A test device for double tensile crack arrest test
By designing a double tensile crack-resistance test device, the problem of lack of double tensile testing equipment in China has been solved, and effective detection of high-strength thick steel plates has been achieved, which reduces the detection cost and cycle, and improves the stability and safety of the test.
Patent Information
- Application Number
- CN202411062012.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-08-05
AI Technical Summary
The lack of dual tensile testing equipment in China has made it difficult to detect crack-resistance performance of high-strength thick steel plates and needs to be transported abroad for testing, with a long cycle and high cost.
A double tensile crack-resistance test device is designed, including a left clamping assembly, a right clamping assembly, a main tensile loading assembly and a secondary tensile loading assembly. The configuration of the collet head and the secondary tensile top block is achieved. The double tensile specimen is effectively fixed and the main and secondary tensile loads are applied evenly, and the buffering assembly prevents the test device from ejecting.
It realizes dual tensile tests safely, effectively and stably in the country, reduces the detection cost and cycle, and significantly improves the stability and safety of the test device.
Smart Images

Figure CN118565969B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of material performance detection, and in particular to a test device for a double tensile crack arrest test. Background Art
[0002] In the past two decades, the increasing size of ships and marine engineering equipment has put forward an urgent demand for high-strength and thick steel plates. For example, the maximum strength of the steel plates used in the 24,000-TEU ultra-large container ships currently in operation has reached 460MPa, and the maximum plate thickness has reached 95mm. With the increase in strength and the increase in plate thickness, the fracture resistance of steel plates decreases, and safety and reliability issues are prominent. In order to ensure the safety of the structure, the International Association of Classification Societies (IACS) requires that high-strength thick steel plates (thickness ≥ 50mm) used in key parts of the side strakes and deck side plates of large container ships must have crack arrest properties, that is, once brittle cracks occur in the structure, the steel plates can stop them, thereby avoiding catastrophic damage.
[0003] At present, the test methods for evaluating the crack arrest performance of high-strength steel thick plates are mainly divided into two categories: one is a large-scale test method represented by double tensile test, ESSO test, etc.; the other is a small-scale test method represented by Charpy impact test, drop hammer test, etc. The specimens used in the first method are large-scale specimens of original plate thickness, and the test conditions are close to the actual use conditions. The results obtained can better reflect the actual crack arrest performance of the steel plate.
[0004] The research and development of double tensile test in the world started relatively early, and a relatively complete test method was formed. However, the test method and the specific structure of the test equipment were unknown. For a period of time, when double tensile test was needed in China, it had to be shipped abroad for testing, which had a long test cycle and high test costs.
[0005] Chinese patent CN201920042254.8 provides an axial tensile and rotary bending test machine, including a driving mechanism, a tensile mechanism and a bending mechanism, wherein the driving mechanism includes a driving motor and a machine shaft for connecting the driving motor with a driving spindle of the experimental sample; the tensile mechanism includes a loading spindle connected to the experimental sample at the first end, a tensile device connected to the second end of the loading spindle to stretch the experimental sample through the loading spindle, and a tensile sensor for measuring the magnitude of the tensile force; the bending mechanism is located in the middle of the loading spindle, including a thrust device for radially pushing the loading spindle and a thrust sensor located between the thrust device and the loading spindle to measure the magnitude of the thrust. The testing machine provided by the patent can simultaneously apply a dual load of axial force and shear force to the experimental sample, and measure the fatigue characteristics of the experimental sample under the action of dual loads, but it cannot simultaneously apply the primary tensile load and the secondary tensile load in the same direction for the dual tensile test. At present, there is no relevant research on test equipment for dual tensile in China, and no test equipment capable of conducting dual tensile tests has been disclosed, which seriously restricts the research progress related to domestic crack arrest steel. Summary of the invention
[0006] The purpose of the present invention is to provide a test device for double tensile crack arrest test, which is used for double tensile test of large-size specimens and provides convenience for the study of crack arrest performance of thick steel plates.
[0007] The invention discloses a test device for a double tensile crack arrest test, comprising:
[0008] A left clamping assembly, the left clamping assembly at least comprising a left clamping plate group, the left clamping plate group being used to clamp and fix the left end of the component to be stretched;
[0009] A right clamping assembly, the right clamping assembly at least comprising a right clamping plate group, the right clamping plate group being used to clamp and fix the right end of the component to be stretched, the right clamping assembly being movably arranged relative to the left clamping assembly;
[0010] A main tensile loading assembly, the main tensile loading assembly comprises a main loading hydraulic cylinder and a bearing crossbeam, the main loading piston of the main loading hydraulic cylinder is coaxially arranged with the bearing crossbeam, the main loading hydraulic cylinder is fixedly connected with the left clamping assembly or the right clamping assembly, and is used to apply a tensile main load to the double tensile specimen in the test, the bearing crossbeam is fixedly connected with the right clamping assembly or the left clamping assembly relative to the main loading piston, and the bearing crossbeam is used to transmit the thrust applied by the main loading piston thereon to the right clamping assembly or the left clamping assembly where it is located, so as to apply the main load of the double tensile test to the assembly to be stretched;
[0011] A secondary tensile loading assembly, the secondary tensile loading assembly is a movable part, which is assembled together with the assembly to be stretched when performing a tensile test, and the secondary tensile loading assembly includes a secondary tensile loading device and a secondary tensile top block, and two of the secondary tensile loading devices and the secondary tensile top block are respectively provided, and the two secondary tensile top blocks are respectively provided on the left and right sides of the crack initiation plate of the double tensile specimen, and are respectively fixed with the crack initiation plate, and the two secondary tensile loading devices are provided between the two secondary tensile top blocks, and the two secondary tensile loading devices are respectively provided at positions close to the front and rear sides of the secondary tensile top blocks, and the two secondary tensile loading devices are respectively used to load the front and rear sides of the two secondary tensile top blocks, so as to load and initiate cracking of the crack initiation plate of the double tensile specimen with the secondary tensile load;
[0012] A left base, the left clamping assembly is fixedly arranged on the left base, and one of the main loading hydraulic cylinder and the bearing crossbeam is fixedly arranged on the left base;
[0013] A right base, the right clamping assembly is fixedly arranged on the right base, and the other of the main loading hydraulic cylinder and the bearing crossbeam is fixedly arranged on the right base;
[0014] A track, on which at least one of the left base and the right base is movably disposed.
[0015] Furthermore, the component to be stretched includes a double-stretch specimen and a clamping part. There are two clamping parts, which are respectively arranged on the left and right sides of the double-stretch specimen. The clamping part is used to cooperate with the left clamping plate group or the right clamping plate group to clamp and fix, thereby achieving clamping and fixing of the double-stretch specimen.
[0016] Further, the left clamping plate group includes two left clamping plates arranged opposite to each other in the front-to-back direction, a left clamping cavity is formed between the two left clamping plates, and a first fixing hole is correspondingly provided on the two left clamping plates, the right clamping plate group includes two right clamping plates arranged opposite to each other in the front-to-back direction, a right clamping cavity is formed between the two right clamping plates, and a second fixing hole is correspondingly provided on the two right clamping plates, the chuck head includes a chuck body, a chuck pad and a chuck through hole, the chuck body is fixedly connected to the double tensile specimen, each chuck body is correspondingly provided with two chuck pads, the two chuck pads are correspondingly arranged on the front and rear sides of the chuck body, the chuck through hole passes through the chuck body and the chuck pad, the chuck body is used to cooperate with the left clamping plate group or the right clamping plate group for clamping, the chuck pad is used to adjust the thickness of the chuck head in the front-to-back direction to cooperate with the left clamping cavity or the right clamping cavity, and the chuck through hole is used to cooperate and fix with the first fixing hole or the second fixing hole.
[0017] Furthermore, the double tensile specimen includes a crack initiation plate and a main tensile plate, the crack initiation plate is arranged on the upper side of the main tensile plate, the center position of the lower end of the crack initiation plate is fixedly connected to the main tensile plate, a prefabricated notch is arranged at the center position of the crack initiation plate, a left through hole is arranged at a position near the left side of the crack initiation plate, and a right through hole is arranged at a position near the right side of the crack initiation plate, the left through hole and the right through hole are respectively used for fixed connection with the secondary tensile top block to load the secondary tensile load.
[0018] Furthermore, the auxiliary stretching top block includes a top block body and an ear plate, there are two ear plates, the two ear plates are arranged at a certain distance, and an auxiliary clamping cavity is formed between the two ear plates, the auxiliary clamping cavity is used to clamp the crack initiation plate, and third fixing holes are correspondingly arranged on the two ear plates. When the auxiliary clamping cavity clamps the crack initiation plate, the third fixing hole is aligned with the left through hole or the right through hole so as to be fixedly connected by a second fixing pin.
[0019] Furthermore, the two surfaces on the top block body outside the two ear plates are recorded as the first top surface and the second top surface, and the two auxiliary tensile loading devices are respectively connected between the first top surface and the second top surface of the two auxiliary tensile top blocks.
[0020] Furthermore, the test device also includes a plurality of buffer components, each of which includes a buffer hydraulic cylinder, a buffer connecting rod and a support member, each buffer component includes two support members, and the two support members are used to support the buffer connecting rod. The buffer hydraulic cylinder is connected to one end of the buffer connecting rod to prevent the double tensile specimen from breaking and causing the test device to bounce.
[0021] Furthermore, there are four buffer components, which are symmetrically arranged vertically and frontally.
[0022] Furthermore, a first support plate and a second support plate are fixedly arranged on the left base, the first support plate is fixedly connected to the left clamping plate group, the first support plate and the second support plate are used to cooperate in supporting the main loading hydraulic cylinder, and a support part is arranged on the right base, the bearing beam is fixedly arranged on the support part, and the support part is fixedly connected to the right clamping plate group.
[0023] Furthermore, there are four main tensile loading components, which are symmetrically arranged up and down and front and back.
[0024] Compared with the prior art, the test device for double tensile crack arrest test described in the present invention has the following advantages:
[0025] The present invention realizes the effective fixation of the double tensile specimen by setting the left clamping assembly, the right clamping assembly, the clamping head and the secondary tensile top block, so that the test device can provide stable primary and secondary tensile loads to the double tensile specimen, and improve the stability of the test process. Among them, the coordination of the secondary tensile top block and the secondary loading device significantly reduces the difficulty of setting the secondary loading device, and ensures the uniformity of the secondary tensile load applied to the crack initiation plate, and ensures the test effect. The setting of the buffer assembly avoids the first clamping assembly or the second clamping assembly from bouncing due to test fracture during the double tensile test, ensuring the safety of the test. The test device provided by the present invention has a simple structure and is easy to operate, and can safely, effectively and stably perform double tensile tests. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a front view of the test device for double tensile crack arrest test according to an embodiment of the present invention, which does not include the secondary tensile loading assembly;
[0027] Figure 2 It is a top view of the test device for the double tensile crack arrest test described in the embodiment after the component to be stretched is installed;
[0028] Figure 3 It is a front view of the double tensile test specimen according to an embodiment of the present invention;
[0029] Figure 4 This is a front view of the component to be stretched according to an embodiment of the present invention;
[0030] Figure 5 A top view of the component to be stretched according to an embodiment of the present invention;
[0031] Figure 6 It is a structural schematic diagram of the auxiliary stretching top block according to an embodiment of the present invention;
[0032] Figure 7 It is a side view of the auxiliary stretching top block according to an embodiment of the present invention;
[0033] Figure 8 It is a schematic diagram of the state of loading and gradient temperature field in the double tensile crack arrest test according to an embodiment of the present invention;
[0034] Fig. 9 It is a structural schematic diagram of the installation of the heat preservation tank and the double tensile test specimen according to the embodiment of the present invention;
[0035] Fig.10 for Fig. 9 A top view of
[0036] Fig.11 This is a schematic diagram of the connection structure of the fourth heat preservation tank and the electric valve, the liquid separation box, the drive pump, and the liquid storage tank according to an embodiment of the present invention;
[0037] Fig.12 It is a schematic diagram of the structure when a thermocouple is arranged on the double tensile specimen according to an embodiment of the present invention;
[0038] Fig.13 Schematic diagram for judging the effectiveness of the double tensile crack arrest test described in an embodiment of the present invention.
[0039] Description of reference numerals:
[0040] 100, left clamping plate group; 110, left clamping plate; 120, left clamping cavity; 130, first fixing hole; 140, first support plate; 200, right clamping plate group; 210, right clamping plate; 220, right clamping cavity; 230, second fixing hole; 300, buffer assembly; 310, buffer hydraulic cylinder; 320, buffer connecting rod; 330, support member; 400, main tensile loading assembly; 410, main loading hydraulic cylinder; 411, main loading piston; 420, bearing beam ; 500, double tensile test specimen; 510, crack initiation plate; 511, left through hole; 512, right through hole; 513, prefabricated notch; 520, main tensile plate; 600, chuck portion; 610, chuck body; 620, chuck pad; 630, chuck through hole; 700, second support plate; 800, support portion; 900, auxiliary tensile top block; 910, top block body; 911, first top surface; 912, second top surface; 920, ear plate; 921, third fixing hole; 93 0, secondary clamping cavity; 1000, insulation tank; 1010, first insulation tank; 1011, first ear plate; 1020, second insulation tank; 1021, second ear plate; 1030, third insulation tank; 1031, third ear plate; 1040, fourth insulation tank; 1041, fourth ear plate; 1050, first connecting piece; 1051, first connecting screw; 1052, first nut; 1060, second connecting piece; 1061, second connecting screw; 1062, second Nut; 1100, housing; 1110, ultra-low temperature tank; 1120, low temperature tank; 1130, high temperature tank; 1200, drive pump; 1210, ultra-low temperature drive pump; 1220, low temperature drive pump; 1230, high temperature drive pump; 1300, liquid storage tank; 1310, ultra-low temperature liquid storage tank; 1320, low temperature liquid storage tank; 1330, high temperature liquid storage tank; 1400, liquid separation box; 1500, electric valve; 1600, temperature control pipeline; 1700, thermocouple. DETAILED DESCRIPTION
[0041] To make the purpose, technical solutions and advantages of the present invention clearer, the present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the described embodiments are part of the embodiments of the present invention, rather than all of the embodiments. The specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. It should be noted that the embodiments of the present invention and the features in the embodiments can be combined with each other without conflict.
[0042] A test device for a double tensile crack arrest test according to an embodiment of the present invention will be described in detail below with reference to the accompanying drawings. Example
[0043] This embodiment provides a test device for double tensile crack arrest test, such as Figure 1-Figure 13 As shown, including:
[0044] A left clamping assembly, the left clamping assembly at least comprising a left clamping plate group 100, the left clamping plate group 100 is used to clamp and fix the left end of the component to be stretched;
[0045] A right clamping assembly, the right clamping assembly at least comprising a right clamping plate group 200, the right clamping plate group 200 is used to clamp and fix the right end of the component to be stretched, and the right clamping assembly is movably arranged relative to the left clamping assembly;
[0046] A main tensile loading assembly 400, the main tensile loading assembly 400 comprises a main loading hydraulic cylinder 410 and a bearing crossbeam 420, the main loading piston 411 of the main loading hydraulic cylinder 410 is coaxially arranged with the bearing crossbeam 420, the main loading hydraulic cylinder 410 is fixedly connected with the left clamping assembly or the right clamping assembly, and is used to apply a tensile main load to the double tensile specimen 500 in the test, the bearing crossbeam 420 is fixedly connected with the right clamping assembly or the left clamping assembly relative to the main loading piston 411, and the bearing crossbeam 420 is used to transmit the thrust applied by the main loading piston 411 thereon to the right clamping assembly or the left clamping assembly where it is located, so as to apply the main load of the double tensile test to the assembly to be stretched;
[0047] A secondary tensile loading assembly, the secondary tensile loading assembly is a movable part, which is assembled together with the component to be stretched when performing a tensile test. The secondary tensile loading assembly includes a secondary tensile loading device (not shown in the drawings) and a secondary tensile top block 900. Two of the secondary tensile loading devices and two of the secondary tensile top blocks 900 are respectively provided. The two secondary tensile top blocks 900 are respectively arranged on the left and right sides of the crack initiation plate 510 of the double tensile specimen 500, and are respectively fixed with the crack initiation plate 510. The two secondary tensile loading devices are arranged between the two secondary tensile top blocks 900, and the two secondary tensile loading devices are respectively arranged at positions close to the front and rear sides of the secondary tensile top blocks 900. The two secondary tensile loading devices are respectively used to load the front and rear sides of the two secondary tensile top blocks 900, so as to load and initiate cracking of the crack initiation plate 510 of the double tensile specimen 500 with the secondary tensile load;
[0048] A left base (not shown in the drawings), the left clamping assembly is fixedly arranged on the left base, and one of the main loading hydraulic cylinder 410 and the bearing crossbeam 420 is fixedly arranged on the left base;
[0049] A right base (not shown in the drawings), the right clamping assembly is fixedly arranged on the right base, and the other of the main loading hydraulic cylinder 410 and the bearing crossbeam 420 is fixedly arranged on the right base;
[0050] A track (not shown in the drawings), on which at least one of the left base and the right base is movably disposed.
[0051] Through the above arrangement, when a double tensile test is required, the component to be stretched is clamped and fixed between the left clamping component and the right clamping component, and the auxiliary tensile loading component is arranged on the upper side of the double tensile specimen 500. The assembly of the auxiliary tensile loading component can be realized by fixing the crack initiation plate 510 of the double tensile specimen 500 with the auxiliary tensile top block 900. The assembly can be realized without setting a corresponding auxiliary tensile loading component fixing device, thereby making the test device structure of the double tensile crack arrest test simpler and the assembly more convenient. This embodiment provides a test device for a double tensile crack arrest test, which can effectively carry out a double tensile crack arrest test, so that domestic crack arrest steel does not need to be transported abroad for testing, which significantly reduces the testing cost and testing cycle. It should be noted that the bearing crossbeam 420 is fixedly connected to the right clamping assembly or the left clamping assembly relative to the main loading piston 411, which means that when the main loading hydraulic cylinder 410 is connected to the left clamping assembly, the bearing crossbeam 420 is fixedly connected to the right clamping assembly, and is arranged opposite to the main loading piston 411; when the main loading hydraulic cylinder 410 is connected to the right clamping assembly, the bearing crossbeam 420 is fixedly connected to the left clamping assembly, and is arranged opposite to the main loading piston 411. Among them, since the test device is used for double tensile test of large-sized specimens, the overall weight of the test device is relatively large, and the track can be selected from heavy steel tracks, and steel rollers that move in coordination with the steel tracks are arranged on the left base and / or the right base, so as to facilitate the movement and adjustment of the equipment. It should be noted that, in the standby state, a certain gap is set between the bearing crossbeam 420 and the main loading piston 411, which is convenient for reserving a certain space for sample installation. After the installation is completed, the main loading piston 411 first moves toward the bearing crossbeam 420, and when it abuts against the bearing crossbeam 420, the main tensile load is loaded. In this embodiment, the main load and the secondary load are applied in the same direction. Optionally, the secondary tensile loading device can be a secondary tensile hydraulic cylinder.
[0052] As an embodiment of the present invention, Figure 4 , Figure 5As shown, the assembly to be stretched includes a double tensile specimen 500 and a clamping part 600. There are two clamping parts 600, which are respectively arranged on the left and right sides of the double tensile specimen 500. The clamping part 600 is used to cooperate with the left clamping plate group 100 or the right clamping plate group 200 for clamping and fixing, thereby achieving the clamping and fixing of the double tensile specimen 500. Among them, the clamping part 600 located on the left side of the double tensile specimen 500 is used to cooperate with the left clamping plate group 100 for clamping and fixing, and the clamping part 600 located on the right side of the double tensile specimen 500 is used to cooperate with the right clamping plate group 200 for clamping and fixing. It should be understood that due to the large size of the double tensile specimen 500, when performing the double tensile test, the main tensile load to be applied to it is also very large. The setting of the clamping part 600 can cooperate with the left clamping plate group 100 and the right clamping plate group 200 for load transfer, thereby ensuring that the main tensile load is stably applied to the double tensile specimen 500.
[0053] In this embodiment, if Figure 1 , Figure 2 , Figure 5As shown, the left clamping plate group 100 includes two left clamping plates 110 arranged opposite to each other in the front-to-back direction, a left clamping cavity 120 is formed between the two left clamping plates 110, and the two left clamping plates 110 are correspondingly provided with first fixing holes 130, the right clamping plate group 200 includes two right clamping plates 210 arranged opposite to each other in the front-to-back direction, a right clamping cavity 220 is formed between the two right clamping plates 210, and the two right clamping plates 210 are correspondingly provided with second fixing holes 230, the clamping head 600 includes a clamping head body 610, a clamping head pad 620 and a clamping head through hole 630, the clamping head body 610 and the double stretching The sample 500 is fixedly connected, and two chuck pads 620 are correspondingly arranged on each chuck body 610. The two chuck pads 620 are correspondingly arranged on the front and rear sides of the chuck body 610. The chuck through hole 630 passes through the chuck body 610 and the chuck pad 620. The chuck body 610 is used to cooperate with the left clamping plate group 100 or the right clamping plate group 200 for clamping. The chuck pad 620 is used to adjust the thickness of the chuck part 600 in the front and rear direction to cooperate with the left clamping cavity 120 or the right clamping cavity 220. The chuck through hole 630 is used to cooperate and fix with the first fixing hole 130 or the second fixing hole 230. When the tensile assembly is clamped and fixed, the clamping part 600 located on the left side of the double tensile specimen 500 extends into the left clamping cavity 120, and the clamping part 600 located on the right side of the double tensile specimen 500 extends into the right clamping cavity 220. At this time, the first fixing hole 130 is aligned with the clamping through hole 630 on the left clamping part 600, and the second fixing hole 230 is aligned with the clamping through hole 630 on the right clamping part 600. Then, the two left clamping plates 110 clamp and fix the left clamping part 600 through the first fixing pin. The right clamping plate 210 clamps and fixes the right clamping part 600. After clamping and fixing, the inner wall of the left clamping plate 110 abuts against the clamping pad 620 of the left clamping part 600, and the inner wall of the right clamping plate 210 abuts against the clamping pad 620 of the right clamping part 600. The setting of the clamping pad 620 can reduce the distance between the clamping part 600 and the inner wall of the left clamping plate 110 or the inner wall of the right clamping plate 210, and reduce the deformation of the left clamping plate 110 or the right clamping plate 210 during clamping and fixing, thereby ensuring uniform and stable application of the main tensile load. It should be noted that the thickness of the clamping body 610 is the same as the thickness of the double tensile specimen 500. In this case, the thickness of the clamping pad 620 can be adjusted according to the specific situation, so that it can be set in conjunction with the left clamping cavity 120 or the right clamping cavity 220, so that the test device can test double tensile specimens 500 of different thicknesses. Optionally, the chuck body 610 is fixedly connected to the double tensile specimen 500 by welding.
[0054] like Figure 3As shown, the double tensile test specimen 500 includes a crack initiation plate 510 and a main tensile plate 520. The crack initiation plate 510 is arranged on the upper side of the main tensile plate 520. The center position of the lower end of the crack initiation plate 510 is fixedly connected to the main tensile plate 520. A prefabricated notch 513 is arranged at the center position of the crack initiation plate 510. A left through hole 511 is arranged near the left side of the crack initiation plate 510. A right through hole 512 is arranged near the right side of the crack initiation plate 510. The left through hole 511 and the right through hole 512 are respectively used to be fixedly connected to the secondary tensile top block 900 to load the secondary tensile load. The prefabricated notch 513 is used to initiate cracking under the force of the secondary tensile load. The crack formed by the prefabricated notch 513 extends to the main tensile plate 520 and stops cracking, thereby realizing the crack arrest performance test of the plate.
[0055] like Figure 6 , Figure 7 As shown, the auxiliary tensile top block 900 includes a top block body 910 and an ear plate 920. There are two ear plates 920, and the two ear plates 920 are arranged at a certain distance. A secondary clamping cavity 930 is formed between the two ear plates 920. The secondary clamping cavity 930 is used to clamp the crack-initiating plate 510. The two ear plates 920 are correspondingly provided with third fixing holes 921. When the auxiliary clamping cavity 930 clamps the crack-initiating plate 510, the third fixing hole 921 is aligned with the left through hole 511 or the right through hole 512 to be fixedly connected through a second fixing pin. Through the above arrangement, the auxiliary tensile top block 900 is fixedly connected to the crack-initiating plate 510, and then the auxiliary tensile top block 900 is overlapped and arranged on the double tensile specimen 500, without the need to set a separate fixing device, which significantly reduces the structural complexity of the test device and improves the installation flexibility of the test device.
[0056] like Figure 6 , Figure 7As shown, the two surfaces on the top block body 910 outside the two ear plates 920 are marked as the first top surface 911 and the second top surface 912, and the two auxiliary tensile loading devices are respectively connected between the first top surface 911 and the second top surface 912 of the two auxiliary tensile top blocks 900. It should be understood that the outer side of the ear plate 920 refers to the side of the ear plate 920 away from the auxiliary clamping cavity 930. The two auxiliary stretching loading devices are respectively connected between the first top surface 911 and the second top surface 912 of the two auxiliary stretching top blocks 900, which means that the auxiliary stretching top block 900 connected to the left through hole 511, its first top surface 911 and the second top surface 912 face the right side, wherein the first top surface 911 is located on the rear side and the second top surface 912 is located on the front side; the auxiliary stretching top block 900 connected to the right through hole 512, its first top surface 911 and the second top surface 912 face the left side, wherein the first top surface 911 is located on the front side and the second top surface 912 is located on the rear side. Therefore, when the auxiliary stretching loading device is set, the auxiliary stretching loading device located on the front side is connected between the second top surface 912 of the left auxiliary stretching top block 900 and the first top surface 911 of the right auxiliary stretching top block 900, and the auxiliary stretching loading device located on the rear side is connected between the first top surface 911 of the left auxiliary stretching top block 900 and the second top surface 912 of the right auxiliary stretching top block 900. Through the above arrangement, when secondary tensile load loading is required, the secondary tensile loading device can be started to synchronously load the first top surface 911 and the second top surface 912 connected thereto. By synchronously starting the two secondary tensile loading devices, synchronous and stable loading of the crack initiation plate 510 can be achieved, thereby ensuring the synchronous and stable conduct of the double tensile test.
[0057] As an optional embodiment of the present invention, the test device also includes a plurality of buffer assemblies 300, the buffer assemblies 300 include a buffer hydraulic cylinder 310, a buffer connecting rod 320 and a support member 330, each buffer assembly 300 includes two support members 330, the two support members 330 are used to support the buffer connecting rod 320, the buffer hydraulic cylinder 310 is connected to one end of the buffer connecting rod 320, and is used to prevent the double tensile specimen 500 from breaking and causing the test device to bounce. It should be understood that when performing a double tensile test, the applied load is extremely large and the specimen may break. The setting of the buffer assembly 300 can effectively reduce the inertial impact caused by the specimen break, thereby preventing the device from bouncing. It should be noted that the buffer hydraulic cylinder 310 and the load-bearing crossbeam 420 are arranged on the same side. In the double tensile test, the clamping assembly on the side where the main loading hydraulic cylinder 410 is located is fixed, and the clamping assembly on the side where the load-bearing beam 420 is located is movably arranged relative to the main loading hydraulic cylinder 410, so as to ensure the displacement requirement of the clamping assembly in the crack arrest test. Therefore, when the specimen breaks, it is often the clamping assembly on the side where the load-bearing beam 420 is located that bounces. Setting the buffer hydraulic cylinder 310 and the load-bearing beam 420 on the same side can effectively prevent bouncing and ensure the safe use of the equipment.
[0058] Among them, Figure 1 , Figure 2 As shown, a first support plate 140 and a second support plate 700 are fixedly arranged on the left base, the first support plate 140 is fixedly connected to the left clamping plate group 100, the first support plate 140 and the second support plate 700 are used to cooperate in supporting the main loading hydraulic cylinder 410, and a support portion 800 is arranged on the right base, the bearing crossbeam 420 is fixedly arranged on the support portion 800, and the support portion 800 is fixedly connected to the right clamping plate group 200. As an optional embodiment, the two support members 330 are respectively connected to the first support plate 140 and the support portion 800. By setting the first support plate 140 and the second support plate 700, the main loading hydraulic cylinder 410 can be stably installed and supported. By setting the support part 800, the installation and fixation of the load-bearing beam 420 can be achieved. During the test, the main loading hydraulic cylinder 410 is turned on, and its main loading piston 411 moves toward the load-bearing beam 420 and finally abuts against it. The load provided by the main loading hydraulic cylinder 410 is transmitted to the load-bearing beam 420 through the main loading piston 411, and finally transmitted to the right clamping plate group 200, so as to apply a uniform main tensile load to the left and right sides of the tensile component.
[0059] The test device can test a plate-shaped double tensile test specimen 500 with a thickness of 10 to 120 mm, a width of 400 to 1500 mm, and a length of 500 to 2000 mm.
[0060] The distance between the right end surface of the left clamping plate group 100 and the left end surface of the right clamping plate group 200 is greater than or equal to 1500 mm. This setting facilitates setting the temperature gradient of the sample, thereby performing a gradient temperature type double tensile test.
[0061] The center distance between the first fixing hole 130 and the second fixing hole 230 is greater than or equal to 4000 mm. Due to the large size of the sample and the setting of the clamping part 600, the overall size of the component to be stretched is large, and the above-mentioned center distance is limited to facilitate the assembly and fixation of the component to be stretched.
[0062] The maximum effective displacement stroke of the main loading hydraulic cylinder 410 is greater than or equal to 600 mm.
[0063] like Figure 1 , Figure 2 As shown, there are four main tensile loading assemblies 400, which are symmetrically arranged up and down and front and back. The up and down, front and back arrangement means that two of the main tensile loading assemblies 400 are arranged near the front side, and the other two main tensile loading assemblies 400 are symmetrically arranged near the rear side with the left clamping plate group 100 or the right clamping plate group 200 as the center, wherein the two main tensile loading assemblies 400 on the front side and the two main tensile loading assemblies 400 on the rear side are symmetrically arranged with the center of the first fixing hole 130 or the second fixing hole 230. The symmetrical arrangement up and down and front and back ensures the uniformity of loading, so as to obtain accurate detection results.
[0064] like Figure 1 , Figure 2 As shown, there are four buffer components 300, which are symmetrically arranged up and down and front and back. The symmetrical arrangement up and down and front and back ensures the uniformity of buffering and effectively prevents the device from bouncing.
[0065] In some other optional embodiments, the clamping part 600 is connected to the left clamping plate group 100 or the right clamping plate group 200 by snapping.
[0066] like Figure 9-12As shown, this embodiment also provides a temperature regulating device for establishing a gradient temperature field on the surface of a double tensile specimen, including a heat preservation tank 1000, a driving pump 1200, a liquid storage tank 1300 and a controller, wherein the heat preservation tank 1000 includes a first heat preservation tank 1010, a second heat preservation tank 1020, a third heat preservation tank 1030 and a fourth heat preservation tank 1040, the left end of the double tensile specimen 500 is located between the first heat preservation tank 1010 and the second heat preservation tank 1020, the right end of the double tensile specimen 500 is located between the third heat preservation tank 1030 and the fourth heat preservation tank 1040, and the fourth heat preservation tank 1010 is located between the first heat preservation tank 1010 and the second heat preservation tank 1020. 040 includes a housing 1100, wherein an ultra-low temperature tank 1110, a low temperature tank 1120 and a high temperature tank 1130 are arranged in sequence from top to bottom in the housing 1100, wherein the driving pump 1200 includes an ultra-low temperature driving pump 1210, a low temperature driving pump 1220 and a high temperature driving pump 1230, wherein the liquid storage tank 1300 includes an ultra-low temperature liquid storage tank 1310, a low temperature liquid storage tank 1320 and a high temperature liquid storage tank 1330, wherein an ultra-low temperature medium is stored in the ultra-low temperature liquid storage tank 1310, a low temperature medium is stored in the low temperature liquid storage tank 1320, and a high temperature medium is stored in the high temperature liquid storage tank 1330;
[0067] The ultra-low temperature tank 1110, the ultra-low temperature driving pump 1210 and the ultra-low temperature liquid storage tank 1310 are sequentially connected through pipelines to form a circulation loop, the low temperature tank 1120, the low temperature driving pump 1220 and the low temperature liquid storage tank 1320 are sequentially connected through pipelines to form a circulation loop, and the high temperature tank 1130, the high temperature driving pump 1230 and the high temperature liquid storage tank 1330 are sequentially connected through pipelines to form a circulation loop;
[0068] The insulation tank 1000 is installed on the surface of the double tensile specimen 500 and is used to adjust the surface temperature of the double tensile specimen 500. The surface of the double tensile specimen 500 is provided with a thermocouple 1700, and the thermocouple 1700 is used to detect the surface temperature of the double tensile specimen 500. The controller controls the working state of the driving pump 1200 according to the temperature information fed back by the thermocouple 1700.
[0069] The temperature control device for establishing a gradient temperature field on the surface of a sample described in the present application can enable the upper half of the double-stretch sample 500 to quickly reach a set low temperature value by setting an ultra-low temperature tank 1110, and can enable the lower half of the double-stretch sample 500 to quickly reach a set high temperature value by setting a high temperature tank 1130. By setting a low temperature tank 1120, the temperature of the surface of the double-stretch sample 500 can be accurately adjusted, and a gradient temperature field can be quickly established on the surface of the double-stretch sample 500. At the same time, the ultra-low temperature tank 1110, the low temperature tank 1120 and the high temperature tank 1130 are independently set, which is convenient for replacement when the corresponding components are deformed or damaged, without replacing the entire insulation tank 1000, thereby saving costs.
[0070] Preferably, the ultra-low temperature medium is liquid nitrogen, the low temperature medium is a combination of alcohol, dry ice and liquid nitrogen, and the high temperature medium is water.
[0071] Preferably, the first insulation tank 1010, the second insulation tank 1020, the third insulation tank 1030 and the fourth insulation tank 1040 are respectively connected to the liquid storage tank 1300. This arrangement enables the liquid storage tank 1300 to separately transport the medium to the first insulation tank 1010, the second insulation tank 1020, the third insulation tank 1030 and the fourth insulation tank 1040, ensuring that the temperature of the medium in the first insulation tank 1010, the second insulation tank 1020, the third insulation tank 1030 and the fourth insulation tank 1040 is the same.
[0072] Preferably, the liquid storage tank 1300 is provided with a liquid return port, and the medium in the liquid storage tank 1300 is transported to the insulation tank 1000 through the driving pump 1200, and then flows back to the liquid storage tank 1300 through the liquid return port to form a circulation loop.
[0073] Preferably, the distance between the uppermost thermocouple 1700 on the surface of the double tensile specimen 500 and the upper end surface of the double tensile specimen 500 is X1, the distance between adjacent thermocouples 1700 in the horizontal direction is X2, and the distance between adjacent thermocouples 1700 in the vertical direction is X3, and X1=X2=2X3.
[0074] Preferably, the first heat preservation tank 1010, the second heat preservation tank 1020, the third heat preservation tank 1030 and the fourth heat preservation tank 1040 have the same structure.
[0075] As a preferred embodiment of the present invention, the temperature control device also includes a liquid separation box 1400 and a plurality of electric valves 1500, the low-temperature tank 1120 includes a plurality of temperature control pipelines 1600 arranged in sequence from top to bottom, the low-temperature tank 1120, the electric valve 1500, the liquid separation box 1400, the low-temperature drive pump 1220 and the low-temperature liquid storage tank 1320 are connected in sequence through pipelines, and the temperature control pipeline 1600 and the electric valve 1500 are connected one-to-one through pipelines, the electric valve 1500 is used to control the flow rate of the low-temperature medium in the temperature control pipeline 1600, and the liquid separation box 1400 is used to transport the low-temperature medium to each temperature control pipeline 1600 respectively.
[0076] Specifically, one end of the liquid separation box 1400 is connected to the electric valve 1500 through a pipeline, and the other end of the liquid separation box 1400 is connected to the low-temperature drive pump 1220 through a pipeline. This arrangement can transport the low-temperature medium to each temperature control pipeline 1600 respectively, thereby realizing independent control of the flow rate of the low-temperature medium in different temperature control pipelines 1600, facilitating precise adjustment of the surface temperature of the double tensile specimen 500 and rapid establishment of a gradient temperature field.
[0077] As a preferred embodiment of the present invention, a first ear plate 1011 is provided at the upper end of the first insulation tank 1010, a second ear plate 1021 is provided at the upper end of the second insulation tank 1020, the first ear plate 1011 and the second ear plate 1021 are fixed together by a first connecting member 1050, a third ear plate 1031 is provided at the upper end of the third insulation tank 1030, a fourth ear plate 1041 is provided at the upper end of the fourth insulation tank 1040, and the third ear plate 1031 and the fourth ear plate 1041 are fixed together by a second connecting member 1060.
[0078] Specifically, this arrangement facilitates installation and disassembly between the heat preservation tank 1000 and the double tensile test specimen 500, and at the same time, the heat preservation tank 1000 is firmly fixed and is not easy to loosen.
[0079] Preferably, the first connecting member 1050 includes a first connecting screw 1051 and a first nut 1052, the first ear plate 1011 is provided with a first through hole, and the second ear plate 1021 is provided with a second through hole, the first connecting screw 1051 connects the first ear plate 1011 and the second ear plate 1021 together through the first through hole and the second through hole in sequence, and then the first nut 1052 is installed on the first connecting screw 1051 for tightening, the second connecting member 1060 includes a second connecting screw 1061 and a second nut 1062, the third ear plate 1031 is provided with a third through hole, and the fourth ear plate 1041 is provided with a fourth through hole, the second connecting screw 1061 connects the third ear plate 1031 and the fourth ear plate 1041 together through the third through hole and the fourth through hole in sequence, and then the second nut 1062 is installed on the second connecting screw 1061 for tightening, this arrangement has a firm connection and is easy to install and disassemble.
[0080] As a preferred embodiment of the present invention, the heat preservation tank 1000 and the double tensile test specimen 500 are bonded together.
[0081] Specifically, this arrangement can ensure close contact between the double-tension specimen 500 and the heat preservation tank 1000, reduce heat loss, and enable the double-tension specimen 500 to reach the required temperature more quickly.
[0082] As a preferred embodiment of the present invention, a first liquid level probe is provided in the ultra-low temperature liquid storage tank 1310, and the first liquid level probe is used to detect the liquid level of the ultra-low temperature medium in the ultra-low temperature liquid storage tank 1310; a second liquid level probe is provided in the low temperature liquid storage tank 1320, and the second liquid level probe is used to detect the liquid level of the low temperature medium in the low temperature liquid storage tank 1320; a third liquid level probe is provided in the high temperature liquid storage tank 1330, and the third liquid level probe is used to detect the liquid level of the high temperature medium in the high temperature liquid storage tank 1330.
[0083] Specifically, this arrangement can monitor the liquid levels of the media in the ultra-low temperature liquid storage tank 1310, the low temperature liquid storage tank 1320 and the high temperature liquid storage tank 1330 in real time to ensure the normal operation of the temperature control equipment.
[0084] As a preferred embodiment of the present invention, a first temperature probe is provided in the ultra-low temperature liquid storage tank 1310, and the first temperature probe is used to detect the temperature of the ultra-low temperature medium in the ultra-low temperature liquid storage tank 1310; a second temperature probe is provided in the low temperature liquid storage tank 1320, and the second temperature probe is used to detect the temperature of the low temperature medium in the low temperature liquid storage tank 1320; a third temperature probe is provided in the high temperature liquid storage tank 1330, and the third temperature probe is used to detect the temperature of the high temperature medium in the high temperature liquid storage tank 1330.
[0085] Specifically, this setting can monitor the temperature of the medium in the ultra-low temperature liquid storage tank 1310, the low temperature liquid storage tank 1320 and the high temperature liquid storage tank 1330 in real time, ensure the stability and accuracy of the medium temperature, facilitate the adjustment of the working state of the temperature control device, and establish a stable gradient temperature field on the surface of the double tensile specimen 500.
[0086] As a preferred embodiment of the present invention, a heater is provided in the high-temperature liquid storage tank 1330, and the heater is used to heat the high-temperature medium.
[0087] Specifically, this arrangement can heat the high-temperature medium in the high-temperature liquid storage tank 1330, which is convenient for adjusting the temperature of the high-temperature medium and ensuring the temperature stability of the high-temperature medium.
[0088] As a preferred embodiment of the present invention, the controller is provided with a touch screen, and the touch screen is used to display the operating status information of the temperature control device and to input the control information of the driving pump 1200 and the electric valve 1500.
[0089] Specifically, this setting can display the operating status information of the temperature control device, so that the operator can intuitively understand the working condition of the equipment and adjust the temperature control device conveniently.
[0090] The present invention also provides a method for establishing a gradient temperature field on the surface of a double tensile specimen, which is used in the temperature control device described above and comprises the following steps:
[0091] Step ST1: Check and ensure that the medium in the liquid storage tank 1300 is at the set liquid level, install the heat preservation tank 1000 on the surface of the double tensile specimen 500, and proceed to step ST2;
[0092] Step ST2: Control the ultra-low temperature driving pump 1210 to operate at a power of P1. When the temperature fed back by the thermocouple 1700 at the upper end of the double tensile specimen 500 reaches the low temperature setting value, control the ultra-low temperature driving pump 1210 to operate at a power of 0.5P1, and enter step ST3;
[0093] Step ST3: Control the high temperature driving pump 1230 to operate at a power of P3. When the temperature fed back by the thermocouple 1700 at the bottom of the double tensile specimen 500 reaches the high temperature setting value, control the high temperature driving pump 1230 to operate at a power of 0.5P3, and enter step ST4;
[0094] Step ST4: Control the low-temperature driving pump 1220 to operate at a power of P2. The controller controls the working state of the electric valve 1500 according to the temperature information fed back by the thermocouple 1700 to adjust the flow rate of the low-temperature medium in the temperature regulating pipeline 1600. When the gradient temperature field on the surface of the double tensile specimen 500 meets the requirements, close the driving pump 1200 and the electric valve 1500, and keep the temperature for a period of T.
[0095] Among them, P1 is the operating power of the ultra-low temperature driving pump 1210 , P2 is the preset operating power of the low temperature driving pump 1220 , and P3 is the preset operating power of the high temperature driving pump 1230 .
[0096] Specifically, the upper half of the double-tension specimen 500 is first made to reach a low-temperature setting value, and then the lower half of the double-tension specimen 500 is made to reach a high-temperature setting value. Then, the working state of the electric valve 1500 is controlled according to the temperature information fed back by the thermocouple 1700, and the flow rate of the low-temperature medium in the temperature control pipeline 1600 is adjusted to establish a gradient temperature field on the surface of the double-tension specimen 500. This method is simple to operate and can quickly establish a gradient temperature field on the surface of the double-tension specimen 500.
[0097] Preferably, the thickness of the double tensile test specimen 500 is H, and the insulation time is 0.5Hmin.
[0098] As a preferred embodiment of the present invention, in step ST4, the temperature gradient in the vertical direction of the gradient temperature field is in the range of 0.25 to 0.35° C. / mm.
[0099] Specifically, by precisely controlling the temperature gradient, the repeatability and accuracy of the experiment can be improved, thereby obtaining more reliable experimental results.
[0100] The above-mentioned temperature control device and temperature control method have the following advantages: 1) By setting the ultra-low temperature tank 1110, the upper part of the double tensile specimen 500 can quickly reach the set low temperature value, and by setting the high temperature tank 1130, the lower part of the double tensile specimen 500 can quickly reach the set high temperature value. By setting the low temperature tank 1120, the temperature of the surface of the double tensile specimen 500 can be accurately adjusted, and a gradient temperature field can be quickly established on the surface of the double tensile specimen 500; 2) The ultra-low temperature tank 1110, the low temperature tank 1120 and the high temperature tank 1130 are independently set, which is convenient for replacement when the corresponding components are deformed or damaged, without replacing the entire insulation tank 1000, saving costs; 3) The low temperature medium is transported to each temperature control pipeline 1600 respectively, so as to realize independent control of the flow rate of the low temperature medium in different temperature control pipelines 1600, which is convenient for accurately adjusting the temperature of the surface of the double tensile specimen 500 and quickly establishing a gradient temperature field. Example
[0101] This embodiment provides a test method for a gradient temperature type double tensile crack arrest test, which is used in the test device as described in Example 1.
[0102] The test method includes:
[0103] Step S1: The left end and the right end of the main stretching plate of the double-stretching specimen are respectively fixedly connected to a clamping head to form a component to be stretched;
[0104] Step S2: placing the component to be stretched in the test device and clamping it;
[0105] Step S3: Assembling the secondary tensile loading assembly and the double tensile specimen;
[0106] Step S4: establishing a gradient temperature field on the double tensile specimen and keeping it warm;
[0107] Step S5: When the holding time is reached, the main tensile test load is loaded and the temperature is kept constant;
[0108] Step S6: starting the secondary tensile loading assembly to apply a secondary tensile load to the crack initiation plate of the double tensile specimen until the specimen cracks;
[0109] Step S7: Unloading the secondary tensile load and the primary tensile load, and judging the effectiveness of the crack arrest test of the sample.
[0110] Among them, in step S1, the double tensile test specimen is welded to the clamping head; the above test steps are simple, the components are installed easily and quickly during the test, and the primary tensile load and the secondary tensile load are applied evenly and smoothly, which helps to improve the effectiveness of the test. In this embodiment, the primary tensile load is first applied to the primary tensile plate 520 to simulate a specific use condition, and then the secondary tensile load is loaded, which can more accurately detect the crack arrest performance of the material.
[0111] As one of the optional embodiments, step S2 includes:
[0112] Step S21: hoist the component to be stretched to the upper side of the test device, and assemble the left clamping head with the left clamping plate group, and assemble the right clamping head with the right clamping plate group;
[0113] Step S22: using a first fixing pin to fix the two ends of the component to be stretched to the left clamping plate group and the right clamping plate group respectively.
[0114] As another optional embodiment, when the clamping head is connected to the left clamping plate group or the right clamping plate group by snapping, it is only necessary to lower the component to be stretched from top to bottom so that the clamping heads at the left and right ends respectively enter the corresponding accommodating spaces of the left clamping plate group and the right clamping plate group to form a snap-fit clamping, which is simple and convenient.
[0115] In this embodiment, step S3 includes:
[0116] Step S31: hoisting two auxiliary tensile top blocks to the upper side of the double tensile specimen, and clamping the ear plates of the two auxiliary tensile top blocks to the left and right sides of the crack initiation plate on the double tensile specimen respectively;
[0117] Step S32: using a second fixing pin to fix the two auxiliary stretching top blocks to the left and right sides of the crack initiation plate respectively;
[0118] Step S33: two auxiliary tensile loading devices are arranged between two auxiliary tensile top blocks, and the position of the output push rod of the auxiliary tensile loading device is adjusted so that the auxiliary tensile loading device is in contact with the two auxiliary tensile top blocks, and the auxiliary tensile loading device will not fall. One of the auxiliary tensile loading devices is arranged at the front side of the double tensile specimen, and the other auxiliary tensile loading device is arranged at the rear side of the double tensile specimen.
[0119] Through the above arrangement, there is no need to set up a fixing structure of the auxiliary tensile loading assembly in the test device. During assembly, after the auxiliary tensile top block is fixed with the crack initiation plate, the auxiliary tensile top block can be set on the double tensile specimen, which significantly simplifies the structure of the test device and improves the assembly efficiency of the auxiliary tensile loading assembly.
[0120] Specifically, step S4 includes:
[0121] Step S41: cooling the end of the main tensile plate of the double tensile specimen close to the crack initiation plate, and maintaining the end of the main tensile plate away from the crack initiation plate at room temperature or heating it to form a trapezoidal temperature field;
[0122] Step S42: When the preset trapezoidal temperature field is reached, the heat preservation time is determined according to the thickness of the sample and the sample is kept warm.
[0123] Among them, the preset trapezoidal temperature field in step S42 refers to: the temperature within the range of 150mm to 350mm from the upper end surface of the main stretching plate is set according to a temperature gradient of 0.25~0.35℃ / mm. For example, in one of the embodiments, the set trapezoidal temperature field is as follows: the temperature 150mm away from the upper end surface of the main stretching plate is -40℃, and the temperature 350mm away from the upper end surface of the main stretching plate is 20℃. It should be noted that in order to ensure the validity of the test results, the temperature gradient within 100mm on both sides of the center line of the left and right directions of the main stretching plate should be uniformly set. For the setting of the temperature gradient field, reference can be made to the prior art and will not be repeated here. Specifically, when setting the trapezoidal temperature field, T-type thermocouples can be set at intervals of 50mm to detect the corresponding gradient temperature.
[0124] Optionally, in step S42, "determining the insulation time according to the thickness of the sample" includes: the thickness of the sample is recorded as H, and the insulation time is H / 2 minutes. In practical applications, the insulation time is 1 mm / min, but since the sample is usually insulated on both sides, the actual insulation time is H / 2 minutes. This setting can ensure that a uniform temperature gradient field is formed from the outside to the inside of the sample to ensure the accuracy of the test results.
[0125] As an embodiment of the present invention, step S5 includes:
[0126] Step S51: start the main loading hydraulic cylinder, and first control it according to the displacement mode, so that the main loading piston moves toward the bearing crossbeam and makes the two abut against each other;
[0127] Step S52: controlling the main loading hydraulic cylinder according to the loading mode so that the main loading piston cooperates with the bearing crossbeam to apply a set main load to the main tensile plate of the double tensile specimen;
[0128] Step S53: After the main load is applied, keep warm for a first preset time, and then execute step S6.
[0129] By setting the main loading load, the specific use conditions of the plate can be simulated for the double tensile specimen, so that the test results are closer to the use conditions, providing good test support for the subsequent use of the plate. The set main load can be set by the operator on the equipment controller, and the value of the main load can be calculated by the technician according to the plate model, temperature gradient shape, etc., which will not be repeated here. In some embodiments, the set main load is 0.5~0.7 of the yield strength of the main tensile plate.
[0130] The first preset time in step S53 is 28-32 seconds, preferably 30 seconds.
[0131] In step S7, the effectiveness of the crack arrest test on the specimen requires that the crack at least meets the following requirements:
[0132] The overall crack propagation path is within the range enclosed by the following five lines:
[0133] Take the center point of the upper end of the main stretching plate in the left and right directions as the starting point, two rays extending to the lower end of the main stretching plate at an angle of 30° to the central axis of the main stretching plate, two parallel lines 100 mm apart from the central axis of the main stretching plate in the left and right directions, and a parallel line 0.7W away from the upper end line of the main stretching plate and parallel to the upper end line, such as Fig.13 As shown;
[0134] And the extension end of the crack is within the range surrounded by the following four lines:
[0135] Taking the center point of the upper end of the main stretching plate in the left-right direction as the starting point, two rays extending to the lower end of the main stretching plate at an angle of 30° to the central axis of the main stretching plate, a parallel line 0.3W away from the upper end line of the main stretching plate and parallel to the upper end line, and a parallel line 0.7W away from the upper end line of the main stretching plate and parallel to the upper end line;
[0136] Where W is the height of the main tensile plate in the double tensile specimen.
[0137] It should be noted that the upper end surface described in this embodiment is defined when the double tensile specimen is set on the test device, W is the height of the main tensile plate when the double tensile specimen is set on the test device, and Figure 8 For example, W is 500 mm. When the test result is judged to be valid, the crack arrest toughness of the double tensile crack arrest test can be calculated according to the existing technology to provide technical support for the subsequent use of the material.
[0138] It should be noted that all the terms used in the present invention to indicate directionality and position, such as "upper", "lower", "left", "right", "front", "back", "vertical", "horizontal", "inner", "outer", "top", "lower", "tail end", "head end", "center", etc., are only used to explain the relative positional relationship and connection status between the components in a certain state, and are only for the convenience of describing the present invention, rather than requiring the present invention to be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the descriptions of "first", "second", etc. in the present invention are only used for descriptive purposes, and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features.
[0139] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A test device for double tensile crack arrest test, It is characterized in that include: A left clamping assembly, the left clamping assembly comprising at least a left clamping plate group (100), the left clamping plate group (100) being used to clamp and fix the left end of the component to be stretched; A right clamping assembly, the right clamping assembly comprising at least a right clamping plate group (200), the right clamping plate group (200) being used to clamp and fix the right end of the component to be stretched, the right clamping assembly being movably arranged relative to the left clamping assembly; A main tensile loading assembly (400), the main tensile loading assembly (400) comprising a main loading hydraulic cylinder (410) and a bearing crossbeam (420), the main loading piston (411) of the main loading hydraulic cylinder (410) being coaxially arranged with the bearing crossbeam (420), the main loading hydraulic cylinder (410) being fixedly connected to the left clamping assembly or the right clamping assembly, and being used to apply a tensile main load to a double tensile specimen (500) during a test, the bearing crossbeam (420) being fixedly connected to the right clamping assembly or the left clamping assembly relative to the main loading piston (411), the bearing crossbeam (420) being used to transmit the thrust applied by the main loading piston (411) thereon to the right clamping assembly or the left clamping assembly where it is located, so as to apply a main load of a double tensile test to the assembly to be stretched; a certain gap is provided between the bearing crossbeam (420) and the main loading piston (411); A secondary tensile loading component, the secondary tensile loading component is a movable part, and is assembled together with the component to be stretched when performing a tensile test, without the need to separately set up a fixing device, the secondary tensile loading component comprises a secondary tensile loading device and a secondary tensile top block (900), two of the secondary tensile loading device and the secondary tensile top block (900) are respectively provided, the two secondary tensile top blocks (900) are respectively provided on the left and right sides of the crack initiation plate (510) of the double tensile specimen (500), and are respectively fixed with the crack initiation plate (510), the two secondary tensile loading devices are provided between the two secondary tensile top blocks (900), and the two secondary tensile loading devices are respectively provided at positions close to the front side and the rear side of the secondary tensile top block (900), and the two secondary tensile loading devices are respectively used to load the front side and the rear side of the two secondary tensile top blocks (900) to load and initiate cracking of the crack initiation plate (510) of the double tensile specimen (500); A left base, the left clamping assembly being fixedly arranged on the left base, and one of the main loading hydraulic cylinder (410) and the bearing crossbeam (420) being fixedly arranged on the left base; A right base, the right clamping assembly being fixedly arranged on the right base, and the other of the main loading hydraulic cylinder (410) and the bearing crossbeam (420) being fixedly arranged on the right base; a track on which at least one of the left base and the right base is movably disposed; The double tension test specimen (500) comprises a crack initiation plate (510) and a main tension plate (520), wherein the crack initiation plate (510) is arranged on the upper side of the main tension plate (520), and the center position of the lower end of the crack initiation plate (510) is fixedly connected to the main tension plate (520), a prefabricated notch (513) is arranged at the center position of the crack initiation plate (510), a left through hole (511) is arranged at a position close to the left side of the crack initiation plate (510), and a right through hole (512) is arranged at a position close to the right side of the crack initiation plate (510), and the left through hole (511) and the right through hole (512) are respectively used for being fixedly connected to the secondary tension top block (900) to load the secondary tension load; The auxiliary stretching top block (900) comprises a top block body (910) and an ear plate (920), wherein there are two ear plates (920), and the two ear plates (920) are arranged at a certain distance, and an auxiliary clamping cavity (930) is formed between the two ear plates (920), and the auxiliary clamping cavity (930) is used to clamp the crack initiation plate (510), and third fixing holes (921) are correspondingly arranged on the two ear plates (920), and when the auxiliary clamping cavity (930) clamps the crack initiation plate (510), the third fixing hole (921) is aligned with the left through hole (511) or the right through hole (512), so as to be fixedly connected via a second fixing pin.
2. The test device for double tensile crack arrest test according to claim 1, It is characterized in that The component to be stretched comprises a double-stretch specimen (500) and a clamping part (600). There are two clamping parts (600), which are respectively arranged on the left and right sides of the double-stretch specimen (500). The clamping parts (600) are used to cooperate with the left clamping plate group (100) or the right clamping plate group (200) to clamp and fix, thereby achieving clamping and fixing of the double-stretch specimen (500).
3. The test device for double tensile crack arrest test according to claim 2, It is characterized in that The left clamping plate group (100) comprises two left clamping plates (110) arranged opposite to each other in the front-to-back direction, a left clamping cavity (120) is formed between the two left clamping plates (110), and the two left clamping plates (110) are provided with first fixing holes (130) correspondingly; the right clamping plate group (200) comprises two right clamping plates (210) arranged opposite to each other in the front-to-back direction, a right clamping cavity (220) is formed between the two right clamping plates (210), and the two right clamping plates (210) are provided with second fixing holes (230) correspondingly; the chuck part (600) comprises a chuck body (610), a chuck pad (620) and a chuck through hole (630), and the chuck body (610) is connected to the double tensile test specimen. (500) is fixedly connected, and two chuck pads (620) are correspondingly arranged on each chuck body (610), and the two chuck pads (620) are correspondingly arranged on the front and rear sides of the chuck body (610), and the chuck through hole (630) passes through the chuck body (610) and the chuck pad (620), and the chuck body (610) is used to cooperate with the left clamping plate group (100) or the right clamping plate group (200) for clamping, and the chuck pad (620) is used to adjust the thickness of the chuck part (600) in the front and rear direction to cooperate with the left clamping cavity (120) or the right clamping cavity (220), and the chuck through hole (630) is used to cooperate with the first fixing hole (130) or the second fixing hole (230) for fixing.
4. The test device for double tensile crack arrest test according to claim 1, It is characterized in that The two surfaces on the top block body (910) outside the two ear plates (920) are marked as a first top surface (911) and a second top surface (912), and the two auxiliary tensile loading devices are respectively connected between the first top surface (911) and the second top surface (912) of the two auxiliary tensile top blocks (900).
5. The test device for double tensile crack arrest test according to claim 1, It is characterized in that The test device further comprises a plurality of buffer assemblies (300), wherein the buffer assemblies (300) comprise a buffer hydraulic cylinder (310), a buffer connecting rod (320) and a support member (330), wherein each buffer assembly (300) comprises two support members (330), wherein the two support members (330) are used to support the buffer connecting rod (320), and the buffer hydraulic cylinder (310) is connected to one end of the buffer connecting rod (320) to prevent the double tensile specimen (500) from breaking and causing the test device to bounce.
6. The test device for double tensile crack arrest test according to claim 5, It is characterized in that There are four buffer components (300), which are symmetrically arranged vertically and frontally.
7. The test device for double tension crack arrest test according to claim 1, It is characterized in that A first support plate (140) and a second support plate (700) are fixedly arranged on the left base, the first support plate (140) is fixedly connected to the left clamping plate group (100), the first support plate (140) and the second support plate (700) are used to cooperate in supporting the main loading hydraulic cylinder (410), a support portion (800) is arranged on the right base, the bearing crossbeam (420) is fixedly arranged on the support portion (800), and the support portion (800) is fixedly connected to the right clamping plate group (200).
8. A test device for a double tensile crack arrest test according to any one of claims 1 to 7, It is characterized in that There are four main tensile loading components (400), which are symmetrically arranged vertically and frontally.