A subway tunnel lining stress monitoring and crack leakage early warning mechanism and its working method
Through membrane microelectrode technology and the principle of current focusing, combined with the conductive concrete layer, the problem of difficult monitoring of the internal strain field of the subway tunnel lining is solved, real-time monitoring and early warning of tunnel lining stress and cracks are achieved, and the life of the tunnel lining is extended. and ensured operational safety.
Patent Information
- Application Number
- CN202410474490.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-19
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-04-19
AI Technical Summary
Existing technology is difficult to effectively monitor the internal strain field of the concrete lining of a subway tunnel, resulting in the inability to timely capture and early warning of cracking and leakage disasters in the tunnel lining, affecting the lifespan and operational safety of the tunnel lining.
Using membrane microelectrode technology and current focusing principle, the membrane focusing electrode system is arranged on the surface of the tunnel lining, combined with the conductive concrete layer, to realize the flow of current within a limited depth range inside the lining, obtain the resistivity of the microelectrode, and monitor the stress in real time and early warning.
Real-time monitoring and early warning of subway tunnel lining stress and cracks are achieved, guiding early targeted repairs, extending the life of the tunnel lining, and ensuring operational safety.
Smart Images

Figure CN118376498B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of subway tunnel lining monitoring, in particular to subway tunnel lining stress and crack leakage monitoring. Background Art
[0002] The subway tunnel lining (also known as the pipe segment) is the key foundation and important prerequisite for ensuring tunnel safety. The subway tunnel lining is coupled with the fatigue effect caused by the vibration load of the train, the erosion of the tunnel's thermal-humid environment, and the aging of concrete materials. In addition, the influence of assembly accuracy will inevitably lead to damage accumulation and resistance attenuation, structural deformation exceeding the limit, and even cracking and leakage. If such cracking and leakage cannot be detected in time and effectively controlled, it will accelerate the damage accumulation and resistance attenuation of the subway tunnel lining, seriously reduce the life of the tunnel lining, and make the subway tunnel lining "short-lived", causing significant economic losses and becoming a bottleneck restricting the safety of subway operations. Therefore, the development of subway tunnel lining disease monitoring and health diagnosis technology, the timely capture and accurate early warning of tunnel lining diseases, and then the early targeted repair are of great significance to ensure the normal operation of the subway lining and avoid catastrophic damage, extend the life of the subway tunnel lining, ensure the safety of subway tunnel operations, and serve the development and utilization of urban underground space.
[0003] Existing subway tunnel concrete lining monitoring is based on optical means or geophysical means such as radiation heat, generalized electricity and stress waves. The information obtained is either lining surface information or large defects inside the lining, or based on discrete point data. There is no unified method for the process of increasing field strain inside the tunnel concrete lining to lining cracking or even leakage. Therefore, how to obtain the internal strain field of the tunnel concrete lining in order to provide targeted guidance for the early repair of subway tunnel lining cracks and leakage disasters, and then to carry out tracking and monitoring of the repair effect, has become a technical problem that needs to be solved urgently by those skilled in the art. Summary of the invention
[0004] In view of the above problems, the present invention proposes a method for monitoring the stress of subway tunnel lining and early warning of cracks and leaks. Based on membrane microelectrode technology and current focusing principle, the compressive strain accumulation and tensile cracking of concrete lining can be effectively obtained, so as to carry out real-time monitoring of the stress of subway tunnel lining and early warning of cracks and leaks.
[0005] The technical scheme of the present invention is as follows: the stress monitoring and crack leakage warning mechanism is a membrane focusing electrode system installed on the surface of the subway tunnel lining to be tested, and the membrane focusing electrode system includes a PET film, a plurality of microelectrodes adhered and fixed on the PET film and distributed in an array, an insulating ring fixedly arranged outside each microelectrode and an integral shielding electrode between adjacent insulating rings, and a loop electrode arranged at a position 10 to 20 cm away from the boundary of the subway tunnel lining to be tested along the longitudinal direction of the tunnel; the microelectrode, the shielding electrode and the loop electrode are isolated from the environment inside the tunnel by the PET film, and the detection current flows within a limited depth range inside the lining by current focusing; in actual work, the microelectrode, the shielding electrode and the loop electrode are connected to the focusing detection equipment, so as to control the equipotential condition between the microelectrode and the shielding electrode, and output the resistivity detection result of each microelectrode;
[0006] In particular, considering that this case needs to be arranged together with the construction of the subway tunnel and put into use together with the subway tunnel, the special operating environment in the subway, that is, the stray current generated by the running of the train, will have the following effects due to the setting of this case:
[0007] If the current flows deep inside the lining, it will exceed the capacity of the existing focusing equipment and involve a large area of steel insulation, which reduces the feasibility. If the entire lining is made of conductive concrete, the stray current of the train will leak into the stratum through the conductive concrete, affecting the ground safety. Based on this, this case also made the following special restrictions on the thickness of the conductive concrete:
[0008] The side of the subway tunnel lining to be tested facing the focusing electrode system is set as conductive concrete, and the thickness of the conductive concrete layer is between the thickness of the tunnel lining concrete protective layer and 20-30% of the lining thickness. The steel bars within the thickness range of the conductive concrete layer are sprayed with insulating paint to achieve electrical insulation.
[0009] In this way, while ensuring that the focused detection equipment can stably obtain the resistivity detection results of each microelectrode, it can also ensure that the stray current generated by the train operation will only pass through the local area where the conductive concrete layer is located, and will not leak into the stratum through the conductive concrete.
[0010] To arrange the membrane focusing electrode system, the lining of the subway tunnel section to be tested needs to be replaced with a conductive concrete-ordinary concrete composite lining containing a conductive concrete layer. The conductive concrete layer is made by adding a carbon fiber-based multiphase conductive filler. The conductive filler uses carbon fiber as a main agent and carbon black, graphite, etc. as auxiliary agents. The composite components and proportions of the conductive filler are determined according to the existing method based on the principle that the resistivity of the conductive concrete is 50 to 100 Ω·m.
[0011] Follow these steps:
[0012] Step 1: a conductive concrete-ordinary concrete composite lining including a conductive concrete layer is set in the subway tunnel section to be tested;
[0013] Step 2: Arrange a membrane focusing electrode system on the conductive concrete-ordinary concrete composite lining;
[0014] Step 3, connecting the array microelectrode, the integral shielding electrode and the loop electrode to the focusing detection device, thereby controlling the potential condition between the microelectrode and the shielding electrode, and obtaining the resistivity detection result of each microelectrode;
[0015] Step 4: prepare a conductive concrete test block identical to the conductive concrete layer in step 1, conduct indoor tests, and study the evolution of strain, cracking and leakage, and water-filled crack opening of conductive concrete induced by force, heat, and moisture through indoor tests, and establish a correlation function between the evolution of strain and the resistivity.
[0016] Step 5: Use the resistivity tomography method to reconstruct the resistivity image of the closed section of the tunnel lining, obtain the resistivity image in real time, and obtain the evolution law of the tunnel lining strain, cracking and leakage, and the opening of water-filled cracks based on the correlation function in step 4, so as to complete the real-time monitoring of the lining stress and the early warning of cracks and leakage.
[0017] The test process of step 4 is as follows: first, prepare a conductive concrete test block of 100×100×100 mm, select any two surfaces as loading surfaces, set copper electrodes of the same size and thickness of 2 mm as the loading surfaces on the two loading surfaces, set a Peek plate with a thickness of 10 mm on the surface of the copper electrode, select any two surfaces from the remaining four surfaces and paste resistance strain gauges as working pieces along the loading direction, arrange temperature compensation sheets on any two surfaces of another unloaded conductive concrete test block, keep the temperature and humidity of the environmental chamber constant, consider temperature and humidity compensation, obtain the strain response of the conductive concrete test block during the step-by-step loading process, measure the resistance between the two copper electrodes simultaneously, and convert the resistivity according to the cross-sectional area and height of the test block, then establish the load-strain-resistivity correlation function; then, for the unloaded condition, keep the temperature or humidity constant, and obtain the strain law of the conductive concrete test block during the gradual increase of humidity or temperature; finally, according to the resistivity response result data under different force, heat and humidity conditions, establish the correlation function between the resistivity of the conductive concrete test block and the three factors of force, heat and humidity.
[0018] The present invention adopts membrane microelectrode technology and current focusing principle. On the basis of existing research on conductive concrete preparation technology, a sensitive concrete layer is formed by controlling the steel insulation and concrete conductive treatment of the current propagation range. The resistivity of the conductive concrete layer has strain-level response accuracy, and at the same time has the functions of crack and leakage warning and monitoring the evolution of water-filled crack opening, so as to achieve the purpose of monitoring the two processes of continuous strain increase and crack and leakage evolution by a physical means, and has significant technical innovation.
[0019] Based on the existing research on conductive concrete and focused DC resistivity method, the present invention provides a subway tunnel concrete lining disease monitoring and health diagnosis method, which can effectively guide the early targeted repair of tunnel lining cracks and leakage disasters.
[0020] The key technology system involved in this invention is of great significance for ensuring the safety of subway operations, leading the development of resilient operation and maintenance technology of domestic subway tunnels, and serving the development and utilization of urban underground space. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a schematic diagram of the flow of current after focusing in the present invention;
[0022] Figure 2 This is a schematic diagram of the structure of the membrane focusing electrode system in the present invention. DETAILED DESCRIPTION
[0023] In order to clearly illustrate the technical features of this patent, this patent is elaborated in detail below through a specific implementation method and in combination with its accompanying drawings.
[0024] The specific steps of this case are as follows:
[0025] a) First, a membrane focusing electrode system is made. The side of the electrode system close to the center of the tunnel is a PET film. The PET film can isolate the focusing electrode system from the heat-humidity-stray current environment inside the tunnel. The focusing electrode system close to the lining side is composed of an array microelectrode, an integral shielding electrode and a loop electrode. The size of each microelectrode is Φ5-10mm, and the horizontal and vertical spacing of the microelectrode is 2-5cm. A 2mm wide insulating ring is arranged around the microelectrode. The outer periphery of the insulating ring is an integral shielding electrode. A loop electrode is arranged 10-20cm away from the boundary of the test area along the longitudinal direction of the tunnel. The microelectrode, shielding electrode and loop electrode are all prepared by platinum electroplating method;
[0026] b) Based on the existing mature technology, a method of adding carbon fiber-based multiphase conductive fillers is used to make a conductive concrete layer in a certain range of concrete near the center of the tunnel. The thickness of the conductive concrete layer is between the thickness of the tunnel lining concrete protective layer and 20-30% of the lining thickness. The steel bars within the thickness range of the conductive concrete layer are sprayed with insulating paint. The composite components and proportions of the conductive fillers are determined according to the existing method based on the principle that the resistivity of the conductive concrete is 50-100Ω·m;
[0027] c) Connect the focusing electrode system to the focusing detection equipment, and set the equipotential condition between the shielding electrode and the microelectrode according to the current focusing principle, so as to force the detection current emitted by the microelectrode to flow into the conductive concrete layer perpendicular to the electrode direction, and then flow in the conductive concrete layer in a columnar shape for a certain distance before returning to the loop electrode, so as to obtain the resistivity detection result of each microelectrode;
[0028] d) Using the same materials and processes as the conductive concrete layer to make conductive concrete test blocks, carry out indoor tests, and study the evolution of strain, cracking and leakage, and water-filled crack opening of conductive concrete induced by force, heat and moisture through indoor tests, and establish their correlation function with resistivity;
[0029] e) Resistivity tomography is used to reconstruct the resistivity image of the closed section of the tunnel lining, and the resistivity image is obtained in real time using the automatic measurement-wireless transmission mode. According to the correlation function established in step d), the compressive strain accumulation and tensile cracking of the concrete lining are obtained, and the information such as the precursor of cracking and leakage and the change of the crack opening after cracking and leakage is obtained, thereby completing the real-time stress monitoring and cracking and leakage warning of the concrete lining.
[0030] There are many specific implementation ways of the present invention. The above is only the preferred implementation mode of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements can be made without departing from the principle of the present invention. These improvements should also be regarded as the protection scope of the present invention.
Claims
1. A working method of a subway tunnel lining stress monitoring and crack and leakage early warning mechanism, characterized in that: The stress monitoring and crack leakage warning mechanism is a membrane focusing electrode system installed on the surface of the subway tunnel lining to be tested, and the membrane focusing electrode system includes a PET film, a plurality of microelectrodes fixed and pasted on the PET film and distributed in an array, an insulating ring fixedly arranged outside each microelectrode, an integral shielding electrode between adjacent insulating rings, and a loop electrode arranged in the longitudinal direction of the tunnel at a position 10 to 20 cm away from the boundary of the subway tunnel lining to be tested; The side of the subway tunnel lining to be tested facing the focusing electrode system is set as conductive concrete, and the thickness of the conductive concrete layer is between the thickness of the tunnel lining concrete protective layer and 20-30% of the lining thickness, and the steel bars within the thickness range of the conductive concrete layer are sprayed with insulating paint to achieve electrical insulation; the microelectrode, the shielding electrode and the loop electrode are isolated from the environment inside the tunnel by the PET film, and the detection current is realized to flow within a limited depth range inside the lining by the current focusing method; Follow these steps: Step 1: a conductive concrete-ordinary concrete composite lining including a conductive concrete layer is set in the subway tunnel section to be tested; Step 2: Arrange a membrane focusing electrode system on the conductive concrete-ordinary concrete composite lining; Step 3, connecting the array microelectrode, the integral shielding electrode and the loop electrode to the focusing detection device, thereby controlling the potential condition between the microelectrode and the shielding electrode, and obtaining the resistivity detection result of each microelectrode; Step 4: prepare a conductive concrete test block identical to the conductive concrete layer in step 1, conduct indoor tests, and study the evolution of strain, cracking and leakage, and water-filled crack opening of conductive concrete induced by force, heat, and moisture through indoor tests, and establish a correlation function between the evolution of strain and the resistivity. The test process of step 4 is as follows: first, prepare a conductive concrete test block of 100×100×100 mm, select any two surfaces as loading surfaces, set copper electrodes of the same size and thickness of 2 mm as the loading surfaces on the two loading surfaces, set a Peek plate with a thickness of 10 mm on the surface of the copper electrode, and select any two surfaces from the remaining four surfaces to paste resistance strain gauges as working sheets along the loading direction, arrange temperature compensation sheets on any two surfaces of another unloaded conductive concrete test block, keep the temperature and humidity of the environmental chamber constant, consider temperature and humidity compensation, obtain the strain response of the conductive concrete test block during the step-by-step loading process, measure the resistance between the two copper electrodes simultaneously, and convert the resistivity according to the cross-sectional area and height of the test block, and then establish the load-strain-resistivity correlation function; then, for the unloaded condition, keep the temperature or humidity constant, and obtain the strain law of the conductive concrete test block during the gradual increase of humidity or temperature; finally, according to the resistivity response result data under different force, heat and humidity conditions, establish the correlation function between the resistivity of the conductive concrete test block and the three factors of force, heat and humidity; Step 5: Use the resistivity tomography method to reconstruct the resistivity image of the closed section of the tunnel lining, obtain the resistivity image in real time, and obtain the evolution law of the tunnel lining strain, cracking and leakage, and the opening of water-filled cracks based on the correlation function in step 4, so as to complete the real-time monitoring of the lining stress and the early warning of cracks and leakage.
2. The working method of a subway tunnel lining stress monitoring and crack and leakage early warning mechanism according to claim 1 is characterized in that: The conductive concrete layer is made by adding carbon fiber-based composite conductive fillers. The conductive fillers are mainly carbon fiber and auxiliary carbon black and graphite. The composite components and proportions of the conductive fillers are determined based on the principle that the resistivity of the conductive concrete is 50-100Ω×m.
Citation Information
Patent Citations