A kind of tert-dodecyl mercaptan and preparation method thereof

Through the reaction of acidified modified montmorillonite with tetrapolypropylene and hydrogen sulfide, a highly efficient catalyst is prepared, which solves the problems of strict catalyst reaction conditions and insufficient porosity of montmorillonite in the existing technology, and realizes the production of tertiary dodecacarbon sulfur. Efficient synthesis of alcohols.

CN118084748BActive Publication Date: 2024-10-15ZIBO RUNXIANG IND & TRADE CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410219476.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-02-28
Publication Date
2024-10-15
Estimated Expiration
2044-02-28

AI Technical Summary

Technical Problem

In the existing technology, the catalyst reaction conditions for the addition of triisobutene and H2S to synthesize tert-dodecyl mercaptan are strict, triisobutene is seriously cracked, the conversion rate and selectivity are not high, and the porosity of montmorillonite is insufficient, resulting in insufficient cation exchange capacity. Take full advantage.

Method used

By acidifying the modified montmorillonite, increasing its specific surface area and pore size, increasing chemical activity, and reacting with tetrapolypropylene and hydrogen sulfide under specific conditions, a mixed catalyst with high catalytic performance is prepared for tertiary ten Synthesis of two-carbon thiols. The method includes grinding, ultrasonic treatment, heating and stirring, drying, dehydration and calcination of montmorillonite, and adding a stabilizer to form a catalyst and improve catalytic performance.

Benefits of technology

Significantly improves the catalytic performance of the catalyst, increases the contact area between the reaction substrate and acidified montmorillonite, promotes the progress of the reaction, solves the problem of cracking of triisobutylene raw material, and improves the selectivity and conversion of tert-dodecyl mercaptan Rate.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to tert-dodecyl mercaptan and a preparation method thereof, and belongs to the technical field of tert-dodecyl mercaptan preparation. The preparation method comprises the following steps: adding tetrapropylene, hydrogen sulfide and a mixed catalyst into a reactor, mixing and reacting to obtain tert-dodecyl mercaptan; the preparation method of the mixed catalyst comprises the following steps: 1) grinding montmorillonite and adding sulfuric acid solution, heating and stirring after ultrasonic treatment, and centrifuging to obtain a preform; 2) mixing the preform and a stabilizer, drying and dehydrating, and calcining to obtain a mixed catalyst. The specific surface area of ​​the montmorillonite modified by acidification is increased, the pore size is also increased, and the montmorillonite has stronger chemical activity, and has high catalytic performance for the synthesis of tert-dodecyl mercaptan.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of tert-dodecyl mercaptan preparation and relates to tert-dodecyl mercaptan and a preparation method thereof. Background Art

[0002] Tert-dodecyl mercaptan, also known as tert-dodecyl mercaptan, tert-dodecyl mercaptan, or TDM for short, is an important mercaptan product, mainly used in the preparation of styrene-butadiene rubber, ABS resin and nitrile rubber, which can effectively reduce the branching degree of polymer chains, adjust the molecular weight, and make the molecular weight distribution uniform. At the same time, tert-dodecyl mercaptan can also be used as a stabilizer and antioxidant for polyolefins, or used in the synthesis of non-ionic surfactants, lubricant additives, organic chemicals, fungicides, pesticides, etc.

[0003] Triisobutylene was used as raw material and H 2 The catalysts for the direct addition of S to synthesize TDM mainly include: clay, silica-alumina catalysts, Lewis acid catalysts and resin catalysts. However, these catalysts generally have problems such as strict reaction conditions and severe cracking of triisobutylene during application. In order to achieve the ideal effect, the reaction usually needs to be carried out at an extremely low temperature, and the synthesis of other products using triisobutylene as a raw material also faces similar challenges of harsh reaction conditions, low conversion rate and low selectivity.

[0004] Montmorillonite is a type of soil-like mineral composed of nanometer-thick silicate sheets with negative charges on the surface, which are stacked together by the electrostatic interaction between the layers. The unit cell in its crystal structure is composed of two layers of silicon-oxygen tetrahedrons sandwiched between a layer of aluminum-oxygen octahedrons. It has a unique one-dimensional layered nanostructure and cation exchange properties, which gives montmorillonite many possibilities for modification and expansion of its application fields. However, the interlayer spacing of montmorillonite crystals is small, and impurity ions are easy to block the pores, which is not conducive to the diffusion and transmission of substances, resulting in the inability to fully utilize the cation exchange capacity. Summary of the invention

[0005] The object of the present invention is to provide tert-dodecyl mercaptan and a preparation method thereof. The specific surface area and pore size of the montmorillonite modified by acidification are increased, and the montmorillonite has stronger chemical activity and is used for the synthesis of tert-dodecyl mercaptan with high catalytic performance.

[0006] The purpose of the present invention can be achieved through the following technical solutions:

[0007] A method for preparing tert-dodecyl mercaptan comprises the following steps: adding tetrapropylene, hydrogen sulfide and a mixed catalyst into a reaction kettle, mixing and reacting to obtain tert-dodecyl mercaptan;

[0008] The preparation method of the mixed catalyst comprises the following steps:

[0009] 1) grinding montmorillonite and adding sulfuric acid solution, heating and stirring after ultrasonic treatment, removing the liquid part after centrifugation, and taking the solid as a preform;

[0010] 2) The preform and the stabilizer are mixed, dried and dehydrated, and then calcined to obtain a mixed catalyst.

[0011] As a preferred technical solution of the present invention, the molar ratio of tetrapropylene to hydrogen sulfide is 3-6:1.

[0012] As a preferred technical solution of the present invention, the amount of the mixed catalyst is 3-5% of the total mass of tetrapropylene and hydrogen sulfide; the present invention uses tetrapropylene as raw material, and the TDM selectivity is extremely high, which solves the problem of cracking triisobutylene raw material.

[0013] As a preferred technical solution of the present invention, the reaction conditions are 100-130° C., 1.5-2.0 MPa, and reaction time of 3-4 hours.

[0014] As a preferred technical solution of the present invention, in step 1), the mass concentration of the sulfuric acid solution is 20-30%; the heating and stirring conditions are 10-1000r / min, 85-95°C, and stirring for 2-3h; the dosage ratio of the montmorillonite to the sulfuric acid solution is 2-2.5g:100-120mL; during the acidification process, H + Replacement of Na between montmorillonite layers + , K + , Ca 2+ Mg 2+ Plasma improves its pores and pore structure.

[0015] As a preferred technical solution of the present invention, in step 1), the ultrasonic treatment conditions are 35-45KHz frequency, 250-280W power, and 8-10min of ultrasound; the sulfuric acid solution is added at a flow rate of 5-8mL / min while grinding the montmorillonite.

[0016] As a preferred technical solution of the present invention, in step 2), the drying and dehydration conditions are at a temperature of 60-65° C. and drying for 3.0-3.5 hours.

[0017] As a preferred technical solution of the present invention, in step 2), the calcination conditions are: a primary calcination at 160-170°C for 20-70 min and a secondary calcination at 550-600°C for 4-6 h.

[0018] As a preferred technical solution of the present invention, in step 2), the mass ratio of the preform to the stabilizer is 10-12:2-3; the stabilizer is one or both of calcium oxide and lanthanum oxide; the addition of calcium oxide / lanthanum oxide can increase the stability of the catalyst and increase its service life at the same time.

[0019] The invention discloses tert-dodecyl mercaptan prepared by the preparation method.

[0020] Beneficial effects of the present invention:

[0021] (1) The present invention slowly adds sulfuric acid solution to montmorillonite, causing the montmorillonite to dissolve and then crystallize. Grinding prevents the crystals from growing, which can effectively reduce the grain size of the montmorillonite. At the same time, grinding while adding sulfuric acid ensures that sulfuric acid is evenly distributed around the montmorillonite, which is beneficial to the reaction between sulfuric acid and montmorillonite.

[0022] (2) The raw materials before calcination contain a lot of free water. At this time, the raw materials are easy to agglomerate and have poor dispersibility. The preform after dehydration is calcined more fully, which is conducive to the formation of the mixed catalyst, and its crystal state is better. The loose structure of montmorillonite is conducive to the release of hydrogen ions of sulfuric acid, which effectively improves the catalytic ability of the mixed catalyst and promotes the reaction.

[0023] (3) The present invention uses sulfuric acid to activate montmorillonite, thereby improving the pores and pore structure of montmorillonite. Compared with natural montmorillonite, the lamellar stacking structure of the acidified montmorillonite becomes loose, and the pores are enlarged, which is conducive to the contact between the reaction substrate and the acidified montmorillonite, and its catalytic performance is significantly improved.

[0024] (4) The present invention can effectively remove impurities between montmorillonite layers by using ultrasonic treatment, increase the specific surface area and interlayer distance of montmorillonite, effectively promote sulfuric acid to penetrate the interlayers of montmorillonite and increase the contact area between sulfuric acid and montmorillonite, so as to maximize the acidification effect of montmorillonite.

[0025] (5) Before the secondary calcination, the first calcination is beneficial to the formation of micropores and the increase of the specific surface area of ​​montmorillonite. The increase of pores is conducive to the contact between the reaction substrate and the acidified montmorillonite, which effectively improves the catalytic performance of the mixed catalyst. DETAILED DESCRIPTION

[0026] In order to further illustrate the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation methods, structures, features and effects of the present invention are described in detail below in combination with the embodiments.

[0027] Example 1

[0028] A method for preparing tert-dodecyl mercaptan comprises the following steps: adding tetrapropylene, hydrogen sulfide and a mixed catalyst into a reaction kettle, mixing and reacting to obtain tert-dodecyl mercaptan; wherein the reaction conditions are 100°C, 1.5 MPa, and a reaction time of 3 hours; the molar ratio of tetrapropylene to hydrogen sulfide is 3:1; and the amount of the mixed catalyst is 3% of the total mass of tetrapropylene and hydrogen sulfide;

[0029] The preparation method of the mixed catalyst comprises the following steps:

[0030] 1) grinding montmorillonite and adding sulfuric acid solution, heating and stirring after ultrasonic treatment, centrifuging, removing the liquid part, and taking the solid as a preform; the mass concentration of the sulfuric acid solution is 20%; the heating and stirring conditions are 400r / min, 85°C, and stirring for 2h; the amount ratio of montmorillonite to sulfuric acid solution is 2g:100mL; the ultrasonic treatment conditions are at a frequency of 35KHz, a power of 250W, and ultrasonication for 8min; the sulfuric acid solution is added at a flow rate of 5mL / min while grinding the montmorillonite;

[0031] 2) The preform and the stabilizer are mixed, dried and dehydrated, and then calcined to obtain a mixed catalyst; wherein the drying and dehydration conditions are at 60°C and drying for 3.0 hours; the calcination conditions are calcination at 160°C for 40 minutes and calcination at 550°C for 4 hours; the mass ratio of the preform and the stabilizer is 10:2; and the stabilizer is calcium oxide.

[0032] Example 2

[0033] A method for preparing tert-dodecyl mercaptan comprises the following steps: adding tetrapropylene, hydrogen sulfide and a mixed catalyst into a reaction kettle and mixing them to react to obtain tert-dodecyl mercaptan; wherein the reaction conditions are 106°C, 1.6 MPa, and 3.2 hours of reaction; the molar ratio of tetrapropylene to hydrogen sulfide is 3.6:1; the amount of the mixed catalyst is 3.4% of the total mass of tetrapropylene and hydrogen sulfide;

[0034] The preparation method of the mixed catalyst comprises the following steps:

[0035] 1) Grinding montmorillonite and adding sulfuric acid solution, heating and stirring after ultrasonic treatment, centrifuging, removing the liquid part, and taking the solid as a preform; the mass concentration of the sulfuric acid solution is 22%; the heating and stirring conditions are 400r / min, 87°C, and stirring for 2.2h; the amount ratio of montmorillonite to sulfuric acid solution is 2.1g:104mL; the ultrasonic treatment conditions are at a frequency of 37KHz, a power of 256W, and ultrasonication for 8.4min; the sulfuric acid solution is added at a flow rate of 5.6mL / min while grinding the montmorillonite;

[0036] 2) The preform and the stabilizer are mixed, dried and dehydrated, and then calcined to obtain a mixed catalyst; wherein the drying and dehydration conditions are at a temperature of 61° C. and drying for 3.1 hours; the calcination conditions are a primary calcination at 162° C. for 40 minutes and a secondary calcination at a temperature of 560° C. for 4.4 hours; the mass ratio of the preform and the stabilizer is 10.4:2.2; and the stabilizer is calcium oxide.

[0037] Example 3

[0038] A method for preparing tert-dodecyl mercaptan comprises the following steps: adding tetrapropylene, hydrogen sulfide and a mixed catalyst into a reaction kettle and mixing them to react to obtain tert-dodecyl mercaptan; wherein the reaction conditions are 112° C., 1.7 MPa, and 3.4 hours of reaction; the molar ratio of tetrapropylene to hydrogen sulfide is 4.2:1; and the amount of the mixed catalyst is 3.8% of the total mass of tetrapropylene and hydrogen sulfide;

[0039] The preparation method of the mixed catalyst comprises the following steps:

[0040] 1) Grinding montmorillonite and adding sulfuric acid solution, heating and stirring after ultrasonic treatment, centrifuging, removing the liquid part, and taking the solid as a preform; the mass concentration of the sulfuric acid solution is 24%; the heating and stirring conditions are 400r / min, 89°C, and stirring for 2.4h; the amount ratio of montmorillonite to sulfuric acid solution is 2.2g:108mL; the ultrasonic treatment conditions are at a frequency of 39KHz, a power of 262W, and ultrasonication for 8.8min; the sulfuric acid solution is added at a flow rate of 6.2mL / min while grinding the montmorillonite;

[0041] 2) The preform and the stabilizer are mixed, dried and dehydrated, and then calcined to obtain a mixed catalyst; wherein the drying and dehydration conditions are at 62°C and drying for 3.2 hours; the calcination conditions are calcination at 164°C for 40 minutes and calcination at 570°C for 4.8 hours; the mass ratio of the preform and the stabilizer is 10.8:2.4; and the stabilizer is calcium oxide.

[0042] Example 4

[0043] A method for preparing tert-dodecyl mercaptan comprises the following steps: adding tetrapropylene, hydrogen sulfide and a mixed catalyst into a reaction kettle, mixing and reacting to obtain tert-dodecyl mercaptan; wherein the reaction conditions are 118° C., 1.8 MPa, and 3.6 hours of reaction; the molar ratio of tetrapropylene to hydrogen sulfide is 4.8:1; the amount of the mixed catalyst is 4.2% of the total mass of tetrapropylene and hydrogen sulfide;

[0044] The preparation method of the mixed catalyst comprises the following steps:

[0045] 1) Grinding montmorillonite and adding sulfuric acid solution, heating and stirring after ultrasonic treatment, centrifuging, removing the liquid part, and taking the solid as a preform; the mass concentration of the sulfuric acid solution is 26%; the heating and stirring conditions are 400r / min, 91°C, and stirring for 2.6h; the amount ratio of montmorillonite to sulfuric acid solution is 2.3g:112mL; the ultrasonic treatment conditions are at a frequency of 41KHz, a power of 268W, and ultrasonication for 9.2min; the sulfuric acid solution is added at a flow rate of 6.8mL / min while grinding the montmorillonite;

[0046] 2) The preform and the stabilizer are mixed, dried and dehydrated, and then calcined to obtain a mixed catalyst; wherein the drying and dehydration conditions are at 63°C and drying for 3.3 hours; the calcination conditions are calcination at 166°C for 40 minutes and calcination at 580°C for 5.2 hours; the mass ratio of the preform and the stabilizer is 11.2:2.6; and the stabilizer is calcium oxide.

[0047] Example 5

[0048] A method for preparing tert-dodecyl mercaptan comprises the following steps: adding tetrapropylene, hydrogen sulfide and a mixed catalyst into a reaction kettle and mixing them to react to obtain tert-dodecyl mercaptan; wherein the reaction conditions are 124°C, 1.9 MPa, and 3.8 hours of reaction; the molar ratio of tetrapropylene to hydrogen sulfide is 5.4:1; the amount of the mixed catalyst is 4.6% of the total mass of tetrapropylene and hydrogen sulfide;

[0049] The preparation method of the mixed catalyst comprises the following steps:

[0050] 1) Grinding montmorillonite and adding sulfuric acid solution, heating and stirring after ultrasonic treatment, centrifuging, removing the liquid part, and taking the solid as a preform; the mass concentration of the sulfuric acid solution is 28%; the heating and stirring conditions are 400r / min, 93°C, and stirring for 2.8h; the amount ratio of montmorillonite to sulfuric acid solution is 2.4g:116mL; the ultrasonic treatment conditions are at a frequency of 43KHz, a power of 274W, and ultrasonication for 9.6min; the sulfuric acid solution is added at a flow rate of 7.4mL / min while grinding the montmorillonite;

[0051] 2) The preform and the stabilizer are mixed, dried and dehydrated, and then calcined to obtain a mixed catalyst; wherein the drying and dehydration conditions are at 64°C and drying for 3.4 hours; the calcination conditions are a primary calcination at 168°C for 40 minutes and a secondary calcination at 590°C for 5.6 hours; the mass ratio of the preform and the stabilizer is 11.6:2.8; and the stabilizer is calcium oxide.

[0052] Example 6

[0053] A method for preparing tert-dodecyl mercaptan comprises the following steps: adding tetrapropylene, hydrogen sulfide and a mixed catalyst into a reaction kettle, mixing and reacting to obtain tert-dodecyl mercaptan; wherein the reaction conditions are 130° C., 2.0 MPa, and 4 hours of reaction; the molar ratio of tetrapropylene to hydrogen sulfide is 6:1; the amount of the mixed catalyst is 5% of the total mass of tetrapropylene and hydrogen sulfide;

[0054] The preparation method of the mixed catalyst comprises the following steps:

[0055] 1) Grinding montmorillonite and adding sulfuric acid solution, heating and stirring after ultrasonic treatment, centrifuging, removing the liquid part, and taking the solid as a preform; the mass concentration of the sulfuric acid solution is 30%; the heating and stirring conditions are 400r / min, 95°C, and stirring for 3h; the amount ratio of montmorillonite to sulfuric acid solution is 2.5g:120mL; the ultrasonic treatment conditions are at a frequency of 45KHz, a power of 280W, and ultrasonication for 10min; the sulfuric acid solution is added at a flow rate of 8mL / min while grinding the montmorillonite;

[0056] 2) The preform and the stabilizer are mixed, dried and dehydrated, and then calcined to obtain a mixed catalyst; wherein the drying and dehydration conditions are at 65°C and drying for 3.5 hours; the calcination conditions are a primary calcination at 170°C for 40 minutes and a secondary calcination at 600°C for 6 hours; the mass ratio of the preform and the stabilizer is 12:3; and the stabilizer is calcium oxide.

[0057] Comparative Example 1

[0058] Compared with Example 5, the difference in Comparative Example 1 is step 1);

[0059] Step 1) adding sulfuric acid solution to montmorillonite, heating and stirring after ultrasonic treatment, centrifuging, removing the liquid part, and taking the solid as a preform; the mass concentration of the sulfuric acid solution is 26%; the heating and stirring conditions are 400r / min, 91°C, and stirring for 2.6h; the amount ratio of the montmorillonite to the sulfuric acid solution is 2.3g:112mL; the ultrasonic treatment conditions are at a frequency of 41KHz, a power of 268W, and ultrasonication for 9.2min; the sulfuric acid solution is added at a flow rate of 6.8mL / min;

[0060] The remaining components, preparation steps and parameters were the same.

[0061] Comparative Example 2

[0062] Compared with Example 5, the difference is that comparative example 2 is not subjected to ultrasonic treatment, and the other components, preparation steps and parameters are the same.

[0063] Comparative Example 3

[0064] Compared with Example 5, the difference is that comparative example 3 is not dried and dehydrated, and the other components, preparation steps and parameters are the same.

[0065] Comparative Example 4

[0066] Compared with Example 5, the difference is that the calcination condition of step 2) of Comparative Example 4 is to perform secondary calcination at a temperature of 580°C for 4 hours; the other components, preparation steps and parameters are the same. The conversion rate of olefins is calculated for Examples 1-6 and Comparative Examples 1-4, and the results are shown in Table 1. Wherein, the conversion rate of olefins = olefin reaction amount / olefin initial amount*100%.

[0067] Table 1

[0068] Olefin conversion rate (%) Example 1 92.6 Example 2 92.8 Example 3 92.9 Example 4 92.8 Example 5 93.2 Example 6 92.7 Comparative Example 1 83.5 Comparative Example 2 79.6 Comparative Example 3 82.1 Comparative Example 4 83.2

[0069] From the test results in Table 1, it can be seen that when Examples 1-6 are compared with Comparative Examples 1-4, the effect of the catalyst prepared by the present invention is significantly better than that of Comparative Examples 1-4.

[0070] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.

Claims

1. A method for preparing tert-dodecyl mercaptan, characterized in that: The method comprises the following steps: adding tetrapropylene, hydrogen sulfide and a mixed catalyst into a reaction kettle, mixing and reacting to obtain tert-dodecyl mercaptan; the preparation method of the mixed catalyst comprises the following steps: 1) grinding montmorillonite and adding sulfuric acid solution, heating and stirring after ultrasonic treatment, centrifuging, removing the liquid part, and taking the solid as a preform; the mass concentration of the sulfuric acid solution is 20-30%; the heating and stirring conditions are 10-1000r / min, 85-95°C, and stirring for 2-3h; the amount ratio of montmorillonite to sulfuric acid solution is 2-2.5g:100-120mL; the ultrasonic treatment conditions are at a frequency of 35-45KHz, a power of 250-280W, and ultrasonication for 8-10min; the sulfuric acid solution is added at a flow rate of 5-8mL / min while grinding the montmorillonite; 2) The preform and the stabilizer are mixed, dried and dehydrated, and then calcined to obtain a mixed catalyst; the mass ratio of the preform and the stabilizer is 10-12:2-3; the stabilizer is calcium oxide; the drying and dehydration conditions are at a temperature of 60-65°C and drying for 3.0-3.5 hours; the calcination conditions are a primary calcination at 160-170°C for 20-70 minutes and a secondary calcination at a temperature of 550-600°C for 4-6 hours.

2. A method for preparing tert-dodecyl mercaptan according to claim 1, characterized in that: The molar ratio of tetrapropylene to hydrogen sulfide is 3-6:

1.

3. A method for preparing tert-dodecyl mercaptan according to claim 1, characterized in that: The amount of the mixed catalyst used is 3-5% of the total mass of tetrapropylene and hydrogen sulfide.

4. A method for preparing tert-dodecyl mercaptan according to claim 1, characterized in that: The reaction conditions are 100-130° C., 1.5-2.0 MPa, and 3-4 hours.

Citation Information

Cited By

  • Preparation method and application of methyl cyclopentadiene dimer mercaptan

    CN120865041A