A uranium adsorbent, its preparation method and application

By encapsulating keggin-type heteropolyacids with a MIL-101(Cr) nanocage structure in uranium adsorbents, the problems of low adsorption capacity and poor selectivity in existing technologies are solved, achieving efficient and rapid uranium adsorption and desorption, which is suitable for the treatment of seawater and uranium-containing wastewater.

CN118341404BActive Publication Date: 2026-11-10INSTITUTE OF PROCESS ENGINEERING CHINESE ACADEMY OF SCIENCES
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410469977.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-04-18
Publication Date
2026-11-10
Estimated Expiration
2044-04-18

AI Technical Summary

Technical Problem

Existing uranium adsorbents have low adsorption capacity, poor selectivity, high regeneration costs, and slow desorption rates in seawater and uranium-containing wastewater, making it difficult to achieve multiple cycles of use.

Method used

Using the metal-organic framework MIL-101(Cr) as a matrix, keggin-type heteropolyacids are encapsulated in situ. By utilizing its nanocage structure and the specific coordination effect of keggin-type heteropolyacids, the selectivity and adsorption capacity of uranium adsorbents are improved, and instantaneous desorption is achieved under mild conditions.

Benefits of technology

It achieves uranium adsorption with high selectivity and high adsorption capacity, with an adsorption capacity of over 280.60 mg/g. It can desorb instantaneously under mild conditions, has a long cycle life, and is suitable for the treatment of uranium-containing wastewater and seawater.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118341404B_ABST
    Figure CN118341404B_ABST
Patent Text Reader

Abstract

The application provides a kind of uranium adsorbent and its preparation method and application, the uranium adsorbent includes metal organic framework, the metal organic framework has nanometer cage structure;The uranium adsorbent also includes keggin type heteropoly acid in situ encapsulated in the nanometer cage structure;The metal organic framework is MIL-101 (Cr);The uranium adsorbent has high selectivity to uranium, and uranium adsorption capacity can be up to 280.60 mg / g or more, long service life, after 8 times of adsorption and desorption cycle, still can keep 94.30% of initial cycle amount;The uranium adsorbent has excellent anti-interference ability, and still shows high selective adsorption to uranium in the presence of interfering ions, can also realize the instantaneous desorption of uranium under mild conditions, and its preparation process is simple, raw material source is extensive, can be widely used in uranium-containing wastewater treatment, uranium ore resource recovery and seawater uranium extraction and other fields.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of precious metal adsorption, separation and recovery technology, specifically relating to a uranium adsorbent, its preparation method and application. Background Technology

[0002] Nuclear energy, with its extremely high energy density and ultra-low carbon dioxide emissions, is widely recognized as an ideal energy source to meet ever-growing energy demands. Uranium, a crucial raw material in nuclear energy production, is an important naturally occurring radioactive element. On one hand, most uranium currently used is extracted from uranium mines. The mining and utilization of uranium typically generates large amounts of uranium-containing wastewater, which is radioactive, highly toxic to organisms, and poses a significant threat to human health, making it a vital uranium resource. On the other hand, seawater contains 4.5 billion tons of uranium, 100 times the reserves on land, representing enormous potential for the long-term development of the nuclear industry. Therefore, with the increasing global demand for uranium, there is an urgent need to extract uranium from seawater or uranium-containing wastewater to support nuclear energy production.

[0003] However, the extremely low concentrations of soluble uranium in seawater (~3 ppb) and uranium-containing wastewater (5-50 ppm), along with the presence of various competing metal ions, make selective uranium extraction extremely challenging. To date, various methods have been developed for extracting uranium from seawater and uranium-containing wastewater, including liquid-liquid extraction, ion exchange, electrochemical extraction, chemical precipitation, membrane separation, and adsorption. Among these, adsorption technology has been widely used due to its simple operation, low application limitations, high efficiency, and cost-effectiveness, and has achieved significant progress in uranium separation and recovery. Clearly, the adsorbent is the most critical factor in the adsorption process. The main challenges faced by adsorbents used for uranium extraction from seawater or uranium-containing wastewater include low adsorption capacity, high regeneration costs, low selectivity, poor recyclability, and slow adsorption and desorption kinetics.

[0004] CN113231048A discloses a uranium adsorbent, its preparation method, and its application. It uses an acyl chloride derivative bridging agent to organically link an oxime-modified polyacrylonitrile adsorbent with active sites to a high-strength jute fiber matrix. Simultaneously, the incompletely grafted functional groups of the bridging agent (such as trimesoyl chloride) can be further hydrolyzed to carboxyl groups, effectively increasing the hydrophilicity and adsorption capacity of the uranium adsorbent. However, its adsorption capacity remains very low, with a maximum adsorption capacity of only 171.26 mg / g. The preparation process is very complex and costly, and the desorption environment and desorption time are not studied.

[0005] CN108854976A discloses an adsorbent for uranium in uranium-containing wastewater and a method for adsorbing uranium into the wastewater. This uranium adsorbent utilizes cyclic aromatic hydrocarbons to modify magnetic graphene oxide, achieving selective uranium adsorption. However, it is susceptible to interference ions (such as Cr). 3+The adsorption rate of ) is still relatively high, and the desorption environment and desorption time have not been studied.

[0006] Therefore, there is an urgent need to develop a uranium adsorbent with high selectivity and high adsorption capacity and its preparation method. This uranium adsorbent can achieve instantaneous desorption under mild conditions and can be recycled multiple times. It is suitable for extracting uranium from seawater or uranium-containing wastewater and has important research significance in the field of nuclear energy production. Summary of the Invention

[0007] To address the shortcomings of existing technologies, the present invention aims to provide a uranium adsorbent, its preparation method, and its applications. The uranium adsorbent comprises a metal-organic framework with a nanocage structure, wherein the metal-organic framework is MIL-101(Cr). The uranium adsorbent also includes a keggin-type heteropolyacid in situ encapsulated within the nanocage structure. The uranium adsorbent of the present invention exhibits high uranium adsorption capacity, good selectivity, long service life, and can achieve instantaneous desorption under mild conditions. Furthermore, its preparation process is simple, and the raw materials are widely available, making it widely applicable for treating uranium-containing wastewater or extracting uranium from seawater.

[0008] To achieve this objective, the present invention adopts the following technical solution:

[0009] In a first aspect, the present invention provides a uranium adsorbent comprising a metal-organic framework having a nanocage structure; the uranium adsorbent further comprising a keggin-type heteropolyacid in situ encapsulated in the nanocage structure; the metal-organic framework being MIL-101(Cr).

[0010] The metal-organic framework MIL-101(Cr) in the uranium adsorbent of this invention has a nanocage structure. Compared with other metal-organic frameworks, MIL-101(Cr) has strong stability and high specific surface area, which can effectively improve the adsorption capacity and cycle life of the uranium adsorbent. Furthermore, the keggin-type heteropolyacid is in situ encapsulated within the nanocage of MIL-101(Cr), which not only solves the problem that keggin-type heteropolyacid cannot be used in water due to its high water solubility, but also utilizes the heteropolyacid anion ([PX) of the keggin-type heteropolyacid. 12 O 40 ] 3- The specific coordination between uranium ions and uranium acyl ions enhances the selective adsorption of uranium by the uranium adsorbent, and ([PX) 12 O 40 ] 3- It exhibits pH-responsive properties, meaning its structure changes with pH, ​​from [PW] 12 O 40 ] 3- Transform into [PW] 11 O 39 ]7- The interaction is easily disrupted, causing the uranium adsorbent to desorb instantaneously (1-10 s) under mild conditions.

[0011] It is worth noting that the uranium adsorbent described in this invention uses a specific metal-organic framework, MIL-101(Cr). Besides utilizing its nanocage structure, MIL-101(Cr) also possesses resistance to strong acids and alkalis, as well as salts, compared to common metal-organic frameworks such as ZIF-8, ZIF-67, and HKUST-1. Its metal source, Cr... 3+ With a small ionic radius, high charge, and strong polarization, the coordinate bonds formed with oxygen-containing ligands have more covalent bonds, and the resulting metal-organic framework has high chemical and thermal stability, thus enabling the uranium adsorbent to exist stably in seawater or uranium-containing wastewater and to adsorb uranium multiple times.

[0012] Preferably, the keggin-type heteropolyacid is phosphotungstic acid and / or phosphomolybdic acid.

[0013] The present invention further preferably uses phosphotungstic acid and / or phosphomolybdic acid because the diameter of phosphotungstic acid and phosphomolybdic acid is about 1.2 nm, which can be adapted to the spherical cavity of MIL-101(Cr) nanocage with an inscribed circle diameter of 1.2 nm pentagonal window and 1.6 × 1.5 nm hexagonal window, so as to achieve in-situ encapsulation. Compared with other types such as Wells-Dawson type and Anderson type heteropolyacids, it has stronger stability and can exist stably in uranium-containing aqueous solution after being encapsulated by MIL-101(Cr). Moreover, it has a simple structure, relatively low price, and can be mass-produced.

[0014] Preferably, the uranium adsorbent contains 13.24 wt% to 43.32 wt%, for example, 13.24 wt%, 15.24 wt%, 17.24 wt%, 19.24 wt%, 21.24 wt%, 23.24 wt%, 25.24 wt%, 27.24 wt%, 29.24 wt%, 31.24 wt%, 33.24 wt%, 35.24 wt%, 37.24 wt%, 39.24 wt%, 41.24 wt%, or 43.32 wt%.

[0015] Preferably, the nanocage structure has an MTN topology.

[0016] The nanocage structure described in this invention has an MTN topology, consisting of spherical cavities with diameters of 3.4 nm and 2.9 nm, respectively. The larger cavity has pentagonal windows (with an inscribed circle diameter of 1.2 nm) and hexagonal windows (1.6 × 1.5 nm), while the smaller cavity only has pentagonal windows. Specifically, as shown... Figure 16 and Figure 17 As shown.

[0017] Preferably, the uranium adsorbent has a flower-like morphology.

[0018] Preferably, the particle size of the uranium adsorbent is 0.2 to 35 μm, for example, it can be 0.2 μm, 0.5 μm, 1 μm, 2 μm, 5 μm, 8 μm, 10 μm, 12 μm, 15 μm, 18 μm, 20 μm, 22 μm, 25 μm, 28 μm, 30 μm, 32 μm or 35 μm.

[0019] Preferably, the specific surface area of ​​the uranium adsorbent is 1802.19–2514.36 m². 2 / g, for example, could be 1802.19m 2 / g, 1853.24m 2 / g、1906.35m 2 / g、1958.54m 2 / g、2001.18m 2 / g, 2054.36m 2 / g、2104.38m 2 / g, 2159.47m 2 / g、2212.09m 2 / g、2269.47m 2 / g、2314.67m 2 / g、2364.59m 2 / g、2427.94m 2 / g、2474.31m 2 / g or 2514.36m 2 / g.

[0020] Preferably, the kinetic data of the uranium adsorbent conform to a pseudo-second-order kinetic model, belonging to chemisorption.

[0021] Preferably, during the adsorption and desorption process, the keggin-type heteropolyacid undergoes an ionic structure transformation in the uranium adsorbent.

[0022] Preferably, the ion transformation includes heteropolyacid anions [PX] 12 O 40 ] 3- With the vacancy heteropolyacid anion [PX 11 O 39 ] 7- The mutual conversions of , where X represents W and / or Mo.

[0023] The specific transformation process is as follows:

[0024] In a second aspect, the present invention provides a method for preparing the uranium adsorbent as described in the first aspect, the method comprising:

[0025] (1) Mix keggin-type heteropolyacid, chromium source, metal-organic framework organic ligand and solvent to obtain a mixed solution;

[0026] (2) The mixed solution in step (1) undergoes a hydrothermal reaction to obtain a hydrothermal reaction product; the hydrothermal reaction product is then washed and dried to obtain the uranium adsorbent.

[0027] The uranium adsorbent of this invention is prepared by a hydrothermal reaction method, in which a chromium source and a metal-organic framework organic ligand undergo a hydrothermal reaction to form a metal-organic framework. During the hydrothermal reaction, a keggin-type heteropolyacid is encapsulated in situ within the nanocage of the metal-organic framework. The preparation process is simple, the raw materials are widely available, and the conditions are mild. The prepared uranium adsorbent has strong stability and a high specific surface area, exhibits high selective adsorption of uranium, can achieve instantaneous desorption under mild conditions, and can still maintain an initial adsorption capacity of up to 94.30% after multiple adsorption-desorption cycles. It can be widely used in uranium-containing wastewater treatment, uranium ore resource recovery, and seawater treatment.

[0028] Preferably, the keggin-type heteropolyacid in step (1) is phosphotungstic acid and / or phosphomolybdic acid.

[0029] Preferably, the ratio of the keggin-type heteropolyacid to the mixed solution is (1.6–13.5):1 mg / mL, for example, it can be 1.6 mg / mL, 2 mg / mL, 2.5 mg / mL, 3 mg / mL, 3.5 mg / mL, 4 mg / mL, 4.5 mg / mL, 5 mg / mL, 5.5 mg / mL, 6 mg / mL, 6.5 mg / mL, 7 mg / mL, 7.5 mg / mL, 8 mg / mL, 8.5 mg / mL, 9 mg / mL, 9.5 mg / mL, 10 mg / mL, 10.5 mg / mL, 11 mg / mL, 11.5 mg / mL, 12 mg / mL, 12.5 mg / mL, 13 mg / mL or 13.5 mg / mL, preferably (8.3–11.7):1 mg / mL.

[0030] The present invention further optimizes the ratio of the keggin-type heteropolyacid to the mixed solution to (8.3-11.7):1 mg / mL, which can further improve the adsorption capacity of the prepared uranium adsorbent. If the ratio of the keggin-type heteropolyacid to the mixed solution is too low, that is, the amount of keggin-type heteropolyacid added is too low, the nanocages of MIL-101(Cr) will not be able to completely encapsulate the keggin-type heteropolyacid, the content of uranium adsorption active material keggin-type heteropolyacid in the adsorbent will be too low, and the adsorption capacity of the prepared uranium adsorbent will decrease significantly. If the ratio of the keggin-type heteropolyacid to the mixed solution is too high, that is, the amount of keggin-type heteropolyacid added is too high, the excess keggin-type heteropolyacid will aggregate due to the aggregation effect at low pH, and after the size increases, it will not be able to enter the nanocage, resulting in a reduction in the amount of heteropolyacid actually encapsulated in the MIL-101(Cr) nanocage, and the adsorption capacity of the prepared uranium adsorbent will also decrease.

[0031] Preferably, the chromium source is chromium nitrate nonahydrate.

[0032] Preferably, the ratio of the chromium source to the mixed solution is (25-40):1 mg / mL, for example, it can be 25:1 mg / mL, 26:1 mg / mL, 27:1 mg / mL, 28:1 mg / mL, 29:1 mg / mL, 30:1 mg / mL, 31:1 mg / mL, 32:1 mg / mL, 33:1 mg / mL, 34:1 mg / mL, 35:1 mg / mL, 36:1 mg / mL, 37:1 mg / mL, 38:1 mg / mL, 39:1 mg / mL or 40:1 mg / mL.

[0033] Preferably, the organic ligand of the metal-organic framework is terephthalic acid.

[0034] Preferably, the molar ratio of the chromium source to the metal-organic framework organic ligand is (1 to 1.2):1, for example, it can be 1:1, 1.03:1, 1.05:1, 1.08:1, 1.1:1, 1.13:1, 1.15:1, 1.18:1 or 1.2:1.

[0035] Preferably, the solvent is water.

[0036] Preferably, the mixing in step (1) is carried out by stirring.

[0037] Preferably, the stirring is performed using a magnetic stirrer.

[0038] Preferably, the stirring speed is 400-550 r / min, for example, it can be 400 r / min, 420 r / min, 440 r / min, 460 r / min, 480 r / min, 500 r / min, 520 r / min, 540 r / min or 550 r / min.

[0039] Preferably, the stirring time is 30 to 50 minutes, for example, 30 minutes, 33 minutes, 35 minutes, 38 minutes, 40 minutes, 43 minutes, 45 minutes, 48 ​​minutes or 50 minutes.

[0040] Preferably, the mixing temperature is 20-35°C, for example, it can be 20°C, 21°C, 22°C, 23°C, 24°C, 25°C, 26°C, 27°C, 28°C, 29°C, 30°C, 31°C, 32°C, 33°C, 34°C or 35°C.

[0041] Preferably, the mixing time is 30 to 60 minutes, for example, it can be 30 minutes, 33 minutes, 35 minutes, 38 minutes, 40 minutes, 43 minutes, 45 minutes, 48 ​​minutes, 50 minutes, 53 minutes, 55 minutes, 58 minutes or 60 minutes.

[0042] Preferably, the temperature of the hydrothermal reaction in step (2) is 180 to 200°C, for example, it can be 180°C, 182°C, 184°C, 186°C, 188°C, 190°C, 192°C, 194°C, 196°C, 198°C or 200°C.

[0043] Preferably, the hydrothermal reaction time is 18 to 24 hours, for example, 18 hours, 19 hours, 20 hours, 21 hours, 22 hours, 23 hours or 24 hours.

[0044] Preferably, after the hydrothermal reaction in step (2), the hydrothermal reaction product is first cooled, and then washed and dried in sequence.

[0045] The cooling process typically involves cooling to room temperature, which is the ambient temperature without heating or cooling, ranging from -35 to 40°C, and generally from 20 to 30°C.

[0046] Preferably, the washing solvent includes any one or a combination of at least two of water, ethanol, N,N dimethylformamide, methanol, acetone or ethyl acetate, wherein typical but non-limiting combinations include combinations of water and ethanol, water and N,N dimethylformamide, ethanol and N,N dimethylformamide, methanol and acetone or acetone and ethyl acetate, etc., and preferably a combination of water and N,N dimethylformamide.

[0047] The water used is deionized water with a conductivity of 1 to 10 MΩ·cm, for example, it can be 1 MΩ·cm, 2 MΩ·cm, 3 MΩ·cm, 4 MΩ·cm, 5 MΩ·cm, 6 MΩ·cm, 7 MΩ·cm, 8 MΩ·cm, 9 MΩ·cm or 10 MΩ·cm.

[0048] Preferably, the washing is an alternating washing process, for example, first washing with water, then washing with dimethylformamide; then washing with water again, then washing with dimethylformamide again, and so on, alternating repeatedly.

[0049] Preferably, the number of washing cycles is ≥3 times, for example, 3, 4, 5, 6, 7, 8 or 9 times.

[0050] Preferably, the drying is carried out under vacuum conditions.

[0051] The present invention does not impose any special restrictions on the vacuum conditions, as long as the drying of the hydrothermal reaction products can be achieved at a temperature of 60-80°C.

[0052] Preferably, the vacuum degree of the vacuum condition is -1 to 0.6 bar, for example, it can be -1 bar, -0.8 bar, -0.5 bar, -0.3 bar, 0.1 bar, 0.2 bar, 0.3 bar, 0.4 bar, 0.5 bar or 0.6 bar.

[0053] The present invention further preferably uses a vacuum degree of -1 to 0.6 bar, which can improve the drying rate and enable the hydrothermal reaction product to be dried in a short time.

[0054] Preferably, the drying temperature is 60-80°C, for example, 60°C, 62°C, 64°C, 66°C, 68°C, 70°C, 72°C, 74°C, 76°C, 78°C or 80°C.

[0055] Preferably, the drying time is 6 to 12 hours, for example, 6 hours, 7 hours, 8 hours, 9 hours, 10 hours, 11 hours or 12 hours.

[0056] As a preferred technical solution of the present invention, the preparation method includes the following steps:

[0057] (1) Mix keggin-type heteropoly acid, chromium nitrate nonahydrate, terephthalic acid and water, and stir at a speed of 400-550 r / min for 30-50 min until a mixed solution is obtained.

[0058] Wherein, the keggin-type heteropolyacid is phosphotungstic acid and / or phosphomolybdic acid, and the ratio of the keggin-type heteropolyacid to the mixed solution is (1.6-13.5) mg / mL; the ratio of the chromium nitrate nonahydrate to the mixed solution is (25-40):1 mg / mL; and the molar ratio of the chromium nitrate nonahydrate to terephthalic acid is (1-1.2):1.

[0059] (2) The mixed solution described in step (1) is subjected to hydrothermal reaction at 180-200°C for 18-24 hours to obtain a hydrothermal reaction product; the hydrothermal reaction product is then cooled, washed at least 3 times, and finally vacuum dried at 60-80°C and -1-0.6 bar for 6-12 hours to obtain the uranium adsorbent.

[0060] Thirdly, the present invention provides an application of the uranium adsorbent as described in the first aspect, wherein the uranium adsorbent is used to adsorb uranium in water.

[0061] The uranium adsorbent provided by this invention can be used to adsorb uranium from water. During the adsorption process, it not only exhibits a saturated adsorption capacity of over 280.60 mg / g (25°C), but also excellent anti-interference ability, meaning it is effective against numerous interfering ions, such as K+. + Ca 2+ Na + Mg 2+ Pb 2+ Cu 2+ 、Sr 2+ Zn 2+ Ba 2+ Co 2+ Ni 2+ or V 5+ Even in the presence of at least one of the ions, it still exhibits highly selective adsorption of uranium; and after 8 adsorption-desorption cycles, its adsorption capacity can still reach 94.30% of the initial adsorption capacity, with a long service life; it can be widely used for the treatment of uranium in seawater or uranium-containing wastewater.

[0062] Preferably, the uranium adsorbent is used to adsorb uranium in uranium-containing wastewater, and the adsorption includes: first mixing the uranium-containing wastewater to be treated and the uranium adsorbent to obtain a mixed solution A, and then adjusting the pH value of the mixed solution A for adsorption.

[0063] Preferably, the ratio of the uranium-containing wastewater to be treated to the uranium adsorbent is (25-75):1 mL / mg, for example, it can be 25:1 mL / mg, 30:1 mL / mg, 35:1 mL / mg, 40:1 mL / mg, 45:1 mL / mg, 50:1 mL / mg, 55:1 mL / mg, 60:1 mL / mg, 65:1 mL / mg, 70:1 mL / mg or 75:1 mL / mg.

[0064] Preferably, the mixing process is accompanied by oscillation.

[0065] Preferably, the oscillation speed is 170 to 210 rad / min, for example, it can be 170 rad / min, 175 rad / min, 180 rad / min, 185 rad / min, 190 rad / min, 195 rad / min, 200 rad / min, 205 rad / min or 210 rad / min.

[0066] Preferably, the pH value of the mixture A is adjusted to 5 to 9, for example, it can be 5, 5.5, 6, 6.5, 7, 7.5, 8, 8.5 or 9, preferably 5.5 to 6.5.

[0067] Preferably, the adsorption temperature is 25℃ to 45℃, for example, it can be 25℃, 28℃, 30℃, 33℃, 35℃, 38℃, 40℃, 43℃ or 45℃.

[0068] Preferably, the adsorption time is 12 to 24 hours, for example, 12 hours, 13 hours, 14 hours, 15 hours, 16 hours, 17 hours, 18 hours, 19 hours, 20 hours, 21 hours, 22 hours, 23 hours or 24 hours.

[0069] As a further preferred technical solution of the present invention, the uranium adsorbent is used to adsorb uranium in uranium-containing wastewater. The adsorption includes: first, mixing the uranium-containing wastewater to be treated and the adsorbent in a ratio of (25-75) mL: 1 mg to obtain a mixed solution A, then adjusting the pH value of the mixed solution A to 5-9, and adsorbing at 25℃-45℃ for 12-24 h.

[0070] Preferably, the uranium adsorbent is used to extract uranium from seawater, and the extraction includes: mixing seawater and uranium adsorbent to obtain a mixture B, and finally adjusting the pH value of the mixture B for extraction.

[0071] Preferably, the ratio of seawater to uranium adsorbent is (200-400):1 mL / mg, for example, it can be 200:1 mL / mg, 220:1 mL / mg, 240:1 mL / mg, 260:1 mL / mg, 280:1 mL / mg, 300:1 mL / mg, 320:1 mL / mg, 340:1 mL / mg, 360:1 mL / mg, 380:1 mL / mg or 400:1 mL / mg.

[0072] Preferably, the mixing process is accompanied by oscillation.

[0073] Preferably, the oscillation speed is 190 to 230 rad / min, for example, it can be 190 rad / min, 195 rad / min, 200 rad / min, 205 rad / min, 210 rad / min, 215 rad / min, 220 rad / min, 225 rad / min or 230 rad / min.

[0074] Preferably, the pH value of the mixture B is adjusted to 5 to 9, for example, it can be 5, 5.5, 6, 6.5, 7, 7.5, 8, 8.5 or 9, preferably 5.5 to 6.5.

[0075] Preferably, the extraction temperature is 25℃ to 45℃, for example, it can be 25℃, 28℃, 30℃, 33℃, 35℃, 38℃, 40℃, 43℃ or 45℃.

[0076] Preferably, the extraction time is 12 to 24 hours, for example, it can be 12 hours, 13 hours, 14 hours, 15 hours, 16 hours, 17 hours, 18 hours, 19 hours, 20 hours, 21 hours, 22 hours, 23 hours or 24 hours.

[0077] As a further preferred technical solution of the present invention, the uranium adsorbent is used to extract uranium from seawater. The extraction includes: mixing the seawater and the uranium adsorbent at a ratio of (200-400):1 mL / mg to obtain a mixture B, and finally adjusting the pH value of the mixture B to 5-9, and extracting at 25℃-45℃ for 12-24 hours.

[0078] Preferably, the uranium adsorbent is desorbed after adsorption saturation. The desorption solvent includes any one or a combination of at least two of hydrochloric acid, nitric acid, sodium carbonate, or sodium bicarbonate. Typical but non-limiting combinations include combinations of hydrochloric acid and nitric acid, combinations of sodium carbonate and sodium bicarbonate, etc., with hydrochloric acid being preferred.

[0079] Preferably, the concentration of the hydrochloric acid is 0.005 to 0.5 mol / L, for example, it can be 0.005 mol / L, 0.01 mol / L, 0.05 mol / L, 0.1 mol / L, 0.15 mol / L, 0.2 mol / L, 0.25 mol / L, 0.3 mol / L, 0.35 mol / L, 0.4 mol / L, 0.45 mol / L or 0.5 mol / L, and most preferably 0.005 to 0.1 mol / L.

[0080] Preferably, the desorption duration is 1 to 10 seconds, for example, it can be 1 second, 1.5 seconds, 2 seconds, 2.5 seconds, 3 seconds, 3.5 seconds, 4 seconds, 4.5 seconds, 5 seconds, 5.5 seconds, 6 seconds, 6.5 seconds, 7 seconds, 7.5 seconds, 8 seconds, 8.5 seconds, 9 seconds, 9.5 seconds or 10 seconds.

[0081] The uranium adsorbent described in this invention can achieve instantaneous desorption within 1 to 10 seconds under mild conditions, namely in 0.005 to 0.1 mol / L hydrochloric acid.

[0082] The numerical range described in this invention includes not only the point values ​​listed above, but also any point values ​​within the numerical ranges not listed above. Due to space limitations and for the sake of brevity, this invention will not exhaustively list all the specific point values ​​included in the range.

[0083] Compared with the prior art, the present invention has the following beneficial effects:

[0084] (1) The uranium adsorbent provided by this invention encapsulates a keggin-type heteropolyacid in situ within a nanocage structure of MIL-101(Cr), and fixes the keggin-type heteropolyacid and MIL-101(Cr) together through hydrogen bonding; the uranium adsorbent possesses the extremely strong stability and high specific surface area of ​​MIL-101(Cr), and can exist stably in seawater or uranium-containing wastewater; simultaneously utilizing the heteropolyacid anions ([PX) of the keggin-type heteropolyacid encapsulated in the nanocage... 12 O 40 ] 3- The specific coordination between [PX] and uranyl ions enables selective adsorption of uranyl ions, greatly improving the adsorption efficiency of uranium, with an initial adsorption capacity as high as 325 mg / g; furthermore, due to the specific coordination between [PX] and uranyl ions, the adsorption of uranium ions is achieved. 12 O 40 ] 3- The uranium adsorbent exhibits pH-responsive characteristics, enabling ultrafast desorption in hydrochloric acid at concentrations as low as 0.005 mol / L, and maintaining 94.30% of its initial adsorption capacity after eight adsorption-desorption cycles. Furthermore, the uranium adsorbent demonstrates excellent resistance to interference, meaning it remains resistant to numerous interfering ions (K+, K+, ...). + Ca 2+ Na + Mg 2+ Pb 2+ Cu 2+ 、Sr 2+ Zn 2+ Ba 2+ Co 2+ Ni 2+ V 5+ Even in the presence of ), it can still exhibit highly selective adsorption of uranium.

[0085] (2) The method for preparing uranium adsorbent provided by the present invention uses hydrothermal reaction to prepare the uranium adsorbent, which has the advantages of simple and controllable preparation process, short cycle, wide availability of raw materials, low cost, and easy scale-up to industrial production.

[0086] (3) Application of the uranium adsorbent provided by the present invention: The uranium adsorbent has high selective adsorption characteristics for uranium in water, and under preferred conditions, the uranium adsorption capacity reaches more than 280.60 mg / g. It can be widely used in the fields of uranium-containing wastewater treatment, uranium ore resource recovery and seawater uranium extraction. Attached Figure Description

[0087] Figure 1 This is a scanning electron microscope image of the uranium adsorbent provided in Embodiment 1 of the present invention;

[0088] Figure 2 This is a bar chart of the uranium adsorption capacity of the uranium adsorbent provided in Example 1 of the present invention at different pH values;

[0089] Figure 3 This is a bar chart showing the uranium adsorption capacity of the uranium adsorbents provided in Comparative Example 1, Example 1, and Examples 4-6 of the present invention at pH 6.

[0090] Figure 4 This is a graph showing the change in uranium adsorption capacity of the uranium adsorbent at different times and a graph showing the adsorption kinetics model provided in Example 1 of the present invention;

[0091] Figure 5 This is a graph showing the variation of uranium adsorption capacity of the uranium adsorbent provided in Example 1 of the present invention at different equilibrium concentrations at 25°C, 35°C, and 45°C.

[0092] Figure 6 This is a desorption rate diagram of the uranium adsorbent provided in Example 1 of the present invention under different desorption solvents;

[0093] Figure 7 This is a diagram showing the desorption rate of the uranium adsorbent provided in Example 1 of the present invention under different concentrations of hydrochloric acid;

[0094] Figure 8 This is a separation factor diagram of the uranium adsorbent provided in Example 1 of the present invention under the presence of different interfering ions;

[0095] Figure 9 This is a graph showing the removal rate of uranium and interfering ions by the uranium adsorbent provided in Example 1 of the present invention in simulated uranium-containing wastewater;

[0096] Figure 10 This is a graph showing the adsorption capacity of the uranium adsorbent provided in Example 1 of the present invention for uranium and interfering elements in spiked seawater;

[0097] Figure 11 This is a graph showing the change in adsorption capacity of the uranium adsorbent provided in Example 1 of the present invention after 8 adsorption-desorption cycles;

[0098] Figure 12 This is the infrared spectrum of the uranium adsorbent before and after adsorbing uranyl ions provided in Example 1 of the present invention;

[0099] Figure 13 These are the XPS full spectra of the uranium adsorbent before and after adsorbing uranyl ions provided in Example 1 of this invention;

[0100] Figure 14 The O2 content of the uranium adsorbent before and after adsorption of uranyl ions provided in Example 1 of this invention is... 1S Spectrum;

[0101] Figure 15 The solid-state NMR spectrometers provided in Example 1 of this invention, before and after adsorbing uranyl ions and after desorption, are shown. 31 P-spectrum;

[0102] Figure 16 A schematic diagram of the large cavity, small cavity, pentagonal window, and hexagonal window in the nanocage structure of the uranium adsorbent provided by the present invention;

[0103] Figure 17 This is a schematic diagram of the nanocage structure connection of the uranium adsorbent provided by the present invention. Detailed Implementation

[0104] The technical solution of the present invention will be further described below with reference to the accompanying drawings and specific embodiments. Those skilled in the art should understand that the embodiments described are merely illustrative of the present invention and should not be considered as specific limitations thereof.

[0105] Unless otherwise specified, the experimental methods used in the following examples and comparative examples are conventional methods; the experimental materials used, unless otherwise specified, were purchased from conventional biochemical reagent manufacturers.

[0106] I. Implementation Examples

[0107] Example 1

[0108] This embodiment provides a uranium adsorbent, the preparation method of which includes the following steps:

[0109] (1) Mix 300 mg phosphotungstic acid, 2 mmol chromium nitrate nonahydrate, 2 mmol terephthalic acid and 30 mL water, and stir at 480 r / min for 40 min until the solution is homogeneous to obtain a mixed solution;

[0110] The ratio of phosphotungstic acid to the mixed solution is 10:1 mg / mL; the ratio of chromium nitrate nonahydrate to the mixed solution is 26.7:1 mg / mL.

[0111] (2) The mixed solution described in step (1) was subjected to hydrothermal reaction at 180°C for 24 hours to obtain a hydrothermal reaction product. The hydrothermal reaction product was then cooled to room temperature (25°C) and washed alternately with deionized water and dimethylformamide, repeated 3 times. Finally, it was vacuum dried at 70°C and 0.1 bar for 9 hours to obtain a gray-green uranium adsorbent.

[0112] Example 2

[0113] This embodiment provides a uranium adsorbent, the preparation method of which includes the following steps:

[0114] (1) Mix 250 mg phosphomolybdic acid, 3 mmol chromium nitrate nonahydrate, 2.5 mmol terephthalic acid and 30 mL water, and stir at 400 r / min for 50 min until the solution is homogeneous to obtain a mixed solution;

[0115] The ratio of phosphomolybdic acid to the mixed solution is 8.3:1 mg / mL; the ratio of chromium nitrate nonahydrate to the mixed solution is 40:1 mg / mL.

[0116] (2) The mixed solution described in step (1) was subjected to hydrothermal reaction at 190°C for 20 h to obtain the hydrothermal reaction product. The hydrothermal reaction product was then cooled to room temperature (28°C), and washed alternately with ethanol and dimethylformamide for 4 times. Finally, it was vacuum dried at 60°C and -1 bar for 12 h to obtain a gray-green uranium adsorbent.

[0117] Example 3

[0118] This embodiment provides a uranium adsorbent, the preparation method of which includes the following steps:

[0119] (1) Mix 350 mg phosphotungstic acid, 2.5 mmol chromium nitrate nonahydrate, 1.7 mmol terephthalic acid and 30 mL water, and stir at 500 r / min for 30 min until the solution is homogeneous to obtain a mixed solution;

[0120] The ratio of phosphomolybdic acid to the mixed solution is 11.7:1 mg / mL; the ratio of chromium nitrate nonahydrate to the mixed solution is 33.3:1 mg / mL.

[0121] (2) The mixed solution described in step (1) was subjected to hydrothermal reaction at 200°C for 18 hours to obtain a hydrothermal reaction product. The hydrothermal reaction product was then cooled to room temperature (20°C), and washed alternately with deionized water and ethanol for 5 times. Finally, it was vacuum dried at 80°C and 0.6 bar for 6 hours to obtain a gray-green uranium adsorbent.

[0122] Examples 4-6

[0123] Keeping all other conditions the same as in Example 1, only changing the amount of phosphotungstic acid added in step (1) of Example 1, the effect of the amount of phosphotungstic acid added on the adsorption capacity of the obtained uranium adsorbent was investigated. Specifically, the mass of phosphotungstic acid in Examples 4 to 6 was 100 mg, 200 mg, and 400 mg, respectively.

[0124] Example 7

[0125] This embodiment provides a uranium adsorbent, the preparation method of which is the same as in Example 1 except that the molar amount of chromium nitrate nonahydrate in step (1) is 1.5 mmol, that is, the ratio of chromium nitrate nonahydrate to the mixed solution is 20:1 mg / mL.

[0126] Example 8

[0127] This embodiment provides a uranium adsorbent, the preparation method of which is the same as in Example 1, except that the molar amount of chromium nitrate nonahydrate in step (1) is 3.2 mmol, that is, the ratio of chromium nitrate nonahydrate to the mixed solution is 42.7:1 mg / mL.

[0128] II. Comparative Example

[0129] Comparative Example 1

[0130] This comparative example provides a uranium adsorbent, the preparation method of which does not include phosphotungstic acid in step (1), and the rest is the same as in Example 1.

[0131] Comparative Example 2

[0132] This comparative example provides a uranium adsorbent, which is the same as in Example 1 except that MIL-101(Cr) is replaced with ZIF-8 and the reaction is carried out at room temperature (25°C).

[0133] Comparative Example 3

[0134] This comparative example provides a uranium adsorbent, which is the same as in Example 1 except that MIL-101(Cr) is replaced with HKUST-1 and the reaction is carried out at room temperature (25°C).

[0135] Comparative Example 4

[0136] This comparative example provides a uranium adsorbent, the preparation method of which is the same as that in Example 1 except that the phosphotungstic acid in step (1) is replaced with ammonium phosphotungstate.

[0137] Comparative Example 5

[0138] This comparative example provides a uranium adsorbent, the preparation method of which is the same as that of Example 1, except that chromium nitrate nonahydrate, terephthalic acid and water are first mixed and hydrothermally reacted to generate MIL-101(Cr); then phosphotungstic acid is mixed with MIL-101(Cr) by impregnation.

[0139] III. Application Examples

[0140] Application Example 1

[0141] This application example provides an application of the uranium adsorbent described in Example 1. The uranium adsorbent is used to adsorb uranium from simulated uranium-containing wastewater. The adsorption includes: first, mixing 125 mL of a solution containing 10 ppm uranium and 11 interfering metal ions (K+) at an equal concentration in a ratio of 25:1 mL / mg. + Mg 2+ Co 2+ Ni 2+ Zn 2+ Ba 2+ 、Sr 2+ Ce 3+ 、Nd 3+ Eu 3+ La 3+ A mixed solution (i.e., simulated uranium-containing wastewater) was prepared by mixing 5 mg of the uranium adsorbent provided in Example 1 to obtain mixed solution A, which was then transferred to a constant temperature water bath shaker (25°C, 180 rpm) and shaken for 24 h for adsorption.

[0142] Application Example 2

[0143] This application example provides an application of the uranium adsorbent described in Example 1, which is used to extract uranium from spiked seawater. The extraction includes: taking 2L of filtered natural seawater (Hainan, China), spiked to a uranium concentration of 10ppm, adjusting the pH of the spiked seawater to 6, transferring it to a plastic container, adding 10mg of the uranium adsorbent provided in Example 1, and placing it in a constant temperature water bath shaker (25℃, 180rpm) for 12h to extract uranium.

[0144] IV. Tests and Results

[0145] 1. Appearance Test: The morphology of the uranium adsorbent provided in Example 1 was characterized using a scanning electron microscope (Zeiss Sigma 300, UK). The results are as follows: Figure 1 As shown, from Figure 1 As can be seen, the uranium adsorbent provided in Example 1 has a morphology of building block flowers and a particle size of 2.5 μm.

[0146] 2. Adsorption experiment:

[0147] All the following tests used a syringe with a 0.22 μm water filter head to draw the supernatant of the test solution, and used an inductively coupled plasma optical emission spectrometer (ICP-OES) to determine the concentration of uranium in the solution before and after adsorption, and calculated the adsorption capacity according to the following formula.

[0148]

[0149] Where C0 (mg / L) is the initial concentration of uranium in the solution, C e (mg / L) is the concentration of uranium in the solution after adsorption equilibrium is reached, V(L) is the solution volume, and m(g) is the mass of adsorbent added.

[0150] ① Preparation of uranium standard solution: Weigh 0.211g of uranyl nitrate hexahydrate into a 25mL beaker, add deionized water to dissolve it, and then transfer it to a 500mL volumetric flask and make up to volume to obtain a uranium standard solution with a concentration of 200ppm. In this invention, uranium solutions of other concentrations are obtained by diluting the 200ppm uranium standard solution prepared above.

[0151] ② The uranium adsorption capacity of the uranium adsorbent provided in Example 1 at different pH values ​​was tested, and the results are as follows: Figure 2 As shown, the optimal adsorption pH was determined, and the specific test procedure is as follows:

[0152] The pH values ​​of the uranium solution were adjusted to 3, 4, 5, 6, 7, 8, and 9 using 0.5 mol / L Na₂CO₃ and 0.1 mol / L HNO₃ solutions, respectively. 5 mg of the uranium adsorbent provided in Example 1 was weighed into a 125 mL plastic bottle, and 120 mL of 20 ppm uranium solution at different pH values ​​(3–9) was added. The solution was then transferred to a constant temperature water bath shaker (25°C, 180 rpm) and shaken for 6 hours to reach adsorption equilibrium. The uranium concentration before and after adsorption was tested, and the uranium adsorption capacity was calculated.

[0153] according to Figure 2 It is known that the optimal adsorption pH value of the uranium adsorbent provided in Example 1 is 6, therefore the pH value of the subsequent adsorption experiment is 6.

[0154] ③ The adsorption capacity (25℃) of the uranium adsorbents provided in Examples 1-8 and Comparative Examples 1-5 was tested, and the results are shown in Table 1. The influence trend of the amount of phosphotungstic acid added on the adsorption effect of the uranium adsorbent was also investigated (the adsorption capacity results of Comparative Example 1, Example 1, and Examples 4-6 as single-factor variables are shown in Table 1). Figure 3 As shown in the image, the specific testing process is as follows:

[0155] Weigh 5 mg of the uranium adsorbent provided in Examples 1-8 and Comparative Examples 1-5 into 125-size plastic bottles, add 120 mL of 20 ppm (pH 6) uranium solution, transfer to a constant temperature water bath shaker (25°C, 180 rpm), shake for 6 h to reach adsorption equilibrium, test the uranium concentration before and after adsorption and calculate the uranium adsorption capacity.

[0156] Table 1

[0157] project Adsorption capacity (mg / g) Example 1 319.18 Example 2 289.60 Example 3 290.67 Example 4 197.52 Example 5 250.44 Example 6 276.42 Example 7 129.42 Example 8 135.88 Comparative Example 1 20.52 Comparative Example 2 168.32 Comparative Example 3 134.00 Comparative Example 4 173.44 Comparative Example 5 162.83

[0158] As shown in Table 1:

[0159] As can be seen from Examples 1 to 3, the uranium adsorbent of the present invention utilizes the synergistic effect of MIL-101(Cr) and keggin-type heteropolyacid to prepare the uranium adsorbent through hydrothermal reaction under specific conditions. The uranium adsorbent exhibits a specific adsorption effect on uranium and has an adsorption capacity of up to 289.60 mg / g or more.

[0160] Combining Comparative Example 1, Example 1, and Examples 4-6, and Figure 3 It can be seen that by further optimizing the ratio of the keggin-type heteropolyacid to the mixed solution to (8.3-11.7):1 mg / mL, that is, controlling the amount of keggin-type heteropolyacid added in step (1) to be 250-350 mg, the uranium adsorption capacity is further improved to above 289.60 mg / g. When the amount of keggin-type heteropolyacid added is 300 mg, the adsorption capacity of the uranium adsorbent reaches its extreme value of 319.18 mg / g; however, as the amount of keggin-type heteropolyacid added gradually decreases, the uranium adsorption capacity of the uranium adsorbent gradually decreases, as in Example 5. When the amount of keggin-type heteropolyacid added was 200 mg, the uranium adsorption capacity decreased to 250.44 mg / g. In Example 4, when the amount of keggin-type heteropolyacid added was reduced to 100 mg, the uranium adsorption capacity decreased to 197.52 mg / g. In Example 6, when the amount of keggin-type heteropolyacid added to the uranium adsorbent was increased to 400 mg, its uranium adsorption capacity decreased to 276.42 mg / g. In Comparative Example 1, when no phosphotungstic acid was added, its uranium adsorption capacity decreased significantly to 20.52 mg / g. It can be seen that the amount of keggin-type heteropolyacid added has a great influence on the adsorption effect of the uranium adsorbent, and the uranium adsorption capacity reaches its extreme value when 300 mg of keggin-type heteropolyacid is added.

[0161] As can be seen from Examples 1 and 7-8, the present invention further optimizes the ratio of chromium nitrate nonahydrate to the mixed solution to (25-40):1 mg / mL, so as to successfully prepare the metal-organic framework MIL-101(Cr) with a nanocage structure and encapsulate the keggin-type heteropolyacid in the nanocage, thereby achieving a synergistic effect between the two and improving the adsorption capacity of the uranium adsorbent; however, when the ratio of chromium nitrate nonahydrate to the mixed solution in Examples 7 or 8 is too low or too high, the adsorption capacity of the uranium adsorbent drops to below 135.88 mg / g.

[0162] As can be seen from Examples 1 and Comparative Examples 2-4, the uranium adsorbent of the present invention utilizes a specific metal-organic framework MIL-101(Cr) and a specific keggin-type heteropolyacid (phosphotungstic acid and / or phosphomolybdic acid) to work together. This fully leverages the extremely strong stability and high specific surface area of ​​the metal-organic framework MIL-101(Cr) to improve the adsorption capacity and lifespan of the uranium adsorbent. Simultaneously, by encapsulating the keggin-type heteropolyacid within its nanocage structure, it not only solves the problem of keggin-type heteropolyacid's inability to be used in water due to its high water solubility, but also utilizes the specific coordination of the keggin-type heteropolyacid with uranyl ions. This allows the uranium adsorbent to exhibit high selective adsorption of uranium even in the presence of numerous interfering ions. Furthermore, its pH-responsive characteristics enable the uranium adsorbent to achieve instantaneous desorption under mild conditions. However, when the metal-organic frameworks used in Comparative Examples 2 and 3 were ZIF-8 and HKUST-1, respectively, the adsorption capacity of the resulting uranium adsorbents was very low, only 168.32 mg / g and 134.00 mg / g, because ZIF-8 and HKUST-1 could not exist stably in uranium-containing aqueous solutions. Moreover, they could not be recycled multiple times and had a short service life. When phosphotungstic acid was replaced with phosphotungstate (ammonium phosphotungstate) in Comparative Example 4, phosphotungstic acid is a strong acid, stronger than sulfuric acid, which can maintain the pH of the solution during synthesis and is easily soluble in water. In contrast, ammonium phosphotungstate is a weak acid and is only slightly soluble in water, which is not conducive to the reaction. This resulted in a reduction in the amount of phosphotungstate ions that actually entered MIL-101(Cr), thus reducing the adsorption capacity of the resulting uranium adsorbent to only 173.44 mg / g.

[0163] As can be seen from Example 1 and Comparative Example 5, the uranium adsorbent of the present invention encapsulates keggin-type heteropolyacids in situ into the nanocages of MIL-101(Cr) through in-situ encapsulation. The two work synergistically, greatly improving the adsorption capacity of the obtained uranium adsorbent. However, when Comparative Example 6 uses the impregnation method, the uneven mixing solution and other factors prevent the keggin-type heteropolyacids from fully entering the nanocages of MIL-101(Cr), resulting in a significant decrease in the adsorption capacity of the obtained uranium adsorbent, which is only 162.83 mg / g.

[0164] ④ The kinetic equilibrium time of the uranium adsorbent provided in Example 1 was tested, and the results are as follows: Figure 4 As shown, the specific testing process is as follows:

[0165] Weigh 5 mg of the uranium adsorbent provided in Example 1 into a 125 mL plastic bottle, add 120 mL of 20 ppm (pH 6) uranium standard solution, transfer to a constant temperature water bath shaker (25°C, 180 rpm), and shake for 10 min, 30 min, 60 min, 100 min, 150 min, 250 min, 350 min, and 500 min respectively. Test the uranium concentration before and after adsorption and calculate the uranium adsorption capacity.

[0166] according to Figure 4 It can be seen that the kinetic data of the uranium adsorbent provided in Example 1 conforms to the pseudo-second-order kinetic model, which belongs to chemical adsorption. The adsorption capacity reaches a maximum of 75% in about 2.5h (150min) and adsorption equilibrium is reached in 6h (360min).

[0167] ⑤ The adsorption capacity variation trend of the uranium adsorbent provided in Example 1 at different equilibrium concentrations at 25℃, 35℃, and 45℃ was tested, and the maximum adsorption capacity was determined. The results are as follows: Figure 5 As shown, the specific testing process is as follows:

[0168] Weigh 5 mg of the adsorbent provided in Example 1 into a 125 mL plastic bottle, add 120 mL of uranium standard solutions with concentrations of 10, 30, 40, 50, and 60 ppm (pH 6), respectively, and transfer them to a constant temperature water bath shaker (180 rpm) at temperatures of 25°C, 35°C, and 45°C. After shaking for 6 hours, test the uranium concentration before and after adsorption and calculate the uranium adsorption capacity.

[0169] according to Figure 5 It can be seen that the isotherm data of the adsorbent provided in Example 1 conforms to the Langmuir adsorption isotherm model, and the simulated maximum adsorption capacity at 25℃, 35℃ and 45℃ is 461.88mg / g, 587.50mg / g and 682.03mg / g, respectively.

[0170] ⑥ The desorption rates of the uranium adsorbent provided in Example 1 in different desorption solvents and in hydrochloric acid solutions of different concentrations were tested, and the results are as follows: Figure 6 and 7 As shown, the specific testing process is as follows:

[0171] Weigh 20 mg of the uranium adsorbent provided in Example 1 into a 500 mL plastic bottle, add 400 mL of 20 ppm (pH 6) uranium standard solution, transfer to a constant temperature water bath shaker (25 °C, 180 rpm), test the uranium concentration before and after adsorption and calculate the uranium adsorption capacity.

[0172] The adsorbed solution was filtered, and the resulting adsorbent was placed in 200 mL of different desorption solvents (HCl, HNO3, NaHCO3, Na2CO3). After shaking for 3 seconds, the concentration of uranium after desorption was measured, and the amount of uranium desorbed, Q, was calculated according to the following formula. j and desorption rate D;

[0173] Q j =C j ×V j

[0174] Q x =(C0-C e )×V

[0175] D = Q j / Q x ×100%

[0176] Among them, C j (mg / L) is the concentration of uranium in the desorption solution, V j (L) is the volume of the desorbed solution, Q x It represents the adsorption capacity of uranium during the adsorption process (mg / g).

[0177] according to Figure 6 It can be seen that the uranium adsorbent provided in Example 1 has a desorption rate of more than 95% when hydrochloric acid and nitric acid are used as desorption solvents. Considering the oxidizing properties of nitric acid and the economy of hydrochloric acid, hydrochloric acid is preferred as the desorption solvent.

[0178] Then, using 0.0005–0.5 mol / L hydrochloric acid solutions as desorption solvents, the desorption rate trend of the uranium adsorbent provided in Example 1 under different concentrations of hydrochloric acid was investigated. The results are as follows: Figure 7 As shown;

[0179] according to Figure 7 It can be seen that hydrochloric acid still has a high desorption rate of 97.02% when the concentration is 0.005 mol / L. When the concentration of hydrochloric acid is less than 0.005 mol / L, the desorption rate decreases significantly. Therefore, the concentration of hydrochloric acid as the desorption solvent is preferably 0.005 mol / L to 0.5 mol / L.

[0180] ⑦ Investigate the effect of interfering ions on the adsorption effect of the uranium adsorbent provided in Example 1, and obtain the separation factor bar chart of the uranium adsorbent provided in Example 1 under the presence of different interfering ions (e.g., Figure 8As shown in the image, the specific testing process is as follows:

[0181] Weigh 5 mg of the uranium adsorbent provided in Example 1 into a 125 mL plastic bottle, and add 120 mL of a solution containing 10 ppm uranium and an equal concentration of coexisting metal ions (K). + Ca 2+ Na + Mg 2+ Pb 2+ Cu 2+ 、Sr 2+ Zn 2+ Ba 2+ Co 2+ Ni 2+ V 5+ A binary mixed solution of uranium and interfering ions was prepared, and the pH was adjusted to 6. The solution was then transferred to a constant temperature water bath shaker (25℃, 180 rpm) and shaken for 6 hours to reach adsorption equilibrium. The concentrations of uranium and interfering ions before and after adsorption were measured. The relative separation factor SF was used to characterize the degree of interference of each interfering ion on uranium adsorption. The greater the deviation of the relative separation factor SF from 1, the easier it is to separate the interfering ions. This indicates that the uranium adsorbent has a stronger anti-interference ability and can achieve efficient separation and adsorption of uranium. The relative separation factor SF was calculated according to the following formula.

[0182]

[0183]

[0184] In the formula, K d u K is the uranium separation factor. d M Separation factors for interfering ions; CO and C e (mg / L) represents the initial and equilibrium concentrations of ions in the solution, respectively; V(L) is the solution volume; and m(g) is the mass of adsorbent added.

[0185] according to Figure 8 It can be seen that the uranium adsorbent provided in Example 1 has a relative separation factor (SF) as high as 22-355117 in the presence of different interfering ions, indicating that the uranium adsorbent exhibits high selectivity for uranyl ions.

[0186] ⑧ The concentrations of uranium and interfering ions in the simulated uranium-containing wastewater before and after adsorption in Application Example 1 were determined, and the removal rate R was calculated according to the following formula. The results are as follows: Figure 9 As shown;

[0187]

[0188] In the formula, C0 and C e(mg / L) represent the initial and equilibrium concentrations of ions in the solution, respectively;

[0189] according to Figure 9 It can be seen that the uranium adsorbent provided in Example 1 has a much higher removal rate of uranyl ions in simulated uranium-containing wastewater than other interfering ions, specifically 80.2%, indicating that the uranium adsorbent can still selectively adsorb uranyl ions in simulated uranium-containing wastewater.

[0190] ⑨ The concentrations of uranium and interfering ions in the seawater before and after extraction in Application Example 2 were determined, and the adsorption capacity was calculated. The results are as follows: Figure 10 As shown.

[0191] according to Figure 10 It can be seen that the uranium adsorbent provided in Example 1 still has a high adsorption capacity for uranyl ions in spiked seawater, specifically 80.50 mg / g.

[0192] ⑩ Adsorption-desorption cycle life test: Weigh 20 mg of the uranium adsorbent provided in Example 1 into a 500 mL plastic bottle, add 400 mL of 20 ppm uranium solution with pH 6, transfer to a constant temperature water bath shaker (25℃, 180 rpm), shake for 6 h, test the uranium concentration before and after adsorption and calculate the uranium adsorption capacity.

[0193] The adsorbed solution was then filtered. The filtered adsorbent was placed in 200 mL of 0.005 mol / L hydrochloric acid solution, shaken for 3 seconds, and then filtered again. The desorbed adsorbent underwent the same cycle eight times. The adsorption capacity of the uranium adsorbent after desorption was tested. Finally, the initial adsorption capacities of the uranium adsorbent before and after desorption were compared. The results are as follows: Figure 11 As shown.

[0194] according to Figure 11 It can be seen that after repeated cycles of 8 times, the uranium adsorbent provided in Example 1 can still maintain 94.30% of the initial adsorption capacity, indicating that the uranium adsorbent described in this invention has a long service life and can be recycled.

[0195] 3. Infrared Spectroscopy Test: An infrared spectrometer (Bruker, Germany, Tensor 27) was used to analyze the uranium adsorbent provided in Example 1 before adsorption of uranyl ions (MIL-101(Cr)@PW). 12 (MIL-101(Cr)@PW) 12 The test was performed using -U), and the results were as follows: Figure 12 As shown.

[0196] according to Figure 12 It can be seen that in MIL-101(Cr)@PW 12 In the infrared spectrum, 1080 cm⁻¹ -1 980cm -1 892cm-1 and 818cm -1 The absorption peaks appearing at 1613 cm⁻¹ are the PO tensile vibration peak of the central tetrahedron, the W=O stretching vibration peak of the terminal end, and the WOW tensile vibration peak, respectively. -1 1505cm -1 1395cm -1 and 749cm -1 The absorption peaks appearing at the positions are the stretching vibration peaks of CC, OCC, C=O, and CH, respectively; in MIL-101(Cr)@PW 12 -U in the infrared spectrum 914cm -1 A new absorption peak appears at [O=U=O], which originates from [O=U=O]. 2+ The antisymmetric vibration, in addition, the blue shift of the W=O absorption peak indicates an interaction between oxygen atoms and uranyl ions.

[0197] 4. Elemental Analysis: Elemental analysis was performed using an X-ray photoelectron spectroscopy (XPS) system (Thermo, ESCALAB 250Xi, USA) to analyze the uranium adsorbent provided in Example 1 before adsorption of uranyl ions (MIL-101(Cr)@PW). 12 (MIL-101(Cr)@PW) 12 The test was performed using -U), and the results were as follows: Figure 13 , 14 As shown.

[0198] according to Figure 13 It can be seen that MIL-101(Cr)@PW 12 After adsorption, new binding energy peaks appear at 392.47 eV and 381.70 eV, which are characteristic peaks of uranyl ions, corresponding to U₄f⁻ and U₂f⁻, respectively. 5 / 2 and U4f 7 / 2 ;

[0199] according to Figure 14 It can be seen that MIL-101(Cr)@PW 12 The binding energy peaks at 530.23 eV, 532.21 eV, and 533.15 eV are attributed to WOW, -COOH, and WOH, respectively. After adsorption, a new UO characteristic peak appears at 530.8 eV, and the binding energy of the WOH peak shifts to a lower value, indicating that the coordination between the terminal oxygen atom in phosphotungstic acid and the uranyl ion is the main mechanism for the adsorption of uranium by the uranium adsorbent.

[0200] 5. Solid-state nuclear magnetic resonance 31 P-spectrum testing: A solid-state nuclear magnetic resonance spectrometer (Bruker, Switzerland, AVANCE IIIHD 500MHz) was used to test the uranium adsorbent provided in Example 1 before and after adsorption of uranyl ions and after desorption. The results are as follows: Figure 15As shown, PW 12 Representative of phosphotungstic acid, MIL-101(Cr)@PW 12 Before adsorption, MIL-101(Cr)@PW 12 -U represents MIL-101(Cr)@PW after adsorption. 12 -UD represents the result after desorption;

[0201] according to Figure 15 It can be seen that MIL-101(Cr)@PW 12 The peak positions of both phosphotungstic acid and phosphotungstic acid are approximately -15 ppm, confirming that the phosphotungstic acid ion in the MIL-101(Cr) nanocage exists in the form of [PW 12 O 40 ] 3- The adsorption peak was -11.5 ppm, and after desorption, the peak returned to approximately -15 ppm, indicating that during the adsorption process, [PW 12 O 40 ] 3- Convert to [PW] 11 O 39 ] 7- It coordinates with uranyl ions and exhibits pH-responsive characteristics during desorption, transforming its structure into [PW] as pH decreases. 12 O 40 ] 3- This disrupts coordination, enabling ultrafast desorption under mild conditions.

[0202] The applicant declares that the above description is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Those skilled in the art should understand that any changes or substitutions that can be easily conceived by those skilled in the art within the technical scope disclosed in the present invention fall within the protection and disclosure scope of the present invention.

Claims

1. An application of a uranium adsorbent, characterized in that, The uranium adsorbent is used to adsorb uranium from uranium-containing wastewater, and the uranium adsorbent includes a metal-organic framework, which has a nanocage structure. The uranium adsorbent also includes a keggin-type heteropolyacid encapsulated in situ within the nanocage structure; the keggin-type heteropolyacid is phosphotungstic acid and / or phosphomolybdic acid; The metal-organic framework is MIL-101(Cr).

2. The application of the uranium adsorbent according to claim 1, characterized in that, The uranium adsorbent contains 13.24 wt% to 43.32 wt% keggin-type heteropolyacids.

3. The application of the uranium adsorbent according to claim 1, characterized in that, The nanocage structure has an MTN topology.

4. The application of the uranium adsorbent according to claim 1, characterized in that, The particle size of the uranium adsorbent is 0.2~35μm.

5. The application of the uranium adsorbent according to claim 1, characterized in that, The specific surface area of ​​the uranium adsorbent is 1802.19~2514.36 m². 2 / g.

6. The application of the uranium adsorbent according to claim 1, characterized in that, During the adsorption and desorption process of the uranium adsorbent, the keggin-type heteropolyacid undergoes an ion transformation.

7. The application of the uranium adsorbent according to claim 6, characterized in that, The ion transformation includes heteropolyacid anions [PX] 12 O 40 ] 3- With the vacancy heteropolyacid anion [PX 11 O 39 ] 7- The mutual conversions of , where X represents W and / or Mo.

8. The application of the uranium adsorbent according to claim 1, characterized in that, The preparation method of the uranium adsorbent includes: (1) A mixed solution is obtained by mixing a keggin-type heteropolyacid, a chromium source, a metal-organic framework organic ligand, and a solvent; the keggin-type heteropolyacid is phosphotungstic acid and / or phosphomolybdic acid; (2) The mixed solution in step (1) undergoes a hydrothermal reaction to obtain a hydrothermal reaction product; the hydrothermal reaction product is then washed and dried to obtain the uranium adsorbent.

9. The application of the uranium adsorbent according to claim 8, characterized in that, The ratio of the keggin-type heteropolyacid to the mixed solution is (1.6~13.5):1 mg / mL.

10. The application of the uranium adsorbent according to claim 9, characterized in that, The ratio of the keggin-type heteropolyacid to the mixed solution was (8.3~11.7):1 mg / mL.

11. The application of the uranium adsorbent according to claim 8, characterized in that, The chromium source is chromium nitrate nonahydrate.

12. The application of the uranium adsorbent according to claim 8, characterized in that, The ratio of the chromium source to the mixed solution is (25~40):1 mg / mL.

13. The application of the uranium adsorbent according to claim 8, characterized in that, The organic ligand of the metal-organic framework is terephthalic acid.

14. The application of the uranium adsorbent according to claim 8, characterized in that, The molar ratio of the chromium source to the metal-organic framework organic ligand is (1~1.2):

1.

15. The application of the uranium adsorbent according to claim 8, characterized in that, The solvent is water.

16. The application of the uranium adsorbent according to claim 8, characterized in that, The mixing in step (1) is carried out by stirring.

17. The application of the uranium adsorbent according to claim 16, characterized in that, The stirring speed is 400~550 r / min.

18. The application of the uranium adsorbent according to claim 16, characterized in that, The stirring time is 30-50 minutes.

19. The application of the uranium adsorbent according to claim 8, characterized in that, The mixing temperature is 20~35℃.

20. The application of the uranium adsorbent according to claim 8, characterized in that, The mixing time is 30-60 minutes.

21. The application of the uranium adsorbent according to claim 8, characterized in that, The temperature of the hydrothermal reaction in step (2) is 180~200℃.

22. The application of the uranium adsorbent according to claim 8, characterized in that, The hydrothermal reaction takes 18-24 hours.

23. The application of the uranium adsorbent according to claim 8, characterized in that, After the hydrothermal reaction in step (2), the hydrothermal reaction product is first cooled, and then washed and dried in sequence.

24. The application of the uranium adsorbent according to claim 23, characterized in that, The washing solvent includes any one or a combination of at least two of the following: water, ethanol, N,N-dimethylformamide, methanol, acetone, or ethyl acetate.

25. The application of the uranium adsorbent according to claim 23, characterized in that, The washing process is repeated at least 3 times.

26. The application of the uranium adsorbent according to claim 23, characterized in that, The drying process is carried out under vacuum conditions.

27. The application of the uranium adsorbent according to claim 26, characterized in that, The vacuum level of the vacuum condition is -1 to 0.6 bar.

28. The application of the uranium adsorbent according to claim 23, characterized in that, The drying temperature is 60~80℃.

29. The application of the uranium adsorbent according to claim 23, characterized in that, The drying time is 6-12 hours.

30. The application of the uranium adsorbent according to claim 8, characterized in that, The preparation method of the uranium adsorbent includes the following steps: (1) Mix keggin-type heteropoly acid, chromium nitrate nonahydrate, terephthalic acid and water, and stir at a speed of 400~550 r / min for 30~50 min until the mixture is homogeneous to obtain a mixed solution; Wherein, the keggin-type heteropolyacid is phosphotungstic acid and / or phosphomolybdic acid, the ratio of the keggin-type heteropolyacid to the mixed solution is (1.6~13.5):1 mg / mL; the ratio of the chromium nitrate nonahydrate to the mixed solution is (25~40):1 mg / mL; the molar ratio of the chromium nitrate nonahydrate to terephthalic acid is (1~1.2):1; (2) The mixed solution described in step (1) is subjected to hydrothermal reaction at 180~200℃ for 18~24h to obtain hydrothermal reaction product; then the hydrothermal reaction product is cooled, washed at least 3 times, and finally vacuum dried at 60~80℃ and -1~0.6bar for 6~12h to obtain the uranium adsorbent.

31. The application according to claim 1, characterized in that, The uranium adsorbent is used to adsorb uranium in uranium-containing wastewater. The adsorption process includes: first mixing the uranium-containing wastewater to be treated and the uranium adsorbent to obtain a mixed solution A, and then adjusting the pH value of the mixed solution A for adsorption.

32. The application according to claim 31, characterized in that, The ratio of the uranium-containing wastewater to be treated to the uranium adsorbent is (25~75):1mL / mg.

33. The application according to claim 31, characterized in that, The pH of the mixture A is adjusted to 5-9.

34. The application according to claim 33, characterized in that, The pH value of the mixture A is 5.5~6.

5.

35. The application according to claim 31, characterized in that, The adsorption temperature is 25℃~45℃.

36. The application according to claim 31, characterized in that, The adsorption time is 12-24 hours.

37. The application according to claim 31, characterized in that, The adsorption process includes: first, mixing the uranium-containing wastewater to be treated and the adsorbent at a ratio of (25~75):1 mL / mg to obtain a mixed solution A; then adjusting the pH of the mixed solution A to 5~9; and adsorbing at 25℃~45℃ for 12~24h.

38. The application according to claim 1, characterized in that, The uranium adsorbent is used to extract uranium from seawater. The extraction includes: mixing seawater and the uranium adsorbent to obtain a mixture B, and finally adjusting the pH value of the mixture B for extraction.

39. The application according to claim 38, characterized in that, The ratio of seawater to uranium adsorbent is (200~400):1 mL / mg.

40. The application according to claim 38, characterized in that, The pH of the mixture B is adjusted to 5-9.

41. The application according to claim 40, characterized in that, The pH value of the mixture B is 5.5~6.

5.

42. The application according to claim 38, characterized in that, The extraction temperature is 25℃~45℃.

43. The application according to claim 38, characterized in that, The extraction time is 12-24 hours.

44. The application according to claim 38, characterized in that, The extraction process includes: mixing the seawater and uranium adsorbent at a ratio of (200~400) mL: 1 mg to obtain mixture B, and finally adjusting the pH of mixture B to 5~9, and extracting at 25℃~45℃ for 12~24 h.

45. The application according to claim 1, characterized in that, After the uranium adsorbent is saturated, it is desorbed. The desorption solvent includes any one or a combination of at least two of hydrochloric acid, nitric acid, sodium carbonate, or sodium bicarbonate.

46. ​​The application according to claim 45, characterized in that, The desorption solvent is hydrochloric acid.

47. The application according to claim 45, characterized in that, The concentration of the hydrochloric acid is 0.005~0.5 mol / L.

48. The application according to claim 47, characterized in that, The concentration of the hydrochloric acid is 0.005~0.1mol / L.

49. The application according to claim 45, characterized in that, The desorption time is 1~10s.

Citation Information

Patent Citations

  • Adsorbent for uranium in uranium-bearing wastewater and adsorption method of uranium-bearing wastewater

    CN108854976A

  • Uranium adsorbent and preparation method and application thereof

    CN113231048A

  • Method for catalytically synthesizing bisphenol F with phosphotungstic acid modified metal organic frame

    CN104211580A

  • Heteropolyacid catalyst and preparation method thereof

    CN108114749A