Scattering measurement method and scattering measurement device

By using infrared measurement light to obtain deep feature parameters of the substrate, the problem that broadband visible light cannot penetrate structures with a depth greater than 1 micrometer is solved, and high-sensitivity measurement of deep features is achieved.

CN118464843BActive Publication Date: 2024-11-15HANGZHOU HFC SEMICONDUCTOR CO
View PDF 13 Cites 0 Cited by

Patent Information

Application Number
CN202410917499.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-10
Publication Date
2024-11-15
Estimated Expiration
2044-07-10

AI Technical Summary

Technical Problem

In existing technologies, broadband visible light has difficulty penetrating the substrate to reach the bottom of the structure under test, which is deeper than 1 micrometer, resulting in the scattered light being unable to effectively reflect the deep feature information of the structure under test.

Method used

The substrate is illuminated with infrared measurement light in the wavelength range of 2μm~7.5μm or 25μm~35μm, which shines through the surface onto the unit under test, and the scattered light is received to obtain characteristic parameters such as diameter, width, depth and sidewall angle.

Benefits of technology

It improves the sensitivity of measuring deep features inside the substrate, and can accurately obtain the characteristic parameters of the unit under test, especially the structure with a depth greater than 1 micrometer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118464843B_ABST
    Figure CN118464843B_ABST
Patent Text Reader

Abstract

The present invention provides a scattering measurement method and a scattering measurement device, wherein a wide-band infrared measurement light is first used to irradiate a substrate, and the infrared measurement light is irradiated to a unit to be measured through the surface of the substrate, wherein the wavelength of the infrared measurement light has a value range of 2μm~7.5μm or 25μm~35μm; then, the infrared measurement light scattered from the substrate and the unit to be measured is received to obtain characteristic parameters of the unit to be measured according to the infrared measurement light. Since the wavelength of the infrared measurement light has a value range of 2μm~7.5μm or 25μm~35μm, the infrared measurement light can effectively penetrate the substrate to irradiate the unit to be measured, so that the infrared measurement light scattered by the substrate and the unit to be measured can effectively reflect the deep characteristic information of the substrate and the unit to be measured in the substrate, thereby improving the sensitivity of measuring the deep characteristics inside the substrate, so that the characteristic parameters of the unit to be measured in the substrate can be accurately and effectively obtained.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a scattering measurement method and a scattering measurement device. Background Art

[0002] In the optical scattering measurement of wafers, a scatterometer is usually used to measure the characteristic parameters of the wafer surface, such as width, depth, height, diameter and angles. When the measurement light emitted by the scatterometer is irradiated onto the wafer surface, the measurement light is scattered by the wafer surface. Then, the scattered light on the wafer surface is collected by a detector and output as a measurement spectrum. Since the scattered light on the wafer surface carries the characteristic information of the wafer surface, by analyzing the scattered light on the wafer surface, the characteristic parameters of the wafer can be effectively obtained, for example, the width, depth or sidewall angle of the opening formed in the substrate can be obtained. At present, in the scattering measurement process of wafers, broadband visible light is mostly used as the measurement light. The wavelength range of broadband visible light is 300 nanometers to 900 nanometers, which is generally suitable for measuring structures to be measured with a depth not exceeding 1 micron, such as openings or buried layers formed in the substrate. However, for the structure to be measured with a depth greater than 1 micron, since broadband visible light cannot effectively penetrate the substrate to reach the bottom of the structure to be measured, the scattered light contains almost no characteristic information of the bottom of the structure to be measured. Therefore, the scattered light of the structure to be measured detected by broadband visible light may not effectively represent the outline of the structure to be measured. Summary of the invention

[0003] The object of the present invention is to provide a scattering measurement method and a scattering measurement device to improve the sensitivity of measuring deep features inside a substrate, thereby effectively obtaining characteristic parameters of a unit to be measured in the substrate.

[0004] To achieve the above-mentioned purpose, the present invention provides a scattering measurement method, comprising: providing a substrate, wherein a unit to be measured is formed in the substrate, and the unit to be measured penetrates a portion of the thickness of the substrate; irradiating the substrate with wide-band infrared measurement light, and the infrared measurement light is irradiated to the unit to be measured through the surface of the substrate, wherein the wavelength of the infrared measurement light ranges from 2μm to 7.5μm or from 25μm to 35μm; receiving infrared measurement light scattered from the substrate and the unit to be measured, so as to obtain characteristic parameters of the unit to be measured according to the infrared measurement light, wherein the characteristic parameters include at least one of diameter, width, depth and sidewall angle.

[0005] Optionally, in the scattering measurement method, at least one dielectric layer is formed on the substrate, and when the wide-band infrared measurement light is used to irradiate the substrate, the infrared measurement light is transmitted from the surface of the dielectric layer through the dielectric layer to irradiate the substrate.

[0006] Optionally, in the scattering measurement method, the material of the dielectric layer is at least one of silicon oxide, silicon nitride, silicon oxynitride and silicon fluoride.

[0007] Optionally, in the scattering measurement method, the dielectric layer has at least one groove, each of the grooves penetrates the dielectric layer, the unit to be tested includes at least one opening, each of the openings extends from the surface of the substrate into the substrate, and the opening is connected to the groove.

[0008] Optionally, in the scattering measurement method, the projection shape of each opening on the surface of the substrate is square or circular, and the depth of each opening is 1 μm to 30 μm.

[0009] Optionally, in the scattering measurement method, the dielectric layer also covers the unit to be tested, and the unit to be tested includes at least one buried structure, and each of the buried structures extends from the surface of the substrate into the substrate.

[0010] Optionally, in the scattering measurement method, the material of the embedded structure is at least one of silicon oxide, silicon nitride, silicon oxynitride and silicon fluoride; and the cross-sectional shape of the embedded structure is an inverted trapezoid or a square.

[0011] Optionally, in the scattering measurement method, the substrate is made of single crystal silicon.

[0012] Optionally, in the scattering measurement method, when the infrared measurement light with a wide band is used to irradiate the substrate, the incident angle of the infrared measurement light is 45° to 90°.

[0013] Based on the same inventive concept, the present invention also provides a scattering measurement device, including: a light source, used to provide wide-band infrared measurement light, the infrared measurement light is transmitted through the surface of the substrate to irradiate the unit to be measured in the substrate, and the unit to be measured penetrates a part of the thickness of the substrate, wherein the wavelength of the infrared measurement light ranges from 2μm to 7.5μm or 25μm to 35μm; a detector, used to receive the infrared measurement light scattered from the substrate and the unit to be measured, so as to obtain the characteristic parameters of the unit to be measured based on the infrared measurement light, wherein the characteristic parameters include at least one of diameter, width, depth and side wall angle.

[0014] In the scattering measurement method and scattering measurement device provided by the present invention, a wide-band infrared measurement light is first used to irradiate the substrate, and the infrared measurement light is irradiated to the unit to be measured through the surface of the substrate, wherein the wavelength of the infrared measurement light has a value range of 2μm~7.5μm or 25μm~35μm; then, the infrared measurement light scattered from the substrate and the unit to be measured is received to obtain the characteristic parameters of the unit to be measured according to the infrared measurement light, and the characteristic parameters include at least one of the diameter, width, depth and sidewall angle. Since the wavelength of the infrared measurement light has a value range of 2μm~7.5μm or 25μm~35μm, the infrared measurement light can effectively penetrate the substrate and irradiate the unit to be measured, so that the infrared measurement light scattered by the substrate and the unit to be measured can effectively reflect the deep characteristic information of the substrate and the unit to be measured in the substrate, thereby improving the sensitivity of measuring the deep characteristics inside the substrate, so that the characteristic parameters of the unit to be measured in the substrate can be accurately and effectively obtained. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 4 is a flow chart of a scattering measurement method according to an embodiment of the present invention.

[0016] Figure 2 It is a cross-sectional schematic diagram of a substrate and a unit to be measured formed in a scattering measurement method according to an embodiment of the present invention.

[0017] Figure 3 It is a schematic diagram of the principle of irradiating a substrate with infrared measuring light in a scattering measurement method according to an embodiment of the present invention.

[0018] Figure 4 It is a cross-sectional schematic diagram of a substrate and a unit to be measured formed in a scattering measurement method according to another embodiment of the present invention.

[0019] Figure 5 It is a schematic diagram of the principle of irradiating a substrate with infrared measuring light in a scattering measurement method according to another embodiment of the present invention.

[0020] Figure 6 It is a schematic diagram of the relationship between the wavelength of infrared measurement light and the light transmittance of the substrate in the scattering measurement method according to an embodiment of the present invention.

[0021] Figure 7 It is a schematic diagram of the principle of a scattering measurement device provided in an embodiment of the present invention.

[0022] In the figure, 100 - substrate; 110 - unit under test; 111 - opening; 112 - buried structure; 120 - dielectric layer; 120a - first dielectric layer; 120b - second dielectric layer; 121 - groove; 200 - light source; 210 - detector. DETAILED DESCRIPTION

[0023] The scatterometry method and scatterometry device proposed by the present invention are further described in detail below in conjunction with the accompanying drawings and specific embodiments. The advantages and features of the present invention will become more apparent from the following description. It should be noted that the accompanying drawings are all in a very simplified form and are not in precise proportions, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.

[0024] Figure 1 FIG. 1 is a flow chart of a scattering measurement method according to an embodiment of the present invention. Figure 1 As shown, this embodiment provides a scattering measurement method, including: step S1: providing a substrate, wherein a unit to be measured is formed in the substrate, and the unit to be measured penetrates a portion of the thickness of the substrate; step S2: irradiating the substrate with wide-band infrared measurement light, wherein the infrared measurement light is irradiated to the unit to be measured through the surface of the substrate, wherein the wavelength of the infrared measurement light ranges from 2μm to 7.5μm or 25μm to 35μm; step S3: receiving infrared measurement light scattered from the substrate and the unit to be measured, so as to obtain characteristic parameters of the unit to be measured according to the infrared measurement light, wherein the characteristic parameters include at least one of diameter, width, depth and sidewall angle.

[0025] Figure 2 It is a cross-sectional schematic diagram of a substrate and a unit to be measured formed in a scattering measurement method according to an embodiment of the present invention. Figure 3 It is a schematic diagram of the principle of irradiating a substrate with infrared measuring light in a scattering measurement method according to an embodiment of the present invention. Figure 4 It is a cross-sectional schematic diagram of a substrate and a unit to be measured formed in a scattering measurement method according to another embodiment of the present invention. Figure 5 FIG. 1 is a schematic diagram showing the principle of the infrared measurement light irradiating the substrate in the scattering measurement method according to another embodiment of the present invention. Figure 2~Figure 5 The scattering measurement method provided in this embodiment is described in more detail.

[0026] like Figure 2 As shown, step S1 is performed to provide a substrate 100 , wherein the material of the substrate 100 may be single crystal silicon.

[0027] Next, a unit under test 110 is formed in the substrate 100 , and the unit under test 110 penetrates a portion of the thickness of the substrate 100 .

[0028] In one embodiment, Figure 2As shown, the unit under test 110 includes at least one opening 111, each of which extends from the surface of the substrate 100 into the substrate 100, wherein the opening 111 can be used as a deep trench or a contact hole. The method for forming the unit under test 110 includes: first, forming at least one dielectric layer 120 on the substrate 100, and the dielectric layer 120 covers the substrate 100. For example, one dielectric layer, two dielectric layers, or three dielectric layers can be formed. The material of the dielectric layer 120 is at least one of silicon oxide, silicon nitride, silicon oxynitride, and silicon fluoride. When more than two dielectric layers 120 are formed on the substrate 100, all dielectric layers 120 are stacked in sequence, and the materials of two adjacent dielectric layers 120 can be different. Among them, the total thickness of the dielectric layer 120 can be 0.01μm~1μm.

[0029] Then, a patterned photoresist layer (not shown) is formed on the dielectric layer 120, and the patterned photoresist layer exposes a portion of the dielectric layer 120. Figure 2 As shown, the patterned photoresist layer is used as a mask, and a dry etching process is adopted to etch the dielectric layer 120 to form at least one groove 121, each of which penetrates the dielectric layer 120, and each of which exposes a portion of the substrate 100; then, the exposed substrate 100 is etched to form at least one opening 111, and the opening 111 extends from the surface of the substrate 100 into the substrate 100, and the opening 111 is connected to the groove 121.

[0030] The number of openings 111 in the unit under test 110 may be, for example, two, three, or six, but is not limited thereto, and may be set according to specific process requirements. The depth D of each opening 111 is 1 μm to 30 μm, for example, 1 μm, 2 μm, 3 μm, 5 μm, 10 μm, 12 μm, 15 μm, 20 μm, 25 μm or 30 μm. The diameter of the opening 111 may be, for example, 0.01 μm to 1 μm, the width of the opening 111 may be, for example, 0.01 μm to 1 μm, and the sidewall angle θ of the opening 111 may be, for example, 85° to 90°, but is not limited thereto, and the diameter, width and sidewall angle of the opening 111 may be set according to actual process requirements. The cross-sectional shape of each opening 111 in the thickness direction of the substrate 100 may be a square or an inverted trapezoid, and the projection shape of each opening 111 on the surface of the substrate 100 may be a square or a circle.

[0031] In another embodiment, Figure 4As shown, the unit under test 110 includes at least one buried structure 112, each of which extends from the surface of the substrate 100 into the substrate 100. Specifically, the method for forming the unit under test 110 includes: first, forming a patterned photoresist layer on the substrate 100, wherein the patterned photoresist layer exposes a portion of the substrate 100; then, using the patterned photoresist layer as a mask, a dry etching process is used to etch a portion of the thickness of the substrate 100 to form at least one groove, wherein the cross-sectional shape of the groove may be a square or an inverted trapezoid; then, a buried layer is filled in the groove to form a buried structure 112; wherein the material of the buried structure 112 is at least one of silicon oxide, silicon nitride, silicon oxynitride, silicon fluoride, polysilicon and metal. The material of all the buried structures 112 may be the same. The depth of the buried structure 112 in the substrate 100, i.e., the thickness of the buried structure 112, may be 1 μm to 30 μm, for example, 1 μm, 2 μm, 3 μm, 5 μm, 10 μm, 12 μm, 15 μm, 20 μm, 25 μm or 30 μm. The cross-sectional shape of the buried structure 112 may be square or inverted trapezoidal. In this embodiment, the cross-sectional shape of the buried structure 112 is square as an example for description.

[0032] Afterwards, at least one dielectric layer 120 is formed on the substrate 100. The dielectric layer 120 covers the unit under test 110, that is, the dielectric layer 120 covers the substrate 100 and all the embedded structures 112. Among them, one dielectric layer 120, two dielectric layers 120 or three dielectric layers 120 can be formed on the substrate 100. For example, a first dielectric layer 120a and a second dielectric layer 120b can be formed on the substrate 100. It should be noted that the number of layers of the dielectric layer 120 is not limited and can be set according to process requirements. The material of the dielectric layer 120 is at least one of silicon oxide, silicon nitride, silicon oxynitride and silicon fluoride. When more than two dielectric layers 120 are formed on the substrate 100, all dielectric layers 120 are stacked in sequence, and the materials of two adjacent dielectric layers 120 can be different. For example, the materials of the first dielectric layer 120a and the second dielectric layer 120b can be different.

[0033] Next, execute step S2, such as Figure 3As shown, a wide-band infrared measurement light is used to illuminate the substrate 100, and the infrared measurement light is transmitted through the surface of the substrate 100 to illuminate the unit to be tested 110, wherein the infrared measurement light is a wide-band infrared light, and its wavelength range is within the range of 2μm~7.5μm, so as to achieve low absorption and low attenuation of the infrared measurement light by the substrate 100, thereby improving the light transmittance of the substrate 100. Preferably, the wavelength of the infrared measurement light can range from 2.5μm to 7μm.

[0034] Alternatively, the infrared measurement light is a wide-band infrared light with a wavelength in the range of 25 μm to 35 μm, so as to achieve low absorption and low attenuation of the infrared measurement light by the substrate 100, thereby improving the light transmittance of the substrate 100. Optionally, the wavelength of the infrared measurement light may be in the range of 29 μm to 35 μm.

[0035] In this embodiment, Figure 3 and Figure 5 As shown, when the infrared measurement light of a wide band is used to irradiate the substrate 100, the infrared measurement light is irradiated from the surface of the dielectric layer 120 through the dielectric layer 120 to the substrate 100, and further irradiated through the substrate 100 to the unit to be tested 110. Specifically, the infrared measurement light is emitted from a light source, and the light source can be a thermal radiation light source or a light emitting diode. In the process of irradiating the substrate 100 with the infrared measurement light, the infrared measurement light is first irradiated to the surface of the dielectric layer 120, and part of the infrared measurement light is irradiated to the substrate 100 below the dielectric layer 120 through the surface of the dielectric layer 120. After the infrared measurement light is irradiated to the substrate 100, it can further irradiate through the substrate 100 to the unit to be tested 110 in the substrate 100, that is, the infrared measurement light can penetrate the substrate 100 without being completely absorbed, and irradiate to the bottom of the unit to be tested 110, thereby irradiating to the bottom of the opening 111 in the unit to be tested 110 or the bottom of the buried structure 112.

[0036] In this embodiment, Figure 3 As shown, the incident angle α of the infrared measurement light is 45° to 90°, preferably, the incident angle α can be 55° to 65°, so as to reduce the error caused by the incident angle and improve the measurement accuracy. The incident angle α is the angle between the infrared measurement light and the normal line of the surface of the substrate 100, that is, the angle between the infrared measurement light and the vertical direction.

[0037] Figure 6 FIG. 1 is a schematic diagram showing the relationship between the wavelength of the infrared measurement light and the light transmittance of the substrate in the scattering measurement method according to an embodiment of the present invention. Figure 6As shown, the wavelength of the infrared measuring light ranges from 2μm to 7.5μm or from 25μm to 35μm. The infrared measuring light has a high transmittance through the substrate. Therefore, it can effectively penetrate the substrate 100 to irradiate the unit to be tested 110, so that the infrared measuring light can reach the bottom of the unit to be tested 110. When the infrared measuring light is scattered in the substrate 100 and the unit to be tested 110, the infrared measuring light scattered by the substrate 100 and the unit to be tested 110 can effectively reflect the deep feature information of the substrate 100 and the unit to be tested 110 in the substrate 100, thereby providing a more accurate measurement result.

[0038] Next, step S3 is performed to receive infrared measurement light scattered from the substrate 100 and the unit to be tested 110, that is, to receive scattered light from the substrate 100 and the unit to be tested 110, so as to obtain characteristic parameters of the unit to be tested 110 according to the infrared measurement light, wherein the characteristic parameters include at least one of diameter, width, depth and sidewall angle.

[0039] In this embodiment, the infrared measurement light scattered from the substrate 100 and the unit to be tested 110 may be received by a detector, and the detector may be, for example, an image sensor. After receiving the infrared measurement light scattered from the substrate 100 and the unit to be tested 110, a model algorithm may be used to analyze the infrared measurement light scattered from the substrate 100 and the unit to be tested 110, that is, to analyze the spectrum of the scattered light scattered from the substrate 100 and the unit to be tested 110, thereby obtaining characteristic parameters of the unit to be tested 110, wherein the model algorithm may be a rigorous coupled wave method (RCWA) or a regression analysis method, etc.

[0040] In this embodiment, the diameter of the unit under test 110 refers to the diameter of the opening 111 or the embedded structure 112 in the unit under test 110 (or the length of the embedded structure 112); the width of the unit under test 110 refers to the width of the opening 111 or the embedded structure 112 in the unit under test 110; the depth of the unit under test 110 refers to the depth of the opening 111 in the unit under test 110, or the depth of the embedded structure 112 in the substrate 100, that is, the thickness of the embedded structure 112; the sidewall angle of the unit under test 110 refers to the angle between the bottom and the sidewall of the opening 111 in the unit under test 110, or the angle between the bottom and the sidewall of the embedded structure 112 in the unit under test 110.

[0041] In the aforementioned step of irradiating the substrate 100 with wide-band infrared measurement light, the wavelength of the infrared measurement light is in the range of 2μm to 7.5μm or 25μm to 35μm, so that the infrared measurement light can effectively penetrate the substrate 100 and irradiate the unit to be tested 110. Therefore, the infrared measurement light scattered by the substrate 100 and the unit to be tested 110 can effectively reflect the deep feature information of the substrate and the unit to be tested 110 in the substrate 100, thereby improving the sensitivity of measuring the deep features inside the substrate.

[0042] Exemplarily, the depth of the opening 111 in the unit to be measured 110 is 3um, and the characteristic parameters (diameter, width, depth and sidewall angle) of the unit to be measured are measured using broadband visible light with a wavelength of 0.3μm-0.9μm, and the measurement sensitivity is 0.023. The characteristic parameters of the unit to be measured are measured using infrared measurement light with a wavelength range of 2μm~7.5μm or 25μm~35μm provided in this embodiment, and the measurement sensitivity is at least 0.381. It can be seen that the scattering measurement method provided in this embodiment can improve the sensitivity of measuring deep features inside the substrate, so that the characteristic parameters of the unit to be measured in the substrate can be accurately and effectively obtained.

[0043] Figure 7 Schematic diagram of the principle of the scattering measurement device provided by the embodiment of the present invention. Figure 7 As shown, this embodiment provides a scattering measurement device, including a light source 200, which is used to provide a wide-band infrared measurement light, the infrared measurement light is transmitted through the surface of the substrate 100 to irradiate the unit to be tested 110 in the substrate 100, and the unit to be tested 110 passes through a part of the thickness of the substrate 100, wherein the wavelength of the infrared measurement light ranges from 2μm to 7.5μm or 25μm to 35μm. The light source 200 can be a thermal radiation light source or a light-emitting diode. The detector 210 is used to receive the infrared measurement light scattered from the substrate 100 and the unit to be tested 110, so as to obtain the characteristic parameters of the unit to be tested 110 according to the infrared measurement light, wherein the characteristic parameters include at least one of diameter, width, depth and sidewall angle. The detector 210 can be an image sensor, for example, a complementary metal oxide semiconductor (CMOS) or a charge coupled device (CCD).

[0044] In this embodiment, a dielectric layer 120 is formed on the substrate 100, and the detector 210 is located above the dielectric layer 120 and is spaced apart from the dielectric layer 120. The receiving angle β of the detector 210 may be 30° to 70°, preferably 45° to 55°, so as to increase the intensity of the received infrared measurement light scattered from the substrate 100 and the unit under test 110, and improve the measurement accuracy.

[0045] In summary, in the scattering measurement method and scattering measurement device provided by the present invention, a wide-band infrared measurement light is first used to irradiate the substrate, and the infrared measurement light is irradiated to the unit to be measured through the surface of the substrate, wherein the wavelength of the infrared measurement light has a value range of 2μm~7.5μm or 25μm~35μm; then, the infrared measurement light scattered from the substrate and the unit to be measured is received to obtain the characteristic parameters of the unit to be measured according to the infrared measurement light. Since the wavelength of the infrared measurement light has a value range of 2μm~7.5μm or 25μm~35μm, the infrared measurement light can effectively penetrate the substrate to irradiate the unit to be measured, so that the infrared measurement light scattered by the substrate and the unit to be measured can effectively reflect the deep characteristic information of the substrate and the unit to be measured in the substrate, thereby improving the sensitivity of measuring the deep characteristics inside the substrate, so that the characteristic parameters of the unit to be measured in the substrate can be accurately and effectively obtained.

[0046] The above description is only a description of the preferred embodiments of the present invention, and is not intended to limit the scope of the present invention. Any changes or modifications made by a person skilled in the art in the field of the present invention based on the above disclosure shall fall within the scope of protection of the claims.

[0047] In addition, it should be recognized that although the present invention has been disclosed as a preferred embodiment, the above embodiment is not intended to limit the present invention. For any technician familiar with the art, without departing from the scope of the technical solution of the present invention, the technical content disclosed above can be used to make many possible changes and modifications to the technical solution of the present invention, or modified into equivalent embodiments of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiment according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still belongs to the scope of protection of the technical solution of the present invention.

Claims

1. A scatterometry method, It is characterized in that include: A substrate is provided, wherein a unit to be tested is formed in the substrate, the unit to be tested penetrates a portion of the thickness of the substrate, and at least one dielectric layer is formed on the substrate, wherein the unit to be tested includes at least one buried structure, each of the buried structures extends from the surface of the substrate into the substrate, the thickness of each of the buried structures is 1 μm to 30 μm, and the dielectric layer also covers the buried structure in the unit to be tested, the buried structure is made of at least one of silicon oxide, silicon nitride, silicon oxynitride, silicon fluoride, polycrystalline silicon and metal, and the substrate is made of single crystal silicon; Using a wide-band infrared measurement light to irradiate the substrate, the infrared measurement light is irradiated from the surface of the dielectric layer through the dielectric layer and the surface of the substrate to the bottom of the embedded structure in the unit to be tested, wherein the wavelength of the infrared measurement light ranges from 2 μm to 7.5 μm or from 25 μm to 35 μm; Infrared measurement light scattered from the substrate and the unit to be tested is received to obtain characteristic parameters of the unit to be tested according to the infrared measurement light, wherein the characteristic parameters include at least one of a diameter, a width, a depth and a sidewall angle of the buried structure.

2. The scatterometry method according to claim 1, It is characterized in that The dielectric layer is made of at least one of silicon oxide, silicon nitride, silicon oxynitride and silicon fluoride.

3. The scattering measurement method according to claim 1, It is characterized in that The cross-sectional shape of the embedded structure is an inverted trapezoid or a square.

4. The scatterometry method according to claim 1, It is characterized in that When the infrared measuring light with a wide wavelength is used to irradiate the substrate, the incident angle of the infrared measuring light is 45° to 90°.

5. A scattering measurement device, It is characterized in that include: A light source, used for providing infrared measurement light of a wide band, wherein the infrared measurement light is irradiated from the surface of the dielectric layer on the substrate through the dielectric layer and the surface of the substrate to the bottom of the unit to be measured in the substrate, wherein the unit to be measured penetrates a part of the thickness of the substrate, wherein the unit to be measured comprises at least one buried structure, wherein each buried structure extends from the surface of the substrate into the substrate, wherein the thickness of each buried structure is 1 μm to 30 μm, and wherein the dielectric layer also covers the buried structure in the unit to be measured, wherein the material of the buried structure is at least one of silicon oxide, silicon nitride, silicon oxynitride, silicon fluoride, polycrystalline silicon and metal, and the material of the substrate is single crystal silicon, wherein the wavelength of the infrared measurement light has a value range of 2 μm to 7.5 μm or 25 μm to 35 μm; A detector is used to receive infrared measurement light scattered from the substrate and the unit to be tested, so as to obtain characteristic parameters of the unit to be tested according to the infrared measurement light, wherein the characteristic parameters include at least one of the diameter, width, depth and sidewall angle of the buried structure.

Citation Information

Patent Citations

  • Methods and apparatus for calculating electromagnetic scattering properties of a structure and for estimation of geometrical and material parameters thereof

    CN105765463A

  • Thin-film material phase transition temperature measurement device and method

    CN109001160A

  • Infrared spectroscopic reflectometer for measurement of high aspect ratio structures

    CN109690235A

  • Dielectric grating based infrared low reflection subwavelength structure

    CN110261947A

  • Methods and systems for measurement of thick films and high aspect ratio structures

    CN110313059A