Preparation method of deep sea soft clay simulation sample for geotechnical test

Through physical and mechanical properties testing of deep-sea soft clay and orthogonal testing methods, the raw material content was calculated and simulated samples with an error of no more than 30% were prepared, which solved the problem of difficulty in obtaining deep-sea soft clay samples and achieved efficient and economical results. Simulate sample preparation to support marine deepwater engineering research.

CN118310836BActive Publication Date: 2024-10-15INST OF ROCK & SOIL MECHANICS CHINESE ACAD OF SCI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410478640.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-04-19
Publication Date
2024-10-15
Estimated Expiration
2044-04-19

AI Technical Summary

Technical Problem

In-situ testing and sampling of deep-sea soft clay are difficult. Existing devices cannot maintain fidelity and pressure, resulting in irrecoverable structures during sample removal, which limits the construction of deep-sea marine projects and geotechnical engineering research.

Method used

A method for preparing deep-sea soft clay simulated samples for geotechnical testing is adopted. By obtaining original deep-sea soft clay samples for physical and mechanical properties tests, evaluation indicators and raw materials are selected, and kaolin is used as the basic skeleton. Orthogonal experiments and information entropy methods are used to calculate the raw materials. The mixing amount ensures that the physical and mechanical index error between the simulated soil sample and the original sample does not exceed 30%.

Benefits of technology

It is possible to prepare deep-sea soft clay simulation samples with high similarity in physical and mechanical properties at low cost and easy operation, overcoming the problem that real deep-sea soft clay samples are rare and difficult to obtain, and meeting the needs of geotechnical testing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FDA0005000129600000011
    Figure FDA0005000129600000011
  • Figure FDA0005000129600000021
    Figure FDA0005000129600000021
  • Figure FDA0005000129600000022
    Figure FDA0005000129600000022
Patent Text Reader

Abstract

The present invention belongs to the field of geotechnical testing of marine geotechnical engineering, and relates to a method for preparing a simulated soil sample of deep-sea soft clay for geotechnical testing, including: 1) obtaining the original sample of real deep-sea soft clay in the intended research sea area, and conducting a physical and mechanical property test on the original sample; 2) selecting the number of physical and mechanical indicators to be evaluated and the type of raw materials in the simulated sample; 3) taking kaolin as the basic skeleton of the simulated soil sample, first determining the admixture ratio of other raw materials except kaolin; 4) then calculating the admixture of kaolin; 5) preparing the simulated soil sample, and carrying out a test of determining the selected physical and mechanical indicators; 6) evaluating the difference in each physical and mechanical indicator between the simulated soil sample and the original sample, so that the error does not exceed 30%. The present invention provides a method for preparing a simulated soil sample of deep-sea soft clay for geotechnical testing, which has easy raw material acquisition, low cost, simple operation, and high similarity in physical and mechanical properties.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of geotechnical testing of marine geotechnical engineering, and relates to a method for preparing deep-sea soil, and in particular to a method for preparing a deep-sea soft clay simulation sample for geotechnical testing. Background Art

[0002] Deep-sea soft clay generally refers to sediments deposited at the bottom of a deep and vast ocean with a water depth of more than 2000m, mainly including products of biological and chemical actions and terrigenous, volcanic, marine authigenic minerals and cosmic dust. Deep-sea soft clay usually has the characteristics of high water content, high porosity, high liquid limit, high compressibility, low shear strength, and high organic matter content. In deep-sea sediments, clay, calcareous organisms, and siliceous organisms are the three basic independent parameters for the classification and naming of deep-sea sediments. Deep-sea sediments can be roughly divided into four categories (deep-sea clay, siliceous mud, calcareous mud, clay-siliceous-calcium mixed mud), which can be further subdivided into 16 types, such as siliceous clay, calcareous mud, clay-siliceous-calcium mixed mud, etc.

[0003] The in-situ testing and sampling of deep-sea soil is very difficult to implement. It requires the help of special ships and equipment, which is expensive and has complicated operating procedures. At the same time, the existing sediment sampling devices generally cannot maintain fidelity and pressure, which inevitably causes irreversible damage and destruction to the original structure of the sediment soil samples during the process of taking the samples out of the deep sea, thus losing the meaning of obtaining undisturbed soil samples in geotechnical engineering research. Because of this, the current understanding of the engineering mechanical properties of deep-sea soil is not clear enough, which restricts the development of deep-water marine engineering construction. However, when conducting geotechnical engineering geotechnical test studies on the interaction between deep-sea foundation soil and structures indoors, a large amount of deep-sea soil samples are required, and it is often difficult to obtain enough deep-sea samples due to limited conditions. Therefore, it is necessary to propose a method for preparing deep-sea soft clay simulation samples for geotechnical tests. Summary of the invention

[0004] In order to solve the above technical problems existing in the background technology, the present invention provides a method for preparing a deep-sea soft clay simulation sample for geotechnical testing, which has easy-to-obtain raw materials, low cost, simple operation and high similarity in physical and mechanical properties.

[0005] In order to achieve the above object, the present invention adopts the following technical solution:

[0006] A method for preparing a simulated deep-sea soft clay sample for geotechnical testing, characterized in that the method comprises the following steps:

[0007] 1) Obtain the original samples of deep-sea soft clay in the proposed study area, conduct physical and mechanical property tests on the original samples, obtain the test results, and classify the deep-sea soil based on the test results;

[0008] 2) According to the physical and mechanical test results obtained in step 1), the physical and mechanical indicators to be evaluated and the types of raw materials for the simulated soil samples are selected;

[0009] 3) Taking kaolin as the basic framework of the simulated soil sample, first determine the dosage ratio of other raw materials except kaolin;

[0010] 4) Calculate the dosage of kaolin;

[0011] 5) preparing a simulated soil sample based on the results of step 3) and step 4), and conducting a test on the physical and mechanical indicators selected in step 2);

[0012] 6) Evaluate the differences between the physical and mechanical indicators of the simulated soil samples and the original samples, so that the errors do not exceed 30%.

[0013] Preferably, the physical and mechanical evaluation indicators in step 2) adopted in the present invention include: moisture content, porosity, liquid limit, compression modulus, undrained shear strength, etc.; the number of the physical and mechanical evaluation indicators to be evaluated is K, and K≥3; the types of raw materials of the simulated soil samples are kaolin, bentonite, diatomaceous earth, calcium carbonate, salt and other raw materials that are easily obtained from the market.

[0014] Preferably, the specific implementation method of step 3) adopted by the present invention is:

[0015] 3.1) According to the mineral composition of the original deep-sea soft clay sample and the type of raw materials of the simulated soil sample, L n (a b )Orthogonal test;

[0016] 3.2) Obtaining orthogonal test results and obtaining orthogonal test samples;

[0017] 3.3) Normalize the orthogonal test results;

[0018] 3.4) Calculating the information entropy of each physical and mechanical evaluation index according to the normalized result in step 3.3);

[0019] 3.5) determining the weight of each physical and mechanical evaluation index according to the information entropy of each physical and mechanical evaluation index in step 3.4);

[0020] 3.6) Taking the original sample as the percentage benchmark, for each physical and mechanical evaluation index, calculate the error between each sample in the orthogonal test and the original sample, and assign points based on linear interpolation to calculate the single score of each sample corresponding to the index in the orthogonal test;

[0021] 3.7) Using the weighted method, the single score q of each sample corresponding to the index in the orthogonal test is ij and the weights W of each physical and mechanical evaluation indexj Multiply them together to calculate the comprehensive score S of each sample in the orthogonal test. i ;

[0022]

[0023] 3.8) The comprehensive score S of each sample in the orthogonal test calculated in step 3.7) i Conduct range analysis to obtain the impact of each variable on the comprehensive score;

[0024] 3.9) According to the influence of step 3.8), the dosage ratio of each raw material except kaolin in the simulated soil sample is determined.

[0025] Preferably, the specific implementation method of step 3.3) adopted by the present invention is: the specific implementation method of the normalization process is: assuming that K physical and mechanical indicators K1, K2, ..., K to be evaluated are determined K , where K j = {X1, X2, ..., X n};X ij is the value of the i-th group of orthogonal tests in the j-th evaluation index; Y ij is the normalized value of the orthogonal test of the i-th group in the j-th evaluation index, where i=1, 2, ..., n; n is the number of evaluation scheme groups, then:

[0026]

[0027] Preferably, the method for obtaining the information entropy in step 3.4) adopted by the present invention is:

[0028]

[0029] in:

[0030]

[0031] If p ij =0, then define:

[0032]

[0033] Preferably, the weights of the physical and mechanical evaluation indicators in step 3.5) of the present invention are calculated as follows:

[0034]

[0035] Among them, j = 1, 2, ..., k.

[0036] Preferably, the specific implementation method of step 3.6) adopted by the present invention is:

[0037] 3.6.1) Define the value of the jth evaluation index of the original sample as X Tj ;

[0038] 3.6.2) Combined with step 3.6.1), calculate the error between each sample and the original sample in the orthogonal test:

[0039] e ij =|X ij -X Tj |

[0040] in:

[0041] e ij is the error value between the actual value of the corresponding index of each sample and the original sample in the i-th group of orthogonal test in the j-th evaluation index;

[0042] 3.6.3) Calculate the single score q of each simulated sample corresponding to the index according to the results of step 3.6.2) ij ;

[0043]

[0044] Preferably, the dosage c of kaolin in step 4) used in the present invention is:

[0045] c 高岭土 =(1-c 膨润土 -c 硅藻土 -c 碳酸钙 )×100%.

[0046] Preferably, the specific implementation of step 5) adopted by the present invention is:

[0047] According to the physical and mechanical evaluation indicators selected in step 2), test the corresponding indicators of the simulated soil sample and obtain the test results;

[0048] Preferably, the specific implementation method of the evaluation of step 6) adopted by the present invention is:

[0049] 6.1) Compare and evaluate the test results obtained in step 5) with the corresponding indicators of the original sample. If the error of the physical and mechanical indicators of the simulated soil sample compared with the corresponding indicators of the original sample does not exceed 30%, that is: Wherein, j = 1, 2...k; the prepared simulated soil sample is qualified; if the error of one indicator of the simulated soil sample compared with the original sample is greater than 30%, step 6.2) should be performed.

[0050] 6.2) For each group of test results X corresponding to the jth index whose error exceeds 30%, ij(i=1,2…n) perform range analysis and obtain the range R. At the same time, draw a chart based on the test results to show how the different levels of the same factor affect the change in the value of the index, and use the chart to determine the trend of the influence of the level change of the factor on the index. Use the range analysis results to determine the factors that need to be adjusted, and use the trend reflected in the chart to adjust the level settings in step 3.1). After adjustment, return to step 3) to step 6). If the error does not exceed 30% after 3 cycles, the prepared simulated soil sample is unqualified. The types of raw materials in the simulated soil sample should be reconsidered.

[0051] A simulated soil sample of deep sea soft clay for geotechnical testing is prepared based on the preparation method of the simulated sample of deep sea soft clay for geotechnical testing as mentioned above.

[0052] The advantages of the present invention are:

[0053] The present invention provides a method for preparing a simulated sample of deep-sea soft clay for geotechnical tests, comprising: 1) obtaining an original sample of deep-sea soft clay in a proposed sea area, conducting a physical and mechanical property test on the original sample, obtaining the test results, and classifying the deep-sea soil based on the test results; 2) selecting the physical and mechanical indexes to be evaluated and the raw material types of the simulated soil sample according to the physical and mechanical test results obtained in step 1); 3) using kaolin as the basic skeleton of the simulated soil sample, first determining the admixture ratio of other raw materials except kaolin; 4) then calculating the admixture of kaolin; 5) preparing a simulated soil sample in combination with the results of step 3) and step 4), and conducting a test of measuring the physical and mechanical indexes selected in step 2); 6) evaluating the difference between the physical and mechanical indexes of the simulated soil sample and the original sample, so that the error does not exceed 30%. The simulated sample prepared by the method for preparing the simulated sample of deep-sea soft clay for geotechnical tests provided by the present invention has a high similarity in physical and mechanical properties, is easy to implement, and can be prepared in large quantities. According to the selected physical and mechanical indicators of deep-sea soft clay, this method introduces information entropy and sets a scientific scoring method to obtain the dosage ratio of each raw material of the simulated soil sample. Based on the orthogonal test, the optimal ratio scheme is obtained with the least test amount, ensuring that the physical and mechanical indicators of the simulated soil sample under the optimal ratio are more than 70% similar to the corresponding indicators of the original soil. Deep-sea soft clay simulated soil samples that meet the requirements of geotechnical tests can be prepared with easily available raw materials. The method is simple and easy to implement, which overcomes the problem that real samples of deep-sea soft clay are rare and difficult to obtain in the current deep-sea environment. Only based on the test data of a small number of real samples of deep-sea soft clay, a large number of simulated soil samples can be artificially prepared according to this method, which meets the needs of geotechnical tests, especially geotechnical model tests, which require a large number of soil samples. DETAILED DESCRIPTION

[0054] The present invention provides a method for preparing a deep-sea soft clay simulation sample for geotechnical testing, the method comprising the following steps:

[0055] The first step is to obtain a small amount of deep-sea soft clay samples from the proposed research area, conduct basic physical and mechanical tests on the original samples, and obtain their basic physical and mechanical indicators. At the same time, test their mineral composition, determine the composition and content of clay minerals in the soil samples, as well as the content of siliceous organisms (biological SiO2) and calcareous organisms (CaCO3); and classify them according to the deep-sea sediment equal triangle diagram classification method.

[0056] The second step is to determine the evaluation indicators of the simulated samples. According to the characteristics of deep-sea sediments such as high water content, high porosity, high liquid limit, high compressibility, low shear strength, and high organic matter content, K (K ≥ 3) physical and mechanical indicators such as water content, porosity, liquid limit, compression modulus, and undrained shear strength are selected as evaluation indicators for the preparation of deep-sea soft clay simulation samples according to actual needs.

[0057] The third step is to determine the types of raw materials for preparing simulated samples. Kaolin is used as the basic skeleton for preparing samples. Then, based on the classification of deep-sea sediments, combined with their physical and mechanical properties, clay mineral composition, and the content of siliceous and calcareous organisms, easily accessible mineral materials such as bentonite, diatomaceous earth (siliceous) and calcium carbonate (calcium) are selected as other auxiliary raw materials for simulating the preparation of deep-sea soft clay, while considering the influence of deep-sea salinity.

[0058] The fourth step is to determine the specific proportions of other raw materials in the simulated sample except kaolin through experiments. First, the orthogonal test method is used to arrange and combine the experimental factors. Since kaolin is used as the basic framework, the number of types of raw materials other than kaolin plus salt is taken as a factor; according to the content of montmorillonite, the content of siliceous organisms, the content of calcareous organisms and the salinity of seawater in the deep-sea soft clay obtained, the dosage of each raw material and the concentration of the salt solution are set to b levels close to them, and the standard orthogonal table closest to the expected number of factors and levels is selected to design L n (a b ) orthogonal test, where n is the number of experimental groups to be conducted. Subsequently, according to the K physical and mechanical evaluation indicators selected in the second step, the corresponding experiments are conducted on the n groups of simulated soil samples and the experimental results are obtained. The entropy weight method is then used to calculate the weight of each evaluation indicator based on the experimental results. The calculation steps are as follows:

[0059] (1) Data normalization. Normalize the orthogonal test results. Suppose K physical and mechanical evaluation indicators K1, K2, ..., K are determined. K , where K j = {X1, X2, ..., X n}. X ij Y is the value of the i-th group of experimental results in the j-th evaluation index; ijis the normalized value of the experimental results of the i-th group in the j-th evaluation index (i = 1, 2, ..., n); n is the number of evaluation scheme groups, then

[0060]

[0061] (2) Calculate the information entropy of each indicator. The information entropy of a set of data is:

[0062]

[0063] in:

[0064]

[0065] If p ij =0, then define:

[0066]

[0067] (3) Determine the weight of each physical and mechanical evaluation index. According to the information entropy calculation formula, the information entropy of each evaluation index is calculated as E1, E2, ..., E k . The weight of each indicator is calculated by information entropy:

[0068]

[0069] After calculating the weight of each physical and mechanical evaluation index, taking the corresponding index of the original deep-sea soft clay sample as 100 as the full score, the error between each group of test data and the corresponding index of the obtained original deep-sea soft clay sample was calculated, and the points were assigned according to linear interpolation to calculate the individual scores of the corresponding indicators of each group of soil samples.

[0070] Define the value of the jth evaluation index of the deep-sea soft clay sample as X Tj ,but:

[0071] e ij =|X ij -X Tj | (6)

[0072] Among them, e ij is the error value between the experimental results of the i-th group in the j-th evaluation index and the actual value of the corresponding index of deep-sea soft clay.

[0073] Then the single score q ij for:

[0074]

[0075] Then, the single score q of each group of soil samples corresponding to the index is calculated by weighting method. ij and the weight W of each evaluation index j Multiply them together to calculate the comprehensive score S of each groupi .

[0076]

[0077] Finally, a range analysis is performed on the comprehensive score to obtain the impact of each variable on the comprehensive score.

[0078] The steps of range analysis are:

[0079] Calculate the average K of the comprehensive scores of each group for each factor and each level xy avg(x=1,2,…,a), (y=1,2,…,b).

[0080] Calculate the range R for each factor.

[0081] R x =max{K 1x avg,…,X bx avg}-min{K 1x avg,…,K bx avg}(x=1,2,…,a) (9)

[0082] max{K 1x avg,…,X bx avg} is the optimal level of the x factor. The range R reflects the influence of different factors on the physical and mechanical properties of soil, that is, the larger the R, the greater the influence of the factor on the physical and mechanical properties of soil.

[0083] max{K 1x avg,…,X bx avg} is the preferred dosage (or concentration) of the raw material.

[0084] The fifth step is to calculate the amount of kaolin used as the basic skeleton of the simulated soil sample. 高岭土 for:

[0085] c 高岭土 =(1-c 膨润土 -c 硅藻土 -c 碳酸钙 )×100% (10)

[0086] The sixth step is to determine whether the simulated deep-sea soft clay sample under the preferred ratio is qualified. According to the preferred dosage (or concentration) of each raw material obtained, a simulated soil sample is prepared, and according to the K physical and mechanical evaluation indicators selected in the second step, the simulated soil sample is tested for the corresponding indicators, and the test results are obtained. The test results are compared with the corresponding indicators of the original deep-sea soft clay soil. If the errors of the K physical and mechanical indicators of the simulated soil sample compared with the corresponding indicators of the original deep-sea soft clay sample do not exceed 30%, that is:

[0087]

[0088] The preferred ratio is the ratio of deep-sea soft clay simulation samples that meets the qualification requirements.

[0089] If there are indicators that cannot satisfy formula (11), then the test results X corresponding to the jth indicator with an error exceeding 30% are ij (i=1,2…n) perform range analysis and obtain range R. The size of range R can reflect the influence of different factors on the index, that is, the larger R is, the greater the influence of the factor on the index. At the same time, draw a chart based on the test results to show the influence of different levels of the same factor on the index value change, and use the chart to judge the influence trend of the level change of the factor on the index. Use the range analysis results to determine the factors that need to be adjusted, and use the trend reflected in the chart to adjust the level setting. After adjustment, repeat the fourth to sixth steps. If the formula (11) is still not satisfied after more than 3 cycles, the simulated soil sample is judged to be unqualified and the test ends. The types of raw materials in the simulated soil sample should be reconsidered.

[0090] The technical solution provided by the present invention is described in detail below in conjunction with specific embodiments:

[0091] This example prepares simulated samples of deep-sea soft clay in a certain sea area (water depth 2000m).

[0092] The first step was to obtain deep-sea soft clay samples from the sea area and conduct a series of physical and mechanical tests indoors. The natural water content was measured to be 103.5%, and the natural density was 1.36 g / cm 3 , particle size distribution is shown in Table 1, specific gravity is 2.77, liquid limit is 92.3%, plastic limit is 38.6%, plasticity index I P The specific surface area is 53.7 and 27.08m 2 / g, the porosity is 3.14, the organic matter content is 8.6%, the compression modulus is 1.37MPa, and the undrained shear strength is 8.7kPa.

[0093] Table 1 Particle size distribution of deep-sea sediments

[0094]

[0095] The clay mineral composition and content of the deep-sea soft clay original soil are shown in Table 2.

[0096] Table 2 Clay mineral composition and content of deep-sea soft clay original soil

[0097]

[0098] The elemental analysis (XRF) test was conducted on the original deep-sea soft clay to test the mineral elements and oxide content. The deep-sea soft clay tested basically does not contain calcium carbonate, but the SiO2 content is 57.49%, and the Al2O3 content is 17.80%. The biological SiO2 content can be calculated as follows:

[0099] C(SiO2) bi o=C(SiO2)-3C(Al2O3)

[0100] In the formula, C is the percentage of oxide; bio represents biomass; 3C(Al2O3) represents the estimated value of non-biological SiO2; according to the above formula, the biological SiO2 content is 4.12%.

[0101] After normalizing the clay content and the CaCO3 and SiO2 contents, the clay content of the deep-sea soft clay in this sea area was 91.31%, and the siliceous biological content was 8.69%.

[0102] According to the isotriangular diagram classification method of deep-sea sediments, this sample belongs to the deep-sea clay class and can be named Ⅰ1 deep-sea clay (clay 50%-100%, calcareous organisms 0%-25%, siliceous organisms 0%-25%).

[0103] In the second step, five indicators, including liquid limit, specific surface area, porosity, compression modulus, and undrained shear strength, were selected as physical and mechanical evaluation indicators.

[0104] In the third step, combined with the high water content, high porosity, high liquid limit, high compressibility, low shear strength, high organic matter content and almost no calcium organisms of the original deep-sea soft clay, bentonite, diatomite and kaolin were selected as raw materials for simulating the preparation of deep-sea soft clay. In addition, the main soluble salt in the seawater in this sea area is sodium chloride, so sodium chloride solution was used to prepare the sample, ignoring the influence of other soluble salts.

[0105] In the fourth step, the content of bentonite, salt solution concentration, and diatomite content were used as three major factors, and the content of montmorillonite, the content of siliceous organisms, and the salinity of seawater in the deep-sea soft clay sample were referred to set four levels to design L 16 (4 3 )Orthogonal test (Table 3, Table 4).

[0106] Table 3 Simulated soil sample L 16 (4 3 )Orthogonal test factor level table

[0107]

[0108] Table 4 Simulated soil sample L 16 (4 3 )Orthogonal test table

[0109]

[0110]

[0111] The minerals used are first dried, crushed and powdered, and then sieved to obtain minerals of different particle sizes. Finally, the variable control method is used and the mixture is mixed with kaolin according to the proportion in Table 4 to obtain soil powder. After adding a certain amount of distilled water or salt solution of different concentrations to the mixed soil powder and mixing and stirring evenly to form mud, the mixture is sealed and left to stand for 24 hours, and then quickly poured into the consolidation barrel to prevent bubbles from being mixed in during the pouring process. The loads of 2.5kPa, 9.5kPa, 25kPa, and 40kPa are used for step-by-step loading and consolidation. After the consolidation is completed, the required size and shape of the test are cut out with a soil cutter and ring cutters of different sizes.

[0112] Then, according to the five physical and mechanical evaluation indicators of liquid limit, specific surface area, porosity, compression modulus and undrained shear strength selected in the second step, the liquid limit, specific surface area, porosity, compression modulus and undrained shear strength of each group of simulated soil samples were measured respectively. The test results are shown in Table 5.

[0113] Table 5 Different physical and mechanical indicators L of simulated soil samples 16 (4 3 )Orthogonal test results X ij Statistics

[0114]

[0115] The test results are processed using the entropy weight method. First, the orthogonal test results X in Table 5 are ij Normalization was performed according to formula (1) (Table 6).

[0116] Table 6 Different physical and mechanical indicators L of simulated soil samples 16 (4 3 ) Orthogonal test normalization result Y ij Statistics

[0117]

[0118] Then, the information entropy E of each indicator is calculated according to formulas (2), (3), and (4). j , calculate the weight W according to formula (5) j (Table 7).

[0119] Table 7 Information entropy and weight statistics of each index of simulated soil samples

[0120]

[0121] Taking the properties of the original deep-sea soft clay sample (Table 8) as the full score of 100, the error between each group of test data and the corresponding index of deep-sea soft clay obtained was calculated by formula (6) (Table 9), and then the single score q of the physical and mechanical evaluation index corresponding to each group of simulated soil samples was calculated according to formula (7): ij (Table 10).

[0122] Table 8 Physical and mechanical indexes of deep-sea soft clay original soil X Tj Statistics

[0123]

[0124] Table 9 Different physical and mechanical properties of simulated soil samples L 16 (4 3 )Orthogonal test error e ij Statistics

[0125]

[0126] Finally, according to formula (8), the single item score q ij and the weight W of each evaluation index j Multiply them together to get the comprehensive score S of each group i (Table 10).

[0127] Table 10 Comprehensive scoring table of simulated soil sample ratios for each group

[0128]

[0129]

[0130] (Note: Comprehensive score S i =a×8.95%+b×12.93%+c×22.24%+d×40.92%+e×14.96%)

[0131] Then perform a range analysis on the comprehensive scores in Table 10, and first calculate the average K of the comprehensive scores of each factor and each level. xy avg (Table 11), and then use formula (9) to calculate the range R of each factor, and finally get the impact of each parameter on the comprehensive score (Table 12).

[0132] Table 11 Average K of comprehensive scores of each group for each factor and each level of simulated soil samples xy avg

[0133]

[0134] Table 12 Range analysis of comprehensive scores of simulated soil samples

[0135]

[0136] According to the range in Table 12, the order of the factors affecting the comprehensive score is as follows: R (salinity) > R (diatomite) > R (bentonite). This shows that salinity has the greatest impact on the comprehensive score of the simulated soil sample, diatomite has a smaller impact on the comprehensive score of the simulated soil sample than salinity, and bentonite has the least impact on the comprehensive score of the simulated soil sample. Since the K2 value in salinity is the largest, the salinity takes the second level, that is, the salt solution concentration in the simulated soil sample is 3.5%; the K1 value in the diatomite content is the largest, so the diatomite content takes the first level, that is, the diatomite content in the simulated soil sample is 7%; the K2 value in the bentonite content is the largest, so the bentonite content takes the second level, that is, the bentonite content in the simulated soil sample is 20%.

[0137] The fifth step is to calculate the kaolin content. According to formula (10), the kaolin content is 73%.

[0138] The sixth step is to determine whether the deep-sea soft clay simulation sample under the optimal ratio meets the requirements of geotechnical tests (Table 13).

[0139] Table 13 Comparison of physical and mechanical indicators of original deep-sea soft clay and simulated soil samples with optimal proportions

[0140]

[0141] After calculation, the error of the five physical and mechanical indicators of liquid limit, specific surface area, porosity, compression modulus and undrained shear strength of the simulated soil sample of the optimal mix ratio compared with the original deep-sea soft clay sample indicators is no more than 30%. Therefore, this mix ratio is a deep-sea soft clay simulation sample ratio that meets the requirements.

[0142] In summary, the ratio of the simulated sample of deep-sea soft clay that meets the requirements for geotechnical tests is: 20% bentonite, 3.5% salt solution concentration, 7% diatomite, and 73% kaolin. The liquid limit, specific surface area, porosity, compression modulus, and undrained shear strength of the simulated deep-sea soft clay obtained by this ratio are close to those of the real soil sample, and can be used as a substitute for deep-sea soft clay in the geotechnical engineering test research of the interaction between deep-sea foundation soil and structures indoors.

Claims

1. A method for preparing a simulated sample of deep-sea soft clay for geotechnical testing, characterized in that: The preparation method of the deep-sea soft clay simulation sample for geotechnical testing comprises the following steps: 1) Obtain original samples of deep-sea soft clay in the proposed study area, conduct physical and mechanical property tests on the original samples and obtain corresponding test results; 2) According to the physical and mechanical test results obtained in step 1), determine the physical and mechanical evaluation indexes of the sample to be evaluated and the types of raw materials to be added to the simulated soil sample; 3) Taking kaolin as the basic framework, first determine the dosage ratio of other raw materials in the simulated soil sample except kaolin; 4) Calculate the dosage ratio of kaolin in the simulated soil sample; 5) preparing simulated samples in combination with the results of step 3) and step 4), and testing the simulated soil samples in combination with the physical and mechanical evaluation indicators selected in step 2); The specific implementation method of step 3) is: 3.1) According to the mineral composition of the original deep-sea soft clay sample and the type of raw materials of the simulated soil sample, L n (a b )Orthogonal test; 3.2) Obtaining orthogonal test results and obtaining orthogonal test samples; 3.3) Normalize the orthogonal test results; 3.4) Calculating the information entropy of each physical and mechanical evaluation index according to the normalized result in step 3.3); 3.5) determining the weight of each physical and mechanical evaluation index according to the information entropy of each physical and mechanical evaluation index in step 3.4); 3.6) Taking the original sample as the percentage benchmark, for each physical and mechanical evaluation index, calculate the error between each sample in the orthogonal test and the original sample, and assign points based on linear interpolation to calculate the single score of each sample corresponding to the index in the orthogonal test; 3.7) Using the weighted method, the single score q of each sample corresponding to the index in the orthogonal test is ij and the weights W of each physical and mechanical evaluation index j Multiply them together to calculate the comprehensive score S of each sample in the orthogonal test. i ; 3.8) The comprehensive score S of each sample in the orthogonal test calculated in step 3.7) i Conduct range analysis to obtain the impact of each variable on the comprehensive score; 3.9) determining the dosage ratio of each raw material except kaolin in the simulated soil sample according to the influence of step 3.8); The specific implementation of step 3.3) is: The specific implementation of the normalization process is: Assume that K physical and mechanical indicators K1, K2, ..., K to be evaluated are determined K , where K j = {X1, X2, ..., X n };X ij is the value of the i-th group of orthogonal tests in the j-th evaluation index; Y ij is the normalized value of the orthogonal test of the i-th group in the j-th evaluation index, where i=1, 2, ..., n; n is the number of evaluation scheme groups, then: The method for obtaining the information entropy in step 3.4) is: in: If p ij =0, then define: The weight of each physical and mechanical evaluation index in step 3.5) is calculated as follows: Wherein, j = 1, 2, ..., k; The specific implementation method of step 3.6) is: 3.6.1) Define the value of the jth evaluation index of the original sample as X Tj ; 3.6.2) Combined with step 3.6.1), calculate the error between the corresponding index of each sample in the orthogonal test and the original sample: e ij =|X ij -X j | in: e ij is the error value between the actual value of the corresponding index of each sample and the original sample in the i-th group of orthogonal test in the j-th evaluation index; 3.6.3) Calculate the single score q of each simulated sample corresponding to the index according to the results of step 3.6.2) ij ; 2. The method for preparing a simulated deep-sea soft clay sample for geotechnical testing according to claim 1 is characterized in that: the physical and mechanical evaluation indicators in the step 2) include but are not limited to water content, porosity, liquid limit, compression modulus and undrained shear strength; the number of the physical and mechanical evaluation indicators is K, and K≥3; the type of raw materials is a combination of one or more of kaolin, bentonite, diatomaceous earth and calcium carbonate.

3. The method for preparing a simulated deep-sea soft clay sample for geotechnical testing according to claim 2, characterized in that: the amount of kaolin added in step 4) is c 高岭土 for: c 高岭土 =(1-c 膨润土 -c 硅藻土 -c 碳酸钙 )×100%。 4. The method for preparing a simulated deep-sea soft clay sample for geotechnical testing according to any one of claims 1 to 3, characterized in that: The specific implementation method of the inspection in step 5) is: 5.1) According to the physical and mechanical evaluation indicators selected in step 2), test the corresponding indicators of the simulated soil sample and obtain the test results; 5.2) Compare and evaluate the test results obtained in step 5.1) with the corresponding indicators of the original sample. If the error of the physical and mechanical indicators of the simulated soil sample compared with the corresponding indicators of the original sample does not exceed 30%, that is: Wherein, j = 1, 2 ... k; the prepared simulated soil sample is qualified; if the error of one index of the simulated soil sample compared with the original sample is greater than 30%, proceed to step 5.3); 5.3) For each group of test results X corresponding to the jth index whose error exceeds 30%, ij (i=1, 2…n) perform range analysis and obtain the range R; draw a chart based on the test results to show how the different levels of the same factor affect the change in the value of the index, and use the chart to determine the trend of the impact of the level change of the factor on the index; use the range analysis results to determine the factors that need to be adjusted, and use the trend reflected in the chart to adjust the dosage ratio of other raw materials in the simulated soil sample except kaolin in step 3), and re-execute steps 3) to 5) based on the adjusted ratio. If the error is still not within 30% after three cycles, the prepared simulated soil sample is unqualified.

5. A simulated soil sample of deep-sea soft clay for geotechnical testing prepared based on the preparation method of a simulated sample of deep-sea soft clay for geotechnical testing as claimed in claim 4.