A surface particle coating device and control method thereof
Through the design of the lifting drive and discharge part of the surface layer particle coating device, the automated cladding of imitation stone products is realized, solving the problems of material dispersion control and uniformity, improving production efficiency and product quality, and reducing costs .
Patent Information
- Application Number
- CN202410400206.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-03
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-04-03
AI Technical Summary
The existing surface coating methods for imitation stone products have insufficient material dispersion control and uniformity, resulting in unstable surface quality of the product and low operating efficiency.
A surface layer particle coating device is designed, including a lifting drive part and a material discharge part. By accurately controlling the lifting and material dispersion of the hopper, it realizes fully automated operation, and the thickness, hardness and attachment of the protective surface layer are monitored in real time through the detection equipment. Focus on adjusting raw material ratio and curing conditions to ensure product quality.
It improves production efficiency, reduces manual operation costs, ensures uniformity and stability of product surface quality, reduces waste of raw materials, and improves production adaptability and flexibility.
Smart Images

Figure CN118342694B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of intelligent control technology, and in particular to a surface particle coating device and a control method thereof. Background Art
[0002] At present, some methods for protecting the surface layer of imitation stone products have been proposed and applied. These methods mainly cover the surface of the substrate with a foam belt or a plastic film belt to form a protective surface layer to achieve the protective effect of the surface layer of imitation stone. However, the existing methods have some problems and shortcomings.
[0003] When coating, the traditional coating method is not convenient to control the amount and uniformity of the material, which easily leads to unstable surface quality of the product and waste. In addition, the existing coating device is not convenient for the lifting and lowering control of the hopper during operation, which easily leads to low work efficiency. Therefore, further improvement is urgently needed. Summary of the invention
[0004] The technical problem to be solved by the present invention is to provide a surface particle coating device and a control method thereof, which improves production efficiency and reduces manual operation costs.
[0005] In order to solve the above technical problems, the technical solution of the present invention is as follows:
[0006] In a first aspect, a surface particle coating device comprises:
[0007] First pillar;
[0008] A second column, parallel to the first column;
[0009] A lifting drive unit, arranged on the first column and the second column;
[0010] The hopper has two ends connected to the lifting drive unit, so that the lifting drive unit drives the hopper to move upward or downward relative to the first column and the second column.
[0011] The material discharging part is located in the hopper and connected with the lifting driving part.
[0012] Furthermore, the lifting drive unit includes:
[0013] A first motor is disposed on the first column, an output shaft of the first motor is connected to a first coupling, and the first coupling is connected to two worm gears;
[0014] One end of the first screw rod is connected to the first coupling through a worm, and the other end is threadedly connected to the first nut, and the first nut is arranged on the second support plate.
[0015] Furthermore, the lifting drive unit also includes:
[0016] A synchronizing shaft, one end of which is connected to the first coupling through another worm, and the other end of which is connected to the second coupling, and the second coupling is arranged on the first column;
[0017] One end of the second screw rod is connected to the second coupling through a worm, and the other end is threadedly connected to the second nut, and the second nut is arranged on the first support plate.
[0018] Furthermore, a first slide rail is provided on one side of the first column; a second slide rail is provided on a side of the second column opposite to the first column; and the lifting drive unit further includes:
[0019] A second support, connected to one end of the hopper and to one end of the first support plate;
[0020] A plurality of second sliders are provided, wherein the plurality of second sliders are provided on the second support, and the second sliders are provided with sliding grooves matching with the second slide rails, so that the second sliders are slidably connected with the second slide rails;
[0021] A first support, connected to the other end of the hopper and to one end of the second support plate;
[0022] The first sliding block is arranged on the first support, and the first sliding block is provided with a sliding groove matched with the first sliding rail, so that the first sliding block is slidably connected with the first sliding rail.
[0023] Furthermore, a partition is provided on the hopper so that the partition divides the hopper into a plurality of separate spaces.
[0024] Furthermore, the discharge part comprises:
[0025] A variable frequency motor, fixedly connected to the second support;
[0026] The blanking shaft has one end penetrating the hopper and connected to the output end of the variable frequency motor, and the other end penetrating the hopper and connected to the bearing seat fixed on the first support.
[0027] Furthermore, the blanking shaft is located in the blanking trough, and a plurality of slot holes are arranged on the blanking shaft.
[0028] Furthermore, a transverse cover plate is provided on the hopper, and a vertical cover plate is provided on the first column.
[0029] Furthermore, four first sliding blocks are provided, and every two first sliding blocks are provided on one first sliding rail, and the two first sliding rails are parallel to each other;
[0030] Four second sliding blocks are provided, and every two second sliding blocks are provided on one second sliding rail, and the two second sliding rails are parallel to each other.
[0031] Furthermore, the slot hole and the blanking shaft are integrally formed.
[0032] In a second aspect, a control method for a surface particle coating device is provided, the method comprising:
[0033] Add the configured granular material into the hopper;
[0034] By controlling the lifting drive unit, the hopper is raised or lowered to a predetermined position along the first column and the second column;
[0035] When the lifting drive unit lifts the hopper to a predetermined position, the discharge unit is controlled to open, so that the material falls from the hopper chute, and the material is spread on the surface of the substrate to form a protective surface layer;
[0036] Curing the protective surface layer, and using testing equipment to test the thickness, hardness, and adhesion index of the cured protective surface layer to determine whether it meets the requirements;
[0037] If the test results do not meet the standards, adjust the raw material ratio or curing conditions and repeat the operation until the quality indicators of the protective surface layer meet the requirements.
[0038] The above solution of the present invention includes at least the following beneficial effects:
[0039] The above-mentioned scheme of the present invention realizes fully automated operation from raw material configuration, mixing and stirring to coating curing, greatly improves production efficiency and reduces manual operation costs. By accurately controlling the lifting mechanism and the material dropping device, the material can be accurately sprinkled on the surface of the substrate to form a uniform protective surface layer, avoiding errors that may be caused by manual operation. The present invention can timely discover and adjust problems in the production process by real-time detection of key indicators such as the thickness, hardness, and adhesion of the protective surface layer to ensure that product quality always meets the requirements. When the test results do not meet the standards, this method allows the adjustment of the raw material ratio or the curing conditions, and the operation is repeated until the quality indicators of the protective surface layer meet the requirements, showing good production adaptability and flexibility. By accurately controlling the use of materials and recycling the protective surface layer that does not meet the standards, this method effectively reduces the waste of raw materials and reduces production costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Figure 1 It is a stereoscopic view of the surface particle coating device of the present invention.
[0041] Figure 2 The surface particle coating device of the present invention Figure 1A three-dimensional image after the vertical cover plate is removed.
[0042] Figure 3 The surface particle coating device of the present invention Figure 1 A three-dimensional image from another perspective after the vertical cover plate is removed.
[0043] Figure 4 The surface particle coating device of the present invention Figure 1 A three-dimensional view with the vertical cover plate and the horizontal cover plate removed.
[0044] Figure 5 It is a partial structural schematic diagram of the surface particle coating device of the present invention.
[0045] Figure 6 The surface particle coating device of the present invention Figure 5 A schematic diagram of the enlarged structure in the middle.
[0046] Figure 7 It is a partial structural schematic diagram of the surface particle coating device of the present invention from another viewing angle.
[0047] Figure 8 The surface particle coating device of the present invention Figure 7 Enlarged schematic diagram of the structure at point B in the middle.
[0048] Fig. 9 It is a schematic diagram of the position of the material drop chute of the surface particle coating device of the present invention.
[0049] Explanation of the reference numerals in the accompanying drawings: 1. vertical cover plate; 2. horizontal cover plate; 21. partition plate; 22. hopper; 221. blanking chute; 23. first support plate; 24. first support seat; 25. first slide block; 26. second support plate; 27. second support seat; 28. second slide block; 3. first column; 31. first slide rail; 4. lifting drive unit; 41. first motor; 42. first screw rod; 43. first coupling; 44. first nut; 45. synchronous shaft; 46. second coupling; 47. second screw rod; 48. second nut; 5. second column; 51. second slide rail; 6. discharge unit; 61. variable frequency motor; 62. blanking shaft; 621. slot. DETAILED DESCRIPTION
[0050] The exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although the exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments set forth herein. On the contrary, these embodiments are provided to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art.
[0051] like Figures 1 to 9As shown, an embodiment of the present invention provides a surface particle coating device, comprising:
[0052] First column 3;
[0053] A second column 5, parallel to the first column 3;
[0054] A lifting drive unit 4 is provided on the first column 3 and the second column 5;
[0055] The hopper 22 has two ends connected to the lifting drive unit 4, so that the lifting drive unit 4 drives the hopper 22 to move upward or downward relative to the first column 3 and the second column 5.
[0056] The discharging portion 6 is located in the hopper 22 and connected to the lifting driving portion 4 .
[0057] In the embodiment of the present invention, the device realizes the smooth lifting and lowering of the hopper 22 along the first column 3 and the second column 5 by setting the lifting drive unit 4. This design not only ensures the stability and accuracy of the lifting process of the hopper 22, but also improves the work efficiency and reduces the difficulty of operation. Secondly, the discharge part 6 is located in the hopper 22 and is connected to the lifting drive unit 4, so that the material can be discharged accurately and quickly at the predetermined position. This structural design not only ensures the uniformity and continuity of the material discharge, but also avoids the waste and pollution of the material, and improves the utilization rate of the raw materials. In addition, since the first column 3 and the second column 5 are parallel to each other, it provides greater flexibility and stability for the lifting and lowering of the hopper 22, ensuring the flatness and quality of the surface particle coating. Therefore, the surface particle coating device not only improves the work efficiency and raw material utilization, but also ensures the surface quality and flatness of the product.
[0058] like Figures 1 to 9 As shown, the lifting drive unit 4 includes:
[0059] A first motor 41 is disposed on the first column 3, wherein an output shaft of the first motor 41 is connected to a first coupling 43, and the first coupling 43 is connected to two worm gears;
[0060] A first screw rod 42, one end of which is connected to a first coupling 43 via a worm, and the other end of which is threadedly connected to a first nut 44, wherein the first nut 44 is disposed on the second support plate 26;
[0061] A synchronization shaft 45, one end of which is connected to the first coupling 43 through another worm, and the other end of which is connected to the second coupling 46, and the second coupling 46 is arranged on the first column 3;
[0062] A second screw rod 47, one end of which is connected to the second coupling 46 through a worm, and the other end of which is threadedly connected to a second nut 48, wherein the second nut 48 is disposed on the first support plate 23; a first slide rail 31 is disposed on one side of the first column 3; a second slide rail 51 is disposed on the side of the second column 5 opposite to the first column 3; the lifting drive unit 4 further includes:
[0063] A second support 27 connected to one end of the hopper 22 and to one end of the first support plate 23;
[0064] A plurality of second sliders 28 are provided, and the plurality of second sliders 28 are provided on the second support 27, and a slide groove matching with the second slide rail 51 is provided on the second slider 28, so that the second slider 28 is slidably connected with the second slide rail 51;
[0065] A first support 24 is connected to the other end of the hopper 22 and to one end of the second support plate 26;
[0066] The first sliding block 25 is disposed on the first support 24 , and a sliding groove matched with the first sliding rail 31 is disposed on the first sliding block 25 , so that the first sliding block 25 is slidably connected with the first sliding rail 31 .
[0067] In the embodiment of the present invention, the first coupling 43 is driven by the first motor 41, and then the two worms are driven to rotate simultaneously, so that the first screw 42 and the second screw 47 can realize synchronous rotation through their respective screw nuts. This design ensures the stability and synchronization of the hopper 22 during the lifting process, and avoids the device failure or product quality problems caused by the asynchronous lifting. Secondly, the setting of the first slide rail 31 and the second slide rail 51, in conjunction with the first slider 25 and the second slider 28, provides a smooth and precise guide for the lifting of the hopper 22. This sliding connection mode not only reduces the friction resistance during the lifting process, but also improves the wear resistance and service life of the device. In addition, the hopper 22 is firmly connected to the lifting drive unit 4 through the first support 24 and the second support 27, ensuring that the hopper 22 will not shake or deflect during the lifting process, thereby ensuring the accuracy and continuity of material discharge. Therefore, the design of the lifting drive unit 4 not only improves the stability and work efficiency of the device, but also ensures the surface quality and precision of the product. It has a compact structure, simple operation and convenient maintenance.
[0068] like Figures 1 to 9 As shown, the hopper 22 is provided with a partition 21, so that the partition 21 divides the hopper 22 into a plurality of separate spaces; the discharge portion 6 includes:
[0069] A variable frequency motor 61 is fixedly connected to the second support 27;
[0070] One end of the blanking shaft 62 passes through the hopper 22 and is connected to the output end of the variable frequency motor 61 , and the other end passes through the hopper 22 and is connected to a bearing seat 63 fixed on the first support 24 .
[0071] In the embodiment of the present invention, by setting a partition 21 on the hopper 22, the interior of the hopper 22 is divided into a plurality of separate spaces, so that materials of different types or properties can be stored and transported separately, avoiding mixing and contamination between materials. At the same time, the plurality of separate spaces can also be flexibly adjusted as needed to adapt to different production needs and material characteristics. Secondly, the discharge part 6 adopts the method of driving the blanking shaft 62 by the variable frequency motor 61 to achieve precise control of material discharge. The variable frequency motor 61 can adjust the speed and direction according to actual needs, thereby controlling the rotation speed and direction of the blanking shaft 62, and then controlling the discharge amount and uniformity of the material. This design not only improves the accuracy and continuity of material discharge, but also avoids waste and pollution of materials. In addition, one end of the blanking shaft 62 is connected to the output end of the variable frequency motor 61, and the other end penetrates the hopper 22 and is connected to the bearing seat 63 fixed on the first support 24. This structural design makes the blanking shaft 62 more stable and reliable during rotation, reduces the possibility of failure, and improves the service life of the device. Therefore, the design of the hopper 22 and the discharge part 6 not only improves the flexibility and adaptability of the device, but also ensures the accuracy and continuity of material discharge. It has a compact structure, simple operation and convenient maintenance.
[0072] like Figures 1 to 9 As shown, the blanking shaft 62 is located in the blanking trough 221, and a plurality of slots 621 are provided on the blanking shaft 62; a transverse cover plate 2 is provided on the hopper 22, and a vertical cover plate 1 is provided on the first column 3; four first slide blocks 25 are provided, and every two first slide blocks 25 are provided on one first slide rail 31, and the two first slide rails 31 are parallel to each other;
[0073] Four second sliding blocks 28 are provided, and every two second sliding blocks 28 are provided on one second slide rail 51 , and the two second slide rails 51 are parallel to each other; the slot 621 and the blanking shaft 62 are integrally formed.
[0074] In the embodiment of the present invention, the blanking shaft 62 is located in the blanking trough 221, and a plurality of slots 621 are provided on the blanking shaft 62. Such a design enables the material to be spread more evenly on the surface of the substrate through the slots 621, thereby improving the uniformity and efficiency of spreading. At the same time, the slots 621 are integrally formed with the blanking shaft 62, thereby enhancing the integrity and stability of the structure. The arrangement of the horizontal cover plate 2 and the vertical cover plate 1 effectively prevents the splashing and scattering of the material during the spreading process, protects the working environment and the safety of the operator, and also reduces the waste of the material. The number and layout design of the first slider 25 and the second slider 28 make the hopper 22 more stable and smooth during the lifting process. The four first sliders 25 are respectively arranged on two mutually parallel first slide rails 31, and the four second sliders 28 are respectively arranged on two mutually parallel second slide rails 51. Such a design not only improves the smoothness of sliding, but also enhances the carrying capacity and stability of the device. The integral molding design of the slots 621 and the blanking shaft 62 not only simplifies the manufacturing process, but also improves the strength and durability of the components. This structural design reduces the number of connection points between components, thereby reducing the possibility of failure and extending the service life of the device. The outer diameter of the blanking shaft 62 is just slightly smaller than the lateral width of the blanking trough 221, so that the blanking shaft 62 can just rotate in the blanking trough 221, so that during the rotation, the granular material can fall into the slot 621. When the slot 621 rotates to a downward direction, the granular material will automatically fall due to its own weight. The depth of the slot 621 is shallower, so that the granular material can be stored without delaying its falling.
[0075] In a second aspect, a control method for a surface particle coating device is provided, the method comprising:
[0076] Step 11, adding the configured granular material into the hopper 22;
[0077] Step 12, by controlling the lifting drive unit 4, the hopper 22 rises or descends along the first column 3 and the second column 5 to a predetermined position;
[0078] Step 13, after the lifting drive unit 4 lifts the hopper 22 to a predetermined position, the discharge unit 6 is controlled to open, so that the material falls from the drop chute 221 in the hopper 22, and the material is spread on the surface of the substrate to form a protective surface layer;
[0079] Step 14, curing the protective surface layer, and using a detection device to detect the thickness, hardness, and adhesion index of the cured protective surface layer to determine whether the requirements are met;
[0080] Step 15: If the test result does not meet the standard, adjust the raw material ratio or curing conditions and repeat the operation until the quality index of the protective surface layer meets the requirement.
[0081] In the embodiment of the present invention, by adding the configured particulate material into the hopper 22, the centralized storage and transportation of the material is realized, which is convenient for the subsequent spreading operation. This control method simplifies the operation process and improves the work efficiency. Secondly, by controlling the lifting drive unit 4, the hopper 22 is raised or lowered to a predetermined position along the first column 3 and the second column 5, and the precise control of the lifting and lowering of the hopper 22 is realized. This control method not only improves the accuracy and stability of the lifting, but also avoids the impact and vibration during the lifting process, and protects the safety of the device and the material. Thirdly, when the lifting drive unit 4 lifts the hopper 22 to the predetermined position, the discharge unit 6 is controlled to open, so that the material falls from the drop chute 221 in the hopper 22, and the material is spread on the surface of the substrate to form a protective surface layer. This control method realizes the uniform spreading of the material and improves the flatness and quality of the protective surface layer. In addition, by curing the protective surface layer and using the detection equipment to detect the thickness, hardness, adhesion and other indicators of the cured protective surface layer, it is judged whether it meets the requirements, and the comprehensive control of the quality of the protective surface layer is realized. If the test results do not meet the standards, the raw material ratio or curing conditions are adjusted and the operation is repeated until the quality index of the protective surface layer meets the requirements. This feedback adjustment mechanism ensures the quality stability and consistency of the product.
[0082] In another preferred embodiment of the present invention, the controller is electrically connected to the first motor 41 and the variable frequency motor 61 respectively, so that the first motor 41 and the variable frequency motor 61 are controlled by the controller to achieve accurate control of the lifting of the hopper, wherein, when specifically controlled, the specific control process includes:
[0083] Determine the target position according to the need for the hopper to be lowered to a specific position in order to evenly spread the granular material;
[0084] The position sensor is used to monitor the current position of the hopper. The controller uses the difference between the target position and the current position (position error) to A control output value Ou is calculated, which is used to adjust the speed and acceleration of the motor to control the movement of the hopper. e(t) represents the position error, that is, the difference between the target position and the current position, and K p Represents proportional gain, K i Indicates the integral gain, K d represents the differential gain, A represents the amplitude, ω represents the angular frequency, represents the phase shift, K f represents the enhancement term coefficient, t represents time, and e(τ) represents the position error at time τ.
[0085] According to the control output value Ou, the working states (such as speed and acceleration) of the first motor 41 and the variable frequency motor 61 are adjusted in real time, and the position of the hopper is continuously monitored.
[0086] In another preferred embodiment of the present invention, before step 11, the following steps may be included:
[0087] Step 111, mixing polylactic acid plastic and plasticizer in proportion to form a colloid;
[0088] Step 112, conveying the colloid to an extruder for processing to form a long and thin strip;
[0089] Step 113, granulating the elongated strips into granules. During the granulation process, the size distribution of the granules is detected and the granulation parameters are adjusted so that the size distribution of the obtained granules meets the requirements;
[0090] Step 114, drying the prepared particles in a dryer to obtain dried particles;
[0091] Step 115, sieving the dried particles to remove the particles to obtain a final particle material.
[0092] In an embodiment of the present invention, polylactic acid plastic and plasticizer are mixed in proportion to form a colloid, thereby ensuring the uniformity and consistency of the raw materials, conveying the colloid to an extruder for processing to form elongated strips, and then granulating the elongated strips. This streamlined operation improves processing efficiency and is also conducive to automated production. During the granulation process, the size distribution of the particles is detected and the granulation parameters are adjusted so that the size distribution of the obtained particles meets the requirements. The prepared particles are dried in a dryer to remove moisture from the particles, enhance the stability of the material, and reduce problems such as agglomeration and deterioration that may occur during storage and use. The dried particles are screened to screen out particles that do not meet the requirements, further improving the purity and quality of the granular material and ensuring the performance and appearance of the final product.
[0093] In another preferred embodiment of the present invention, the above step 111 may include:
[0094] The amount of plasticizer (citrate ester) added was determined to be 10% of the weight of the polylactic acid. The polylactic acid particles and epoxy soybean oil were placed in a mixer at a ratio of 9:1 and mixed at 50°C for 1 hour to ensure that the plasticizer was evenly distributed in the polylactic acid particles. During the mixing process, after mixing at 50°C for 1 hour, the mixing temperature was increased to 60°C. This temperature helped to evenly distribute the plasticizer without causing degradation of the polylactic acid. At the same time, the stirring speed was set to 400rpm.
[0095] In a preferred embodiment of the present invention, the above step 112 may include:
[0096] Step 1121, quantitatively supplying the colloid into a silo of an extruder through a feeding device, and adjusting the temperature parameters of the extruder so that the temperature of each zone meets the processing temperature of the colloid;
[0097] Step 1122, controlling the screw speed of the extruder to adjust the speed of the extruder, and melt the gelatinous material and extrude the melt;
[0098] Step 1123, the melt is molded through a die device, and the die aperture is set to 1-5 mm to obtain an elongated extruded strip.
[0099] In an embodiment of the present invention, the colloid is quantitatively supplied to the extruder silo, and the temperature parameters are adjusted to meet the processing temperature. The quantitative feeding is beneficial to control the amount of raw materials used in each processing and ensure the output. The temperature parameters are adjusted to fully melt the colloid and ensure the extrusion effect; the extruder screw speed is controlled to adjust the extrusion speed, and the colloid is melted and extruded. The screw speed is controlled to accurately adjust the extrusion speed to obtain a uniform melt, so that the colloid is completely melted, which is beneficial to extrusion molding; the melt is molded through a die head device to obtain a slender extruded strip. The die head aperture is set reasonably to obtain a slender strip product with uniform specifications. Extrusion molding can enable the product to obtain better shape stability. Therefore, the present invention standardizes the extrusion process parameters, realizes quantitative feeding, complete melting and standardized extrusion of the colloid, which is beneficial to obtain slender strips with uniform shape, and provides high-quality raw materials for subsequent pelletizing, thereby ensuring the quality of the finished product.
[0100] In another preferred embodiment of the present invention, the above step 1121 may include: setting industrial cameras at several positions of the colloid conveying pipeline to take images of the colloid; Extract the edge features of the colloid image, where E is the image edge feature value, is the gradient magnitude at the image coordinate (i, j), w1(i, j) is the weight coefficient of the pixel (i, j), n1 is the number of rows in the image, m is the number of columns in the image, τ E is the threshold of the gradient amplitude; according to the edge features of the colloid image, Extract texture features, where CON is the contrast of the image, f(i1, j1) represents the grayscale value at the image coordinate (i1, j1), d is the distance between adjacent pixels, w2(i1, j1) is the weight coefficient of the pixel (i1, j1), τ CON is the contrast threshold; i1 is the row index of the image pixel, ranging from 1 to n1-1; j1 is the column index of the image pixel, ranging from 1 to m.
[0101] In another preferred embodiment of the present invention, an image sample library of colloid morphological changes is constructed based on edge features and texture features, including image data in different morphological states, and the edge features and texture features of each sample are used to form a feature vector as data in the sample library, which includes feature vectors of samples of different morphologies and corresponding state labels; according to d i =w3 T K(x,x i )w3 obtains the similarity d between the real-time image and the i-th sample i ,in, Where K(·) is a kernel function, T represents the transposition operation, σ represents the variance parameter in the Gaussian kernel function, n2 represents the total number of sample images, and x is the feature vector of the real-time image. i is the feature vector of the i-th sample image in the sample library, n2 is the number of samples, w3 is the weight control vector, if the real-time image is j The most similar, then the morphological state of the real-time image is judged to be the same as the sample x j same.
[0102] In another preferred embodiment of the present invention, according to the morphological state s of the real-time image and the weight control vector w3, by Adjust the feeding speed by Adjust the feeding time by Adjust the feeding amount, where v, t, and m are the adjusted feeding speed, time, and amount parameters, v0, t0, and m0 are the original parameter values, s0 is the reference state of the normal form, and k v , k t , k m They are all weighted feedback control coefficient vectors of state deviations to achieve precise control of the feeding process and ensure the filling degree of the colloid in the silo.
[0103] In another preferred embodiment of the present invention, by Calculate the evaluation index U of the density uniformity of the colloid, where: According to the evaluation index U of the uniformity of the density of the colloid, Calculate the adjusted stirring speed in the silo to achieve uniform pre-plasticization of the colloid in the silo, where i1 is the detection point in the silo, is the detected density value of the colloid, n3 is the number of detection points, and w4 is the weight vector.
[0104] In a preferred embodiment of the present invention, the above step 113 may include:
[0105] Step 1131, conveying the long and thin extruded strips to a pelletizer through a conveying device for pelletization, and adjusting the cutter speed of the pelletizer and the feeding rate of the long and thin strips according to product requirements to control the cutting length of the pellets;
[0106] Step 1132, screening the cut particles by a screening device, collecting the screened particles of each size respectively, and in the granulation process, detecting the distribution of particle size by an online detection system, and comparing it with the standard distribution to obtain the detection result, and optimizing and adjusting the operating parameters of the pelletizer according to the detection result, so that the particle size distribution meets the requirements;
[0107] Step 1133, collect the particles of each size class that have been adjusted to meet the requirements, mix them to the required ratio, and obtain the finished particle product.
[0108] In an embodiment of the present invention, in step 1131, the conveying device can continuously and stably convey the extruded strip to the granulator to ensure the supply of raw materials for subsequent processes. The parameters of the granulator can be adjusted to control the cutting length of the particles and obtain particles with different specifications. In step 1132, screening can separate particles of different particle sizes according to particle size. The online detection system can monitor the particle size distribution in real time and compare it with the standard distribution to achieve closed-loop control to ensure that the particle size distribution meets the requirements. In step 1133, particles of each particle size are collected and mixed in proportion to obtain finished particle products with different formulation requirements. After passing the quality inspection, they are packaged to ensure product quality. The present invention realizes the monitoring and regulation of the granulation process, ensures the quality of the particle product, and improves the controllability and automation level of the production process.
[0109] In another preferred embodiment of the present invention, in step 1131, when specifically implemented, it may include: the speed of the pelletizer cutter is n3, the feeding rate of the sliver is v1, and the product length requirement is L, then Where n0 is the original rotation speed and feeding rate, L0 is the reference product length, and is the control coefficient vector, and w5 is the weight vector.
[0110] In another preferred embodiment of the present invention, the above step 1132 may include:
[0111] Step 11321, the image acquisition module acquires an image of the particle flow process;
[0112] Step 11322, processing the acquired image, identifying each particle and calculating the projected area;
[0113] Step 11323, calculating the particle size distribution of the particles based on the projected area data of all particles;
[0114] Step 11324, comparing the measured particle size distribution with the set standard particle size distribution to obtain a deviation result between the measured particle size and the standard particle size;
[0115] Step 11325, based on the deviation result, the control module calculates new granulation parameter setting values, and feeds the calculated new granulation parameter setting values back to the control system of the granulator to complete the closed-loop control of the parameters until the particle size distribution is stabilized within the standard distribution range.
[0116] In an embodiment of the present invention, in step 11321, image acquisition can obtain real-time images during the granulation process. In step 11322, image processing can identify each particle, calculate the projected area, and obtain the particle size data of all particles. In step 11323, the particle size distribution is calculated, which can intuitively reflect the overall particle size of the current particles. In step 11324, the measured actual particle size distribution is compared with the standard distribution, and the deviation of the current particle size distribution can be quantified. In step 11325, new parameters are calculated based on the deviation results to complete closed-loop control, so that the actual particle size distribution gradually approaches the standard distribution, thereby ensuring the quality of granulation. The present invention realizes image monitoring and intelligent control of the granulation process, continuously optimizes the parameters of granulation to obtain an ideal particle size distribution, and improves the automation and precision of the process.
[0117] In another preferred embodiment of the present invention, in step 11322, the acquired image is denoised to obtain a denoised image, and the denoised image is segmented to obtain a segmented image. Calculate the weight w of the pth pixel in the image p , according to the weight w p And the segmented image R i ,pass Calculate the area N of the entire particle region i , where h(·) is the calculation weight w p function, γ1 and γ2 are parameters, I p Represents the image intensity value of the pth pixel, R p Indicates the area where the p-th pixel is located.
[0118] In step 11323, in this step, the particles generated during the granulation process are monitored in real time using image processing technology. The images of the particles are captured by the image acquisition module, and then the projected areas of these particles are analyzed. The projected area of each particle is calculated by the image processing algorithm, and the size (particle diameter) of the particles can be estimated based on these area data. Based on the size data of all particles, a particle size distribution diagram of the particles is constructed, which shows the proportion or number of particles of different sizes. Step 11324 compares the actual particle size distribution obtained from step 11323 with the pre-set standard particle size distribution. This comparison can reveal the deviation between the particle size distribution in actual production and the ideal (or standard) distribution. By quantifying this deviation, the gap between the current production status and the desired target can be clarified. Step 11325, based on the deviation results obtained in step 11324, the control module calculates new granulation parameters (such as the tool speed of the pelletizer, the feed rate, etc.) to reduce or eliminate this deviation. The new parameter setting values are fed back to the control system of the pelletizer to adjust the production process until the particle size distribution is stabilized within the standard distribution range, thereby achieving precise control and optimization of the production process. For example, suppose the production goal is to produce polylactic acid plastic particles with a particle size range of 2mm to 4mm. After the production starts, step 11323 finds through image acquisition and processing that the particle size distribution of the produced particles is mainly concentrated in the range of 1.5mm to 3.5mm, which deviates from the standard distribution. In step 11324, through analysis and comparison, it is concluded that the average particle size of the current particles is small, and the production parameters need to be adjusted to increase the particle size. In step 11325, based on the deviation results, the control module calculates that the tool speed of the pelletizer needs to be increased and the feed rate needs to be slowed down. These new parameters are fed back to the control system of the pelletizer for adjustment. After a period of production and adjustment, the particle size distribution is evaluated again and it is found that it has stabilized within the expected range of 2mm to 4mm, indicating that the production process has been effectively controlled and optimized.
[0119] In a preferred embodiment of the present invention, in the above step 114, after granulation, the particles usually contain a certain amount of moisture, which may be introduced during the granulation process or contained in the raw materials themselves. Excessive moisture will affect the storage stability and subsequent processing performance of the particles, and may cause the particles to agglomerate during storage. Therefore, the prepared particles need to be placed in a dryer for drying to remove excess moisture. In step 115, the dried particles need to be sieved to remove particles that do not meet the product size requirements. This includes particles that are too large or too small, as well as any irregular particles that may be formed during the production process. The sieving process is carried out using a series of sieves with different apertures, and the specifications of the sieves can be set according to the final use and size requirements of the particles. Screening can not only remove unqualified particles, but also classify the particles according to different size ranges as needed. For example, polylactic acid (PLA) particles are produced. After granulation, the particles contain about 5% moisture. This moisture content is too high for preservation because it may produce steam during the preservation process, affecting the preservation quality. In step 114, the particles are placed in a dryer and dried at a temperature of 60°C for 4 hours to reduce the moisture content to less than 1%, which meets the preservation requirements. Subsequently, in step 115, in order to ensure smoothness during the preservation process and high-quality finished products, the dried particles are screened through a series of screens. The screens used have an aperture of 1mm and 3mm to remove particles outside this size range. After screening, a batch of particles with a particle size between 1mm and 3mm are obtained. The size distribution of this batch of particles is suitable for use and can ensure that the preserved product has good details and strength.
[0120] In an embodiment of the present invention, step 14, in this step, the protective surface layer that has been formed needs to undergo a series of quality tests to ensure that its performance meets specific requirements. These tests include: thickness, measuring the uniformity of the protective surface layer and whether it reaches the designed thickness, which is crucial to the protective performance. Hardness, determining the compression and scratch resistance of the protective layer, as well as its performance stability under different conditions. Adhesion, evaluating the bonding strength between the protective layer and the substrate, which is related to the durability and protective ability of the protective layer during use. Step 15, if the test results in step 14 show that any indicator of the protective surface layer does not meet the predetermined standard, it is necessary to make adjustments to the production process, including: modifying the parameters of the curing process (such as temperature, time, ambient humidity, etc.) to optimize the performance of the protective surface layer. After adjustment, the test of step 14 needs to be repeated until all quality indicators meet the requirements. For example, the thickness of the protective surface layer measured by the testing instrument is 0.25mm (the standard is 0.3mm) and the hardness is 5H (the standard is 6H), and the adhesion test shows that the adhesion between the protective surface layer and the base layer is good and meets the requirements. Because the thickness and hardness did not meet the predetermined standards, the production team decided to adjust the raw material ratio in step 15, increase the proportion of components that thicken the film and enhance the hardness, and fine-tune the exposure time of the UV curing lamp to enhance the hardness of the film. After the adjustment, the thickness and hardness test was performed again. This time, the thickness of the protective surface layer reached 0.3mm and the hardness was increased to 6H, meeting all the predetermined quality standards. Through this process, it is ensured that the protective surface layer produced by it can meet the design requirements and provide excellent screen protection effects.
[0121] The above is a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A surface particle coating device, characterized in that: include: First column (3); A second column (5) parallel to the first column (3); A lifting drive unit (4) is arranged on the first column (3) and the second column (5); The hopper (22) has two ends respectively connected to the lifting drive unit (4) so that the lifting drive unit (4) drives the hopper (22) to move upward or downward relative to the first column (3) and the second column (5) under the drive of the lifting drive unit (4); The material discharge part (6) is located in the hopper (22) and is connected to the lifting drive part (4); the lifting drive part (4) comprises: A first motor (41) is arranged on the first column (3), the output shaft of the first motor (41) is connected to a first coupling (43), and the first coupling (43) is connected to two worm gears; A first screw rod (42) has one end connected to the first coupling (43) via a worm, and the other end is threadedly connected to a first nut (44), wherein the first nut (44) is arranged on the second support plate (26); the lifting drive unit (4) further comprises: A synchronizing shaft (45), one end of which is connected to the first coupling (43) via another worm gear, and the other end of which is connected to the second coupling (46), and the second coupling (46) is arranged on the first column (3); A second screw rod (47) has one end connected to the second coupling (46) via a worm, and the other end threadedly connected to a second nut (48), wherein the second nut (48) is arranged on the first support plate (23); a first slide rail (31) is arranged on one side of the first column (3); a second slide rail (51) is arranged on the side of the second column (5) opposite to the first column (3); the lifting drive unit (4) further comprises: A second support (27) connected to one end of the hopper (22) and to one end of the first support plate (23); A plurality of second sliders (28) are provided, wherein the plurality of second sliders (28) are provided on the second support (27), and a slide groove matching the second slide rail (51) is provided on the second slider (28) so that the second slider (28) is slidably connected to the second slide rail (51); A first support (24) connected to the other end of the hopper (22) and connected to one end of a second support plate (26); A first sliding block (25) is arranged on the first support (24), and a sliding groove matching the first sliding rail (31) is arranged on the first sliding block (25), so that the first sliding block (25) and the first sliding rail (31) are slidably connected; a partition (21) is arranged on the hopper (22), so that the partition (21) divides the hopper (22) into a plurality of separate spaces; the discharge portion (6) comprises: A variable frequency motor (61) fixedly connected to the second support (27); A blanking shaft (62), one end of which passes through the hopper (22) and is connected to the output end of the variable frequency motor (61), and the other end of which passes through the hopper (22) and is connected to a bearing seat (63) fixed on the first support (24); the blanking shaft (62) is located in the blanking trough (221), and a plurality of slot holes (621) are provided on the blanking shaft (62); a transverse cover plate (2) is provided on the hopper (22), and a vertical cover plate (1) is provided on the first column (3); four first slide blocks (25) are provided, and every two first slide blocks (25) are provided on one first slide rail (31), and the two first slide rails (31) are parallel to each other; Four second sliding blocks (28) are provided, and every two second sliding blocks (28) are provided on one second sliding rail (51), and the two second sliding rails (51) are parallel to each other; The controller is electrically connected to the first motor (41) and the variable frequency motor (61) respectively, so that the first motor (41) and the variable frequency motor (61) are controlled by the controller to achieve accurate control of the lifting and lowering of the hopper, wherein the specific control process includes: Determine the target position according to the need for the hopper to be lowered to a specific position in order to evenly spread the granular material; The position sensor is used to monitor the current position of the hopper. The controller uses the difference between the target position and the current position to Calculate a control output value , control output value Used to adjust the speed and acceleration of the motor to control the movement of the hopper, where: Represents the position error, that is, the difference between the target position and the current position, represents the proportional gain, represents the integral gain, represents the differential gain, represents the amplitude, represents the angular frequency, represents the phase shift, represents the enhancement term coefficient, Indicates time, Indicated in Position error at the moment; According to the control output value , adjusting the working states of the first motor (41) and the variable frequency motor (61) in real time, and continuously monitoring the position of the hopper.
2. A control method for a surface particle coating device as claimed in claim 1, characterized in that: The method comprises: Adding the configured granular material into the hopper (22); By controlling the lifting drive unit (4), the hopper (22) is raised or lowered along the first column (3) and the second column (5) to a predetermined position; When the lifting drive unit (4) lifts the hopper (22) to a predetermined position, the discharge unit (6) is controlled to open, so that the material falls from the material drop chute (221) in the hopper (22), and the material is spread on the surface of the substrate to form a protective surface layer; Curing the protective surface layer, and using testing equipment to test the thickness, hardness, and adhesion index of the cured protective surface layer to determine whether it meets the requirements; If the test results do not meet the standards, adjust the raw material ratio or curing conditions and repeat the operation until the quality indicators of the protective surface layer meet the requirements.