Fluid stirring composite material hot extrusion device and method
The metal jet impeller-less stirring technology of the fluid stirring composite material hot extrusion device solves the problems of wettability and agglomeration of nano-silicon carbide ceramic particles in the hot extrusion process of silicon-aluminum alloy, improves the mechanical properties of composite materials and extends the service life of glass lubricants.
Patent Information
- Application Number
- CN202410946416.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2044-07-16
AI Technical Summary
During the hot extrusion process of silicon-aluminum alloy reinforced with nano-silicon carbide ceramic particles, there are problems such as poor wettability between nano-silicon carbide ceramic particles and silicon-aluminum alloy matrix, difficulty in controlling agglomeration, poor stirring and dispersion effect, and thermal stress corrosion of solid glass lubricating parts during stirring.
A fluid-stirred composite material hot extrusion device is used. Through metal jet impeller-free stirring technology, the molten metal jet ejected from the jet orifice is used to shear jet stir the molten aluminum matrix composite material reinforced with nano-silicon carbide particles, thereby controlling the particle distribution density and avoiding direct contact with solid glass lubricating parts.
It improves the wettability of nano-silicon carbide ceramic particles with silicon-aluminum alloy matrix, avoids agglomeration, enhances the mechanical properties of composite materials, and extends the service life of solid glass lubricants.
Smart Images

Figure CN118492098B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of hot extrusion production of nano-particle ceramic reinforced aluminum-based composite materials, and in particular relates to a fluid stirring composite material hot extrusion device and method. Background Art
[0002] Aluminum-based alloy is a new type of lightweight and heat-resistant structural material with the advantages of light weight, high strength, corrosion resistance, wear resistance, and high temperature resistance. Aluminum-based alloy castings and forgings are mainly used as structural materials for key components of aerospace engines. They can also be used as preformed materials for superplastic forming to prepare parts for aviation and aerospace engines, as well as wings and shells of ultra-high-speed aircraft.
[0003] However, although the addition of silicon carbide ceramic particles to aluminum-based alloys improves room temperature and high temperature mechanical properties, the toughness is seriously reduced. Therefore, people have proposed to add nano-silicon carbide ceramic particles to aluminum-based alloys to enhance the toughness of silicon-aluminum alloy substrates.
[0004] However, in the preparation process of hot extrusion of nano-silicon carbide ceramic particles reinforced silicon-aluminum alloy, the following problems still exist:
[0005] Nano-SiC ceramic particles have poor wettability with Si-Al alloy matrix.
[0006] Nano-SiC ceramic particles are agglomerated, and the distribution density of nano-SiC ceramic particles is difficult to control, which seriously affects the mechanical properties of the composite material.
[0007] The existing paddle rotation stirring method is not suitable for stirring and dispersing nanoparticles in molten metal.
[0008] During the stirring process, nano-silicon carbide ceramic particles reinforce the thermal stress corrosion of silicon-aluminum alloy melt on solid glass lubricated parts.
[0009] Therefore, there is an urgent need for a fluid stirring composite material hot extrusion device and method to effectively solve the deficiencies in the prior art. Summary of the invention
[0010] In view of the above problems, the purpose of the present invention is to provide a fluid-stirred composite material hot extrusion device and method to solve the problems of thermal stress corrosion of solid glass lubricating parts and poor mechanical properties of composite materials in the existing preparation process of nano-silicon carbide ceramic particle reinforced silicon aluminum alloy hot extrusion.
[0011] In order to achieve the above object, the present invention adopts the following technical solutions:
[0012] On one hand, the present invention provides a fluid stirring composite material hot extrusion device, comprising a frame, a lifting drive mechanism, a die, a core punch and a stirring punch, wherein the die and the lifting drive mechanism are arranged on the frame, and the die has a heating cavity and a hot extrusion hole located at the bottom of the heating cavity;
[0013] The lower end of the stirring punch is slidably matched with the inner wall of the heating chamber, and the upper end of the stirring punch is connected to the lifting drive mechanism. The stirring punch is a hollow structure and a jet hole is provided on the lower end surface. When the lifting drive mechanism drives the stirring punch to reciprocate up and down, the metal liquid jet ejected from the jet hole stirs the metal melt in the heating chamber;
[0014] The core punch penetrates the inner cavity of the stirring punch and slides with the stirring punch, and the upper end of the core punch slides with the guide hole provided on the frame; when the stirring punch stirs the molten metal, the core punch descends to block the hot extrusion hole, and the core punch is relatively locked with the frame;
[0015] When the core punch and the stirring punch are locked relative to each other, the lower end of the core punch blocks the jet hole of the stirring punch, and the lifting drive mechanism drives the core punch and the stirring punch to move synchronously. The metal material in the heating chamber that is softened and solidified by process temperature control is hot extruded through the hot extrusion hole.
[0016] In a possible implementation, the heat extrusion hole at the bottom of the heating chamber is funnel-shaped, and a glass lubricating member is provided on the bottom inner wall of the heat extrusion hole.
[0017] In one possible implementation, the stirring punch includes a tube and a transfer plate and a hollow stirring plate connected to the upper and lower ends of the tube, wherein the hollow stirring plate is accommodated in the heating chamber of the die and slidingly cooperates with the inner wall of the heating chamber; the jet holes are arranged on the hollow stirring plate; and the transfer plate is connected to the lifting drive mechanism.
[0018] In one possible implementation, the jet holes include a plurality of outer stirring jet holes arranged circumferentially and a plurality of inner stirring jet holes arranged circumferentially, wherein the inner stirring jet holes are located on the inner side of the outer stirring jet holes, the inner stirring jet holes are inclined outward from top to bottom, and the outer stirring jet holes are inclined inward from top to bottom, and the axes of the inner stirring jet holes and the outer stirring jet holes are non-coplanar.
[0019] In one possible implementation, the core punch includes a center column and a hanging ring and a sealing disk arranged at the upper and lower ends of the center column, wherein the lower end of the center column is inserted into the cylinder and the sealing disk is located below the hollow stirring disk; the sealing disk is used to seal the hot extrusion holes at the bottom of the heating chamber and the jet holes on the hollow stirring disk.
[0020] In one possible implementation, the lower end face of the core punch is axially provided with a Morse taper hole, a sealing core shaft is inserted in the Morse taper hole, and the lower end of the sealing core shaft is a conical surface structure, which is sealed with the hot extrusion hole through the conical surface structure to achieve secondary sealing of the heating chamber.
[0021] In one possible implementation, the die includes a die body and an upper cover arranged on the top of the die body, the hot extrusion hole is arranged at the bottom of the die body, a heating coil is arranged in the side wall of the die body, and the upper cover is provided with internal pressure and atmosphere control holes and feeding holes.
[0022] In one possible implementation, the lifting drive mechanism includes a plurality of hydraulic cylinders arranged along the circumferential direction, the hydraulic cylinder including a hydraulic cylinder body and a hydraulic push rod slidingly matched with the hydraulic cylinder body, wherein the hydraulic cylinder body is fixed on the frame, and the hydraulic push rod is connected to the stirring punch.
[0023] Another aspect of the present invention provides a hot extrusion method using the fluid stirring composite material hot extrusion device as described above, comprising the following steps:
[0024] Step S1: The core convex mold and the stirring convex mold are relatively locked, and the lifting drive mechanism drives the core convex mold and the stirring convex mold to descend to the bottom of the heating chamber, the lower end of the core convex mold blocks the hot extrusion hole, and then the upper end of the core convex mold is locked relative to the frame;
[0025] Step S2: adding nano-silicon carbide particle reinforced aluminum-based composite material powder into the heating chamber and then sealing the chamber, wherein the heating chamber heats the nano-silicon carbide particle reinforced aluminum-based composite material powder to form a nano-silicon carbide particle reinforced aluminum-based composite material melt;
[0026] Step S3: the core punch and the stirring punch are unlocked, and the lifting drive mechanism drives the stirring punch to reciprocate up and down, and the metal liquid jet ejected from the jet hole of the stirring punch performs shear jet stirring on the nano-silicon carbide particle reinforced aluminum-based composite material melt;
[0027] Step S4: the lifting drive mechanism drives the stirring convex mold to rise to the top of the heating chamber;
[0028] Step S5: the core punch is unlocked from the frame, and the core punch is lifted upward by an external lifting device until the core punch seals the jet hole of the stirring punch, and the core punch and the stirring punch are relatively locked;
[0029] Step S6: The heating chamber is subjected to process temperature control to change the nano-silicon carbide particle reinforced aluminum-based composite material melt into a softened solid state;
[0030] Step S7: The lifting drive mechanism drives the core punch and the stirring punch to move downward synchronously, and the softened solid nano-silicon carbide particle reinforced aluminum-based composite material is hot extruded through the hot extrusion hole.
[0031] The advantages and beneficial effects of the present invention are as follows: the present invention provides a fluid stirring composite material hot extrusion device, which adopts metal jet paddleless stirring, improves the wettability of nano silicon carbide ceramic particles and silicon aluminum alloy matrix through long-term stirring, and avoids the agglomeration of silicon carbide ceramic particles, and can well control the distribution density of nano silicon carbide ceramic particles, thereby improving the mechanical properties of the composite material.
[0032] The present invention provides a fluid stirring composite material hot extrusion device and method, which uses metal jets to perform paddleless stirring. Compared with the existing paddle rotating stirring method, since one powered rotating paddle stirring shaft is reduced, the probability of metal material processing being contaminated is further reduced. During the stirring process, the nano-silicon carbide ceramic particle reinforced silicon aluminum alloy melt has no thermal stress corrosion and contact with the solid glass lubricating part, thereby improving the service life of the solid glass lubricating part.
[0033] Other features and advantages of the present invention will be described in the following description, and partly become apparent from the description, or understood by practicing the present invention. The purpose and other advantages of the present invention can be realized and obtained by the structures particularly pointed out in the written description and the accompanying drawings.
[0034] The technical solution of the present invention is further described in detail below through the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:
[0036] Figure 1 This is an axonometric view of a fluid stirring composite material hot extrusion device of the present invention;
[0037] Figure 2 It is a cross-sectional view of a fluid stirring composite material hot extrusion device of the present invention;
[0038] Figure 3 for Figure 2 A partial enlarged schematic diagram in the middle;
[0039] Figure 4 It is an axonometric view of the core punch of the present invention;
[0040] Figure 5 It is one of the axonometric views of the stirring punch in the present invention;
[0041] Figure 6 This is the second axonometric view of the stirring punch in the present invention;
[0042] Figure 7Schematic diagram of jet stirring of the stirring convex mold in the present invention;
[0043] Figure 8 A schematic diagram of a stirring working state of a fluid stirring composite material hot extrusion device of the present invention;
[0044] Fig. 9 for Figure 8 A local enlarged schematic diagram of point B;
[0045] Fig.10 It is a schematic diagram of the extrusion working state of a fluid stirring composite material hot extrusion device of the present invention;
[0046] Fig.11 for Fig.10 A partial enlarged schematic diagram of point C in the middle.
[0047] In the figure: 1-frame, 101-frame positioning hole, 2-lifting drive mechanism, 201-hydraulic push rod, 202-hydraulic cylinder, 3-die, 301-die body, 302-upper cover, 303-internal pressure and atmosphere control hole, 304-feeding hole, 305-heating coil, 306-hot extrusion hole, 4-core punch, 401-center column, 402-sealing disk, 403-upper radial locking hole, 404-lower radial locking hole, 405-Mohs taper hole, 406-lifting ring, 5-stirring punch, 501-adapter plate, 502-cylinder, 503-hollow stirring plate, 504-external stirring jet hole, 505-internal stirring jet hole, 506-center hole, 507-stirring punch positioning hole, 6-glass lubricating part, 7-sealing core shaft, 701-lower extrusion sealing cone shaft, 702-Mohs taper shaft, 703-bottom plane, 8-core punch locking stirring punch device, 9-core punch locking frame device, 10-heating chamber, 11-lower stirring chamber, 12-upper stirring chamber, 14-high-speed jet I, 15-high-speed jet II. DETAILED DESCRIPTION
[0048] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0049] The preferred embodiments of the present invention are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.
[0050] An embodiment of the present invention provides a fluid stirring composite material hot extrusion device, which improves the wettability of nano silicon carbide ceramic particles with silicon aluminum alloy matrix and avoids the agglomeration of silicon carbide ceramic particles, thereby improving the mechanical properties of the composite material. Figures 1 to 11 As shown, the fluid stirring composite material hot extrusion device comprises a frame 1, a lifting drive mechanism 2, a die 3, a core punch 4 and a stirring punch 5, wherein the die 3 and the lifting drive mechanism 2 are arranged on the frame 1, the die 3 has a heating cavity 10 and a hot extrusion hole 306 located at the bottom of the heating cavity 10; the lower end of the stirring punch 5 is slidably matched with the inner wall of the heating cavity 10, the upper end of the stirring punch 5 is connected to the lifting drive mechanism 2, the stirring punch 5 is a hollow structure and a jet hole is provided on the lower end surface, when the lifting drive mechanism 2 drives the stirring punch 5 to reciprocate up and down, the metal liquid jet ejected by the jet hole stirs the metal melt in the heating cavity 10. The core punch 4 penetrates the inner cavity of the stirring punch 5 and is slidably matched with the stirring punch 5, and the upper end of the core punch 4 is slidably matched with the guide hole provided on the frame 1; when the stirring punch 5 stirs the metal melt, the core punch 4 descends to block the hot extrusion hole 306, and the upper end of the core punch 4 is relatively locked with the frame 1 through the core punch locking frame device 9. The core punch 4 is relatively locked with the stirring punch 5 through the core punch locking stirring punch device 8, and the lower end of the core punch 4 blocks the jet hole of the stirring punch 5. The lifting drive mechanism 2 drives the core punch 4 and the stirring punch 5 to move synchronously, and the metal material in the heating chamber 10 that is softened in a solid state through process temperature control is hot extruded through the hot extrusion hole 306.
[0051] See also Figure 1 , Figure 2 As shown, in the embodiment of the present invention, the frame 1 includes a bottom plate, an intermediate plate and a top plate which are arranged in sequence from bottom to top, the bottom plate is fixed to the ground, the bottom plate, the intermediate plate and the top plate are connected by a plurality of columns, the intermediate plate is provided with a mounting hole for mounting the die 3, and the lifting drive mechanism 2 is arranged on the intermediate plate. The top plate is provided with a guide hole for the core punch 4 to pass through, and the core punch 4 and the guide hole form a cylindrical pair.
[0052] See also Fig.11As shown, in the embodiment of the present invention, the die 3 includes a die body 301 and an upper cover 302 arranged on the top of the die body 301, a hot extrusion hole 306 is arranged at the bottom of the die body 301, a heating coil 305 is arranged in the side wall of the die body 301, and the central hole of the upper cover 302 and the cylinder 502 of the stirring punch 5 form a cylindrical hot extrusion pair. The upper cover 302 is provided with an internal pressure and atmosphere control hole 303 and a feeding hole 304, the internal pressure and atmosphere control hole 303 is used to control the gas pressure and composition of the smelting inside the heating chamber 10, and the feeding hole 304 is used to add powder material to the inside of the heating chamber 10. The heating coil 305 can form the powder material inside the heating chamber 10 into a molten alloy melt. The bottom of the die body 301 contains a hot extrusion hole 306, the hot extrusion hole 306 is funnel-shaped, and the bottom inner wall of the hot extrusion hole 306 is provided with a glass lubricating member 6.
[0053] See also Figure 5 , Figure 6 As shown, in an embodiment of the present invention, the stirring punch 5 includes a cylinder 502 and a transfer plate 501 and a hollow stirring plate 503 connected to the upper and lower ends of the cylinder 502, wherein the hollow stirring plate 503 is accommodated in the heating chamber 10 of the die 3 and slidingly cooperates with the inner wall of the heating chamber 10; the jet holes are arranged on the hollow stirring plate 503; the transfer plate 501 is connected to the lifting drive mechanism 2, and the cylinder 502 is provided with a center hole 506.
[0054] Specifically, the jet holes include a plurality of outer stirring jet holes 504 arranged along the circumferential direction and a plurality of inner stirring jet holes 505 arranged along the circumferential direction, wherein the inner stirring jet holes 505 are located on the inner side of the outer stirring jet holes 504, the inner stirring jet holes 505 are inclined outward from top to bottom, and the outer stirring jet holes 504 are inclined inward from top to bottom, that is, the spatial axes of the inner stirring jet holes 505 and the outer stirring jet holes 504 are not parallel to the center line of the hollow stirring disk 503.
[0055] In this embodiment, the hollow stirring disk 503 contains at least sixteen inner stirring jet holes 505 and sixteen outer stirring jet holes 504, and the inner stirring jet holes 505 and the outer stirring jet holes 504 are arranged alternately at intervals, that is, the axes of the inner stirring jet holes 505 and the outer stirring jet holes 504 are not coplanar. When the hollow stirring disk 503 moves at a lifting speed v, due to the area multiple relationship n between the horizontal cross section of the hollow stirring disk 503 and the flow cross section of the jet hole, the outer stirring jet holes 504 and the inner stirring jet holes 505 will respectively eject high-speed jets Ⅰ14 and high-speed jets Ⅱ15 at n×v times the speed. High-speed jets Ⅰ14 and Ⅱ15 will form shear flow stirring vortices in the space perpendicular line segment fluid region, see Figure 7The fluid stirring formed by the high-speed jet I 14, high-speed jet II 15 and the shear flow stirring vortex in the lower stirring chamber 11 can effectively disperse the nano-silicon carbide particles in the aluminum-based melt, thereby effectively solving the problem of agglomeration of nano-reinforced particles in metal-based composite materials.
[0056] See also Figure 4 As shown, in the embodiment of the present invention, the core punch 4 includes a center column 401 and a hanging ring 406 and a sealing disk 402 arranged at the upper and lower ends of the center column 401, wherein the lower end of the center column 401 is inserted into the center hole 506 of the cylinder 502, and the sealing disk 402 is located below the hollow stirring disk 503; the sealing disk 402 is used to block the hot extrusion hole 306 at the bottom of the heating chamber 10 and the jet hole on the hollow stirring disk 503. Preferably, a gap is left between the outer circumference of the sealing disk 402 and the inner wall of the heating chamber 10.
[0057] Further, see Figure 3 , Figure 4 As shown, the lower end surface of the core punch 4 is provided with a Morse taper hole 405 along the axial direction, and a plugging mandrel 7 is inserted in the Morse taper hole 405. The lower end of the plugging mandrel 7 is a conical structure, and the conical structure is sealed with the hot extrusion hole 306 to achieve secondary sealing of the heating chamber 10. The plugging mandrel 7 has a double insurance effect to prevent the sealing disk 402 from micro-seeping high-temperature alloy liquid under the bottom and damaging the glass lubricating part 6.
[0058] Specifically, the plugging mandrel 7 includes a coaxially arranged lower extrusion plugging cone shaft 701 and a Morse taper shaft 702, the outer circumferential surface of the lower extrusion plugging cone shaft 701 is the above-mentioned cone surface structure, and the Morse taper shaft 702 is inserted into the Morse taper hole 405. Preferably, the material of the core punch 4 is metal, and the material of the plugging mandrel 7 is ceramic. As the process temperature changes, the material expansion coefficients of the core punch 4 and the plugging mandrel 7 are different. Therefore, during the heating stage of the heating chamber 10, the Morse taper shaft 702 and the Morse taper hole 405 are in a gap loose state to avoid the plugging mandrel 7 from bursting. After the metal jet is stirred and combined, the bottom plane 703 of the plugging mandrel 7 is knocked on the outside of the hot extrusion hole 306 to make the lower extrusion plugging cone shaft 701 out of contact with the hot extrusion hole 306, and at the same time, the Morse taper shaft 702 and the Morse taper hole 405 are tightly fitted.
[0059] See also Figure 1 , Figure 2 As shown, in the embodiment of the present invention, the lifting drive mechanism 2 includes a plurality of hydraulic cylinders arranged along the circumferential direction, the hydraulic cylinder includes a hydraulic cylinder body 202 and a hydraulic push rod 201 slidably matched with the hydraulic cylinder body 202, wherein the hydraulic cylinder body 202 is fixed on the frame 1, and the hydraulic push rod 201 is connected to the stirring convex mold 5. The plurality of hydraulic cylinders synchronously drive the stirring convex mold 5 to lift relative to the frame 1.
[0060] In the embodiment of the present invention, the core punch locking frame device 9 and the core punch locking stirring punch device 8 are both locking bolts, the guide hole side wall of the frame 1 is provided with a frame positioning hole 101, the core punch 4 is provided with an upper radial locking hole 403 and a lower radial locking hole 404, the core punch locking frame device 9 passes through the frame positioning hole 101 and is inserted into the upper radial locking hole 403, so as to achieve the relative locking of the core punch 4 and the frame 1. The outer side wall of the adapter plate 501 is provided with a stirring punch positioning hole 507, the core punch locking stirring punch device 8 passes through the stirring punch positioning hole 507 and is inserted into the lower radial locking hole 404 of the core punch 4, so as to achieve the relative locking of the core punch 4 and the stirring punch 5.
[0061] In this embodiment, the glass lubricating member 6 is installed in the hot extrusion hole 306 of the concave mold 3, and the glass lubricating member 6 is in the shape of a funnel. The glass lubricating member 6 is a consumable material, and it is particularly cumbersome to replace the glass lubricating member 6. The replacement of the glass lubricating member 6 requires the disassembly of many parts above it, so it is very necessary to increase the service life of the glass lubricating member 6.
[0062] Due to process reasons, the time for heating and stirring the nano-silicon carbide particle reinforced aluminum-based composite material is many times longer than the time for hot extrusion. In the heating and stirring process of the metal composite material, the present invention seals the hot extrusion hole 306 through the sealing disk 402 of the core punch 4, and seals and cooperates with the hot extrusion hole 306 through the lower extrusion sealing cone shaft 701 of the sealing mandrel 7, thereby realizing the secondary sealing of the heating chamber 10. In this way, the metal composite material in the heating chamber 10 does not contact the glass lubricating member 6 during the heating and stirring process, which alleviates the glass lubricating member 6 from being corroded by thermal stress and fluid, and improves the service life of the glass lubricating member 6, thereby improving the surface quality of the nano-silicon carbide particle reinforced aluminum-based composite material.
[0063] The present invention provides a fluid-stirred composite material hot extrusion device, which adopts metal jet paddleless stirring, improves the wettability of nano-silicon carbide ceramic particles and silicon-aluminum alloy matrix through long-term stirring, and avoids the agglomeration of silicon carbide ceramic particles. It can well control the distribution density of nano-silicon carbide ceramic particles, thereby improving the mechanical properties of the composite material.
[0064] Based on the above design concept, another embodiment of the present invention provides a fluid stirring composite material hot extrusion method, which is implemented using the fluid stirring composite material hot extrusion device provided in the above embodiment. Figures 1 to 11 As shown, the fluid stirring composite material hot extrusion method comprises the following steps:
[0065] Step S1: The core punch 4 and the stirring punch 5 are relatively locked, and the lifting drive mechanism 2 drives the core punch 4 and the stirring punch 5 to descend to the bottom of the heating chamber 10, and the sealing disk 402 of the core punch 4 is fitted with the upper end surface of the hot extrusion hole 306, and the hot extrusion hole 306 is pressed and sealed, and then the upper end of the core punch 4 is locked relative to the frame 1; at this time, the gap between the Morse taper shaft 702 of the sealing core shaft 7 and the Morse taper hole 405 of the core punch 4 is loose, and the inner wall of the glass lubricating member 6 is in contact with the external air for cooling, see Figure 2 , Figure 3 shown.
[0066] Step S2: adding nano-silicon carbide particle reinforced aluminum-based composite material powder into the heating chamber 10 and then sealing the chamber, wherein the heating chamber 10 heats the nano-silicon carbide particle reinforced aluminum-based composite material powder to form a nano-silicon carbide particle reinforced aluminum-based composite material melt;
[0067] Specifically, the smelting auxiliary equipment controls the internal pressure and atmosphere of the heating chamber 10 through the internal pressure and atmosphere control hole 303, and controls the solid powder by adding trace element materials in the smelting process through the feeding hole 304. The heating coil 305 inside the die body 301 can form the internal powder material into a molten alloy melt.
[0068] Step S3: the core punch 4 and the stirring punch 5 are unlocked, and the lifting drive mechanism 2 drives the stirring punch 5 to reciprocate up and down, and the metal liquid jet ejected from the jet hole of the stirring punch 5 performs shear jet stirring on the nano-silicon carbide particle reinforced aluminum-based composite material melt;
[0069] Specifically, the hollow stirring plate 503 of the stirring convex mold 5 divides the heating chamber 10 into a lower stirring chamber 11 and an upper stirring chamber 12. The up and down movement of the hollow stirring plate 503 performs paddle-free liquid metal shear jet stirring on the nano-SiC particle reinforced aluminum-based composite material melt in the lower stirring chamber 11 and the upper stirring chamber 12. Figure 8 , Fig. 9 shown.
[0070] Step S4: the lifting drive mechanism 2 drives the stirring convex mold 5 to rise to the top of the heating chamber 10;
[0071] Specifically, before the stirring punch 5 rises, a cylindrical tool is first used to knock the bottom plane 703 of the sealing core shaft 7 from bottom to top through the center of the glass lubricating part 6, so that the lower extrusion sealing cone shaft 701 of the sealing core shaft 7 is released from the fit with the hot extrusion hole 306, and at the same time, the Morse taper shaft 702 of the sealing core shaft 7 is taper-locked with the Morse taper hole 405 of the core punch 4.
[0072] Step S5: The core punch 4 is unlocked from the frame 1, and the external lifting equipment lifts the core punch 4 upwards through the lifting ring 406 until the upper end surface of the sealing disk 402 of the core punch 4 seals the jet hole of the hollow stirring disk 503, and then the core punch 4 and the stirring punch 5 are relatively locked, and the external lifting equipment is evacuated.
[0073] Step S6: The heating chamber 10 is subjected to process temperature control to change the nano-silicon carbide particle reinforced aluminum-based composite material melt into a softened solid state.
[0074] Step S7: The lifting drive mechanism 2 drives the core punch 4 and the stirring punch 5 to move downward synchronously, and the softened solid nano-silicon carbide particle reinforced aluminum-based composite material is hot extruded through the hot extrusion hole 306, see Fig.10 , Fig.11 shown.
[0075] In the embodiments of the present invention, the prediction of the paddleless liquid metal shear jet stirring effect of the nano-silicon carbide particle reinforced aluminum-based composite melt can be simulated by flow field analysis software. The quantification of the paddleless liquid metal shear jet stirring effect of the nano-silicon carbide particle reinforced aluminum-based composite melt can be subsequently observed microscopically by metallurgical inspection means and quantitatively analyzed by macroscopic mechanical means. A characterization relationship is established between the metal melt shear flow stirring process and simulation analysis, hot extrusion lubrication effect, microscopic metallographic structure, and macroscopic mechanical properties of the nano-silicon carbide particle reinforced aluminum-based composite material.
[0076] The present invention provides a fluid stirring composite material hot extrusion device and method, which uses metal jets to perform paddleless stirring. Compared with the existing paddle rotating stirring method, since one powered rotating paddle stirring shaft is reduced, the probability of metal material processing being contaminated is further reduced. During the stirring process, the nano-silicon carbide ceramic particle reinforced silicon aluminum alloy melt has no thermal stress corrosion and contact corrosion on the solid glass lubricating parts, thereby improving the service life of the solid glass lubricating parts.
[0077] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A fluid stirring composite material hot extrusion device, characterized in that: The invention comprises a frame (1), a lifting drive mechanism (2), a concave mold (3), a core convex mold (4) and a stirring convex mold (5), wherein the concave mold (3) and the lifting drive mechanism (2) are arranged on the frame (1), and the concave mold (3) has a heating cavity (10) and a hot extrusion hole (306) located at the bottom of the heating cavity (10); The lower end of the stirring punch (5) is slidably matched with the inner wall of the heating chamber (10), the upper end of the stirring punch (5) is connected to the lifting drive mechanism (2), the stirring punch (5) is a hollow structure and a jet hole is provided on the lower end surface, and when the lifting drive mechanism (2) drives the stirring punch (5) to reciprocate up and down, the metal liquid jet ejected from the jet hole stirs the metal melt in the heating chamber (10); The core punch (4) penetrates the inner cavity of the stirring punch (5) and is slidably matched with the stirring punch (5), and the upper end of the core punch (4) is slidably matched with a guide hole provided on the frame (1); when the stirring punch (5) stirs the molten metal, the core punch (4) descends to block the hot extrusion hole (306), and the core punch (4) and the frame (1) are relatively locked; When the core punch (4) and the stirring punch (5) are locked relative to each other, the lower end of the core punch (4) blocks the jet hole of the stirring punch (5), and the lifting drive mechanism (2) drives the core punch (4) and the stirring punch (5) to move synchronously, and the metal material in the heating chamber (10) that is softened and solidified by process temperature control passes through the hot extrusion hole (306) and is hot extruded into shape.
2. The fluid stirring composite material hot extrusion device according to claim 1 is characterized in that: The hot extrusion hole (306) at the bottom of the heating chamber (10) is in a funnel shape, and a glass lubricating member (6) is provided on the inner wall at the bottom of the hot extrusion hole (306).
3. The fluid stirring composite material hot extrusion device according to claim 1, characterized in that: The stirring convex mold (5) comprises a cylinder (502) and a transfer plate (501) and a hollow stirring plate (503) connected to the upper and lower ends of the cylinder (502), wherein the hollow stirring plate (503) is accommodated in the heating chamber (10) of the concave mold (3) and slidably cooperates with the inner wall of the heating chamber (10); the jet holes are arranged on the hollow stirring plate (503); and the transfer plate (501) is connected to the lifting drive mechanism (2).
4. The fluid stirring composite material hot extrusion device according to claim 3 is characterized in that: The jet holes include a plurality of outer stirring jet holes (504) arranged along the circumferential direction and a plurality of inner stirring jet holes (505) arranged along the circumferential direction, wherein the inner stirring jet holes (505) are located inside the outer stirring jet holes (504), the inner stirring jet holes (505) are inclined outward from top to bottom, and the outer stirring jet holes (504) are inclined inward from top to bottom, and the axes of the inner stirring jet holes (505) and the outer stirring jet holes (504) are not coplanar.
5. The fluid stirring composite material hot extrusion device according to claim 3 is characterized in that: The core punch (4) comprises a central column (401) and hanging rings (406) and a sealing disk (402) arranged at the upper and lower ends of the central column (401), wherein the lower end of the central column (401) is inserted into the cylinder (502), and the sealing disk (402) is located below the hollow stirring disk (503); the sealing disk (402) is used to seal the hot extrusion hole (306) at the bottom of the heating chamber (10) and to seal the jet hole on the hollow stirring disk (503).
6. The fluid-stirring composite material hot extrusion device according to claim 5, characterized in that: The lower end surface of the core punch (4) is provided with a Morse taper hole (405) along the axial direction, a plugging mandrel (7) is inserted into the Morse taper hole (405), and the lower end of the plugging mandrel (7) is a conical surface structure, which is sealed with the hot extrusion hole (306) through the conical surface structure to achieve secondary sealing of the heating chamber (10).
7. The fluid-stirring composite material hot extrusion device according to claim 1, characterized in that: The die (3) comprises a die body (301) and an upper cover (302) arranged on the top of the die body (301); the hot extrusion hole (306) is arranged at the bottom of the die body (301); a heating coil (305) is arranged in the side wall of the die body (301); and an internal pressure and atmosphere control hole (303) and a material feeding hole (304) are arranged on the upper cover (302).
8. The fluid-stirring composite material hot extrusion device according to claim 1, characterized in that: The lifting drive mechanism (2) comprises a plurality of hydraulic cylinders arranged along the circumferential direction, the hydraulic cylinder comprising a hydraulic cylinder body (202) and a hydraulic push rod (201) slidably engaged with the hydraulic cylinder body (202), wherein the hydraulic cylinder body (202) is fixed on the frame (1), and the hydraulic push rod (201) is connected to the stirring convex mold (5).
9. A hot extrusion method using the fluid stirring composite material hot extrusion device according to any one of claims 1 to 8, characterized in that: The following steps are involved: Step S1: the core punch (4) and the stirring punch (5) are locked relative to each other, the lifting drive mechanism (2) drives the core punch (4) and the stirring punch (5) to descend to the bottom of the heating chamber (10), the lower end of the core punch (4) blocks the hot extrusion hole (306), and then the upper end of the core punch (4) is locked relative to the frame (1); Step S2: adding nano-silicon carbide particle reinforced aluminum-based composite material powder into the heating chamber (10) and then sealing the chamber, wherein the heating chamber (10) heats the nano-silicon carbide particle reinforced aluminum-based composite material powder to form a nano-silicon carbide particle reinforced aluminum-based composite material melt; Step S3: the core punch (4) and the stirring punch (5) are unlocked, and the lifting drive mechanism (2) drives the stirring punch (5) to reciprocate up and down, so that the metal liquid jet ejected from the jet hole of the stirring punch (5) performs shear jet stirring on the nano-silicon carbide particle reinforced aluminum-based composite material melt; Step S4: the lifting drive mechanism (2) drives the stirring convex mold (5) to rise to the top of the heating chamber (10); Step S5: the core punch (4) and the frame (1) are unlocked, and the core punch (4) is lifted upward by an external lifting device until the core punch (4) seals the jet hole of the stirring punch (5), thereby locking the core punch (4) and the stirring punch (5) relative to each other; Step S6: the heating chamber (10) performs process temperature control to change the nano-silicon carbide particle reinforced aluminum-based composite material melt into a softened solid state; Step S7: the lifting drive mechanism (2) drives the core punch (4) and the stirring punch (5) to move downward synchronously, and the softened solid nano-silicon carbide particle reinforced aluminum-based composite material is hot extruded through the hot extrusion hole (306).
Citation Information
Patent Citations
Manufacturing method and manufacturing device of low-density corrosion-resistant high-strength aluminum alloy
CN114277270A
Metal matrix composite hot extrusion lubricant replacement device and method
CN114798791A
Diecasting smelting furnace with gravity mix
CN2605945Y
Manufacture of compound wire rod
JP1984030419A
Processes and / or Machines for Producing Continuous Plastic Deformation, and / or Compositions and / or Manufactures Produced Thereby
US20220281005A1