A contactless card-type PC anti-counterfeiting certificate and its preparation method
Through multi-layer structure and laser etching technology, combined with visible light and ultraviolet ink, the problem of insufficient anti-counterfeiting performance of contactless card documents is solved, and the four-fold anti-counterfeiting and ultraviolet light durability of documents is realized, ensuring the security and difficulty of information tamper.
Patent Information
- Application Number
- CN202410703662.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-03
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-06-03
AI Technical Summary
During the production process, contactless card documents have problems such as insufficient anti-counterfeiting performance, easy to imitate and tamper, especially polycarbonate materials are not durable to ultraviolet light, resulting in a degradation of anti-counterfeiting performance.
Non-contact card PC anti-counterfeiting certificates using multi-layer structures include surface protection layer, surface laser etching layer, surface printing layer, bearing layer, pad level layer, bottom printing layer, bottom laser etching layer and bottom protection layer. Thermal lamination is combined with visible light-changing ink and ultraviolet light-visible fluorescent ink, and laser etching technology is used to form a multi-layer anti-counterfeiting function.
The four-fold anti-counterfeiting performance of the certificate is realized, which is difficult to imitate and tamper with, enhances the optical anti-counterfeiting function, improves the durability of ultraviolet light, and makes the information difficult to tamper with through chemical changes after laser etching.
Smart Images

Figure CN118569294B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of anti-counterfeiting card making, and in particular relates to a contactless card type PC anti-counterfeiting certificate and a preparation method thereof. Background Art
[0002] A contactless card-type certificate is a certificate made using contactless IC card technology. This certificate, also known as a radio frequency card, consists of an IC chip, an induction antenna, and is composited with multiple layers of polyester material. It has both visual and machine-readable functions. Its built-in chip can store personal information, ID card number and other data, and can be authenticated and read by a card reader. The contactless IC card is placed close to the reader surface within a certain distance range (usually 20-50mm) and completes the data reading and writing operations through the transmission of radio waves. Contactless card-type certificates are widely used in access control systems, financial systems, medical systems and other scenarios to ensure information security and data privacy.
[0003] Take the second generation of resident ID cards in my country as an example. It is a contactless IC card. This kind of ID card uses RFID radio frequency identification technology and has a built-in smart chip, which has a high degree of anti-counterfeiting performance. In addition, transportation cards are also a kind of contactless IC card, which can be used for consumption payment in public transportation such as buses and rail transit. In addition to identity documents and transportation cards, contactless card-type ID cards can also be applied to other fields, such as student ID cards, medical cards, etc. They can store users' personal information and health records, and realize information sharing and data transmission functions. In general, contactless card-type ID cards play an increasingly important role in modern society. They not only improve the efficiency and security of information management, but also facilitate people's daily life.
[0004] In addition, different types of contactless card documents may have some subtle differences in the production process, and the specific steps may need to be adjusted according to the actual needs and production conditions of the document. While providing convenience and efficiency, contactless card documents also have some potential defects, but when personal information is not shared or the reading system fails, the physical anti-counterfeiting of visual identification can allow staff to quickly identify the authenticity. These defects may affect the security, reliability and user experience of the document. PC material has good rigidity, heat resistance and excellent notch impact resistance, but polycarbonate is not resistant to UV light and will turn yellow when exposed to UV light for a long time. To improve the UV resistance of PC materials, adding a small amount of UV inhibitors generally has a poor effect, so excessive addition of UV inhibitors is often required. However, this will cause the precipitation of UV inhibitors and reduce the mechanical properties of plastic materials. Summary of the invention
[0005] Purpose of the invention: The present invention aims to provide a contactless card-type PC anti-counterfeiting document and a preparation method thereof. In the card-type anti-counterfeiting document of the present invention, the protective layer, the printing layer, the component layer and the chip are all irreversibly integrated into the document and are difficult to remove. At the same time, it has quadruple anti-counterfeiting properties, making it difficult to imitate and tamper with, and has better anti-counterfeiting performance.
[0006] To solve the above problems, the present invention provides the following technical solutions: a contactless card-type PC anti-counterfeiting certificate, which includes, from top to bottom, a surface protection layer, a surface laser etching layer, a surface printing layer, a bearing layer, a leveling layer, a bottom printing layer, a bottom laser etching layer and a bottom protection layer combined by thermal lamination, a chip and an induction antenna electrically connected to the chip are arranged between the leveling layer and the bearing layer, a personal information area is arranged on the front side of the surface printing layer, and a visible light-variable ink is coated in the personal information area under visible light, and a general information area is arranged on the back side of the bottom printing layer, and a visible fluorescent ink is coated in the general information area under ultraviolet light.
[0007] Further preferably, a photo area is provided on the front side of the surface printing layer, in which a photo of the cardholder is printed by inkjet printing, laser printing or UV flatbed printing, and a photo window is etched on the surface laser etching layer corresponding to the photo area by laser.
[0008] Preferably, the surface and bottom protective layers are both transparent PC substrates with a light transmittance of ≥80%; and / or, the surface printing layer, the bearing layer, the leveling layer and the bottom printing layer are all white opaque PC substrates.
[0009] Preferably, the thickness of the surface protection layer is 150±5.0% μm, the thickness of the surface laser etching substrate is 100±5.0% μm, the thickness of the surface printing layer is 105±5.0% μm, the thickness of the bearing layer is 105±5.0% μm, the thickness of the leveling layer is 220±3.0% μm, the thickness of the bottom printing layer is 105±5.0% μm, the thickness of the bottom laser etching substrate is 50±5.0% μm, and the thickness of the bottom protection layer is 150±5.0% μm.
[0010] Preferably, the preparation step of the white opaque PC substrate is as follows: taking raw materials according to the following weight ratio: 60-80 parts of PC granular plastic, 10-16 parts of acrylonitrile-styrene copolymer, 20-30 parts of hydroxy ternary chloroacetic acid resin, 5-10 parts of titanium dioxide, 5-10 parts of erucic acid amide, 3-6 parts of temperature-sensitive microcapsules, 2-5 parts of aluminum powder, 3-5 parts of anti-ultraviolet agent, 2-5 parts of rare earth coupling agent and 0.5-3 parts of tetrapod-shaped zinc oxide crystal, mixing hydroxy ternary chloroacetic acid resin, acrylonitrile-styrene copolymer, erucic acid amide, anti-ultraviolet agent , four-needle zinc oxide whiskers are extruded and granulated through a twin-screw extruder to obtain a premix, the screw temperature range is 160-200°C, and the rotation speed is 150-300 rpm; then PC resin, premix, rare earth coupling agent, titanium dioxide, aluminum powder, and temperature-sensitive microcapsules are extruded and granulated through a twin-screw extruder to obtain pellets, the screw temperature range is 220-260°C, and the rotation speed is 150-300 rpm. After the pellets are cooled, they are sent to a planetary extruder for plasticization, and finally the plasticized molten material is sent to a calender for sheeting, decanting, cooling, and slicing to obtain the finished product.
[0011] Preferably, the preparation method of the visible light-variable ink is as follows: prepare the following raw materials in parts by weight: 50-60 parts of hydroxy acrylic resin, 25-30 parts of hydroxy epoxy resin, 7-10 parts of cyanate resin, 6-12 parts of nano-alumina solution, 0.7-2.2 parts of toluene diisocyanate, 3-6 parts of oligomeric linseed oil, 0.5-1.5 parts of rare earth coupling agent, 5-10 parts of colorant, 5-10 parts of inorganic light-variable powder, neopentyl glycol polymethyl ethylene oxide dipropylene glycol, 1.5-2.5 parts of acrylic acid ester; first slowly stir the colorant, inorganic optically variable powder, toluene diisocyanate and oligomeric linseed oil in a mixer to make them fully moistened and evenly distributed; then add hydroxy acrylic resin, hydroxy epoxy resin, cyanate resin, nano alumina solution and rare earth coupling agent neopentyl glycol polymethyl ethylene oxide diacrylate into a high-speed mixer and stir rapidly. The stirring temperature is controlled at 35°C-40°C until it is completely stirred and evenly distributed, and then filtered to obtain a visible optically variable ink under visible light.
[0012] Preferably, the preparation method of the fluorescent ink visible under ultraviolet light is as follows: prepare the following raw materials in parts by weight: 50-70 parts of epoxy acrylate, 20-25 parts of polyamide resin, 20-25 parts of cyanate resin, 5-7 parts of propylene glycol, 2-6 parts of inorganic fluorescent pigment, 3-5 parts of photoinitiator, 1.5-2 parts of photosensitizer TPO, 5-12 parts of nano alumina solution, 1.2-2.6 parts of acryloyl morpholine, 15-25 parts of tripropylene glycol diacrylate, 4-8 parts of polymethyl methacrylate, 2-6 parts of rare earth coupling agent, 4-8 parts of PE wax, 0.6-2 parts of silicone light diffuser and 1.2-2 parts of neopentyl glycol polymethyl ethylene oxide diacrylate; first add epoxy acrylate, reactive polyamide resin, cyanate resin, photoinitiator, photosensitizer TPO, nano alumina solution into a mixer; Alumina solution, acryloyl morpholine, and tripropylene glycol diacrylate are added and stirred until they are completely evenly mixed to obtain varnish, which is ready for use. Propylene glycol, neopentyl glycol polymethyl ethylene oxide diacrylate, PE wax, and inorganic fluorescent pigment are mixed and slowly stirred to fully and evenly wet them. After stirring evenly, varnish, polymethyl methacrylate, rare earth coupling agent, and silicone light diffuser are added and stirred rapidly until they are completely evenly mixed and filtered to obtain fluorescent ink visible under ultraviolet light.
[0013] Preferably, the nano-alumina solution is obtained by adding nano-alumina into anhydrous ethanol and uniformly dispersing the nano-alumina by ultrasonic dispersion or mechanical stirring, and the concentration thereof is 5-10 mg / ml.
[0014] Preferably, the fluorescent color of the inorganic fluorescent pigment is fluorescent yellow, fluorescent orange, fluorescent purple, fluorescent green or fluorescent blue.
[0015] Preferably, the bearing layer and the leveling layer constitute a component layer for embedding the chip, the component layer is provided with a cavity for accommodating the chip, and the chip is encapsulated in the component layer; the cavity comprises an upper recessed hole provided in the bearing layer and a lower recessed hole provided in the leveling layer, the width of the upper recessed hole is greater than the width of the lower recessed hole, and the chip and the cavity are loosely fitted; and / or, a wire groove for accommodating an inductive antenna is provided in the component layer, and the inductive antenna is encapsulated in the component layer.
[0016] A method for preparing the contactless card-type PC anti-counterfeiting certificate, the specific preparation method comprising:
[0017] S1. Prepare visible light-variable ink and ultraviolet light-visible fluorescent ink; use a lithographic UV printer to apply the visible light-variable ink to the personal information area of the top printing layer, and use screen printing to apply the ultraviolet light-visible fluorescent ink to the general information area on the back of the bottom printing layer;
[0018] S2. A wire groove for accommodating the antenna is provided between the bearing layer and the leveling layer. A fully automatic antenna implantation machine is used to wind the polyurethane enameled copper wire into the antenna. Concave holes are respectively provided on the bearing layer and the leveling layer at positions in contact with the chip. Then the chip is placed between the bearing layer and the leveling layer. The encapsulation resin surface of the chip is fixed in the concave hole of the leveling layer by a sealing glue. The chip and the induction antenna are electrically connected. Then the bearing layer is placed on the leveling layer. The layers are thermally laminated into one piece by a laminating machine to obtain a component layer.
[0019] S3. A surface protection layer, a surface laser etching layer, and a surface printing layer are placed on the front side of the component layer from top to bottom, and a bottom printing layer, a bottom laser etching layer, and a bottom protection layer are placed on the back side of the component layer from top to bottom. After alignment, a laminator is used for heat lamination to produce a finished product certificate;
[0020] S4. Use a laser to etch personal information on the surface laser etching layer corresponding to the personal information area, and etch general information on the bottom laser etching layer corresponding to the general information area. Use a reader / writer corresponding to the chip model to write personal electronic data into the chip to complete the certificate production.
[0021] Preferably, the method further includes the following steps: in step S1, a photo of the cardholder is printed in the photo area of the surface printed layer by inkjet printing, laser printing or UV flatbed printing; in step S4, a photo window is etched on the surface laser etching layer corresponding to the photo area by laser.
[0022] Beneficial effects:
[0023] In the card-type anti-counterfeiting certificate of the present invention, the protective layer, the printing layer, the component layer and the chip are all irreversibly fused in the certificate, which is difficult to remove, and thus difficult to imitate and tamper with, and has better anti-counterfeiting performance. In addition, the present invention can directly combine the certificate by hot pressing, and there is no need to print relevant information on the printing layer in advance by ink. It only needs to apply ink on the printing layer and then hot press each layer to form, and then laser etch the corresponding text and pattern. The present invention improves the defect that PC resin is easily aged by ultraviolet rays under the synergistic effect of hydroxy ternary chloroacetic acid resin and anti-ultraviolet agent. The present invention solves the problem that ink is easily destroyed under hot lamination conditions by using cyanate resin and nano alumina solution. Under visible light, the personal information on the front side presents two different colors as the visual angle and light change. It has strong light-variable characteristics and large color difference, forming the first layer of anti-counterfeiting; the general information on the back side fluoresces under ultraviolet light, enhancing the optical anti-counterfeiting function of the certificate, forming the second layer of anti-counterfeiting; through the high energy of laser etching, the relevant personal information and general information are etched on the laser etching layer in a destructive way. The etched area will produce a change in depth and expose the ink on the printed layer to give it a concave effect. Since the substrate undergoes irreversible chemical changes after laser etching, the personal information obtained by laser etching is difficult to tamper with, forming the third layer of anti-counterfeiting; combined with the white opaque PC substrate with temperature-sensitive temperature-changing effect, it forms the fourth layer of anti-counterfeiting. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 This is a schematic diagram of the structure of Example 1 of the present invention.
[0025] Among them, 1. surface protection layer, 2. surface laser etching layer, 3. surface printing layer, 4. bearing layer, 5. leveling layer, 6. bottom printing layer, 7. bottom laser etching layer, 8. bottom protection layer, 9. chip, 10. sensing antenna. DETAILED DESCRIPTION
[0026] The embodiments of the present invention are described in detail below in conjunction with the accompanying drawings: This embodiment is implemented under the premise of the technical solution of the present invention, and a detailed implementation method and a specific operation process are given, but the protection scope of the present invention is not limited to the following embodiments. If the specific conditions are not specified in the embodiments, they are carried out according to conventional conditions or conditions recommended by the manufacturer. If the manufacturer of the reagents or instruments used is not specified, they are all conventional products that can be purchased commercially.
[0027] Example 1
[0028] like Figure 1As shown, this embodiment provides a contactless card-type PC anti-counterfeiting certificate, which includes, from top to bottom, a surface protection layer, a surface laser etching layer, a surface printing layer, a bearing layer, a leveling layer, a bottom printing layer, a bottom laser etching layer and a bottom protection layer combined by thermal lamination, a chip and an induction antenna electrically connected to the chip are arranged between the leveling layer and the bearing layer, a personal information area is arranged on the front of the surface printing layer, and a visible light-variable ink is coated in the personal information area under visible light, and a general information area is arranged on the back of the bottom printing layer, and a fluorescent ink is coated in the general information area under ultraviolet light. A photo area is also arranged on the front of the surface printing layer, in which a photo of the certificate holder is printed by inkjet printing, laser printing or UV flatbed, and a photo window is etched on the surface laser etching layer corresponding to the photo area by laser.
[0029] The production process of the above-mentioned contactless card documents involves multiple steps to ensure the security, durability and functionality of the documents. The following is the process of producing contactless card documents:
[0030] S1. Prepare visible light-variable ink and ultraviolet light-visible fluorescent ink; use a lithographic UV printer to apply the visible light-variable ink to the personal information area of the top printing layer, and use screen printing to apply the ultraviolet light-visible fluorescent ink to the general information area of the bottom printing layer;
[0031] S2. A wire slot for accommodating the antenna is provided between the bearing layer and the leveling layer (the position of the wire slot can be designed based on the chip manufacturer's technical parameters for the optimal antenna line type to ensure that the resonant frequency and Q value meet the application requirements). A fully automatic antenna implantation machine is used to wind the induction antenna (polyurethane enameled copper wire) through ultrasonic wire embedding technology (different layout specifications can be wound according to needs); since the chip of the contactless card is sandwiched inside the component layer and the chip has a certain thickness, concave holes of different specifications and sizes must be punched out at the position where the chip contacts the bearing layer and the leveling layer. During production and processing, two different specifications of punching machines are used. The die is punched; then the chip filling machine is used to implant the chip into the concave hole between the bearing and the leveling layer. The chip's encapsulation resin surface is fixed in the concave hole of the leveling layer by the sealing glue. The chip and the induction antenna are welded by the fully automatic welding machine, and then the bearing layer is placed on the leveling layer. After being thermally laminated by the fully automatic laminating machine, the component layer is obtained; the thermal lamination process parameters are: pressure parameter: 10-12 MPa; lamination temperature: 220-250℃; lamination time: 15-90s; heat conduction technology ensures uniform pressure distribution, and a stable hot kerosene heating system ensures temperature uniformity. The chip, antenna and other components are assembled and packaged by the shell. The packaging increases the durability and stability of the access card, ensuring that it can work normally in various environments.
[0032] S3. On the front side of the component layer, a surface protection layer, a surface laser etching layer, and a surface printing layer are placed in order from top to bottom. On the back side of the component layer, a bottom printing layer, a bottom laser etching layer, and a bottom protection layer are placed in order from top to bottom. After alignment, they are hot-laminated using a laminator to produce a finished certificate. If large quantities of certificates are produced, a semi-automatic stacking machine can be used to stack and position various layers such as PC. Hot-press positioning and video online detection can be used to detect whether the laminated structure is missing, thereby improving the efficiency of large-scale certificate production. After lamination, the large cards are automatically transported to the card cutting operation surface through a fully automatic punching system. Large cards are automatically positioned in the Y direction to ensure accurate positioning. Each column of the card will be positioned and automatically cut.
[0033] S4. Use laser to etch personal information on the laser etching layer corresponding to the personal information area. The personal information includes the name, ID number, validity period and other information of the holder. According to the type and purpose of the certificate, the personal information can be customized as needed, including determining the size, font, pattern and other information of the information to ensure the authenticity and accuracy of the certificate. The laser etching layer can form a personal information window when etched by laser, through which the visible light-variable ink coated on the surface printing layer can be exposed; under visible light, the personal information presents two different colors with the change of visual angle and light, with strong light-variable characteristics and large color difference. In addition, the etched area will produce a change in depth, so that the personal information has a concave effect similar to gravure printing, presenting a good visual effect, and can be identified without any instrument or equipment. Its color angle effect cannot be reproduced by any high-definition scanner, color copier and other equipment, and the printing characteristics cannot be imitated by any other ink and printing method. The anti-counterfeiting reliability is extremely strong, which enhances the optical anti-counterfeiting function of the certificate. Etch the general information on the bottom laser etching layer corresponding to the general information area. The general information includes the shading, lace, pattern, text and logo on the card, which are the unified contents that all certificates need to print. Since the etched area will produce a change in depth, it also has a concave effect, which has a good visual effect. In addition, under ultraviolet light, these general information emits fluorescence, which enhances the optical anti-counterfeiting function of the certificate. Due to the high energy of laser etching, the relevant personal information and general information are etched on the laser etching layer in a destructive way. The etched area will produce a change in depth and expose the ink on the printing layer. Since the substrate undergoes irreversible chemical changes after laser etching, the personal information obtained by laser etching is difficult to tamper with. Use the reader corresponding to the chip model to write personal electronic data into the chip (encode and initialize the embedded chip, and write the cardholder's personal information, data, etc. into the chip. This process needs to ensure the accuracy and security of the data to prevent data leakage or tampering.) to complete the certificate. The quality inspection of the contactless card documents is carried out, including appearance inspection (whether there are scratches on the surface, ink position, color change, dust and dirt detection), performance testing and data verification, etc. Ensure that each document meets the standards and quality requirements. The documents that pass the quality inspection can be issued to the cardholder for use. The cardholder can use the documents on devices that support contactless IC card technology, such as access control systems, public transportation systems, financial systems, etc.
[0034] Further preferably, if it is necessary to display the photo of the cardholder, in step S1, a photo area is provided on the front side of the surface printed layer, and the photo of the cardholder is printed out by inkjet printing, laser printing or UV flatbed printing; then in step S4, a photo window is etched on the surface laser etching layer corresponding to the photo area by laser, thereby revealing the photo of the cardholder.
[0035] Since lamination using glue may introduce bubbles, impurities or unevenness inside the PC card, thus affecting its quality and performance. In addition, glue may react chemically with the PC card material, resulting in discoloration, deformation or other adverse consequences. Therefore, the present invention adopts a hot lamination process to make the card. Hot lamination is the process of fusing two or more layers of materials together by heating and pressure. In PC card hot lamination, special hot lamination equipment is usually used to tightly combine the different layers of the PC card by precisely controlling the temperature and pressure. This bonding is achieved by melting and recrystallization of the material itself, rather than relying on glue. By combining in a laminating manner, a strong bonding strength can be obtained, making it difficult for the printed layer and the component layer to be peeled off, which can protect the anti-counterfeiting pattern and general information of the card.
[0036] The surface and bottom protective layers are both transparent PC substrates with a light transmittance of ≥80%. The surface printing layer, the bearing layer, the leveling layer and the bottom printing layer are all white opaque substrates. The transparent substrate can be completely or partially colored, provided that it is transparent in at least part of the visible spectrum, so that an observer can see through, for example, the transparent substrate and the laminated material, and the printed layer pattern can be observed from both the front and back sides of the laminated product. "Transparent" in the context of the present invention means: "providing optical transparency in at least part of the visible spectrum (400nm-700nm wavelength)".
[0037] The thickness of the surface protection layer is 150 μm, the thickness of the surface laser etching substrate is 100 μm, the thickness of the surface printing layer is 105 μm, the thickness of the bearing layer is 105 μm, the thickness of the leveling layer is 220 μm, the thickness of the bottom printing layer is 105 μm, the thickness of the bottom laser etching substrate is 50 μm, and the thickness of the bottom protection layer is 150 μm.
[0038] In the above embodiment, the white opaque PC substrate used can be purchased from the market or prepared by itself. In this embodiment, the white opaque PC substrate is preferably prepared by the following method. The preparation steps are as follows: take the raw materials according to the following weight ratio: 70 parts of PC granular plastic, 13 parts of acrylonitrile-styrene copolymer, 25 parts of hydroxy ternary chloroacetic acid resin, 7 parts of titanium dioxide, 7 parts of erucic acid amide, 4 parts of temperature-sensitive microcapsules, 3 parts of aluminum powder, 4 parts of anti-ultraviolet agent, 3 parts of rare earth coupling agent and 2 parts of tetrapod-shaped zinc oxide crystals, mix the hydroxy ternary chloroacetic acid resin, acrylonitrile-styrene copolymer, erucic acid amide and 2 parts of tetrapod-shaped zinc oxide crystals. The amide, anti-ultraviolet agent and four-needle zinc oxide whisker are extruded and granulated by a twin-screw extruder to obtain a premix, the screw temperature range is 180°C, and the speed is 200 rpm; then the PC resin, premix, rare earth coupling agent, titanium dioxide, aluminum powder and temperature-sensitive microcapsules are extruded and granulated by a twin-screw extruder to obtain pellets, the screw temperature range is 240°C, and the speed is 200 rpm. After the pellets are cooled, they are sent to a planetary extruder for plasticization, and the heating temperature of the planetary extruder is controlled at 140°C; the molten material plasticized by the planetary extruder is sent to a calender for sheeting, decanting, cooling and slicing to obtain a finished product.
[0039] Among them, PC materials have good rigidity, heat resistance and excellent notch impact resistance, but polycarbonate is not resistant to ultraviolet light and will turn yellow when exposed to ultraviolet light for a long time. Hydroxy ternary chloroacetic acid resin has the characteristics of being odorless and non-toxic, with low water absorption and water vapor permeability, high toughness, plasticity and high heat resistance. Its heat resistance is also very excellent, and it can withstand high temperatures up to 200°C without affecting its performance. The present invention can combine the excellent properties of the two by blending hydroxy ternary chloroacetic acid resin with PC. In addition, hydroxy ternary chloroacetic acid resin can also effectively prevent PC substrate aging and discoloration, and maintain long-term color vividness. If you want to improve the ultraviolet resistance of PC materials, adding a small amount of anti-ultraviolet agent generally has a poor effect, so it is often necessary to add an excessive amount of anti-ultraviolet agent. However, this will cause the precipitation of the anti-ultraviolet agent and reduce the mechanical properties of the plastic material. The present invention improves the ultraviolet resistance of the substrate by blending hydroxy ternary chloroacetic acid resin with PC, preventing aging and discoloration. In addition, as long as a small amount of anti-ultraviolet agent is combined, the ultraviolet resistance of the substrate is improved without reducing the mechanical properties of the substrate. Hydroxyl ternary chloroacetic acid resin has excellent dispersibility for inorganic pigment titanium dioxide and can also enhance the arrangement of aluminum powder. In addition, the hydroxyl functional group enables the ternary chloroacetic acid resin to cross-link with the thermosetting resin in the ink to obtain excellent chemical resistance (alcohol resistance) and water resistance. It can also resist various chemical corrosions such as acids, alkalis, and solvents, so that it can maintain stable performance in various complex environments. The four-needle zinc oxide whisker has a unique three-dimensional four-needle structure, which enables it to be evenly distributed in the matrix material, thereby isotropically improving the physical properties of the material and giving the material a variety of unique functional properties. These properties include wear resistance, reinforcement, anti-aging, antistatic, antibacterial, etc. The anti-ultraviolet agent is 2-hydroxy-4-octyloxybenzophenone. AS resin not only has high gloss, high transparency, high impact, good heat resistance and mechanical properties. It has high rigidity, high chemical stability, water resistance, oil resistance, acid resistance, alkali resistance, alcohol resistance, and can also improve the compatibility of hydroxy ternary chloroacetic acid resin with PC resin. Thermosensitive microcapsules are also a common pigment on the market. Their average particle size is 3-10μm. They are microcapsule powders with a moisture content of ≤3%. They contain invisible dyes, color formers and temperature control agents. In practical applications, we regard them as a special color powder. In addition to red and blue, thermosensitive microcapsules have other colors. There are a total of fifteen colors of thermosensitive microcapsules. Any of these colors can be used in production and printing. Each color of thermosensitive microcapsules also has different types of thermosensitive microcapsules with specified color change temperatures ranging from -15℃ to 70℃. When a specific temperature range is reached, the color will disappear, and when it leaves the temperature range, the color will reappear.
[0040] The base layer (component layer, printing layer) and the surface layer (protective layer) used in the present invention are both PC-based materials, and the two are melted together by heating and laminating to form an integral structure, which solves the problem of lamination strength of each layer and achieves good interlayer bonding strength.
[0041] In the above embodiment, the visible light-variable ink used can be purchased from the market or prepared by itself. In this embodiment, the visible light-variable ink prepared by the following method is preferred: prepare the following raw materials in parts by weight: 55 parts of hydroxyl acrylic resin, 27 parts of hydroxyl epoxy resin, 8 parts of cyanate resin, 9 parts of nano-alumina solution, 1.5 parts of toluene diisocyanate, 4 parts of oligomeric linseed oil, 1 part of rare earth coupling agent, 8 parts of colorant, 8 parts of inorganic light-variable powder, 10 parts of neopentyl glycol polymethyl ethylene oxide dipropylene glycol, 10 parts of hydroxyl acrylic resin, 27 parts of hydroxyl epoxy resin, 8 parts of cyanate resin, 9 parts of nano-alumina solution ...5 parts of hydroxyl epoxy resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of cyanate resin, 25 parts of ester; first slowly stir the colorant, inorganic optically variable powder, toluene diisocyanate and oligomeric linseed oil in a mixer (speed 500r / min) to make them fully and evenly wetted; then add hydroxy acrylic resin, hydroxy epoxy resin, cyanate resin, nano alumina solution, rare earth coupling agent, and neopentyl glycol polymethyl ethylene oxide diacrylate into a high-speed mixer and stir rapidly (speed 1500r / min), and control the stirring temperature at 38°C until it is completely stirred and evenly filtered to obtain a visible optically variable ink under visible light.
[0042] The inorganic light-changing powder can be selected from: rare earth color-changing pigments, tungsten oxide mica color-changing pigments, microcapsule color-changing pigments, or a mixture of two or more thereof, wherein the microcapsule color-changing pigments are water-soluble inorganic color-changing materials in microencapsulated form.
[0043] The particle size of the pigment is about 400-600 meshes. The pigment is a mixture of at least two of benzidine yellow, phthalocyanine blue, permanent red, pink, ruby and fast dark red.
[0044] The nano-alumina solution is prepared by adding nano-alumina into anhydrous ethanol and uniformly dispersing the nano-alumina through ultrasonic dispersion or mechanical stirring, and the concentration thereof is 8 mg / ml.
[0045] Among them, the ink of the present invention forms a blending system of hydroxy acrylic resin, hydroxy epoxy resin and cyanate resin to make up for their respective deficiencies. By compounding the three resins, a better performance can be obtained. Under the action of the curing agent toluene diisocyanate, the three resins are cured by reaction, and the cured ink has excellent fullness, gloss, hardness, solvent resistance, and weather resistance. It does not change color or turn yellow during the subsequent high-temperature thermal lamination process. After the cross-linking component is added, it cannot be stored for a long time and should be used in time. Cyanate ester resin CE has excellent high-temperature mechanical properties, and its bending strength and tensile strength are higher than those of bifunctional epoxy resin; it has extremely low water absorption; low molding shrinkage and good dimensional stability; good heat resistance, moisture and heat resistance, and flame retardancy, and good bonding performance with PC materials; during the post-process hot pressing, the ink can penetrate into the tiny gaps between PC materials, and after curing, it forms a strong bond, further improving the ink's body strength, and significantly improving the ink's bonding performance to the upper and lower layers of PC materials; rare earth coupling agents can improve the compatibility between different materials and improve the interface bonding strength. During the post-process high-temperature hot pressing, the coupling agent can also promote the formation of chemical bonds between the ink and PC materials, thereby enhancing the bonding strength. The role of the rare earth coupling agent is to improve the ink's bonding performance to the upper and lower layers of materials during the post-process hot pressing and improve the body strength.
[0046] In the above embodiment, the fluorescent ink visible under ultraviolet light used can be purchased on the market or prepared by itself. In this embodiment, the fluorescent ink visible under ultraviolet light is preferably prepared by the following method: prepare the following raw materials in parts by weight: 60 parts of epoxy acrylate, 22 parts of reactive polyamide resin, 22 parts of cyanate resin, 6 parts of propylene glycol, 4 parts of inorganic fluorescent pigment, 4 parts of photoinitiator, 1.8 parts of photosensitizer TPO, 5-12 parts of nano-alumina solution, 2 parts of acryloyl morpholine, 20 parts of tripropylene glycol diacrylate, 6 parts of polymethyl methacrylate, 4 parts of rare earth coupling agent, 6 parts of PE wax, 1 part of organosilicon light diffuser and 1.6 parts of neopentyl glycol polymethyl ethylene oxide diacrylate; first add epoxy acrylate, reactive polyamide resin, cyanate resin, photoinitiator, photosensitizer TPO, nano-alumina solution, acryloyl morpholine, tripropylene glycol diacrylate into a blender, and stir after adding. Stir (speed 1500r / min) until completely stirred to obtain varnish, which is ready for use; mix propylene glycol, neopentyl glycol polymethyl ethylene oxide diacrylate, PE wax and inorganic fluorescent pigment, and stir slowly (speed 500r / min) to make them fully and evenly wetted; after stirring evenly, add varnish, polymethyl methacrylate, rare earth coupling agent, and silicone light diffuser, and stir quickly (speed 1500r / min) until completely stirred and evenly filtered to obtain fluorescent ink visible under ultraviolet light.
[0047] The nano-alumina solution is prepared by adding nano-alumina into anhydrous ethanol and uniformly dispersing the nano-alumina through ultrasonic dispersion or mechanical stirring, and the concentration thereof is 8 mg / ml.
[0048] The fluorescent color of the inorganic fluorescent pigment may be one of fluorescent yellow, fluorescent orange, fluorescent purple, fluorescent green and fluorescent blue.
[0049] The fluorescent ink visible under ultraviolet light of the present invention uses epoxy acrylate as the main prepolymer, which has the characteristics of fast curing rate, strong adhesion and flexibility. The molecules of reactive polyamide resin and epoxy acrylate are cross-linked to form macromolecules with three-dimensional network structure, which produces extensive cross-linking. In addition, the cyano group in the cyanate reacts with the functional groups (such as hydroxyl, amino, etc.) of the reactive polyamide resin to form covalent bonds, thereby realizing cross-linking. In addition, the synergistic effect of nano-alumina solution, acryloyl morpholine, tripropylene glycol diacrylate and other auxiliary agents improve the overall adhesion, flexibility, wear resistance, curing effect and reduce viscosity of UV ink; wherein, tripropylene glycol diacrylate adjusts the viscosity of the ink, promotes uniform mixing of UV ink and improves printing effect, and can promote the curing rate of the ink under ultraviolet light; the addition of PE improves the lubricity of the ink to improve its wear resistance, and polyethylene wax floats on the surface to form a protective layer to block the inhibition of oxygen on light-induced curing. The nano-alumina solution releases oxygen when the coating is cured to increase the cross-linking density; the hardness, wear resistance and high temperature resistance of the coating can be improved. The silicone light diffuser is KMP-590, and its function is to increase the diffusion performance of light, reduce fluorescence quenching, and play a role in enhancing color. Polymethyl methacrylate has high transparency and high hardness after curing and forming. It can enhance the strength and light transmittance after curing and film formation. In the present invention, it is used to enhance the light transmittance of the ink layer after the ink is film-formed. When the light irradiates the place where the ink is sprayed, the light can quickly pass through the ink layer to irradiate the discoloration substance in the film. Neopentyl glycol polymethyl oxirane diacrylate has excellent physical and chemical properties, such as light resistance, heat resistance, weather resistance, chemical corrosion resistance, etc., and also shows excellent adhesion, toughness, adhesion and anti-yellowing properties. The ester has low shrinkage when curing, and can reduce the viscosity of the system. Neopentyl glycol polymethyl oxirane diacrylate also has the problem of enhancing flexibility and preventing the ink layer from bursting when bending, and can also react with other monomers through free radical polymerization. In addition, it can also improve the flexibility of the cured film and enhance the adhesion to plastic products.
[0050] In order to verify the technical effect of the technical solution of the present invention, the performance of the contactless card-type PC anti-counterfeiting certificate prepared in the above embodiment was tested, and the performance test results are shown in Table 1.
[0051] Table 1. Test results of the contactless card-type PC anti-counterfeiting certificate prepared in Example 1
[0052]
[0053]
[0054] Deviation from the indicators will result in the product not meeting international standards and being unacceptable.
[0055] When selecting the raw materials for the PC substrate and the ink, the present invention fully considers factors such as compatibility with the materials used, thermal stability, and curing conditions. In addition, the impact of subsequent heat lamination on the ink must also be considered. Hot pressing process parameters such as temperature, pressure, and time will also have an important impact on the ink bonding strength. After a large number of tests and verifications, the selected materials and process parameters are optimized and adjusted accordingly to ensure that the final product can meet the specific bonding strength requirements. Samples were prepared and tested according to the preparation process in the embodiment. The UV resistance test (ISO 4892-2cycle2) was 2.35, the boiling-UV resistance test (ISO 4892-2cycle2) was 2.98, and the notched impact strength (GB / T 1843-2008) was 52.2kJ / m 2 The interlayer peel strength (ISO / IEC7810) is 1.65N / mm. After 5000 bending cycle tests, the card has no delamination or cracks, and the reading and writing functions are normal.
[0056] Comparative Example 1
[0057] As described in Example 1, the difference is that: in the preparation process of the white opaque PC substrate, the amount of PC granular plastic is 70 parts, the amount of acrylonitrile-styrene copolymer is 13 parts, and the amount of hydroxy ternary vinyl acetate resin is 10 parts, and the other steps and conditions are consistent with Example 1. In this comparative example, the technical effect is reduced when the proportion of PC granular plastic, acrylonitrile-styrene copolymer and hydroxy ternary vinyl acetate resin is not within the scope of the present invention. Samples were prepared and tested according to the preparation process. The UV resistance test of the obtained samples was 3.08, the boiling-UV resistance test was 4.12, and the notched impact strength was 45.5 kJ / m 2 The interlayer peel strength is 1.28N / mm, and no delamination or cracks occur after 5000 bending cycle tests.
[0058] Comparative Example 2
[0059] As described in Example 1, the difference is that no hydroxy ternary chloroacetic acid resin is added, and the other steps and conditions are consistent with Example 1. This comparative example has poor UV resistance and water boiling aging resistance when no hydroxy ternary chloroacetic acid resin is added. Samples were prepared and tested according to the preparation process. The UV resistance test of the obtained sample was 8.42, the water boiling-UV resistance test was 9.64, and the notched impact strength was 50.1 kJ / m 2The interlayer peel strength is 1.39N / mm, and no delamination or cracks occur after 5000 bending cycle tests.
[0060] Comparative Example 3
[0061] As described in Example 1, the difference is that: no hydroxy ternary chloroacetic acid resin is added, the amount of anti-ultraviolet agent added is changed to 15 parts, and the other steps and conditions are consistent with Example 1. In this comparative example, since no hydroxy ternary chloroacetic acid resin is added, an excessive amount of anti-ultraviolet agent is added, and the UV resistance and water boiling aging resistance are improved, but the mechanical properties of the plastic material are reduced. Samples were prepared and tested according to the preparation process, and the UV resistance test of the obtained samples was 3.89, the water boiling-UV resistance test was 4.05, and the notched impact strength was 34.2 kJ / m 2 The interlayer peel strength is 1.08N / mm, and cracks appear after 5000 bending cycle tests.
[0062] Comparative Example 4
[0063] As described in Example 1, the difference is that in the process of preparing the visible light-variable ink under visible light, the cyanate resin is replaced with polyurethane acrylate, and the other steps and conditions are the same as those in Example 1. The visible light-variable ink under visible light in this comparative example has poor high temperature resistance, and after heat lamination, the visible light-variable ink layer cracks.
[0064] Comparative Example 5
[0065] As described in Example 1, the difference is that: no nano-alumina solution is added during the preparation of the visible light-variable ink and the visible fluorescent ink under ultraviolet light, and the other steps and conditions are the same as those in Example 1. In this comparative example, since no nano-alumina solution is added, the ink has poor high temperature resistance, cracks appear on the front and back ink layers, and the overall structure is destroyed after thermal lamination, and the adhesion to the printed layer is reduced.
[0066] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A contactless card-type PC anti-counterfeiting document, characterized in that: It includes, from top to bottom, a surface protection layer, a surface laser etching layer, a surface printing layer, a bearing layer, a leveling layer, a bottom printing layer, a bottom laser etching layer and a bottom protection layer, each layer is bonded by thermal lamination, a chip and an induction antenna electrically connected to the chip are arranged between the leveling layer and the bearing layer, a personal information area is arranged on the front side of the surface printing layer, and a light-variable ink visible under visible light is coated in the personal information area, and a general information area is arranged on the back side of the bottom printing layer, and a fluorescent ink visible under ultraviolet light is coated in the general information area; the surface protection layer and the bottom protection layer are both transparent PC substrates, and the light transmittance is ≥80%; and / or the surface printing layer, the bearing layer, the leveling layer and the bottom printing layer are all white opaque PC substrates; The preparation method of the white opaque PC substrate comprises the following steps: taking raw materials according to the following weight ratio: 60-80 parts of PC granular plastic, 10-16 parts of acrylonitrile-styrene copolymer, 20-30 parts of hydroxy ternary chloroacetic acid resin, 5-10 parts of titanium dioxide, 5-10 parts of erucic acid amide, 3-6 parts of temperature-sensitive microcapsules, 2-5 parts of aluminum powder, 3-5 parts of anti-ultraviolet agent, 2-5 parts of rare earth coupling agent and 0.5-3 parts of tetrapod-shaped zinc oxide crystals, extruding and granulating the hydroxy ternary chloroacetic acid resin, acrylonitrile-styrene copolymer, erucic acid amide, anti-ultraviolet agent and tetrapod-shaped zinc oxide whiskers through a twin-screw extruder to obtain a premix, wherein the screw temperature range is 160-200° C. and the rotation speed is 150-300 rpm; Then, PC resin, premix, rare earth coupling agent, titanium dioxide, aluminum powder and temperature-sensitive microcapsules are extruded and granulated through a twin-screw extruder to obtain pellets. The screw temperature range is 220-260°C and the rotation speed is 150-300 rpm. After the pellets are cooled, they are sent to a planetary extruder for plasticization. Finally, the plasticized molten material is sent to a calender for sheeting, decanting, cooling and slicing to obtain the finished product.
2. A contactless card-type PC anti-counterfeiting document according to claim 1, characterized in that: The thickness of the surface protection layer is 150±5.0%μm, the thickness of the substrate of the surface laser etching layer is 100±5.0%μm, the thickness of the surface printing layer is 105±5.0%μm, the thickness of the bearing layer is 105±5.0%μm, the thickness of the leveling layer is 220±3.0%μm, the thickness of the bottom printing layer is 105±5.0%μm, the thickness of the substrate of the bottom laser etching layer is 50±5.0%μm, and the thickness of the bottom protection layer is 150±5.0%μm.
3. A contactless card-type PC anti-counterfeiting document according to claim 1, characterized in that: The preparation method of the visible light-variable ink is as follows: prepare the following raw materials in parts by weight: 50-60 parts of hydroxy acrylic resin, 25-30 parts of hydroxy epoxy resin, 7-10 parts of cyanate resin, 6-12 parts of nano-alumina solution, 0.7-2.2 parts of toluene diisocyanate, 3-6 parts of oligomeric linseed oil, 0.5-1.5 parts of rare earth coupling agent, 5-10 parts of colorant, 5-10 parts of inorganic light-variable powder, neopentyl glycol polymethyl ethylene oxide diacrylate ester 1.5-2.5 parts; first slowly stir the colorant, inorganic optically variable powder, toluene diisocyanate and oligomeric linseed oil in a mixer to make them fully moistened and evenly distributed; then add hydroxy acrylic resin, hydroxy epoxy resin, cyanate resin, nano alumina solution, rare earth coupling agent, and neopentyl glycol polymethyl ethylene oxide diacrylate into a high-speed mixer and stir rapidly. The stirring temperature is controlled at 35°C-40°C until it is completely stirred and evenly distributed, and then filtered to obtain a visible optically variable ink under visible light.
4. A contactless card-type PC anti-counterfeiting document according to claim 1, characterized in that: The preparation method of the fluorescent ink visible under ultraviolet light is as follows: prepare the following raw materials in parts by weight: 50-70 parts of epoxy acrylate, 20-25 parts of polyamide resin, 20-25 parts of cyanate resin, 5-7 parts of propylene glycol, 2-6 parts of inorganic fluorescent pigment, 3-5 parts of photoinitiator, 1.5-2 parts of photosensitizer TPO, 5-12 parts of nano alumina solution, 1.2-2.6 parts of acryloyl morpholine, 15-25 parts of tripropylene glycol diacrylate, 4-8 parts of polymethyl methacrylate, 2-6 parts of rare earth coupling agent, 4-8 parts of PE wax, 0.01 parts of organic silicon light diffuser, 1.2-2.6 parts of acryloyl morpholine, 1.2-2.6 parts of acryloyl morpholine, 15-25 parts of tripropylene glycol diacrylate, 4-8 parts of polymethyl methacrylate, 2-6 parts of rare earth coupling agent, 4-8 parts of PE wax, 0.01 parts of organic silicon light diffuser, 0.02 parts of propylene glycol solution, 0.03 parts of propylene glycol solution, 0.04 parts of propylene glycol solution, 0.05 parts of propylene glycol solution, 0.06 parts of propylene glycol solution, 0.07 parts of propylene glycol solution, 0.08 parts of propylene glycol solution, 0.09 parts of propylene glycol solution, 0.10 parts of propylene glycol solution, 0.10 parts of propylene glycol solution, .6-2 parts and 1.2-2 parts of neopentyl glycol polymethyl oxirane diacrylate; first add epoxy acrylate, reactive polyamide resin, cyanate resin, photoinitiator, photosensitizer TPO, nano alumina solution, acryloyl morpholine, tripropylene glycol diacrylate into a blender, stir until completely stirred to obtain varnish, which is ready for use; mix propylene glycol, neopentyl glycol polymethyl oxirane diacrylate, PE wax and inorganic fluorescent pigment, stir slowly to make it fully wetted and evenly mixed; after stirring evenly, add varnish, polymethyl methacrylate, rare earth coupling agent, silicone light diffuser, stir quickly until completely stirred to obtain fluorescent ink visible under ultraviolet light after filtering.
5. A contactless card-type PC anti-counterfeiting document according to claim 4, characterized in that: The fluorescent color of the inorganic fluorescent pigment is fluorescent yellow, fluorescent orange, fluorescent purple, fluorescent green or fluorescent blue.
6. A contactless card-type PC anti-counterfeiting document according to claim 1, characterized in that: The bearing layer and the leveling layer constitute a component layer for embedding the chip, the component layer is provided with a cavity for accommodating the chip, and the chip is encapsulated in the component layer; the cavity comprises an upper recessed hole provided in the bearing layer and a lower recessed hole provided in the leveling layer, the width of the upper recessed hole is greater than the width of the lower recessed hole, and the chip and the cavity are in a clearance fit; and / or, a wire groove for accommodating an induction antenna is provided in the component layer, and the induction antenna is encapsulated in the component layer.
7. A method for preparing a contactless card-type PC anti-counterfeiting certificate according to any one of claims 1 to 6, characterized in that: The specific preparation method comprises: S1. Prepare visible light-variable ink and ultraviolet light-visible fluorescent ink; use a lithographic UV printer to apply the visible light-variable ink to the personal information area of the top printing layer, and use screen printing to apply the ultraviolet light-visible fluorescent ink to the general information area on the back of the bottom printing layer; S2. A wire slot for accommodating the antenna is provided between the bearing layer and the leveling layer, and the polyurethane enameled copper wire is wound with the antenna by a fully automatic antenna implantation machine. Concave holes are respectively provided on the bearing layer and the leveling layer at positions in contact with the chip, and then the chip is placed between the bearing layer and the leveling layer. The encapsulation resin surface of the chip is fixed in the concave hole of the leveling layer by a sealing glue, and the chip and the induction antenna are electrically connected. Then, the bearing layer is placed on the leveling layer, and the layers are thermally laminated into one by a laminating machine to obtain a component layer; S3. A surface protection layer, a surface laser etching layer, and a surface printing layer are placed on the front side of the component layer from top to bottom, and a bottom printing layer, a bottom laser etching layer, and a bottom protection layer are placed on the back side of the component layer from top to bottom. After alignment, a laminator is used for heat lamination to produce a finished product certificate; S4. Use a laser to etch personal information on the surface laser etching layer corresponding to the personal information area, and etch general information on the bottom laser etching layer corresponding to the general information area. Use a reader / writer corresponding to the chip model to write personal electronic data into the chip to complete the certificate production.
8. The preparation method according to claim 7, characterized in that: The following steps are also included: In step S1, a photo of the cardholder is printed in the photo area of the surface printing layer by inkjet printing, laser printing or UV flatbed printing; In step S4, a photo window is etched on the surface laser etching layer corresponding to the photo area by laser.