Diamond-based transistor device, manufacturing method thereof and electronic device

By forming a groove structure and a heavy boron doped buried layer on the diamond substrate, the problem of insufficient performance of diamond-based transistor devices is solved, and the mobility and performance of conductive channels are significantly improved.

CN117766571BActive Publication Date: 2024-11-22深圳平湖实验室
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202311864997.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-12-29
Publication Date
2024-11-22
Estimated Expiration
2043-12-29

AI Technical Summary

Technical Problem

Existing diamond-based transistor devices have insufficient performance and are difficult to meet the needs of high-frequency RF and high-voltage applications.

Method used

By forming a diamond epitaxial layer on the diamond substrate and thermochemical etching using metal nickel to generate a groove structure, depositing a surface hydrogen cut-off layer and passivation layer, forming atomic smooth side walls, combined with heavy boron doped buried layer , improve the mobility of conductive channels.

Benefits of technology

Increases the device's conductive channel mobility and improves the performance of diamond-based transistor devices, especially in high-frequency RF and high-voltage applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN117766571B_ABST
    Figure CN117766571B_ABST
Patent Text Reader

Abstract

The present invention discloses a diamond-based transistor device, a manufacturing method thereof and an electronic device. A first groove, a second groove and a first connecting wall are arranged in a surface hydrogen cutoff layer. The first groove and the second groove both have side walls and a second connecting arm connecting all the side walls. The inclination angles of all the side walls relative to the surface of a diamond substrate are greater than 0 degree. The first connecting wall and the second connecting wall are parallel to the surface of the diamond substrate. A source metal contact and a drain metal contact are respectively located on the surfaces of the second connecting walls of the first groove and the second groove, and are electrically connected to the surface hydrogen cutoff layer through a surface passivation layer. A gate metal is located on the surface of the first connecting wall. Therefore, all the side walls are smooth wall surfaces, and all the side walls are of the diamond {111} crystal plane family. The inclination angles between the side walls and the diamond substrate are greater than 0 degree. Therefore, the mobility of the conductive channel of the device can be increased, thereby improving the performance of the diamond-based transistor device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a diamond-based transistor device, a manufacturing method thereof and an electronic device. Background Art

[0002] As the next generation of wide bandgap compound semiconductors, diamond has the highest intrinsic thermal conductivity of 2280W / mK (much higher than the thermal conductivity of gallium nitride (253W / mK) and silicon carbide (370W / mK) among wide bandgap semiconductors, high breakdown electric field strength>10MV / cm, high carrier saturation drift velocity of about 2.3e7cm / s, high carrier mobility (hole body mobility can reach up to about 2100cm2 / Vs), etc. The main application scenarios of diamond devices are high-frequency RF transistors and high-voltage transistors and diodes, which are aimed at wireless communications and power electronics scenarios.

[0003] How to improve the performance of diamond-based transistor devices is an urgent problem to be solved by those skilled in the art. Summary of the invention

[0004] The present invention provides a diamond-based transistor device, a manufacturing method thereof and an electronic device, which are used to improve the performance of the diamond-based transistor device.

[0005] In a first aspect, the present application provides a diamond-based transistor device, comprising: a metal layer (6), a diamond substrate (1), and a diamond epitaxial layer (2), a surface hydrogen cutoff layer (4), and a surface passivation layer (5) sequentially stacked on the diamond substrate (1);

[0006] The surface of the diamond epitaxial layer (2) is provided with a first groove (7), a second groove (8) and a first connecting wall (9) connecting the first groove and the second groove; the first groove (7) and the second groove (8) both have side walls and a second connecting wall (12) connecting all the side walls; the inclination angles of all the side walls relative to the surface of the diamond substrate (1) are greater than 0 degrees; and the first connecting wall (9) and the second connecting wall (12) are both parallel to the surface of the diamond substrate (1);

[0007] The metal layer (6) comprises a source metal contact (61), a drain metal contact (62) and a gate metal (63); the source metal contact (61) is located on the surface of the second connecting wall (12) of the first groove (7), and is electrically connected to the surface hydrogen stop layer (4) through the surface passivation layer (5); the drain metal contact (62) is located on the surface of the second connecting wall (12) of the second groove (8), and is electrically connected to the surface hydrogen stop layer (4) through the surface passivation layer (5); and the gate metal (63) is located on the surface of the first connecting wall (9).

[0008] In a possible implementation, all the side walls belong to the {111} crystal plane family.

[0009] In a possible implementation, the side wall includes a first side wall (10) and a second side wall (11);

[0010] The inclination angle of the first side wall (10) relative to the surface of the diamond substrate (1) is 125 degrees, and the inclination angle of the second side wall (11) relative to the surface of the diamond substrate (1) is 55 degrees;

[0011] The depth of the first groove (7) and the second groove (8) relative to the diamond substrate (1) is 0-100 μm.

[0012] In a possible implementation, the diamond-based transistor device further includes at least one heavily boron-doped buried layer (14);

[0013] The heavily boron-doped buried layer (14) is located between the diamond epitaxial layer (2) and the surface hydrogen cut-off layer (4), and an orthographic projection of the heavily boron-doped buried layer (14) on the diamond substrate (1) overlaps with an orthographic projection of the second connecting wall (12) of the first groove (7) on the diamond substrate (1), an orthographic projection of the second connecting wall (12) of the second groove (8) on the diamond substrate (1), and an orthographic projection of the first connecting wall (9) on the diamond substrate (1).

[0014] In a second aspect, the present application provides a method for manufacturing a diamond-based transistor device as described in any one of the first aspects, comprising:

[0015] Forming a diamond epitaxial layer (2) on a diamond substrate (1);

[0016] Depositing metal nickel on the diamond epitaxial layer (2) to perform thermochemical etching on the diamond epitaxial layer (2) to generate a first groove (7) and a second groove (8), wherein the first groove (7) and the second groove (8) are connected via a first connecting wall (9), the first groove (7) and the second groove (8) both have side walls and a first connecting wall (12) connecting all the side walls, the inclination angles of all the side walls relative to the surface of the diamond substrate (1) are greater than 0 degrees, and the first connecting wall (9) and the second connecting wall (12) are both parallel to the surface of the diamond substrate (1);

[0017] The diamond epitaxial layer (2) is treated by a diamond surface hydrogenation process to generate a surface hydrogen cutoff layer (4) on the surface of the diamond epitaxial layer (2);

[0018] Depositing a surface passivation layer (5) on the surface of the surface hydrogen cutoff layer (4);

[0019] The passivation layer (5) on the surface of the second connecting wall (12) of the first groove (7) and the surface passivation layer (5) on the surface of the second connecting wall (12) of the second groove (8) are etched using a photolithography development and etching process, and metal layers (6) are grown on the surfaces after the etching process to obtain a source metal contact (61) located in the first groove (7) and a drain metal contact (62) located in the second groove (8), wherein the source metal contact (61) and the drain metal contact (62) are both electrically connected to the surface hydrogen cut-off layer (4) through the surface passivation layer (5);

[0020] A metal layer (6) is grown on the surface of the first connecting wall (9) to obtain a gate metal (63).

[0021] In a possible implementation, metal nickel is deposited on the diamond epitaxial layer (2) to perform thermochemical etching on the diamond epitaxial layer (2) to generate a first groove (7) and a second groove (8), comprising:

[0022] Performing photolithography on the diamond epitaxial layer (3) covered with a photoresist film;

[0023] A vacuum evaporation process is used to deposit metal nickel on the diamond epitaxial layer (2) after photolithography, so as to perform thermochemical etching on the diamond epitaxial layer (2) to generate a first groove (7) and a second groove (8).

[0024] In a possible implementation, a metal layer (6) is grown on the surface of the first connecting wall (9) to obtain a gate metal (63), comprising:

[0025] Spin coating photoresist on the surface of the surface passivation layer (5);

[0026] The photoresist is processed by a photolithography and development process, and metal is deposited on the processed surface;

[0027] The deposited metal is processed by a lift-off process to obtain the gate metal (63).

[0028] In a possible implementation, obtaining a source metal contact (61) located in the first groove (7) and a drain metal contact (62) located in the second groove (8) includes:

[0029] Etching the surface passivation layer (5) on the surface of the second connecting wall (12) of the first groove (7) until the surface hydrogen stop layer (4) is reached, and etching the surface passivation layer (5) on the surface of the second connecting wall (12) of the second groove (8) until the surface hydrogen stop layer (4) is reached;

[0030] A source metal contact (61) is formed through the surface passivation layer (5) and electrically connected to the surface hydrogen cutoff layer (4) and located in the first groove, and a drain metal contact (62) is formed through the surface passivation layer (5) and electrically connected to the surface hydrogen cutoff layer (4) and located in the second groove (8).

[0031] In a possible implementation manner, the diamond epitaxial layer (2) is treated by a diamond surface hydrogenation process, and after a surface hydrogen cutoff layer (4) is generated on the surfaces of the first groove (7), the second groove (8) and the first connecting wall (9), the method further comprises:

[0032] placing the surface hydrogen cutoff layer (4) in a specific gas for physical adsorption;

[0033] The specific gases include some or all of the following: nitrogen dioxide, ozone, nitric oxide, and sulfur dioxide.

[0034] In a possible implementation, before obtaining the source metal contact (61) located in the first groove (7) and the drain metal contact (62) located in the second groove (8), the method further includes:

[0035] Use room temperature ion implantation process to implant heavy doping with target concentration and target energy in specific areas;

[0036] The specific area is an orthographic projection area of ​​the source metal contact (61) on the diamond substrate (1), and an orthographic projection area of ​​the drain metal contact (62) on the diamond substrate (1).

[0037] In a possible implementation, after depositing metal nickel on the diamond epitaxial layer (2) to perform thermochemical etching on the diamond epitaxial layer (2) to generate the first groove (7) and the second groove (8), the method further comprises:

[0038] An epitaxial process is used to generate at least one heavily boron-doped buried layer (14) on the surface of the diamond epitaxial layer (2), wherein an orthographic projection of the heavily boron-doped buried layer (14) on the diamond substrate (1) overlaps with an orthographic projection of the second connecting wall (12) of the first groove (7) on the diamond substrate (1), an orthographic projection of the second connecting wall (12) of the second groove (8) on the diamond substrate (1), and an orthographic projection of the first connecting wall (9) on the diamond substrate (1).

[0039] In a third aspect, the present application provides an electronic device, comprising: a substrate, and a diamond-based transistor device as described in any one of the first aspects, wherein the diamond-based transistor device is disposed on the substrate.

[0040] The beneficial effects of the present invention are as follows:

[0041] The present invention provides a diamond-based transistor device, a manufacturing method thereof and an electronic device. A first groove, a second groove and a first connecting wall connecting the first groove and the second groove are arranged in a surface hydrogen cutoff layer. The first groove and the second groove both have side walls and a second connecting wall connecting all the side walls. All the side walls are of the diamond {111} crystal plane family and have an inclination angle relative to the surface of a diamond substrate greater than 0 degree. The first connecting wall and the second connecting wall are both parallel to the surface of the diamond substrate. A metal layer comprises a source metal contact, a drain metal contact and a gate metal. The source metal contact is located on the surface of the second connecting wall of the first groove, the drain metal contact is located on the surface of the second connecting wall of the second groove, and the gate metal is located on the surface of the first connecting wall. Since the first groove and the second groove are obtained by depositing metal nickel on a diamond epitaxial layer to perform thermochemical etching on the diamond epitaxial layer, the side walls are atomically smooth wall surfaces and are of the diamond {111} crystal plane family. The inclination angles between the side walls and the diamond substrate are greater than 0 degree. Therefore, the mobility of the conductive channel of the device can be increased, thereby improving the performance of the diamond-based transistor device. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0043] Figure 1 A cross-sectional view of a diamond-based transistor device provided in an embodiment of the present application;

[0044] Figure 2 A schematic diagram of the structure of a groove provided in an embodiment of the present application;

[0045] Figure 3 A cross-sectional view of another diamond-based transistor device provided in an embodiment of the present application;

[0046] Figure 4 A cross-sectional view of another diamond-based transistor device provided in an embodiment of the present application;

[0047] Figure 5 A flow chart of a method for manufacturing a diamond-based transistor device provided in an embodiment of the present application;

[0048] Figure 6a A schematic diagram of a nickel metal area defined on a surface provided in an embodiment of the present application;

[0049] Figure 6b A schematic diagram of a cross section of a groove etched along a diamond surface provided in an embodiment of the present application;

[0050] Figure 7 A schematic cross-sectional view of forming a first groove and a second groove, growing a surface hydrogen cutoff layer, and covering a surface passivation layer in a device provided in an embodiment of the present application;

[0051] Figure 8 A schematic cross-sectional view of a device provided in an embodiment of the present application, in which openings are provided at the bottom of a first groove and a second groove, and source and drain metals are deposited to form ohmic contacts;

[0052] Fig. 9 A schematic diagram of a top-down device structure of a diamond-based transistor device provided in an embodiment of the present application;

[0053] Fig.10 A schematic diagram of the structure of an electronic device provided in an embodiment of the present application. DETAILED DESCRIPTION

[0054] The following will be combined with the accompanying drawings to describe in detail a diamond-based transistor device, a method for manufacturing the same, and a specific implementation of an electronic device provided by an embodiment of the present invention. It should be noted that the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0055] The embodiment of the present invention provides a diamond-based transistor device, such as Figure 1 and Figure 2 As shown, it includes: a metal layer 6, a diamond substrate 1, and a diamond epitaxial layer 2, a surface hydrogen cutoff layer 4 and a surface passivation layer 5 which are sequentially stacked on the diamond substrate 1;

[0056] The diamond epitaxial layer 2 is provided with a first groove 7, a second groove 8 and a first connecting wall 9 connecting the first groove 7 and the second groove 8. The first groove 7 and the second groove 8 both have side walls and a second connecting wall 12 connecting all the side walls. All the side walls are arranged opposite to each other and have an inclination angle greater than 0 degree relative to the surface of the diamond substrate 1. The first connecting wall 9 and the second connecting wall 12 are both parallel to the surface 1 of the diamond substrate.

[0057] The metal layer 6 includes a source metal contact 61, a drain metal contact 62 and a gate metal 63. The source metal contact 61 is located on the surface of the second connecting wall 12 of the first groove 7, and is electrically connected to the surface hydrogen cutoff layer 4 through the surface passivation layer 5. The drain metal contact 62 is located on the surface of the second connecting wall 12 of the second groove 8, and is electrically connected to the surface hydrogen cutoff layer 4 through the surface passivation layer 5. The gate metal 63 is located on the surface of the first connecting wall 9.

[0058] The first groove 7 and the second groove 8 are obtained by depositing metal nickel on the diamond epitaxial layer 2 to perform thermochemical reaction etching on the diamond epitaxial layer 2 .

[0059] In a specific implementation, the diamond substrate 1 may be synthesized using the HPHT method. <100> The crystal-oriented single crystal diamond substrate is preferably a single crystal diamond substrate having a size of 4x4x0.5 mm.

[0060] MPCVD (microwave plasma chemical vapor deposition) diamond epitaxy is performed on the diamond substrate 1 to obtain a diamond epitaxial layer 2, wherein the radio frequency frequency of the MPCVD may be 2.45 GHz.

[0061] After obtaining the diamond epitaxial layer 2, metal nickel is deposited on the diamond epitaxial layer 2, and a thermochemical reaction occurs between the metal nickel and the diamond in contact therewith, and thermochemical etching is performed on the diamond surface to obtain the first groove 7 and the second groove 8. Specifically, the carbon atoms on the surface of the diamond epitaxial layer 2 undergo a solid solution reaction with the nickel metal and diffuse to the nickel metal surface; the nickel metal surface is oxidized by water vapor, and the dissolved carbon atoms diffuse to the nickel oxide according to the concentration gradient; the nickel oxide reacts with the carbon atoms diffused to the surface, and the carbon atoms react with the oxygen atoms in the nickel oxide to generate gaseous carbon dioxide and carbon monoxide; these steps continue to occur during the wet annealing process, and the process of carbon dioxide and carbon monoxide detaching from the surface nickel oxide also inhibits the saturation of carbon atoms in the nickel metal; the thermochemical reaction continues, and high-speed thermochemical etching is achieved on the diamond surface.

[0062] It should be noted that the entire process of forming the first groove 7 and the second groove 8 under the steam heating condition is a wet annealing process.

[0063] In the specific implementation, Figure 2As shown, the side walls of the first groove 7 and the second groove 8 may include four side walls, namely the first side wall 10, the second side wall 11, the third side wall (not shown in the figure) and the fourth side wall (not shown in the figure). The first side wall 10, the second side wall 11, the third side wall and the fourth side wall all belong to the {111} crystal plane family, which is a diamond {111} crystal plane family composed of carbon atoms with three covalent bonds. Relative to all orientation planes, its thermochemical reaction etching is the most stable.

[0064] The first side wall 10 and the second side wall 11 are arranged opposite to each other, and the third side wall and the fourth side wall are arranged opposite to each other.

[0065] It should be noted that the diamond epitaxial layer 2 in the embodiment of the present application is diamond <100> Crystal direction; it should also be noted that when performing thermochemical etching, since the dissolved carbon atoms diffuse toward the nickel oxide according to the concentration gradient, the first groove 7 and the second groove 8 formed are both inverted trapezoidal structures, that is, the first groove 7 and the second groove 8 have a first side wall and a second side wall opposite to each other, and also have a second connecting wall connecting the first side wall and the second side wall.

[0066] After the first groove 7 and the second groove 8 are obtained, a hydrogenation reaction is performed on the diamond surface, and the diamond surface is exposed to hydrogen plasma to obtain a surface hydrogen termination layer (H-termination surface) 4. Under the surface hydrogen termination layer 4 structure of the diamond, the carbon atoms and hydrogen atoms on the diamond surface form bonds (CH), inducing a p-type conductive region in the diamond, namely, a two-dimensional hole gas (2DHG). The depth of the longitudinal distribution of the two-dimensional hole gas (2DHG) is about 0.2nm.

[0067] It should be noted that the above-mentioned p-type conductive region is distributed in a layer about 0.2 nm vertically downward from the surface of the diamond material.

[0068] In one embodiment, in order to increase the 2DHG concentration, the diamond surface hydrogen cutoff layer 4 can be exposed to a specific gas for physical adsorption, such as nitrogen dioxide (NO2), ozone (O3), nitric oxide (NO) or sulfur dioxide (SO2) and other gases, thereby increasing the surface concentration of two-dimensional hole gas on the diamond surface.

[0069] In the scenario of physical adsorption of nitrogen dioxide (NO2) on the surface, the surface concentration of two-dimensional hole gas (2DHG) can reach 3.8e13 / cm2 through calculation, and the experimental value can reach 9e13 / cm2. The surface density of two-dimensional hole gas (2DHG) strongly depends on the type of adsorbed molecules.

[0070] It should be noted that not all gases with adsorption function are suitable for the embodiments of the present application. For example, the adsorption of nitrogen dioxide (NO2), ozone (O3), nitric oxide (NO) or sulfur dioxide (SO2) can increase the surface density of the two-dimensional vacancy gas (2DHG), while the adsorption of nitrous oxide or carbon dioxide has little or no effect on the surface density of the two-dimensional vacancy gas (2DHG). The specific gas with adsorption function used in the implementation can be obtained through experiments. In addition, the surface charge concentration of the two-dimensional vacancy gas (2DHG) of the system calculated by water molecule adsorption is about 0.35e13 / cm2, which is one order of magnitude smaller than the diamond surface hydrogen cutoff layer 4 adsorbing nitrogen dioxide.

[0071] In a specific implementation, the first side wall 10 has an inclination angle of 125 degrees relative to the surface of the diamond substrate 1 , and the second side wall 11 has an inclination angle of 55 degrees relative to the surface of the diamond substrate 1 ; the depth of the first groove 7 and the second groove 8 relative to the diamond substrate 1 is 0-100 μm.

[0072] Correspondingly, the inclination angle of the third side wall relative to the surface of the diamond substrate 1 is 125 degrees, and the inclination angle of the fourth side wall 11 relative to the surface of the diamond substrate 1 is 55 degrees.

[0073] In one embodiment, a surface passivation layer 5 is deposited on the surface of the surface hydrogen cutoff layer 4. Preferably, the surface passivation layer 5 is an aluminum oxide film layer. The surface passivation layer 5 can protect the gas molecules physically adsorbed on the device surface and improve the reliability of the diamond device.

[0074] Furthermore, holes are opened in the surface passivation layer 5 on the surface of the second connecting wall 12 located in the first groove 7 and the surface passivation layer 5 on the surface of the second connecting wall 12 located in the second groove 8, and then metals are deposited using a PVD (physical vapor deposition) method, for example, titanium (Ti), aluminum (Al) and gold (Au) are deposited in sequence, and through wet etching and annealing processes, ohmic contacts (source metal contact 61, drain metal contact 62) of the device are formed.

[0075] Furthermore, a gate metal 6 is deposited on the surface. Preferably, the gate metal 6 may be made of metal aluminum (Al), and a lift-off process is used to define the gate region.

[0076] In one embodiment, the diamond-based transistor device may further include at least one heavily boron-doped buried layer 14, such as Figure 3 and Figure 4 As shown;

[0077] The heavily boron-doped buried layer 14 is located between the diamond epitaxial layer 2 and the surface hydrogen cutoff layer 4, and the orthographic projection of the heavily boron-doped buried layer 14 on the diamond substrate 1 overlaps with the orthographic projection of the second connecting wall 12 of the first groove 7 on the diamond substrate 1, the orthographic projection of the second connecting wall 12 of the second groove 8 on the diamond substrate 1, and the orthographic projection of the first connecting wall 9 on the diamond substrate 1.

[0078] In the embodiment of the present application, the heavily boron-doped region corresponds to the interior of the diamond under the gate metal 63, the source metal contact 61, and the drain metal contact 62. Preferably, the thickness of the heavily boron-doped buried layer 14 is less than 2 nm, the doping concentration is >1e20 / cm3, and the distance from the diamond surface is 2 to 10 nm. The heavily boron-doped buried layer 14 can partially enhance the charge surface density of the two-dimensional hole gas (2DHG) (the region under the gate metal layer) and the ohmic contact of the source and drain regions (the region under the source metal contact 61 and the drain metal contact 62). Preferably, in the structure of the device, the source metal contact 61 extends and is connected to the external source contact pad; the drain metal contact 62 extends and is connected to the external drain contact pad; and the gate metal 63 extends and is connected to the gate contact pad. The gate metal 63, the source metal contact 61, and the drain metal contact 62 can all be interconnected through interlayer metal to overlap the contact pad with the active area.

[0079] like Figure 3 As shown, the heavily boron doped buried layer 14 may include a layer such as Figure 4 As shown, the heavily boron-doped buried layer 14 may also include multiple layers. The multiple layers of heavily boron-doped buried layer 14 may better enhance the charge surface density of the two-dimensional hole gas (2DHG) and the ohmic contact of the source and drain regions.

[0080] Based on the same inventive concept, an embodiment of the present invention further provides a method for manufacturing a diamond-based transistor device. The implementation principle of the manufacturing method is similar to the implementation principle of the aforementioned diamond-based transistor device. The specific implementation method of the manufacturing method can refer to the embodiment of the aforementioned diamond-based transistor device, and the repeated parts will not be repeated.

[0081] Specifically, an embodiment of the present invention provides a method for manufacturing a diamond-based transistor device, such as Figure 5 As shown, including:

[0082] S501, forming a diamond epitaxial layer 2 on a diamond substrate 1;

[0083] S502, depositing metal nickel on the diamond epitaxial layer 2 to perform thermochemical etching on the diamond epitaxial layer 2 to generate a first groove 7 and a second groove 8, wherein the first groove 7 and the second groove 8 are connected by a first connecting wall 9, the first groove 7 and the second groove 8 both have side walls and a second connecting wall 12 connecting all the side walls, the inclination angles of all the side walls relative to the surface of the diamond substrate 1 are greater than 0 degrees, and the first connecting wall 9 and the second connecting wall 12 are both parallel to the surface of the diamond substrate 1;

[0084] S503, treating the diamond epitaxial layer 2 with a diamond surface hydrogenation process to generate a surface hydrogen cutoff layer 4 on the surfaces of the first groove 7, the second groove 8 and the first connecting wall 12;

[0085] S504, depositing a surface passivation layer 5 on the surface of the surface hydrogen cutoff layer 4;

[0086] S505, etching the surface passivation layer 5 on the surface of the second connecting wall 12 of the first groove 7 and the surface passivation layer 5 on the surface of the second connecting wall 12 of the second groove 8 by using a photolithography development and etching process, and growing metal layers 6 on the surfaces after the etching respectively, to obtain a source metal contact 61 located in the first groove 7 and a drain metal contact 62 located in the second groove 8, wherein the source metal contact 61 and the drain metal contact 62 are both electrically connected to the surface hydrogen cutoff layer 4 through the surface passivation layer 5;

[0087] S506 , growing a metal layer 6 on the surface of the first connecting wall 9 to obtain a gate metal 63 .

[0088] In one embodiment, first prepare <100> A diamond substrate 1 having a crystal orientation of 4 mm by 4 mm by 0.5 mm, or <100> The diamond substrate 1 with a crystal orientation of 4.5 x 4.5 x 0.5 mm can be synthesized by HPHT method, preferably, a diamond substrate with low impurity concentration is selected, such as nitrogen atom and boron atom concentration <5 ppb and <1 ppb respectively. Optionally, a IIa type single crystal diamond (100) substrate synthesized by chemical vapor deposition can also be used.

[0089] preparation <100> After preparing a diamond substrate 1 with a crystal direction of 4 mm x 4 mm x 0.5 mm, <100> Diamond epitaxy is performed on a diamond substrate 1 having a crystal direction of 4 mm by 4 mm by 0.5 mm by using MPCVD (microwave plasma chemical vapor deposition) to obtain a diamond epitaxial layer 2 .

[0090] Preferably, the total reaction gas flow of the microwave plasma chemical vapor deposition is 400-900 sccm, wherein the main carrier gas is hydrogen, the components include 2.5%-8.5% methane and 5%-15% argon, the reaction pressure is greater than 15 kPa, and the heating temperature of the diamond substrate 1 is about 800°C-900°C.

[0091] Optionally, in a specific implementation, after the diamond epitaxial layer 2 is generated, a laser cut process may be used to obtain a separate diamond epitaxial layer 2. Preferably, the thickness of the diamond epitaxial layer 2 is 400 μm to 700 μm.

[0092] After obtaining the diamond epitaxial layer 2, the next step is to form a first groove 7 and a second groove 8 on the diamond epitaxial layer 2. Currently, traditional wet etching is ineffective for diamond. The embodiment of the present application uses anisotropic diamond etching of the thermochemical reaction between nickel and diamond in high-temperature water vapor. The diamond under the nickel metal layer is selectively etched to obtain the first groove 7 and the second groove 8.

[0093] In one embodiment, metal nickel is deposited on the diamond epitaxial layer 2 to perform thermochemical etching on the diamond epitaxial layer 2 to generate the first groove 7 and the second groove 8, including:

[0094] Performing photolithographic development on the diamond epitaxial layer 2 covered with the photoresist film;

[0095] By using a vacuum evaporation process, a specific pattern of metal nickel is deposited on the diamond epitaxial layer 2 after photolithography and development, so as to perform thermochemical etching on the diamond epitaxial layer 2 to generate a first groove 7 and a second groove 8 .

[0096] In a specific implementation, the diamond substrate 1 and the diamond epitaxial layer 2 are first cleaned by SPM to remove surface contamination, and then a photoresist is spin-coated on the surface of the diamond epitaxial layer 2. With the help of a photolithography development process, an opening of a specific pattern is formed on the photoresist on the diamond surface. Then, a vacuum evaporation process is used to deposit about 0.2 μm of metallic nickel on the surface of the diamond epitaxial layer 2, and a lift-off process is used to form a metallic nickel deposition with a specific pattern.

[0097] Furthermore, the device is treated at 900°C to 1000°C for 10 to 40 minutes in a water vapor environment in a quartz tube, and water vapor is allowed to enter the quartz tube by using 400 sccm of nitrogen gas as a carrier gas (through an ultrapure water bubbling method), thereby forming a diamond etched structure. Finally, the device is treated in a hot acid mixture HMA (preferably, such as H2SO4 / HNO3 (3:1) at 220°C for 20 minutes to remove the nickel and nickel oxide film layers deposited on the diamond surface at this time, thereby obtaining a diamond etched structure, namely, the first groove 7 and the second groove 8.

[0098] It should be noted that the present application uses metal nickel to etch the diamond epitaxial layer 2. Compared with the related art using plasma process to test diamond, it can reduce the diamond surface damage caused by plasma etching, thereby reducing the probability of device performance.

[0099] The first groove 7 and the second groove 8 obtained by the method provided in the embodiment of the present application are as follows: Figure 6a and Figure 6b As shown, the first groove 7 and the second groove 8 are both truncated etched grooves.

[0100] like Figure 6a and Figure 6b As shown, a schematic diagram of anisotropic etching cross-section of the thermochemical reaction between nickel and diamond in high-temperature water vapor, the size of the nickel metal film layer on the surface is 100 times 100 μm; Figure 6a Schematic diagram of the nickel metal region defined on the surface; Figure 6b Schematic diagram of the cross section of a groove etched along the surface of a diamond.

[0101] from Figure 6b It can be seen that in the embodiment of the present application, the inclination angle of the first side wall 10 relative to the surface of the diamond substrate 1 is 125 degrees, and the inclination angle of the second side wall 11 relative to the surface of the diamond substrate 1 is 55 degrees; the depth of the first groove 7 and the second groove 8 relative to the diamond substrate is 46 μm.

[0102] It should be noted that, during the process of etching diamond with nickel, the thickness of the area on the surface of the diamond epitaxial layer 2 that is not covered by the nickel metal deposition does not change.

[0103] After the first groove 7 and the second groove 8 are formed, the diamond epitaxial layer 2 is treated using a diamond surface hydrogenation process to generate a surface hydrogen cutoff layer 4 on the surface of the diamond epitaxial layer 2. Preferably, the diamond device is heated to 700° C. in an MPCVD chamber, the reaction power is 1 kW to 1.5 kW, and the radio frequency is 2.45 GHz; the surface of the diamond device is exposed to the hydrogen microwave plasma for preferably 1 hour, and the reaction pressure of the cavity is 40 mbar, thereby generating a surface hydrogen cutoff layer 4 of the diamond.

[0104] Optionally, in one embodiment, the diamond epitaxial layer 2 is treated by a diamond surface hydrogenation process, and after a surface hydrogen cutoff layer 4 is generated on the surface of the diamond epitaxial layer 2, the method further includes:

[0105] Placing the surface hydrogen cutoff layer 4 in a specific gas for physical adsorption;

[0106] Among them, specific gases include some or all of the following: nitrogen dioxide, ozone, nitric oxide, and sulfur dioxide.

[0107] Specifically, after obtaining the surface hydrogen cutoff layer 4, the diamond surface hydrogen cutoff layer 4 is exposed to gases such as nitrogen dioxide, ozone (O3), nitrogen monoxide (NO) and sulfur dioxide (SO2) to further increase the surface concentration of diamond two-dimensional vacancy gas. Preferably, the diamond surface is exposed to a high concentration of nitrogen dioxide gas (containing 2% nitrogen dioxide in a nitrogen carrier gas) for 30 minutes to 40 minutes.

[0108] In one embodiment, a surface passivation layer 5 deposited on the surface of the diamond groove structure is preferably an aluminum oxide film layer, and the ALD (atomic layer deposition) process method can be used. The thickness of the aluminum oxide is 15 to 20 nm, and the preferred reaction temperature is 150°C.

[0109] like Figure 7 , which is a schematic cross-sectional view of forming the first groove 7 and the second groove 8 , growing the surface hydrogen cutoff layer 4 and covering the surface passivation layer 5 .

[0110] In one embodiment, obtaining the source metal contact 61 located in the first groove 7 and the drain metal contact 62 located in the second groove 8 includes:

[0111] Etching the surface passivation layer 5 on the surface of the second connecting wall 12 of the first groove 7 until the surface hydrogen cutoff layer 4 is reached, and etching the surface passivation layer 5 on the surface of the second connecting wall 12 of the second groove 8 until the surface hydrogen cutoff layer 4 is reached;

[0112] A source metal contact 61 is formed through the surface passivation layer 5 and electrically connected to the surface hydrogen cutoff layer 4 and located in the first groove, and a drain metal contact 62 is formed through the surface passivation layer 5 and electrically connected to the surface hydrogen cutoff layer (4) and located in the second groove 8.

[0113] Specifically, the second connecting wall 12 of the first groove 7 and the second connecting wall 12 of the second groove 8 are opened by photolithography and development, and the aluminum oxide film is etched to reach the surface hydrogen cutoff layer 4. Further, a metal layer is grown, and a lift-off process is used to obtain source and drain contacts of the device.

[0114] Preferably, in one embodiment, before obtaining the source metal contact (61) located in the first groove (7) and the drain metal contact (62) located in the second groove (8), the method further comprises:

[0115] Use room temperature ion implantation process to implant heavy doping with target concentration and target energy in specific areas;

[0116] The specific area is an orthographic projection area of ​​the source metal contact (61) on the diamond substrate (1), and an orthographic projection area of ​​the drain metal contact (62) on the diamond substrate (1).

[0117] Specifically, before the metal layer growth process, room temperature ion implantation can be used, with a heavy doping concentration of 2e16 / cm2 and an implantation energy of 37keV, followed by annealing at 1100°C in a vacuum, and further, Ti / Al / Au contacts (PVD growth, then wet etching) are grown as source and drain contacts, followed by Ar annealing at 600°C to form ohmic contacts. Optionally, metal gold deposition is used as the source and drain contacts of the device, and a lift-off process is used to define the source and drain regions.

[0118] like Figure 8 , which is a schematic cross-sectional view of a device provided in an embodiment of the present application after openings are made at the bottom of the first groove and the second groove and ohmic contacts are deposited.

[0119] In one embodiment, a metal layer 6 is grown on the surface of the first connecting wall 9 to obtain a gate metal 63, including:

[0120] Spin-coat a photoresist on the surface of the surface passivation layer 5;

[0121] The photoresist is processed by a photolithography and development process, and metal is deposited on the processed surface;

[0122] The deposited metal is processed by a lift-off process to obtain the gate metal (63).

[0123] Specifically, a photoresist is spin-coated on the surface of the surface passivation layer, an opening of the photoresist layer is opened by a photolithography development method, a gate metal is deposited, and a lift-off process is used to define a gate region.

[0124] In one embodiment, after depositing metal nickel on the diamond epitaxial layer 2 to perform thermochemical etching on the diamond epitaxial layer 2 to generate the first groove 7 and the second groove 8, the method further includes:

[0125] An epitaxial process is used to generate at least one heavily boron-doped buried layer 14, wherein the orthographic projection of the heavily boron-doped buried layer 14 on the diamond substrate 1 overlaps with the orthographic projection of the second connecting wall 12 of the first groove 7 on the diamond substrate 1, the orthographic projection of the second connecting wall 12 of the second groove 8 on the diamond substrate 1, and the orthographic projection of the first connecting wall 9 on the diamond substrate 1.

[0126] Specifically, after generating the first groove 7 and the second groove 8, a heavily boron-doped buried layer 14 is generated by an epitaxial method on the surface of the first connecting wall 9, the surface of the second connecting wall 12 of the first groove 7, and the surface of the second connecting wall 12 of the second groove 8 to increase the concentration of 2DHG in the horizontal direction of the device and form an ohmic contact between the source metal contact 61 and the drain metal contact 62.

[0127] The thickness of the heavily boron-doped buried layer 14 is preferably 0.36 nm to 2 nm. The position of the heavily boron-doped buried layer 14 corresponding to the first connecting wall 9 is preferably 0.2 nm to 10 nm away from the surface hydrogen stop layer 4 in the longitudinal direction. The position of the heavily boron-doped buried layer 14 corresponding to the second connecting wall 12 of the first groove 7 and the position of the heavily boron-doped buried layer 14 corresponding to the second connecting wall 12 of the second groove 7 are opened on the silicon dioxide mask by a photolithography method to define the bottom area of ​​the source metal contact 61 and the drain metal contact 62 for selective epitaxy of the heavily boron-doped buried layer 14, preferably 0.2 nm to 10 nm away from the surface hydrogen stop layer 4 in the longitudinal direction. The heavily boron-doped buried layer 14 can be doped with gas-phase boron by adding diborane (B2H6) during the MOCVD epitaxy process, and the heavy boron doping concentration is preferably 1e20 to 1e21 / cm3.

[0128] like Fig. 9 As shown, it is a schematic diagram of the top view of the device structure of the diamond-based transistor device provided by the embodiment of the present invention, including a diamond substrate 1 (not shown), a diamond epitaxial layer 2 (not shown), a first groove 7, a second groove 8, a surface hydrogen cutoff layer 4 (all covered), a surface passivation layer 5 (all covered except the source metal contact and drain metal contact areas), a gate metal 63, a source metal contact 61, a drain metal contact 62, and a heavily boron-doped buried layer 14 (not shown). The blank space between the first groove 7, the second groove 8 and the gate metal 63 is the area where the diamond table does not cover the gate metal layer. Among them, the gate metal 63, the source metal contact 61, and the drain metal contact 62 are led out through the top metal interconnection at the back end.

[0129] The diamond-based transistor device and the manufacturing method thereof provided in the embodiments of the present invention aim to enhance the device performance in terms of channel mobility and two-dimensional hole gas density under the same LGS (gate-source distance) and LGD (gate-drain distance) channel length conditions. Figure 2 As shown, in the truncated etched groove morphology, atomically smooth terrace surfaces (first connecting wall) and terrace sidewalls (first sidewall, second sidewall, third sidewall and fourth sidewall) ({111} crystal plane family) can be obtained; for the rougher truncated etched groove bottom (second connecting wall), we use it as the area for ohmic contact between the source and drain.

[0130] Further, in Figure 3 and Figure 4 In the present invention, MPCVD (diamond epitaxy) is performed on a diamond substrate 1 to obtain a diamond epitaxial layer 2. During the MPCVD diamond epitaxy process, gas phase boron doping is performed by diborane (B2H6) to obtain a heavily boron doped buried layer 14. The heavy boron doping concentration can reach 1e20 / cm3 to 1e21 / cm3 or more. An undoped diamond epitaxial layer 2 is epitaxially grown on the diamond substrate 1. The activation energy of boron doping decreases with the increase of the doping level and disappears at the metal-insulator transition. Due to heavy boron doping, the mobility of the local area is reduced. The way to overcome this difficulty is to generate free holes (heavy boron doped layer, the doping level is greater than the critical concentration of metal-medium conversion) and delocalized carriers in specific areas of the device to allow the device to contribute to the output current in the low doping concentration area. The quantum effect of the very thin heavily boron doped buried layer 14 is required to cause hole delocalization, while allowing hole carriers to be distributed near the heavily boron doped buried layer 14 area due to wave function expansion.

[0131] Numerical simulations predict that for a heavily boron-doped buried layer thickness of about 2nm, up to 95% of hole transport will occur in the intrinsic region outside the heavily boron-doped buried layer. This greatly improves the ohmic contact performance of the source and drain metal contacts, and increases the two-dimensional hole gas density in the horizontal direction on the table, greatly increasing the lateral current density of the device.

[0132] Furthermore, due to the use of anisotropic diamond etching with thermochemical reaction, part of the two-dimensional hole gas conductive channel is located at the bottom of the (111) crystal plane of the sidewall of the first groove 7 of the device, induced by the surface hydrogen cutoff layer 4 of the diamond and the optional physical gas adsorption layer thereon. Since the diamond {111} plane family composed of carbon atoms has three covalent bonds, the electron carrier mobility of diamond on the (111) crystal plane can reach 308cm 2 / Vs, is the (100) crystal plane electron carrier mobility 117cm 2 / Vs is nearly 3 times. The present invention greatly improves the mobility of the conductive channel of the diamond table sidewall (first sidewall, second sidewall, third sidewall, fourth sidewall), and obtains a diamond-based high power density transistor device with higher current density.

[0133] Further, we can repeat the selective heavy boron doping of the buried layer 14 epitaxy in the source metal contact and drain metal contact bottom regions, and in the diamond region at the bottom of the gate, such as Figure 4 As shown, a heavily boron-doped buried layer 14 with longitudinal periodic distribution is obtained.

[0134] The thickness of the heavily boron-doped buried layer 14 is preferably 0.36 nm to 2 nm. The longitudinal spacing of each layer of the heavily boron-doped buried layer 14 inside the heavily boron-doped buried layer 14 is preferably 0.2 nm to 10 nm between any layer of the heavily boron-doped buried layer 14 and the adjacent heavily boron-doped buried layer 14. The free hole density in the illustrated area is further enhanced, the ohmic contact characteristics of the device are further improved, and the on-current of the device is increased.

[0135] Based on the same inventive concept, an embodiment of the present invention further provides an electronic device, the implementation principle of which is similar to the implementation principle of the aforementioned diamond-based transistor device. The specific implementation method of the electronic device can refer to the embodiment of the aforementioned diamond-based transistor device, and the repeated parts will not be repeated.

[0136] Specifically, an electronic device provided by an embodiment of the present invention is Fig.10 As shown, it includes: a substrate 1101 and a diamond-based transistor device 1102 as described in the above embodiment, and the diamond-based transistor device 1102 is arranged on the substrate 1101.

[0137] The electronic device may be any electronic device including a diamond-based transistor device, such as an AC motor, a frequency converter, a switching power supply, a lighting circuit, etc.

[0138] Those skilled in the art may make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.

Claims

1. A diamond-based transistor device, characterized in that: include: A metal layer (6), a diamond substrate (1), and a diamond epitaxial layer (2), a surface hydrogen cutoff layer (4), and a surface passivation layer (5) sequentially stacked on the diamond substrate (1); The surface of the diamond epitaxial layer (2) is provided with a first groove (7), a second groove (8) and a first connecting wall (9) connecting the first groove (7) and the second groove (8); the first groove (7) and the second groove (8) both have side walls and a second connecting wall (12) connecting all the side walls; the inclination angles of all the side walls relative to the surface of the diamond substrate (1) are greater than 0 degrees; and the first connecting wall (9) and the second connecting wall (12) are both parallel to the surface of the diamond substrate (1); The metal layer (6) comprises a source metal contact (61), a drain metal contact (62) and a gate metal (63); the source metal contact (61) is located on the surface of the second connecting wall (12) of the first groove (7), and is electrically connected to the surface hydrogen stop layer (4) through the surface passivation layer (5); the drain metal contact (62) is located on the surface of the second connecting wall (12) of the second groove (8), and is electrically connected to the surface hydrogen stop layer (4) through the surface passivation layer (5); and the gate metal (63) is located on the surface of the first connecting wall (9); Wherein, the diamond-based transistor device further comprises at least one heavily boron-doped buried layer (14); The heavily boron-doped buried layer (14) is located between the diamond epitaxial layer (2) and the surface hydrogen cut-off layer (4), and an orthographic projection of the heavily boron-doped buried layer (14) on the diamond substrate (1) overlaps with an orthographic projection of the second connecting wall (12) of the first groove (7) on the diamond substrate (1), an orthographic projection of the second connecting wall (12) of the second groove (8) on the diamond substrate (1), and an orthographic projection of the first connecting wall (9) on the diamond substrate (1).

2. The diamond-based transistor device according to claim 1, characterized in that All of the side walls belong to the {111} crystal plane family.

3. The diamond-based transistor device according to claim 2, characterized in that The side wall comprises a first side wall (10) and a second side wall (11); The inclination angle of the first side wall (10) relative to the surface of the diamond substrate (1) is 125 degrees, and the inclination angle of the second side wall (11) relative to the surface of the diamond substrate (1) is 55 degrees.

4. A method for manufacturing a diamond-based transistor device according to any one of claims 1 to 3, characterized in that: include: Forming a diamond epitaxial layer (2) on a diamond substrate (1); Depositing metal nickel on the diamond epitaxial layer (2) to perform thermochemical etching on the diamond epitaxial layer (2) to generate a first groove (7) and a second groove (8), wherein the first groove (7) and the second groove (8) are connected via a first connecting wall (9), the first groove (7) and the second groove (8) both have side walls and a second connecting wall (12) connecting all the side walls, the inclination angles of all the side walls relative to the surface of the diamond substrate (1) are greater than 0 degrees, and the first connecting wall (9) and the second connecting wall (12) are both parallel to the surface of the diamond substrate (1); The diamond epitaxial layer (2) is treated by a diamond surface hydrogenation process to generate a surface hydrogen cutoff layer (4) on the surface of the diamond epitaxial layer (2); Depositing a surface passivation layer (5) on the surface of the surface hydrogen cutoff layer (4); The surface passivation layer (5) on the surface of the second connecting wall (12) of the first groove (7) and the surface passivation layer (5) on the surface of the second connecting wall (12) of the second groove (8) are etched using a photolithography development and etching process, and metal layers (6) are grown on the surfaces after the etching process to obtain a source metal contact (61) located in the first groove (7) and a drain metal contact (62) located in the second groove (8), wherein the source metal contact (61) and the drain metal contact (62) are both electrically connected to the surface hydrogen cut-off layer (4) through the surface passivation layer (5); Growing a metal layer (6) on the surface of the first connecting wall (9) to obtain a gate metal (63); Wherein, after depositing metal nickel on the diamond epitaxial layer (2) to perform thermochemical etching on the diamond epitaxial layer (2) to generate the first groove (7) and the second groove (8), the method further comprises: An epitaxial process is used to generate at least one heavily boron-doped buried layer (14) on the surface of the diamond epitaxial layer (2), wherein an orthographic projection of the heavily boron-doped buried layer (14) on the diamond substrate (1) overlaps with an orthographic projection of the second connecting wall (12) of the first groove (7) on the diamond substrate (1), an orthographic projection of the second connecting wall (12) of the second groove (8) on the diamond substrate (1), and an orthographic projection of the first connecting wall (9) on the diamond substrate (1).

5. The method according to claim 4, characterized in that Depositing metal nickel on the diamond epitaxial layer (2) to perform thermochemical etching on the diamond epitaxial layer (2) to generate a first groove (7) and a second groove (8), comprising: Performing photolithography on the diamond epitaxial layer (2) covered with a photoresist film; A vacuum evaporation process is used to deposit metal nickel on the diamond epitaxial layer (2) after photolithography, so as to perform thermochemical etching on the diamond epitaxial layer (2) to generate a first groove (7) and a second groove (8).

6. The method according to claim 4, characterized in that Growing a metal layer (6) on the surface of the first connecting wall (9) to obtain a gate metal (63), comprising: Spin coating photoresist on the surface of the surface passivation layer (5); The photoresist is processed by a photolithography and development process, and metal is deposited on the processed surface; The deposited metal is processed by a lift-off process to obtain the gate metal (63).

7. The method according to claim 4, characterized in that The step of obtaining a source metal contact (61) located in the first groove (7) and a drain metal contact (62) located in the second groove (8) comprises: Etching the surface passivation layer (5) on the surface of the second connecting wall (12) of the first groove (7) until the surface hydrogen stop layer (4) is reached, and etching the surface passivation layer (5) on the surface of the second connecting wall (12) of the second groove (8) until the surface hydrogen stop layer (4) is reached; A source metal contact (61) is formed through the surface passivation layer (5) and electrically connected to the surface hydrogen cutoff layer (4) and located in the first groove, and a drain metal contact (62) is formed through the surface passivation layer (5) and electrically connected to the surface hydrogen cutoff layer (4) and located in the second groove (8).

8. The method according to claim 4, characterized in that The method further comprises: treating the diamond epitaxial layer (2) by using a diamond surface hydrogenation process to generate a surface hydrogen cut-off layer on the surfaces of the first groove (7), the second groove (8) and the first connecting wall (9); placing the surface hydrogen cutoff layer (4) in a specific gas for physical adsorption; The specific gases include some or all of the following: nitrogen dioxide, ozone, nitric oxide, and sulfur dioxide.

9. The method according to claim 4, characterized in that Before obtaining the source metal contact (61) located in the first groove (7) and the drain metal contact (62) located in the second groove (8), the method further includes: Use room temperature ion implantation process to implant heavy doping with target concentration and target energy in specific areas; The specific area is an orthographic projection area of ​​the source metal contact (61) on the diamond substrate (1), and an orthographic projection area of ​​the drain metal contact (62) on the diamond substrate (1).

10. An electronic device, characterized in that: include: A substrate, and a diamond-based transistor device according to any one of claims 1 to 3, wherein the diamond-based transistor device is arranged on the substrate.