A kind of steel bridge deck wet interface rapid drying equipment and drying method

Drying equipment through diffuse reflection lidar detection and electric heating tube adjustment, combined with porous structural insulation materials, solves the problems of low efficiency and high energy consumption of traditional fire drying methods, and achieves efficient and precise drying of the wet interface of the steel bridge deck. Extended equipment service life.

CN117367084BActive Publication Date: 2024-10-25POLY CHANGDA ENGINEERING CO LTD
View PDF 13 Cites 0 Cited by

Patent Information

Application Number
CN202311305908.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-10-10
Publication Date
2024-10-25
Estimated Expiration
2043-10-10

AI Technical Summary

Technical Problem

The traditional fire drying method has low efficiency, low drying accuracy, high energy consumption, high labor lag, and high risk factor. It cannot meet the actual needs of rapid drying of the wet interface of the steel bridge deck, especially in the humid environment along the coast of South China, which causes the steel deck to soften. , warping and coating peeling, reducing service life.

Method used

Diffuse reflection lidar is used to detect the reflectivity of the steel plate bridge deck, humidity information is generated through the control module, the hot air flow output by the electric heating tube is adjusted, and the heating component and air supply component are combined to achieve precise drying, and through the porous structure of molecular sieves and polyparaphenylene Insulation materials made of ethylene glycol diformate composite reduce heat loss.

Benefits of technology

It improves drying efficiency, reduces energy loss, ensures drying accuracy, reduces heat loss, avoids the accumulation of moisture inside the insulation material, and extends the service life of the equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117367084B_ABST
    Figure CN117367084B_ABST
Patent Text Reader

Abstract

The present invention discloses a steel bridge deck wet interface rapid drying device and drying method, belonging to the technical field of bridge deck drying. The drying device includes a control module and a detection module and a drying module that are communicatively connected to the control module; the detection module includes a diffuse reflection laser radar, the diffuse reflection laser radar is used to collect the reflectivity of the steel plate bridge deck and transmit it to the control module, the control module generates humidity information according to the measured reflectivity and instructs the drying module to output a hot air flow of corresponding temperature to dry the steel plate bridge deck, the control module controls the air outlet temperature of the air distribution orifice plate to achieve precise drying, automatic operation, improve drying efficiency, and reduce energy loss; at the same time, excellent thermal insulation material is prepared to be coated on the outer wall of the pipeline during the hot air flow transmission process, thereby reducing heat loss, further reducing energy consumption, and achieving energy conservation and emission reduction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of bridge deck drying, and in particular to a steel bridge deck wet interface rapid drying device and a drying method. Background Art

[0002] At present, the construction requirements of steel plate bridge deck paving projects in my country are very strict, and the annual construction time is short, which leads to a generally long construction period for steel bridge deck paving. This situation is particularly evident in the subtropical monsoon climate region in southern my country.

[0003] The typhoon area along the coast of South China is located in the offshore environment, with a complex construction environment, high air humidity and high salt spray, which has a great impact on the sandblasting and rust removal of steel plate bridge decks, waterproof bonding layer coating and epoxy asphalt concrete construction. At present, there is no effective drying method and related equipment in the field of rapid drying of wet interfaces of steel plate bridge decks. The traditional fire drying method has low efficiency, high energy consumption, idle workers, and a relatively high risk factor, which cannot meet actual needs.

[0004] The traditional fire drying method for steel bridge decks usually relies on directly heating the air to evaporate moisture. Heat can only be transferred from the air to the surface of the object, and then the moisture inside the object is gradually evaporated by conduction and convection. This process is very slow, especially for the humid environment of the coastal areas of South China, it takes longer to completely dry. The direct air heating method is difficult to control the drying temperature and humidity, which can easily lead to overheating or over-drying, which is unacceptable for some sensitive steel bridge decks. It will cause the steel bridge deck to soften, warp or even deform, resulting in the coating being loose and easy to fall off, which will reduce the service life of the steel bridge deck.

[0005] In addition, traditional fire drying is energy-intensive, as direct heating of the air requires a large amount of fuel or electricity supply, resulting in high energy consumption. Running fire drying equipment for a long time will also lead to energy waste and increased costs. Considering the increasingly serious energy shortage and environmental problems, it is very important to reduce energy consumption. Summary of the invention

[0006] The purpose of the present invention is to provide a steel bridge deck wet interface rapid drying device and drying method, which is used to solve the problems of low efficiency, low drying accuracy, high energy consumption, idleness, relatively high risk factor and failure to meet actual needs of the traditional fire drying method in the prior art.

[0007] The purpose of the present invention can be achieved through the following technical solutions:

[0008] A rapid drying device for a wet interface of a steel bridge deck comprises a control module and a detection module and a drying module which are communicatively connected to the control module; the detection module comprises a diffuse reflection laser radar, the diffuse reflection laser radar is used to collect the reflectivity of the steel plate bridge deck and transmit it to the control module, the control module generates humidity information according to the measured reflectivity, and instructs the drying module to output a hot air flow of corresponding temperature to dry the steel plate bridge deck.

[0009] As a further solution of the present invention, the drying module includes a heating component and an air supply component; the heating component includes a shell and an electric heating tube, the electric heating tube is evenly laid in the shell, and the outer wall of the electric heating tube is provided with a plurality of heating fins;

[0010] The air supply component includes a fan and an air distribution hole plate. The shell input end is connected to the fan, and the shell output end is connected to the air distribution hole plate. The airflow delivered by the fan is heated by the electric heating pipe and delivered to the air distribution hole plate to dry the steel plate bridge deck.

[0011] As a further solution of the present invention, the detection module also includes a temperature sensor, which is used to collect the air outlet temperature information of the heating component and the air outlet temperature information of the air distribution orifice plate and transmit them to the control module. The control module instructs the electric heating tube to adjust the temperature according to the measured temperature information so that the air outlet temperature of the air distribution orifice plate matches the measured humidity.

[0012] As a further solution of the present invention, the control module is further provided with a temperature threshold, and the temperature threshold includes a maximum temperature threshold, a minimum temperature threshold and a limit temperature threshold;

[0013] Wherein, the minimum temperature threshold and the maximum temperature threshold constitute a first temperature interval; the maximum temperature threshold and the limit temperature threshold constitute a second temperature interval;

[0014] The control module determines the collected air outlet temperature of the air distribution orifice plate, and controls the electric heating tube to adjust the temperature according to the determination result.

[0015] As a further solution of the present invention, the judgment of the collected air outlet temperature of the air distribution orifice plate includes the following steps:

[0016] If the collected air outlet temperature of the air distribution orifice plate is lower than the minimum temperature threshold, the electric heating tube is controlled to start heating;

[0017] If the collected air outlet temperature of the air distribution orifice plate is equal to the maximum temperature threshold, the electric heating tube is controlled to stop heating;

[0018] If the collected air outlet temperature of the air distribution orifice plate is equal to the limit temperature threshold, the power supply of the electric heating tube is cut off;

[0019] Wherein, if the detected temperature is within the first temperature range, it means that the electric heating tube is heating normally;

[0020] If the detected temperature is within the second temperature range, it means that the electric heating tube fails to stop heating normally.

[0021] As a further solution of the present invention, it also includes an alarm prompt module, which is communicatively connected with the control module; the alarm prompt module includes a buzzer, the temperature sensor detects that the air outlet temperature of the air distribution orifice plate is equal to the extreme temperature threshold, and the control module controls the buzzer to light up and sound an alarm.

[0022] As a further solution of the present invention, the drying module further comprises a movable frame, and the frame is used to install the heating component and the air supply component;

[0023] The detection module also includes a ranging radar;

[0024] The alarm prompt module also includes an audible and visual alarm;

[0025] The distance measuring radar is installed on the frame and is used to measure the distance between the frame and the construction equipment;

[0026] When the ranging radar detects that the distance is lower than or higher than a preset distance threshold interval, the control module controls the sound and light alarm to sound an alarm.

[0027] As a further solution of the present invention, the air supply assembly also includes a flange, an air distribution plate, an air inlet pipe and a trapezoidal air duct, the flange is installed at the output end of the shell, the input end of the trapezoidal air duct is connected to the flange through the air inlet pipe, and the output end of the trapezoidal air duct is connected to the air distribution orifice plate through the air distribution plate.

[0028] As a further solution of the present invention, it also includes a display module that is communicatively connected to the control module, and the display module is used to display the information received by the control module.

[0029] A method for rapidly drying a wet interface of a steel bridge deck comprises the following steps:

[0030] (1) Set the ranging radar parameters to ensure that the distance between the drying equipment and the construction equipment is within the preset distance threshold range;

[0031] (2) As the drying equipment moves forward, the diffuse reflection laser radar starts to work, scanning the steel bridge deck and feeding back the reflectivity of the steel bridge deck to the control module;

[0032] (3) The control module controls the electric heating tube to adjust the temperature until the air outlet temperature of the air distribution orifice plate matches the measured humidity, and the air delivery component distributes the hot air flow heated by the heating component to the steel bridge deck for drying;

[0033] (4) When drying is completed, the electric heating tube stops working first. After the temperature of the heating component drops below 60°C, the fan stops working and the drying equipment is shut down and powered off.

[0034] Beneficial effects of the present invention:

[0035] (1) The present invention discloses a rapid drying device and drying method for the wet interface of a steel bridge deck. The reflectivity of the steel bridge deck is detected by a diffuse reflection laser radar to obtain the humidity of the steel bridge deck. The control module controls the air outlet temperature of the air distribution orifice plate to achieve precise drying and automated operation, thereby improving drying efficiency and reducing energy loss. At the same time, excellent thermal insulation materials are prepared and coated on the outer wall of the pipeline during the hot air flow transportation process, thereby reducing heat loss, further reducing energy consumption, and achieving energy conservation and emission reduction.

[0036] (2) Furthermore, by compounding a porous molecular sieve with polyethylene terephthalate to form a thermal insulation material, due to the hydrophobic barrier property of polyethylene terephthalate, moisture will be discharged along the pores of the modified molecular sieve. During the process of moisture being discharged along the pores of the modified molecular sieve, it will be adsorbed by the modified molecular sieve. However, since the thermal insulation material is coated on the outer wall of the high-temperature gas pipeline, the moisture adsorbed on the modified molecular sieve is desorbed by absorbing heat, thereby achieving the discharge of moisture, avoiding the accumulation of moisture inside the thermal insulation material and causing rust and corrosion of the gas pipeline. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] The present invention will be further described below in conjunction with the accompanying drawings.

[0038] Figure 1 It is a system block diagram of the drying equipment of the present invention;

[0039] Figure 2 is an axonometric plan view of a drying module of the present invention;

[0040] Figure 3 is a front plan view of the drying module of the present invention;

[0041] Figure 4 is a cross-sectional view of a heating assembly of the present invention;

[0042] Figure 5 It is a top view of the heating component of the present invention.

[0043] In the figure: 1. air inlet interface; 2. heating component; 3. flange; 4. air inlet pipe; 5. trapezoidal air duct; 6. air distribution plate; 7. air distribution hole plate; 8. universal wheel; 9. frame; 10. electric heating tube; 11. heating fins; 12. shell. DETAILED DESCRIPTION

[0044] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0045] like Figure 1-5 As shown, a rapid drying device for the wet interface of a steel bridge deck includes a control module, a detection module, a drying module and a display module, wherein the detection module, the drying module and the display module are respectively connected to the control module for communication; the detection module includes a diffuse reflection laser radar, which is used to collect the reflectivity of the steel plate bridge deck and transmit it to the control module, and the control module generates humidity information according to the measured reflectivity, and instructs the drying module to output a corresponding hot air flow to dry the steel plate bridge deck.

[0046] Among them, the diffuse reflection laser radar sends a laser beam to the steel plate bridge deck. When the laser beam collides with the moisture on the bridge deck, it will be reflected. The diffuse reflection laser radar receives the reflected light and analyzes the reflectivity. The reflectivity is proportional to the moisture content on the steel plate bridge deck. The humidity information of the steel plate bridge deck can be obtained by measuring the reflectivity. The control module receives the reflectivity data transmitted by the diffuse reflection laser radar and converts the reflectivity into a specific humidity value. The control module adjusts the temperature and intensity of the hot air flow according to different humidity conditions to achieve precise drying of the steel plate bridge deck. The drying module outputs the corresponding hot air flow according to the instructions sent by the control module. The hot air flow has a certain temperature and speed. When it is sprayed onto the steel plate bridge deck, it can accelerate the evaporation and volatilization of moisture, thereby achieving the drying effect on the steel plate bridge deck.

[0047] Humidity refers to the content of liquid water molecules. Humidity will affect the optical properties of the surface of an object, so the humidity can be indirectly inferred by changing the intensity of the reflected light. When the laser is irradiated on the surface of the target object, if there is moisture on the surface of the object, the moisture will absorb part of the laser energy and scatter the light. In this way, when the laser is reflected back, the intensity of the echo signal will be affected by the humidity. By analyzing the changes in the intensity of the received reflected light, the humidity can be indirectly detected.

[0048] The humidity at different levels is measured by a humidity sensor, and the reflectivity obtained by irradiating the diffuse reflection laser radar is compared, and the reflectivity of the diffuse reflection laser radar under different humidity is stored. At each humidity level, the measurement is repeated multiple times to obtain reliable data. The humidity data measured by the humidity sensor and the reflectivity data measured by the diffuse reflection laser radar are recorded and sorted to ensure that each set of data corresponds to the corresponding humidity level. The data are stored in the memory through multiple sampling to obtain the reflectivity of the diffuse reflection laser radar under different humidity. The reflectivity obtained by irradiating the steel plate bridge deck with the diffuse reflection laser radar is transmitted to the control module. The control module obtains the corresponding humidity information through the processor according to the obtained reflectivity. The controller controls the drying module to output the dry airflow of the corresponding temperature for drying, thereby achieving fine, precise and rapid drying and reducing unnecessary energy waste.

[0049] The drying module includes a heating component 2 and an air supply component; the heating component 2 includes a shell 12 and an electric heating tube 10, the electric heating tube 10 is evenly laid in the shell 12, and a plurality of heating fins 11 are arranged on the outer wall of the electric heating tube 10; the air supply component includes an air inlet interface 1, a fan, an air distribution hole plate 7, a flange 3, an air distribution plate 6, an air inlet pipe 4 and a trapezoidal air duct 5, the fan is connected to the input end of the electric heating tube 10 evenly laid in the shell 12 through the air inlet interface 1, and the output end of the electric heating tube 10 is connected to the shell 12 The output end of the shell 12 is connected to the air inlet pipe 4 through the flange 3, the air inlet pipe 4 is connected to the air distribution plate 6 through the trapezoidal air duct 5, and the air distribution plate 6 is connected to the air distribution hole plate 7; wherein, the fan is connected to the air inlet interface 1 through a high-pressure hose, and the flange 3 is connected to the air inlet pipe 4 through a 304 stainless steel heat-resistant bellows; the heating component 2 and the air supply component are installed on a frame 9 with a size of 19160mm*880mm*1600mm, and a universal wheel 8 is installed at the bottom of the frame 9 for easy movement and steering.

[0050] The detection module also includes a temperature sensor, which is used to collect the air outlet temperature information of the heating component 2 and the air outlet temperature information of the air distribution orifice plate 7 and transmit it to the control module. The control module instructs the electric heating tube 10 to adjust the temperature according to the measured temperature information so that the air outlet temperature of the air distribution orifice plate 7 matches the measured humidity;

[0051] The control module is also provided with temperature thresholds, which include a maximum temperature threshold, a minimum temperature threshold and an extreme temperature threshold;

[0052] Among them, the minimum temperature threshold and the maximum temperature threshold constitute a first temperature interval; the maximum temperature threshold and the limit temperature threshold constitute a second temperature interval; the control module judges the collected air outlet temperature of the air distribution orifice plate 7, and controls the electric heating tube 10 to adjust the temperature according to the judgment result;

[0053] The judgment of the collected air outlet temperature of the air distribution orifice plate 7 includes the following steps:

[0054] If the collected air outlet temperature of the air distribution orifice plate 7 is lower than the minimum temperature threshold, the electric heating tube 10 is controlled to start heating;

[0055] If the collected air outlet temperature of the air distribution orifice plate 7 is equal to the maximum temperature threshold, the electric heating tube 10 is controlled to stop heating;

[0056] If the collected air outlet temperature of the air distribution orifice plate 7 is equal to the limit temperature threshold, the power supply of the electric heating tube 10 is cut off to force the heating to stop;

[0057] If the detected temperature is within the first temperature range, it means that the electric heating tube 10 is heating normally;

[0058] If the detected temperature is within the second temperature range, it means that the electric heating tube 10 fails to stop heating normally.

[0059] It also includes an alarm prompt module, which is in communication with the control module; the alarm prompt module includes a buzzer, and the temperature sensor detects that the air outlet temperature of the air distribution hole plate 7 is equal to the limit temperature threshold, and the control module controls the buzzer to light up and sound an alarm;

[0060] The detection module also includes a ranging radar; the alarm prompt module also includes an audible and visual alarm; the ranging radar is installed on the frame 9 and is used to measure the distance between the frame 9 and the construction equipment; when the ranging radar detects a distance lower than or higher than a preset distance threshold interval, the control module controls the audible and visual alarm to sound an alarm; the display module is used to display the information received by the control module.

[0061] In one embodiment, the high-temperature air flow heated by the heating component 2 is evenly distributed to five trapezoidal air distribution plates 6 through a five-hole flange 3. Each trapezoidal air distribution plate 6 is further divided into 6 air ducts, which further evenly distribute the air to the air distribution hole plate 7 for drying.

[0062] In one embodiment, there are three ranging radars, which are evenly installed behind the frame 9 and connected to the display module. Two sound and light alarms are respectively installed on the construction equipment (control engineering vehicles, towing engineering vehicles, etc.), and the other sound and light alarm is installed at the rear end of the frame 9. The ranging radars and the sound and light alarms are connected to the display module. The parameters are set. When the drying equipment is traveling in front of the construction equipment (such as a paver or other engineering vehicles, etc.), when the distance between the two is less than 3m (the lower limit of the preset distance threshold) or the distance is greater than 6m (the upper limit of the preset distance threshold), the sound and light alarm will give an alarm prompt, and the display screen of the display module will give a reminder. The specific values ​​can be set according to actual construction needs.

[0063] Six diffuse reflection laser radars are designed and evenly installed on the front extension frame of the frame 9. Each diffuse reflection laser radar has a radiation width of 3.16m and a reflectivity of 2%-94%. According to the actual construction situation, the reflectivity of different wet interfaces is collected and stored in the memory as reference data. Different reflectivities correspond to wet interfaces with different humidity. The reflectivity is transmitted back to the controller as a feedback signal for processing, so as to perform corresponding heating actions to adapt to the heating requirements of different wet interfaces.

[0064] The working principle of the steel bridge deck wet interface rapid drying device and drying method disclosed in the present invention is as follows:

[0065] The diffuse reflection laser radar sends a laser beam to the steel bridge deck. When the laser beam collides with the moisture on the bridge deck, it will be reflected. The diffuse reflection laser radar receives the reflected light and analyzes the reflectivity. The reflectivity is proportional to the moisture content on the steel bridge deck. The humidity information of the steel bridge deck can be obtained by measuring the reflectivity. The control module receives the reflectivity data transmitted by the diffuse reflection laser radar and converts the reflectivity into a specific humidity value. The control module adjusts the temperature and intensity of the hot air flow according to different humidity conditions to achieve precise drying of the steel bridge deck. The drying module outputs the corresponding hot air flow according to the instructions sent by the control module. The hot air flow has a certain temperature and speed. When it is sprayed onto the steel bridge deck, it can accelerate the evaporation and volatilization of moisture, thereby achieving the drying effect on the steel bridge deck.

[0066] A drying method for rapidly drying the wet interface of a steel bridge deck using the above drying equipment comprises the following steps:

[0067] (1) Set the ranging radar parameters to ensure that the distance between the drying equipment and the construction equipment is within the preset distance threshold range;

[0068] (2) As the drying equipment moves forward, the diffuse reflection laser radar starts to work, scanning the steel bridge deck and feeding back the reflectivity of the steel bridge deck to the control module;

[0069] (3) The control module controls the electric heating tube 10 to adjust the temperature until the air outlet temperature of the air distribution hole plate 7 matches the measured humidity, and the air delivery component distributes the hot air flow heated by the heating component 2 to the steel bridge deck for drying;

[0070] (4) After drying is completed, the electric heating tube 10 stops working first. After the temperature of the heating component 2 drops below 60°C, the fan stops working and the drying equipment is shut down and powered off.

[0071] In order to prevent the high-temperature airflow from causing heat loss during the transportation process, which will increase the heat loss of the drying equipment and increase energy consumption, the outer wall of the pipeline during the hot air flow transportation process is covered with insulation material for insulation, thereby reducing heat loss, reducing energy consumption, and achieving the purpose of energy saving and emission reduction.

[0072] The preparation of the thermal insulation material comprises the following steps:

[0073] 1) Preparation of modified molecular sieves:

[0074] 1,4-dibromobutane, 1-methylpyrrolidine and deionized water were mixed and reacted at 80° C. for 40 hours to prepare a template, wherein the molar ratio of 1,4-dibromobutane, 1-methylpyrrolidine and deionized water was 1:2:15;

[0075] Mixing silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and a template agent to obtain a mixture to be crystallized, subjecting the mixture to be crystallized to a hydrothermal crystallization treatment, filtering, washing and drying to obtain the modified molecular sieve, wherein the molar ratio of the silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and the template agent is 100:5:20:1000:10:1, the crystallization temperature of the hydrothermal crystallization treatment is 120°C, and the crystallization time is 100h;

[0076] 2) Preparation of insulation materials:

[0077] Mix polyethylene terephthalate and monomethyl pyrrolidone, heat and stir at 120°C for 15 minutes to form a homogeneous solution, mix modified molecular sieve, dodecyltrimethylammonium bromide and phenol and disperse them by ultrasonic for 30 minutes to obtain a dispersion, transfer the dispersion and the homogeneous solution to a reactor, add tin trichloride and 3-aminopropyltrimethoxysilane, stir at 180°C for 15 hours, separate, wash, dry, draw and weave to obtain a thermal insulation material;

[0078] The mass ratio of the polyethylene terephthalate, monomethyl pyrrolidone, modified molecular sieve, dodecyltrimethylammonium bromide, phenol, tin trichloride and 3-aminopropyltrimethoxysilane is 1:0.1-0.2:1-1.2:0.2-0.3:15:0.02-0.05:0.5-0.7.

[0079] Example 1

[0080] Preparation of modified molecular sieves:

[0081] 1,4-dibromobutane, 1-methylpyrrolidine and deionized water were mixed and reacted at 80° C. for 40 hours to prepare a template, wherein the molar ratio of 1,4-dibromobutane, 1-methylpyrrolidine and deionized water was 1:2:15;

[0082] Mixing silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and a template agent to obtain a mixture to be crystallized, subjecting the mixture to be crystallized to a hydrothermal crystallization treatment, filtering, washing and drying to obtain the modified molecular sieve, wherein the molar ratio of the silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and the template agent is 100:5:20:1000:10:1, the crystallization temperature of the hydrothermal crystallization treatment is 120°C, and the crystallization time is 100h;

[0083] Preparation of insulation materials:

[0084] 1 part by mass of polyethylene terephthalate and 0.1 part by mass of monomethyl pyrrolidone are mixed, heated and stirred at 120°C for 15 minutes to form a homogeneous solution, 1 part by mass of modified molecular sieve, 0.2 parts by mass of dodecyltrimethylammonium bromide and 15 parts by mass of phenol are mixed and ultrasonically dispersed for 30 minutes to obtain a dispersion, the dispersion and the homogeneous solution are transferred to a reactor, 0.02 parts by mass of tin trichloride and 0.5 parts by mass of 3-aminopropyltrimethoxysilane are added, stirred at 180°C for 15 hours, separated, washed, dried, drawn and spun to obtain a thermal insulation material.

[0085] Example 2

[0086] Preparation of modified molecular sieves:

[0087] 1,4-dibromobutane, 1-methylpyrrolidine and deionized water were mixed and reacted at 80° C. for 40 hours to prepare a template, wherein the molar ratio of 1,4-dibromobutane, 1-methylpyrrolidine and deionized water was 1:2:15;

[0088] Mixing silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and a template agent to obtain a mixture to be crystallized, subjecting the mixture to be crystallized to a hydrothermal crystallization treatment, filtering, washing and drying to obtain the modified molecular sieve, wherein the molar ratio of the silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and the template agent is 100:5:20:1000:10:1, the crystallization temperature of the hydrothermal crystallization treatment is 120°C, and the crystallization time is 100h;

[0089] Preparation of insulation materials:

[0090] 1 part by mass of polyethylene terephthalate and 0.15 part by mass of monomethyl pyrrolidone are mixed, heated and stirred at 120°C for 15 minutes to form a homogeneous solution, 1.1 parts by mass of modified molecular sieve, 0.25 parts by mass of dodecyltrimethylammonium bromide and 15 parts by mass of phenol are mixed and ultrasonically dispersed for 30 minutes to obtain a dispersion, the dispersion and the homogeneous solution are transferred to a reactor, 0.035 parts by mass of tin trichloride and 0.6 parts by mass of 3-aminopropyltrimethoxysilane are added, stirred at 180°C for 15 hours, separated, washed, dried, drawn and spun to obtain a thermal insulation material.

[0091] Example 3

[0092] 1,4-dibromobutane, 1-methylpyrrolidine and deionized water were mixed and reacted at 80° C. for 40 hours to prepare a template, wherein the molar ratio of 1,4-dibromobutane, 1-methylpyrrolidine and deionized water was 1:2:15;

[0093] Mixing silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and a template agent to obtain a mixture to be crystallized, subjecting the mixture to be crystallized to a hydrothermal crystallization treatment, filtering, washing and drying to obtain the modified molecular sieve, wherein the molar ratio of the silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and the template agent is 100:5:20:1000:10:1, the crystallization temperature of the hydrothermal crystallization treatment is 120°C, and the crystallization time is 100h;

[0094] Preparation of insulation materials:

[0095] 1 part by mass of polyethylene terephthalate and 0.2 parts by mass of monomethyl pyrrolidone are mixed, heated and stirred at 120°C for 15 minutes to form a homogeneous solution, 1.2 parts by mass of modified molecular sieve, 0.3 parts by mass of dodecyltrimethylammonium bromide and 15 parts by mass of phenol are mixed and ultrasonically dispersed for 30 minutes to obtain a dispersion, the dispersion and the homogeneous solution are transferred to a reactor, 0.05 parts by mass of tin trichloride and 0.7 parts by mass of 3-aminopropyltrimethoxysilane are added, stirred at 180°C for 15 hours, separated, washed, dried, drawn and spun to obtain a thermal insulation material.

[0096] Comparative Example 1

[0097] Preparation of modified molecular sieves:

[0098] 1,4-dibromobutane, 1-methylpyrrolidine and deionized water were mixed and reacted at 80° C. for 40 hours to prepare a template, wherein the molar ratio of 1,4-dibromobutane, 1-methylpyrrolidine and deionized water was 1:2:15;

[0099] Mixing silica sol, sodium aluminate, sodium hydroxide, deionized water and a template agent to obtain a mixture to be crystallized, subjecting the mixture to be crystallized to a hydrothermal crystallization treatment, filtering, washing and drying to obtain the modified molecular sieve, wherein the molar ratio of the silica sol, sodium aluminate, sodium hydroxide, deionized water and the template agent is 100:5:20:1000:1, the crystallization temperature of the hydrothermal crystallization treatment is 120°C, and the crystallization time is 100h;

[0100] Preparation of insulation materials:

[0101] 1 part by mass of polyethylene terephthalate and 0.1 part by mass of monomethyl pyrrolidone are mixed, heated and stirred at 120°C for 15 minutes to form a homogeneous solution, 1 part by mass of modified molecular sieve, 0.2 parts by mass of dodecyltrimethylammonium bromide and 15 parts by mass of phenol are mixed and ultrasonically dispersed for 30 minutes to obtain a dispersion, the dispersion and the homogeneous solution are transferred to a reactor, 0.02 parts by mass of tin trichloride and 0.5 parts by mass of 3-aminopropyltrimethoxysilane are added, stirred at 180°C for 15 hours, separated, washed, dried, drawn and spun to obtain a thermal insulation material.

[0102] Comparative Example 2

[0103] Preparation of modified molecular sieves:

[0104] 1,4-dibromobutane, 1-methylpyrrolidine and deionized water were mixed and reacted at 80° C. for 40 hours to prepare a template, wherein the molar ratio of 1,4-dibromobutane, 1-methylpyrrolidine and deionized water was 1:2:15;

[0105] Mixing silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and a template agent to obtain a mixture to be crystallized, subjecting the mixture to be crystallized to a hydrothermal crystallization treatment, filtering, washing and drying to obtain the modified molecular sieve, wherein the molar ratio of the silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and the template agent is 100:5:20:1000:10:1, the crystallization temperature of the hydrothermal crystallization treatment is 120°C, and the crystallization time is 100h;

[0106] Preparation of insulation materials:

[0107] 1 part by mass of polyethylene terephthalate and 0.1 part by mass of monomethyl pyrrolidone are mixed, heated and stirred at 120°C for 15 minutes to form a homogeneous solution, 1 part by mass of modified molecular sieve, 0.2 part by mass of dodecyltrimethylammonium bromide and 15 parts by mass of phenol are mixed and ultrasonically dispersed for 30 minutes to obtain a dispersion, the dispersion and the homogeneous solution are transferred to a reactor, 0.02 part by mass of tin trichloride is added, stirred at 180°C for 15 hours, separated, washed, dried, drawn and spun to obtain a thermal insulation material.

[0108] Comparative Example 3

[0109] Preparation of modified molecular sieves:

[0110] 1,4-dibromobutane, 1-methylpyrrolidine and deionized water were mixed and reacted at 80° C. for 40 hours to prepare a template, wherein the molar ratio of 1,4-dibromobutane, 1-methylpyrrolidine and deionized water was 1:2:15;

[0111] Mixing silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and a template agent to obtain a mixture to be crystallized, subjecting the mixture to be crystallized to a hydrothermal crystallization treatment, filtering, washing and drying to obtain the modified molecular sieve, wherein the molar ratio of the silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and the template agent is 100:5:20:1000:10:1, the crystallization temperature of the hydrothermal crystallization treatment is 120°C, and the crystallization time is 100h;

[0112] Preparation of insulation materials:

[0113] 1 part by mass of polyethylene terephthalate and 0.1 part by mass of monomethyl pyrrolidone are mixed, heated and stirred at 120°C for 15 minutes to form a homogeneous solution, 1 part by mass of modified molecular sieve, 0.2 part by mass of dodecyltrimethylammonium bromide and 15 parts by mass of phenol are mixed and ultrasonically dispersed for 30 minutes to obtain a dispersion, the dispersion and the homogeneous solution are transferred to a reactor, 0.5 part by mass of 3-aminopropyltrimethoxysilane is added, stirred at 180°C for 15 hours, separated, washed, dried, drawn and spun to obtain a thermal insulation material.

[0114] Performance Test:

[0115] Conduct flame retardant performance test according to standard GB / T 17591-2006;

[0116] Carry out moisture permeability test according to standard GB / T 12704.2-2009;

[0117] Heat transfer coefficient test is carried out according to standard GB / T 13475-2008;

[0118] The tear strength test was carried out according to standard GB / T 3917.1-2009.

[0119] Comparative Examples 1-3 were prepared on the basis of Example 1. The thermal insulation materials obtained from Examples 1-3 and Comparative Examples 1-3 were tested according to the above standards. The test results are shown in Table 1 below:

[0120] Table 1

[0121]

[0122] It can be seen from Table 1 that the flame retardant grade of Comparative Example 1 is significantly worse than that of Example 1, and its moisture permeability and tear strength are reduced, the heat transfer coefficient is increased, and the thermal insulation effect is reduced; the moisture permeability of Comparative Example 2 is significantly reduced, the heat transfer coefficient is significantly increased, the thermal insulation effect is significantly reduced, and the tear strength is lower than that of Example 1; the tear strength of Comparative Example 3 is further reduced than that of Comparative Example 2.

[0123] The thermal insulation material is made by compounding a porous molecular sieve with polyethylene terephthalate. Due to the hydrophobic barrier property of polyethylene terephthalate, moisture will be discharged along the pores of the modified molecular sieve. The moisture will be adsorbed by the modified molecular sieve during the discharge process along the pores of the modified molecular sieve. However, since the thermal insulation material is coated on the outer wall of the high-temperature gas pipeline, the moisture adsorbed on the modified molecular sieve is desorbed by absorbing heat, thereby achieving the discharge of moisture and avoiding the accumulation of moisture inside the thermal insulation material, which causes rust and corrosion of the gas pipeline.

[0124] Furthermore, the preparation of the thermal insulation material is carried out by exposing the abundant silicon hydroxyl groups on the surface of the modified molecular sieve after surface treatment, which reacts with the ester groups of polyethylene terephthalate to form a stable ester bond connection, thereby grafting the modified molecular sieve onto the polyethylene terephthalate to obtain the thermal insulation material. The modified molecular sieve and the polyethylene terephthalate are covalently bonded at the interface, so that the obtained thermal insulation material has excellent thermal stability and mechanical properties.

[0125] Furthermore, by introducing sodium bromide in the preparation process of the modified molecular sieve, the formation and growth of the molecular sieve crystals are facilitated. Bromine has a strong bonding force in the crystal lattice, which can effectively reduce the gaps between the molecular sieve crystals and increase the density and stability of the molecular sieve crystals. After sodium bromide is introduced into the molecular sieve, the bromine element will be adsorbed in the molecular sieve lattice, and its flame retardant properties will improve the overall flame retardant properties of the molecular sieve material.

[0126] Furthermore, during the condensation reaction between the modified molecular sieve and the ester group of polyethylene terephthalate, tin trichloride is added as a catalyst to participate in the reaction, promoting the ester group complex reaction through coordination, thereby improving the reaction rate and yield; at the same time, a complex structure is formed between the tin trichloride and the modified molecular sieve, thereby enhancing the interaction force between the ester group and the modified molecular sieve and improving the mechanical strength of the thermal insulation material.

[0127] Furthermore, during the condensation reaction between the modified molecular sieve and the ester group of polyethylene terephthalate, 3-aminopropyltrimethoxysilane is added to connect the free ester groups to form longer polymer chains and a more stable network structure, thereby improving the thermal insulation effect and moisture permeability of the thermal insulation material.

[0128] The above describes some embodiments of the present invention in detail, but the contents are only preferred embodiments of the present invention and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made within the scope of the present invention should still fall within the scope of the patent coverage of the present invention.

Claims

1. A steel bridge deck wet interface rapid drying device, characterized in that: It includes a control module and a detection module and a drying module that are communicatively connected to the control module; the detection module includes a diffuse reflection laser radar, and the diffuse reflection laser radar is used to collect the reflectivity of the steel plate bridge deck and transmit it to the control module; the control module generates humidity information according to the measured reflectivity, and instructs the drying module to output a hot air flow of corresponding temperature to dry the steel plate bridge deck; The drying module includes a heating component and an air supply component; the heating component includes a shell and an electric heating tube, the electric heating tube is evenly laid in the shell, and the outer wall of the electric heating tube is provided with a plurality of heating fins; The air delivery component includes a fan and an air distribution hole plate, the housing input end is connected to the fan, the housing output end is connected to the air distribution hole plate, the air flow delivered by the fan is heated by the electric heating pipe and delivered to the air distribution hole plate to dry the steel plate bridge deck; the outer wall of the pipeline of the air delivery component is coated with a heat preservation material; The control module is also provided with temperature thresholds, which include a maximum temperature threshold, a minimum temperature threshold and an extreme temperature threshold; Wherein, the minimum temperature threshold and the maximum temperature threshold constitute a first temperature interval; the maximum temperature threshold and the limit temperature threshold constitute a second temperature interval; The control module determines the collected air outlet temperature of the air distribution orifice plate, and controls the electric heating tube to adjust the temperature according to the determination result; The judgment of the collected air outlet temperature of the air distribution orifice plate includes the following steps: If the collected air outlet temperature of the air distribution orifice plate is lower than the minimum temperature threshold, the electric heating tube is controlled to start heating; If the collected air outlet temperature of the air distribution orifice plate is equal to the maximum temperature threshold, the electric heating tube is controlled to stop heating; If the collected air outlet temperature of the air distribution orifice plate is equal to the limit temperature threshold, the power supply of the electric heating tube is cut off; Wherein, if the detected temperature is within the first temperature range, it means that the electric heating tube is heating normally; If the detected temperature is within the second temperature range, it means that the electric heating tube fails to stop heating normally. The detection module also includes a temperature sensor, which is used to collect the air outlet temperature information of the heating component and the air outlet temperature information of the air distribution orifice plate and transmit them to the control module. The control module instructs the electric heating tube to adjust the temperature according to the measured temperature information, so that the air outlet temperature of the air distribution orifice plate matches the measured humidity; The preparation method of the thermal insulation material comprises the following steps: S1. Preparation of modified molecular sieves: 1,4-dibromobutane, 1-methylpyrrolidine and deionized water were mixed and reacted at 80° C. for 40 hours to prepare a template, wherein the molar ratio of 1,4-dibromobutane, 1-methylpyrrolidine and deionized water was 1:2:15; Mixing silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and a template agent to obtain a mixture to be crystallized, subjecting the mixture to be crystallized to a hydrothermal crystallization treatment, filtering, washing and drying to obtain the modified molecular sieve, wherein the molar ratio of the silica sol, sodium aluminate, sodium hydroxide, deionized water, sodium bromide and the template agent is 100:5:20:1000:10:1, the crystallization temperature of the hydrothermal crystallization treatment is 120°C, and the crystallization time is 100h; S2. Preparation of thermal insulation materials: Mix polyethylene terephthalate and monomethyl pyrrolidone, heat and stir at 120°C for 15 minutes to form a homogeneous solution, mix modified molecular sieve, dodecyltrimethylammonium bromide and phenol and disperse them by ultrasonic for 30 minutes to obtain a dispersion, transfer the dispersion and the homogeneous solution to a reactor, add tin trichloride and 3-aminopropyltrimethoxysilane, stir at 180°C for 15 hours, separate, wash, dry, draw and weave to obtain a thermal insulation material; The mass ratio of the polyethylene terephthalate, monomethyl pyrrolidone, modified molecular sieve, dodecyltrimethylammonium bromide, phenol, tin trichloride and 3-aminopropyltrimethoxysilane is 1:0.1-0.2:1-1.2:0.2-0.3:15:0.02-0.05:0.5-0.

7.

2. The steel bridge deck wet interface rapid drying equipment according to claim 1 is characterized in that: It also includes an alarm prompt module, which is communicatively connected to the control module; the alarm prompt module includes a buzzer, and the temperature sensor detects that the air outlet temperature of the air distribution orifice plate is equal to the extreme temperature threshold, and the control module controls the buzzer to light up and sound an alarm.

3. The steel bridge deck wet interface rapid drying equipment according to claim 2 is characterized in that: The drying module further comprises a movable frame, and the frame is used for mounting the heating component and the air supply component; The detection module also includes a ranging radar; The alarm prompt module also includes an audible and visual alarm; The distance measuring radar is installed on the frame and is used to measure the distance between the frame and the construction equipment; When the ranging radar detects that the distance is lower than or higher than a preset distance threshold interval, the control module controls the sound and light alarm to sound an alarm.

4. The steel bridge deck wet interface rapid drying equipment according to claim 1 is characterized in that: The air supply assembly also includes a flange, an air distribution plate, an air inlet pipe and a trapezoidal air duct. The flange is installed at the output end of the shell, the input end of the trapezoidal air duct is connected to the flange through the air inlet pipe, and the output end of the trapezoidal air duct is connected to the air distribution orifice plate through the air distribution plate.

5. The steel bridge deck wet interface rapid drying equipment according to claim 1 is characterized in that: It also includes a display module that is communicatively connected to the control module, and the display module is used to display the information received by the control module.

6. A drying method for rapidly drying the wet interface of a steel bridge deck using the drying equipment according to claim 5, characterized in that: The following steps are involved: (1) Set the ranging radar parameters to ensure that the distance between the drying equipment and the construction equipment is within the preset distance threshold range; (2) As the drying equipment moves forward, the diffuse reflection laser radar starts to work, scanning the steel bridge deck and feeding back the reflectivity of the steel bridge deck to the control module; (3) The control module controls the electric heating tube to adjust the temperature until the air outlet temperature of the air distribution orifice plate matches the measured humidity, and the air delivery component distributes the hot air flow heated by the heating component to the steel bridge deck for drying; (4) When drying is completed, the electric heating tube stops working first. After the temperature of the heating component drops below 60°C, the fan stops working and the drying equipment is shut down and powered off.

Citation Information

Patent Citations

  • Waterproof, high- / low-temperature-resistant and low-VOC (Volatile Organic Compound) polyurethane coating capable of being cured quickly

    CN106752850A

  • Method for synthesizing TNU-9 molecular sieve

    CN110407227A

  • Laser radar drying system, method and device

    CN112240685A

  • Pedestrian overpass for municipal engineering

    CN113106857A

  • Bridge floor detection method, device and equipment and storage medium

    CN115790460A