A preparation method of perampanel fine granules

By using titanium dioxide and binder homogeneous treatment in the preparation of perampanel fine granules, combined with centrifugal granulation technology, optimizing the ratio of lactose and mannitol, the API content uniformity and stability issues were solved and achieved Efficient preparation in compliance with pharmacopoeial requirements.

CN118415997BActive Publication Date: 2024-10-18HQ PHARMA (SHANGHAI) CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410892004.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-04
Publication Date
2024-10-18
Estimated Expiration
2044-07-04

AI Technical Summary

Technical Problem

The API content uniformity of perampanel fine granules in the prior art is low and the stability is poor, making it difficult to meet the pharmacopoeia requirements.

Method used

Use titanium dioxide in water and stir to form a suspension. Add the binder solution, perampanel and silica. After homogenization, add lactose, yellow iron oxide and mannitol for centrifugal granulation. Control the drying temperature and particle size distribution. Optimize the amount of fillers and binders to ensure that the API is evenly dispersed in the particles.

Benefits of technology

The API content uniformity is improved, the stability is improved, the particle size distribution meets the pharmacopoeia requirements, the production process is simple, the cost is low, and the dissolution behavior is similar to the reference preparation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
  • Figure SMS_4
    Figure SMS_4
Patent Text Reader

Abstract

The present invention relates to the technical field of pharmaceutical preparations, and in particular to a method for preparing perampanel fine granules, the preparation method comprising the following steps: (1) titanium dioxide is placed in water and stirred to obtain a suspension; (2) the suspension is added to a 2-5wt% binder solution, and then perampanel and silicon dioxide are added, homogenized, to obtain an API suspension; (3) lactose, yellow ferric oxide and mannitol are added to a granulator, and then 1-3wt% binder solution and API suspension are added in sequence for granulation, and the mixture is dried and sieved to obtain the result. The present invention has the advantages of high uniformity of API content and good stability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of pharmaceutical preparations, and in particular to a method for preparing perampanel fine granules. Background Art

[0002] Perampanel is a potent, non-competitive and highly selective α-amino-3-hydroxy-5-methyl-4-isoxazolepropionic acid (AMPA) glutamate receptor antagonist, with the chemical name 2-(2-oxy-1-phenyl-5-pyridin-2-yl-1,2-dihydropyridin-3-yl)benzonitrile hydrate (4:3). It is mainly used to treat partial seizures of epilepsy in adults and children aged four years and above (with or without provoked generalized seizures). The mechanism of action is different from that of other anti-epileptic drugs, so it can be used in combination with other common anti-epileptic drugs to better control epileptic seizures. Its structural formula is as follows:

[0003] .

[0004] According to the definition of the 2020 edition of the Chinese Pharmacopoeia, granules refer to dry granular preparations with a certain particle size made by mixing raw materials with suitable excipients. Usually, dry granulation, wet granulation and other methods are used for preparation. According to the particle size and particle size distribution determination method (General Rule 0982 Second Method Double Screening Method), the sum of the materials that cannot pass through the No. 1 sieve (2000μm) and the materials that can pass through the No. 5 sieve (180μm) shall not exceed 15%. According to the definition of the Japanese Pharmacopoeia (JP18), fine granules refer to fine granules that can pass through the 850μm sieve, the proportion of materials retained on the 500μm sieve is less than 10%, and the proportion of materials passing through the 75μm sieve is less than 30%.

[0005] Compared with conventional dosage forms, fine granules have the advantages of ① easy to swallow; ② rapid onset of action; ③ easy to adjust the dosage; ④ easy to mix evenly; ⑤ bitterness suppression, etc. Fine granules are a patient-friendly dosage form, especially popular with patients who may have swallowing disorders (such as the elderly and children) because they can ensure compliance with medication.

[0006] Japan has designed a unique equipment for the preparation of fine granules; this equipment is complex in structure, expensive, and extremely difficult to process. For children with epilepsy, fine granules have better compliance and are easy to take, but the API in this product accounts for a small proportion and is a low-dose drug. The content uniformity of fine granules is a difficult challenge in the product preparation process. Therefore, it is urgent to develop a perampanel fine granule with stable product quality, reliable efficacy, reasonable dissolution, content uniformity that meets the requirements of the pharmacopoeia, and a simple preparation process.

[0007] pH-solubility studies of perampanel revealed that API dissolution was pH-dependent, dissolving rapidly and completely in pH 1.2 hydrochloric acid solution, but dissolving slowly in weakly acidic or neutral media.

[0008] At present, most of the existing technologies are research and development of perampanel API compounds, crystal forms, compositions, components, preparation methods and product applications. For example, the Chinese invention patent application CN1942443A discloses "crystals of 1,2-dihydropyridine compounds and their production methods", which involves the preparation methods and uses of hydrate crystal forms and anhydrate crystal forms (type I, type III, type V) (a therapeutic or preventive agent for epilepsy, hepatic encephalopathy, etc.).

[0009] Chinese invention patent application CN116549402A discloses a perampanel fine particle composition, preparation method and application, wherein the raw materials of the composition include: perampanel or its hydrate, lactose, mannitol, adhesive and glidant; the mass ratio of lactose and mannitol is 1:3-3:1. The preparation method includes first taking part of the adhesive to prepare an adhesive solution 1, then preparing the remaining adhesive into a solution, and then adding the raw materials other than mannitol and lactose into the solution to prepare an adhesive solution 2; finally, mixing mannitol and lactose as a base material, first pumping into the adhesive solution 1, then pumping into the adhesive solution 2, performing fluidized bed granulation, and drying. The present invention adopts a specific ratio of lactose mannitol and a preparation method, so that the active ingredient has a dissolution behavior that is not inferior to the reference preparation, especially in a pH 4.0 medium where the API is poorly soluble, the dissolution is fast and complete. However, the invention does not focus on the uniformity of the API content and the stability of the preparation of the fine particle preparation.

[0010] The inventors found that the API content uniformity of the above-mentioned fine particle preparations was low and the stability was poor, both of which need to be further improved.

[0011] Therefore, it is very necessary to develop a perampanel fine granule and a preparation method thereof that can solve the above-mentioned technical problems. Summary of the invention

[0012] The purpose of the present invention is to overcome the deficiencies of the prior art and provide a perampanel fine granule with high API content uniformity and good stability and a preparation method thereof.

[0013] The present invention is achieved through the following technical solutions:

[0014] A method for preparing perampanel fine granules comprises the following steps:

[0015] (1) Titanium dioxide is placed in water and stirred to obtain a suspension;

[0016] (2) adding the suspension to a 2-5 wt% binder solution, then adding perampanel and silicon dioxide, homogenizing and sieving to obtain an API suspension;

[0017] (3) Add lactose, yellow ferric oxide and mannitol into a granulator, and then add 1-3 wt% binder solution and API suspension in sequence for granulation, and obtain the granules after drying and sieving.

[0018] Preferably, the process parameters of the homogenization in step (2) are: rotation speed 3000-5000 rpm, homogenization time 5-15 min.

[0019] Preferably, the sieving mesh number in step (2) is 60-100 mesh.

[0020] Preferably, the granulation comprises centrifugal granulation.

[0021] More preferably, the process parameters of the centrifugal granulation are as follows: spheronization speed: 200-350 rpm, atomization pressure: 1-1.4 bar, liquid spraying speed: 10-50 rpm, air inlet speed: 300-600 rpm, air outlet speed: 350-650 rpm.

[0022] Preferably, the granulation temperature in step (3) is controlled at 25-28°C.

[0023] Preferably, the drying temperature in step (3) is controlled at 40°C, and the drying is performed until LOD ≤ 1.0%.

[0024] Preferably, in step (3), lactose and mannitol are first sieved through a 40-mesh sieve before being added to the granulator.

[0025] Preferably, the composition comprises the following components in parts by weight: 0.5-2 parts of perampanel, 15-80 parts of lactose, 18-78 parts of mannitol, 2-6 parts of binder, 0.5-2.0 parts of silicon dioxide, 0.1-2.0 parts of yellow iron oxide, and 0.01-0.2 parts of titanium dioxide.

[0026] More preferably, the mass ratio of lactose to mannitol is 1:4-4:1.

[0027] More preferably, the mass percentage of the binder in the perampanel fine granules is 2%-4%.

[0028] Preferably, the particle size distribution of the perampanel fine granules is such that the particles that do not pass through a 0.5 mm sieve account for less than 10%, and the particles that pass through a 0.075 mm sieve account for no more than 30%.

[0029] 1. The active ingredient of fine particles for oral consumption is perampanel, accounting for 1.04-2.0% of the prescription, of which the effective amount of the active ingredient is 10.4-20 mg / g.

[0030] 2. The fillers lactose and mannitol account for about 85-95% of the prescription composition, wherein the preferred prescription ratio of lactose and mannitol is about 4:1-1:4, and more preferably 1:1.

[0031] 3. The binder is cellulose ether and its derivatives, preferably one or more conventional pharmaceutical binders such as hydroxypropyl methylcellulose, hydroxypropyl cellulose, gelatin, etc., among which hydroxypropyl cellulose is preferred, accounting for 2-6% of the prescription, more preferably 2-4%.

[0032] 4. The colorant is a conventional synthetic pigment and a natural pigment, preferably carmine, sunset yellow, curcumin, yellow iron oxide, etc., among which yellow iron oxide is preferred, accounting for 0.1-2.0% of the prescription, and more preferably 0.2-0.5%.

[0033] 5. The sunscreen is one or more of titanium dioxide, zinc oxide, sodium dihydroxyacetate, etc., among which titanium dioxide is preferred, accounting for 0.01-0.2% of the prescription, and more preferably 0.02-0.1%.

[0034] 6. The glidant is one or more conventional pharmaceutical glidants such as silicon dioxide, stearic acid, calcium stearate, talc, etc., among which silicon dioxide is preferred, accounting for 0.5-2.0% of the prescription, and more preferably 0.6-1.5%.

[0035] The beneficial effects of the present invention are:

[0036] The API (perampanel) in the fine granules prepared by the present invention accounts for a relatively small proportion. For fine granules, the uniform dispersion of API in the granules has been a long-standing problem. The present invention adopts a unique API addition method, which is to add the API in the binder solution, so that the API is evenly dispersed in the granules, and its content uniformity meets the requirements of the pharmacopoeia.

[0037] The present invention optimizes the dosage of fillers (lactose and mannitol) so that the active ingredient has a dissolution behavior that is not inferior to that of a reference preparation and the particle size distribution is similar to that of the reference preparation.

[0038] The invention optimizes the dosage of the filler and the concentration of the binder, so that the particle size distribution of the fine granules is close to that of the reference preparation and complies with the provisions of the pharmacopoeia.

[0039] Compared with conventional fine granules which require the use of complex and expensive imported special granulation equipment, the preparation process of the present invention is relatively simple, and can be easily prepared by selecting traditional centrifugal granulation equipment, and the production cost is relatively low. DETAILED DESCRIPTION

[0040] The present invention will be further described below in conjunction with specific embodiments, and the advantages and features of the present invention will become clearer as the description proceeds. However, these embodiments are exemplary only and do not constitute any limitation to the scope of the present invention. It should be understood by those skilled in the art that the details and forms of the technical solution of the present invention may be modified or replaced without departing from the spirit and scope of the present invention, but these modifications and replacements all fall within the scope of protection of the present invention.

[0041] Glossary:

[0042] HPC is hydroxypropyl cellulose, also known as hydroxypropyl cellulose.

[0043] API is a pharmaceutical active ingredient, and in the present invention specifically refers to perampanel (3 / 4 water).

[0044] RLD-26A71K: a reference preparation purchased from Ace Co., Ltd.

[0045] The hydroxypropyl cellulose in each embodiment of the present invention was purchased from Anhui Shanhe Pharmaceutical Excipients Co., Ltd., model SH-SL.

[0046] The difference between Examples 1 to 3 is that the mass ratio of lactose to mannitol is different, which is 4:1 for Example 1, 1:1 for Example 2, and 1:4 for Example 3. The specific prescriptions of each example are as follows:

[0047]

[0048] The difference between Example 4 and Example 6 is that the amount of hydroxypropyl cellulose is different, which is 2.0%, 4.0% and 1.0% respectively. The specific prescriptions of each example are as follows:

[0049]

[0050] The preparation process of Examples 1-6 is the same as that of Preparation Example 1.

[0051] Example 7

[0052] Components Dosage (mg / g) Perampanel (3 / 4 water) 10.40 lactose 483.00 Mannitol 473.00 Hydroxypropyl methylcellulose 20.00 Silicon dioxide 8.00 Yellow Iron Oxide 5.00 Titanium Dioxide 0.60 total 1000.0

[0053] The preparation process of Example 7 is the same as that of Preparation Example 2.

[0054] Preparation Example 1:

[0055] (1) Mannitol and lactose are passed through a 40-mesh sieve.

[0056] (2) Preparation of 1.5% HPC solution: Dissolve 50% of the prescribed amount of HPC in hot purified water and stir until completely dissolved to prepare a 1.5% HPC solution.

[0057] (3) Preparation of 3% HPC solution: The remaining 50% of the prescribed amount of HPC is dissolved in hot purified water to prepare a 3% HPC solution; titanium dioxide is placed in room temperature purified water and stirred to form a suspension. Then it is added to the fully dispersed HPC solution and stirred continuously. While stirring, the sieved API and silica are slowly added. The API suspension is homogenized using a homogenizer at 3000 rpm for 10 minutes to fully disperse the API and silica, which are then passed through an 80-mesh sieve. A small amount of purified water is left to rinse the container. Stirring is continued during the granulation process.

[0058] (4) Centrifugal granulation: Add lactose, yellow iron oxide and mannitol into the centrifugal granulator, set the spheronization speed to 200rpm, atomization pressure to 1bar, liquid spray speed to 10rpm, air inlet speed to 300rpm, air outlet speed to 350rpm, first spray in 1.5% HPC solution for masterbatch granulation, then spray in API suspension for drug loading. The material temperature is controlled at 25-28℃ throughout the process, and the material is dried after drug loading.

[0059] (5) Drying: Control the material temperature at 40°C and dry until the particle LOD ≤ 1.0%.

[0060] (6) Screening: Screen through a 0.5 mm sieve.

[0061] Preparation Example 2

[0062] (1) Mannitol and lactose are passed through a 40-mesh sieve.

[0063] (2) Preparation of 3% HPC solution: Dissolve 50% of the prescribed amount of HPC in hot purified water and stir until completely dissolved to prepare a 3% HPC solution.

[0064] (3) Preparation of 5% HPC solution: The remaining 50% of the prescribed amount of HPC is dissolved in hot purified water to prepare a 5% HPC solution; titanium dioxide is placed in room temperature purified water and stirred to form a suspension. Then it is added to the fully dispersed HPC solution and stirred continuously. While stirring, the sieved API and silica are slowly added. The API suspension is homogenized using a homogenizer at 3000 rpm for 10 minutes to fully disperse the API and silica, which are passed through an 80-mesh sieve. A small amount of purified water is left to rinse the container. Stirring is continued during the granulation process.

[0065] (4) Centrifugal granulation: Add lactose, yellow iron oxide and mannitol into the centrifugal granulator, set the spheronization speed to 350rpm, atomization pressure to 1.4bar, liquid spray speed to 20rpm, air inlet speed to 400rpm, air outlet speed to 450rpm, first spray in 3% HPC solution for masterbatch granulation, then spray in API suspension for drug loading. The material temperature is controlled at 25-28℃ throughout the process, and the material is dried after drug loading.

[0066] (5) Drying: Control the material temperature at 40°C and dry until the particle LOD ≤ 1.0%.

[0067] (6) Screening: Screen through a 0.5 mm sieve.

[0068] Comparative Example 1

[0069] The formulation composition is the same as that of Example 5, except that the preparation process is different and the timing of adding the API is different, as follows:

[0070] (1) Mannitol and lactose are passed through a 40-mesh sieve.

[0071] (2) Preparation of 1.5% HPC solution: Dissolve 50% of the prescribed amount of HPC in hot purified water and stir until completely dissolved to prepare a 1.5% HPC solution.

[0072] (3) Preparation of 3% HPC solution: The remaining 50% of the prescribed amount of HPC is dissolved in hot purified water to prepare a 3% HPC solution; titanium dioxide is placed in room temperature purified water and stirred to form a suspension. Then it is added to the fully dispersed HPC solution and stirred continuously. While stirring, the sieved silicon dioxide is slowly added and homogenized using a homogenizer to obtain a suspension. The homogenization parameter is 3000 rpm, and the homogenization is performed for 10 minutes to fully disperse the silicon dioxide. A small amount of purified water is left to rinse the container. Stirring is continued during the granulation process.

[0073] (4) Centrifugal granulation: Add lactose, yellow iron oxide, API and mannitol into the centrifugal granulator, set the spheronization speed to 200rpm, atomization pressure to 1bar, liquid spray speed to 10rpm, air inlet speed to 300rpm, air outlet speed to 350rpm, first spray in 1.5% HPC solution for masterbatch granulation, then spray in the suspension for drug application. The material temperature is controlled at 25-28℃ throughout the process, and the material is dried after drug loading.

[0074] (5) Drying: Control the material temperature at 40°C and dry until the particle LOD ≤ 1.0%.

[0075] (6) Screening: Screen through a 0.5 mm sieve.

[0076] Comparative Example 2

[0077] The formula composition is the same as that of Example 1, except that the preparation process is different and no 1.5% HPC solution is prepared. The specific details are as follows:

[0078] (1) Mannitol and lactose are passed through a 40-mesh sieve.

[0079] (2) Preparation of 3% HPC solution: Dissolve the entire amount of HPC in hot purified water to prepare a 3% HPC solution; place titanium dioxide in room temperature purified water and stir to form a suspension. Then add it to the fully dispersed HPC solution and continue stirring. Slowly add the sieved API and silicon dioxide while stirring. Use a homogenizer to homogenize to obtain an API suspension. The homogenization parameter is 3000 rpm. Homogenize for 10 minutes to fully disperse the silicon dioxide and API. Use a small amount of purified water to rinse the container. Continue stirring during the granulation process.

[0080] (3) Centrifugal granulation: Add lactose, yellow iron oxide and mannitol into the centrifugal granulator, set the spheronization speed to 200 rpm, atomization pressure to 1 bar, spray speed to 10 rpm, air inlet speed to 300 rpm, air outlet speed to 350 rpm, and spray the API suspension for drug loading and granulation. The material temperature is controlled at 25-28 °C throughout the process, and the material is dried after drug loading.

[0081] (4) Drying: Control the material temperature at 40°C and dry until the particle LOD ≤ 1.0%.

[0082] (5) Screening: Screen through a 0.5 mm sieve.

[0083] Comparative Example 3

[0084] The formula composition is different from that of Example 5, except that the preparation process is different and the method of adding mannitol is different, as follows:

[0085] (1) Mannitol and lactose are passed through a 40-mesh sieve.

[0086] (2) Preparation of 1.5% HPC solution: Dissolve 50% of the prescribed amount of HPC in hot purified water and stir until completely dissolved to prepare a 1.5% HPC solution.

[0087] (3) Preparation of 3% HPC solution: The remaining 50% of the prescribed amount of HPC is dissolved in hot purified water to prepare a 3% HPC solution; titanium dioxide is placed in room temperature purified water and stirred to form a suspension. Then it is added to the fully dispersed HPC solution and stirred continuously. The API and 5 times the amount of mannitol in the API are mixed evenly, and the mixture of API and mannitol and silicon dioxide are slowly added while stirring. Use a homogenizer to homogenize to obtain an API suspension. The homogenization parameter is 3000rpm. Homogenize for 10 minutes to fully disperse the silicon dioxide, mannitol and API. A small amount of purified water is left to rinse the container. Stir continuously during the granulation process.

[0088] (4) Centrifugal granulation: Add lactose, yellow iron oxide and the remaining mannitol into the centrifugal granulator, set the spheronization speed: 200rpm, atomization pressure: 1bar, spray speed: 10rpm, air inlet speed: 300rpm, air outlet speed: 350rpm, first spray in 1.5% HPC solution for masterbatch granulation, then spray in API suspension for drug loading. The material temperature is controlled at 25-28℃ throughout the process, and drying is performed after drug loading is completed.

[0089] (5) Drying: Control the material temperature at 40°C and dry until the particle LOD ≤ 1.0%.

[0090] (6) Screening: Screen through a 0.5 mm sieve.

[0091] Comparative Example 4

[0092] The formulation composition is the same as that of Example 5, except that the preparation is carried out according to the preparation method of Example 1 of CN116549402A, as follows:

[0093] (1) Mannitol and lactose are passed through a 40-mesh sieve.

[0094] (2) taking 50% of the binder and adding water to prepare a binder solution 1 with a mass concentration of 1.5%; ② preparing a solution with a mass concentration of 3% with the remaining binder, and then adding the raw materials except mannitol and lactose to the solution, and continuously stirring until the suspension is uniform, to prepare a binder solution 2;

[0095] (3) Granulation: Mannitol and lactose were used as base materials: Chongqing Jinggong's DPL-Ⅱ fluidized bed was used for granulation, and the parameters were set as follows: inlet air temperature: 60°C, heater temperature 90°C, fan frequency 25Hz, atomization pressure 0.15mPa, and the fluidized bed was preheated until the material temperature displayed was 30°C. Lactose and mannitol were placed in the fluidized bed for granulation; the peristaltic pump speed was set to 8rpm, and granulation was started. Binder solution 1 was pumped in first, with an initial pump speed of 12rpm, and the speed was increased by 5rpm every 10min until it reached 38rpm and remained unchanged. After the pumping was completed, the equipment parameters were kept unchanged, and the binder solution 2 was continuously pumped in until the pumping was completed.

[0096] (4) Drying: Increase the fan frequency to 35 Hz, set the heater temperature to 70 °C, and start drying until the particle LOD ≤ 1.0%.

[0097] (5) Screening: Screen through a 0.5 mm sieve.

[0098] Test Example 1 Dissolution Behavior Test

[0099] Based on the dissolution behavior of the self-developed preparation and the control preparation RLD-26A71K in pH 6.8 phosphate buffer, the dissolution behavior of the products of Examples 1-3 was evaluated with a similarity factor f2. The results are shown in Table 1:

[0100] Table 1 Dissolution data of Example 1-Example 3

[0101]

[0102] Note: f2 is calculated based on the corresponding points of 5, 10, 15, 20, 30, 45 min for the control preparation and the self-developed preparation.

[0103] As can be seen from the dissolution behavior in Table 1, the dissolution behaviors of Examples 1-3 are similar to those of the reference preparation. Therefore, the ratio of lactose to mannitol in the formulation is preferably 1:4-4:1.

[0104] In pH 4.0 acetate buffer, the dissolution behaviors of the self-made preparations and the control preparations were tested. The dissolution behaviors of the products of Examples 4-7 were evaluated with the similarity factor f2. The results are shown in Tables 2 and 3:

[0105] Table 2 Dissolution data of Example 4-Example 6

[0106]

[0107] Note: f2 is calculated based on the corresponding points of 5, 10, 15, 20, 30 min for the control preparation and the self-developed preparation, the same below.

[0108] Table 3 Dissolution data of Example 7

[0109]

[0110] From the dissolution behavior, it can be seen that Examples 5 and 7 show that different types of adhesives are suitable for this prescription process; when the amount of hydroxypropyl cellulose is in the range of 2.0%-4.0%, the in vitro dissolution behavior is similar to that of the reference preparation.

[0111] The particle size distribution test results of Test Example 2 are shown in Table 4:

[0112] Table 4 Particle size distribution results of Examples 1-3

[0113]

[0114] Note: "Disc" in Table 4 refers to the bottom disc, i.e. the pore size is less than 125 μm.

[0115] The particle size distribution test results show that the particle size distribution of Example 2 is closest to that of the reference preparation, and the particle sizes of Examples 1 and 3 are smaller than that of the reference preparation.

[0116] Test Example 3 Content Uniformity Test

[0117] The test was carried out with reference to the General Chapter 0941 of the Chinese Pharmacopoeia, and the results are shown in Table 5.

[0118] Table 5 Content uniformity test results

[0119] name A+2.2S Example 1 7.8 Example 2 9.7 Example 3 11.2 Example 4 10.4 Example 5 8.2 Example 6 10.4 Example 7 8.3 Comparative Example 1 23.1 Comparative Example 2 25.0 Comparative Example 3 19.8 Comparative Example 4 14.8 limit A+2.2S should not be greater than 15.0

[0120] Test Example 4: Stability Test

[0121] The detection method was based on the import registration standard JX20160328 for Perampanel Tablets, and the results are shown in Table 6.

[0122] Table 6 Stability test results

[0123]

[0124] Conclusion: For Comparative Examples 1-3, A+2.2S is greater than 15, and the content uniformity is unqualified. The A+2.2S of Comparative Example 4 is 14.8, which is close to the upper limit. The A+2.2S of each embodiment is significantly less than 15.0. The content uniformity results of the self-made preparation products prepared by the present invention are good. The samples of Examples 1, 5 and Comparative Examples 1-3 are qualified for related substances under the accelerated 3-month condition. However, compared with Examples 1 and 5, the impurity content of Comparative Examples 1-3 increases rapidly when accelerated for 3 months, and the stability is poor. The related substances of Comparative Example 4 increase rapidly under the accelerated 3-month condition, and other single impurities have the risk of exceeding the limit. Therefore, by changing the timing of adding API, the preparation method of the binder and the addition method of mannitol, the problems of unqualified content uniformity of low-dose fine granules and effective control of related substance growth are successfully improved, and this process is simple and suitable for commercial production.

[0125] The above detailed description is a specific description of one feasible embodiment of the present invention. The embodiment is not intended to limit the patent scope of the present invention. Any equivalent implementation or modification that does not deviate from the present invention should be included in the scope of the technical solution of the present invention.

Claims

1. A method for preparing perampanel fine granules, characterized in that: The steps include: (1) Titanium dioxide is placed in water and stirred to obtain a suspension; (2) adding the suspension to a 2-5 wt% binder solution, then adding perampanel and silicon dioxide, homogenizing and sieving to obtain an API suspension; (3) adding lactose, yellow ferric oxide and mannitol into a granulator, and then sequentially adding 1-3 wt% of a binder solution and an API suspension to granulate, and drying and sieving to obtain a granulated product; The process parameters of the homogenization in step (2) are: rotation speed 3000-5000rpm, homogenization 5-15min; the sieving mesh number is 60-100 mesh; In step (3), lactose and mannitol are first sieved through a 40-mesh sieve before being added to the granulator; The granulation in step (3) includes centrifugal granulation; the process parameters of the centrifugal granulation are as follows: spheronization speed: 200-350rpm, atomization pressure: 1-1.4bar, spraying speed: 10-50rpm, air inlet speed: 300-600rpm, air outlet speed: 350-650rpm; The perampanel fine granules include the following components in parts by weight: 0.5-2 parts of perampanel, 15-80 parts of lactose, 18-78 parts of mannitol, 2-6 parts of binder, 0.5-2.0 parts of silicon dioxide, 0.1-2.0 parts of yellow iron oxide, and 0.01-0.2 parts of titanium dioxide; The mass ratio of lactose to mannitol is 1:4-4:1; the mass percentage of the total mass of lactose and mannitol in the perampanel fine granules is 85-95%; The binder is hydroxypropyl methylcellulose or hydroxypropyl cellulose; the mass percentage of the binder in the perampanel fine granules is 2%-6%.

2. The preparation method according to claim 1, characterized in that: The granulation temperature in step (3) is controlled at 25-28°C.

3. The preparation method according to claim 1, characterized in that: The drying temperature in step (3) is controlled at 40-55°C and dried to LOD ≤ 1.0%.

4. The preparation method according to any one of claims 1 to 3, characterized in that: The particle size distribution of the perampanel fine granules is such that the proportion of particles that do not pass through a 0.5 mm sieve is less than 10%, and the proportion of particles that pass through a 0.075 mm sieve is no more than 30%.

Citation Information

Patent Citations

  • Crystal of 1,2-dihydropyridine compound and method for producing same

    CN1942443A

  • Perampanel fine particle composition, preparation method and application

    CN116549402A