Hollow core anti-resonant optical fiber processing equipment control method and system
By setting up a control system in the hollow-core anti-resonant optical fiber processing equipment to dynamically adjust the deposition rate, the problems of uneven deposition and microstructure deformation are solved, and the preform quality and optical fiber transmission efficiency are improved.
Patent Information
- Application Number
- CN202411008144.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-07-26
AI Technical Summary
During the processing of hollow-core antiresonant optical fibers, the deposition rate is difficult to dynamically adjust, resulting in uneven deposition of glass materials and microstructural deformation, which affects the quality of the preform and the transmission efficiency of the optical fiber.
By setting up a control system in the processing equipment, predicting chemical reagent flow fluctuations, calculating raw material purity changes and temperature change indexes, using linear regression analysis models to calculate rate correction coefficients, and dynamically adjusting the deposition rate to ensure the stability of the deposition process.
It effectively ensures the quality of the preform and the transmission efficiency of the hollow-core anti-resonant fiber, reduces uneven deposition and microstructural damage, and improves the precision and stability of the processing process.
Smart Images

Figure CN118550260B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of optical fiber processing equipment control, and in particular to a hollow-core anti-resonance optical fiber processing equipment control method and system. Background Art
[0002] Hollow-core-anti-resonant-fiber (HC-ARF) is a new type of optical fiber that has attracted widespread attention in the fields of optical communications, sensing and laser technology in recent years. Unlike traditional solid-core optical fibers, the design principle of hollow-core anti-resonant optical fibers is based on the anti-resonance effect. It achieves efficient light propagation by controlling the microstructure around the core. The processing of hollow-core anti-resonant optical fibers has extremely high requirements for equipment control, and requires precise technology and equipment to achieve high-quality optical fiber manufacturing.
[0003] When manufacturing hollow-core antiresonant optical fiber preform, it is necessary to deposit high-purity glass material on the substrate through chemical vapor deposition technology to form the basic structure of the optical fiber preform. During the preform manufacturing process, the processing equipment usually deposits high-purity glass material on the substrate according to a preset deposition rate. Due to the uncertainties in the actual processing process, the deposition rate cannot be dynamically adjusted according to the uncertainties that arise during processing. First, it may cause uneven deposition of glass materials and affect the quality of the preform. Second, the microstructure in the preform may be deformed or damaged during the deposition process, affecting the antiresonance effect of the hollow-core antiresonant optical fiber and reducing its transmission efficiency. Summary of the invention
[0004] The purpose of the present invention is to provide a hollow-core anti-resonant optical fiber processing equipment control method and system, which can dynamically adjust the deposition rate according to the uncertain factors occurring during the processing during the preform manufacturing process, thereby ensuring the quality of the preform and improving the transmission efficiency of the hollow-core anti-resonant optical fiber, so as to solve the shortcomings of the background technology.
[0005] In order to achieve the above object, the present invention provides the following technical solution: a method for controlling a hollow-core anti-resonant optical fiber processing device, the control method comprising the following steps:
[0006] Before the processing equipment manufactures the preform based on the chemical vapor deposition technology, the control system generates the initial deposition rate of the processing equipment according to the database, and predicts whether the flow of chemical reagents will fluctuate during the deposition process during the operation of the processing equipment, and outputs the flow fluctuation value when the chemical reagent flow is predicted to fluctuate;
[0007] Calculate the change in the purity of the raw materials at each time point, and accumulate the change at discrete time points to obtain the cumulative change in purity over a period of time. Use a temperature sensor to monitor the temperature conditions in the deposition environment, generate a temperature change index based on the temperature conditions, and analyze whether each monitoring target is qualified based on flow fluctuation assignment, cumulative change, and temperature change index. If unqualified, the control system controls the processing equipment to stop running and sends a warning signal;
[0008] If qualified, the flow fluctuation assignment, cumulative change, and temperature change index are substituted into the linear regression analysis model to calculate the output rate correction coefficient, and based on the comparison result between the rate correction coefficient and the coefficient threshold, it is determined whether the deposition rate needs to be dynamically adjusted. If the deposition rate needs to be adjusted, the adjusted deposition rate is updated based on the adjustment algorithm, and the control system controls the processing equipment to manufacture preform rods at the adjusted deposition rate.
[0009] In a preferred embodiment, analyzing whether each monitoring target is qualified based on flow fluctuation assignment, cumulative change, and temperature change index includes the following steps:
[0010] The obtained flow fluctuation value is compared with the second fluctuation threshold, and the second fluctuation threshold is greater than the first fluctuation threshold. If the flow fluctuation value is greater than the second fluctuation threshold, it is judged that the chemical reagent flow monitoring is unqualified, and the control system controls the processing equipment to stop running and sends a warning signal;
[0011] The obtained cumulative change is compared with the change threshold. If the cumulative change is greater than the change threshold, it is judged that the purity of the raw material does not meet the standard, and the control system controls the processing equipment to stop running and sends a warning signal;
[0012] The obtained temperature change index is compared with the index threshold. If the temperature change index is greater than the index threshold, it is judged that the temperature fluctuation is too large, and the control system controls the processing equipment to stop running and sends a warning signal;
[0013] If the flow fluctuation value is less than or equal to the second fluctuation threshold, the cumulative change is less than or equal to the change threshold, and the temperature change index is less than or equal to the index threshold, it is confirmed that each monitoring target is qualified.
[0014] In a preferred embodiment, the flow fluctuation assignment, the cumulative change, and the temperature change index are substituted into the linear regression analysis model to calculate the output rate correction coefficient, and the comparison result between the rate correction coefficient and the coefficient threshold is used to determine whether the deposition rate needs to be dynamically adjusted, including the following steps:
[0015] Substitute the flow fluctuation assignment, cumulative change, and temperature change index into the linear regression analysis model to calculate the output rate correction coefficient. The function expression is:
[0016] , where is the rate correction factor, Assign a value to the flow fluctuation, is the cumulative change, is the temperature change index, , , are the proportional coefficients of flow fluctuation, cumulative change, and temperature change index, respectively, and , , All are greater than 0;
[0017] The obtained rate correction coefficient is compared with the preset coefficient threshold. If the rate correction coefficient is less than or equal to the coefficient threshold, it is determined that there is no need to dynamically adjust the deposition rate. If the rate correction coefficient is greater than the coefficient threshold, it is determined that there is a need to dynamically adjust the deposition rate.
[0018] In a preferred embodiment, if the deposition rate needs to be adjusted, the adjusted deposition rate is updated based on the adjustment algorithm, including the following steps:
[0019] The adjusted deposition rate is updated based on the adjustment algorithm, and the algorithm expression is:
[0020] , where is the adjusted deposition rate, is the initial deposition rate, is the rate correction factor, is the coefficient threshold, and the control system controls the processing equipment to manufacture the preform rod at the adjusted deposition rate.
[0021] In a preferred embodiment, predicting whether the flow rate of chemical reagents during deposition will fluctuate during operation of the processing equipment comprises the following steps:
[0022] During the operation of the processing equipment, the speed deviation of the delivery pump blades and the inlet and outlet pressure deviation of the delivery pipe are obtained during the chemical reagent delivery. The speed deviation of the delivery pump blades and the inlet and outlet pressure deviation of the delivery pipe are normalized so that the value ranges of the speed deviation of the delivery pump blades and the inlet and outlet pressure deviation of the delivery pipe are mapped to [0,1], and the normalized value of the speed deviation and the normalized value of the pressure deviation are obtained. The normalized value of the speed deviation is added to the normalized value of the pressure deviation to obtain the flow fluctuation assignment, and whether the chemical reagent flow will fluctuate is predicted based on the comparison result of the flow fluctuation assignment with the first fluctuation threshold.
[0023] In a preferred embodiment, when the chemical reagent flow rate is predicted to fluctuate, the flow rate fluctuation assignment is output, comprising the following steps:
[0024] If the flow fluctuation assignment is less than or equal to the first fluctuation threshold, it is predicted that the chemical reagent flow will not fluctuate. If the flow fluctuation assignment is greater than the first fluctuation threshold, it is predicted that the chemical reagent flow will fluctuate. When it is predicted that the chemical reagent flow will fluctuate, the flow fluctuation assignment is output.
[0025] In a preferred embodiment, accumulating the changes at discrete time points to obtain the cumulative change of purity over a period of time comprises the following steps:
[0026] Collect the time series data of raw materials. The time series data includes the purity of raw materials at each time point. The purity of raw materials at each time point is obtained by online mass spectrometer. Calculate the change of raw material purity at each time point. The expression is: , where For the The change in purity at each time point, For the Purity at each time point, For the purity at each time point, and , assuming the purity index is , the time series is , the corresponding purity is , the changes are accumulated at discrete time points to obtain the cumulative change of purity over a period of time, and the expression is:
[0027] , where For the The change in purity at each time point, Indicates A point in time, Indicates a point in time.
[0028] In a preferred embodiment, the temperature condition in the deposition environment is monitored by a temperature sensor, and a temperature change index is generated according to the temperature condition, including the following steps:
[0029] The temperature of the deposition environment is obtained multiple times during the monitoring period by the temperature sensor, and a temperature set is established by combining the temperatures obtained multiple times. The temperature change index of the temperature set is calculated. The function expression is:
[0030] , where is the temperature change index, For the The temperature obtained at each monitoring time point, is the average temperature, is the number of monitoring time points.
[0031] In a preferred embodiment, the logic for obtaining the speed deviation of the pump blades of the delivery pump is as follows: the speed of the pump blades of the delivery pump is collected in real time by a Hall effect sensor installed at the pump blade shaft of the delivery pump, the speed difference is obtained by subtracting the speed of the pump blades of the delivery pump at the previous moment from the speed of the pump blades of the delivery pump at the current moment, and the absolute value of the speed difference is taken as the speed deviation of the pump blades of the delivery pump;
[0032] The logic for obtaining the inlet and outlet pressure deviation of the delivery pipe is as follows: the inlet pressure is collected in real time by the pressure sensor at the inlet of the delivery pipe, the outlet pressure is collected in real time by the pressure sensor at the outlet of the delivery pipe, the pressure difference is obtained by subtracting the outlet pressure from the inlet pressure, and the absolute value of the pressure difference is taken as the inlet and outlet pressure deviation of the delivery pipe.
[0033] A hollow-core anti-resonant optical fiber processing equipment control system, including an initialization module, a reagent flow analysis module, a purity analysis module, a temperature analysis module, a coefficient calculation module, and a dynamic adjustment module;
[0034] Initialization module: before the processing equipment manufactures the preform based on the chemical vapor deposition technology, the initial deposition rate of the processing equipment is generated according to the database;
[0035] Reagent flow analysis module: During the operation of the processing equipment, the pump blade speed deviation of the delivery pump and the inlet and outlet pressure deviation of the delivery pipe are obtained during the chemical reagent delivery. After pre-processing the pump blade speed deviation and the inlet and outlet pressure deviation of the delivery pipe, it is predicted whether the chemical reagent flow will fluctuate during the deposition process. When the chemical reagent flow is predicted to fluctuate, the flow fluctuation value is output;
[0036] Purity analysis module: collects time series data of raw materials, including the purity of raw materials at each time point, calculates the change in purity of raw materials at each time point, and accumulates the change at discrete time points to obtain the cumulative change in purity over a period of time;
[0037] Temperature analysis module: monitors the temperature conditions in the deposition environment through temperature sensors and generates a temperature change index based on the temperature conditions;
[0038] Coefficient calculation module: based on the flow fluctuation assignment, cumulative change, and temperature change index, analyze whether each monitoring target is qualified. If not qualified, control the processing equipment to stop running and send a warning signal. If qualified, substitute the flow fluctuation assignment, cumulative change, and temperature change index into the linear regression analysis model to calculate the output rate correction coefficient, and judge whether the deposition rate needs to be dynamically adjusted based on the comparison result between the rate correction coefficient and the coefficient threshold;
[0039] Dynamic adjustment module: If the deposition rate needs to be adjusted, the adjusted deposition rate is updated based on the adjustment algorithm, and the processing equipment is controlled to manufacture preforms at the adjusted deposition rate.
[0040] In the above technical solution, the technical effects and advantages provided by the present invention are:
[0041] The present invention predicts whether the flow of chemical reagents will fluctuate during the deposition process by pre-processing the pump blade speed deviation of the delivery pump and the inlet and outlet pressure deviation of the delivery pipe. When the chemical reagent flow is predicted to fluctuate, the flow fluctuation assignment is output, and the change amount is accumulated at discrete time points to obtain the cumulative change amount of purity within a period of time. The temperature change index is generated according to the temperature condition, and the flow fluctuation assignment, the cumulative change amount, and the temperature change index are substituted into the linear regression analysis model to calculate the output rate correction coefficient, and it is determined whether the deposition rate needs to be dynamically adjusted according to the comparison result of the rate correction coefficient and the coefficient threshold value, and the adjusted deposition rate is updated based on the adjustment algorithm. The control system controls the processing equipment to manufacture the preform at the adjusted deposition rate. The control system can dynamically adjust the deposition rate according to the uncertain factors that appear during the processing during the preform manufacturing process, thereby ensuring the quality of the preform and improving the transmission efficiency of the hollow core anti-resonance optical fiber. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For ordinary technicians in this field, other drawings can also be obtained based on these drawings.
[0043] Figure 1 The figure is a flow chart of the method of the present invention. DETAILED DESCRIPTION
[0044] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0045] Example 1: Please refer to Figure 1 As shown, the hollow-core anti-resonant optical fiber processing equipment control method described in this embodiment includes the following steps:
[0046] Before the processing equipment manufactures preform rods based on chemical vapor deposition technology, the control system generates an initial deposition rate of the processing equipment according to the database. During the operation of the processing equipment, the pump blade speed deviation of the delivery pump and the inlet and outlet pressure deviation of the delivery pipe are obtained during the chemical reagent delivery. After pre-processing the pump blade speed deviation of the delivery pump and the inlet and outlet pressure deviation of the delivery pipe, it is predicted whether the chemical reagent flow rate will fluctuate during the deposition process. When the chemical reagent flow rate is predicted to fluctuate, the flow fluctuation value is output, and the time series data of the raw materials are collected. The time series data includes the purity of the raw materials at each time point, and the change in the purity of the raw materials at each time point is calculated. The change is accumulated at discrete time points to obtain the cumulative change in purity over a period of time. The temperature condition in the deposition environment is monitored by a temperature sensor, and a temperature change index is generated according to the temperature condition. Whether each monitoring target is qualified is analyzed based on the flow fluctuation assignment, cumulative change, and temperature change index. If unqualified, the control system controls the processing equipment to stop running and sends a warning signal. If qualified, the flow fluctuation assignment, cumulative change, and temperature change index are substituted into the linear regression analysis model to calculate the output rate correction coefficient, and whether the deposition rate needs to be dynamically adjusted is determined based on the comparison result between the rate correction coefficient and the coefficient threshold. If the deposition rate needs to be adjusted, the adjusted deposition rate is updated based on the adjustment algorithm, and the control system controls the processing equipment to manufacture preforms at the adjusted deposition rate.
[0047] The present application predicts whether the flow of chemical reagents will fluctuate during the deposition process by pre-processing the deviation of the speed of the pump blades and the deviation of the inlet and outlet pressures of the delivery pipe. When the chemical reagent flow is predicted to fluctuate, the flow fluctuation assignment is output, and the change amount is accumulated at discrete time points to obtain the cumulative change amount of purity over a period of time. The temperature change index is generated according to the temperature condition, and the flow fluctuation assignment, the cumulative change amount, and the temperature change index are substituted into the linear regression analysis model to calculate the output rate correction coefficient, and the deposition rate needs to be dynamically adjusted according to the comparison result between the rate correction coefficient and the coefficient threshold. The deposition rate after adjustment is updated based on the adjustment algorithm, and the control system controls the processing equipment to manufacture the preform at the adjusted deposition rate. The control system can dynamically adjust the deposition rate according to the uncertain factors that occur during the processing during the preform manufacturing process, thereby ensuring the quality of the preform and improving the transmission efficiency of the hollow core anti-resonant optical fiber.
[0048] Embodiment 2: Before the processing equipment manufactures the preform based on the chemical vapor deposition technology, the control system generates the initial deposition rate of the processing equipment according to the database, including the following steps:
[0049] Collect historical production data, including information on different materials, deposition conditions, deposition rate, purity, etc., classify the data by material type, process conditions, equipment model, etc., set the initial conditions of the current production task, including material type, target purity, equipment model, etc., query the database according to the initial conditions, find historical production data under similar conditions, match the queried historical data, filter out historical records of deposition effects, extract relevant deposition parameters from the matched historical data, including deposition rate, temperature, pressure, airflow rate, etc., obtain the initial deposition rate based on the extracted historical data and the specific requirements of the current production task.
[0050] During the operation of the processing equipment, the pump blade speed deviation of the delivery pump and the inlet and outlet pressure deviation of the delivery pipe are obtained during the chemical reagent delivery. After pre-processing the pump blade speed deviation of the delivery pump and the inlet and outlet pressure deviation of the delivery pipe, it is predicted whether the chemical reagent flow rate will fluctuate during the deposition process. When the chemical reagent flow rate is predicted to fluctuate, the flow fluctuation value is output, including the following steps:
[0051] During the operation of the processing equipment, the pump blade speed deviation of the delivery pump and the inlet and outlet pressure deviation of the delivery pipe during chemical reagent delivery are obtained, and the pump blade speed deviation of the delivery pump and the inlet and outlet pressure deviation of the delivery pipe are normalized so that the value ranges of the pump blade speed deviation of the delivery pump and the inlet and outlet pressure deviation of the delivery pipe are mapped to [0,1], and the speed deviation normalized value and the pressure deviation normalized value are obtained. The speed deviation normalized value is added to the pressure deviation normalized value to obtain the flow fluctuation assignment, and whether the chemical reagent flow will fluctuate is predicted based on the comparison result of the flow fluctuation assignment value and the first fluctuation threshold value;
[0052] If the flow fluctuation assignment is less than or equal to the first fluctuation threshold, it is predicted that the chemical reagent flow will not fluctuate. If the flow fluctuation assignment is greater than the first fluctuation threshold, it is predicted that the chemical reagent flow will fluctuate. When it is predicted that the chemical reagent flow will fluctuate, the flow fluctuation assignment is output.
[0053] The logic for obtaining the pump blade speed deviation of the delivery pump is as follows: the pump blade speed of the delivery pump is collected in real time through the Hall effect sensor installed at the pump blade shaft of the delivery pump, the speed difference is obtained by subtracting the pump blade speed of the delivery pump at the previous moment from the current moment, and the absolute value of the speed difference is taken as the pump blade speed deviation of the delivery pump. The larger the pump blade speed deviation of the delivery pump, the greater the difference in the pump blade speed of the delivery pump at two moments, and the more likely the chemical reagent flow rate is to fluctuate;
[0054] The logic for obtaining the inlet and outlet pressure deviation of the delivery pipe is as follows: the inlet pressure is collected in real time through the pressure sensor at the inlet of the delivery pipe, and the outlet pressure is collected in real time through the pressure sensor at the outlet of the delivery pipe. The pressure difference is obtained by subtracting the outlet pressure from the inlet pressure, and the absolute value of the pressure difference is taken as the inlet and outlet pressure deviation of the delivery pipe. The larger the inlet and outlet pressure deviation of the delivery pipe, the greater the difference between the inlet and outlet pressures of the chemical reagent delivery pipe, and there may be leakage or blockage, which may cause fluctuations in the flow of chemical reagents.
[0055] Collecting time series data of raw materials, including the purity of raw materials at each time point, calculating the change in purity of raw materials at each time point, and accumulating the change at discrete time points to obtain the cumulative change in purity over a period of time, including the following steps:
[0056] Collect the time series data of raw materials. The time series data includes the purity of raw materials at each time point. The purity of raw materials at each time point is obtained by online mass spectrometer. Calculate the change of raw material purity at each time point. The expression is: , where For the The change in purity at each time point, For the Purity at each time point, For the purity at each time point, and , assuming the purity index is , the time series is , the corresponding purity is , the changes are accumulated at discrete time points to obtain the cumulative change of purity over a period of time, and the expression is:
[0057] , where For the The change in purity at each time point, Indicates A point in time, Indicates At each time point, the larger the cumulative change, the faster the purity of the raw materials decreases per unit time.
[0058] The purity of the raw materials at each time point is obtained by an online mass spectrometer. The steps for obtaining the purity of the raw materials by an online mass spectrometer are:
[0059] During the preform manufacturing process, an online mass spectrometer is connected to a material delivery pipeline or a reaction chamber, and a small amount of raw material samples are collected in real time and introduced into the mass spectrometer for analysis. The mass spectrometer ionizes, separates and detects the samples to obtain a mass spectrum of the raw materials. The mass spectrometer analyzes the mass spectrum to determine the molecular composition and purity of the raw materials. This step belongs to the prior art and will not be described in detail in this application.
[0060] The temperature condition in the deposition environment is monitored by a temperature sensor, and a temperature change index is generated according to the temperature condition, including the following steps:
[0061] The temperature of the deposition environment is obtained multiple times during the monitoring period by the temperature sensor, and a temperature set is established by combining the temperatures obtained multiple times. The temperature change index of the temperature set is calculated. The function expression is:
[0062] , where is the temperature change index, For the The temperature obtained at each monitoring time point, is the average temperature, is the number of monitoring time points. The larger the temperature change index is, the greater the temperature change amplitude of the sedimentary environment is during the monitoring period.
[0063] Based on the flow fluctuation assignment, cumulative change, and temperature change index, each monitoring target is analyzed to see if it is qualified. If it is unqualified, the control system controls the processing equipment to stop running and sends a warning signal, including the following steps:
[0064] The obtained flow fluctuation value is compared with the second fluctuation threshold, and the second fluctuation threshold is greater than the first fluctuation threshold. If the flow fluctuation value is greater than the second fluctuation threshold, it is judged that the chemical reagent flow monitoring is unqualified, and the control system controls the processing equipment to stop running and sends a warning signal;
[0065] The obtained cumulative change is compared with the change threshold. If the cumulative change is greater than the change threshold, it is judged that the purity of the raw material does not meet the standard, and the control system controls the processing equipment to stop running and sends a warning signal;
[0066] The obtained temperature change index is compared with the index threshold. If the temperature change index is greater than the index threshold, it is judged that the temperature fluctuation is too large, and the control system controls the processing equipment to stop running and sends a warning signal;
[0067] If the flow fluctuation value is less than or equal to the second fluctuation threshold, the cumulative change is less than or equal to the change threshold, and the temperature change index is less than or equal to the index threshold, it is confirmed that each monitoring target is qualified.
[0068] If qualified, the flow fluctuation assignment, cumulative change, and temperature change index are substituted into the linear regression analysis model to calculate the output rate correction coefficient, and the comparison result between the rate correction coefficient and the coefficient threshold is used to determine whether the deposition rate needs to be dynamically adjusted, including the following steps:
[0069] Substitute the flow fluctuation assignment, cumulative change, and temperature change index into the linear regression analysis model to calculate the output rate correction coefficient. The function expression is:
[0070] , where is the rate correction factor, Assign a value to the flow fluctuation, is the cumulative change, is the temperature change index, , , are the proportional coefficients of flow fluctuation, cumulative change, and temperature change index, respectively, and , , All are greater than 0;
[0071] The larger the flow fluctuation value is, the greater the flow fluctuation of the chemical reagent is during the preform manufacturing process, and the more the deposition rate needs to be reduced, specifically:
[0072] In the chemical vapor deposition (CVD) process, the concentration and flow rate of reactants directly affect the uniformity and stability of the reaction. Large flow fluctuations will lead to changes in reaction conditions, thereby affecting the reaction rate and the properties of the products. If the flow fluctuation is large, the reaction conditions (such as reaction temperature, gas phase concentration, etc.) during the deposition process will be unstable, resulting in large fluctuations in the quality of the preform. Reducing the deposition rate can extend the residence time of chemical reagents in the reaction area, so that even if there is a flow fluctuation, the reactants still have enough time to participate in the reaction, reducing the risk of uneven deposition. By reducing the deposition rate, the stability and consistency of the reaction can be improved, and the impact of flow fluctuations on product quality can be reduced;
[0073] The flow fluctuation of chemical reagents will lead to uneven deposition rate, thus affecting the uniformity of preforms. Especially for preforms with high purity requirements, any small flow fluctuation may lead to uneven deposition layer thickness or uneven component distribution. The uneven deposition layer will lead to defects in the subsequent processing of preforms, such as unstable structure and inconsistent optical properties. Reducing the deposition rate can make the deposition process slower and more uniform. The influence of the flow fluctuation of chemical reagents on the deposition rate is averaged, thereby improving the uniformity of the deposition layer. By reducing the deposition rate, a more uniform deposition layer can be obtained, the generation of defects can be reduced, and the quality of preforms can be improved.
[0074] Fluctuations in the flow rate of chemical reagents may introduce bubbles, particles or other impurities into the deposition layer, resulting in defects inside the preform. These defects will seriously affect the mechanical and optical properties of the preform. Impurities and defects caused by flow fluctuations will reduce the quality and performance of the preform and increase the difficulty and cost of subsequent processing. Reducing the deposition rate can give particles and impurities in the gas phase more time to be deposited and removed, while reducing the probability of bubbles and particles being captured in the deposition layer. By reducing the deposition rate, the introduction of defects and impurities can be reduced, and the purity and quality of the preform can be improved.
[0075] In the case of large flow fluctuations, maintaining a high deposition rate will increase the difficulty of process control. The control system needs to be adjusted frequently, which is prone to overshoot or undershoot, resulting in instability in the deposition process. The increased difficulty of process control may lead to instability in the preform production process and fluctuations in product quality. Reducing the deposition rate can reduce the requirements for the control system's response speed and accuracy, allowing the control system to more smoothly adjust the flow of chemical reagents and reaction conditions. By reducing the deposition rate, the accuracy and stability of process control can be improved to ensure the smooth operation of the deposition process.
[0076] The greater the cumulative change, the more the purity of the raw materials decreases during the preform manufacturing process, that is, the more impurities there are in the raw materials, and the more the deposition rate needs to be reduced, specifically:
[0077] High impurity concentration will directly affect the structure and performance of the preform. At high deposition rate, impurities are quickly deposited in the preform, resulting in uneven impurity distribution and defects. Reducing the deposition rate can slow down the accumulation of impurities, allowing impurities to be more evenly distributed in the material, reducing local defects and stress concentration, improving the uniformity and purity of the material, and reducing quality problems caused by impurities.
[0078] In a slower deposition process, the system has more time to diffuse and remove impurities, and separate impurities through thermal diffusion or chemical reaction. The slower deposition rate allows more time for impurities to diffuse to the surface or gas phase, thereby being removed or reduced, improving the purity of the deposited layer and reducing the impact of impurities on the performance of the preform.
[0079] A high deposition rate will cause the material to condense quickly, and impurities cannot be discharged in time, forming defects such as bubbles and inclusions. These defects will reduce the mechanical strength and optical properties of the material. A lower deposition rate can make the material deposit evenly layer by layer, giving impurities more time to be discharged or reacted, thus forming a more uniform and dense deposition layer. The structure of the preform is denser, the internal defects are reduced, and the performance is more stable.
[0080] At high deposition rates, the control system needs to frequently adjust deposition parameters to cope with purity changes, which increases the complexity and error of process control. Slower deposition rates make process changes more gradual, giving the control system more time to adjust and react, thereby improving the accuracy and stability of process control, reducing process fluctuations, and improving product consistency and quality.
[0081] Materials with high impurity content are prone to thermal stress and cracks during rapid cooling, especially at high deposition rates, where thermal stress accumulates faster and the risk of cracks is higher. A lower deposition rate allows the material to be deposited and cooled layer by layer, reducing the accumulation and release of thermal stress and the risk of crack formation.
[0082] The larger the temperature change index is, the greater the temperature change of the deposition environment is during the preform manufacturing process, and the more the deposition rate needs to be reduced. Specifically:
[0083] Temperature changes can lead to uneven deposition rate and reaction rate, which in turn affects the uniformity of the deposited layer. Under high temperature changes, the solidification rate and surface energy of the material will change, leading to uneven deposition. Reducing the deposition rate can give the material more time to adjust and self-organize, thereby forming a more uniform deposition layer, improving the uniformity of the preform and reducing the inconsistency between layers caused by temperature changes.
[0084] Temperature changes can cause thermal stress. Especially at high deposition rates, rapid cooling or heating of the material can produce large thermal stress and strain, causing deformation or cracking of the preform. Reducing the deposition rate can gradually adapt the material to temperature changes, reduce the accumulation and release of thermal stress, reduce the risk of deformation and cracking, reduce deformation and cracking of the preform, and improve mechanical strength and durability.
[0085] Temperature changes can affect the rate and balance of chemical reactions, leading to unstable chemical reactions during deposition, affecting the quality and purity of the deposits. Reducing the deposition rate can extend the residence time of chemical reagents in the reaction area, so that the chemical reaction can maintain a high stability even under temperature changes, thereby improving the stability of the deposition process and ensuring the quality and purity of the deposits.
[0086] When the temperature changes greatly, the process control system needs to frequently adjust the deposition parameters to cope with the temperature change, which increases the complexity and error of the control. The slower deposition rate makes the impact of temperature change on the system more gradual, and the control system has more time to adjust and compensate, which improves the accuracy and stability of process control and reduces the quality fluctuation caused by temperature fluctuation.
[0087] Temperature changes will affect the diffusion and deposition of impurities. Especially at high temperatures, impurities are more likely to enter the deposition layer and form defects and impurities. A slower deposition rate can give impurities more time to be discharged or reacted, thereby reducing the formation of impurities and defects, improving the purity and quality of preforms, and reducing defects.
[0088] The larger the rate correction coefficient is, the more it is necessary to adjust the deposition rate. The obtained rate correction coefficient is compared with the preset coefficient threshold. If the rate correction coefficient is less than or equal to the coefficient threshold, it is determined that there is no need to dynamically adjust the deposition rate. If the rate correction coefficient is greater than the coefficient threshold, it is determined that the deposition rate needs to be dynamically adjusted.
[0089] If the deposition rate needs to be adjusted, the adjusted deposition rate is updated based on the adjustment algorithm, and the control system controls the processing equipment to manufacture the preform at the adjusted deposition rate, including the following steps:
[0090] The adjusted deposition rate is updated based on the adjustment algorithm, and the algorithm expression is:
[0091] , where is the adjusted deposition rate, is the initial deposition rate, is the rate correction factor, is the coefficient threshold, and the control system controls the processing equipment to manufacture the preform rod at the adjusted deposition rate.
[0092] Embodiment 3: The hollow-core anti-resonant optical fiber processing equipment control system described in this embodiment includes an initialization module, a reagent flow analysis module, a purity analysis module, a temperature analysis module, a coefficient calculation module, and a dynamic adjustment module;
[0093] Initialization module: Before the processing equipment manufactures the preform based on the chemical vapor deposition technology, the initial deposition rate of the processing equipment is generated according to the database, and the initial deposition rate is sent to the dynamic adjustment module;
[0094] Reagent flow analysis module: During the operation of the processing equipment, the pump blade speed deviation of the delivery pump and the inlet and outlet pressure deviation of the delivery pipe are obtained during the chemical reagent delivery. After pre-processing the pump blade speed deviation and the inlet and outlet pressure deviation of the delivery pipe, it is predicted whether the chemical reagent flow will fluctuate during the deposition process. When the chemical reagent flow is predicted to fluctuate, the flow fluctuation value is output and sent to the coefficient calculation module;
[0095] Purity analysis module: collects time series data of raw materials, including the purity of raw materials at each time point, calculates the change in purity of raw materials at each time point, and accumulates the change at discrete time points to obtain the cumulative change in purity over a period of time, and sends the cumulative change to the coefficient calculation module;
[0096] Temperature analysis module: monitors the temperature conditions in the deposition environment through a temperature sensor, generates a temperature change index based on the temperature conditions, and sends the temperature change index to the coefficient calculation module;
[0097] Coefficient calculation module: based on the flow fluctuation assignment, cumulative change, and temperature change index, analyze whether each monitoring target is qualified. If unqualified, control the processing equipment to stop running and send a warning signal. If qualified, substitute the flow fluctuation assignment, cumulative change, and temperature change index into the linear regression analysis model to calculate the output rate correction coefficient, and judge whether the deposition rate needs to be dynamically adjusted based on the comparison result between the rate correction coefficient and the coefficient threshold. The judgment result and the rate correction coefficient are sent to the dynamic adjustment module;
[0098] Dynamic adjustment module: If the deposition rate needs to be adjusted, the adjusted deposition rate is updated based on the adjustment algorithm, and the processing equipment is controlled to manufacture preforms at the adjusted deposition rate.
[0099] The above formulas are all dimensionless and numerical calculations. The formula is a formula for the most recent real situation obtained by collecting a large amount of data and performing software simulation. The preset parameters in the formula are set by technicians in this field according to actual conditions.
[0100] In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.
[0101] The preferred embodiments of the present invention disclosed above are only used to help explain the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to only specific implementation methods. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.
Claims
1. A method for controlling hollow core anti-resonant optical fiber processing equipment, characterized in that: The control method comprises the following steps: Before the processing equipment manufactures the preform based on the chemical vapor deposition technology, the control system generates the initial deposition rate of the processing equipment according to the database, and predicts whether the flow of chemical reagents will fluctuate during the deposition process during the operation of the processing equipment, and outputs the flow fluctuation value when the chemical reagent flow is predicted to fluctuate; Calculate the change in the purity of the raw materials at each time point, and accumulate the change at discrete time points to obtain the cumulative change in purity over a period of time. Use a temperature sensor to monitor the temperature conditions in the deposition environment, generate a temperature change index based on the temperature conditions, and analyze whether each monitoring target is qualified based on flow fluctuation assignment, cumulative change, and temperature change index. If unqualified, the control system controls the processing equipment to stop running and sends a warning signal; If qualified, the flow fluctuation assignment, cumulative change, and temperature change index are substituted into the linear regression analysis model to calculate the output rate correction coefficient, and based on the comparison result between the rate correction coefficient and the coefficient threshold, it is determined whether the deposition rate needs to be dynamically adjusted. If the deposition rate needs to be adjusted, the adjusted deposition rate is updated based on the adjustment algorithm, and the control system controls the processing equipment to manufacture preform rods at the adjusted deposition rate.
2. The hollow core anti-resonant optical fiber processing equipment control method according to claim 1, characterized in that: Based on the flow fluctuation assignment, cumulative change, and temperature change index, the following steps are included to analyze whether each monitoring target is qualified: The obtained flow fluctuation value is compared with the second fluctuation threshold, and the second fluctuation threshold is greater than the first fluctuation threshold. If the flow fluctuation value is greater than the second fluctuation threshold, it is judged that the chemical reagent flow monitoring is unqualified, and the control system controls the processing equipment to stop running and sends a warning signal; The obtained cumulative change is compared with the change threshold. If the cumulative change is greater than the change threshold, it is judged that the purity of the raw material does not meet the standard, and the control system controls the processing equipment to stop running and sends a warning signal; The obtained temperature change index is compared with the index threshold. If the temperature change index is greater than the index threshold, it is judged that the temperature fluctuation is too large, and the control system controls the processing equipment to stop running and sends a warning signal; If the flow fluctuation value is less than or equal to the second fluctuation threshold, the cumulative change is less than or equal to the change threshold, and the temperature change index is less than or equal to the index threshold, it is confirmed that each monitoring target is qualified.
3. The hollow-core anti-resonant optical fiber processing equipment control method according to claim 2, characterized in that: Substituting the flow fluctuation assignment, cumulative change, and temperature change index into the linear regression analysis model to calculate the output rate correction coefficient, and judging whether the deposition rate needs to be dynamically adjusted based on the comparison result between the rate correction coefficient and the coefficient threshold, including the following steps: Substitute the flow fluctuation assignment, cumulative change, and temperature change index into the linear regression analysis model to calculate the output rate correction coefficient. The function expression is: , where is the rate correction factor, Assign a value to the flow fluctuation, is the cumulative change, is the temperature change index, , , are the proportional coefficients of flow fluctuation, cumulative change, and temperature change index, respectively, and , , All are greater than 0; The obtained rate correction coefficient is compared with the preset coefficient threshold. If the rate correction coefficient is less than or equal to the coefficient threshold, it is determined that there is no need to dynamically adjust the deposition rate. If the rate correction coefficient is greater than the coefficient threshold, it is determined that there is a need to dynamically adjust the deposition rate.
4. The hollow-core anti-resonant optical fiber processing equipment control method according to claim 3, characterized in that: If the deposition rate needs to be adjusted, the adjusted deposition rate is updated based on the adjustment algorithm, including the following steps: The adjusted deposition rate is updated based on the adjustment algorithm, and the algorithm expression is: , where is the adjusted deposition rate, is the initial deposition rate, is the rate correction factor, is the coefficient threshold, and the control system controls the processing equipment to manufacture the preform rod at the adjusted deposition rate.
5. The hollow-core anti-resonant optical fiber processing equipment control method according to claim 4, characterized in that: Predicting whether chemical flow rates will fluctuate during deposition while the process equipment is running includes the following steps: During the operation of the processing equipment, the speed deviation of the delivery pump blades and the inlet and outlet pressure deviation of the delivery pipe are obtained during the chemical reagent delivery. The speed deviation of the delivery pump blades and the inlet and outlet pressure deviation of the delivery pipe are normalized so that the value ranges of the speed deviation of the delivery pump blades and the inlet and outlet pressure deviation of the delivery pipe are mapped to [0,1], and the normalized value of the speed deviation and the normalized value of the pressure deviation are obtained. The normalized value of the speed deviation is added to the normalized value of the pressure deviation to obtain the flow fluctuation assignment, and whether the chemical reagent flow will fluctuate is predicted based on the comparison result of the flow fluctuation assignment with the first fluctuation threshold.
6. The hollow-core anti-resonant optical fiber processing equipment control method according to claim 5, characterized in that: When the chemical reagent flow rate is predicted to fluctuate, the flow rate fluctuation assignment is output, including the following steps: If the flow fluctuation assignment is less than or equal to the first fluctuation threshold, it is predicted that the chemical reagent flow will not fluctuate. If the flow fluctuation assignment is greater than the first fluctuation threshold, it is predicted that the chemical reagent flow will fluctuate. When it is predicted that the chemical reagent flow will fluctuate, the flow fluctuation assignment is output.
7. The hollow-core anti-resonant optical fiber processing equipment control method according to claim 6, characterized in that: Accumulating the changes at discrete time points to obtain the cumulative change of purity over a period of time includes the following steps: Collect the time series data of raw materials. The time series data includes the purity of raw materials at each time point. The purity of raw materials at each time point is obtained by online mass spectrometer. Calculate the change in the purity of raw materials at each time point. The expression is: , where For the The change in purity at each time point, For the Purity at each time point, For the purity at each time point, and , assuming the purity index is , the time series is , the corresponding purity is , the changes are accumulated at discrete time points to obtain the cumulative change of purity over a period of time, and the expression is: , where For the The change in purity at each time point, Indicates A point in time, Indicates a point in time.
8. The hollow-core anti-resonant optical fiber processing equipment control method according to claim 7, characterized in that: The temperature condition in the deposition environment is monitored by a temperature sensor, and a temperature change index is generated according to the temperature condition, including the following steps: The temperature of the deposition environment is obtained multiple times during the monitoring period by the temperature sensor, and a temperature set is established by combining the temperatures obtained multiple times. The temperature change index of the temperature set is calculated. The function expression is: , where is the temperature change index, For the The temperature obtained at each monitoring time point, is the average temperature, is the number of monitoring time points.
9. The hollow-core anti-resonant optical fiber processing equipment control method according to claim 5, characterized in that: The logic for obtaining the pump blade speed deviation of the delivery pump is as follows: the pump blade speed of the delivery pump is collected in real time by a Hall effect sensor installed at the pump blade shaft of the delivery pump, the speed difference is obtained by subtracting the pump blade speed of the delivery pump at the previous moment from the current moment, and the absolute value of the speed difference is taken as the pump blade speed deviation of the delivery pump; The logic for obtaining the inlet and outlet pressure deviation of the delivery pipe is as follows: the inlet pressure is collected in real time by the pressure sensor at the inlet of the delivery pipe, the outlet pressure is collected in real time by the pressure sensor at the outlet of the delivery pipe, the pressure difference is obtained by subtracting the outlet pressure from the inlet pressure, and the absolute value of the pressure difference is taken as the inlet and outlet pressure deviation of the delivery pipe.
10. A hollow core anti-resonant optical fiber processing equipment control system, used to implement the control method according to any one of claims 1 to 9, characterized in that: It includes an initialization module, a reagent flow analysis module, a purity analysis module, a temperature analysis module, a coefficient calculation module, and a dynamic adjustment module; Initialization module: before the processing equipment manufactures the preform based on the chemical vapor deposition technology, the initial deposition rate of the processing equipment is generated according to the database; Reagent flow analysis module: During the operation of the processing equipment, the pump blade speed deviation of the delivery pump and the inlet and outlet pressure deviation of the delivery pipe are obtained during the chemical reagent delivery. After pre-processing the pump blade speed deviation and the inlet and outlet pressure deviation of the delivery pipe, it is predicted whether the chemical reagent flow will fluctuate during the deposition process. When the chemical reagent flow is predicted to fluctuate, the flow fluctuation value is output; Purity analysis module: collects time series data of raw materials, including the purity of raw materials at each time point, calculates the change in purity of raw materials at each time point, and accumulates the change at discrete time points to obtain the cumulative change in purity over a period of time; Temperature analysis module: monitors the temperature conditions in the deposition environment through temperature sensors and generates a temperature change index based on the temperature conditions; Coefficient calculation module: based on the flow fluctuation assignment, cumulative change, and temperature change index, analyze whether each monitoring target is qualified. If not qualified, control the processing equipment to stop running and send a warning signal. If qualified, substitute the flow fluctuation assignment, cumulative change, and temperature change index into the linear regression analysis model to calculate the output rate correction coefficient, and judge whether the deposition rate needs to be dynamically adjusted based on the comparison result between the rate correction coefficient and the coefficient threshold; Dynamic adjustment module: If the deposition rate needs to be adjusted, the adjusted deposition rate is updated based on the adjustment algorithm, and the processing equipment is controlled to manufacture preforms at the adjusted deposition rate.
Citation Information
Patent Citations
System and method for intelligently managing and controlling geometrical parameters of loose body of optical fiber preform
CN111925113A
Control method for improving parameter uniformity of optical fiber preform
CN112408776A
Methods for producing a hollow-core fiber and for producing a preform for a hollow-core fiber
CN113939483A
Optical fiber preform rod deposition workshop process test rod putting scheduling method and system
CN116203911A
Drawing simulation method for multi-layer tube type anti-resonance hollow-core optical fiber