A kind of bean vegetable seed coating agent and preparation method thereof
By using the coating agent of bentonite/polyaspartic acid and modified β-cyclodextrin composite agent, the problems of short-lasting coating effect and poor salt-alkali resistance of legume and vegetable seeds are solved, and the coating of legume and vegetable seeds is realized. Efficient disease control and yield improvement.
Patent Information
- Application Number
- CN202410985775.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-07-23
AI Technical Summary
Existing seed coating agents for legumes and vegetables are not long-lasting in the late growth period and have poor salt-alkali tolerance, resulting in serious diseases and poor growth.
Bentonite/polyaspartic acid mixture and modified β-cyclodextrin composite agent are used to form a stable network structure through ball milling, amination, amidation and epoxidation to improve the sustained release performance and drought resistance of the coating agent. ability.
It significantly improves the drought resistance and disease control performance of legume vegetables, prolongs the coating effect, increases the yield and protein content of legume vegetables, and is suitable for planting in ordinary and saline-alkali soils.
Smart Images

Figure SMS_1 
Figure SMS_2 
Figure SMS_3
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of seed coating agents, and particularly relates to a bean vegetable seed coating agent and a preparation method thereof. Background Art
[0002] Seed coating is a high-tech technology developed in the mid-1980s to promote agricultural production and harvest. After sowing, seeds coated with seed coating agents can quickly absorb water and swell; as the embryo in the seed gradually develops and the seedlings continue to grow, the seed coating agent will slowly release the various active ingredients it contains, which are gradually absorbed into the body by the seed seedlings, thereby achieving the purpose of preventing and controlling seedling diseases and pests, promoting growth and development, and increasing crop yields.
[0003] The skin of bean vegetable seeds is delicate and easily broken and damaged, which can lead to the invasion of pathogens. In addition, bean vegetable seeds themselves contain polysaccharides and starch, which can easily become a "culture medium" for pathogens and cause the occurrence of diseases and pests, affecting yields and planting returns. In severe cases, there may even be no harvest.
[0004] At present, bean vegetable seeds are usually coated. By forming a protective layer containing pesticides, fungicides, compound fertilizers, plant growth regulators and trace elements on the surface of bean vegetable seeds, the growth of bean vegetable crops can be promoted, pests and diseases can be reduced, and yield can be increased.
[0005] In this regard, the prior art discloses the following:
[0006] CN118120391A discloses a seed coating agent and its application, and specifically discloses that the raw material components of the coating agent include special coating powder, adhesive and coating agent; the coating powder includes clay, heavy powder and light powder; the adhesive can be selected from at least one of sodium carboxymethyl cellulose, polyvinyl alcohol, polyvinyl acetate, polyvinyl pyrrolidone and polyacrylic acid; the coating agent includes film-forming agent, color paste, pearl powder, wax emulsion, antifreeze, rheological additive, preservative and water;
[0007] After the seeds are coated with the coating agent prepared by the patent, the coated seeds are of uniform size and can reduce the negative impact of pesticides and other ingredients on the seed germination rate. However, the coating agent prepared by the patent is not effective for a long time, and the disease phenomenon is more serious in the later growth stage of bean vegetables.
[0008] CN114557351A discloses a cyclodextrin derivative-based seed coating material and its preparation method and application, and specifically discloses that the coating material includes a cyclodextrin derivative gel and an ethyl cellulose solution; the preparation method of the cyclodextrin derivative gel is to prepare a β-cyclodextrin derivative solution, and then add humate and urea to obtain a mixed solution A; take gibberellin, insecticide and fungicide, dissolve them in water to obtain a mixed solution B; add the mixed solution A to the mixed solution B, add benzoic acid, an initiator and a cross-linking agent to obtain a gel, and wash and dry to obtain the cyclodextrin derivative gel; the preparation method of the ethyl cellulose solution is to dissolve ethyl cellulose and lactic acid in an ethanol solution to obtain an ethyl cellulose solution;
[0009] This patent solves the problem of loss of active ingredients and environmental pollution caused by poor seed coating viscosity and pesticide stability. However, the coating agent produced by this patent has poor salt and alkali resistance. After the seeds are coated, their growth and development in the saline-alkali environment are poor.
[0010] Therefore, the bean vegetable seed coating agent and its preparation method in the prior art have the following technical problems:
[0011] 1. The effect of coating is not long-lasting, and the disease phenomenon is serious in the late growth period of bean vegetables;
[0012] 2. The coating agent has poor salt and alkali resistance. After the seeds are coated, their growth and development in a saline and alkali environment are poor. Summary of the invention
[0013] In order to solve the technical problems existing in the prior art, the present invention provides a bean vegetable seed coating agent and a preparation method thereof, which can improve the salt-alkali resistance of bean vegetables, have good disease prevention and control performance throughout the growth period, and can effectively promote the growth of bean vegetables.
[0014] In view of the above technical problems, the present invention adopts the following technical solutions:
[0015] A method for preparing a bean vegetable seed coating agent comprises the steps of preparing a bentonite / polyaspartic acid mixture, preparing a composite agent and mixing. The specific operations are as follows:
[0016] 1. Preparation of Bentonite / Polyaspartic Acid Mixture
[0017] (1) Aminated bentonite
[0018] The bentonite is placed in a sodium hydroxide solution and stirred for 3.0-3.3 hours at a temperature of 56-60°C. After the stirring is completed, the bentonite is filtered and dried, and then placed in an ethanol solution for ball milling. The ball milling time is 28-32 minutes, the ball milling speed is 208-215 rpm, and the ball-to-material ratio is 3-5:1. After the ball milling is completed, pentaerythritol and glycerol are added and stirred for 25-29 minutes at a temperature of 53-55°C. After the stirring is completed, 3-aminopropyltriethoxysilane is added, the temperature is increased to 68-72°C, and the reaction is carried out at 68-72°C for 5.8-6.2 hours. After the reaction is completed, the bentonite is dried to obtain an amination bentonite.
[0019] The mass concentration of the sodium hydroxide solution is 22-26%;
[0020] The mass concentration of the ethanol solution is 43-47%;
[0021] The mass ratio of the bentonite, sodium hydroxide solution, ethanol solution, pentaerythritol, glycerol and 3-aminopropyltriethoxysilane is 6.3-6.7:50-54:61-65:0.7-0.9:0.8-1.2:0.5-0.7;
[0022] (2) Amide reaction
[0023] The polyaspartic acid is placed in dichloromethane, and after stirring, thionyl chloride is added dropwise. After the addition is completed, the temperature is raised to 60-64°C for reaction, and the reaction time is 9.8-10.2 hours. After the reaction is completed, the modified polyaspartic acid is obtained by rotary evaporation. The modified polyaspartic acid and amino bentonite are added to N, N-dimethylformamide, and ultrasonic oscillation treatment is performed. The ultrasonic time is 15-19 minutes, the ultrasonic frequency is 23-25kHz, and the ultrasonic power is 107-112W. After the ultrasonic oscillation treatment is completed, the temperature is raised to 60-64°C at a rate of 0.8-1.2°C / min, and the reaction is carried out at 60-64°C for 46-50 hours. After the reaction is completed, the mixture is washed and dried to obtain a bentonite / polyaspartic acid mixture.
[0024] The mass volume ratio of the polyaspartic acid, dichloromethane and thionyl chloride is 9-11 g: 63-67 mL: 18-22 g;
[0025] The mass volume ratio of the N,N-dimethylformamide, modified polyaspartic acid and amino bentonite is 106-115 mL: 0.04-0.06 g: 1.8-2.2 g;
[0026] 2. Preparation of composite agent
[0027] (1) Preparation of epoxidized lignin
[0028] Adding γ-glycidyloxypropyltrimethoxysilane to an ethanol solution and stirring, and obtaining a modifier after stirring evenly; placing lignin in the modifier, adding polyethylene glycol 2000 for ultrasonic treatment, the ultrasonic time is 18-22 minutes, the ultrasonic frequency is 33-37kHz, and the ultrasonic power is 85-90W. After the ultrasonic treatment, the temperature is increased to 70-72°C at a rate of 1.0-1.4°C / min, and the reaction is stirred for 9.5-10.4 hours. After the reaction is completed, filtering and drying are performed to obtain epoxidized lignin;
[0029] The mass concentration of the ethanol solution is 43-47%;
[0030] The mass ratio of the ethanol solution to γ-glycidyloxypropyltrimethoxysilane is 73-77:0.7-0.9;
[0031] The mass ratio of the lignin, the modifier, and polyethylene glycol 2000 is 11-13:95-99:1.2-1.4;
[0032] (2) Composite
[0033] Add β-cyclodextrin to deionized water, then add epoxidized lignin, stir evenly, then add 30-34wt% sodium hydroxide solution, adjust the pH to 11.2-11.8, stir at a speed of 172-186rpm for 4.8-5.3h, wash and dry after the reaction, and obtain modified β-cyclodextrin; place the modified β-cyclodextrin in N,N-dimethylformamide, then add chitosan and stir, the stirring temperature is 67-69°C, the stirring speed is 128-134rpm, the stirring time is 4.4-4.6h, and after the stirring is completed, naturally cool to room temperature, wash and dry to obtain a composite agent;
[0034] The mass ratio of the β-cyclodextrin, deionized water and epoxidized lignin is 7.6-8.0:117-123:10.2-10.4;
[0035] The mass ratio of the modified beta-cyclodextrin, N,N-dimethylformamide and chitosan is 12.3-12.7:106-115:2.6-2.8.
[0036] 3. Mix
[0037] The bentonite / polyaspartic acid mixture, humic acid, carbendazim, oxazolidinone, a growth agent and a nutrient component are mixed, and the mixture is evenly mixed and then ground to a particle size of 75-85 μm to prepare a mixture 1; the composite agent is mixed with the mixture 1, and the mixture is evenly stirred, and the mixture is heated to 63-67° C. at a rate of 0.4-0.6° C. / min, and the stirring is continued at 63-67° C., the stirring speed is 115-124 rpm, and the stirring time is 2.1-2.5 hours. After the stirring is completed, the mixture is ground to a particle size of 50-70 μm to prepare a coating agent;
[0038] The mass ratio of the bentonite / polyaspartic acid mixture, humic acid, carbendazim, benomyl, growth agent and nutrient components is 98-102:13-15:2.4-2.6:1.5-1.7:1.3-1.6:2.5-3.0;
[0039] The growth agent is a mixture of indolebutyric acid and α-naphthylacetic acid, and the mass ratio of the indolebutyric acid to the α-naphthylacetic acid is 0.8-1.2:1;
[0040] The nutrient component is a mixture of dipotassium hydrogen phosphate, sodium molybdate and zinc sulfate, and the mass ratio of the dipotassium hydrogen phosphate, sodium molybdate and zinc sulfate is 3.8-4.2:1.6-1.8:1.7-2.0;
[0041] The mass ratio of the composite agent to the mixed material is 52-54:86-90.
[0042] A bean vegetable seed coating agent is prepared by the above preparation method.
[0043] Compared with the prior art, the present invention has achieved the following beneficial effects:
[0044] 1. The present invention firstly uses ball milling treatment, and combines pentaerythritol and glycerol components to activate bentonite, which can improve the surface activation performance of bentonite and increase the number of hydroxyl groups. Then, it is treated with aminosilane so that the surface of bentonite contains amino groups. Polyaspartic acid is treated with acyl chloride to obtain modified polyaspartic acid, and the surface of polyaspartic acid is modified with acyl chloride groups. Amide reaction is carried out by amino and acyl chloride groups, so that bentonite and polyaspartic acid are combined through chemical bonds. Polyaspartic acid can form a good coating on bentonite, and the combination is firm, thereby achieving uniform existence of polyaspartic acid in bentonite, avoiding re-agglomeration, and achieving sufficient adsorption of fungicides, nutrients, growth factors and the like.
[0045] The present invention performs epoxidation treatment on lignin, modifies epoxy groups on the surface of lignin, and then mixes with beta-cyclodextrin, wherein the hydroxyl groups of the beta-cyclodextrin react with the epoxy groups of the lignin, and form new epoxy groups under alkaline conditions to obtain modified cyclodextrin, and then compound the modified cyclodextrin with chitosan, so that the epoxy groups of the modified cyclodextrin react with the amino groups of the chitosan to obtain a composite agent, and finally realizes the cross-linking of beta-cyclodextrin, lignin and chitosan to form a stable network structure, and in the mixing step, the mixture is completely coated to achieve the sustained release performance of the coating agent. The coating has good air permeability, excellent stability and high biocompatibility. After the seeds are coated, they have good water absorption and water retention capacity, and they can absorb a large amount of surrounding water and then release it slowly, which greatly enhances the drought resistance of bean vegetables and reduces the adverse effects of saline-alkali environment on seeds, which is beneficial to promote the development of seeds. The nutrients, fungicides and growth agents loaded can be released slowly, always have a high disease prevention rate, and can continuously provide nutrition for seeds, promote seed germination and growth, and ultimately increase the yield and protein content of bean vegetables.
[0046] 2. The coating agent prepared by the present invention is used to coat soybean seeds and used for planting in a common soybean planting base. After 6 days, the germination rate is 97.4-98.5%, the incidence of gray spot is 1.1-1.5%, the incidence of anthracnose is 1.4-1.8%, the yield per mu is 288-294 kg, and the protein content is 42.3-43.2%;
[0047] It is used for planting in saline-alkali land planting bases. The pH of the saline-alkali land planting base is 8.7, the conductivity is 1.63dS / m, the germination rate after 6 days is 93.1-96.7%, the incidence of gray spot is 1.5-2.0%, the incidence of anthracnose is 1.7-2.2%, the yield per mu is 273-281kg, and the protein content is 39.0-40.3%;
[0048] 3. The coating agent prepared by the present invention is used to coat kidney bean seeds and used for planting in a common kidney bean planting base. After 6 days, the germination rate is 98.3-99.1%, the incidence of root rot is 1.3-1.7%, the incidence of leaf spot is 1.6-2.0%, the empty cell rate is 1.2-1.5%, and the yield per mu is 2884-2904 kg;
[0049] For planting in saline-alkali land planting bases, the germination rate after 6 days is 96.8-97.3%, the incidence of root rot is 1.6-2.1%, the incidence of leaf spot is 1.9-2.4%, the empty cell rate is 1.6-2.0%, and the yield per mu is 2812-2835kg;
[0050] 4. The coating agent prepared by the present invention is used to coat cowpea seeds and used for planting in ordinary cowpea planting bases. After 6 days, the germination rate is 97.2-98.3%, the incidence of root rot is 0.8-1.2%, the incidence of leaf spot is 1.5-2.1%, and the yield per mu is 3189-3245 kg;
[0051] Used for planting in saline-alkali land planting bases, the germination rate is 96.4-97.5% after 6 days, the incidence of root rot is 1.2-1.5%, the incidence of leaf spot is 1.4-1.7%, and the yield per mu is 3109-3187kg. DETAILED DESCRIPTION
[0052] In order to more clearly understand the technical features, purposes and effects of the present invention, specific embodiments of the present invention are now described.
[0053] Example 1
[0054] 1. Preparation of Bentonite / Polyaspartic Acid Mixture
[0055] (1) Aminated bentonite
[0056] 6.5 g of bentonite was placed in 52 g of sodium hydroxide solution and stirred for 3.2 h at a temperature of 58° C. After the stirring was completed, the mixture was filtered and dried, and then placed in 63 g of ethanol solution for ball milling for 30 min at a ball milling speed of 211 rpm and a ball-to-material ratio of 4:1. After the ball milling was completed, 0.8 g of pentaerythritol and 1.0 g of glycerol were added and stirred for 27 min at a temperature of 54° C. After the stirring was completed, 0.6 g of 3-aminopropyltriethoxysilane was added, the temperature was raised to 70° C., and the mixture was reacted at 70° C. for 6 h. After the reaction was completed, the mixture was dried to obtain amino bentonite;
[0057] The mass concentration of the sodium hydroxide solution is 24%;
[0058] The mass concentration of the ethanol solution is 45%;
[0059] (2) Amide reaction
[0060] 10 g of polyaspartic acid was placed in 65 mL of dichloromethane, and 20 g of thionyl chloride was added dropwise after stirring. After the addition was completed, the temperature was raised to 62°C for reaction for 10 h. After the reaction was completed, the modified polyaspartic acid was obtained by rotary evaporation. 0.05 g of modified polyaspartic acid and 2 g of amino bentonite were added to 110 mL of N, N-dimethylformamide, and ultrasonic oscillation treatment was performed. The ultrasonic time was 17 min, the ultrasonic frequency was 24 kHz, and the ultrasonic power was 110 W. After the ultrasonic oscillation treatment was completed, the temperature was raised to 62°C at a rate of 1.0°C / min, and the mixture was reacted at 62°C for 48 h. After the reaction was completed, the mixture was washed and dried to obtain a bentonite / polyaspartic acid mixture.
[0061] 2. Preparation of composite agent
[0062] (1) Preparation of epoxidized lignin
[0063] Add 0.8 g of γ-glycidyloxypropyltrimethoxysilane to 75 g of ethanol solution and stir until uniform to obtain a modifier; place 12 g of lignin in 97 g of the modifier, add 1.3 g of polyethylene glycol 2000 for ultrasonic treatment, the ultrasonic time is 20 min, the ultrasonic frequency is 35 kHz, the ultrasonic power is 87 W, after the ultrasonic treatment, heat to 71 ° C at a rate of 1.2 ° C / min, stir to react for 10 hours, after the reaction is completed, filter and dry to obtain epoxidized lignin;
[0064] The mass concentration of the ethanol solution is 45%;
[0065] (2) Composite
[0066] 7.8g of β-cyclodextrin was added to 120g of deionized water, and then 10.3g of epoxidized lignin was added. After stirring evenly, 32wt% of sodium hydroxide solution was added, and the pH was adjusted to 11.5. The mixture was stirred at a speed of 180rpm for 5h. After the reaction was completed, the mixture was washed and dried to obtain modified β-cyclodextrin. 12.5g of modified β-cyclodextrin was placed in 110g of N,N-dimethylformamide, and then 2.7g of chitosan was added and stirred. The stirring temperature was 68°C, the stirring speed was 130rpm, and the stirring time was 4.5h. After stirring, it was naturally cooled to room temperature, washed and dried to obtain a composite agent.
[0067] 3. Mix
[0068] 100 g of bentonite / polyaspartic acid mixture, 14 g of humic acid, 2.5 g of carbendazim, 1.6 g of oxadiazine, 1.5 g of growth agent and 2.7 g of nutrients were mixed, and the mixture was evenly ground to a particle size of 80 μm to prepare a mixture 1; 53 g of the composite agent was mixed with 88 g of the mixture 1, and the mixture was evenly stirred, and the mixture was heated to 75° C. at a rate of 0.5° C. / min, and the mixture was continuously stirred at 75° C. with a stirring speed of 120 rpm for 2.3 h. After the stirring was completed, the mixture was ground to a particle size of 60 μm to prepare a coating agent;
[0069] The growth agent is a mixture of indolebutyric acid and α-naphthylacetic acid, and the mass ratio of the indolebutyric acid to the α-naphthylacetic acid is 1:1;
[0070] The nutrient component is a mixture of dipotassium hydrogen phosphate, sodium molybdate and zinc sulfate, and the mass ratio of the dipotassium hydrogen phosphate, sodium molybdate and zinc sulfate is 4.0:1.7:1.9.
[0071] Example 2
[0072] 1. Preparation of Bentonite / Polyaspartic Acid Mixture
[0073] (1) Aminated bentonite
[0074] 6.3 g of bentonite was placed in 50 g of sodium hydroxide solution and stirred for 3.0 h at a temperature of 56° C. After the stirring was completed, the mixture was filtered and dried, and then placed in 61 g of ethanol solution for ball milling for 28 min at a ball milling speed of 208 rpm and a ball-to-material ratio of 3:1. After the ball milling was completed, 0.7 g of pentaerythritol and 0.8 g of glycerol were added and stirred for 25 min at a temperature of 53° C. After the stirring was completed, 0.5 g of 3-aminopropyltriethoxysilane was added, the temperature was raised to 68° C., and the mixture was reacted at 68° C. for 5.8 h. After the reaction was completed, the mixture was dried to obtain amino bentonite;
[0075] The mass concentration of the sodium hydroxide solution is 22%;
[0076] The mass concentration of the ethanol solution is 43%;
[0077] (2) Amide reaction
[0078] 9 g of polyaspartic acid was placed in 63 mL of dichloromethane, and 18 g of thionyl chloride was added dropwise after stirring. After the addition was completed, the temperature was raised to 60°C for reaction for 9.8 h. After the reaction was completed, the modified polyaspartic acid was obtained by rotary evaporation. 0.04 g of modified polyaspartic acid and 1.8 g of amino bentonite were added to 106 mL of N, N-dimethylformamide, and ultrasonic oscillation treatment was performed. The ultrasonic time was 15 min, the ultrasonic frequency was 23 kHz, and the ultrasonic power was 107 W. After the ultrasonic oscillation treatment was completed, the temperature was raised to 60°C at a rate of 0.8°C / min, and the mixture was reacted at 60°C for 46 h. After the reaction was completed, the mixture was washed and dried to obtain a bentonite / polyaspartic acid mixture.
[0079] 2. Preparation of composite agent
[0080] (1) Preparation of epoxidized lignin
[0081] 0.7 g of γ-glycidyloxypropyltrimethoxysilane was added to 73 g of ethanol solution and stirred, and a modifier was obtained after uniform stirring; 11 g of lignin was placed in 95 g of the modifier, and 1.2 g of polyethylene glycol 2000 was added for ultrasonic treatment, the ultrasonic time was 18 min, the ultrasonic frequency was 33 kHz, and the ultrasonic power was 85 W. After the ultrasonic treatment, the temperature was raised to 70 ° C at a rate of 1.0 ° C / min, and the reaction was stirred for 9.5 hours. After the reaction was completed, it was filtered and dried to obtain epoxidized lignin;
[0082] The mass concentration of the ethanol solution is 43%;
[0083] (2) Composite
[0084] 7.6g of β-cyclodextrin was added to 117g of deionized water, and then 10.2g of epoxidized lignin was added. After stirring evenly, 30wt% of sodium hydroxide solution was added, and the pH was adjusted to 11.2. The mixture was stirred at a speed of 172rpm for 4.8h. After the reaction was completed, the mixture was washed and dried to obtain modified β-cyclodextrin. 12.3g of modified β-cyclodextrin was placed in 106g of N,N-dimethylformamide, and then 2.6g of chitosan was added and stirred. The stirring temperature was 67°C, the stirring speed was 128rpm, and the stirring time was 4.4h. After stirring, the mixture was naturally cooled to room temperature, washed and dried to obtain a composite agent.
[0085] 3. Mix
[0086] 98 g of bentonite / polyaspartic acid mixture, 13 g of humic acid, 2.4 g of carbendazim, 1.5 g of oxadiazine, 1.3 g of growth agent and 2.5 g of nutrient components were mixed, and the mixture was evenly mixed and then ground to a particle size of 75 μm to prepare a mixture 1; 52 g of the composite agent was mixed with 86 g of the mixture 1, and the mixture was evenly stirred, and the mixture was heated to 63° C. at a rate of 0.4° C. / min, and the mixture was continuously stirred at 63° C. with a stirring speed of 115 rpm for 2.1 h. After the stirring was completed, the mixture was ground to a particle size of 50 μm to prepare a coating agent;
[0087] The growth agent is a mixture of indolebutyric acid and α-naphthylacetic acid, and the mass ratio of the indolebutyric acid to the α-naphthylacetic acid is 0.8:1;
[0088] The nutrient component is a mixture of dipotassium hydrogen phosphate, sodium molybdate and zinc sulfate, and the mass ratio of the dipotassium hydrogen phosphate, sodium molybdate and zinc sulfate is 3.8:1.6:1.7.
[0089] Example 3
[0090] 1. Preparation of Bentonite / Polyaspartic Acid Mixture
[0091] (1) Aminated bentonite
[0092] 6.7 g of bentonite was placed in 54 g of sodium hydroxide solution and stirred for 3.3 h at a temperature of 60° C. After the stirring was completed, the mixture was filtered and dried, and then placed in 65 g of ethanol solution for ball milling for 32 min at a ball milling speed of 215 rpm and a ball-to-material ratio of 5:1. After the ball milling was completed, 0.9 g of pentaerythritol and 1.2 g of glycerol were added and stirred for 29 min at a temperature of 55° C. After the stirring was completed, 0.7 g of 3-aminopropyltriethoxysilane was added, the temperature was raised to 72° C., and the mixture was reacted at 72° C. for 6.2 h. After the reaction was completed, the mixture was dried to obtain amino bentonite;
[0093] The mass concentration of the sodium hydroxide solution is 26%;
[0094] The mass concentration of the ethanol solution is 47%;
[0095] (2) Amide reaction
[0096] 11 g of polyaspartic acid was placed in 67 mL of dichloromethane, and 22 g of thionyl chloride was added dropwise after stirring. After the addition was completed, the temperature was raised to 64°C for reaction for 10.2 h. After the reaction was completed, the modified polyaspartic acid was obtained by rotary evaporation. 0.06 g of modified polyaspartic acid and 2.2 g of amino bentonite were added to 115 mL of N, N-dimethylformamide, and ultrasonic oscillation treatment was performed. The ultrasonic time was 19 min, the ultrasonic frequency was 25 kHz, and the ultrasonic power was 112 W. After the ultrasonic oscillation treatment was completed, the temperature was raised to 64°C at a rate of 1.2°C / min, and the mixture was reacted at 64°C for 50 h. After the reaction was completed, the mixture was washed and dried to obtain a bentonite / polyaspartic acid mixture.
[0097] 2. Preparation of composite agent
[0098] (1) Preparation of epoxidized lignin
[0099] Add 0.9 g of γ-glycidyloxypropyltrimethoxysilane to 77 g of ethanol solution and stir until uniform to obtain a modifier; place 13 g of lignin in 99 g of the modifier, add 1.4 g of polyethylene glycol 2000 for ultrasonic treatment, the ultrasonic time is 22 min, the ultrasonic frequency is 37 kHz, the ultrasonic power is 90 W, after the ultrasonic treatment, heat to 72 ° C at a rate of 1.4 ° C / min, stir to react for 10.4 h, after the reaction is completed, filter and dry to obtain epoxidized lignin;
[0100] The mass concentration of the ethanol solution is 47%;
[0101] (2) Composite
[0102] 8.0g of β-cyclodextrin was added to 123g of deionized water, and then 10.4g of epoxidized lignin was added. After stirring evenly, 34wt% of sodium hydroxide solution was added, and the pH was adjusted to 11.8. The mixture was stirred at a speed of 186rpm for 5.3h. After the reaction was completed, the mixture was washed and dried to obtain modified β-cyclodextrin. 12.7g of modified β-cyclodextrin was placed in 115g of N,N-dimethylformamide, and then 2.8g of chitosan was added and stirred. The stirring temperature was 69°C, the stirring speed was 134rpm, and the stirring time was 4.6h. After stirring, the mixture was naturally cooled to room temperature, washed and dried to obtain a composite agent.
[0103] 3. Mix
[0104] 102 g of bentonite / polyaspartic acid mixture, 15 g of humic acid, 2.6 g of carbendazim, 1.7 g of oxadipate, 1.6 g of growth agent and 3.0 g of nutrients were mixed, and the mixture was evenly ground to a particle size of 85 μm to prepare a mixture 1; 54 g of the composite agent was mixed with 90 g of the mixture 1, and the mixture was evenly stirred, and the mixture was heated to 67° C. at a rate of 0.6° C. / min, and the mixture was continuously stirred at 67° C. at a stirring speed of 124 rpm for 2.5 h. After the stirring was completed, the mixture was ground to a particle size of 70 μm to prepare a coating agent;
[0105] The growth agent is a mixture of indolebutyric acid and α-naphthylacetic acid, and the mass ratio of the indolebutyric acid to the α-naphthylacetic acid is 1.2:1;
[0106] The nutrient component is a mixture of dipotassium hydrogen phosphate, sodium molybdate and zinc sulfate, and the mass ratio of the dipotassium hydrogen phosphate, sodium molybdate and zinc sulfate is 4.2:1.8:2.0.
[0107] Comparative Example 1
[0108] Based on Example 1, the change is that in the step of preparing the bentonite / polyaspartic acid mixture, the amination step of bentonite and the modification step of polyaspartic acid are omitted;
[0109] The compounding step comprises mixing 0.05 g of polyaspartic acid and 2 g of bentonite, and subjecting the mixture to ultrasonic oscillation treatment, wherein the ultrasonic oscillation time is 17 min, the ultrasonic frequency is 24 kHz, and the ultrasonic power is 110 W. After the ultrasonic oscillation is completed, a bentonite / polyaspartic acid mixture is obtained.
[0110] The rest of the operations are the same.
[0111] Comparative Example 2
[0112] Based on Example 1, the change is that the preparation method of the composite agent is:
[0113] (1) The preparation step of epoxidized lignin is omitted, and in the compounding step, an equal amount of epoxidized lignin is replaced by lignin;
[0114] (2) The compounding step is:
[0115] 7.8 g of β-cyclodextrin was added to 120 g of deionized water, and then 10.3 g of lignin was added. After stirring evenly, 32 wt% of sodium hydroxide solution was added, and the pH was adjusted to 11.5. The mixture was stirred at a speed of 180 rpm for 5 h. After the reaction was completed, the mixture was washed and dried to obtain modified β-cyclodextrin. 12.5 g of modified β-cyclodextrin and 2.7 g of chitosan were mixed and stirred at a stirring temperature of 68° C., a stirring speed of 130 rpm, and a stirring time of 4.5 h. After the stirring was completed, the mixture was naturally cooled to room temperature to obtain a composite agent.
[0116] The rest of the operations are the same.
[0117] Test Example 1
[0118] (1) General soybean cultivation
[0119] The coating agents prepared in Example 1-3 and Comparative Example 1-2 were used to coat soybean seeds, the soybean variety was Fudou No. 9, and the mass ratio of the coating agent to the soybean seeds was controlled to be 2.3:200, to prepare coated soybean seeds;
[0120] A common soybean planting base was selected in Shouguang City, Weifang City, Shandong Province. The planting base had a total area of 10 mu, which was divided into 5 blocks on average, with an average area of 2 mu per block. Then, the coated soybean seeds prepared by the coating agents of Examples 1-3 and Comparative Examples 1-2 were respectively sown, and the corresponding management was as follows:
[0121]
[0122] Among them, the sowing method adopted is equal hole sowing, 2 seeds per hole, plant spacing 30cm, row spacing 40cm; the conventional planting method was used to plant soybeans, and the soil conditions, water and fertilizer management, etc. of the 5 planting bases were controlled to be consistent during sowing. After 6 days of sowing, the soybean germination rate of planting bases 1-5 was counted respectively, and the incidence of soybean gray spot and anthracnose during the growth cycle was counted, and the per mu yield was counted. The protein content of the harvested soybeans was tested, and the statistical results are as follows:
[0123]
[0124] (2) Soybean cultivation in saline-alkali land
[0125] The coating agents prepared in Example 1-3 and Comparative Example 1-2 were used to coat soybean seeds, the soybean variety was Fudou No. 9, and the mass ratio of the coating agent to the soybean seeds was controlled to be 2.3:200, to prepare coated soybean seeds;
[0126] A saline-alkali land planting base was selected in Binhai District, Weifang City, Shandong Province. The pH of the saline-alkali land planting base was 8.7, the conductivity was 1.63 dS / m, the planting base was 10 mu in total, and was divided into 5 blocks on average, each block was 2 mu on average, and then the coated soybean seeds prepared by the coating agents of Examples 1-3 and Comparative Examples 1-2 were respectively used for sowing, and the corresponding management was as follows:
[0127]
[0128] Among them, the sowing method adopted is equal hole sowing, 2 seeds per hole, plant spacing 30cm, row spacing 40cm; the conventional planting method was used to plant soybeans, and the soil conditions, water and fertilizer management, etc. of the 5 planting bases were controlled to be consistent during sowing. After 6 days of sowing, the soybean germination rate of planting bases 1-5 was counted respectively, and the incidence of soybean gray spot and anthracnose during the growth cycle was counted, and the per mu yield was counted. The protein content of the harvested soybeans was tested, and the statistical results are as follows:
[0129]
[0130] Test Example 2
[0131] (1) Common bean cultivation
[0132] The bean seeds were coated with the coating agents prepared in Examples 1-3 and Comparative Examples 1-2, respectively. The bean variety was Shuangqing 35, and the mass ratio of the coating agent to the bean seeds was controlled to be 2.3:200, to prepare coated bean seeds;
[0133] A common bean planting base was selected in Shouguang City, Weifang City, Shandong Province. The planting base was 10 mu in total and was divided into 5 blocks, with an average of 2 mu per block. Then, the coated bean seeds prepared by the coating agents of Examples 1-3 and Comparative Examples 1-2 were respectively sown, and the corresponding management was as follows:
[0134]
[0135] Among them, the sowing method adopted iso-hole sowing, 2 seeds per hole, plant spacing 30cm, row spacing 40cm; conventional planting methods were used to plant kidney beans, and the soil conditions, water and fertilizer management, etc. of the 5 planting bases were controlled to be consistent during sowing. After 6 days of sowing, the germination rate of kidney beans in planting bases 1-5 was counted respectively, and the incidence of root rot and leaf spot of kidney beans during the growth cycle was counted, and the empty room rate and per mu yield were counted. The statistical results are as follows:
[0136]
[0137] (2) Planting beans on saline-alkali land
[0138] The bean seeds were coated with the coating agents prepared in Examples 1-3 and Comparative Examples 1-2, respectively. The bean variety was Shuangqing 35, and the mass ratio of the coating agent to the bean seeds was controlled to be 2.3:200, to prepare coated bean seeds;
[0139] A saline-alkali land planting base was selected in Binhai District, Weifang City, Shandong Province. The pH of the saline-alkali land planting base was 8.7, the conductivity was 1.63 dS / m, the planting base was 10 mu in total, and was divided into 5 blocks on average, with an average of 2 mu per block. Then, the coated kidney bean seeds prepared by the coating agents of Examples 1-3 and Comparative Examples 1-2 were respectively used for sowing, and the corresponding management was as follows:
[0140]
[0141] Among them, the sowing method adopts the equal hole sowing method, 2 seeds per hole, 30cm plant spacing, and 40cm row spacing; conventional planting methods are used to plant kidney beans, and the soil conditions, water and fertilizer management, etc. of the 5 planting bases are controlled to be consistent during sowing. After 6 days of sowing, the germination rate of kidney beans in planting bases 1-5 was counted respectively, and the incidence of root rot and leaf spot of kidney beans during the growth cycle was counted, and the empty room rate and per mu yield were counted. The statistical results are as follows:
[0142]
[0143] Test Example 3
[0144] (1) Common planting of cowpea
[0145] The cowpea seeds were coated with the coating agents prepared in Example 1-3 and Comparative Example 1-2, the cowpea variety was cowpea 28-2, and the mass ratio of the coating agent to the cowpea seeds was controlled to be 2.3:200, to obtain coated cowpea seeds;
[0146] A common cowpea planting base was selected in Shouguang City, Weifang City, Shandong Province. The planting base was 10 mu in total and was divided into 5 blocks, each of which was 2 mu on average. Then, the coated cowpea seeds prepared by the coating agents of Examples 1-3 and Comparative Examples 1-2 were respectively sown, and the corresponding management was as follows:
[0147]
[0148] Among them, the sowing method adopted is equal hole sowing, 2 seeds per hole, plant spacing 30cm, row spacing 40cm; the cowpea was planted using conventional planting methods, and the soil conditions, water and fertilizer management, etc. of the 5 planting bases were controlled to be consistent during sowing. After 6 days of sowing, the cowpea germination rate of planting bases 1-5 was counted respectively, and the incidence of root rot and virus disease and yield of cowpea during the growth cycle were counted. The statistical results are as follows:
[0149]
[0150] (2) Cowpea cultivation in saline-alkali land
[0151] The cowpea seeds were coated with the coating agents prepared in Example 1-3 and Comparative Example 1-2, the cowpea variety was cowpea 28-2, and the mass ratio of the coating agent to the cowpea seeds was controlled to be 2.3:200, to obtain coated cowpea seeds;
[0152] A saline-alkali land planting base was selected in Binhai District, Weifang City, Shandong Province. The pH of the saline-alkali land planting base was 8.7, the conductivity was 1.63 dS / m, the planting base was 10 mu in total, and was divided into 5 blocks on average, with an average of 2 mu per block. Then, the coated cowpea seeds prepared by the coating agents of Examples 1-3 and Comparative Examples 1-2 were respectively used for sowing, and the corresponding management was as follows:
[0153]
[0154] Among them, the sowing method adopted is equal hole sowing, 2 seeds per hole, plant spacing 30cm, row spacing 40cm; the cowpea was planted using conventional planting methods, and the soil conditions, water and fertilizer management, etc. of the 5 planting bases were controlled to be consistent during sowing. After 6 days of sowing, the germination rate of cowpea in planting bases 1-5 was counted respectively, and the incidence of root rot and virus disease and yield of cowpea during the growth cycle were counted. The statistical results are as follows:
[0155]
[0156] Comparative Example 1 omits the amination step of bentonite and the modification step of polyaspartic acid. In the compounding step, polyaspartic acid and bentonite are directly mixed, and the mixing is only physical. Moreover, bentonite is easy to agglomerate, and the connection between polyaspartic acid and bentonite is unstable. The obtained bentonite / polyaspartic acid mixture has poor binding force and poor stability. It cannot completely adsorb fungicides, nutrients and growth agents, thereby affecting the sustained-release performance of the coating agent. After being used for coating bean vegetable seeds, it cannot continuously provide nutrients and other substances to the bean vegetable seeds, and has poor water absorption and water retention capacity. The saline-alkali environment has an adverse effect on the seeds, affects the development of the seeds and the growth of the crops, increases the incidence rate, and ultimately reduces the yield and protein content of the bean vegetables.
[0157] In the step of preparing the composite agent in Comparative Example 2, β-cyclodextrin, lignin and chitosan are simply mixed. The three cannot be effectively cross-linked, and thus a stable network structure cannot be formed. In the mixing step, the mixture cannot be completely wrapped, thereby affecting the sustained-release performance of nutrients, fungicides and growth agents, reducing water absorption and water retention performance, and finally affecting the germination of legume vegetable seeds, reducing yield and protein content.
[0158] The invention firstly adopts ball milling treatment, and combines pentaerythritol and glycerol components to carry out activation treatment on bentonite, which can improve the surface activation performance of bentonite and increase the number of hydroxyl groups, and then carries out aminosilane treatment so that the surface of bentonite contains amino groups; polyaspartic acid is subjected to acyl chloride treatment to obtain modified polyaspartic acid, the surface of which is modified with acyl chloride groups, and amidation reaction is carried out by amino groups and acyl chloride groups so that bentonite and polyaspartic acid are combined through chemical bonds, and polyaspartic acid can form a good coating on bentonite, and the combination is firm, thereby realizing the uniform existence of polyaspartic acid in bentonite, avoiding the phenomenon of re-agglomeration, and realizing the full adsorption of fungicides, nutrients, growth and other components;
[0159] The present invention performs epoxidation treatment on lignin, modifies epoxy groups on the surface of lignin, and then mixes with beta-cyclodextrin, wherein the hydroxyl groups of the beta-cyclodextrin react with the epoxy groups of the lignin, and form new epoxy groups under alkaline conditions to obtain modified cyclodextrin, and then compound the modified cyclodextrin with chitosan, so that the epoxy groups of the modified cyclodextrin react with the amino groups of the chitosan to obtain a composite agent, and finally realizes the cross-linking of beta-cyclodextrin, lignin and chitosan to form a stable network structure, and in the mixing step, the mixture is completely coated to achieve the sustained release performance of the coating agent. It has good air permeability, excellent stability and high biocompatibility. After the seeds are coated, they have good water absorption and water retention capabilities, and they can absorb a large amount of surrounding water and then release it slowly, which greatly enhances the drought resistance of legumes and reduces the adverse effects of saline-alkali environment on seeds, which is beneficial to promote seed development. The loaded nutrients, fungicides and growth agents can be slowly released, always have a high disease prevention rate, and can continuously provide nutrition for seeds, promote seed germination and growth, and ultimately increase the yield and protein content of legumes and vegetables.
[0160] Unless otherwise specified, all ratios and percentages described in the present invention are by mass ratios and percentages are by mass percentages.
[0161] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for preparing a bean vegetable seed coating agent, characterized in that: The preparation method comprises the steps of preparing a bentonite / polyaspartic acid mixture, preparing a composite agent and mixing; The preparation of the bentonite / polyaspartic acid mixture includes the steps of amination of bentonite and amide reaction; The step of aminating bentonite is to place bentonite in a sodium hydroxide solution for a first stirring, filter and dry the bentonite after the stirring, and then place the bentonite in an ethanol solution for ball milling. After the ball milling, add pentaerythritol and glycerol, and stir the bentonite for a second time. After the stirring, add 3-aminopropyltriethoxysilane, raise the temperature to 68-72° C., react at 68-72° C. for 5.8-6.2 hours, and dry the bentonite after the reaction to obtain the aminating bentonite. The amide reaction comprises the following steps: placing polyaspartic acid in dichloromethane, stirring evenly, then dripping thionyl chloride, heating to 60-64°C for reaction after the dripping is completed, and the reaction time is 9.8-10.2 hours. After the reaction is completed, rotary evaporation is performed to obtain modified polyaspartic acid; adding modified polyaspartic acid and amino bentonite to N,N-dimethylformamide, and performing ultrasonic oscillation treatment. After the ultrasonic oscillation treatment is completed, heating to 60-64°C at a rate of 0.8-1.2°C / min, reacting at 60-64°C for 46-50 hours, washing and drying after the reaction is completed, and obtaining a bentonite / polyaspartic acid mixture; The preparation of the composite agent comprises the steps of preparing epoxidized lignin and compounding; The step of epoxidizing lignin is to add γ-glycidyloxypropyltrimethoxysilane to an ethanol solution and stir the mixture to obtain a modifier; place lignin in the modifier, add polyethylene glycol 2000 for ultrasonic treatment, and after the ultrasonic treatment, heat the mixture to 70-72° C. at a rate of 1.0-1.4° C. / min, stir the mixture for reaction for 9.5-10.4 hours, and filter and dry the mixture after the reaction to obtain epoxidized lignin; The compounding step comprises: adding β-cyclodextrin to deionized water, then adding epoxidized lignin, stirring evenly, adding 30-34wt% sodium hydroxide solution, adjusting the pH to 11.2-11.8, performing a stirring reaction, washing and drying after the reaction is completed, and obtaining modified β-cyclodextrin; placing the modified β-cyclodextrin in N,N-dimethylformamide, and then adding chitosan for a second stirring, cooling naturally to room temperature after the stirring is completed, washing and drying, and obtaining a composite agent; The mixing step comprises mixing the bentonite / polyaspartic acid mixture, humic acid, carbendazim, oxazolidinone, a growth agent and a nutrient component, and grinding the mixture to a particle size of 75-85 μm after mixing evenly to obtain a mixture 1; mixing the composite agent with the mixture 1, stirring evenly, heating the mixture to 63-67° C. at a rate of 0.4-0.6° C. / min, continuing stirring at 63-67° C., the stirring speed is 115-124 rpm, the stirring time is 2.1-2.5 h, and grinding the mixture to a particle size of 50-70 μm after the stirring is completed to obtain a coating agent; The mass ratio of the bentonite / polyaspartic acid mixture, humic acid, carbendazim, benomyl, growth agent and nutrient components is 98-102:13-15:2.4-2.6:1.5-1.7:1.3-1.6:2.5-3.0; The mass ratio of the composite agent to the mixed material is 52-54:86-90; The growth agent is a mixture of indolebutyric acid and α-naphthylacetic acid; The nutrient component is a mixture of dipotassium hydrogen phosphate, sodium molybdate and zinc sulfate.
2. The method for preparing a bean vegetable seed coating agent according to claim 1, characterized in that: In the step of aminating bentonite, the mass concentration of the sodium hydroxide solution is 22-26%; The mass concentration of the ethanol solution is 43-47%; The mass ratio of the bentonite, sodium hydroxide solution, ethanol solution, pentaerythritol, glycerol and 3-aminopropyltriethoxysilane is 6.3-6.7:50-54:61-65:0.7-0.9:0.8-1.2:0.5-0.7; The stirring time is 3.0-3.3h and the stirring temperature is 56-60°C; The ball milling treatment comprises a ball milling time of 28-32 minutes, a ball milling speed of 208-215 rpm, and a ball-to-material ratio of 3-5:1; The secondary stirring has a stirring time of 25-29 minutes and a stirring temperature of 53-55°C.
3. The method for preparing a bean vegetable seed coating agent according to claim 1, characterized in that: In the step of amide reaction, the mass volume ratio of polyaspartic acid, dichloromethane and thionyl chloride is 9-11 g:63-67 mL:18-22 g; The mass volume ratio of the N,N-dimethylformamide, modified polyaspartic acid and amino bentonite is 106-115 mL: 0.04-0.06 g: 1.8-2.2 g; The ultrasonic oscillation treatment has an ultrasonic time of 15-19 min, an ultrasonic frequency of 23-25 kHz, and an ultrasonic power of 107-112 W.
4. The method for preparing a bean vegetable seed coating agent according to claim 1, characterized in that: In the step of preparing epoxidized lignin, the mass concentration of the ethanol solution is 43-47%; The mass ratio of the ethanol solution to γ-glycidyloxypropyltrimethoxysilane is 73-77:0.7-0.9; The mass ratio of the lignin, the modifier and the polyethylene glycol 2000 is 11-13:95-99:1.2-1.4; The ultrasonic treatment has an ultrasonic time of 18-22 min, an ultrasonic frequency of 33-37 kHz, and an ultrasonic power of 85-90 W.
5. The method for preparing a bean vegetable seed coating agent according to claim 1, characterized in that: In the compounding step, the mass ratio of the β-cyclodextrin, deionized water, and epoxidized lignin is 7.6-8.0:117-123:10.2-10.4; The mass ratio of the modified β-cyclodextrin, N,N-dimethylformamide and chitosan is 12.3-12.7:106-115:2.6-2.8; The stirring reaction was performed at a speed of 172-186 rpm and a time of 4.8-5.3 h. The secondary stirring has a stirring temperature of 67-69° C., a stirring speed of 128-134 rpm, and a stirring time of 4.4-4.6 h.
6. The method for preparing a bean vegetable seed coating agent according to claim 1, characterized in that: In the growth agent, the mass ratio of indolebutyric acid to α-naphthylacetic acid is 0.8-1.2:1; Among the nutritional ingredients, the mass ratio of dipotassium hydrogen phosphate, sodium molybdate and zinc sulfate is 3.8-4.2:1.6-1.8:1.7-2.
0.
7. A bean vegetable seed coating agent prepared according to the preparation method according to any one of claims 1 to 6.