile reproduction technology allows users to perceive object characteristics through bare-finger touchscreens, enabling efficient and natural interaction on multimedia terminals. This technology holds significant research value and has thus garnered widespread attention from researchers both domestically and internationally. Physically, surface tactile sensation involves the interaction between the roughness of an object's surface and the skin (fingertips), resulting in varying frictional forces due to differences in surface structure. Therefore, by controlling surface friction, different tactile sensations can be simulated. Summary of the Invention

[0004] This disclosure provides a piezoelectric sensor, its driving method, and a tactile feedback device, the specific solutions of which are as follows:

[0005] This disclosure provides a driving method for a piezoelectric sensor, the piezoelectric sensor comprising: a substrate, and a first electrode layer, a piezoelectric thin film layer, and a second electrode layer located on the substrate; wherein the first electrode layer is grounded, and the second electrode layer is coupled to a driving signal terminal;

[0006] The driving method includes: applying a grounding signal to the first electrode layer and applying a driving signal consisting of a superposition of DC voltage and AC voltage to the second electrode layer.

[0007] In one possible implementation, in the driving method provided in the embodiments of this disclosure, the piezoelectric thin film layer deforms under the action of the alternating electric field formed between the first electrode layer and the second electrode layer, generating a force that satisfies the following formula:

[0008] F=μ·[a0+a1sin(ωt)]·d 33 ;

[0009] Where F is the applied force, μ is a coefficient, a0 is the DC voltage value, a1sin(ωt) is the AC voltage value, a1 is the peak value of the driving signal waveform, and d 33 is the piezoelectric constant.

[0010] In one possible implementation, in the driving method provided in the embodiments of this disclosure, a0 is greater than 0.

[0011] In one possible implementation, in the driving method provided in the embodiments of this disclosure, a0-|a1|≥0.

[0012] In one possible implementation, in the driving method provided in the embodiments of this disclosure, a0 = |a1|.

[0013] In one possible implementation, in the driving method provided in the embodiments of this disclosure, the substrate includes a flexible substrate or a glass substrate.

[0014] In one possible implementation, in the driving method provided in the embodiments of this disclosure, the thickness of the piezoelectric thin film layer is 1 μm to 10 μm.

[0015] In one possible implementation, in the driving method provided in the embodiments of this disclosure, the density of the piezoelectric thin film layer is 95% to 100%.

[0016] In one possible implementation, in the driving method provided in the embodiments of this disclosure, the piezoelectric thin film layer comprises lead zirconate titanate, and the atomic percentage ratio of the lead zirconate titanate is as follows:

[0017] Pb / (Zr+Ti)=0.9~1.1, Zr / (Zr+Ti)=48%~53%.

[0018] In one possible implementation, in the driving method provided in the embodiments of this disclosure, the DC voltage value is greater than 0.

[0019] In one possible implementation, in the driving method provided in the embodiments of this disclosure, the voltage value of the DC voltage is equal to the peak value of the AC voltage.

[0020] Accordingly, this disclosure also provides a piezoelectric sensor, which is driven by any of the driving methods described above in this disclosure; the piezoelectric sensor includes: a substrate, and a first electrode layer, a piezoelectric thin film layer and a second electrode layer located on the substrate; wherein the first electrode layer is grounded and the second electrode layer is coupled to a driving signal terminal.

[0021] In one possible implementation, the piezoelectric sensor provided in the embodiments of this disclosure further includes a first barrier layer located between the first electrode layer and the piezoelectric thin film layer, the first barrier layer being used to block ions from the piezoelectric thin film layer from diffusing to the first electrode layer.

[0022] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the material of the first barrier layer is Ti.

[0023] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the thickness of the first blocking layer is less than 10 nm.

[0024] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the transmittance of the first blocking layer is greater than or equal to 60%.

[0025] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the material of the first barrier layer includes Pt, HfO2, or LiNbO3.

[0026] In one possible implementation, the piezoelectric sensor provided in the embodiments of this disclosure further includes a second barrier layer located between the first barrier layer and the piezoelectric thin film layer. The material of the second barrier layer is different from that of the first barrier layer. The second barrier layer is used to prevent ions from the piezoelectric thin film layer from diffusing to the first electrode layer.

[0027] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the material of the second barrier layer is HfO2 or LiNbO3.

[0028] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the thickness of the second blocking layer is less than 50 nm.

[0029] In one possible implementation, the piezoelectric sensor provided in the embodiments of this disclosure further includes:

[0030] An organic insulating layer is located on the side of the second electrode layer opposite to the substrate. The organic insulating layer has a first via, and the orthographic projection of the first via on the substrate overlaps with the orthographic projection of the second electrode layer on the substrate.

[0031] An inorganic insulating layer is located on the side of the organic insulating layer opposite to the substrate, and the inorganic insulating layer does not overlap with the first via at least partially;

[0032] A wiring layer is located on the side of the inorganic insulating layer opposite to the substrate. The wiring layer includes wiring, one end of which is electrically connected to the second electrode layer through at least a portion of the first via.

[0033] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the inorganic insulating layer covers the sidewall of the first via and extends to contact the second electrode layer.

[0034] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, at the same sidewall of the first via, the contact boundary between the inorganic insulating layer and the second electrode layer is a first boundary, and the contact boundary between the organic insulating layer and the second electrode is a second boundary. The distance between the first boundary and the second boundary is greater than 30% and less than 60% of the thickness of the piezoelectric thin film layer.

[0035] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the inorganic insulating layer covers the sidewall of the first via and the second electrode layer exposed by the first via. The portion of the inorganic insulating layer covering the second electrode layer has at least one second via. One end of the trace is electrically connected to the second electrode layer through the first via and the second via.

[0036] In one possible implementation, the piezoelectric sensor provided in the embodiments of this disclosure further includes: a bonding electrode disposed in the same layer as the first electrode layer, the bonding electrode being disposed near the edge of the substrate, and the other end of the trace being electrically connected to the bonding electrode through a third via disposed on the inorganic insulating layer and the organic insulating layer, the bonding electrode being used to connect to the drive signal terminal.

[0037] In one possible implementation, the piezoelectric sensor provided in the embodiments of this disclosure has one layer of inorganic insulating layer.

[0038] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the material of the inorganic insulating layer includes SiO2, Al2O3, or Si3N4.

[0039] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the inorganic insulating layer comprises at least two sub-layers stacked together, the two sub-layers being made of different materials.

[0040] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the material of each sublayer includes SiO2, Al2O3 or Si3N4.

[0041] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the wiring layer has a mesh-like structure, and the material of the wiring layer is Ti / Ni / Au, Ti / Au, or Ti / Al / Ti.

[0042] In one possible implementation, in the piezoelectric sensor provided in the embodiments of this disclosure, the thickness of the inorganic insulating layer is 100 nm to 300 nm.

[0043] Accordingly, embodiments of this disclosure also provide a tactile feedback device, including a piezoelectric sensor as described in any of the preceding embodiments of this disclosure. Attached Figure Description

[0044] Figure 1 This is a schematic diagram of the structure of a piezoelectric sensor provided in related technologies;

[0045] Figure 2 This is a schematic diagram of the structure of a piezoelectric sensor provided in an embodiment of this disclosure;

[0046] Figure 3 This is a schematic diagram of the structure of another piezoelectric sensor provided in an embodiment of the present disclosure;

[0047] Figure 4 This is a schematic diagram of the structure of another piezoelectric sensor provided in an embodiment of the present disclosure;

[0048] Figure 5 This is a schematic diagram of the structure of another piezoelectric sensor provided in an embodiment of the present disclosure;

[0049] Figure 6 This is a schematic diagram of the structure of another piezoelectric sensor provided in an embodiment of the present disclosure;

[0050] Figure 7 This is a schematic diagram of the structure of another piezoelectric sensor provided in an embodiment of the present disclosure;

[0051] Figure 8 A schematic diagram of a driving signal provided in an embodiment of this disclosure;

[0052] Figure 9 A schematic diagram of yet another driving signal provided in an embodiment of this disclosure;

[0053] Figure 10 The relationship curve between the vibration displacement of the piezoelectric sensor and the driving signal loaded on the second electrode layer provided in the embodiments of this disclosure;

[0054] Figure 11 This is a schematic diagram illustrating the effect of vibration from a piezoelectric sensor.

[0055] Figure 12 This is a schematic diagram of the structure of a piezoelectric sensor provided in related technologies;

[0056] Figure 13 This is a schematic diagram of the structure of another piezoelectric sensor provided in related technologies;

[0057] Figure 14 This is a top view of part of the film layer in a piezoelectric sensor;

[0058] Figure 15 for Figure 14 A magnified view of a portion of the image;

[0059] Figure 16 The graphs show the vibration displacement-drive signal curves of five piezoelectric sensors under different driving conditions. Detailed Implementation

[0060] To make the objectives, technical solutions, and advantages of the embodiments of this disclosure clearer, the technical solutions of the embodiments of this disclosure will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some, not all, of the embodiments of this disclosure. Furthermore, the embodiments and features in the embodiments of this disclosure can be combined with each other without conflict. All other embodiments obtained by those skilled in the art based on the described embodiments of this disclosure without creative effort are within the scope of protection of this disclosure.

[0061] Unless otherwise defined, the technical or scientific terms used in this disclosure shall have the ordinary meaning understood by one of ordinary skill in the art to which this disclosure pertains. The terms "comprising" or "including," and similar terms as used in this disclosure, mean that an element or object preceding the term encompasses the elements or objects listed following the term and their equivalents, without excluding other elements or objects. Terms such as "connected" or "linked" are not limited to physical or mechanical connections, but may include electrical connections, whether direct or indirect. Terms such as "inner," "outer," "upper," and "lower" are used only to indicate relative positional relationships; these relative positional relationships may change accordingly when the absolute position of the described objects changes.

[0062] It should be noted that the dimensions and shapes of the figures in the accompanying drawings do not reflect actual proportions and are intended only to illustrate the content of this disclosure. Furthermore, the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout.

[0063] Thin-film piezoelectric materials possess high dielectric constants and transparency, making them ideal for sensor structures integrated into screens. Among them, lead zirconate titanate (PZT) piezoelectric ceramics are currently widely used due to their excellent piezoelectric properties. For example... Figure 1 As shown, Figure 1The structure of the PZT thin-film piezoelectric sensor includes a substrate 1 and a first electrode layer 2, a piezoelectric thin film layer 3, a second electrode layer 4, an insulating layer 5, and a wiring layer 6 located on the substrate 1. The wiring layer 6 is electrically connected to the second electrode layer 4 through a via penetrating the insulating layer 5. The piezoelectric thin film layer 3 is deposited on the first electrode layer 2 and then annealed. Due to the influence of the crystal orientation and thermal expansion coefficient of the first electrode layer 2, as well as the non-constant thermal expansion coefficient of PZT, internal stress is easily generated in the piezoelectric thin film layer 3 after annealing. If the piezoelectric thin film layer 3 is deposited on the first electrode layer 2 (ITO), and if the crystallization annealing temperature of the piezoelectric thin film layer 3 is 500℃-700℃, considering the influence of the thermal expansion coefficient, a tensile stress exists on the PZT / ITO interface after returning to room temperature (indicated by the arrow). Generally, the driving mechanism of a PZT thin film piezoelectric sensor is to apply a ground signal to the first electrode layer 2 and a sine wave signal with a symmetrical signal center at 0V to the second electrode layer 4. Since the tensile stress on the PZT / ITO interface greatly affects the operation of the PZT thin film piezoelectric sensor (actuator), if the second electrode layer 4 is still applied with a sine wave signal with a symmetrical signal center at 0V, the PZT thin film piezoelectric sensor will not work effectively.

[0064] In view of this, embodiments of this disclosure provide a method for driving a piezoelectric sensor, such as... Figures 2-7 As shown, the piezoelectric sensor includes: a substrate 1, and a first electrode layer 2, a piezoelectric thin film layer 3, and a second electrode layer 4 located on the substrate 1; wherein, the first electrode layer 2 is grounded, and the second electrode layer 4 is coupled to a drive signal terminal.

[0065] Used for driving Figures 2-7 The driving method of the piezoelectric sensor shown includes: applying a ground signal to the first electrode layer 2 and applying a DC voltage V to the second electrode layer 4. dc and AC voltage V dc The superimposed driving signal V, such as Figure 8 As shown, V dc =a0, AC voltage V AC The peak value is a1.

[0066] The driving method provided in this embodiment applies a DC voltage V to the second electrode layer 4 of the piezoelectric sensor. dc and AC voltage V AC Superimposed drive signal V, DC voltage V dc This allows for the preferential orientation of electric domains within the piezoelectric thin film layer, overcoming the stress within the layer and thus overcoming the constraints of the substrate 1. This enables the piezoelectric thin film layer to operate under DC voltage V. dc and AC voltage V AC The superimposed driving signal V results in a large vibration displacement, which can improve the performance of the piezoelectric sensor.

[0067] It should be noted that, in this embodiment, a ground signal is applied to the first electrode layer 2 close to the substrate 1, and a DC voltage V is applied to the second electrode layer 4 far from the substrate 1. dc and AC voltage V dc Taking the superimposed driving signal V as an example, in specific implementations, a ground signal can also be applied to the second electrode layer 4, which is farther away from the substrate 1, and a DC voltage V can be applied to the first electrode layer 2, which is closer to the substrate 1. dc and AC voltage V dc Superimposed driving signal V.

[0068] In specific implementations, the substrate 1 provided in the embodiments of this disclosure may include a flexible substrate (e.g., PI) or a glass substrate.

[0069] Of course, in specific implementation, the substrate 1 can also be a substrate made of silicon or silicon dioxide (SiO2), a substrate made of sapphire, or a substrate made of metal wafers. There are no limitations here. Those skilled in the art can set the substrate 1 according to the actual application needs.

[0070] In specific implementations, the fabrication process of the piezoelectric thin film layer 3 provided in this disclosure embodiment can be a vapor deposition process (CVD), a sputtering process, or a sol-gel process.

[0071] In specific implementations, the thickness of the piezoelectric thin film layer 3 provided in this embodiment can be 1 μm to 10 μm.

[0072] In specific implementations, the density of the piezoelectric thin film layer 3 provided in this embodiment is 95% to 100%.

[0073] In specific implementations, the material of the piezoelectric thin film layer 3 provided in this embodiment may include lead zirconate titanate (Pb(Zr,Ti)O3, PZT), and the atomic percentage ratio of lead zirconate titanate is as follows:

[0074] Pb / (Zr+Ti) = 0.9~1.1, Zr / (Zr+Ti) = 48%~53%. The piezoelectric thin film layer 3 formed in this way has an excellent piezoelectric coefficient, which ensures the piezoelectric characteristics of the corresponding piezoelectric sensor.

[0075] In specific implementations, the piezoelectric thin film layer 3 is not limited to the PZT mentioned above, but can also be aluminum nitride (AlN), ZnO (zinc oxide), barium titanate (BaTiO3), lead titanate (PbTiO3), potassium niobate (KNbO3), lithium niobate (LiNbO3), lithium tantalate (LiTaO3), or lanthanum gallium silicate (La3Ga5SiO3).14 At least one of the following can be used, and the specific material for fabricating the piezoelectric thin film layer can be selected according to the actual needs of those skilled in the art, without limitation. Among them, when using PZT to fabricate the piezoelectric thin film layer, since PZT has a high piezoelectric coefficient, it ensures the piezoelectric characteristics of the corresponding piezoelectric sensor, and the corresponding piezoelectric sensor can be applied to haptic feedback devices. Moreover, PZT has high light transmittance, so when it is integrated into a display device, it does not affect the display quality of the display device.

[0076] In specific implementation, in the driving method provided in the embodiments of this disclosure, such as Figures 2-7 As shown, due to the application of a ground signal to the first electrode layer 2, a DC voltage V is applied to the second electrode layer 4. dc and AC voltage V dc The superimposed driving signal V creates an alternating electric field between the first electrode layer 2 and the second electrode layer 4. Under the action of the alternating electric field between the first electrode layer 2 and the second electrode layer 4, the piezoelectric thin film layer 3 deforms and generates a force F, which satisfies the following formula:

[0077] F=μ·[a0+a1sin(ωt)]·d 33 ;

[0078] Where μ is a coefficient, a0 is the applied DC voltage value, a1sin(ωt) is the applied AC voltage value, a1 is the peak value of the drive signal waveform, and d 33 is the piezoelectric constant.

[0079] Specifically, the force F can be determined based on the tactile feedback effect required by the user, and then the driving signal V that needs to be applied to the second electrode layer 4 can be determined based on the force F, thereby determining a0 and a1.

[0080] Specifically, the peak value of a driving signal waveform (generally a sinusoidal waveform) is the maximum value relative to the 0-point scale, and can be positive or negative. The peak-to-peak value of the driving signal waveform is the difference between the maximum and minimum values, and can only be positive. The peak-to-peak value describes the magnitude of the signal value's range of variation. The relationship between peak-to-peak value and peak value: The peak value refers to the difference between the highest or lowest value of the signal and the average value within one period. Generally, the peak value is only defined for signals that are symmetrical vertically. That is, the peak value is equal to half the peak-to-peak value.

[0081] In specific implementation, in the driving method provided in the embodiments of this disclosure, such as Figure 8 As shown, the DC voltage V dcThe voltage value a0 is greater than 0. Compared to related technologies that only apply an AC voltage signal to the second electrode layer 4, the driving method provided in this embodiment can preferentially orient the electric domains inside the piezoelectric thin film layer 3, overcome the stress inside the piezoelectric thin film layer 3, and enable the piezoelectric thin film layer 3 to operate under DC voltage V. dc and AC voltage V AC The superimposed driving signal V results in a large vibration displacement, which improves the performance of the piezoelectric sensor.

[0082] In practical implementation, in order to further improve the vibration displacement of the piezoelectric thin film layer, in the driving method provided in the embodiments of this disclosure, the DC voltage V dc The voltage value a0 satisfies: a0-|a1|≥0.

[0083] In specific implementation, in the driving method provided in the embodiments of this disclosure, such as Figure 9 As shown, the DC voltage V dc The voltage value a0 and the AC voltage V AC When the peak value a1 satisfies a0=|a1|, the piezoelectric sensor can obtain the best driving effect, and the vibration displacement of the piezoelectric thin film layer 3 is the largest.

[0084] like Figure 10 As shown, Figure 10 The relationship curve between the vibration displacement (nm) of the piezoelectric sensor and the driving signal (V) applied to the second electrode layer provided in the embodiments of this disclosure, wherein V PP (Voltage Peak-Peak) is the peak-to-peak voltage. In this embodiment of the disclosure, V... PP When 2a1 = 2a0, the vibrational displacement of the piezoelectric thin film layer 3 is relatively large. From Figure 10 It can be seen that point A represents applying an AC voltage signal only to the second electrode layer 4, while point B represents applying a DC voltage of 5V and an AC voltage signal (V) simultaneously to the second electrode layer 4. PP =10V) driving signal, point C indicates that a DC voltage of 5V and an AC voltage signal (V) are simultaneously applied to the second electrode layer 4. PP =14V) driving signal, point D indicates that a DC voltage of 8V and an AC voltage signal (V) are simultaneously applied to the second electrode layer 4. PP =16V) driving signal, point E indicates that a DC voltage of 10V and an AC voltage signal (V) are simultaneously applied to the second electrode layer 4. PP =20V) driving signal, point F indicates that a DC voltage of 12V and an AC voltage signal (V) are simultaneously applied to the second electrode layer 4. PP=24V) driving signal, where B, D, E, and F are the vibration displacement changes of the piezoelectric thin film layer when a0 = a1. It can be seen that compared to point A where only AC voltage is applied, the piezoelectric thin film layers corresponding to B, D, E, and F have larger vibration displacements. The vibration displacements of B and C do not change because a0 at point C is less than a1. Therefore, only when a0 = a1 does the piezoelectric thin film layer have a large vibration displacement, such as Figure 11 As shown, Figure 11 This is a schematic diagram of the vibration effect of a piezoelectric sensor obtained by laser vibration measurement.

[0085] In summary, the embodiments of this disclosure simultaneously apply a driving signal consisting of a superimposed DC voltage and an AC voltage to the second electrode layer, wherein the DC voltage value is equal to the AC voltage V. AC When the peak value a1 is reached, the piezoelectric thin film layer has a large vibration displacement, thereby improving the performance of the piezoelectric sensor.

[0086] The specific structure of the piezoelectric sensor provided in the embodiments of this disclosure is described below:

[0087] This disclosure provides an embodiment of a piezoelectric sensor, such as... Figures 2-7 As shown, the piezoelectric sensor is driven by the aforementioned piezoelectric sensor driving method, which enables the piezoelectric sensor to have a large vibration displacement; the piezoelectric sensor includes: a substrate 1, and a first electrode layer 2, a piezoelectric thin film layer 3 and a second electrode layer 4 located on the substrate 1; wherein, the first electrode layer 2 is grounded and the second electrode layer 4 is coupled to the driving signal terminal.

[0088] There are many methods for fabricating piezoelectric thin film layers (PZT), including dry deposition (sputtering) and wet deposition (sol-gel method). However, to achieve good piezoelectric constant characteristics, PZT materials need to undergo a high-temperature annealing process. This process requires PZT grain growth in an air environment at 550℃-650℃ to form a good solid solution phase. When integrating the oscillator structure into a display device, in order not to affect the display quality, the oscillator structure needs to use a transparent electrode (such as ITO) as the base electrode and growth layer. However, the following problems exist: Firstly, since ITO mainly conducts electricity through oxygen vacancies, but PZT is a perovskite phase and requires sufficient grain size to form piezoelectric properties, PZT requires high-temperature oxygen annealing. This annealing process will cause a significant increase in ITO resistance, an increase in circuit resistance, and a decrease in conductivity, which is not conducive to high-frequency driving of the device. Furthermore, because Pb ions in PZT have a very small ionic radius, they easily diffuse between oxides. Once a PZT film is directly fabricated on ITO, under different high-temperature annealing processes, as verified by the inventors of this invention, Pb ions diffuse by approximately 100 nm. This diffusion not only increases the resistance of ITO but also leads to Pb ion deficiency in the PZT film, causing the perovskite phase to transition to the pyrochlore phase, reducing the piezoelectric properties of PZT, and thus reducing the performance of the piezoelectric device. Therefore, in the piezoelectric sensor provided in the embodiments of this disclosure, as... Figure 2 As shown, it also includes a first barrier layer 7 located between the first electrode layer 2 and the piezoelectric thin film layer 3, the first barrier layer 7 being used to block the diffusion of ions from the piezoelectric thin film layer 3 to the first electrode layer 2.

[0089] The piezoelectric sensor provided in this embodiment of the invention uses a piezoelectric thin film layer 3 (e.g., PZT) that can be formed by dry or wet deposition. However, to achieve good piezoelectric constant characteristics, the PZT material needs to undergo a high-temperature annealing process. This process requires PZT grain growth in an air environment at 550℃-650℃ to form a good solid solution phase. Since the first electrode layer 2 (e.g., ITO) mainly conducts electricity through oxygen vacancies, during the high-temperature annealing process, oxygen in PZT diffuses to the oxygen vacancy sites in ITO, causing an increase in ITO resistance (a decrease in conductivity), which is detrimental to high-frequency drive of the device. Furthermore, due to the small radius of Pb ions, Pb ions easily diffuse between oxides. This diffusion not only increases the ITO resistance but also causes Pb ion deficiency in the PZT film, causing the phase to transition to pyrochlore, thereby reducing the piezoelectric performance of PZT. In this embodiment, a first barrier layer 7 is provided between the piezoelectric thin film layer 3 and the first electrode layer 2. The first barrier layer 7 can prevent ions (e.g., O, Pb) in the piezoelectric thin film layer 3 from diffusing into the first electrode layer 2. Thus, when the piezoelectric thin film layer 3 is subjected to a high-temperature annealing process, the conductivity of ITO can be maintained while preventing Pb from diffusing into ITO, and the PZT perovskite crystalline phase can be easily maintained, thereby improving the piezoelectric performance of the piezoelectric thin film layer 3.

[0090] It should be noted that the first electrode layer may include a patterned plurality of first electrodes, or it may be a structure of an entire surface; the second electrode layer includes a patterned plurality of second electrodes.

[0091] In specific implementation, the first electrode layer 2 and the second electrode layer 4 can be made of indium tin oxide (ITO), or indium zinc oxide (IZO), or of course, one of titanium-gold (Ti-Au) alloy, titanium-aluminum-titanium (Ti-Al-Ti) alloy, or titanium-molybdenum (Ti-Mo) alloy. In addition, they can be made of one of titanium (Ti), gold (Au), silver (Ag), molybdenum (Mo), copper (Cu), tungsten (W), or chromium (Cr). Those skilled in the art can set the above-mentioned first electrode layer and second electrode layer according to the actual application needs, and there is no limitation here.

[0092] In specific implementations, in the piezoelectric sensor provided in the embodiments of this disclosure, such as Figure 2 As shown, the material of the first barrier layer 7 can be Ti, because Ti has stable properties, is a metal that is not easily oxidized at high temperatures, and has a relatively thin thickness after the first barrier layer 7 is formed.

[0093] In specific implementation, in order to ensure the transparency of the piezoelectric sensor, the thickness of the first barrier layer in the piezoelectric sensor provided in the embodiments of this disclosure is less than 10nm, such as 9nm, 8nm, 7nm, 6nm, 5nm, 4nm, etc.

[0094] In specific implementations, in the piezoelectric sensor provided in the embodiments of this disclosure, such as Figure 2 As shown, the transmittance of the first blocking layer 7 is greater than or equal to 60%, such as 60%, 70%, 80%, 90%, etc. Thus, when the piezoelectric sensor of this disclosure is integrated into a display device, the display quality of the display device is not affected.

[0095] In specific implementations, in the piezoelectric sensor provided in the embodiments of this disclosure, such as Figure 2 As shown, the material of the first barrier layer 7 may also include Pt, HfO2 or LiNbO3, but is not limited to these.

[0096] In practical implementation, although the first barrier layer 7 made of Ti can prevent most of the ions in PZT from diffusing to the first electrode layer 2, in order to further improve the conductivity of the first electrode layer 2 and the piezoelectric properties of the piezoelectric thin film layer 3, in the piezoelectric sensor provided in the embodiments of this disclosure, such as... Figure 3 As shown, it also includes a second barrier layer 8 located between the first barrier layer 7 and the piezoelectric thin film layer 3. The material of the second barrier layer 8 is different from that of the first barrier layer 7. The second barrier layer 8 is used to further block the diffusion of ions from the piezoelectric thin film layer 3 to the first electrode layer 2.

[0097] In specific implementations, in the piezoelectric sensor provided in the embodiments of this disclosure, the material of the second barrier layer can be HfO2 or LiNbO3.

[0098] Specifically, when the material of the second barrier layer is HfO2, HfO2 can be used as a seed layer. For film growth, if orientation is required, a seed layer is always needed. In this way, when a piezoelectric material layer is subsequently fabricated on the second barrier layer, the crystal orientation of the piezoelectric material layer will be related to the orientation of the second barrier layer, which is beneficial to the crystal orientation of the piezoelectric material layer and improves the piezoelectric performance of the piezoelectric material layer.

[0099] Specifically, when the material of the second barrier layer is LiNbO3 (abbreviated as LNO), LiNbO3 can also be used as a seed layer. Since LiNbO3 itself is conductive, compared with HfO2, LiNbO3 can further improve conductivity while preventing the diffusion of Pb and O.

[0100] When fabricating piezoelectric material layers (such as PZT) using dry or wet processes, micropores will inevitably be present in the process. Once there are pores in the PZT, the first electrode layer and the second electrode layer will connect, forming a short circuit. Since LNO is a conductor, using HfO2 as a second barrier layer is more effective than using LNO as a second barrier layer in preventing short circuits between the first and second electrode layers when pores are formed in the PZT layer.

[0101] Therefore, HfO2 or LiNbO3 can be selected as the second barrier layer according to actual needs.

[0102] In specific implementations, in the piezoelectric sensor provided in the embodiments of this disclosure, the thickness of the second barrier layer is less than 50nm, for example, 40nm, 30nm, 20nm, or 10nm.

[0103] like Figure 12 As shown, Figure 12 The piezoelectric sensor structure in the related technology includes a substrate 1 and a first electrode layer 2, a piezoelectric thin film layer 3, a second electrode layer 4, an insulating layer 5, and a wiring layer 6 sequentially stacked on the substrate 1. The wiring layer 6 is electrically connected to the second electrode layer 4 through a via penetrating the insulating layer 5. The structure also includes an insulating layer 5 located on the side of the second electrode layer 4 facing away from the substrate 1, and a wiring layer 6 located on the side of the insulating layer 5 facing away from the substrate 1. The wiring layer 6 is electrically connected to the second electrode layer 4 through a via penetrating the insulating layer 5. The insulating layer 5 is made of an inorganic material. The first electrode layer 2 is grounded, and the wiring layer 6 is connected to a drive signal terminal. To avoid short circuits, an insulating layer 5 is required between the second electrode layer 4 and the wiring layer 6. However, the fabrication process of the piezoelectric thin film layer 3 (e.g., PZT material) generally includes dry etching and wet etching. The piezoelectric thin film layer 3 includes a bottom edge aa that contacts the first electrode layer 2 and a side edge bb adjacent to the bottom edge aa. When using wet etching, the piezoelectric thin film layer 3 is very prone to forming a chamfered structure (i.e., an angle θ is formed between the side edge bb and the first electrode layer 2), which is generally 60° to 85°. When using dry etching, the angle θ between the side edge bb and the first electrode layer 2 is generally 85° to 95°. It should be noted that the embodiment disclosed herein uses wet etching to fabricate the piezoelectric thin film layer 3 as an example, i.e., the angle θ between the side edge bb and the first electrode layer 2 is generally 60° to 85°. Figure 12 The inorganic insulating layer 5 between the trace layer 6 and the second electrode layer 4 cannot fill the chamfered structure (θ) of the piezoelectric thin film layer 3, which easily leads to the risk of trace breakage in the trace layer 6. Therefore, if... Figure 13 As shown, an organic insulating layer 10 is used to fill the chamfer (θ) of the piezoelectric thin film layer 3 between the wiring layer 6 and the second electrode layer 4. However, due to the poor adhesion between the organic insulating layer 10 and the wiring layer 6, the wiring layer 6 is prone to detachment (e.g., ...). Figure 13 (As shown). Therefore, in specific implementations, in the piezoelectric sensor provided in the embodiments of this disclosure, as... Figures 4-7 As shown, the piezoelectric sensor also includes:

[0104] An organic insulating layer 10 is located on the side of the second electrode layer 4 away from the substrate 1. The organic insulating layer 10 has a first via V1. The orthographic projection of the first via V1 on the substrate 1 overlaps with the orthographic projection of the second electrode layer 4 on the substrate 1.

[0105] The inorganic insulating layer 20 is located on the side of the organic insulating layer 10 away from the substrate 1, and the inorganic insulating layer 20 does not overlap with the first via V1 at least partially.

[0106] The wiring layer 6 is located on the side of the inorganic insulating layer 20 away from the substrate 1. The wiring layer 6 includes wiring, one end of which is electrically connected to the second electrode layer 4 through at least a portion of the first via V1.

[0107] This disclosure embodiment Figures 4-7 By setting an inorganic insulating layer 20 between the wiring layer 6 and the organic insulating layer 10, the inorganic insulating layer 20 has strong adhesion to the wiring layer 6. Based on the fact that the organic insulating layer 10 solves the chamfering problem of the piezoelectric thin film layer 3, the inorganic insulating layer 20 can solve the problem of poor adhesion between the organic insulating layer 10 and the wiring layer 6, thereby preventing the wiring layer 6 from falling off.

[0108] In specific implementations, in the piezoelectric sensor provided in the embodiments of this disclosure, such as Figure 4 and Figure 6 As shown, the inorganic insulating layer 20 covers the sidewall of the first via V1 and extends to contact the second electrode layer 4. Due to the influence of the manufacturing process, the cross-section of the first via V1 along the thickness direction of the piezoelectric sensor is generally an inverted trapezoidal structure. By setting the inorganic insulating layer 20 to cover the sidewall of the first via V1 and extend to contact the second electrode layer 4, the inorganic insulating layer 20 has a buffering effect within the first via V1, so that the subsequent fabricated wiring layer 6 will not experience a breakage problem at the first via V1.

[0109] In specific implementations, in the piezoelectric sensor provided in the embodiments of this disclosure, such as Figure 4 and Figure 6As shown, at the first via V1, the contact boundary between the inorganic insulating layer 20 and the second electrode layer 4 is the first boundary, and the contact boundary between the organic insulating layer 10 and the second electrode layer 4 is the second boundary. The distance d between the first boundary and the second boundary can be greater than 30% and less than 60% of the thickness of the piezoelectric thin film layer 3. Specifically, since the thickness of the piezoelectric thin film layer 3 is generally 1μm to 10μm, for example, the thickness of the piezoelectric thin film layer 3 is 1μm, 2μm, 3μm, 4μm, 5μm, 6μm, 7μm, 8μm, 9μm, or 10μm. For example, taking the thickness of the piezoelectric thin film layer 3 as 3μm, then d is greater than 0.9μm and less than 1.8μm; taking the thickness of the piezoelectric thin film layer 3 as 6μm, then d is greater than 1.8μm and less than 3.6μm; taking the thickness of the piezoelectric thin film layer 3 as 9μm, then d is greater than 2.7μm and less than 5.4μm; and so on.

[0110] In practical implementation, since the wiring layer is generally made of metal and the second electrode layer is generally made of indium tin oxide (ITO), the adhesion between the metal and ITO is poor. To prevent peeling between the wiring layer and the second electrode layer, which could prevent the transmission of electrical signals, the piezoelectric sensor provided in this embodiment of the present disclosure, such as... Figure 5 and Figure 7 As shown, the inorganic insulating layer 20 covers the sidewall of the first via V1 and the exposed second electrode layer 4. The portion of the inorganic insulating layer 20 covering the second electrode layer 4 has at least one second via V2. One end of the trace (6) is electrically connected to the second electrode layer 4 through the first via V1 and the second via V2. In this way, the trace layer 6 is partially in contact with the inorganic insulating layer 20 and partially electrically connected to the second electrode layer 4 through the first via V1 and the second via V2. Since the adhesion between the trace layer 6 and the inorganic insulating layer 20 is strong, the adhesion between the trace layer 6 and the second electrode layer 4 can be improved while ensuring the electrical connection between the trace layer 6 and the second electrode layer 4.

[0111] In specific implementations, in the piezoelectric sensor provided in the embodiments of this disclosure, such as Figures 4-7As shown, it also includes: a bonding electrode 30 disposed in the same layer as the first electrode layer 2. The bonding electrode 30 is disposed close to the edge of the substrate 1. The other end of the trace (6) is electrically connected to the bonding electrode 30 through a third via V3 disposed on the inorganic insulating layer 20 and the organic insulating layer 10. The bonding electrode 30 is used to connect to the drive signal terminal. Specifically, a drive signal consisting of a superposition of DC voltage and AC voltage is applied to the second electrode layer 4 through the drive voltage input terminal. In this way, an alternating electric field can be formed between the first electrode layer 2 and the second electrode layer 4. The frequency of the alternating electric field is the same as the frequency of the AC voltage signal. Under the action of the alternating electric field, the piezoelectric thin film layer 3 deforms and generates a vibration signal. The frequency of this vibration signal is the same as the frequency of the alternating electric field. When the frequency of the vibration signal is close to or equal to the natural frequency of the substrate, the substrate resonates, the amplitude is enhanced, and a tactile feedback signal is generated. When a finger touches the surface of the substrate, the change in friction force can be clearly felt. In practical applications, the friction force on the surface of the substrate can be adjusted by the resonance generated between the piezoelectric thin film layer and the substrate, thereby realizing the reproduction of the texture of the object on the surface of the substrate.

[0112] In practical implementation, to make it clearer... Figure 5 The middle routing layer is electrically connected to the second electrode layer 4 through the second via V2, such as... Figure 14 and Figure 15 As shown, Figure 14 This is a top view of the second electrode layer 4, the second via V2, and the routing layer 6. Figure 15 for Figure 14 The enlarged schematic diagram within the dashed box shows that piezoelectric sensors are generally combined with display devices to achieve tactile reproduction. In order to improve the transmittance of the piezoelectric sensor, the shape of the wiring layer 6 can be a grid structure. Each grid line of the grid structure corresponds to multiple second vias V2 on the inorganic insulating layer 20 below, so that the wiring layer 6 can be electrically connected to the second electrode layer 4 through the second vias V2.

[0113] In specific implementations, in the vibration panel provided in the embodiments of this disclosure, the material of the wiring layer can be Ti / Ni / Au, where Ti can be 10nm, Ni can be 400nm, and Au can be 100nm; or, the material of the wiring layer can be Ti / Au, where Ti can be 10nm and Au can be 400nm; or, the material of the wiring layer can be Ti / Al / Ti, where Ti can be 10nm and Al can be 300nm.

[0114] In specific implementations, in the piezoelectric sensor provided in the embodiments of this disclosure, such as Figure 4 and Figure 5As shown, the number of inorganic insulating layers 20 can be one. Specifically, the material of the inorganic insulating layer 20 can be at least one of SiO2, Al2O3, or Si3N4.

[0115] In specific implementation, in the touch panel provided in the embodiments of this disclosure, such as Figure 6 and Figure 7 As shown, the inorganic insulating layer 20 may include at least two sub-insulating layers (21 and 22) stacked together, with the two sub-insulating layers (21 and 22) made of different materials. This allows the outermost sub-insulating layer 22 to be made of a material with good adhesion to the wiring layer 6, depending on the material of the wiring layer 6. Specifically, the materials of each sub-insulating layer (21 and 22) may include, but are not limited to, SiO2, Al2O3, or Si3N4. For example, if the material of the wiring layer 6 is Cr, then the material of the outermost sub-insulating layer 22 may be Si3N4.

[0116] In specific implementation, in the vibration panel provided in the embodiments of this disclosure, such as Figures 4-7 As shown, the thickness of the inorganic insulating layer 20 can be 100nm to 300nm, for example, the thickness of the inorganic insulating layer 20 can be 100nm, 200nm or 300nm.

[0117] To reduce the risk of short circuits, refer to Figures 2-7 The edge of the second electrode layer 4 can be recessed relative to the edge of the piezoelectric thin film layer 3. In a specific implementation, the recess of the edge of the second electrode layer 4 relative to the edge of the piezoelectric thin film layer 3 is greater than or equal to 100 micrometers and less than or equal to 500 micrometers. For example, the recess can be 150 micrometers.

[0118] To further reduce the risk of short circuits, the edge of the piezoelectric thin film layer 3 can be recessed relative to the edge of the first electrode layer 2.

[0119] It should be noted that the embodiments provided in this disclosure... Figure 2 Only in Figure 1 Based on this, a first barrier layer 7 is set. Figure 3 Only in Figure 1 Based on this, a first barrier layer 7 and a second barrier layer 8 are set. Figures 4-7 Is Figure 13 An inorganic insulating layer is set between the organic insulating layer and the wiring layer. Of course, in specific implementation, the setting scheme of the barrier layer can be superimposed with the setting scheme of the organic insulating layer and the inorganic insulating layer. That is, a first barrier layer and / or a second barrier layer can be set between the first electrode layer and the piezoelectric film layer, while an inorganic insulating layer and an organic insulating layer are set between the second electrode layer and the wiring layer. The setting is selected according to actual needs.

[0120] The inventors of this case have driven several piezoelectric sensors with different structures provided in the embodiments of this disclosure using the aforementioned driving method for a piezoelectric sensor.

[0121] The structures of the five piezoelectric sensors provided in this disclosure are as follows:

[0122] 1. Glass / ITO / PZT / ITO, the thickness of each film layer is: 500um / 500nm / 2000nm / 250nm.

[0123] 2. Glass / ITO / Ti / PZT / ITO, the thickness of each film layer is: 500um / 250nm / 5-10nm / 2000nm / 250nm.

[0124] 3. Glass / ITO / LNO / PZT / ITO, the thickness of each film layer is: 500um / 250um / 100-200nm / 2000nm / 250nm.

[0125] 4. Glass / ITO / Pt / PZT / ITO, the thickness of each film layer is: 500um / 250nm / 100nm / 2000nm / 250nm.

[0126] 5. Glass / ITO / HfO2 / PZT / ITO, the thickness of each film layer is: 500um / 10-20nm / 2000nm / 250nm.

[0127] In the above structures, Glass represents the substrate, the two ITOs represent the first electrode layer and the second electrode layer, respectively, PZT represents the piezoelectric thin film layer, and Ti, LNO, Pt and HfO2 all represent the first barrier layer.

[0128] When driving the above five types of piezoelectric sensors, the first electrode layer is grounded, and the second electrode layer is loaded with a signal consisting of a superposition of DC and AC voltages, where the DC voltage value is equal to the peak value of the AC voltage. Figure 16 As shown, Figure 16 The graphs show the vibration displacement-drive signal curves of five piezoelectric sensors under different driving conditions. It can be seen that by applying a signal of superimposed DC voltage and AC voltage to the second electrode layer provided in this embodiment to drive the piezoelectric sensor, the piezoelectric thin film layer can obtain a large vibration displacement, thereby improving the performance of the piezoelectric sensor.

[0129] Exemplary examples provided by embodiments of this disclosure Figure 4 Taking a piezoelectric sensor as an example, the fabrication Figure 4 The piezoelectric sensor shown may include the following steps:

[0130] First, a first electrode layer, a piezoelectric thin film material layer, and a second electrode layer are sequentially formed on a substrate.

[0131] Specifically, the first electrode layer may include a patterned plurality of first electrodes, or it may be a structure of an entire surface; the second electrode layer includes a patterned plurality of second electrodes.

[0132] Secondly, the piezoelectric thin film material layer is subjected to polarization treatment;

[0133] Specifically, a strong DC electric field is applied to the piezoelectric thin film material layer, causing the dipole moments in the piezoelectric thin film material layer to form an ordered arrangement, thus creating pre-polarization characteristics. Generally, polarization involves grounding the first electrode layer (0V / GND) and applying a DC voltage to the second electrode layer. The DC voltage application process can be performed between room temperature and 120°C, with a DC voltage >15V and a polarization time >5 minutes. This polarization process can further improve the performance of the PZT mobile thin film layer.

[0134] Next, the polarized piezoelectric thin film material layer is patterned to form a piezoelectric thin film layer located between the first electrode layer and the second electrode layer.

[0135] Specifically, patterned piezoelectric thin film layers can be formed using dry deposition (sputter) or wet deposition (sol-gel).

[0136] Next, an organic insulating layer is formed on the side of the second electrode layer away from the substrate. The organic insulating layer has a first via, and the orthographic projection of the first via on the substrate overlaps with the orthographic projection of the second electrode layer on the substrate.

[0137] Next, an inorganic insulating layer is formed on the side of the organic insulating layer that is away from the substrate, and the inorganic insulating layer does not overlap with the first via at least partially.

[0138] Next, a wiring layer is formed on the side of the inorganic insulating layer away from the substrate, and the wiring layer is electrically connected to the second electrode layer through at least a portion of the first via.

[0139] It should be noted that when fabricating the structures of other piezoelectric sensors provided in the embodiments of this disclosure, the piezoelectric thin film material layer needs to be polarized before forming the patterned piezoelectric thin film layer.

[0140] The piezoelectric sensor provided in this disclosure can be applied in fields such as medical, automotive electronics, and motion tracking systems. It is particularly suitable for wearable devices, external or implantable medical monitoring and treatment, or applications in fields such as artificial intelligence-based electronic skin. Specifically, the piezoelectric sensor can be applied to devices that generate vibration and mechanical properties, such as brake pads, keyboards, mobile terminals, game controllers, and automotive components.

[0141] Based on the same inventive concept, this disclosure also provides a haptic feedback device, including the piezoelectric sensor described above. Since the principle by which this haptic feedback device solves the problem is similar to that of the aforementioned piezoelectric sensor, the implementation of this haptic feedback device can refer to the implementation of the aforementioned piezoelectric sensor, and repeated details will not be elaborated further. This haptic feedback device can be any product or component with display or touch functionality, such as a mobile phone, tablet computer, television, monitor, laptop computer, digital photo frame, or navigator.

[0142] In specific implementations, the tactile feedback device provided in the embodiments of this disclosure may also include other functional structures well known to those skilled in the art, which will not be described in detail here.

[0143] In practical implementation, haptic feedback devices can be integrated with touchscreens. The touchscreen can determine the location of the human touch, thereby generating corresponding vibration waveforms, amplitudes, and frequencies, enabling human-computer interaction. Alternatively, a piezoelectric sensor within the haptic feedback device can determine the location of the human touch, generating corresponding vibration waveforms, amplitudes, and frequencies, also enabling human-computer interaction. Of course, haptic feedback devices can also be applied in fields such as medical care, automotive electronics, and motion tracking systems, depending on specific needs, which will not be detailed here.

[0144] This disclosure provides a piezoelectric sensor, its driving method, and a tactile feedback device. By applying a driving signal consisting of a superimposed DC voltage and an AC voltage to the second electrode layer of the piezoelectric sensor, the DC voltage can preferentially orient the electric domains inside the piezoelectric thin film layer, overcome the stress inside the piezoelectric thin film layer, and thus overcome the constraint of the substrate. This allows the piezoelectric thin film layer to have a large vibration displacement under the driving signal consisting of the superimposed DC voltage and AC voltage, thereby improving the performance of the piezoelectric sensor.

[0145] Although preferred embodiments of this disclosure have been described, those skilled in the art, upon learning the basic inventive concept, can make other changes and modifications to these embodiments. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments as well as all changes and modifications falling within the scope of this disclosure.

[0146] Obviously, those skilled in the art can make various modifications and variations to the embodiments of this disclosure without departing from the spirit and scope of the embodiments of this disclosure. Therefore, if these modifications and variations to the embodiments of this disclosure fall within the scope of the claims of this disclosure and their equivalents, this disclosure is also intended to include these modifications and variations.

Claims

1. A driving method for a piezoelectric sensor, wherein, The piezoelectric sensor includes: a substrate, and a first electrode layer, a piezoelectric thin film layer, and a second electrode layer located on the substrate; wherein the first electrode layer is grounded, and the second electrode layer is coupled to a drive signal terminal; The driving method includes: loading a grounding signal onto the first electrode layer and loading a driving signal consisting of a superposition of DC voltage and AC voltage onto the second electrode layer; The piezoelectric thin film layer deforms and generates a force under the action of the alternating electric field formed between the first electrode layer and the second electrode layer. The force satisfies the following formula: F=µ [a0+a1sin(ωt)] d 33 ; Where F is the applied force, µ is a coefficient, a0 is the DC voltage value, a1sin(ωt) is the AC voltage value, a1 is the peak value of the driving signal waveform, and d 33 is the piezoelectric constant.

2. The driving method as described in claim 1, wherein, a0 is greater than 0.

3. The driving method as described in claim 2, wherein, a0-|a1|≥0.

4. The driving method as described in claim 3, wherein, a0 = |a1|.

5. The driving method according to any one of claims 1-4, wherein, The substrate includes a flexible substrate or a glass substrate.

6. The driving method according to any one of claims 1-5, wherein, The thickness of the piezoelectric thin film layer is 1 μm to 10 μm.

7. The driving method according to any one of claims 1-6, wherein, The density of the piezoelectric thin film layer is 95% to 100%.

8. The driving method according to any one of claims 1-7, wherein, The piezoelectric thin film layer comprises lead zirconate titanate, and the atomic percentage ratios of the lead zirconate titanate are as follows: Pb / (Zr+Ti)=0.9~1.1, Zr / (Zr+Ti)=48%~53%.

9. A piezoelectric sensor, wherein, The piezoelectric sensor is driven by the driving method described in any one of claims 1-8; the piezoelectric sensor includes: a substrate, and a first electrode layer, a piezoelectric thin film layer and a second electrode layer located on the substrate; wherein the first electrode layer is grounded and the second electrode layer is coupled to a driving signal terminal.

10. The piezoelectric sensor as claimed in claim 9, wherein, It also includes a first barrier layer located between the first electrode layer and the piezoelectric thin film layer, the first barrier layer being used to prevent ions from the piezoelectric thin film layer from diffusing into the first electrode layer.

11. The piezoelectric sensor as claimed in claim 10, wherein, The material of the first barrier layer is Ti.

12. The piezoelectric sensor as claimed in claim 11, wherein, The thickness of the first barrier layer is less than 10 nm.

13. The piezoelectric sensor as claimed in claim 11, wherein, The transmittance of the first barrier layer is greater than or equal to 60%.

14. The piezoelectric sensor as claimed in claim 10, wherein, The material of the first barrier layer includes Pt, HfO2 or LiNbO3.

15. The piezoelectric sensor as claimed in claim 11, wherein, It also includes a second barrier layer located between the first barrier layer and the piezoelectric thin film layer. The material of the second barrier layer is different from that of the first barrier layer. The second barrier layer is used to prevent ions from the piezoelectric thin film layer from diffusing to the first electrode layer.

16. The piezoelectric sensor as claimed in claim 15, wherein, The material of the second barrier layer is HfO2 or LiNbO3.

17. The piezoelectric sensor as claimed in claim 16, wherein, The thickness of the second barrier layer is less than 50 nm.

18. The piezoelectric sensor according to any one of claims 9-17, wherein, Also includes: An organic insulating layer is located on the side of the second electrode layer opposite to the substrate. The organic insulating layer has a first via, and the orthographic projection of the first via on the substrate overlaps with the orthographic projection of the second electrode layer on the substrate. An inorganic insulating layer is located on the side of the organic insulating layer opposite to the substrate, and the inorganic insulating layer does not overlap with the first via at least partially; A wiring layer is located on the side of the inorganic insulating layer opposite to the substrate. The wiring layer includes wiring, one end of which is electrically connected to the second electrode layer through at least a portion of the first via.

19. The piezoelectric sensor as claimed in claim 18, wherein, The inorganic insulating layer covers the sidewall of the first via and extends to contact the second electrode layer.

20. The piezoelectric sensor as claimed in claim 19, wherein, At the same sidewall of the first via, the contact boundary between the inorganic insulating layer and the second electrode layer is the first boundary, and the contact boundary between the organic insulating layer and the second electrode is the second boundary. The distance between the first boundary and the second boundary is greater than 30% and less than 60% of the thickness of the piezoelectric film layer.

21. The piezoelectric sensor as claimed in claim 18, wherein, The inorganic insulating layer covers the sidewall of the first via and the second electrode layer exposed by the first via. The portion of the inorganic insulating layer covering the second electrode layer has at least one second via. One end of the trace is electrically connected to the second electrode layer through the first via and the second via.

22. The piezoelectric sensor according to any one of claims 19-21, wherein, It also includes: a bonding electrode disposed in the same layer as the first electrode layer, the bonding electrode being disposed near the edge of the substrate, and the other end of the trace being electrically connected to the bonding electrode through a third via disposed on the inorganic insulating layer and the organic insulating layer, the bonding electrode being used to connect the drive signal terminal.

23. The piezoelectric sensor according to any one of claims 18-22, wherein, The inorganic insulating layer consists of one layer.

24. The piezoelectric sensor as claimed in claim 23, wherein, The inorganic insulating layer is made of materials including SiO2, Al2O3, or Si3N4.

25. The piezoelectric sensor according to any one of claims 18-22, wherein, The inorganic insulating layer comprises at least two sub-layers stacked together, the two sub-layers being made of different materials.

26. The piezoelectric sensor as claimed in claim 25, wherein, The materials of each of the sublayers include SiO2, Al2O3 or Si3N4.

27. The piezoelectric sensor according to any one of claims 18-22, wherein, The wiring layer has a mesh-like structure, and the material of the wiring layer is Ti / Ni / Au, Ti / Au, or Ti / Al / Ti.

28. The piezoelectric sensor according to any one of claims 18-22, wherein, The thickness of the inorganic insulating layer is 100nm~300nm.

29. A haptic feedback device, wherein, Including the piezoelectric sensor as described in any one of claims 9-28.

Citation Information

Patent Citations

  • Piezoelectric driving apparatus, method of manufacturing the same, motor, robot, and pump

    CN107017334A

  • Deformation unit for tactile feedback, display panel and driving circuit

    CN110347264A

  • Display panel

    CN111769080A

  • High-frequency strain excitation method and device

    CN112271951A

  • Display substrate and display device

    CN210575960U