Pole piece manufacturing method and pole piece manufacturing device
By using the roller clamp mechanism and gravure roller technology in the pole piece manufacturing process, the precise coating of insulating slurry and active material slurry is achieved, which solves the problems of high pole piece manufacturing cost and difficulty in inserting the electrode assembly into the shell, and improves the battery Monolithic reliability.
Patent Information
- Application Number
- CN202410488945.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-23
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-04-23
AI Technical Summary
In the existing pole piece manufacturing process, it is difficult to accurately control the coating thickness of the insulating slurry and active material slurry, which results in high pole piece manufacturing costs and difficulty in inserting the electrode assembly into the shell, and prone to the problem of pole tab redundancy.
A roller clamp mechanism is used to transport the current collector, and the insulating slurry and active material slurry are coated on it successively, or multiple insulating slurries are coated at the same time, and the active material slurry is set between them, and ultra-thin coating is achieved through a gravure roller. cloth to ensure consistent coating thickness.
The coating quality of the insulating slurry and active material slurry is improved, the manufacturing cost of the pole piece is reduced, the process of inserting the electrode assembly into the shell is simplified, and the reliability of the battery cell is enhanced.
Smart Images

Figure CN118099350B_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of batteries, and more specifically, to a method and device for manufacturing a pole piece. Background Art
[0002] Batteries are widely used in the field of new energy, such as electric vehicles and new energy vehicles. New energy vehicles and electric vehicles have become a new trend in the development of the automotive industry. Batteries include electrode assemblies, which are the components in the battery where electrochemical reactions occur. Electrode assemblies are mainly composed of positive and negative electrode sheets wound or stacked.
[0003] When manufacturing pole pieces, it is necessary to coat the current collector with insulating slurry and active material slurry. After drying, the insulating slurry forms an insulating layer, which is used to reduce the risk of contact between the positive pole piece and the negative pole piece when folding the pole ear. In the current coating process, the active material slurry and the insulating layer slurry are squeezed out and coated together through the coating head at the head position of the coating machine. The distance between the coating head and the current collector will give priority to ensuring the coating thickness of the active material slurry, resulting in a larger gap between the insulating slurry extrusion port and the current collector, and a thicker coating thickness of the insulating slurry, which increases the consumption of the insulating slurry and leads to a higher manufacturing cost of the pole piece. Summary of the invention
[0004] The purpose of the embodiments of the present application is to provide a pole piece manufacturing method and a pole piece manufacturing device, which are intended to improve the problem of high manufacturing cost of pole pieces in related technologies.
[0005] In a first aspect, an embodiment of the present application provides a method for manufacturing a pole piece, the method comprising: step S100: providing a current collector; step S200: applying a first slurry on the current collector; step S250: conveying the current collector through a roller clamping mechanism, the roller clamping mechanism comprising a first roller body and a second roller body, the first roller body comprising a first roller segment and a second roller segment, the second roller segment and the first roller segment are arranged along the axial direction of the first roller body, the diameter of the second roller segment is larger than the diameter of the first roller segment, the second roller segment and the second roller body are used to contact a portion of the current collector that is not coated with the first slurry to cooperate in conveying the current collector, and a gap is set between the first roller segment and the first slurry; step S300: applying a second slurry on the current collector so that the second slurry and the first slurry are arranged in the width direction of the current collector; wherein, before step S200, one of the first slurry and the second slurry is an active material slurry, and the other of the first slurry and the second slurry is an insulating slurry.
[0006] In the above technical scheme, when the pole piece manufacturing method is used to manufacture the pole piece, the insulating slurry can be first coated on the current collector, and then the active material slurry can be coated on the current collector, or the active material slurry can be first coated on the current collector, and then the insulating slurry can be coated on the current collector. In this way, the insulating slurry and the active material slurry are coated separately, and the coating of the insulating slurry and the coating of the active material slurry do not affect each other, which can improve the coating quality of the insulating slurry and the active material slurry, facilitate accurate control of the coating thickness of the insulating slurry and the active material slurry, and help reduce the manufacturing cost of the pole piece. In addition, the electrode assembly manufactured using the pole piece can be more conveniently put into the shell, and the risk of redundant pole ears is reduced, which is conducive to improving the reliability of the battery cell. The second roller segment and the second roller body can both contact the part of the current collector that is not coated with the first slurry, so as to cooperate in conveying the current collector. The first roller body and the second roller body will not contact the first slurry coated on the current collector, and it is not easy to damage the first slurry coated on the current collector, which is conducive to improving the coating quality of the first slurry and facilitating the control of the coating thickness of the first slurry. In addition, conveying the current collector by means of a roller clamp mechanism can reduce the risk of the current collector shaking, making it easier to coat the second slurry on the current collector, thereby helping to improve the coating quality of the second slurry.
[0007] As an optional technical solution of an embodiment of the present application, the first slurry is the insulating slurry, and the second slurry is the active material slurry; the step S300 includes: step S310: coating the active material slurry on the current collector, and making the active material slurry cover a portion of the insulating slurry.
[0008] In the above technical solution, when manufacturing the pole piece, the insulating slurry is first coated on the current collector, and then the active material slurry is coated on the current collector. In this way, when coating the active material slurry, the active material slurry can cover a part of the insulating slurry, reducing the risk of the current collector being exposed.
[0009] As an optional technical solution of an embodiment of the present application, the step S200 includes: step S210: applying a plurality of the first slurries on the current collector so that the plurality of the first slurries are arranged along the width direction of the current collector; the step S300 includes: step S320: applying the second slurry between two adjacent first slurries.
[0010] In the above technical solution, by coating multiple first slurries on the current collector and coating the second slurry between two adjacent first slurries, and then through die-cutting, multiple pole pieces can be produced at one time, which is beneficial to improving the production efficiency of the pole pieces and reducing the production cost of the pole pieces.
[0011] As an optional technical solution of an embodiment of the present application, the step S210 includes: step S211: simultaneously coating a plurality of the first slurries on the current collector.
[0012] In the above technical solution, since multiple first slurries are arranged at intervals along the width direction of the current collector, by simultaneously coating multiple first slurries on the current collector, it is not only beneficial to improve production efficiency and reduce production costs, but also there is no order relationship in the coating of the multiple first slurries, and it is not easy to affect each other during coating, which is beneficial to improve the coating quality of the first slurry.
[0013] As an optional technical solution of an embodiment of the present application, the step S200 includes: step S220: coating the insulating slurry on the current collector by a gravure roller.
[0014] In the above technical solution, the insulating slurry is coated on the current collector by a gravure roller, which facilitates ultra-thin coating and enables the thickness of the insulating slurry to be more consistent.
[0015] As an optional technical solution of an embodiment of the present application, after the step S300, the pole piece manufacturing method further includes: step S400: drying the first slurry and the second slurry.
[0016] In the above technical solution, the first slurry and the second slurry are dried to form an insulating layer and an active material layer on the current collector.
[0017] In a second aspect, an embodiment of the present application further provides a pole piece manufacturing device, the pole piece manufacturing device comprising an unwinding mechanism, a first coating mechanism, a roller clamping mechanism and a second coating mechanism, the unwinding mechanism being used to unwind the current collector; the first coating mechanism being arranged downstream of the unwinding mechanism, the first coating mechanism being used to coat a first slurry on the current collector; the roller clamping mechanism being arranged downstream of the first coating mechanism, the roller clamping mechanism comprising a first roller body and a second roller body, the first roller body comprising a first roller segment and a second roller segment, the second roller segment and the first roller segment being arranged along the axial direction of the first roller body, the second The diameter of the roller segment is larger than the diameter of the first roller segment. The second roller segment and the second roller body are used to contact the part of the current collector that is not coated with the first slurry to cooperate with the conveying of the current collector. The first roller segment and the first slurry are arranged in a gap. The second coating mechanism is arranged downstream of the roller clamp mechanism. The second coating mechanism is used to coat the second slurry on the current collector. The second slurry and the first slurry are arranged in the width direction of the current collector. One of the first slurry and the second slurry is an active material slurry, and one of the first slurry and the second slurry is an insulating slurry. Both the second roller segment and the second roller body can contact the part of the current collector that is not coated with the first slurry, so as to cooperate with the conveying of the current collector. Neither the first roller body nor the second roller body will contact the first slurry coated on the current collector, and it is not easy to damage the first slurry coated on the current collector, which is conducive to improving the coating quality of the first slurry and facilitating the control of the coating thickness of the first slurry. In addition, conveying the current collector through the roller clamp mechanism can reduce the risk of the current collector shaking, facilitate the coating of the second slurry on the current collector, and facilitate the coating of the second slurry, which is conducive to improving the coating quality of the second slurry.
[0018] In the above technical solution, when the pole piece manufacturing device is used to manufacture the pole piece, the insulating slurry can be first coated on the current collector, and then the active material slurry can be coated on the current collector, or the active material slurry can be first coated on the current collector, and then the insulating slurry can be coated on the current collector. In this way, the insulating slurry and the active material slurry are coated separately, and the coating of the insulating slurry and the coating of the active material slurry do not affect each other, which can improve the coating quality of the insulating slurry and the active material slurry, facilitate accurate control of the coating thickness of the insulating slurry and the active material slurry, and help reduce the manufacturing cost of the pole piece. In addition, the electrode assembly manufactured using the pole piece can be more conveniently put into the shell, and the risk of redundant pole ears is reduced, which is conducive to improving the reliability of the battery cell.
[0019] As an optional technical solution of an embodiment of the present application, the plane where the axis of the first roller body and the axis of the second roller body are located is parallel to a vertical plane.
[0020] In the above technical solution, by making the plane where the axis of the first roller body and the axis of the second roller body are located parallel to the vertical plane, the risk of the current collector being wrinkled after passing through the roller clamping mechanism can be reduced.
[0021] As an optional technical solution of the embodiment of the present application, the roller clamping mechanism further includes a first driving member, the first driving member is connected to the second roller body, and the first driving member is used to drive the second roller body to rotate.
[0022] In the above technical solution, the first driving member is arranged to drive the second roller to actively rotate, so that the second roller cooperates with the first roller to transport the collector, so that the roller clamping mechanism forms a tension barrier between the first coating mechanism and the second coating mechanism, thereby balancing the tension of the collector during transportation.
[0023] As an optional technical solution of an embodiment of the present application, the second coating mechanism includes a coating head, and there is a first gap between the coating head and the second roller body, the first gap is used for the current collector to pass through, and the coating head is used to coat the second slurry on the current collector.
[0024] In the above technical solution, there is a first gap between the coating head and the second roller body, and the first gap is used for the pole piece to pass through. When the pole piece passes through the first gap, the coating head can coat the second slurry on the current collector. The pole piece manufacturing device uses the second roller body to support the current collector, so that it is convenient for the coating head to coat the active material slurry on the current collector. The second roller body can cooperate with the first roller body to transport the current collector and support the current collector. One component plays multiple roles, which is conducive to simplifying the structure of the pole piece manufacturing device and reducing the cost of the pole piece manufacturing device.
[0025] As an optional technical solution of an embodiment of the present application, the first coating mechanism includes a reservoir and a gravure roller, the reservoir is used to store the first slurry; the gravure roller is rotatably connected to the reservoir, and the gravure roller is used to coat the first slurry in the reservoir onto the current collector.
[0026] In the above technical solution, the gravure roller is rotatably arranged in the material storage container, a part of the gravure roller is located outside the material storage container, and another part of the gravure roller is located inside the material storage container. During the rotation of the gravure roller, the first slurry in the material storage container can be dipped and the first slurry can be coated on the current collector. Coating the insulating slurry on the current collector through the gravure roller facilitates ultra-thin coating and can make the thickness consistency of the insulating slurry higher.
[0027] As an optional technical solution of the embodiment of the present application, the first coating mechanism further includes a second driving member, the second driving member is connected to the gravure roller, and the second driving member is used to drive the gravure roller to rotate.
[0028] In the above technical solution, by providing a second driving member to drive the gravure roller to actively rotate, the linear velocity of any point on the outer circumference of the gravure roller can be greater than the conveying velocity of the current collector, thereby facilitating improving the coating effect of the first slurry.
[0029] As an optional technical solution of the embodiment of the present application, the diameter of the gravure roller is D, which satisfies: 100mm≤D≤300mm.
[0030] In the above technical solution, by making D≤300mm, the diameter of the gravure roller is small, which is conducive to controlling the consistency of the coating thickness of the first slurry, and the first slurry can be coated thinner. By making D≥100mm, the diameter of the gravure roller is not too small, so that the gravure roller has sufficient strength and reduces the risk of gravure roller breakage. Therefore, when 100mm≤D≤300mm, the strength of the gravure roller and the coating effect can be taken into account.
[0031] As an optional technical solution of the embodiment of the present application, 120mm≤D≤160mm.
[0032] In the above technical solution, by making D≤160mm, the diameter of the gravure roller is smaller, which is more conducive to controlling the consistency of the coating thickness of the first slurry, and the first slurry can be coated thinner. By making D≥120mm, the diameter of the gravure roller is not too small, so that the gravure roller has sufficient strength and reduces the risk of gravure roller breakage. Therefore, when 120mm≤D≤160mm, the strength of the gravure roller and the coating effect can be taken into account.
[0033] As an optional technical solution of an embodiment of the present application, the first slurry is the insulating slurry, and the second slurry is the active material slurry; the first coating mechanism includes a plurality of the gravure rollers, and the plurality of the gravure rollers are arranged at intervals along the width direction of the current collector, and the gravure rollers are used to coat the insulating slurry on the current collector.
[0034] In the above technical solution, by arranging multiple gravure rollers and arranging the multiple gravure rollers at intervals along the width direction of the current collector, multiple insulating slurry strips can be coated on the current collector at the same time, thereby improving the production efficiency of the pole piece and reducing the production cost of the pole piece.
[0035] As an optional technical solution of an embodiment of the present application, the first slurry is the insulating slurry, and the second slurry is the active material slurry; the pole piece manufacturing device includes a plurality of the first coating mechanisms, and the plurality of the first coating mechanisms are arranged along the width direction of the current collector, and each of the first coating mechanisms includes a gravure roller, and the gravure roller is used to apply the insulating slurry to the current collector.
[0036] In the above technical solution, by providing multiple first coating mechanisms and arranging the multiple first coating mechanisms along the width direction of the current collector, multiple insulating slurry strips can be coated on the current collector at the same time, thereby improving the production efficiency of the pole piece and reducing the production cost of the pole piece.
[0037] As an optional technical solution of an embodiment of the present application, the first coating mechanism includes a pressure roller, and the pressure roller is used to press the current collector onto the gravure roller.
[0038] In the above technical solution, a pressure roller is provided to press the current collector onto the gravure roller, so that the gravure roller can stably apply the first slurry to the current collector, which is beneficial to improving the consistency of the first slurry coating.
[0039] As an optional technical solution of the embodiment of the present application, the pressure rollers are arranged both upstream and downstream of the gravure roller.
[0040] In the above technical solution, pressure rollers are arranged upstream and downstream of the gravure roller to improve the effect of pressing the current collector to the gravure roller, so that the gravure roller can more stably apply the first slurry to the current collector, which is beneficial to improving the consistency of the first slurry coating.
[0041] As an optional technical solution of an embodiment of the present application, the first coating mechanism includes an adjustment structure, the adjustment structure is connected to the pressure roller, and the adjustment structure is used to adjust the position of the pressure roller along the thickness direction of the current collector.
[0042] In the above technical solution, by setting an adjustment structure to adjust the position of the pressure roller along the thickness direction of the current collector, the contact length between the gravure roller and the current collector can be adjusted, that is, the feed amount of the current collector in contact with the gravure roller can be adjusted. By adjusting the feed amount of the current collector in contact with the gravure roller, the risk of missing coating can be reduced.
[0043] As an optional technical solution of the embodiment of the present application, the first coating mechanism further includes a scraper, and the scraper is used to scrape off excess first slurry on the gravure roller.
[0044] In the above technical solution, a scraper is provided to scrape off the excess first slurry on the gravure roller, which is beneficial to controlling the coating thickness and coating consistency of the first slurry.
[0045] As an optional technical solution of an embodiment of the present application, the position of the first coating mechanism along the width direction of the current collector is adjustable.
[0046] In the above technical solution, by making the position of the first coating mechanism adjustable along the width direction of the current collector, the position of the first coating mechanism in the width direction of the current collector can be adjusted as needed to meet the manufacturing requirements of different pole pieces, which is beneficial to improving the adaptability of the pole piece manufacturing device to manufacturing pole pieces of different models.
[0047] As an optional technical solution of an embodiment of the present application, the pole piece manufacturing device includes a guide member, which extends along the width direction of the current collector, and the first coating mechanism is guided and cooperated with the guide member.
[0048] In the above technical solution, a guide is provided to guide the first coating mechanism to move along the width direction of the current collector, thereby reducing the risk of the first coating mechanism running off the track when adjusting the position of the first coating mechanism.
[0049] As an optional technical solution of an embodiment of the present application, the pole piece manufacturing device also includes a drying mechanism, which is arranged downstream of the second coating mechanism, and the drying mechanism is used to dry the first slurry and the second slurry.
[0050] In the above technical solution, a drying mechanism is provided to dry the first slurry and the second slurry to form an insulating layer and an active material layer on the current collector. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.
[0052] Figure 1 A schematic block diagram of a pole piece manufacturing method provided in some embodiments of the present application;
[0053] Figure 2 A schematic block diagram of a pole piece manufacturing method provided in some other embodiments of the present application;
[0054] Figure 3 A schematic block diagram of a pole piece manufacturing method provided in some other embodiments of the present application;
[0055] Figure 4 A schematic block diagram of a pole piece manufacturing method provided in some further embodiments of the present application;
[0056] Figure 5 A schematic block diagram of a pole piece manufacturing method provided in some embodiments of the present application;
[0057] Figure 6A schematic block diagram of a pole piece manufacturing method provided in some other embodiments of the present application;
[0058] Figure 7 A schematic block diagram of a pole piece manufacturing method provided in some other embodiments of the present application;
[0059] Figure 8 A schematic block diagram of a pole piece manufacturing device provided in some embodiments of the present application;
[0060] Fig. 9 A schematic diagram of the structure of a pole piece manufacturing device provided in some embodiments of the present application;
[0061] Fig.10 A schematic diagram of the structure of a roller clamp mechanism provided in some embodiments of the present application;
[0062] Fig.11 A schematic block diagram of the connection between a second roller and a first driving member provided in some embodiments of the present application;
[0063] Fig.12 A schematic diagram of the structure of a first coating mechanism provided in some embodiments of the present application;
[0064] Fig.13 A schematic structural diagram of a first coating mechanism provided in some other embodiments of the present application;
[0065] Fig.14 A schematic diagram of the structure of a pole piece manufacturing device provided in some other embodiments of the present application;
[0066] Fig.15 A schematic diagram of the structure of the connection between the pressure roller and the adjustment structure provided in some embodiments of the present application;
[0067] Fig.16 A schematic structural diagram of a first coating mechanism provided in some other embodiments of the present application;
[0068] Fig.17 A schematic structural diagram of a pole piece manufacturing device provided in some other embodiments of the present application.
[0069] Icons: 10-pole piece manufacturing method; 20-pole piece manufacturing device; 210-unwinding mechanism; 220-first coating mechanism; 221-gravure roller; 222-accumulator; 223-second driving member; 224-scraper; 2241-front scraper; 2242-side scraper; 225-guide; 230-second coating mechanism; 231-coating head; 240-roller clamping mechanism; 241-first roller body; 2411-first roller segment; 2412-second roller segment; 242-second roller body; 243-first driving member; 251-overroller; 252-winding mechanism; 261-pressing roller; 262-adjusting structure; 2621-adjusting handle; 2622-first mounting seat; 2623-screw; 263-second mounting seat; 270-drying mechanism; 31-current collector; 32-insulating slurry. DETAILED DESCRIPTION
[0070] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0071] Unless otherwise defined, all technical and scientific terms used in this application have the same meanings as those commonly understood by technicians in the technical field of this application; the terms used in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application; the terms "including" and "having" in the specification and claims of this application and the above-mentioned drawings and any variations thereof are intended to cover non-exclusive inclusions. The terms "first", "second", etc. in the specification and claims of this application or the above-mentioned drawings are used to distinguish different objects, rather than to describe a specific order or a primary and secondary relationship.
[0072] Reference to "embodiment" in this application means that a particular feature, structure, or characteristic described in conjunction with the embodiment may be included in at least one embodiment of the present application. The appearance of the phrase in various places in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments.
[0073] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", and "attached" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0074] The term "and / or" in this application is only a description of the association relationship of associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this application generally indicates that the associated objects before and after are in an "or" relationship.
[0075] In the embodiments of the present application, the same reference numerals represent the same components, and for the sake of brevity, detailed descriptions of the same components are omitted in different embodiments. It should be understood that the thickness, length, width and other dimensions of various components in the embodiments of the present application shown in the drawings, as well as the overall thickness, length, width and other dimensions of the integrated device are only exemplary descriptions and should not constitute any limitation to the present application.
[0076] The term “plurality” used in this application refers to two or more (including two).
[0077] In the present application, battery cells may include lithium-ion secondary batteries, lithium-ion primary batteries, lithium-sulfur batteries, sodium-lithium-ion batteries, sodium-ion batteries or magnesium-ion batteries, etc., and the embodiments of the present application do not limit this. Battery cells may be cylindrical, flat, rectangular or other shapes, etc., and the embodiments of the present application do not limit this. Battery cells are generally divided into three types according to the packaging method: cylindrical battery cells, square battery cells and soft-pack battery cells, and the embodiments of the present application do not limit this.
[0078] The battery mentioned in the embodiments of the present application refers to a single physical module including one or more battery cells to provide higher voltage and capacity. For example, the battery mentioned in the present application may include a battery module or a battery pack. The battery generally includes a box for encapsulating one or more battery cells. The box can prevent liquid or other foreign matter from affecting the charging or discharging of the battery cells to a certain extent.
[0079] The battery cell includes an electrode assembly and an electrolyte. The electrode assembly is composed of a positive electrode sheet, a negative electrode sheet and a separator. The battery cell mainly relies on the movement of metal ions between the positive electrode sheet and the negative electrode sheet to work. The positive electrode sheet includes a positive electrode collector and a positive electrode active material layer. The positive electrode active material layer is coated on the surface of the positive electrode collector. The positive electrode collector not coated with the positive electrode active material layer protrudes from the positive electrode collector coated with the positive electrode active material layer. The positive electrode collector not coated with the positive electrode active material layer serves as a positive electrode ear. Taking lithium-ion batteries as an example, the material of the positive electrode collector can be aluminum, and the positive electrode active material can be lithium cobalt oxide, lithium iron phosphate, ternary lithium or lithium manganese oxide. The negative electrode sheet includes a negative electrode collector and a negative electrode active material layer. The negative electrode active material layer is coated on the surface of the negative electrode collector. The negative electrode collector not coated with the negative electrode active material layer protrudes from the negative electrode collector coated with the negative electrode active material layer. The negative electrode collector not coated with the negative electrode active material layer serves as a negative electrode ear. The material of the negative electrode collector can be copper, and the negative electrode active material can be carbon or silicon. In order to ensure that a large current can pass without melting, the number of positive pole ears is multiple and stacked together, and the number of negative pole ears is multiple and stacked together. The material of the isolation film can be PP (polypropylene) or PE (polyethylene). In addition, the electrode assembly can be a winding structure or a laminated structure, and the embodiments of the present application are not limited to this.
[0080] At present, from the perspective of market development, the application of batteries is becoming more and more extensive. Batteries are not only used in energy storage power systems such as hydropower, thermal power, wind power and solar power stations, but also widely used in electric vehicles such as electric bicycles, electric motorcycles, electric cars, as well as military equipment and aerospace and other fields. With the continuous expansion of battery application areas, its market demand is also constantly expanding.
[0081] The battery includes an electrode assembly, which is the part of the battery where the electrochemical reaction occurs. The electrode assembly is mainly composed of a positive electrode sheet and a negative electrode sheet wound or stacked. At present, the manufacturing cost of the electrode sheet is relatively high.
[0082] When manufacturing pole pieces, it is necessary to coat the current collector with insulating slurry and active material slurry. After drying, the insulating slurry forms an insulating layer, which is used to reduce the risk of contact between the positive pole piece and the negative pole piece when folding the pole ear. In the current coating process, the active material slurry and the insulating layer slurry are squeezed out and coated together by a coating head at the head position of the coating machine. The distance between the coating head and the current collector will give priority to ensuring the coating thickness of the active material slurry, resulting in a larger gap between the insulating slurry extrusion port and the current collector, and a thicker coating thickness of the insulating slurry, which increases the consumption of the insulating slurry and leads to a higher manufacturing cost of the pole piece. In addition, due to the thick insulating slurry, the electrode assembly manufactured using this pole piece is more difficult to enter the shell. Even if it can be entered, it is easy to cause pole ear redundancy, resulting in a series of reliability problems.
[0083] In view of this, an embodiment of the present application provides a method for manufacturing a pole piece, the method comprising: step S100: providing a current collector; step S200: coating a first slurry on the current collector; step S300: coating a second slurry on the current collector, so that the second slurry and the first slurry are arranged in the width direction of the current collector. Before step S200 and step S300, one of the first slurry and the second slurry is an active material slurry, and the other of the first slurry and the second slurry is an insulating slurry.
[0084] When the pole piece manufacturing method is used to manufacture the pole piece, the insulating slurry can be first coated on the current collector, and then the active material slurry can be coated on the current collector, or the active material slurry can be first coated on the current collector, and then the insulating slurry can be coated on the current collector. In this way, the insulating slurry and the active material slurry are coated separately, and the coating of the insulating slurry and the coating of the active material slurry do not affect each other, which can improve the coating quality of the insulating slurry and the active material slurry, facilitate accurate control of the coating thickness of the insulating slurry and the active material slurry, and help reduce the manufacturing cost of the pole piece. In addition, the electrode assembly manufactured using the pole piece can be more conveniently put into the shell, and the risk of redundant pole ears is reduced, which is conducive to improving the reliability of the battery cell.
[0085] The technical solution described in the embodiment of the present application is applicable to the manufacture of pole pieces and can reduce the manufacturing cost of pole pieces.
[0086] Please refer to Figure 1 , Figure 1 A schematic block diagram of a pole piece manufacturing method 10 provided in some embodiments of the present application. The present application embodiment provides a pole piece manufacturing method 10, and the pole piece manufacturing method 10 includes:
[0087] Step S100: providing a current collector 31;
[0088] Step S200: coating the first slurry on the current collector 31;
[0089] Step S300: coating the second slurry on the current collector 31 so that the second slurry and the first slurry are arranged in the width direction of the current collector 31;
[0090] In which, before step S200 and step S300 , one of the first slurry and the second slurry is an active material slurry, and the other of the first slurry and the second slurry is an insulating slurry 32 .
[0091] One of the first slurry and the second slurry is an active material slurry, and the other of the first slurry and the second slurry is an insulating slurry 32. When the first slurry is an insulating slurry 32, the second slurry is an active material slurry. When the first slurry is an active material slurry, the second slurry is an insulating slurry 32. The first slurry and the second slurry coated on the current collector 31 are arranged along the width direction of the current collector 31.
[0092] Step S200 and step S300 have a sequential order. Specifically, step S200 is performed first, and then step S300 is performed. For example, when the first slurry is an insulating slurry 32 and the second slurry is an active material slurry, the insulating slurry 32 is first applied to the current collector 31, and after the insulating slurry 32 is applied, the active material slurry is applied to the current collector 31. For another example, when the first slurry is an active material slurry and the second slurry is an insulating slurry 32, the active material slurry is first applied to the current collector 31, and after the active material slurry is applied, the insulating slurry 32 is applied to the current collector 31.
[0093] When the pole piece manufacturing method 10 is used to manufacture the pole piece, the insulating slurry 32 can be first coated on the current collector 31, and then the active material slurry can be coated on the current collector 31, or the active material slurry can be first coated on the current collector 31, and then the insulating slurry 32 can be coated on the current collector 31. In this way, the insulating slurry 32 and the active material slurry are coated separately, and the coating of the insulating slurry 32 and the coating of the active material slurry do not affect each other, which can improve the coating quality of the insulating slurry 32 and the active material slurry, facilitate accurate control of the coating thickness of the insulating slurry 32 and the active material slurry, and help reduce the manufacturing cost of the pole piece. In addition, the electrode assembly manufactured using the pole piece can be more conveniently put into the shell, and the risk of redundant pole ears is reduced, which is conducive to improving the reliability of the battery cell.
[0094] Please refer to Figure 2 , Figure 2 This is a schematic block diagram of a pole piece manufacturing method 10 provided in some other embodiments of the present application. In some other embodiments, the first slurry is an insulating slurry 32, and the second slurry is an active material slurry.
[0095] Step S300 includes:
[0096] Step S310 : coating the active material slurry on the current collector 31 , and making the active material slurry cover a part of the insulating slurry 32 .
[0097] The first slurry is the insulating slurry 32, and the second slurry is the active material slurry. During manufacturing, the insulating slurry 32 is first applied to the current collector 31, and after the insulating slurry 32 is applied, the active material slurry is applied to the current collector 31. When applying the active material slurry, the active material slurry covers the insulating slurry 32 on one side of the current collector 31 close to the active material slurry along the width direction of the current collector 31.
[0098] When manufacturing the pole piece, the insulating paste 32 is first coated on the current collector 31, and then the active material paste is coated on the current collector 31. In this way, when the active material paste is coated, the active material paste can cover a part of the insulating paste 32, reducing the risk of the current collector 31 being exposed.
[0099] Please refer to Figure 3 , Figure 3 A schematic block diagram of a pole piece manufacturing method 10 provided in some other embodiments of the present application. In some other embodiments, before step S300 and after step S200, the pole piece manufacturing method 10 further includes:
[0100] Step S250: transporting the current collector 31 through the roller clamp mechanism 240;
[0101] The roller clamp mechanism 240 includes a first roller body 241 and a second roller body 242. The first roller body 241 includes a first roller segment 2411 and a second roller segment 2412. The second roller segment 2412 and the first roller segment 2411 are arranged along the axial direction of the first roller body 241. The diameter of the second roller segment 2412 is greater than the diameter of the first roller segment 2411. The second roller segment 2412 and the second roller body 242 are used to contact the portion of the current collector 31 that is not coated with the first slurry to cooperate in conveying the current collector 31. A gap is set between the first roller segment 2411 and the first slurry.
[0102] After coating the first slurry on the current collector 31 and before coating the second slurry on the current collector 31 , the pole piece manufacturing method 10 further includes: transporting the current collector 31 by a roller clamping mechanism 240 .
[0103] The roller clamp mechanism 240 includes a first roller body 241 and a second roller body 242, wherein the first roller body 241 includes a first roller segment 2411 and a second roller segment 2412 arranged along its axial direction, and the diameter of the first roller segment 2411 is smaller than the diameter of the second roller segment 2412. A second gap is provided between the second roller segment 2412 and the second roller body 242 for the portion of the current collector 31 not coated with the first slurry to pass through, and the second roller segment 2412 and the second roller body 242 are both used to contact the portion of the current collector 31 not coated with the first slurry, thereby transporting the current collector 31. A third gap is provided between the first roller segment 2411 and the second roller body 242 for the portion of the current collector 31 coated with the first slurry to pass through, and the width of the third gap is greater than the width of the second gap, so that there is a gap between the first roller segment 2411 and the first slurry, that is, the first roller segment 2411 does not contact the first slurry coated on the current collector 31.
[0104] It should be noted that the first roller body 241 may include a plurality of second roller segments 2412 , and along the axial direction of the first roller body 241 , the first roller segments 2411 and the second roller segments 2412 are alternately arranged.
[0105] The second roller segment 2412 and the second roller body 242 can both contact the portion of the current collector 31 that is not coated with the first slurry, thereby cooperating in conveying the current collector 31. The first roller body 241 and the second roller body 242 will not contact the first slurry coated on the current collector 31, and are not likely to damage the first slurry coated on the current collector 31, which is beneficial to improving the coating quality of the first slurry and facilitating the control of the coating thickness of the first slurry. In addition, conveying the current collector 31 through the roller clamp mechanism 240 can reduce the risk of the current collector 31 shaking, facilitate coating the second slurry on the current collector 31, and help improve the coating quality of the second slurry.
[0106] Please refer to Figure 4 , Figure 4 A schematic block diagram of a pole piece manufacturing method 10 provided in some further embodiments of the present application. In some further embodiments, step S200 includes:
[0107] Step S210: coating a plurality of first slurries on the current collector 31 so that the plurality of first slurries are arranged along the width direction of the current collector 31;
[0108] Step S300 includes:
[0109] Step S320: applying the second slurry between two adjacent first slurries.
[0110] When the first slurry is an insulating slurry 32 and the second slurry is an active material slurry, a plurality of insulating slurries 32 are coated on the current collector 31 so that the plurality of insulating slurries 32 are spaced apart along the width direction of the current collector 31. After drying, a plurality of insulating layers spaced apart along the width direction of the current collector 31 can be formed. The active material slurry is coated between two adjacent insulating slurries 32, and after drying, an active material layer can be formed between the two adjacent insulating layers.
[0111] By coating a plurality of first slurries on the current collector 31 and coating a second slurry between two adjacent first slurries, and then die-cutting, a plurality of pole pieces can be produced at one time, which is beneficial to improving the production efficiency of the pole pieces and reducing the production cost of the pole pieces.
[0112] Please refer to Figure 5 , Figure 5 A schematic block diagram of a pole piece manufacturing method 10 provided in some embodiments of the present application. In some other embodiments, step S210 includes:
[0113] Step S211 : coating a plurality of first slurries on the current collector 31 simultaneously.
[0114] Since the multiple first slurries are arranged at intervals along the width direction of the current collector 31, by simultaneously coating the multiple first slurries on the current collector 31, it is not only beneficial to improve production efficiency and reduce production costs, but also there is no order relationship in the coating of the multiple first slurries, and it is not easy to affect each other during coating, which is beneficial to improve the coating quality of the first slurry.
[0115] Please refer to Figure 6 , Figure 6 A schematic block diagram of a pole piece manufacturing method 10 provided in some other embodiments of the present application. In some other embodiments, step S200 includes:
[0116] Step S220 : coating the insulating slurry 32 on the current collector 31 by using the gravure roller 221 .
[0117] The gravure roller 221 is a roller body structure, and a continuous mesh pattern may be engraved on the outer circumference of the gravure roller 221 to enable the insulating slurry 32 to be evenly and densely coated on the current collector 31 .
[0118] The insulating slurry 32 is coated on the current collector 31 by the gravure roller 221 , which facilitates ultra-thin coating and enables the thickness of the insulating slurry 32 to be more consistent.
[0119] Please refer to Figure 7 , Figure 7 A schematic block diagram of a pole piece manufacturing method 10 provided in some other embodiments of the present application. In some other embodiments, after step S300, the pole piece manufacturing method 10 further includes:
[0120] Step S400: drying the first slurry and the second slurry.
[0121] By drying the first slurry and the second slurry, an insulating layer and an active material layer are formed on the current collector 31 .
[0122] Please refer to Figure 8 and Fig. 9 , Figure 8 A schematic block diagram of a pole piece manufacturing device 20 provided in some embodiments of the present application. Fig. 9A schematic diagram of the structure of a pole piece manufacturing device 20 provided for some embodiments of the present application. The embodiment of the present application also provides a pole piece manufacturing device 20, which includes an unwinding mechanism 210, a first coating mechanism 220 and a second coating mechanism 230, and the unwinding mechanism 210 is used to unwind the current collector 31. The first coating mechanism 220 is arranged downstream of the unwinding mechanism 210, and the first coating mechanism 220 is used to apply a first slurry on the current collector 31. The second coating mechanism 230 is arranged downstream of the first coating mechanism 220, and the second coating mechanism 230 is used to apply a second slurry on the current collector 31, and the second slurry and the first slurry are arranged in the width direction of the current collector 31. One of the first slurry and the second slurry is an active material slurry, and one of the first slurry and the second slurry is an insulating slurry 32.
[0123] The unwinding mechanism 210 is a mechanism for unwinding the current collector 31. The unwinding mechanism 210 may include an unwinding roller, which is used to set the current collector roll, and the current collector roll is unwound by rotating the unwinding roller.
[0124] Along the conveying direction of the current collector 31, the first coating mechanism 220 is located downstream of the unwinding mechanism 210 and upstream of the second coating mechanism 230, and the first coating mechanism 220 is used to coat the first slurry on the current collector 31. Along the conveying direction of the current collector 31, the second coating mechanism 230 is located downstream of the first coating mechanism 220, and the second coating mechanism 230 is used to coat the second slurry on the current collector 31, so that the second slurry and the first slurry are arranged along the width direction of the current collector 31. When the first slurry is the insulating slurry 32 and the second slurry is the active material slurry, the first coating mechanism 220 is used to coat the insulating slurry 32 on the current collector 31, and the second coating mechanism 230 is used to coat the active material slurry on the current collector 31. When the first slurry is active material slurry and the second slurry is insulating slurry 32 , the first coating mechanism 220 is used to coat the active material slurry on the current collector 31 , and the second coating mechanism 230 is used to coat the insulating slurry 32 on the current collector 31 .
[0125] When the pole piece manufacturing device 20 is used to manufacture the pole piece, the insulating slurry 32 can be first coated on the current collector 31, and then the active material slurry can be coated on the current collector 31, or the active material slurry can be first coated on the current collector 31, and then the insulating slurry 32 can be coated on the current collector 31. In this way, the insulating slurry 32 and the active material slurry are coated separately, and the coating of the insulating slurry 32 and the coating of the active material slurry do not affect each other, which can improve the coating quality of the insulating slurry 32 and the active material slurry, facilitate accurate control of the coating thickness of the insulating slurry 32 and the active material slurry, and help reduce the manufacturing cost of the pole piece. In addition, the electrode assembly manufactured using the pole piece can be more conveniently put into the shell, and the risk of redundant pole ears is reduced, which is conducive to improving the reliability of the battery cell.
[0126] In some embodiments, the pole piece manufacturing device 20 further includes a roller 251 and a winding mechanism 252. The roller 251 is used for winding the current collector 31 to support the current collector 31. The winding mechanism 252 is disposed downstream of the second coating mechanism 230 and is used to wind up the current collector 31.
[0127] Please refer to Figure 8 , Fig. 9 and Fig.10 , Fig.10 A schematic diagram of the structure of a roller clamping mechanism 240 provided for some embodiments of the present application. In some embodiments, the first slurry is an insulating slurry 32, and the second slurry is an active material slurry. The pole piece manufacturing device 20 includes a roller clamping mechanism 240, and the roller clamping mechanism 240 is arranged downstream of the first coating mechanism 220 and upstream of the second coating mechanism 230. The roller clamping mechanism 240 includes a first roller body 241 and a second roller body 242, and the first roller body 241 includes a first roller segment 2411 and a second roller segment 2412, and the second roller segment 2412 and the first roller segment 2411 are arranged along the axial direction of the first roller body 241. The diameter of the second roller segment 2412 is greater than the diameter of the first roller segment 2411, and the second roller segment 2412 and the second roller body 242 are used to contact the portion of the current collector 31 that is not coated with the insulating slurry 32, so as to cooperate in conveying the current collector 31. The first roller segment 2411 is set with a gap between the insulating slurry 32.
[0128] The first slurry may be an insulating slurry 32 , and the second slurry may be an active material slurry. The first coating mechanism 220 is used to coat the insulating slurry 32 on the current collector 31 , and the second coating mechanism 230 is used to coat the active material slurry on the current collector 31 .
[0129] Along the conveying direction of the current collector 31, the roller clamp mechanism 240 is located downstream of the first coating mechanism 220, and the roller clamp mechanism 240 is located upstream of the second coating mechanism 230. The current collector 31 passes through the first coating mechanism 220, the roller clamp mechanism 240 and the second coating mechanism 230 in sequence.
[0130] The roller clamp mechanism 240 includes a first roller body 241 and a second roller body 242, wherein the first roller body 241 includes a first roller segment 2411 and a second roller segment 2412 arranged along its axial direction, and the diameter of the first roller segment 2411 is smaller than the diameter of the second roller segment 2412. A second gap is provided between the second roller segment 2412 and the second roller body 242 for the portion of the current collector 31 not coated with the insulating slurry 32 to pass through, and the second roller segment 2412 and the second roller body 242 are both used to contact the portion of the current collector 31 not coated with the insulating slurry 32, thereby transporting the current collector 31. A third gap is provided between the first roller segment 2411 and the second roller body 242 for the portion of the current collector 31 coated with the insulating slurry 32 to pass through, and the width of the third gap is greater than the width of the second gap, so that there is a gap between the first roller segment 2411 and the insulating slurry 32, that is, the first roller segment 2411 does not contact the insulating slurry 32 coated on the current collector 31. It should be noted that the first roller body 241 may include a plurality of second roller segments 2412 , and along the axial direction of the first roller body 241 , the first roller segments 2411 and the second roller segments 2412 are alternately arranged.
[0131] The second roller segment 2412 and the second roller body 242 can both contact the portion of the current collector 31 that is not coated with the insulating slurry 32, thereby cooperating in conveying the current collector 31. The first roller body 241 and the second roller body 242 will not contact the insulating slurry 32 coated on the current collector 31, and are not likely to damage the insulating slurry 32 coated on the current collector 31, which is beneficial to improving the coating quality of the insulating slurry 32 and facilitating the control of the coating thickness of the insulating slurry 32. In addition, conveying the current collector 31 through the roller clamp mechanism 240 can reduce the risk of the current collector 31 shaking, facilitate coating the active material slurry on the current collector 31, and help improve the coating quality of the active material slurry.
[0132] Please refer to Fig. 9 and Fig.10 In some embodiments, the planes where the axis of the first roller body 241 and the axis of the second roller body 242 are located are parallel to the vertical plane.
[0133] “The plane where the axis of the first roller 241 and the axis of the second roller 242 are located is parallel to the vertical plane” means that the plane where the axis of the first roller 241 and the axis of the second roller 242 are located is approximately parallel to the vertical plane. The angle between the plane where the axis of the first roller 241 and the axis of the second roller 242 are located and the vertical plane is less than or equal to 5°.
[0134] By making the plane where the axis of the first roller body 241 and the axis of the second roller body 242 are located parallel to the vertical plane, the risk of the current collector 31 being wrinkled after passing through the roller clamp mechanism 240 can be reduced.
[0135] Please refer to Fig. 9 , Fig.10 and Fig.11 , Fig.11 A schematic diagram of the connection between the second roller 242 and the first driving member 243 provided in some embodiments of the present application. In some embodiments, the roller clamping mechanism 240 further includes a first driving member 243, which is connected to the second roller 242 and is used to drive the second roller 242 to rotate.
[0136] The first driving member 243 may include a rotating driving member, which is connected to the second roller body 242, and drives the second roller body 242 to rotate. The rotating driving member may be a motor, an internal combustion engine, etc. The first driving member 243 may also include a linear driving member and a transmission mechanism, wherein the linear driving member is connected to the second roller body 242 through the transmission mechanism, and the transmission mechanism converts the linear motion output by the linear driving member into the rotational motion of the second roller body 242. The linear driving member may be a linear electric cylinder, a linear air cylinder, a linear oil cylinder, etc. The transmission mechanism may be a crank rocker mechanism, a worm mechanism, etc.
[0137] By setting the first driving member 243 to drive the second roller 242 to actively rotate, the second roller 242 and the first roller 241 cooperate to transport the collector 31, so that the roller clamping mechanism 240 forms a tension barrier between the first coating mechanism 220 and the second coating mechanism 230, so that the tension of the collector 31 is balanced during the transportation process.
[0138] Please refer to Fig. 9 , Fig.10 and Fig.11 In some embodiments, the second coating mechanism 230 includes a coating head 231, and a first gap is formed between the coating head 231 and the second roller 242. The first gap is used for the current collector 31 to pass through, and the coating head 231 is used to coat the second slurry on the current collector 31.
[0139] The coating head 231 is disposed opposite to the second roller body 242 . The second roller body 242 can support the current collector 31 . The coating head 231 can coat the second slurry on the current collector 31 supported by the second roller body 242 .
[0140] There is a first gap between the coating head 231 and the second roller body 242, and the first gap is used for the pole piece to pass through. When the pole piece passes through the first gap, the coating head 231 can coat the second slurry on the current collector 31. The pole piece manufacturing device 20 uses the second roller body 242 to support the current collector 31, so that it is convenient for the coating head 231 to coat the active material slurry on the current collector 31. The second roller body 242 can cooperate with the first roller body 241 to transport the current collector 31, and can also support the current collector 31. One component plays multiple roles, which is conducive to simplifying the structure of the pole piece manufacturing device 20 and reducing the cost of the pole piece manufacturing device 20.
[0141] Please refer to Fig. 9 and Fig.12 , Fig.12 A schematic diagram of the structure of the first coating mechanism 220 provided in some embodiments of the present application. In some embodiments, the first coating mechanism 220 includes a reservoir 222 and a gravure roller 221, and the reservoir 222 is used to store the first slurry. The gravure roller 221 is rotatably connected to the reservoir 222, and the gravure roller 221 is used to apply the first slurry in the reservoir 222 to the current collector 31.
[0142] The accumulator 222 is a container for storing the first slurry. The accumulator 222 may be a storage bin, a storage tank, a storage box, etc. The gravure roller 221 is rotatably disposed in the accumulator 222, a portion of the gravure roller 221 is located outside the accumulator 222, and another portion of the gravure roller 221 is located inside the accumulator 222. The gravure roller 221 can apply the first slurry in the accumulator 222 to the current collector 31 during its rotation relative to the accumulator 222.
[0143] The insulating slurry 32 is coated on the current collector 31 by the gravure roller 221 , which facilitates ultra-thin coating and enables the thickness of the insulating slurry 32 to be more consistent.
[0144] Please refer to Fig. 9 and Fig.12 In some embodiments, the first coating mechanism 220 further includes a second driving member 223 , and the second driving member 223 is connected to the gravure roller 221 , and the second driving member 223 is used to drive the gravure roller 221 to rotate.
[0145] The second driving member 223 may include a rotating driving member, which is connected to the gravure roller 221, and the rotating driving member drives the gravure roller 221 to rotate. The rotating driving member may be a motor, an internal combustion engine, etc. The second driving member 223 may also include a linear driving member and a transmission mechanism, wherein the linear driving member is connected to the gravure roller 221 through the transmission mechanism, and the transmission mechanism converts the linear motion output by the linear driving member into the rotational motion of the gravure roller 221. The linear driving member may be a linear electric cylinder, a linear air cylinder, a linear oil cylinder, etc. The transmission mechanism may be a crank rocker mechanism, a worm mechanism, etc.
[0146] By providing the second driving member 223 to drive the gravure roller 221 to actively rotate, the linear velocity of any point on the outer circumference of the gravure roller 221 can be greater than the conveying velocity of the current collector 31, thereby facilitating the coating effect of the first slurry.
[0147] Please refer to Fig. 9 and Fig.12 In some embodiments, the diameter of the gravure roller 221 is D, satisfying: 100 mm ≤ D ≤ 300 mm.
[0148] The diameter of the gravure roller 221 may be: D=100 mm, 120 mm, 140 mm, 160 mm, 180 mm, 200 mm, 220 mm, 240 mm, 260 mm, 280 mm, 300 mm, etc.
[0149] By setting D≤300mm, the diameter of the gravure roller 221 is small, which is conducive to controlling the consistency of the coating thickness of the first slurry, and the first slurry can be coated thinner. By setting D≥100mm, the diameter of the gravure roller 221 is not too small, so that the gravure roller 221 has sufficient strength, reducing the risk of the gravure roller 221 breaking. Therefore, when 100mm≤D≤300mm, the strength of the gravure roller 221 and the coating effect can be taken into account.
[0150] Optionally, 120mm≤D≤160mm.
[0151] The diameter of the gravure roller 221 may be: D=120 mm, 125 mm, 130 mm, 135 mm, 140 mm, 145 mm, 150 mm, 155 mm, 160 mm, etc.
[0152] By setting D≤160mm, the diameter of the gravure roller 221 is smaller, which is more conducive to controlling the consistency of the coating thickness of the first slurry, and the first slurry can be coated thinner. By setting D≥120mm, the diameter of the gravure roller 221 is not too small, so that the gravure roller 221 has sufficient strength, reducing the risk of the gravure roller 221 breaking. Therefore, when 120mm≤D≤160mm, the strength of the gravure roller 221 and the coating effect can be taken into account.
[0153] Please refer to Fig. 9 and Fig.13 , Fig.13 A schematic diagram of the structure of the first coating mechanism 220 provided in other embodiments of the present application. In other embodiments, the first slurry is an insulating slurry 32, and the second slurry is an active material slurry. The first coating mechanism 220 includes a plurality of gravure rollers 221, which are arranged at intervals along the width direction of the current collector 31, and the gravure rollers 221 are used to coat the insulating slurry 32 on the current collector 31.
[0154] The first coating mechanism 220 includes a plurality of gravure rollers 221, and the plurality of gravure rollers 221 share a hopper 222. Along the width direction of the current collector 31, the plurality of gravure rollers 221 are arranged at intervals.
[0155] By providing multiple gravure rollers 221 and arranging the multiple gravure rollers 221 at intervals along the width direction of the current collector 31, multiple insulating slurry 32 can be coated on the current collector 31 at the same time, thereby improving the production efficiency of the pole piece and reducing the production cost of the pole piece.
[0156] In other embodiments, the first slurry is an insulating slurry 32, and the second slurry is an active material slurry. The pole piece manufacturing device 20 includes a plurality of first coating mechanisms 220, and the plurality of first coating mechanisms 220 are arranged along the width direction of the current collector 31. Each first coating mechanism 220 includes a gravure roller 221, and the gravure roller 221 is used to apply the insulating slurry 32 to the current collector 31.
[0157] The first coating mechanism 220 includes a gravure roller 221 and a accumulator 222 . The gravure roller 221 is rotatably connected to the accumulator 222 . A portion of the gravure roller 221 is located inside the accumulator 222 , and another portion of the gravure roller 221 is located outside the accumulator 222 .
[0158] The pole piece manufacturing device 20 includes a plurality of first coating mechanisms 220 arranged along the width direction of the current collector 31 , so as to coat a plurality of insulating pastes 32 in the width direction of the current collector 31 .
[0159] By providing a plurality of first coating mechanisms 220 and arranging the plurality of first coating mechanisms 220 along the width direction of the current collector 31 , a plurality of insulating slurry 32 can be coated on the current collector 31 at the same time, thereby improving the production efficiency of the pole piece and reducing the production cost of the pole piece.
[0160] Please refer to Fig.14 , Fig.14 The schematic diagram of the structure of the electrode manufacturing device 20 provided in some other embodiments of the present application. In some embodiments, the first coating mechanism 220 includes a pressing roller 261 , and the pressing roller 261 is used to press the current collector 31 onto the gravure roller 221 .
[0161] The pressing roller 261 is a roller body used to press the current collector 31 onto the gravure roller 221. The pressing roller 261 may be disposed upstream and / or downstream of the gravure roller 221.
[0162] By providing the pressing roller 261 to press the current collector 31 onto the gravure roller 221 , the gravure roller 221 can stably apply the first slurry to the current collector 31 , which is beneficial to improving the consistency of the first slurry coating.
[0163] In some embodiments, pressure rollers 261 are disposed both upstream and downstream of the gravure roller 221 .
[0164] Along the conveying direction of the current collector 31 , the gravure roller 221 is located between the two pressing rollers 261 .
[0165] By arranging pressure rollers 261 both upstream and downstream of the gravure roller 221 to improve the effect of pressing the current collector 31 to the gravure roller 221, the gravure roller 221 can more stably apply the first slurry to the current collector 31, which is beneficial to improving the consistency of the first slurry coating.
[0166] Please refer to Fig.14 and Fig.15 , Fig.15 A schematic diagram of the connection between the pressure roller 261 and the adjustment structure 262 provided in some embodiments of the present application. In some embodiments, the first coating mechanism 220 includes an adjustment structure 262, which is connected to the pressure roller 261. The adjustment structure 262 is used to adjust the position of the pressure roller 261 along the thickness direction of the current collector 31.
[0167] The adjustment structure 262 is a structure for adjusting the position of the pressure roller 261 along the thickness direction of the current collector 31. Optionally, the adjustment structure 262 includes an adjustment handle 2621, a first mounting seat 2622, a lead screw 2623 and a second mounting seat 263, wherein the first mounting seat 2622 and the second mounting seat 263 are slidably connected along the thickness direction of the current collector 31, the second mounting seat 263 is used to install the pressure roller 261, the lead screw 2623 is rotatably disposed on the first mounting seat 2622, the second mounting seat 263 is threadedly matched with the lead screw 2623, the adjustment handle 2621 is connected to the lead screw 2623, and the adjustment handle 2621 is used to drive the lead screw 2623 to rotate. When it is necessary to adjust the position of the pressure roller 261 along the thickness direction of the current collector 31, the adjustment handle 2621 is rotated, and the adjustment handle 2621 drives the screw 2623 to rotate. Since the second mounting seat 263 is slidably connected to the first mounting seat 2622 along the thickness direction of the current collector 31, the rotation of the second mounting seat 263 is restricted. The second mounting seat 263 is threadedly connected to the screw 2623. Therefore, the second mounting seat 263 will move relative to the first mounting seat 2622 along the thickness direction of the current collector 31 driven by the screw 2623 to achieve the adjustment of the position of the pressure roller 261.
[0168] By setting the adjustment structure 262 to adjust the position of the pressure roller 261 along the thickness direction of the current collector 31, the contact length between the gravure roller 221 and the current collector 31 can be adjusted, that is, the feed amount of the current collector 31 in contact with the gravure roller 221 can be adjusted. By adjusting the feed amount of the current collector 31 in contact with the gravure roller 221, the risk of missing coating can be reduced.
[0169] Please refer to Fig.16 , Fig.16 The first coating mechanism 220 is a schematic diagram of the structure of some other embodiments of the present application. In some embodiments, the first coating mechanism 220 further includes a scraper 224, and the scraper 224 is used to scrape off the excess first slurry on the gravure roller 221.
[0170] The scraper 224 may be disposed in the accumulator 222 . The scraper 224 is located at the side where the gravure roller 221 first rotates out of the accumulator 222 . The scraper 224 is used to scrape the outer surface of the gravure roller 221 , thereby scraping off excess first slurry.
[0171] The scraper 224 is provided to scrape off the excess first slurry on the gravure roller 221, which is helpful to control the coating thickness and coating consistency of the first slurry.
[0172] Optionally, the scraper 224 may include a positive scraper 2241, the blade of which is tangent to the outer circumference of the gravure roller 221, and the positive scraper 2241 is used to scrape off the excess first slurry on the outer circumference of the gravure roller 221. In addition, the positive scraper 2241 can also block the first slurry, reduce the probability of the first slurry being ejected from the storage tank 222, reduce the risk of splashing of the first slurry, and make it difficult for the first slurry to be thrown onto the current collector 31.
[0173] The scraper 224 may further include a side scraper 2242, the blade of which contacts the end surface of the gravure roller 221, and the side scraper 2242 is used to scrape off the excess first slurry on the end surface of the gravure roller 221. In addition, the side scraper 2242 can also block the first slurry, reduce the probability of the first slurry being ejected from the storage tank 222, reduce the risk of splashing of the first slurry, and make it difficult for the first slurry to be thrown onto the current collector 31. The scraper 224 may include two side scrapers 2242, which are respectively disposed at both ends of the gravure roller 221, and the two side scrapers 2242 are respectively used to scrape off the excess first slurry on the two end surfaces of the gravure roller 221.
[0174] In some embodiments, the position of the first coating mechanism 220 along the width direction of the current collector 31 is adjustable.
[0175] The first coating mechanism 220 is configured to be able to change the position of the first coating mechanism 220 in the width direction of the current collector 31. Optionally, the pole piece manufacturing device 20 includes a frame, and the first coating mechanism 220 is adjustably arranged on the frame along the width direction of the current collector 31.
[0176] By making the position of the first coating mechanism 220 adjustable along the width direction of the current collector 31, the position of the first coating mechanism 220 in the width direction of the current collector 31 can be adjusted as needed to meet the manufacturing requirements of different pole pieces, which is beneficial to improving the adaptability of the pole piece manufacturing device 20 to manufacturing pole pieces of different models.
[0177] Please refer to Fig.16 , Fig.16 The schematic diagram of the structure of the first coating mechanism 220 provided in some other embodiments of the present application. In some other embodiments, the pole piece manufacturing device 20 includes a guide member 225, the guide member 225 extends along the width direction of the current collector 31, and the first coating mechanism 220 cooperates with the guide member 225 in a guiding manner.
[0178] The guide member 225 is a component for guiding the first coating mechanism 220 to move in the width direction of the current collector 31. In some embodiments, the guide member 225 is a guide rail, the first coating mechanism 220 is connected to the guide member 225, and the first coating mechanism 220 can slide relative to the guide rail, thereby changing the position of the first coating mechanism 220 in the width direction of the current collector 31. In other embodiments, the guide member 225 is a guide rod.
[0179] The guide member 225 is provided to guide the first coating mechanism 220 to move along the width direction of the current collector 31 , thereby reducing the risk of the first coating mechanism 220 running off when adjusting the position of the first coating mechanism 220 .
[0180] Please refer to Fig.17 , Fig.17 The schematic diagram of the structure of the electrode manufacturing device 20 provided in some other embodiments of the present application. In some other embodiments, the electrode manufacturing device 20 further includes a drying mechanism 270, which is arranged downstream of the second coating mechanism 230. The drying mechanism 270 is used to dry the first slurry and the second slurry.
[0181] The drying mechanism 270 is disposed downstream of the second coating mechanism 230 along the conveying direction of the current collector 31. The current collector 31 passes through the unwinding mechanism 210, the first coating mechanism 220, the roller clamping mechanism 240, the second coating mechanism 230, the drying mechanism 270 and the winding mechanism 252 in sequence.
[0182] The drying mechanism 270 is provided to dry the first slurry and the second slurry to form an insulating layer and an active material layer on the current collector 31 .
[0183] According to some embodiments of this application, please refer to Figure 1 to Figure 17 .
[0184] The present application embodiment provides a pole piece manufacturing method 10, and the pole piece manufacturing method 10 includes:
[0185] Step S100: providing a current collector 31;
[0186] Step S200: coating the first slurry on the current collector 31;
[0187] Step S300: coating the second slurry on the current collector 31 so that the second slurry and the first slurry are arranged in the width direction of the current collector 31;
[0188] In which, before step S200 and step S300 , one of the first slurry and the second slurry is an active material slurry, and the other of the first slurry and the second slurry is an insulating slurry 32 .
[0189] When the pole piece manufacturing method 10 is used to manufacture the pole piece, the insulating slurry 32 can be first coated on the current collector 31, and then the active material slurry can be coated on the current collector 31, or the active material slurry can be first coated on the current collector 31, and then the insulating slurry 32 can be coated on the current collector 31. In this way, the insulating slurry 32 and the active material slurry are coated separately, and the coating of the insulating slurry 32 and the coating of the active material slurry do not affect each other, which can improve the coating quality of the insulating slurry 32 and the active material slurry, facilitate accurate control of the coating thickness of the insulating slurry 32 and the active material slurry, and help reduce the manufacturing cost of the pole piece. In addition, the electrode assembly manufactured using the pole piece can be more conveniently put into the shell, and the risk of redundant pole ears is reduced, which is conducive to improving the reliability of the battery cell.
[0190] The first slurry is an insulating slurry 32, and the second slurry is an active material slurry; step S300 includes:
[0191] Step S310: Apply active material slurry on the current collector 31, and make the active material slurry cover a part of the insulating slurry 32. When manufacturing the pole piece, first apply the insulating slurry 32 on the current collector 31, and then apply the active material slurry on the current collector 31, so that when applying the active material slurry, the active material slurry can cover a part of the insulating slurry 32, reducing the risk of the current collector 31 being exposed.
[0192] Before step S300 and after step S200, the pole piece manufacturing method 10 further includes: step S250: conveying the current collector 31 through the roller clamp mechanism 240. The roller clamp mechanism 240 includes a first roller body 241 and a second roller body 242. The first roller body 241 includes a first roller segment 2411 and a second roller segment 2412. The second roller segment 2412 and the first roller segment 2411 are arranged along the axial direction of the first roller body 241. The diameter of the second roller segment 2412 is greater than the diameter of the first roller segment 2411. The second roller segment 2412 and the second roller body 242 are used to contact the portion of the current collector 31 that is not coated with the insulating slurry 32, so as to cooperate in conveying the current collector 31. The first roller segment 2411 and the insulating slurry 32 are arranged in a gap. Both the second roller segment 2412 and the second roller body 242 can contact the portion of the current collector 31 that is not coated with the insulating slurry 32, so as to cooperate in conveying the current collector 31. Neither the first roller body 241 nor the second roller body 242 will contact the insulating slurry 32 coated on the current collector 31, and is not likely to damage the insulating slurry 32 coated on the current collector 31, which is beneficial to improving the coating quality of the insulating slurry 32 and facilitating the control of the coating thickness of the insulating slurry 32. In addition, the current collector 31 is transported by the roller clamp mechanism 240, which can reduce the risk of the current collector 31 shaking, facilitates the coating of the active material slurry on the current collector 31, and is beneficial to improving the coating quality of the active material slurry.
[0193] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.
Claims
1. A method for manufacturing a pole piece, characterized in that: include: Step S100: providing a current collector; Step S200: coating a first slurry on the current collector; Step S250: conveying the current collector through a roller clamping mechanism, wherein the roller clamping mechanism comprises a first roller body and a second roller body, wherein the first roller body comprises a first roller segment and a second roller segment, wherein the second roller segment and the first roller segment are arranged along the axial direction of the first roller body, wherein the diameter of the second roller segment is greater than the diameter of the first roller segment, wherein the second roller segment and the second roller body are used to contact a portion of the current collector that is not coated with the first slurry, so as to cooperate in conveying the current collector, and a gap is set between the first roller segment and the first slurry; Step S300: coating the second slurry on the current collector so that the second slurry and the first slurry are arranged in the width direction of the current collector; Wherein, in step S200, before step S300, one of the first slurry and the second slurry is an active material slurry, and the other of the first slurry and the second slurry is an insulating slurry; In the step S300 , the second slurry is coated on the current collector supported by the second roller by a coating head.
2. The pole piece manufacturing method according to claim 1, characterized in that: The first slurry is the insulating slurry, and the second slurry is the active material slurry; The step S300 includes: Step S310: coating the active material slurry on the current collector, and allowing the active material slurry to cover a portion of the insulating slurry.
3. The pole piece manufacturing method according to claim 2, characterized in that: The step S200 includes: Step S210: coating a plurality of the first slurries on the current collector so that the plurality of the first slurries are arranged along the width direction of the current collector; The step S300 includes: Step S320: applying the second slurry between two adjacent first slurries.
4. The pole piece manufacturing method according to claim 3, characterized in that: The step S210 includes: Step S211: coating a plurality of the first slurries on the current collector simultaneously.
5. The pole piece manufacturing method according to claim 2, characterized in that: The step S200 includes: Step S220: coating the insulating slurry on the current collector by using a gravure roller.
6. The pole piece manufacturing method according to claim 1, characterized in that: After step S300, the pole piece manufacturing method further includes: Step S400: drying the first slurry and the second slurry.
7. A pole piece manufacturing device, characterized in that: include: An unwinding mechanism, used for unwinding the current collector; A first coating mechanism, disposed downstream of the unwinding mechanism, and used for coating a first slurry on the current collector; A roller clamping mechanism is arranged downstream of the first coating mechanism, the roller clamping mechanism comprises a first roller body and a second roller body, the first roller body comprises a first roller segment and a second roller segment, the second roller segment and the first roller segment are arranged along the axial direction of the first roller body, the diameter of the second roller segment is larger than the diameter of the first roller segment, the second roller segment and the second roller body are used to contact the portion of the current collector that is not coated with the first slurry to cooperate in conveying the current collector, and a gap is set between the first roller segment and the first slurry; a second coating mechanism, disposed downstream of the roller clamp mechanism, the second coating mechanism being used to coat a second slurry on the current collector, the second slurry and the first slurry being arranged in a width direction of the current collector, one of the first slurry and the second slurry being an active material slurry, and one of the first slurry and the second slurry being an insulating slurry; The second coating mechanism includes a coating head, and a first gap is defined between the coating head and the second roller body, wherein the first gap is used for the current collector to pass through, and the coating head is used for coating the second slurry on the current collector supported by the second roller body.
8. The pole piece manufacturing device according to claim 7, characterized in that: The planes where the axes of the first roller body and the second roller body are located are parallel to a vertical plane.
9. The pole piece manufacturing device according to claim 7, characterized in that: The roller clamping mechanism further includes a first driving member, the first driving member is connected to the second roller body, and the first driving member is used to drive the second roller body to rotate.
10. The pole piece manufacturing device according to any one of claims 7 to 9, characterized in that: The first coating mechanism comprises: A storage container, used for storing the first slurry; A gravure roller is rotatably connected to the material storage container, and is used to apply the first slurry in the material storage container to the current collector.
11. The pole piece manufacturing device according to claim 10, characterized in that: The first coating mechanism further includes a second driving member, the second driving member is connected to the gravure roller, and the second driving member is used to drive the gravure roller to rotate.
12. The pole piece manufacturing device according to claim 10, characterized in that: The diameter of the gravure roller is D, which satisfies: 100mm≤D≤300mm.
13. The pole piece manufacturing device according to claim 12, characterized in that: 120mm≤D≤160mm.
14. The pole piece manufacturing device according to claim 10, characterized in that: The first slurry is the insulating slurry, and the second slurry is the active material slurry; The first coating mechanism includes a plurality of gravure rollers, which are arranged at intervals along the width direction of the current collector, and the gravure rollers are used to coat the insulating slurry on the current collector.
15. The pole piece manufacturing device according to claim 10, characterized in that: The first slurry is the insulating slurry, and the second slurry is the active material slurry; The pole piece manufacturing device includes a plurality of the first coating mechanisms, which are arranged along the width direction of the current collector, and each of the first coating mechanisms includes a gravure roller, which is used to coat the insulating slurry on the current collector.
16. The pole piece manufacturing device according to claim 10, characterized in that: The first coating mechanism includes a pressing roller, and the pressing roller is used to press the current collector onto the gravure roller.
17. The pole piece manufacturing device according to claim 16, characterized in that: The pressure rollers are arranged upstream and downstream of the gravure roller.
18. The pole piece manufacturing device according to claim 16, characterized in that: The first coating mechanism includes an adjusting structure, the adjusting structure is connected to the pressing roller, and the adjusting structure is used to adjust the position of the pressing roller along the thickness direction of the current collector.
19. The pole piece manufacturing device according to claim 10, characterized in that: The first coating mechanism further includes a scraper, and the scraper is used to scrape off excess first slurry on the gravure roller.
20. The pole piece manufacturing device according to any one of claims 7 to 9, characterized in that: The position of the first coating mechanism along the width direction of the current collector is adjustable.
21. The pole piece manufacturing device according to claim 20, characterized in that: The pole piece manufacturing device comprises a guide member, the guide member extends along the width direction of the current collector, and the first coating mechanism cooperates with the guide member in a guiding manner.
22. The pole piece manufacturing device according to any one of claims 7 to 9, characterized in that: The pole piece manufacturing device further includes a drying mechanism, which is disposed downstream of the second coating mechanism and is used to dry the first slurry and the second slurry.