Processing method of copper spherical friction pair of plunger pump
By pre-machining protrusions into the steel matrix to reduce the amount of copper alloy used, the problem of copper alloy waste in the machining of plunger pump cylinder blocks is solved, achieving efficient utilization of copper alloys and reducing production costs.
Patent Information
- Application Number
- CN202411063158.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2044-08-05
AI Technical Summary
The current piston pump cylinder block machining process results in significant waste of copper alloy, which is difficult to recycle and reuse, leading to increased production costs.
Pre-machine protrusions into the steel substrate to reduce the volume of the molten copper pool. Drill through holes to reduce the amount of copper alloy used. Use interference fit and welding to improve the connection stability and avoid copper alloy waste.
It effectively reduces the amount of copper alloy used, lowers production costs, simplifies processing procedures, improves copper alloy recycling efficiency, and reduces waste generation.
Smart Images

Figure CN118559370B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of metal casting, in particular to a method for processing a copper spherical friction pair of a plunger pump. Background Art
[0002] The plunger pump is an important working part in hydraulic and pneumatic transmission, and is a type of positive displacement pump and reciprocating pump. The cylinder body is the key friction pair part of the plunger pump and is also the core of the plunger pump. The performance and quality of the cylinder body directly affect the transmission efficiency and service life of the plunger pump. Figure 6 As shown in the figure, the most widely used material for plunger pump cylinders is copper-steel bimetallic composite materials. Copper as the working layer of the friction pair has good characteristics such as anti-friction, wear resistance and fatigue resistance. At the same time, the soft and hard phase structures determine that it has good anti-seizure, embedding and compliance. Steel as the base material of the plunger pump cylinder plays a role in bearing and impact resistance. The copper-steel bimetallic composite material formed by the combination of the two has the excellent properties of both materials.
[0003] The existing cylinder manufacturing method mainly adopts the melting casting method. By utilizing the characteristic that the melting point of copper is lower than that of steel, a molten copper pool is firstly processed on the steel substrate, and then a copper alloy is placed in the molten copper pool of the steel substrate. Then, the workpiece is placed in a multi-temperature zone sintering furnace as a whole. After three stages of preheating, heating and cooling, the copper alloy is melted in the molten copper pool. After cooling, a composite bimetallic plunger pump cylinder blank is obtained. Finally, a through hole is cut from the center of the cylinder along the axis of the cylinder to install the main shaft; the molten copper pool is cut off, and finally, the copper alloy layer is processed into a spherical friction pair working surface that is concave downward; during the drilling process, the center of the copper cast spherical friction pair blank needs to be completely removed, and the copper alloy chips and steel chips formed by drilling are mixed and difficult to separate and recycle, and are finally sold as steel chip waste, resulting in a waste of copper alloy. Summary of the invention
[0004] In view of the shortcomings of the prior art, the technical problem solved by the present invention is to provide a method for processing a copper spherical friction pair of a plunger pump, thereby solving the problem of waste of copper alloy caused by the existing processing process of the friction pair of the plunger pump.
[0005] In order to solve the above problems, the technical solution adopted by the present invention is: a processing method for a copper spherical friction pair of a plunger pump, comprising the following steps; S100: cutting raw materials into a steel matrix with a steel rod, and mechanically processing a molten copper pool at one end of the steel matrix, and a convex column is provided in the middle of the molten copper pool; S200: cleaning the surface of the steel matrix and then coating it with a metal activator; S300: calculating the required volume of the copper alloy, and placing the copper alloy that meets the required volume in the molten copper pool of the steel matrix; S400: sending the steel matrix and the copper alloy into a melting furnace, and obtaining a copper-steel bimetallic composite cylinder body after preheating, staged heating and cooling, and the heating temperature is greater than or equal to the melting point of the copper alloy and less than the melting point of the steel matrix; S500: then turning off the copper molten pool, and processing the copper alloy layer into a spherical surface to complete the friction pair processing.
[0006] The beneficial effects of this scheme are as follows: the existing bimetallic casting of cylinder bodies all use copper alloys in the molten copper pool, and after three stages of preheating, heating and cooling, a composite bimetallic plunger pump cylinder body blank is obtained; then a through hole is drilled in the center of the cylinder body blank. This method reserves a convex column in the casting pool, and then the copper alloy is cast. Since the convex column will be machined into a through hole after the cylinder body blank is formed, it is used to install the main shaft; by setting the convex column in the steel matrix, the convex column is used to reduce the volume of the molten copper pool, thereby reducing the amount of copper. Since the part where copper is reduced is the drilling part, the copper alloy area required for the friction pair will not be reduced; thereby solving the problem that it is difficult to separate and recycle copper alloy in the mixed waste after drilling and cutting, resulting in copper and steel scraps mixed together, and finally only steel scraps can be sold as waste, further causing the value of copper alloy to depreciate; there is no need to use other methods to recycle copper alloy, thereby effectively reducing production costs. The amount of copper alloy is reduced before casting, the copper reduction process is simple, the technical transformation difficulty is low, and it is easy to promote and use.
[0007] Furthermore, the step S100 also includes drilling the steel substrate to simultaneously process through holes and plunger holes, and a convex ring is reserved at the edge of the through hole to form a molten copper pool.
[0008] The through hole is formed by drilling first, thereby reducing the thickness of the boss, and the elastic deformation of the convex ring relative to the boss is larger. At the same time, the method of drilling first can reduce the stress concentration inside the steel matrix, so that it is not easy to form cracks between the copper alloy and the steel matrix after the copper alloy is melt-cast and cooled. Secondly, by drilling first, when the through hole is subsequently fine-machined, it is not necessary to drill again, and the through hole is only machined to the required size by turning; thus, there is no need to transfer the cylinder body from the drilling machine to the lathe, and repeat the clamping twice, which reduces the subsequent fine-machining steps.
[0009] Furthermore, the step S100 also includes drilling holes in the steel substrate, and processing through holes and plunger holes simultaneously, with a finishing allowance reserved for the through holes, and interference fit between the boss and the through holes. The boss is removed first during the subsequent turning by adopting the interference fit between the boss and the through hole, and the boss can be reused many times; the thermal conductivity of the copper alloy is greater than that of the steel body, so that when cooling, the copper alloy cools down faster than the steel body, and because the boss is a solid body, the temperature difference between the column and the copper alloy is further increased, so that after the copper alloy is melted and cooled, due to the cooling and shrinkage of the copper alloy, cracks are easily formed at the connection between the copper alloy and the edge of the steel substrate, thereby facilitating the removal of the boss.
[0010] Furthermore, the height of the protrusion is not less than the thickness of the copper alloy after being melted in the molten copper pool, so that the liquid level of the molten copper alloy will not exceed the height of the protrusion, thereby preventing the copper alloy from being left on the surface of the protrusion and causing waste of the copper alloy after cutting.
[0011] Furthermore, the cylindrical shape is provided with a chamfer at the upper end. The chamfer forms a truncated cone shape, and the inclined surface of the truncated cone increases the surface area in contact with the copper alloy, which helps to improve the mechanical anchoring effect at the weld, so that the copper alloy can fit with the steel matrix in a larger area. At the same time, the chamfered inclined surface cooperates with the vertical side surface, so that the two metals are not easy to fall off; the chamfer can reduce burrs during the machining process.
[0012] Furthermore, the protrusion is cylindrical, and the side of the protrusion is perpendicular to the bottom of the molten copper pool. With the cylindrical design, since the volume of the cylinder is larger than the volume of the protrusion with a truncated cone at the upper end, the volume of the molten copper pool is further reduced, thereby further reducing the amount of copper used.
[0013] Furthermore, the boss is integrally formed with the steel base, which is convenient for processing and reduces the number of processing steps, and the integrally formed connection is more stable.
[0014] Furthermore, the boss is sealed and welded to the steel substrate. The size of the boss is easily adjusted by welding, and there is no need to redesign the steel substrate cutting fixture. A circle of weld is formed between the boss and the molten copper pool of the steel substrate by sealing welding, leaving no gap, thereby preventing copper alloy from flowing into the gap and causing waste. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 is a cross-sectional view of the steel substrate of the present invention;
[0016] Figure 2 It is a schematic diagram after cutting;
[0017] Figure 3 This is a schematic diagram of the steel substrate of Example 2;
[0018] Figure 4 This is a schematic diagram of the steel substrate of Example 3;
[0019] Figure 5 This is a schematic diagram of the steel substrate of Example 4;
[0020] Figure 6 It is a schematic diagram of the existing plunger pump structure.
[0021] The reference numerals in the drawings of the specification include: steel substrate 1, molten copper pool 2, protruding column 3, copper alloy 4. DETAILED DESCRIPTION
[0022] The following is further described in detail through specific implementation methods:
[0023] Example 1 This is as attached Figure 1 , Figure 2 As shown: A method for processing a copper spherical friction pair of a plunger pump, comprising the following steps;
[0024] S100: Cutting raw materials into a steel matrix with a steel rod, and processing a molten copper pool 2 at one end of the steel matrix, wherein a convex column 3 is provided in the middle of the molten copper pool 2, and the convex column 3 is cylindrical; the height of the convex column 3 is greater than the thickness of the copper alloy 4 after being melted and cast in the molten copper pool 2;
[0025] S200: Clean the steel substrate surface and then apply metal activator;
[0026] S300: placing the copper alloy 4 in a molten copper pool 2 formed by melting and casting a steel matrix;
[0027] S400: sending the steel matrix and the copper alloy 4 into a melting and casting furnace, and obtaining a copper-steel bimetallic composite cylinder body after preheating, stage heating and cooling; the specific steps are as follows;
[0028] S401: Preheating: transport the steel matrix and copper alloy 4 to the preheating zone in the casting furnace, and preheat them with nitrogen with a purity of ≥99.999% as the protective gas, the preheating temperature is 800-950°C, and the holding time is 30-60min;
[0029] S402: Heating: The steel matrix and the copper alloy 4 are transported to the heating zone in the melting furnace, and three-stage heating is performed using nitrogen with a purity of ≥99.999% as the protective gas; the first stage heating temperature is 900-1050°C, and the holding time is 30-60min; the second stage heating temperature is 1050-1150°C, and the holding time is 30-60min; the third stage heating temperature is 1050-1120°C, and the holding time is 30-60min;
[0030] S403: variable speed cooling: after the heat preservation is completed, the steel matrix and the molten copper alloy 4 are transported to the cooling zone device for water spraying for cooling for 5-10 minutes, and then air-cooled to room temperature.
[0031] S500: After the plunger hole and through hole are drilled synchronously in the cylinder body, the plunger hole and through hole are repaired by turning until they meet the size requirements; then the copper molten pool is turned away, and the 4 layers of copper alloy are processed into a spherical surface to complete the friction pair processing.
[0032] The existing bimetallic casting of cylinder bodies all adopts copper alloy 4 in the molten copper pool 2, and undergoes three stages of preheating, heating and cooling to obtain a composite bimetallic plunger pump cylinder body blank; then a through hole is drilled in the center of the cylinder body blank; this method reserves a boss 3 in the casting pool, and then the copper alloy 4 is cast, because the boss 3 will be machined into a through hole after the cylinder body blank is formed, which is used to install the main shaft; by setting the boss 3 in the steel matrix, the boss 3 is used to reduce the volume of the molten copper pool 2, thereby reducing the amount of copper; because the part where copper is reduced is the drilling part, the area of copper alloy 4 required by the friction pair will not be reduced; thereby solving the problem that copper alloy 4 is difficult to recover on the material after turning, and there is no need to use other methods to recover copper alloy 4, thereby effectively reducing production costs. The amount of copper alloy 4 is reduced before casting, and the copper reduction process is simple, and only the steel matrix mold needs to be improved. The technical transformation is low in difficulty and is easy to promote and use.
[0033] The height of the cylinder is greater than the thickness of the copper alloy 4 after being melted in the molten copper pool 2, so that the liquid level of the melted copper alloy 4 will not exceed the height of the protrusion 3, thereby not leaving the copper alloy 4 on the surface of the protrusion 3, causing waste of the copper alloy 4 after cutting.
[0034] Embodiment 2, a method for processing a copper spherical friction pair of a plunger pump, comprising the following steps:
[0035] S100: Cutting raw materials into a steel matrix with a steel rod, and processing a molten copper pool 2 at one end of the steel matrix, a convex column 3 is provided in the middle of the molten copper pool 2, and the convex column 3 and the molten copper pool are integrally formed by mechanical processing; drilling the steel matrix, and simultaneously processing a through hole and a plunger hole, and reserving a convex ring at the edge of the through hole to form the molten copper pool 2, the bottom of the molten copper pool 2 is a spherical surface, and the height of the convex ring is greater than the thickness of the copper alloy 4 after being melted and cast in the molten copper pool 2;
[0036] S200: Clean the steel substrate surface and then apply metal activator;
[0037] S300: Calculate the required volume of the copper alloy 4, and place the copper alloy 4 that meets the required volume into the molten copper pool 2 of the steel matrix;
[0038] S400: sending the steel matrix and the copper alloy 4 into a melting furnace, and obtaining a copper-steel bimetallic composite cylinder body after preheating, staged heating and cooling; the specific steps are as in Example 1;
[0039] S500: The through hole is turned to form a through hole that meets the size requirements, and then the copper molten pool is turned to form a friction pair.
[0040] The through hole is formed by drilling first, thereby reducing the thickness of the boss 3, and the elastic deformation of the convex ring relative to the boss 3 is larger. At the same time, the method of drilling first can reduce the stress concentration inside the steel matrix, so that it is not easy to form cracks between the copper alloy 4 and the steel matrix after the copper alloy 4 is melt-cast and cooled. Secondly, by drilling first, when the through hole is subsequently finely processed, it is not necessary to drill again, and the through hole is only processed to the required size by turning; thus, there is no need to transfer the cylinder body from the drilling machine to the lathe, and repeat the clamping twice, which reduces the subsequent fine processing steps.
[0041] Embodiment 3, a method for processing a copper spherical friction pair of a plunger pump, comprising the following steps:
[0042] S100: Cutting raw materials into a steel matrix with a steel rod, and processing a molten copper pool 2 at one end of the steel matrix, drilling the steel matrix, and simultaneously processing through holes and plunger holes, and reserving a finishing allowance for the through holes; a boss 3 is provided in the middle of the molten copper pool 2, and the boss 3 is interference fit with the main shaft; the height of the boss 3 is greater than the thickness of the copper alloy 4 after being melted and cast in the molten copper pool 2.
[0043] S200: Clean the steel substrate surface and then apply metal activator;
[0044] S300: Calculate the required volume of the copper alloy 4, and place the copper alloy 4 that meets the required volume into the molten copper pool 2 of the steel matrix;
[0045] S400: sending the steel matrix and the copper alloy 4 into a melting furnace, and obtaining a copper-steel bimetallic composite cylinder body after preheating, staged heating and cooling; the specific steps are as in Example 1;
[0046] S500: Remove the boss 3 and trim the through hole by turning to form a through hole that meets the size requirements.
[0047] The boss 3 is interference-fitted with the through hole, and the boss 3 is removed first during the subsequent turning, and the boss 3 can be reused multiple times. The thermal conductivity of the copper alloy is greater than that of the steel body, so that when cooling, the copper alloy cools faster than the steel body, and because the boss 3 is a solid body, the temperature difference between the column and the copper alloy is further increased, so that after the copper alloy is melted and cooled, due to the cooling and shrinkage of the copper alloy, cracks are easily formed at the edge connection between the copper alloy and the steel substrate, which makes it easier to remove the boss 3.
[0048] Example 4 Figure 5 As shown, the same points as Example 1 are not repeated here, and the difference lies in that, a method for processing a copper spherical friction pair of a plunger pump, the step S100: cutting on the surface of a steel substrate to form an annular molten copper pool 2, the bottom of the molten copper pool 2 is a spherical surface, and a convex column 3 is reserved in the center of the molten copper pool 2, the convex column 3 is cylindrical and has a chamfer on the upper end.
[0049] The truncated cone is formed by chamfering, and the inclined surface of the cone increases the surface area in contact with the copper alloy 4, which helps to improve the mechanical anchoring effect at the weld, so that the copper alloy 4 can fit with the steel substrate in a larger area. At the same time, the inclined surface cooperates with the vertical side surface, making it difficult for the two metals to fall off, so that the copper alloy 4 and the steel substrate are firmly fused into one.
[0050] The similarities between Example 5 and Example 1 are not repeated here, and the difference lies in that, step S100: a disc-shaped molten copper pool 2 is cut on the surface of the steel substrate, the bottom of the molten copper pool 2 is a plane, and a cylindrical protrusion 3 is welded and sealed at the bottom of the disc; the height of the protrusion 3 is greater than the thickness of the copper alloy 4 after being melted in the molten copper pool 2. The welding method is convenient for adjusting the size of the protrusion 3, and there is no need to redesign the steel substrate cutting fixture. A circle of welds is formed between the protrusion 3 and the molten copper pool 2 of the steel substrate by sealing welding, leaving no gap, so as to avoid the copper alloy 4 flowing into the gap and causing waste.
[0051] The above is only an embodiment of the present invention, and the common knowledge such as the known specific structure and characteristics in the scheme is not described in detail here. It should be pointed out that for those skilled in the art, several deformations and improvements can be made without departing from the structure of the present invention, which should also be regarded as the protection scope of the present invention, and these will not affect the effect of the implementation of the present invention and the practicality of the patent. The scope of protection required by this application shall be based on the content of its claims, and the specific implementation methods and other records in the specification can be used to interpret the content of the claims.
Claims
1. A method for processing a copper spherical friction pair of a plunger pump. Features: The steps include: S100: Cutting raw materials into a steel matrix with a steel bar, and machining a molten copper pool at one end of the steel matrix, with a convex column in the middle of the molten copper pool; S200: Clean the steel substrate surface and then apply metal activator; S300: Calculating the required volume of copper alloy, and placing the copper alloy meeting the required volume into the molten copper pool of the steel matrix; S400: placing a steel matrix and a copper alloy into a melting furnace, and obtaining a copper-steel bimetallic composite cylinder body after preheating, stage heating, and cooling, wherein the heating temperature of the stage heating is greater than or equal to the melting point of the copper alloy and less than the melting point of the steel matrix; S500: The copper molten pool is then turned away, and the copper alloy layer is processed into a spherical surface to complete the friction pair processing.
2. The method for processing the copper spherical friction pair of the plunger pump according to claim 1, Features: The height of the protruding column is not less than the thickness of the copper alloy after being melted in the molten copper pool.
3. The method for processing the copper spherical friction pair of the plunger pump according to claim 1, Features: The step S100 also includes drilling the steel substrate to simultaneously form a through hole and a plunger hole, wherein the through hole shapes the protruding column into an annular flange.
4. The method for processing the copper spherical friction pair of the plunger pump according to claim 1, Features: The step S100 also includes drilling the steel substrate to simultaneously process the through hole and the plunger hole, with a finishing allowance reserved for the through hole and an interference fit between the boss and the through hole.
5. The method for processing the copper spherical friction pair of the plunger pump according to claim 1, Features: The protruding column is cylindrical and has a chamfered upper end.
6. The method for processing the copper spherical friction pair of the plunger pump according to claim 1, Features: The convex column is cylindrical and coaxial with the steel substrate.
7. The method for processing the copper spherical friction pair of the plunger pump according to claim 1, Features: The convex column is integrally formed with the steel base.
8. The method for processing the copper spherical friction pair of the plunger pump according to claim 1, Features: The convex column is sealed and welded to the steel substrate.
Citation Information
Patent Citations
Technique for processing alloying material of steel and copper
CN101195157A
Method for casting cylindrical surfaces and holes of steel matrix and copper alloy of hydraulic plunger pump cylinder body
CN102513521A
Plunger pump cylinder structure for compositing copper alloy and compositing method thereof
CN104500387A
Machining method of axial plunger pump cylinder body
CN106553021A
Copper-steel composite cathode steel bar and manufacturing process thereof
CN110965081A