Method for manufacturing detection probe for simultaneous detection of ion implantation dose and temperature and detection method
By constructing a detection probe with a patterned electrode layer and a pyroelectric material film layer on a silicon wafer, the problem of inaccurate ion implantation dose and temperature detection in the existing technology is solved, and a higher-precision detection effect is achieved.
Patent Information
- Application Number
- CN202410627039.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-21
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-05-21
AI Technical Summary
Existing ion implantation dose detection methods cannot achieve high-precision measurement, especially when high-resolution, small-dose implantation has large errors, and temperature detection is inaccurate, affecting the performance of semiconductor products.
Design a detection probe by growing an insulating dielectric film layer and a pyroelectric material film layer on a silicon wafer, forming a patterned electrode layer on it, and combining photolithography and etching processes to form openings to optimize the probe structure. , to achieve simultaneous detection of dose and temperature during ion implantation.
It improves the accuracy and response speed of ion implantation dose detection, reduces manufacturing complexity and cost, avoids errors caused by instability during ion beam flight, and ensures accurate measurement of temperature and dose.
Smart Images

Figure CN118213288B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of ion implantation, and in particular to a method for manufacturing a detection probe for simultaneously detecting ion implantation dose and temperature, and a detection method. Background Art
[0002] In the semiconductor manufacturing process, ion implantation is a key step to change the electrical properties of semiconductor materials. It is crucial to control the concentration and depth distribution of impurities. At the same time, monitoring the dose and temperature during ion implantation is of great significance to ensure product quality and process control. However, existing monitoring equipment often cannot achieve high-precision measurement of dose and substrate temperature at the same time, and mainly detects the dose of ion implantation.
[0003] The current dose detection method mainly uses the angle Faraday cup for detection. The ions generated by the ion source are accelerated by the accelerator tube to form an ion beam. Before the ion beam enters the ion implantation chamber, it passes through a circular through hole. The Faraday cup is set around the circular through hole. The cross-section of the ion beam is larger than the circular through hole. Therefore, when the ion beam passes through the circular through hole, some ions will be detected by the Faraday cup. The Faraday cup is used to detect the amount of ions in the ion beam, and finally the amount of ions implanted into the wafer is obtained.
[0004] However, the current ion implantation detection method still has the following shortcomings:
[0005] 1. Since the Faraday cup detection mode is theoretically still a random inspection method, because the Faraday cup only detects a small area in the ion beam, the final result is to calculate the dose of the ion beam based on the value detected by the Faraday cup, assuming that the ions in the ion beam are completely uniformly distributed. This dose detection method has little error in the high-dose implantation process, but it has a very large impact on high-resolution, small-dose ion implantation, resulting in inaccurate ion implantation, thereby affecting the performance of the semiconductor power device.
[0006] 2. Since there is a distance between the Faraday cup detection position and the wafer, the ion beam needs to fly a certain distance after detection. There are many uncertainties in this flight process, which can easily cause inaccurate ion status and quantity. In particular, some processes will use electron spray to neutralize the ions before injecting them into the wafer, so that they form neutral atoms and are injected into the wafer. At this time, the impact on the ion implantation dose is greater, and the final detection data does not match the actual injection dose. Summary of the invention
[0007] The first technical problem to be solved by the present invention is to provide a method for manufacturing a detection probe for simultaneously detecting ion implantation dose and temperature. The manufacturing method can manufacture a detection probe that is convenient for simultaneously detecting ion implantation dose and temperature, making the detected dose more accurate.
[0008] The second technical problem to be solved by the present invention is to provide a detection method for simultaneously detecting ion implantation dose and temperature, which can simultaneously detect the implantation dose and temperature of the wafer during ion implantation, and the detection result is more accurate.
[0009] In order to solve the above-mentioned first technical problem, the technical solution of the present invention is: a method for manufacturing a detection probe for simultaneous detection of ion implantation dose and temperature, comprising the following steps:
[0010] S1, growing a front insulating dielectric thin film layer and a back insulating dielectric thin film layer on the front and back of the silicon wafer respectively;
[0011] S2. A patterned lower electrode layer is fabricated on the front insulating dielectric film layer, wherein the lower electrode layer includes an equal number of functional lower electrodes and pin lower electrodes arranged in pairs, wherein the functional lower electrodes are discretely distributed in the middle of the silicon wafer, and the pin lower electrodes are located outside the functional lower electrodes, and a lower connecting wire is connected between each functional lower electrode and the pin lower electrode;
[0012] S3, depositing a pyroelectric material thin film layer on the functional lower electrode;
[0013] S4. Growing an upper electrode layer on the front insulating dielectric film layer and the pyroelectric material film layer; wherein the upper electrode layer comprises an equal number of functional upper electrodes and pin upper electrodes arranged in pairs, the functional upper electrodes are located on the upper surface of the pyroelectric material film layer, the pin upper electrodes are located on the upper surface of the front insulating dielectric film layer and are discretely distributed, an upper connecting wire is connected between each pin upper electrode and the corresponding functional upper electrode; the upper connecting wire and the lower connecting wire are independent of each other and do not contact each other; the pin upper electrode and the pin lower electrode are independent of each other and do not contact each other, and the mutually superimposed functional upper electrode, the pyroelectric material film layer and the functional lower electrode constitute a probe monomer;
[0014] S5, forming a photoresist pattern layer on the surface of the back insulating dielectric film layer, wherein the photoresist pattern layer has pattern grooves corresponding to the pyroelectric material film layer one by one;
[0015] S6, using the photoresist pattern layer as a mask, etching the back insulating dielectric film layer and the silicon wafer from the back side to form open grooves corresponding to the pyroelectric material film layer one by one, and the bottom of the open grooves is flush with the back side of the front insulating dielectric film layer;
[0016] S7, removing the photoresist pattern layer and the back insulating dielectric film layer;
[0017] S8. Fix a glass sheet on the back of the silicon wafer in a vacuum environment.
[0018] Preferably, the silicon wafer is a single crystal silicon wafer, and the front insulating dielectric film layer and the back insulating dielectric film layer are silicon nitride layers or silicon dioxide layers or a combination of silicon nitride layers and silicon dioxide layers.
[0019] Preferably, the lower electrode layer is any one of gold, platinum, silver, copper, tungsten and molybdenum or an alloy of several of them, and the thickness of the lower electrode layer is 50nm-5um.
[0020] Preferably, the pyroelectric material in the pyroelectric material film layer is one of triethylene glycol sulfate and its derivatives, adamantane formate, polyvinylidene fluoride, lithium tantalate, lithium niobate, zinc oxide, aluminum nitride, lead zirconate titanate (PZT), barium strontium titanate, lead tantalate scandate, and lead magnesium niobate titanate.
[0021] Preferably, the thickness of the pyroelectric material film layer is 50nm-5um.
[0022] Preferably, in step S7, polishing equipment is used to grind and remove the insulating dielectric film layer on the back side.
[0023] Preferably, the glass sheet is fixed in step S8 by using ultraviolet light assisted bonding, anodic bonding or intermediate layer bonding technology.
[0024] After adopting the above technical scheme, the effects of the present invention are: 1. The photolithography, etching and thin film processes used in the detection probe manufacturing method of the present invention can be effectively compatible with the CMOS process, mass-produced, and have obvious manufacturing cost-effectiveness; 2. The integration is high. By integrating the upper electrode, the lower electrode and the pyroelectric material film layer on the same silicon wafer, the simultaneous measurement of dose and temperature is achieved, reducing the complexity and cost of the manufacturing process; 3. By opening an open groove and fixing it with a glass sheet to form a vacuum chamber, the bottom of the groove is flush with the back of the front insulating dielectric film layer, which can further optimize the sensitive area, ensure that the heat generated during ion injection can directly act on the pyroelectric material, reduce heat transfer, and ensure that the voltage generated between the upper electrode and the lower electrode due to the pyroelectric effect is stable, thereby improving the response speed and sensitivity of each probe monomer.
[0025] To solve the second technical problem mentioned above, the technical solution of the present invention is: a detection method for simultaneously detecting ion implantation dose and temperature, the detection method uses a detection device, the detection device includes a conversion circuit board and the detection probe, the detection probe is bonded to the conversion circuit board to form a wafer tray, the conversion circuit board is provided with an external plug connected to the controller; the conversion circuit board is provided with lead electrodes corresponding to the pin upper electrode and the pin lower electrode one by one, each lead electrode is conductively connected to the corresponding pin upper electrode and pin lower electrode; a placement area for convenient wafer placement is provided on the wafer tray, and each probe monomer together constitutes a detection area, and at least a part of the probe monomers in the detection area are outside the placement area;
[0026] The detection method first places a detection device on an ion implanter for calibration, and obtains a standard corresponding relationship between the voltage, temperature and implantation dose between a functional upper electrode and a functional lower electrode; then places the detection device in a vacuum implantation chamber of the ion implanter and connects an external connector to a controller, places a wafer in a placement area and fixes it, and then starts the ion implanter, and an ion beam is implanted on the wafer according to a set scanning route, and the scanning area of the ion beam is greater than or equal to the detection area, so that ions are implanted into the wafer and also into the functional upper electrode, and the voltage between the functional upper electrode and the functional lower electrode is detected in real time, and the dose and temperature during the current ion implantation are calculated according to the standard corresponding relationship.
[0027] After adopting the above technical scheme, the effects of the present invention are as follows: first, the detection method uses the detection device directly as a wafer holder during ion implantation, that is, the wafer is directly fixed on the detection probe, and the detection area at this time is the end of the ion implantation into the wafer, so that the instability of the ion beam during the flight process can be avoided, resulting in inaccurate detection results, and the error can be reduced as much as possible; secondly, the detection method utilizes the above detection probe, and when the detection probe is used, the ions are implanted into the wafer and also implanted into the functional upper electrode. Since the functional upper electrode will quickly stop the implanted ion beam or atomic beam in the functional upper electrode during high-speed ion implantation, and effectively generate heat energy at the same time, and the heat will be quickly conducted to the pyroelectric material film layer. The pyroelectric material will generate electric charge when the temperature changes, and its function is to convert the temperature change into a measurable electrical signal, so that a voltage will be formed between the functional upper electrode and the functional lower electrode on the upper and lower sides of the pyroelectric material film layer, and the implanted dose and temperature can be accurately obtained through the voltage, and the detection result is more accurate, and the response speed is also faster, and the ion implantation parameters can be more accurately controlled, and the negative impact caused by excessive temperature can be avoided.
[0028] Preferably, the detection method also includes a self-calibration method, and the self-calibration method is started after the detection device has been used for a period of time; during calibration, the wafer is not placed and ion injection is directly started, at which time the scanning area of the ion beam will cover all functional upper electrodes, and the voltage between all functional upper electrodes and corresponding functional lower electrodes is detected; the voltage difference between the probe monomer in the placement area and the probe monomer outside the placement area is compared and an error compensation coefficient is calculated, and the correspondence between the voltage, temperature and injection dose is updated by the error compensation coefficient to form an updated compensation correspondence, and then the compensation correspondence is used to calculate the current ion injection dose and temperature during ion injection. Therefore, the self-calibration method can perform self-calibration on the detection device after being used for a period of time, and all functional upper electrodes originally covered by the wafer will be injected with ions during self-calibration, so the detection results between the probe monomer in the placement area and the probe monomer outside the placement area can be calculated to calculate the error compensation coefficient, thereby realizing self-calibration. After the self-calibration method is used, the service life of the detection device can be further extended, and the accuracy of long-term detection can be guaranteed.
[0029] Preferably, the specific method of conductive connection between each lead electrode and the corresponding pin upper electrode and pin lower electrode is welding, wire bonding or conductive adhesive bonding. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] The present invention is further described below in conjunction with the accompanying drawings and embodiments.
[0031] Figure 1 is a schematic diagram of the structure after the lower electrode layer is manufactured in an embodiment of the present invention;
[0032] Figure 2 is a schematic diagram of the structure after a pyroelectric material thin film layer is deposited in an embodiment of the present invention;
[0033] Figure 3 is a schematic diagram of the structure after the upper electrode layer is manufactured in an embodiment of the present invention;
[0034] Figure 4 It is a schematic diagram of the structure of the detection device;
[0035] Figure 5 It is a partial structural cross-sectional view of a silicon wafer, a front insulating dielectric film layer, and a back insulating dielectric film layer;
[0036] Figure 6 It is a cross-sectional view of the local structure after the lower electrode layer is made;
[0037] Figure 7 It is a cross-sectional view of the local structure after the pyroelectric material thin film layer is deposited;
[0038] Figure 8It is a cross-sectional view of the local structure after the upper electrode layer is made;
[0039] Fig. 9 It is a cross-sectional view of the local structure after the opening groove is formed;
[0040] Fig.10 It is a cross-sectional view of the local structure after the photoresist pattern layer and the back insulating dielectric film layer;
[0041] Fig.11 It is a schematic diagram of the structure after the glass sheet is set;
[0042] In the accompanying drawings: In the accompanying drawings: 1. Silicon wafer; 2. Front insulating dielectric film layer; 21. Silicon dioxide layer; 22. Silicon nitride layer; 3. Lower electrode layer; 31. Functional lower electrode; 32. Pin lower electrode; 33. Lower connecting wire; 4. Placement area; 5. Back insulating dielectric film layer; 6. Pyroelectric material film layer; 7. Upper electrode layer; 71. Functional upper electrode; 72. Pin upper electrode; 73. Upper connecting wire; 8. External plug; 9. Controller; 10. Open slot; 11. Glass sheet; 12. Conversion circuit board; 13. Lead-out electrode. DETAILED DESCRIPTION
[0043] The present invention is further described in detail below through specific examples.
[0044] like Figures 1 to 11 As shown, a method for manufacturing a detection probe for simultaneous detection of ion implantation dose and temperature comprises the following steps:
[0045] S1, growing a front insulating dielectric thin film layer 2 and a back insulating dielectric thin film layer 5 on the front and back of the silicon wafer 1 respectively;
[0046] First, the silicon wafer 1 preferably uses single crystal silicon. The single crystal silicon wafer 1 needs to be thoroughly cleaned to remove the pollutants and oxide layer on the surface. Then, a uniform dielectric film is grown on the front and back of the silicon wafer 1 by chemical vapor deposition, physical vapor deposition or atomic layer deposition. The function of the insulating dielectric film layer is to provide insulation and mechanical support. The insulating dielectric film layer not only prevents direct contact between the surface of the silicon wafer 1 and the external environment, reduces the risk of chemical corrosion and physical damage, but also provides a stable substrate for subsequent electrodes and pyroelectric materials. The silicon wafer 1 is a single crystal silicon wafer 1, and the front insulating dielectric film layer 2 and the back insulating dielectric film layer 5 are silicon nitride layers 22 or silicon dioxide layers 21 or a combination of silicon nitride layers 22 and silicon dioxide layers 21, and the thickness range is between 50nm and 10um.
[0047] In this embodiment, the preferred combination layer is firstly, a four-inch n-Si (100) single crystal silicon wafer 1 is used as a substrate, and is thoroughly cleaned and pretreated to ensure the cleanliness of the surface. In an ultra-clean environment, a 500nm thick silicon dioxide 101 is grown by thermal oxidation, and then sent to a low-pressure chemical vapor deposition (LPCVD) device to grow a 300nm thick silicon nitride (Si3N4) layer on the surface of the silicon dioxide to form a composite dielectric thin film layer. The LPCVD process is carried out in a vacuum chamber, with dichlorosilane and ammonia as source gases, which react on the surface of the heated silicon wafer 1 to form a uniform silicon nitride layer 22.
[0048] S2. A patterned lower electrode layer 3 is fabricated on the front insulating dielectric film layer 2, wherein the lower electrode layer 3 includes equal numbers of functional lower electrodes 31 and pin lower electrodes 32 arranged in pairs, wherein the functional lower electrodes 31 are discretely distributed in the middle of the silicon wafer 1, and the pin lower electrodes 32 are located outside the functional lower electrodes 31, and a lower connecting wire 33 is connected between each functional lower electrode 31 and the pin lower electrode 32; wherein the number of the functional lower electrodes 31 is multiple and arranged in an array. The lower connecting wire 33 can be formed by metal bonding or welding after the functional lower electrode 31 and the pin lower electrode 32 are formed.
[0049] The design of the patterned lower electrode layer 3 is to achieve specific electrical properties. These electrodes are used to apply voltage to the pyroelectric material or collect the charge generated by it. The design of the array arrangement can optimize the electric field distribution and improve the charge collection efficiency, thereby enhancing the sensitivity and resolution of the detection probe. The lower electrode layer 3 is any one or several alloys of gold, platinum, silver, copper, tungsten, and molybdenum, and the thickness of the lower electrode layer 3 is 50nm-5um. The lower electrode layer 3 can be prepared by sputtering, electroplating technology, electron beam evaporation, thermal evaporation and other technologies. Ohmic electrical contact is formed between the lower electrode and the pyroelectric material film layer 6 to better collect the voltage generated by the temperature difference in the pyroelectric material.
[0050] Using a standard ultraviolet lithography process, the silicon nitride layer 22 is first cleaned, and then a photosensitive resin of model AZ6130 is spin-coated. The photosensitive resin is exposed using an ultraviolet lithography machine to form a desired pattern. The exposed photosensitive resin is developed to remove the photosensitive resin in the exposed area, leaving the desired pattern. Subsequently, a 300nm thick metal film is deposited using electron beam evaporation deposition technology, and peeled off in acetone to form a patterned lower electrode layer 3.
[0051] S3, depositing a pyroelectric material thin film layer 6 on the functional lower electrode 31;
[0052] Using ultraviolet lithography technology, define the pattern area just covering the pattern of the patterned lower electrode layer 3. Using magnetron sputtering, deposit a 1um thick lead zirconate titanate (PZT) pyroelectric film, and remove the excess pyroelectric film in acetone to form a pyroelectric material film layer 6 with a size and shape that meets the design requirements.
[0053] The pyroelectric material film is the core part of the detection. The pyroelectric material will generate electric charge when the temperature changes. Its function is to convert the temperature change into a measurable electrical signal. When the ion beam or atomic beam is injected, the kinetic energy is converted into thermal energy and stops in the upper electrode layer 7. The temperature change measured by the pyroelectric material can be converted into the injection dose and temperature.
[0054] Preferably, the pyroelectric material in the pyroelectric material film layer 6 is one of triethylene glycol sulfate and its derivatives, adamantane amine formate, polyvinylidene fluoride, lithium tantalate, lithium niobate, zinc oxide, aluminum nitride, lead zirconate titanate (PZT), barium strontium titanate, lead tantalate scandate, and lead magnesium niobate titanate. The thickness of the pyroelectric material film layer 6 is 50nm-5um.
[0055] Pyroelectric materials release electric charges outward when the temperature changes. The fundamental principle is that the spontaneous polarization intensity of the material changes with the temperature. The structure of pyroelectric materials does not have a symmetric center, and orderly arranged electric dipole moments appear, which show spontaneous polarization in a unified vector direction to the outside as a whole. Positive / negative bound charges appear on the surface of the material in the direction of the polarization vector, so the surface will absorb equal amounts of free charges of opposite signs in the environment, and thus will not show electrical properties to the outside. When the temperature of the pyroelectric material changes due to external stimuli, the intensity of spontaneous polarization will change, and the amount of bound charge on the surface will change accordingly. After a certain number of bound charges are neutralized, the excess free charges will form an electric field in space, showing charge to the outside. If the surface of the material is connected to an external circuit, the positive and negative free charges will flow to form a current, which is the pyroelectric current.
[0056] The detection probe in the solution of the present invention is provided with an open groove 10 during manufacture, and the bottom of the open groove 10 is flush with the front insulating dielectric film layer 2, which directly reduces the heat loss as much as possible and ensures that the pyroelectric material can be used in ion implantation.
[0057] S4, growing an upper electrode layer 7 on the front insulating dielectric film layer 2 and the pyroelectric material film layer 6; wherein the upper electrode layer 7 comprises equal numbers of functional upper electrodes 71 and pin upper electrodes 72 arranged in pairs, the functional upper electrodes 71 being located on the upper surface of the pyroelectric material film layer 6, the pin upper electrodes 72 being located on the upper surface of the front insulating dielectric film layer 2 and being discretely distributed, an upper connecting wire 73 being connected between each pin upper electrode 72 and the corresponding functional upper electrode 71; the upper connecting wire 73 and the lower connecting wire 33 being independent of each other and not in contact; the pin upper electrode 72 and the pin lower electrode 32 being independent of each other and not in contact, and the mutually superimposed functional upper electrode 71, the pyroelectric material film layer 6 and the functional lower electrode 31 forming a probe monomer;
[0058] The main function of the functional upper electrode 71 is to ensure that the charge generated by the pyroelectric material can be efficiently and stably transmitted to the measurement circuit. At the same time, it also plays a role in protecting the pyroelectric material to prevent it from chemical corrosion or physical damage. The components of the upper electrode layer 7 can be the same as or different from those of the lower electrode layer 3. The metal of the outermost layer is preferably a metal with high density and good thermal conductivity, such as gold, platinum, molybdenum, tungsten, lead, silver, and copper, with a thickness of 50nm to 5um. The metal with high density can quickly stop the injected ion beam or atomic beam in the metal and effectively generate heat energy. Good thermal conductivity can quickly conduct heat to the surface of the pyroelectric material to enhance the detection sensitivity. The functional upper electrode 71 needs to form excellent electrical contact with the pyroelectric material to maximize the collection of charges. There is no electrical contact between the functional upper electrode 71 and the functional lower electrode 31, which effectively measures the voltage signal caused by the temperature difference from the pyroelectric material. The upper connecting wire 73, the functional upper electrode 71, and the pin upper electrode 72 are formed by metal bonding process or welding.
[0059] The functional upper electrode 71 is formed by an overlay process, in which a 300 nm thick metal film is deposited in a high vacuum electron beam evaporation device and then peeled off in acetone to form an upper electrode layer 7 , while the functional upper electrode 71 covers the pyroelectric material film layer 6 .
[0060] S5, forming a photoresist pattern layer on the surface of the back insulating dielectric film layer 5, the photoresist pattern layer having pattern grooves corresponding to the pyroelectric material film layer 6 one by one;
[0061] S6, using the photoresist pattern layer as a mask, a deep silicon etching device is used to etch the back insulating dielectric film layer 5 and the silicon wafer 1 from the back side using a dry etching process to form an open groove 10 corresponding to the pyroelectric material film layer 6. The depth of the photoetching makes the bottom of the open groove 10 flush with the back side of the front insulating dielectric film layer 2; at this time, the pyroelectric material film layer 6 is completely suspended on the back insulating dielectric film layer 5. This step can ensure that ions or heat can directly act on the pyroelectric material, thereby improving the response speed and sensitivity of the probe.
[0062] S7, removing the photoresist pattern layer and the back insulating dielectric film layer 5, wherein the back insulating dielectric film layer 5 can be removed by etching or mechanical methods, for example, by polishing the back insulating dielectric film layer 5. The photoresist pattern layer can be directly removed by a photoresist stripping process.
[0063] S8, fix the glass sheet 11 on the back of the silicon sheet 1 in a vacuum environment. In step S8, the glass sheet 11 is fixed by ultraviolet light assisted bonding, anodic bonding, or interlayer bonding technology. When the glass sheet 11 is fixed, the open groove 10 forms a closed vacuum chamber, which reduces heat conduction, increases the temperature difference between the two sides of the pyroelectric material, and increases the detection sensitivity.
[0064] In addition, an embodiment of the present invention also discloses a detection method for simultaneously detecting ion implantation dose and temperature. The detection method uses a detection device, and the detection device includes a conversion circuit board 12 and the detection probe. The detection probe is bonded to the conversion circuit board 12 to form a wafer tray. The conversion circuit board 12 is provided with an external plug 8 connected to the controller 9; the conversion circuit board 12 is provided with lead electrodes 13 corresponding to the pin upper electrode 72 and the pin lower electrode 32 one by one, and each lead electrode 13 is conductively connected to the corresponding pin upper electrode 72 and the pin lower electrode 32; the specific method of conductive connection between each lead electrode 13 and the corresponding pin upper electrode 72 and the pin lower electrode 32 is welding, wire bonding or conductive adhesive bonding. A placement area 4 for convenient wafer placement is provided on the wafer tray, and each probe monomer together constitutes a detection area, and at least a part of the probe monomers in the detection area are outside the placement area 4;
[0065] The detection method first places the detection device on the ion implanter for calibration, and obtains the standard correspondence between the voltage, temperature and implantation dose between the functional upper electrode 71 and the functional lower electrode 31; then the detection device is placed in the vacuum implantation chamber of the ion implanter and the external connector 8 is connected to the controller 9, the wafer is placed in the placement area 4 and fixed, and then the ion implanter is started, and the ion beam is injected into the wafer according to the set scanning route. The scanning area of the ion beam is greater than or equal to the detection area, so that the ions are injected into the wafer and also injected into the functional upper electrode 71. The voltage between the functional upper electrode 71 and the functional lower electrode 31 is detected in real time, and the dose and temperature of the current ion implantation are calculated according to the standard correspondence.
[0066] Preferably, the detection method also includes a self-calibration method, and the self-calibration method is started after the detection device has been used for a period of time; during calibration, the wafer is not placed and ion injection is directly started, at which time the scanning area of the ion beam will cover all the functional upper electrodes 71, and the voltage between all the functional upper electrodes 71 and the corresponding functional lower electrodes 31 is detected; the voltage difference between the probe monomer in the placement area 4 and the probe monomer outside the placement area 4 is compared and the error compensation coefficient is calculated, and the correspondence between the voltage, temperature and injection dose is updated by the error compensation coefficient to form an updated compensation correspondence, and then the compensation correspondence is used to calculate the current ion injection dose and temperature during ion injection. The self-calibration method can perform self-calibration on the detection device after being used for a period of time, and all the functional upper electrodes 71 originally covered by the wafer will be injected with ions during self-calibration, so the detection results between the probe monomer in the placement area 4 and the probe monomer outside the placement area 4 can be calculated to calculate the error compensation coefficient, thereby realizing self-calibration. After the self-calibration method is used, the service life of the detection device can be further extended, and the accuracy of long-term detection can be guaranteed.
[0067] The above-described embodiments are merely descriptions of preferred implementations of the present invention and are not intended to limit the scope of the present invention. Various modifications and alterations to the technical solutions of the present invention without departing from the spirit of the present invention should fall within the scope of protection defined by the claims of the present invention.
Claims
1. A method for manufacturing a detection probe for simultaneous detection of ion implantation dose and temperature, characterized in that: The following steps are involved: S1, growing a front insulating dielectric thin film layer and a back insulating dielectric thin film layer on the front and back of the silicon wafer respectively; S2. A patterned lower electrode layer is fabricated on the front insulating dielectric film layer, wherein the lower electrode layer includes an equal number of functional lower electrodes and pin lower electrodes arranged in pairs, wherein the functional lower electrodes are discretely distributed in the middle of the silicon wafer, and the pin lower electrodes are located outside the functional lower electrodes, and a lower connecting wire is connected between each functional lower electrode and the pin lower electrode; S3, depositing a pyroelectric material thin film layer on the functional lower electrode; S4, growing an upper electrode layer on the front insulating dielectric film layer and the pyroelectric material film layer; The upper electrode layer includes an equal number of functional upper electrodes and pin upper electrodes arranged in pairs, the functional upper electrodes are located on the upper surface of the pyroelectric material film layer, the pin upper electrodes are located on the upper surface of the front insulating dielectric film layer and are discretely distributed, an upper connecting wire is connected between each pin upper electrode and the corresponding functional upper electrode; the upper connecting wire and the lower connecting wire are independent of each other and do not contact each other; the pin upper electrode and the pin lower electrode are independent of each other and do not contact each other, and the mutually superimposed functional upper electrode, the pyroelectric material film layer and the functional lower electrode constitute a probe monomer; S5, forming a photoresist pattern layer on the surface of the back insulating dielectric film layer, wherein the photoresist pattern layer has pattern grooves corresponding to the pyroelectric material film layer one by one; S6, using the photoresist pattern layer as a mask, etching the back insulating dielectric film layer and the silicon wafer from the back side to form open grooves corresponding to the pyroelectric material film layer one by one, and the bottom of the open grooves is flush with the back side of the front insulating dielectric film layer; S7, removing the photoresist pattern layer and the back insulating dielectric film layer; S8. Fix a glass sheet on the back of the silicon wafer in a vacuum environment.
2. The method for manufacturing a detection probe for simultaneous detection of ion implantation dose and temperature as claimed in claim 1, characterized in that: The silicon wafer is a single crystal silicon wafer, and the front insulating dielectric film layer and the back insulating dielectric film layer are silicon nitride layers or silicon dioxide layers or a composite layer of silicon nitride layers and silicon dioxide layers stacked together.
3. The method for manufacturing a detection probe for simultaneous detection of ion implantation dose and temperature as claimed in claim 2, characterized in that: The lower electrode layer is any one of gold, platinum, silver, copper, tungsten and molybdenum or an alloy of several of them, and the thickness of the lower electrode layer is 50nm-5um.
4. The method for manufacturing a detection probe for simultaneous detection of ion implantation dose and temperature as claimed in claim 3, characterized in that: The pyroelectric material in the pyroelectric material film layer is one of triethylene glycol sulfate and its derivatives, adamantane formate, polyvinylidene fluoride, lithium tantalate, lithium niobate, zinc oxide, aluminum nitride, lead zirconate titanate (PZT), barium strontium titanate, lead tantalate scandate, and lead magnesium niobate titanate.
5. The method for manufacturing a detection probe for simultaneous detection of ion implantation dose and temperature as claimed in claim 4, characterized in that: The thickness of the pyroelectric material film layer is 50nm-5um.
6. The method for manufacturing a detection probe for simultaneous detection of ion implantation dose and temperature as claimed in claim 5, characterized in that: In step S7, polishing equipment is used to grind and remove the insulating dielectric film layer on the back side.
7. The method for manufacturing a detection probe for simultaneous detection of ion implantation dose and temperature as claimed in claim 6, characterized in that: In the step S8, the glass sheet is fixed by ultraviolet light assisted bonding, anodic bonding or intermediate layer bonding technology.
8. A method for simultaneously detecting ion implantation dose and temperature, characterized in that: The detection method uses a detection device, which includes a conversion circuit board and the detection probe as claimed in claim 1, the detection probe is bonded to the conversion circuit board to form a wafer tray, the conversion circuit board is provided with an external plug connected to the controller; the conversion circuit board is provided with lead electrodes corresponding to the pin upper electrodes and the pin lower electrodes one by one, and each lead electrode is conductively connected to the corresponding pin upper electrode and pin lower electrode; A placement area is provided on the wafer tray for convenient wafer placement, and each probe unit together forms a detection area, wherein at least a part of the probe units in the detection area are outside the placement area; The detection method first places the detection device on the ion implanter for calibration, and obtains the standard corresponding relationship between the voltage, temperature and implantation dose between the functional upper electrode and the functional lower electrode; Then the detection device is placed in the vacuum injection chamber of the ion implanter and the external plug is connected to the controller. After the wafer is placed in the placement area and fixed, the ion implanter is started, and the ion beam is injected into the wafer according to the set scanning route. The scanning area of the ion beam is greater than or equal to the detection area, so that the ions are injected into the wafer and also injected into the functional upper electrode. The voltage between the functional upper electrode and the functional lower electrode is detected in real time, and the dose and temperature of the current ion implantation are calculated according to the standard corresponding relationship.
9. A method for simultaneously detecting ion implantation dose and temperature as claimed in claim 8, characterized in that: The detection method also includes a self-calibration method. The self-calibration method is started after the detection device has been used for a period of time. During calibration, the wafer is not placed and ion injection is directly started. At this time, the scanning area of the ion beam will cover all functional upper electrodes, and the voltage between all functional upper electrodes and corresponding functional lower electrodes will be detected. The voltage difference between the probe monomer in the placement area and the probe monomer outside the placement area is compared and an error compensation coefficient is calculated. The corresponding relationship between the voltage, temperature and injection dose is updated through the error compensation coefficient to form an updated compensation corresponding relationship. When ion injection is performed later, the compensation corresponding relationship is used to calculate the current ion injection dose and temperature.
10. A method for simultaneously detecting ion implantation dose and temperature as claimed in claim 9, characterized in that: The specific method of conductive connection between each lead electrode and the corresponding pin upper electrode and pin lower electrode is welding, wire bonding or conductive adhesive bonding.