A pole piece coating system based on a single-layer double coating die assembly
Through the pole piece coating system of the single-layer double coating die assembly, the area of the tab area is reduced and the uniformity of the electrode material is improved, which solves the problems of energy density and edge effect in the coating of lithium-ion battery pole pieces. Improved battery performance and production efficiency.
Patent Information
- Application Number
- CN202410972037.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-19
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2044-07-19
AI Technical Summary
There are large blank areas during the coating process of lithium-ion battery pole pieces, which results in a reduction in energy density. The edge effect causes uneven thickness of the electrode material, affecting battery performance and life. In addition, the existing single-die coating process is more affected by edge effects. Large, affecting production efficiency and product yield.
Adopting a pole piece coating system based on a single-layer double-coating die assembly, through the combination of a single-layer double-coating die and a feeding assembly, an independent double-cavity structure and a double-feeding structure are realized, and a servo motor is used to drive and feed the cylinder. The component feeds the slurry into the die head, ensuring that the tab area is reduced and the material uniformity is improved.
Effectively reduce the area of the tab area, make full use of the electrode area, increase the energy density of the battery core, improve the uniformity of electrode materials, improve production efficiency and product yield, and reduce raw material waste and production costs.
Smart Images

Figure CN118513209B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of lithium ion battery production equipment, and in particular to a pole piece coating system based on a single-layer double coating die head assembly. Background Art
[0002] Compared with traditional batteries, lithium-ion batteries have the advantages of higher energy, stronger discharge capacity and longer cycle life. In addition, their energy storage efficiency can exceed 90% and their safety performance is good. Therefore, lithium-ion batteries have great development prospects in electric vehicles and storage power sources.
[0003] When the pole piece is coated in the production process of lithium-ion batteries, a pole ear area is reserved at the head of the battery cell pole piece for welding the pole ear. The general coating method is to install the gasket in the die head, and control the coating of the die head to reach the two areas of the coating area and the blank area. In order to reduce the internal resistance of the battery cell and improve the performance and safety of the battery cell, the pole ear area is generally set in the middle of the pole piece. However, in the prior art, there is a large blank area in the middle of the pole piece. This large blank area cannot be fully utilized, which leads to a decrease in the energy density of the battery cell and affects the performance of the battery. Therefore, in order to reduce the area of the pole ear area and make full use of the pole piece area, a pole piece coating method that can improve the energy density is needed.
[0004] In addition, since general coating devices are affected by the edge effect, the coating thickness at the edge and head and tail of the pole piece is uneven. The coating edge effect refers to the phenomenon that the thickness of the electrode material is uneven at the edge during the coating process of the positive and negative electrode materials of the lithium battery due to the limitations of the coating mechanical structure and coating process. This uneven thickness distribution will cause local overcharge or over-discharge of the electrode material during use, thereby affecting the performance and life of the lithium battery. The existing single-die coating process will be more affected by the edge effect, which will affect the production efficiency and product yield to a certain extent. Summary of the invention
[0005] The technical problem to be solved by the present invention is the need to provide a pole piece coating system based on a single-layer double coating die head assembly, which aims to effectively reduce the area of the pole ear area and make full use of the pole piece area to improve the energy density of the battery cell; on this basis, it also aims to improve the uniformity of the electrode material to improve production efficiency and product yield.
[0006] In this regard, the present invention provides a pole piece coating system based on a single-layer double coating die head assembly, which adopts a single-layer double coating die head assembly, wherein the single-layer double coating die head assembly comprises a single-layer double coating die head, a coating roller assembly and a feeding assembly, wherein the single-layer double coating die head is connected to the feeding assembly and is arranged on one side of the coating roller assembly; the single-layer double coating die head comprises an upper die head, a gasket and a lower die head, wherein a front mold cavity and a rear mold cavity are arranged on the top of the lower die head, wherein the feeding assembly comprises an upper layer feeding device and a lower layer feeding device, wherein the front mold cavity is connected to the lower layer feeding device, and the rear mold cavity is connected to the upper layer feeding device The gasket comprises a first gasket and a second gasket which are stacked in sequence, the stacked gaskets are arranged between the upper die head and the lower die head, the first gasket is arranged on a side close to the upper die head, the second gasket is arranged on a side close to the lower die head, and the front die cavity and the rear die cavity are isolated from each other by the gaskets; the feeding component feeds the slurry into the single-layer double-coating die head through a coating valve, and when the rear die cavity is fed and coated, a complete first coating area is obtained; when the front die cavity is fed and coated at intervals, an alternating second coating area, a blank area and a third coating area are obtained;
[0007] The first gasket is provided with a first gasket coating area and a first gasket tab coating area, the first gasket coating area and the first gasket tab coating area are adjacent and coated alternately; the second gasket is provided with a first opening and a second opening, the two sides of the first opening correspond to the bottom of the first gasket coating area and the top of the rear mold cavity respectively, and the two sides of the second opening correspond to the bottom of the first gasket tab coating area and the top of the front mold cavity respectively, so that the slurry is guided to the first gasket through the second gasket, and the first gasket cooperates with the feeding assembly for coating;
[0008] The coating process of the pole piece coating system includes the following steps:
[0009] Step S1, driving the upper layer feeding device through a servo motor, opening the upper layer feeding valve of the upper layer feeding device, delivering the slurry to the rear mold cavity through the feeding cylinder assembly, and the slurry in the rear mold cavity passes through the first opening to the first gasket coating area to coat the pole piece, thereby obtaining a complete first coating area on the pole piece;
[0010] Step S2, the rear mold cavity starts coating, and at the same time, the lower layer feeding device is driven by a servo motor to open the lower layer feeding valve of the lower layer feeding device, and the slurry is sent to the front mold cavity through the feeding cylinder assembly, and the slurry in the front mold cavity passes through the second opening to the first gasket tab coating area to coat the gap portion adjacent to the first coating area, and a second coating area is obtained on the pole piece, and the second coating area is the tab coating area;
[0011] Step S3, after the front mold cavity completes coating of the second coating area above the blank area, the front mold cavity stops coating;
[0012] Step S4, after the front mold cavity stops coating for a preset time, the front mold cavity continues coating, and then forms a blank area between the second coating area and the third coating area, until the front mold cavity completes the third coating area below the blank area, then the front mold cavity and the rear mold cavity are controlled to stop coating at the same time, and jump back to the step S1, and cycle until the electrode coating process is completed; the blank area is used for welding the pole ear, and the third coating area is the pole ear coating area.
[0013] A further improvement of the present invention is that, in step S4, the front mold cavity stops coating for a preset time until the blank length of the blank area reaches a preset gap of the pole piece.
[0014] A further improvement of the present invention is that a first gasket fixing hole and a first gasket reinforcing rib are provided on the first gasket, the first gasket fixing hole is provided on the side of the first gasket away from the coating roller assembly, and the first gasket reinforcing rib is evenly provided in the first gasket coating area.
[0015] A further improvement of the present invention is that the length of the first gasket coating area is greater than the length of the first gasket tab coating area, the length of the first opening is adapted to the length of the first gasket coating area, and the length of the second opening is adapted to the length of the first gasket tab coating area.
[0016] A further improvement of the present invention is that the bottom height of the first gasket coating area is lower than the bottom height of the first gasket tab coating area.
[0017] A further improvement of the present invention is that a second gasket fixing hole is provided on the second gasket, the second gasket fixing hole is arranged on the side of the second gasket away from the coating roller assembly and corresponds to the position of the first gasket fixing hole.
[0018] A further improvement of the present invention is that the cross section of the front mold cavity is larger than the cross section of the rear mold cavity.
[0019] A further improvement of the present invention is that the feeding assembly also includes a first extrusion head feeding elbow, a second extrusion head feeding elbow, a third extrusion head feeding elbow, a fourth extrusion head feeding elbow, a feeding cylinder assembly, a return pipe elbow, a return collection pipe, a return cylinder assembly and a servo motor; the upper die head and the upper layer feeding device are connected through the first extrusion head feeding elbow, the third extrusion head feeding elbow and the clamp fixing structure; the lower die head and the lower layer feeding device are connected through the second extrusion head feeding elbow, the fourth extrusion head feeding elbow and the clamp fixing structure to realize two sets of independently controlled feeding structures; the bottom of the upper die head is connected to the rear die cavity through the first gasket coating area and the first opening, and the rear die cavity is connected to the first extrusion head feeding elbow; the top of the lower die head is connected to the front die cavity through the first gasket ear coating area and the second opening, and the front die cavity is connected to the second extrusion head feeding elbow to realize an independent double cavity structure.
[0020] A further improvement of the present invention is that the feeding assembly feeds the slurry into the single-layer double-coating die head through the coating valve, the upper feeding device in the feeding assembly is driven by a servo motor, the upper feeding valve is opened, and the slurry is fed to the upper die head through the feeding cylinder assembly, and the lower feeding device in the feeding assembly is driven by a servo motor, the lower feeding valve is opened, and the slurry is fed to the lower die head through the feeding cylinder assembly; when the coating is stopped, the servo motors corresponding to the upper return valve of the upper feeding device and the lower return valve of the lower feeding device work, and the excess slurry is fed back to the return collection pipe through the return cylinder assembly and the return pipe elbow.
[0021] A further improvement of the present invention is that the coating speed in steps S1 to S4 is controlled by a coating valve.
[0022] Compared with the prior art, the beneficial effect of the present invention lies in that: in the single-layer double-coating die head assembly, a first gasket coating area and a first gasket tab coating area are provided on the first gasket, and the first gasket coating area and the first gasket tab coating area are adjacent to each other and are coated alternately; a first opening and a second opening are provided on the second gasket, and the two sides of the first opening respectively correspond to the bottom of the first gasket coating area and the top of the rear mold cavity, and the two sides of the second opening respectively correspond to the bottom of the first gasket tab coating area and the top of the front mold cavity, thereby guiding the slurry to the first gasket through the second gasket, and the first gasket cooperates with the feeding assembly for coating, thereby realizing an independent double material cavity structure; on this basis, two sets of independently controlled feeding structures are realized by designing and optimizing the feeding assembly, thereby not only effectively reducing the area of the tab area and making full use of the pole area to improve the energy density of the battery cell; but also effectively improving the uniformity of the electrode material to improve the production efficiency and product yield. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 A schematic diagram of the structure of an embodiment of the present invention;
[0024] Figure 2 A schematic diagram of a three-dimensional structure of an embodiment of the present invention;
[0025] Figure 3 A composition diagram of a feeding assembly according to an embodiment of the present invention;
[0026] Figure 4 This is a schematic structural diagram of a first gasket according to an embodiment of the present invention;
[0027] Figure 5 A schematic structural diagram of a second gasket according to an embodiment of the present invention;
[0028] Figure 6 This is a schematic structural diagram of stacked gaskets according to an embodiment of the present invention;
[0029] Figure 7 The figure is a schematic diagram of the structure of a pole piece obtained by processing according to an embodiment of the present invention. DETAILED DESCRIPTION
[0030] In the description of the present invention, if it involves a description of orientation, for example, the orientation or position relationship indicated by "upper", "lower", "front", "back", "left", "right", etc. is based on the orientation or position relationship shown in the drawings, which is only for the convenience of describing the present invention and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. If a certain technical feature is referred to as "set", "fixed", "connected", or "installed" on another technical feature, it can be directly set, fixed, or connected to the other technical feature, or it can be indirectly set, fixed, connected, or installed on the other technical feature.
[0031] In the description of the present invention, if "several" is involved, it means more than one; if "multiple" is involved, it means more than two; if "greater than", "less than", or "exceed" is involved, it should be understood as not including the number itself; if "above", "below", or "within" is involved, it should be understood as including the number itself. If "first", "second", etc. are involved, they should be understood as being used only to distinguish the names of the same or similar technical features, and should not be understood as implying / indicating the relative importance of the technical features, the number of the technical features, or the order of the technical features.
[0032] The preferred embodiments of the present invention will be further described in detail below in conjunction with the accompanying drawings.
[0033] like Figures 1 to 7As shown, this embodiment provides a pole piece coating system based on a single-layer double coating die head assembly, which adopts a single-layer double coating die head assembly, wherein the single-layer double coating die head assembly comprises a single-layer double coating die head 1, a coating roller assembly 5 and a feeding assembly 6, wherein the single-layer double coating die head 1 is connected to the feeding assembly 6 and is arranged on one side of the coating roller assembly 5; the single-layer double coating die head 1 comprises an upper die head 2, a gasket 3 and a lower die head 4, wherein a front mold cavity 41 and a rear mold cavity 42 are arranged on the top of the lower die head 4, wherein the feeding assembly 6 comprises an upper layer feeding device 7 and a lower layer feeding device 8, wherein the front mold cavity 41 is connected to the lower layer feeding device 8, and the rear mold cavity 42 is connected to the upper layer feeding device 7; wherein the gasket 3 and the lower die head 4 are provided with a front mold cavity 41 and a rear mold cavity 42, wherein the feeding assembly 6 comprises an upper layer feeding device 7 and a lower layer feeding device 8, wherein the front mold cavity 41 is connected to the lower layer feeding device 8, and the rear mold cavity 42 is connected to the upper layer feeding device 7; wherein the gasket 3 and the lower die head 4 are provided with a front mold cavity 41 and a rear mold cavity 42, wherein the feeding assembly 6 comprises an upper layer feeding device 7 and a lower layer feeding device 8, wherein the front mold cavity 41 and the lower layer feeding device 8 are connected, and the rear mold cavity 42 and the upper layer feeding device 7 are connected ... The sheet 3 includes a first gasket 31 and a second gasket 32 stacked in sequence. The stacked gasket 3 is arranged between the upper die head 2 and the lower die head 4. The first gasket 31 is arranged on a side close to the upper die head 2, and the second gasket 32 is arranged on a side close to the lower die head 4. The front die cavity 41 and the rear die cavity 42 are isolated by the gasket 3. The feeding component 6 feeds the slurry into the single-layer double-coating die head 1 through a coating valve. When the rear die cavity 42 is fed and coated, a complete first coating area 30 is obtained. When the front die cavity 41 is fed and coated at intervals, an alternating second coating area 312, a blank area 314 and a third coating area 313 are obtained.
[0034] The first gasket 31 is provided with a first gasket coating area 37 and a first gasket tab coating area 38, and the first gasket coating area 37 and the first gasket tab coating area 38 are adjacent to each other and are coated alternately; the second gasket 32 is provided with a first opening 33 and a second opening 34, and the two sides of the first opening 33 respectively correspond to the bottom of the first gasket coating area 37 and the top of the rear mold cavity 42, and the two sides of the second opening 34 respectively correspond to the bottom of the first gasket tab coating area 38 and the top of the front mold cavity 41, so that the slurry is guided to the first gasket 31 through the second gasket 32, and the first gasket 31 cooperates with the feeding assembly 6 for coating; the first gasket coating area 37 refers to the first gasket, which is used to realize the main coating area corresponding to the first coating area 30; the first gasket tab coating area 38 refers to the first gasket, which is used to realize the coating areas at both ends of the tab welding positions corresponding to the second coating area 312 and the third coating area 313 in the gap part.
[0035] The coating process of the pole piece coating system includes the following steps:
[0036] Step S1, driving the upper layer feeding device 7 by a servo motor, opening the upper layer feeding valve 71 of the upper layer feeding device 7, delivering the slurry to the rear mold cavity 42 through the feeding cylinder assembly, and the slurry in the rear mold cavity 42 passes through the first opening 33 to the first gasket coating area 37 to coat the electrode piece, thereby obtaining a complete first coating area 30 on the electrode piece;
[0037] Step S2, the rear mold cavity 42 starts coating, and the lower layer feeding device 8 is driven by a servo motor, the lower layer feeding valve 81 of the lower layer feeding device 8 is opened, and the slurry is sent to the front mold cavity 41 through the feeding cylinder assembly, and the slurry in the front mold cavity 41 passes through the second opening 34 to the first gasket tab coating area 38 to coat the gap portion adjacent to the first coating area 30, and a second coating area 312 is obtained on the pole piece, and the second coating area 312 is the tab coating area;
[0038] Step S3, after the front mold cavity 41 completes coating of the second coating area 312 above the blank area 314, the front mold cavity 41 stops coating;
[0039] Step S4, after the front mold cavity 41 stops coating for a preset time, the front mold cavity 41 continues coating, and then forms a blank area 314 between the second coating area 312 and the third coating area 313, until the front mold cavity 41 completes the third coating area 313 below the blank area 314, then the front mold cavity 41 and the rear mold cavity 42 are controlled to stop coating at the same time, and jump back to the step S1, and cycle until the electrode coating process is completed; the blank area 314 is used for welding the pole ear, and the third coating area 313 is the pole ear coating area.
[0040] It should be noted that since the electrode coating involves at least two coating processes, and the widths of the two coating processes are different, the required spraying pressures are also different. If the single feed port and single material cavity form of the existing technology is directly adopted, it will inevitably fail to meet the actual application requirements of such different spraying pressures, which will lead to uneven coating thickness at the edge and head and tail of the electrode, resulting in edge effect.
[0041] In order to overcome this practical technical problem, this embodiment adopts a double feed and double material chamber structure. Figure 1As shown, the first gasket 31 is provided with a first gasket coating area 37 and a first gasket tab coating area 38, and the first gasket coating area 37 and the first gasket tab coating area 38 are adjacent to each other and are coated alternately; the second gasket 32 is provided with a first opening 33 and a second opening 34, and the two sides of the first opening 33 respectively correspond to the bottom of the first gasket coating area 37 and the top of the rear mold cavity 42, that is, one side of the first opening 33 is connected with the bottom of the first gasket coating area 37, and the other side of the first opening 33 is connected with the top of the rear mold cavity 42. In one step of coating, the feed cylinder assembly 13 delivers the slurry to the rear mold cavity 42, and the slurry in the rear mold cavity 42 passes through the first opening 33 to the first gasket coating area 37 to coat the pole piece, so as to obtain a complete first coating area 30 on the pole piece. The two sides of the second opening 34 respectively correspond to the bottom of the first gasket tab coating area 38 and the top of the front mold cavity 41, that is, one side of the second opening 34 is connected to the bottom of the first gasket tab coating area 38, and the other side of the second opening 34 is connected to the top of the front mold cavity 41. In another step of coating, the slurry is guided to the first gasket 31 through the second gasket 32, and the first gasket 31 cooperates with the feeding assembly 6 to perform alternating coating through the first gasket tab coating area 38. Therefore, unlike the prior art, this embodiment realizes a double cavity structure in which the front mold cavity 41 and the rear mold cavity 42 are independent of each other.
[0042] On this basis, in conjunction with the double-cavity structure, the feeding assembly 6 described in this embodiment also includes a first extrusion head feeding elbow 9, a second extrusion head feeding elbow 10, a third extrusion head feeding elbow 11, a fourth extrusion head feeding elbow 12 and a feeding cylinder assembly 13, etc. The upper die head 2 and the upper layer feeding device 7 are connected through the first extrusion head feeding elbow 9, the third extrusion head feeding elbow 11 and the clamp fixing structure, and the lower die head 4 and the lower layer feeding device 8 are connected through the second extrusion head feeding elbow 10, the fourth extrusion head feeding elbow 12 and the clamp fixing structure to realize two sets of independently controlled feeding structures, which are matched with the double-cavity structure described above to meet the actual application requirements of spraying different pressures, avoid edge effects, and make the coating thickness of the edge and the head and tail of the electrode more uniform and controllable.
[0043] In the prior art, in addition to the edge effect, the coating adopts a simple zebra coating. This simple zebra coating structure achieves the effect of simple spacing between the material area and the blank area. The blank area will occupy a larger area, but in actual applications, an area as wide as the material area is not required to weld the tabs, which not only causes a waste of raw materials such as foil, but also affects the energy density of the battery.
[0044] In this regard, it is also worth noting that, unlike the prior art, based on the structure of independent double feeds and double material cavities, this embodiment uses a combined first gasket 31 and a second gasket 32 that are stacked in sequence. The battery slurry is guided by the second gasket 32. In different coating steps, it is coated from different coating areas of the first gasket 31, including an overall coated first gasket coating area 37 and an alternately coated first gasket tab coating area 38. Specifically, see the above-mentioned steps S1 to S4, so that the front mold cavity 41 and the rear mold cavity 42 each have a set of adapted and independently controlled loading and feeding systems, so as to achieve the following. Figure 7 The final coating effect shown reasonably and fully utilizes a small area between the second coating area 312 and the third coating area 313 as a blank area 314 .
[0045] Therefore, through the technical solution provided in this embodiment, in addition to meeting the requirements of the electrode ear welding, only a small area is used as the blank area 314 to better ensure the energy density of the battery cell, and greatly reduce the waste of raw materials such as foil, thereby reducing production costs.
[0046] In step S4 of this embodiment, the preset time for the front mold cavity 41 to stop coating is until the blank length of the blank area 314 reaches the preset gap of the pole piece. In other words, the preset time for the front mold cavity 41 to stop coating can be set according to actual conditions and needs, as long as the blank length of the blank area 314 can meet the requirements of pole piece welding. The blank length of the blank area 314 is preferably less than the length of the second coating area 312, so that less than half of the gap portion can be used as the blank area 314; the gap portion refers to the area between the two first coating areas 30, that is, the area where the second coating area 312, the blank area 314 and the third coating area 313 are located.
[0047] like Figure 4 As shown, in this embodiment, the first gasket 31 is provided with a first gasket fixing hole 35 and a first gasket reinforcement rib 39. The first gasket fixing hole 35 is arranged on the side of the first gasket 31 away from the coating roller assembly 5 to utilize the rear end position to achieve rapid fixation and assembly; the first gasket reinforcement rib 39 is evenly arranged in the first gasket coating area 37 to ensure its strength and prevent deformation.
[0048] like Figures 4 to 6As shown, in this embodiment, the length of the first gasket coating area 37 is greater than the length of the first gasket tab coating area 38, the length of the first opening 33 is adapted to the length of the first gasket coating area 37, and the length of the second opening 34 is adapted to the length of the first gasket tab coating area 38. In other words, the length of the first coating area 30 of this embodiment is greater than the length of the gap part, thereby ensuring that the first coating area 30 accounts for a larger proportion as much as possible, thereby improving the energy density of the pole piece and its battery cell.
[0049] like Figures 4 to 6 As shown, in this embodiment, the bottom height of the first gasket coating area 37 is lower than the bottom height of the first gasket tab coating area 38. This design is because the first gasket coating area 37 is used to achieve coating of the first coating area 30, and the first gasket tab coating area 38 is used to achieve coating of the second coating area 312 and the third coating area 313. Therefore, the coating height of the two different areas can be controlled to facilitate the control of the blank area 314.
[0050] like Figure 5 As shown, in this embodiment, a second gasket fixing hole 36 is provided on the second gasket 32. The second gasket fixing hole 36 is arranged on the side of the second gasket 32 away from the coating roller assembly 5 and corresponds to the position of the first gasket fixing hole 35, so as to facilitate the rapid fixation and assembly of the gasket structure and prevent misalignment between the first gasket 31 and the second gasket 32.
[0051] The cross section of the front mold cavity 41 of this embodiment is larger than the cross section of the rear mold cavity 42. The reason for this design of this embodiment is that, since the opening area of the first opening 33 is larger than the opening area of the second opening 34, the slurry in the rear mold cavity 42 can be coated at a faster speed during the coating process, so the storage space of its material cavity can be appropriately reduced; and correspondingly, the second coating area 312 and the third coating area 313 corresponding to the front mold cavity 41 are smaller in area and need to be coated at a slightly slower speed. Therefore, the front mold cavity 41 with a larger cross section is selected to better realize the slurry storage, which is convenient for subsequent material return to avoid the raw materials from overflowing when coating is not needed.
[0052] like Figures 1 to 3As shown, the feeding assembly 6 in this embodiment also includes a first extrusion head feeding elbow 9, a second extrusion head feeding elbow 10, a third extrusion head feeding elbow 11, a fourth extrusion head feeding elbow 12, a feeding cylinder assembly 13, a return pipe elbow 14, a return collection pipe 15, a return cylinder assembly 16 and a servo motor 17. The upper die head 2 and the upper layer feeding device 7 are connected through the first extrusion head feeding elbow 9, the third extrusion head feeding elbow 11 and the clamp fixing structure, and the lower die head 4 and the lower layer feeding device 8 are connected through the second extrusion head feeding elbow. 10. The fourth extrusion head feed elbow 12 is connected to the clamp fixing structure to realize two sets of independently controlled feeding structures; the bottom of the upper die head 2 is connected to the rear die cavity 42 through the first gasket coating area 37 and the first opening 33, and the rear die cavity 42 is connected to the first extrusion head feed elbow 9; the top of the lower die head 4 is connected to the front die cavity 41 through the first gasket ear coating area 38 and the second opening 34, and the front die cavity 41 is connected to the second extrusion head feed elbow 10 to realize an independent double cavity structure.
[0053] The feeding component 6 in this embodiment feeds the slurry into the single-layer double coating die head 1 through the coating valve, the upper feeding device 7 in the feeding component 6 is driven by the servo motor 17, the upper feed valve 71 is opened, and the slurry is fed to the upper die head 2 through the feeding cylinder component 13, the lower feeding device 8 in the feeding component 6 is driven by the servo motor 17, the lower feed valve 81 is opened, and the slurry is fed to the lower die head 4 through the feeding cylinder component 13; when the coating is stopped, the servo motors corresponding to the upper return valve 72 of the upper feeding device 7 and the lower return valve 82 of the lower feeding device 8 work, and the excess slurry is fed back to the return collection pipe 15 through the return cylinder component 16 and the return pipe elbow 14.
[0054] More preferably, the coating speed is controlled by the coating valve in steps S1 to S4 of this embodiment. The electrode is significantly less affected by the edge effect during coating, and the thickness of the electrode head and the electrode tail can be consistent with the middle area of the electrode. The coating speed is controlled by the coating valve so that the thickness of the electrode head and the electrode tail is consistent with the middle area of the electrode. The faster the coating valve is opened, the faster the coating speed is, the smaller the thickness of the electrode head and the electrode tail is, and vice versa.
[0055] More preferably, the present embodiment may further include a pre-coating step before the step S1, in which coating is first performed at the same coating speed, and the thickness of the electrode head, the electrode middle area and the electrode tail of each coating area (including the first coating area 30, the second coating area 312 and the third coating area 313) at the same coating speed is detected and recorded respectively, and the corresponding relationship between the coating speed and the thickness in each area is established for the electrode head, the electrode middle area and the electrode tail; therefore, in the actual electrode coating process, the coating speed can be adjusted and controlled by using the coating valve according to the corresponding relationship between the coating speed and the thickness in each area. For example, if the thickness of the pole piece head is greater than the thickness of the middle area at the same coating speed, then, in the actual pole piece coating process, the coating speed of the pole piece head is increased proportionally according to the ratio between the thickness of the pole piece head and the thickness of the middle area, so that its thickness becomes smaller, so as to be consistent with the middle area of the pole piece; conversely, if the thickness of the pole piece head is smaller than the thickness of the middle area at the same coating speed, then, in the actual pole piece coating process, the coating speed of the pole piece head is reduced proportionally according to the ratio between the thickness of the pole piece head and the thickness of the middle area, so that its thickness becomes larger, so as to be consistent with the middle area of the pole piece. The same is true for the process of adjusting and controlling the coating speed of the pole piece tail. Therefore, this embodiment can make the thickness of the pole piece head and the pole piece tail as consistent as possible with the middle area of the pole piece, more effectively reduce the influence of the edge effect, no longer need a better gasket structure to improve efficiency, and effectively reduce the precision requirements of processing. The pole piece head and the pole piece tail are also called the pole piece edges of each coating area.
[0056] Compared with the prior art, the area of the blank area 314 of the present application is greatly reduced. In the blank area 314, there is also a key point to handle the coating size of each joint. Therefore, the present application realizes the control of the joint by designing a new combined gasket 3 and adjusting the servo valve, and realizes the matching electrode coating process based on the single-layer double coating die head coating device. The data of the actual measured size of the product will be sorted and analyzed below.
[0057] First, the present embodiment is applied to the negative electrode sheet, and the single-sided thickness after coating and drying is tested to obtain the test data of the single-sided thickness. The unit of each test data is um, and the product thickness dimension requirement is 92±5um; the test shows that the data applied to the negative electrode sheet can be maintained within the required range. Next, the present embodiment is applied to the positive electrode sheet, and the single-sided thickness after coating and drying is tested to obtain the test data of the single-sided thickness. The unit of each test data is um, and the product thickness dimension requirement is 117±5um; the test shows that the data applied to the positive electrode sheet can also be maintained within the required range. Therefore, after the present embodiment greatly reduces the area of the blank area 313, it also well guarantees the coating size at each seam.
[0058] In summary, in the single-layer double-coating die head assembly of this embodiment, the first gasket 31 is provided with a first gasket coating area 37 and a first gasket tab coating area 38, and the first gasket coating area 37 and the first gasket tab coating area 38 are adjacent and alternately coated; the second gasket 32 is provided with a first opening 33 and a second opening 34, and the two sides of the first opening 33 correspond to the bottom of the first gasket coating area 37 and the top of the rear mold cavity 42 respectively, and the two sides of the second opening 34 correspond to the bottom of the first gasket tab coating area 38 respectively. Corresponding to the top of the front mold cavity 41, the slurry is guided to the first gasket 31 through the second gasket 32, and the first gasket 31 cooperates with the feeding assembly 6 for coating, thereby realizing an independent dual-cavity structure; on this basis, two sets of independently controlled feeding structures are realized through the design and optimization of the feeding assembly 6, thereby not only effectively reducing the area of the pole ear area and making full use of the pole piece area to improve the energy density of the battery cell; it can also effectively improve the uniformity of the electrode material to improve production efficiency and product yield.
[0059] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the protection scope of the present invention.
Claims
1. A pole piece coating system based on a single-layer double coating die head assembly, characterized in that: A single-layer double coating die head assembly is used, the single-layer double coating die head assembly comprising a single-layer double coating die head (1), a coating roller assembly (5) and a feeding assembly (6), the single-layer double coating die head (1) being connected to the feeding assembly (6) and being arranged on one side of the coating roller assembly (5); the single-layer double coating die head (1) comprising an upper die head (2), a gasket (3) and a lower die head (4), the top of the lower die head (4) being provided with a front die cavity (41) and a rear die cavity (42), the feeding assembly (6) comprising an upper layer feeding device (7) and a lower layer feeding device (8), the front die cavity (41) being connected to the lower layer feeding device (8), and the rear die cavity (42) being connected to the upper layer feeding device (7); the gasket (3) comprising a first gasket ( The stacked gasket (3) is arranged between the upper die head (2) and the lower die head (4), the first gasket (31) is arranged on a side close to the upper die head (2), and the second gasket (32) is arranged on a side close to the lower die head (4), and the front die cavity (41) and the rear die cavity (42) are isolated from each other by the gasket (3); the feeding component (6) feeds the slurry into the single-layer double-coating die head (1) through a coating valve, and when the rear die cavity (42) is fed with material for coating, a complete first coating area (30) is obtained; when the front die cavity (41) is fed with material for coating at intervals, alternating second coating areas (312), blank areas (314) and third coating areas (313) are obtained; The first gasket (31) is provided with a first gasket coating area (37) and a first gasket tab coating area (38), the first gasket coating area (37) and the first gasket tab coating area (38) being adjacent to each other and coated alternately; the second gasket (32) is provided with a first opening (33) and a second opening (34), the two sides of the first opening (33) respectively corresponding to the bottom of the first gasket coating area (37) and the top of the rear mold cavity (42), and the two sides of the second opening (34) respectively corresponding to the bottom of the first gasket tab coating area (38) and the top of the front mold cavity (41), so that the slurry is guided to the first gasket (31) through the second gasket (32), and the first gasket (31) cooperates with the feeding assembly (6) for coating; The coating process of the pole piece coating system includes the following steps: Step S1, driving the upper layer feeding device (7) by a servo motor, opening the upper layer feeding valve (71) of the upper layer feeding device (7), delivering the slurry to the rear mold cavity (42) by a feeding cylinder assembly, and the slurry in the rear mold cavity (42) passes through the first opening (33) to the first gasket coating area (37), coating the pole piece, and obtaining a complete first coating area (30) on the pole piece; Step S2, the rear mold cavity (42) starts coating, and at the same time, the lower layer feeding device (8) is driven by a servo motor to open the lower layer feeding valve (81) of the lower layer feeding device (8), and the slurry is sent to the front mold cavity (41) through the feeding cylinder assembly, and the slurry in the front mold cavity (41) passes through the second opening (34) to the first gasket tab coating area (38) to coat the gap portion adjacent to the first coating area (30), thereby obtaining a second coating area (312) on the pole piece, and the second coating area (312) is the tab coating area; Step S3, after the front mold cavity (41) completes coating of the second coating area (312) above the blank area (314), the front mold cavity (41) stops coating; Step S4, after the front mold cavity (41) stops coating for a preset time, the front mold cavity (41) continues coating, thereby forming a blank area (314) between the second coating area (312) and the third coating area (313), until the front mold cavity (41) completes the third coating area (313) below the blank area (314), then the front mold cavity (41) and the rear mold cavity (42) are controlled to stop coating at the same time, and jump back to the step S1, and the cycle is repeated until the electrode coating process is completed; the blank area (314) is used for welding the electrode lug, and the third coating area (313) is the electrode lug coating area.
2. The pole piece coating system based on the single-layer double coating die head assembly according to claim 1 is characterized in that: In the step S4, the front mold cavity (41) stops coating for a preset time until the blank length of the blank area (314) reaches a preset gap between the pole pieces.
3. The pole piece coating system based on the single-layer double coating die head assembly according to claim 1 or 2, characterized in that: The first gasket (31) is provided with a first gasket fixing hole (35) and a first gasket reinforcing rib (39); the first gasket fixing hole (35) is arranged on a side of the first gasket (31) away from the coating roller assembly (5); and the first gasket reinforcing rib (39) is evenly arranged in the first gasket coating area (37).
4. The pole piece coating system based on the single-layer double coating die head assembly according to claim 1 or 2, characterized in that: The length of the first gasket coating area (37) is greater than the length of the first gasket tab coating area (38), the length of the first opening (33) is adapted to the length of the first gasket coating area (37), and the length of the second opening (34) is adapted to the length of the first gasket tab coating area (38).
5. The pole piece coating system based on the single-layer double coating die head assembly according to claim 1 or 2, characterized in that: The bottom height of the first gasket coating area (37) is lower than the bottom height of the first gasket tab coating area (38).
6. The pole piece coating system based on the single-layer double coating die head assembly according to claim 3 is characterized in that: The second gasket (32) is provided with a second gasket fixing hole (36), which is arranged on a side of the second gasket (32) away from the coating roller assembly (5) and corresponds to the position of the first gasket fixing hole (35).
7. The pole piece coating system based on the single-layer double coating die head assembly according to claim 1 or 2, characterized in that: The cross section of the front mold cavity (41) is larger than the cross section of the rear mold cavity (42).
8. The pole piece coating system based on the single-layer double coating die head assembly according to claim 1 or 2, characterized in that: The feeding assembly (6) further comprises a first extrusion head feeding elbow (9), a second extrusion head feeding elbow (10), a third extrusion head feeding elbow (11), a fourth extrusion head feeding elbow (12), a feeding cylinder assembly (13), a return pipe elbow (14), a return collection pipe (15), a return cylinder assembly (16) and a servo motor (17); the upper die head (2) and the upper layer feeding device (7) are connected via the first extrusion head feeding elbow (9), the third extrusion head feeding elbow (11) and the clamp fixing structure; the lower die head (4) and the lower layer feeding device (8) are connected via the second extrusion head feeding elbow ( 10), the fourth extrusion head feed elbow (12) is connected to the clamp fixing structure to realize two sets of independently controlled feed structures; the bottom of the upper die head (2) is connected to the rear die cavity (42) through the first gasket coating area (37) and the first opening (33), and the rear die cavity (42) is connected to the first extrusion head feed elbow (9); the top of the lower die head (4) is connected to the front die cavity (41) through the first gasket tab coating area (38) and the second opening (34), and the front die cavity (41) is connected to the second extrusion head feed elbow (10), so as to realize an independent double-cavity structure.
9. The pole piece coating system based on the single-layer double coating die head assembly according to claim 8, characterized in that: The feeding assembly (6) feeds the slurry into the single-layer double coating die head (1) through the coating valve; the upper feeding device (7) in the feeding assembly (6) is driven by the servo motor (17), the upper feeding valve (71) is opened, and the slurry is fed into the upper die head (2) through the feeding cylinder assembly (13); the lower feeding device (8) in the feeding assembly (6) is driven by the servo motor (17), the lower feeding valve (81) is opened, and the slurry is fed into the lower die head (4) through the feeding cylinder assembly (13); when the coating is stopped, the servo motors corresponding to the upper return valve (72) of the upper feeding device (7) and the lower return valve (82) of the lower feeding device (8) are operated, and the excess slurry is fed back to the return collection pipe (15) through the return cylinder assembly (16) and the return pipe elbow (14).
10. The pole piece coating system based on the single-layer double coating die head assembly according to claim 1 or 2, characterized in that: The coating speed in steps S1 to S4 is controlled by a coating valve.
Citation Information
Cited By
Slot die for manufacturing secondary battery electrode