Tin bath side wall with composite graphite lining, tin bath and hot replacement method

The modular design of the composite graphite liner allows for easy replacement of damaged filler liners, solving the problem of oxidation and detachment of the graphite liner in the tin bath, reducing maintenance costs, and ensuring production safety.

CN117401893BActive Publication Date: 2024-11-26CHINA TRIUMPH INT ENG CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202311471708.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-11-07
Publication Date
2024-11-26
Estimated Expiration
2043-11-07

AI Technical Summary

Technical Problem

The existing graphite lining of the tin bath is prone to oxidation and detachment during long-term production, causing the molten glass to stick to the side wall bricks, increasing the difficulty of accident handling and losses.

Method used

The composite graphite lining design includes fixed and filler linings. The split design, connected by pressure rods, allows for easy replacement of damaged filler linings and prevents the glass strip from contacting the sidewall bricks.

Benefits of technology

This reduces the maintenance cost of the tin bath sidewall lining, ensures production safety, avoids the adhesion of glass strips to the sidewall bricks, and improves production continuity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117401893B_ABST
    Figure CN117401893B_ABST
Patent Text Reader

Abstract

The present invention relates to glass thermal equipment, and provides a tin bath side wall with a composite graphite lining, a tin bath and a hot replacement method, comprising: a side wall brick, an L-shaped lining embedding groove is provided on the inner side wall of the side wall brick; a lining assembly, the lining assembly comprising a fixed lining, a filling lining and a pressure rod, the fixed lining and the filling lining are both made of graphite material, the cross section of the fixed lining is L-shaped and the cross section of the filling lining is rectangular, the fixed lining comprises a vertical lining part and a horizontal lining part vertically connected to the bottom end of the vertical lining part, the horizontal lining part of the fixed lining is clamped in the horizontal groove part of the lining embedding groove, the vertical lining part of the fixed lining is clamped in the vertical groove part of the lining embedding groove and a vacant area is reserved for the filling lining, and the filling lining is installed on the side wall brick through the pressure rod to fill the vacant area. The present invention greatly reduces the lining maintenance cost of the tin bath side wall, so that the tin bath graphite lining can meet the requirements of long-term production safety.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to glass thermal equipment, in particular to a tin bath side wall with a composite graphite lining, a tin bath and a hot state replacement method. Background Art

[0002] The tin bath is an important thermal equipment in the float glass production line. The glass liquid is melted in the melting furnace, flows into the tin bath through the flow channel, and then spreads on the tin liquid surface. After the edge drawing machine, it reaches the appropriate thickness and plate width, and enters the annealing furnace after gradual cooling. Graphite is usually set on both sides of the tin liquid tank, and the graphite lining is set on the side wall bricks. The non-bonding property of graphite and glass liquid is used to ensure that when an accident occurs in production, the glass liquid does not stick to the refractory bricks on the edge, and the glass liquid can be smoothly sent out of the tin bath, reducing the difficulty of accident handling and reducing the losses caused by the accident.

[0003] The setting of graphite lining is very mature for tin bath design and glass production. The technicians have made a lot of improvements in graphite materials and detailed structures, and have achieved good results. However, problems still exist. The main problem is that in long-term production, especially for production lines with long kiln age, the oxidation and shedding of graphite will make part or all of the graphite lining lose its function. When handling accidents, the glass liquid adheres to the side wall bricks and is difficult to separate, resulting in full tank accidents and causing significant losses to production. Summary of the invention

[0004] In view of the shortcomings of the prior art mentioned above, the technical problem to be solved by the present invention is to provide a tin bath side wall, a tin bath and a hot replacement method with a composite graphite lining, which utilizes a split design of a fixed lining and a filling lining to greatly reduce the lining maintenance cost of the tin bath side wall, so that the tin bath graphite lining can meet the requirements of long-term production safety.

[0005] In order to solve the above technical problems, the present invention provides a tin bath side wall with a composite graphite lining, comprising:

[0006] Side wall bricks, the inner side wall of the side wall bricks is provided with an L-shaped lining embedding groove, the lining embedding groove includes a vertical groove portion and a horizontal groove portion vertically connected to the bottom end of the vertical groove portion;

[0007] A lining assembly, the lining assembly includes a fixed lining, a filling lining and a pressure rod, the fixed lining and the filling lining are both made of graphite material, the cross-section of the fixed lining is L-shaped and the cross-section of the filling lining is rectangular, the fixed lining includes a vertical lining portion and a horizontal lining portion vertically connected to the bottom end of the vertical lining portion, the horizontal lining portion of the fixed lining is clamped in the horizontal groove portion of the lining embedding groove, the vertical lining portion of the fixed lining is clamped in the vertical groove portion of the lining embedding groove and a vacant area is reserved for the filling lining, and the filling lining is installed on the side wall bricks through the pressure rod to fill the vacant area.

[0008] Preferably, the filling liner and the pressure rod are connected by bolts.

[0009] Preferably, a first positioning groove is provided on the top wall of the side wall brick, and the first positioning groove is adapted to the shape and size of the pressure rod.

[0010] Preferably, a second positioning groove is provided on the top wall of the filling liner, and the second positioning groove matches the shape and size of the pressure rod.

[0011] Preferably, the compression rod is T-shaped, and comprises a longitudinal rod portion and a transverse rod portion which are vertically connected, the longitudinal rod portion and the transverse rod portion are both arranged horizontally, the longitudinal rod portion is connected to the filling lining, and the transverse rod portion is arranged at the top wall of the side wall bricks.

[0012] Preferably, the end of the cross bar portion away from the longitudinal bar portion is provided with a groove for welding.

[0013] Preferably, the tin bath side wall with composite graphite lining further comprises a tin bath steel shell, the tin bath steel shell wraps the outer side wall of the side wall bricks, and the pressure rod is welded to the tin bath steel shell.

[0014] The present invention also provides a tin bath, comprising:

[0015] Tin bath bottom, the bottom of the tin bath is made of tin bath bricks;

[0016] The tin bath side wall with the composite graphite lining has a transverse groove portion of the lining embedded groove that is lower than the upper surface of the tin bath bottom.

[0017] The present invention also provides a method for hot replacement of the tin bath side wall with the composite graphite lining, comprising the following steps:

[0018] Assembly steps of lining components: Assemble the filling lining and pressure rod in cold state according to the drawings, verify the position to be replaced, and place them on both sides of the tin bath for use;

[0019] Steps for making a small water bag: Make a small water bag and connect the water pipe of the small water bag;

[0020] Glass strip narrowing step: adjust the glass production plan, narrow the current glass strip to the preset width specification, so that the distance between the glass strip and the side wall bricks meets the replacement space requirements of the filling lining;

[0021] The replacement steps of the filling lining are as follows: the staff wears heat-insulating clothing, opens the edge sealing material of the side wall of the tin bath near the filling lining to be replaced, and takes out the filling lining to be replaced; two staff members put the spare filling lining into the empty area of ​​the lining embedding groove, and press the spare filling lining with a long hook tool; one staff member uses a small water bag to block the flame in the tin bath; one staff member welds and fixes the pressure rod to the tin bath steel shell of the tin bath; after completion, re-stuff the edge sealing material and continue to replace the next damaged filling lining.

[0022] Preferably, the hot replacement method further comprises a step of detecting the lining composite assembly: observing the degree of loss of the filled lining in the tin bath in real time by means of detection equipment or manually; if the filled lining has been partially or completely oxidized and lost, it needs to be replaced.

[0023] As described above, the tin bath side wall with composite graphite lining, tin bath and hot replacement method of the present invention have the following beneficial effects: when the filling lining in the tin bath is oxidized and the material gradually falls off and is lost, a new filling lining is assembled in advance in a cold state, and the filling lining and the pressure rod are connected by a connector for standby use, and then the assembled filling lining is placed in the tin bath in a hot state, and the pressure rod is fixed to the side wall brick after the position is determined. The filling lining is pressed on the fixed lining to refill the vacant area, and when the glass ribbon is widened to the side wall brick, the filling lining can block the glass ribbon again to prevent the glass ribbon from contacting the side wall brick. Therefore, the tin bath side wall with composite graphite lining of the present invention utilizes the split design of the fixed lining and the filling lining, which greatly reduces the lining maintenance cost of the tin bath side wall, so that the tin bath graphite lining can meet the requirements of long-term production safety. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 Shown is a cross-sectional view of a tin bath of the present invention;

[0025] Figure 2 A cross-sectional view of a tin bath sidewall with a composite graphite lining according to the present invention is shown;

[0026] Figure 3 Shown is a top view of the side wall bricks;

[0027] Figure 4 Display as Figure 3 Sectional view along line AA;

[0028] Figure 5 Shown is a top view of a fixed liner;

[0029] Figure 6 A side view of a fixed liner is shown;

[0030] Figure 7A top view showing a padded liner;

[0031] Figure 8 Shown is a side view of a padded liner;

[0032] Fig. 9 Shown is a top view of the strut;

[0033] Fig.10 Shown is a side view of a strut.

[0034] Component number description

[0035] 1 Glass ribbon

[0036] 2 Tin Liquid

[0037] 3 side wall tiles

[0038] 4 Tin bath bottom brick

[0039] 5 Tin bath steel shell

[0040] 6 Edge banding

[0041] 7 Fixed lining

[0042] 8 Filling lining

[0043] 9. Pressure rod

[0044] 10 Bolts

[0045] 11 First positioning groove

[0046] 12 Second positioning slot

[0047] 13 slope DETAILED DESCRIPTION

[0048] The following is a description of the implementation of the present invention by means of specific embodiments. Those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification.

[0049] It should be noted that the structures, proportions, sizes, etc. illustrated in the drawings of this specification are only used to match the contents disclosed in the specification for people familiar with this technology to understand and read, and are not used to limit the limiting conditions for the implementation of the present invention, so they have no substantial technical significance. Any modification of the structure, change of the proportion relationship or adjustment of the size, without affecting the effects and purposes that can be achieved by the present invention, should still fall within the scope of the technical content disclosed by the present invention. At the same time, the terms such as "upper", "lower", "left", "right", "middle" and "one" quoted in this specification are only for the convenience of description, and are not used to limit the scope of the implementation of the present invention. The change or adjustment of their relative relationship should also be regarded as the scope of the implementation of the present invention without substantially changing the technical content.

[0050] like Figure 1 As shown, the present invention provides a tin bath, comprising:

[0051] Tin bath bottom, which is made of tin bath bottom bricks 4; the material of tin bath bottom bricks is generally clay or calcium aluminate;

[0052] and tin bath side walls with composite graphite lining.

[0053] Among them, the composite graphite lining is composed of two detachable and assembled graphite lining parts. With this arrangement, even if the graphite lining leaking out of the tin liquid is oxidized or falls off, one of the graphite lining parts can be easily replaced, thereby greatly reducing the maintenance cost.

[0054] Specifically, in order to facilitate the replacement of one of the graphite lining components of the tin bath side wall with the composite graphite lining, Figure 1 and Figure 2 , the tin bath sidewall with composite graphite lining includes:

[0055] The side wall brick 3 has an L-shaped lining embedding groove on its inner side wall, and the lining embedding groove includes a vertical groove portion and a horizontal groove portion vertically connected to the bottom end of the vertical groove portion;

[0056] The lining assembly includes a fixed lining 7, a filling lining 8 and a pressure rod 9. The fixed lining 7 and the filling lining 8 are both made of graphite material. The cross-section of the fixed lining 7 is L-shaped and the cross-section of the filling lining 8 is rectangular. The fixed lining 7 includes a vertical lining portion and a horizontal lining portion vertically connected to the bottom end of the vertical lining portion. The horizontal lining portion of the fixed lining 7 is clamped in the horizontal groove portion of the lining embedding groove. The vertical lining portion of the fixed lining 7 is clamped in the vertical groove portion of the lining embedding groove and a vacant area is reserved for the filling lining 8. The filling lining 8 is installed on the side wall brick 3 through the pressure rod 9 to fill the vacant area.

[0057] In the present invention, the material of the side wall bricks 3 is generally clay or calcium aluminate, the material of the fixed lining 7 and the filling lining 8 is generally high-purity high-carbon graphite, and the material of the pressure rod 9 is generally heat-resistant steel. The trough pool surrounded by the tin bath bottom bricks and the side wall bricks contains molten tin liquid. The glass ribbon floats on the tin liquid and spreads out, and is formed under the action of the edge drawing machine. An L-shaped lining embedding groove (referred to as the L-shaped groove) is opened on the side wall bricks, and the fixed lining 7 is embedded in the side wall bricks. The L-shaped space surrounded by the tin bath bottom bricks and the side wall bricks prevents the fixed lining 7 from floating away under the buoyancy and convection of the tin liquid, and can be stably embedded in the side wall bricks. It should be noted that the installation of this graphite lining structure needs to be carried out simultaneously with the construction of the side wall bricks, otherwise, when the side wall bricks are closed, the fixed lining 7 will not be installed. When the glass ribbon 1 is as wide as the side wall bricks, the filling lining 8 and / or the fixed lining 7 blocks the glass ribbon 1, and the glass ribbon 1 and the graphite lining are not wetted or adhered. By adjusting the edge drawing machine or other auxiliary means, the glass ribbon and the graphite lining can be easily separated to avoid the occurrence of full tank accidents.

[0058] During the long-term production process, the top of the existing one-piece graphite lining is gradually oxidized due to frequent exposure to space, and the graphite material on the top of the existing one-piece graphite lining gradually falls off and is lost. When the glass ribbon is as wide as the side wall bricks, the existing one-piece graphite lining cannot block the glass ribbon, and the glass ribbon is in contact and adhesion with the side wall bricks, which is prone to accidents, and the structure of the existing one-piece graphite lining determines that it is difficult to remove and replace it in a hot state. Based on this, the composite graphite lining structure of the present invention solves this problem. When the filling lining 8 located in the tin bath is oxidized and the material gradually falls off and is lost, a new filling lining 8 is assembled in a cold state in advance, and the filling lining 8 is connected to the pressure rod through a connector for standby use, and then the assembled filling lining 8 is placed in the tin bath in a hot state, and the pressure rod is fixed to the side wall brick 3 after the position is determined. The filling liner 8 is pressed on the fixed liner 7 to refill the vacant area. When the glass ribbon 1 is as wide as the side wall bricks, the filling liner 8 can block the glass ribbon 1 again to prevent the glass ribbon 1 from contacting the side wall bricks.

[0059] Therefore, the tin bath side wall with composite graphite lining of the present invention utilizes the split design of fixed lining 7 and filling lining 8, which greatly reduces the lining maintenance cost of the tin bath side wall, so that the tin bath graphite lining can meet the requirements of long-term production safety.

[0060] like Figure 1 As described above, in order to make the fixed lining 7 more stably embedded in the side wall bricks, the transverse groove portion of the lining embedding groove is lower than the upper surface of the tin bath bottom.

[0061] like Figure 2 As shown, in order to facilitate the disassembly and assembly of the filling type liner 8 and the pressure rod 9, the filling type liner 8 and the pressure rod 9 are connected by bolts 10.

[0062] like Figure 3 and Figure 4 As shown, in order to position and install the compression rod 9 , a first positioning groove 11 is provided on the top wall of the side wall brick 3 , and the shape and size of the first positioning groove 11 are matched with the compression rod 9 .

[0063] The number of the first positioning grooves 11 is generally 1 to 4, preferably 2 to 3; the width of the groove is generally 30 to 80 mm, preferably 20 to 40 mm; the depth is 10 to 30 mm, preferably 12 to 20 mm.

[0064] The side wall bricks can be opened with holes for setting connection components. The number of holes is generally 1 to 4, preferably 2. The upper part is a round hole or a truncated cone hole, and the lower part is a round hole, which makes it easy to fix the side wall bricks on the steel plate.

[0065] like Figure 5 and Figure 6 As shown, the cross section of the fixed lining 7 is L-shaped, and the length is adapted to the size of the side wall bricks. The W1 size is generally 40-70 mm, preferably 50-60 mm; the W2 size is generally 60-100 mm, preferably 70-80 mm; the H1 size is generally 40-70 mm, preferably 50-60 mm; the H2 size is generally 150-200 mm, preferably 160-170 mm.

[0066] like Figure 7 and Figure 8 As shown, in order to position and install the pressure rod 9, a second positioning groove 12 is provided on the top wall of the filling liner 8, and the second positioning groove 12 matches the shape and size of the pressure rod 9. The shape of the second positioning groove 12 is generally T-shaped or rectangular, preferably T-shaped, the purpose is to increase the contact area between the pressure rod and the filling liner 8, so that the filling liner 8 is more stable in the tin liquid. The depth of the second positioning groove 12 is generally 8 to 20 mm, preferably 12 to 14 mm. A threaded hole is drilled in the middle of each second positioning groove 12, the number is generally 1 to 3, preferably 2 to 3. The diameter of the hole is generally M6 to M12, preferably M8 to M10.

[0067] like Fig. 9 and Fig.10 As shown, in order to simplify the structure of the compression rod 9, the compression rod 9 is T-shaped, and the compression rod 9 includes a vertically connected longitudinal rod portion and a transverse rod portion, both of which are arranged horizontally, the longitudinal rod portion is connected to the filling lining 8, and the transverse rod portion is arranged at the top wall of the side wall brick 3. The thickness of the compression rod 9 is generally 10 to 30 mm, preferably 10 to 18 mm. The transverse rod portion cooperates with the slot on the upper surface of the side wall brick, and the width is generally 20 to 80 mm, preferably 20 to 40 mm.

[0068] The tin bath side wall with composite graphite lining also includes a tin bath steel shell 5, which wraps the outer side wall of the side wall brick 3, and the pressure rod 9 is welded to the tin bath steel shell 5. The end of the cross bar away from the longitudinal bar is provided with a groove 13 for welding, which is convenient for welding with the tin bath steel shell 5. In the figure, the longitudinal bar is matched with the groove on the upper surface of the filling liner 8, and the longitudinal bar is provided with a circular hole, the number of which is consistent with the threaded hole on each groove of the filling liner 8, and the hole diameter is matched with the diameter of the threaded hole.

[0069] The present invention also provides a method for hot replacement of the tin bath side wall with the composite graphite lining, comprising the following steps:

[0070] Assembly steps of the lining assembly: assemble the filling lining 8 and the pressure rod 9 in a cold state according to the drawing, verify the position to be replaced, and place them on both sides of the tin bath for use;

[0071] Steps for making a small water bag: Make a small water bag (for example, the length of the small water bag is about 700m and the width is about 250mm) and connect the water pipe of the small water bag;

[0072] Glass strip narrowing step: adjusting the glass production plan, narrowing the current glass strip 1 to a preset width specification, so that the distance between the glass strip 1 and the side wall brick 3 meets the replacement space requirement of the filling lining 8;

[0073] Replacement steps of the filling lining: the staff wears heat-insulating clothing, opens the edge sealing material 6 of the side wall of the tin bath near the filling lining 8 to be replaced, and takes out the filling lining 8 to be replaced; two staff members put the spare filling lining 8 into the empty area of ​​the lining embedding groove, and press the spare filling lining 8 with a long hook tool; one staff member uses a small water bag to block the flame in the tin bath; one staff member welds and fixes the pressure rod 9 to the tin bath steel shell 5 of the tin bath; after completion, re-stuff the edge sealing material 6 and continue to replace the next damaged filling lining 8.

[0074] The hot replacement method of the present invention can conveniently replace the filling liner 8 of the lining assembly during the production of the glass ribbon.

[0075] Furthermore, the hot replacement method also includes a step of detecting the lining composite component: observing the degree of wear of the filling lining 8 in the tin bath in real time through detection equipment or manual work. If the filling lining 8 has been partially or completely oxidized and lost, it needs to be replaced.

[0076] In summary, the present invention utilizes the split design of fixed lining and filling lining, which greatly reduces the lining maintenance cost of the tin bath side wall, so that the tin bath graphite lining can meet the requirements of long-term production safety. Therefore, the present invention effectively overcomes various shortcomings in the prior art and has high industrial utilization value.

[0077] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A tin bath side wall with a composite graphite lining, characterized in that: include: A side wall brick (3), wherein an L-shaped lining embedding groove is provided on the inner side wall of the side wall brick (3), and the lining embedding groove comprises a vertical groove portion and a horizontal groove portion vertically connected to the bottom end of the vertical groove portion; A lining assembly, the lining assembly comprising a fixed lining (7), a filling lining (8) and a pressure rod (9), the fixed lining (7) and the filling lining (8) are both made of graphite material, the cross section of the fixed lining (7) is L-shaped and the cross section of the filling lining (8) is rectangular, the fixed lining (7) comprises a vertical lining portion and a horizontal lining portion vertically connected to the bottom end of the vertical lining portion, the horizontal lining portion of the fixed lining (7) is clamped in the horizontal groove portion of the lining embedding groove, the vertical lining portion of the fixed lining (7) is clamped in the vertical groove portion of the lining embedding groove and a vacant area is reserved for the filling lining (8), and the filling lining (8) is installed on the side wall brick (3) through the pressure rod (9) to fill the vacant area.

2. The tin bath sidewall with composite graphite lining according to claim 1, characterized in that: The filling liner (8) and the pressure rod (9) are connected via bolts (10).

3. The tin bath sidewall with composite graphite lining according to claim 1, characterized in that: A first positioning groove (11) is provided on the top wall of the side wall brick (3), and the first positioning groove (11) is adapted to the shape and size of the pressure rod (9).

4. The tin bath sidewall with composite graphite lining according to claim 1, characterized in that: A second positioning groove (12) is provided on the top wall of the filling-type liner (8), and the second positioning groove (12) matches the shape and size of the pressure rod (9).

5. The tin bath sidewall with composite graphite lining according to claim 1, characterized in that: The compression rod (9) is T-shaped and comprises a longitudinal rod portion and a transverse rod portion which are vertically connected. The longitudinal rod portion and the transverse rod portion are both arranged horizontally. The longitudinal rod portion is connected to the filling lining (8), and the transverse rod portion is arranged at the top wall of the side wall brick (3).

6. The tin bath sidewall with composite graphite lining according to claim 5, characterized in that: The end of the cross bar portion away from the longitudinal bar portion is provided with a groove (13) for welding.

7. The tin bath sidewall with composite graphite lining according to claim 1, characterized in that: The tin bath side wall with composite graphite lining also includes a tin bath steel shell (5), the tin bath steel shell (5) wraps around the outer side wall of the side wall brick (3), and the pressure rod (9) is welded to the tin bath steel shell (5).

8. A tin bath, characterized in that: include: A tin bath bottom, the tin bath bottom being built with tin bath bottom bricks (4); According to any one of claims 1 to 7 of the tin bath side wall with a composite graphite lining, the transverse groove portion of the lining embedded groove is lower than the upper surface of the tin bath bottom.

9. A method for hot replacement of a tin bath side wall with a composite graphite lining according to any one of claims 1 to 7, characterized in that: The following steps are involved: The assembly steps of the lining assembly are as follows: assemble the filling lining (8) and the pressure rod (9) in a cold state according to the drawing, verify the position to be replaced, and place them on both sides of the tin bath for use; Steps for making a small water bag: Make a small water bag and connect the water pipe of the small water bag; The step of narrowing the glass strip: adjusting the glass production plan to narrow the current glass strip (1) to a preset width specification so that the distance between the glass strip (1) and the side wall brick (3) meets the replacement space requirement of the filling lining (8); The replacement steps of the filling lining are as follows: the staff wearing heat-insulating clothing opens the sealing material (6) of the side wall of the tin bath near the filling lining (8) to be replaced, and takes out the filling lining (8) to be replaced; two staff members put the spare filling lining (8) into the empty area of ​​the lining embedding groove, and press the spare filling lining (8) with a long hook tool; one staff member uses a small water bag to block the flame in the tin bath; one staff member welds and fixes the pressure rod (9) to the tin bath steel shell (5) of the tin bath; after completion, re-insert the sealing material (6) and continue to replace the next damaged filling lining (8).

10. The hot replacement method according to claim 9, characterized in that: The hot replacement method also includes a step of detecting the lining composite component: observing the degree of loss of the filling lining (8) in the tin bath in real time by means of a detection device or manually; if the filling lining (8) has been partially or completely oxidized and lost, it needs to be replaced.

Citation Information

Patent Citations

  • Mounting structure of tin groove graphite lining

    CN109851208A

  • Graphite flange device of float glass tin bath

    CN214142083U

  • Method for producing plate glass and device for producing the plate glass

    JP2000313628A

  • Glass manufacturing chamber containing buoyant side wall liners of graphite

    US3481729A