Aluminum extrusion splitter combination die
By using a detachable mold core and modular design, combined with transition sections and fastening components, the waste caused by mold wear is solved, the connection strength and applicability of the mold are improved, and the efficient use and flexibility of the mold are achieved.
Patent Information
- Application Number
- CN202411073772.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-07
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-08-07
AI Technical Summary
The core and die holes of the flow divider are prone to wear under high temperature and high pressure, which can lead to failure in profile forming and scrap the entire mold, resulting in waste.
The design employs a detachable core and module, combining the structures of the first and second transition sections. It utilizes components such as fastening bolts, fastening rings, and glass rings to enhance connection strength, and strengthens the core's resistance to lateral pressure through prestressed steel strands and radial stress members.
It reduces the frequency of mold changes, reduces waste, improves the flexibility and applicability of molds, enhances the connection strength between the mold core and the flow divider bridge, and reduces material spillage and mold core misalignment.
Smart Images

Figure CN118577642B_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of diversion dies and relates to an aluminum extrusion diversion combination die. Background Art
[0002] The diverter die is suitable for manufacturing profiles with holes. Its structure consists of two parts: an upper die and a lower die. The upper die has multiple diverter holes and a die core. The surface of the lower die is recessed to form a welding chamber. The lower die also has a die hole running through it, and the die hole is directly connected to the welding chamber. When the upper die and the lower die are combined, the welding chamber is connected to the diverter hole, and the die core passes through the die hole. There is a gap between the die core and the die hole, which is a die cavity for forming the cross-sectional shape of the profile.
[0003] The general function of the upper die is to divert the ingot through the diversion holes on it, and to shape the inner wall of the hole of the perforated profile through the core of the upper die. The general function of the lower die is to gather the metal material flowing out of the diversion holes of the upper die through the welding chamber, and to shape the outer wall of the hole of the perforated profile through the die hole.
[0004] The operating conditions of the diverter mold are high temperature and high pressure. The mold cavity formed by the mold core and the mold hole is used to form the cross-sectional shape of the profile. At the same time, the extruded material also exerts a great reaction force on the mold core and the mold hole. After long-term use, the mold core and the mold hole are more likely to suffer from greater wear, which may lead to failure of the profile molding. If failure occurs, the entire set of molds will be scrapped, causing great waste. Summary of the invention
[0005] Aiming at the waste caused by the failure of existing die core or die hole, which leads to the scrapping of the whole set of dies, an aluminum extrusion diversion combined die is provided.
[0006] The present application provides an aluminum extrusion splitter assembly die, which is specifically implemented by the following technical solutions:
[0007] An aluminum extrusion diversion combination die comprises an upper die and a lower die, wherein the upper die comprises an upper die main body, a die core and a first mounting assembly, wherein the upper die main body is provided with a plurality of diversion holes, and a portion of the upper die main body located between adjacent diversion holes is set as a diversion bridge, one end of the diversion bridge is set as a first transition section, and the cross-sectional area of the first transition section gradually decreases in a direction away from the lower die, one end of the die core is set as a second transition section, and the cross-sectional area of the second transition section gradually increases in a direction away from the lower die, the end faces of the first transition section and the second transition section are fitted together, and the first transition section and the second transition section are detachably connected via a first mounting assembly; the lower die comprises a lower die main body, a module and a second mounting assembly, wherein an end face of the lower die main body is concavely formed with a welding chamber, the bottom face of the welding chamber is penetrated by a first tapered hole extending axially along the lower die main body, the large end of the first tapered hole is arranged toward the upper die main body, the module is penetrated by a die hole, the outer peripheral surface of the module is set as a conical surface adapted to the first tapered hole, and the module is detachably connected to the lower die main body via a second mounting assembly.
[0008] Through the above technical solution, firstly, by setting up a detachable mold core and module, when the mold core or the inner wall of the mold hole is damaged due to material extrusion, the mold core and the module can be replaced in time without replacing the entire mold, thereby reducing unnecessary waste.
[0009] Secondly, by setting the first transition section and the second transition section, when the material moves in the diverter hole, the component force of the extrusion force applied by the material to the first transition section and the second transition section will force the mold core and the diverter bridge to approach each other, thereby reducing the occurrence of the mold core detaching from the diverter bridge, that is, greatly improving the connection strength between the mold core and the diverter bridge.
[0010] Furthermore, through the cooperation between the module and the first tapered hole, when the material flows in the welding chamber, the material exerts an extrusion pressure on the surface of the module along the axial direction of the lower mold body. This extrusion pressure will force the module to be more embedded in the lower mold body and also play a centering role, thereby greatly improving the connection strength and cooperation accuracy between the module and the lower mold body.
[0011] Optionally, the first mounting assembly includes two fastening bolts, the mold core is penetrated by a first through hole, the end of the mold core away from the diversion bridge is provided with a countersunk hole, the countersunk hole is connected to the first through hole, the end face of the first transition section is provided with a first threaded hole, the fastening bolt passes through the first through hole and is threadedly connected to the first threaded hole, and the screw head of the fastening bolt is located in the countersunk hole.
[0012] Through the above technical solution, by setting the fastening bolts, the fastening bolts can quickly achieve the fixation between the mold core and the diverter bridge.
[0013] Optionally, a square block is integrally formed at one end of the module away from the upper mold body, and a square hole is provided at the small end of the first conical hole to match the square block; the second mounting assembly includes a fastening ring and a disc spring, the inner circumference of the fastening ring is set to a conical surface, the large end of the conical surface of the fastening ring is arranged toward the upper mold body, the outer circumference of the fastening ring is provided with a screw thread, and an annular step block is integrally formed at the bottom of the welding chamber, the inner circumference of the step block is provided with a second threaded hole, the second threaded hole cooperates with the screw thread, and the end face of the fastening ring is fitted and pressed against the end face of the module; a first ring groove is provided at the end of the outer circumference of the fastening ring away from the upper mold body, the disc spring is located in the first ring groove, and the elastic force of the disc spring forces the module to move in a direction away from the upper mold body.
[0014] Through the above technical solution, a fastening ring is provided, and when the fastening ring is screwed in, the end face of the fastening ring fits and presses against the end face of the module to prevent the module from detaching from the lower mold body, and through the disc spring, the disc spring can increase the pre-tightening force to reduce the fitting clearance between the screw thread and the second threaded hole, and improve the module's ability to resist detachment from the lower mold body.
[0015] Secondly, the square block and the square hole cooperate to prevent rotation, so as to ensure that the mold hole and the mold core of the module are in a relatively precise position.
[0016] Optionally, the second mounting assembly further comprises a first glass ring and a second glass ring, wherein an end of the outer circumferential surface of the fastening ring facing the upper mold body is provided with an annular first chamfer, and the first glass ring is embedded in the first chamfer; an end of the inner circumferential surface of the fastening ring away from the upper mold body is provided with an annular second chamfer, and the second glass ring is embedded in the second chamfer.
[0017] Through the above technical solution, by arranging the first glass ring and the second glass ring, the gaps between the fastening ring and the step block and the bottom surface of the welding chamber can be filled, thereby reducing the occurrence of high-pressure material overflowing into the gap. In addition, the glass ring has the characteristics of high temperature resistance and high hardness. The glass ring is difficult to be damaged by the high-pressure material and can maintain a strong gap filling effect.
[0018] Optionally, a tic-tac-toe hole is formed on the end face of the first transition section, a tic-tac-toe protrusion is integrally formed on the end face of the second transition section, the tic-tac-toe protrusion is plugged and connected to the tic-tac-toe hole, the diverter bridge is penetrated by a second through hole, the mold core is penetrated by a third through hole, the third through hole is located in the hollow area of the tic-tac-toe protrusion, and the third through hole is connected to the second through hole; the first mounting assembly includes a steel strand, a first anchor seat, a second anchor seat, an end cover, a sleeve and two groups of clips, the sleeve passes through the second through hole and the third through hole at the same time, and the outer diameter of the sleeve is equal to the inner diameters of the second through hole and the third through hole, the inner circumference of the sleeve is integrally formed with a plurality of prestressed protrusions arranged in an axially staggered manner along the sleeve, the steel strand bypasses each prestressed protrusion in turn, and the shape of the steel strand located in the sleeve is wavy; a second tapered hole is provided at the end of the second through hole away from the mold core, and the third through hole A third conical hole is provided at the end of the hole away from the diverter bridge, the large end of the second conical hole and the large end of the third conical hole are set apart, the outer circumferential surface of the first anchor seat is set as a conical surface adapted to the second conical hole, and the outer circumferential surface of the second anchor seat is set as a conical surface adapted to the third conical hole; the first anchor seat is penetrated by a fourth conical hole, and the second anchor seat is penetrated by a fifth conical hole, the large end of the fourth conical hole and the large end of the fifth conical hole are set apart, two groups of clips are respectively located in the fourth conical hole and the fifth conical hole, one group of clips includes three clips, and each clip is evenly spaced around the circumference, the steel strand passes through the central area enclosed by each clip, and the side of the clip is provided with a friction protrusion, the friction protrusion bites into the surface of the steel strand, and the steel strand is in a stretched and taut state; the end cover is welded to seal the large port of the fourth conical hole to hide the steel strand.
[0019] Through the above technical scheme, when installing the mold core, first put the sleeve with the steel strand into the second through hole to complete the assembly of the first anchor seat, the second anchor seat and the clip, and then realize the positioning of the mold core and the diversion bridge through the cooperation of the tic-tac-toe hole and the tic-tac-toe protrusion. In this process, the two ends of the steel strand pass through the second conical hole and the third conical hole respectively, and the two ends of the steel strand pass through the central area respectively surrounded by the two groups of clips, and then use the hydraulic jack to tension the steel strand, the steel strand is elastically stretched, and during the elastic retraction of the steel strand, the steel strand will drive the clip to wedge more tightly into the fourth conical hole or the fifth conical hole, and the three clips in the same group are close to each other to tightly bite the steel strand, thereby preventing the further elastic retraction of the steel strand, and fixing the steel strand so that the steel strand is in a taut state, and then cut off the excess part of the steel strand, and weld the end cover to the large port of the fourth conical hole to hide the steel strand, thereby reducing the occurrence of material flowing into the fourth conical hole.
[0020] When a new mold core needs to be replaced, a drill is used to drill through the end cover and the clip in sequence, so that the connection between one end of the steel strand and the clip fails, and then the steel strand can be taken out from the end of the mold core.
[0021] In this way, by setting up prestressed steel strands, the prestress of the steel strands forces the core and the diversion bridge to be close to each other, so as to greatly improve the connection strength of the core, and also greatly improve the lateral pressure resistance of the core, thereby reducing the extrusion and displacement deformation of the core.
[0022] The anti-rotation strength of the mold core can be improved by cooperating the tic-tac-toe holes and the tic-tac-toe protrusions.
[0023] By providing the prestressed protrusion, the shape of the steel strand located in the sleeve is made wavy, thereby increasing the length of the steel strand in the second through hole and the third through hole, so as to improve the elastic stretching amount and prestressed strength of the steel strand.
[0024] Optionally, the first mounting assembly further includes a radial stress member, which includes a fixed rod and a plurality of connecting rods, the fixed rod being coaxially arranged with the third through hole, the connecting rods being arranged at intervals along the axial direction of the fixed rod, and the axis of each connecting rod being located in different radial planes of the fixed rod, a wedge block being fixed to one end of the connecting rod, and the other end of the connecting rod being hingedly connected to the fixed rod around the axis of the fixed rod; the inner circumferential surface of the third through hole is integrally formed with wedge-shaped protrusions corresponding to each wedge block; the steel strand passes around each connecting rod in turn; when the steel strand is tightened, the steel strand abuts against the connecting rod to force the connecting rod to swing relative to the fixed rod, so that the inclined surface of the wedge block presses against the inclined surface of the wedge-shaped protrusion.
[0025] Through the above technical solution, when the steel strand is tightened, the steel strand abuts against the connecting rod to force the connecting rod to swing relative to the fixed rod, so that the inclined surface of the wedge block presses on the inclined surface of the wedge-shaped protrusion, that is, the elastic force of the steel strand is converted into a radial outward force along the third through hole. This force can resist the inward extrusion force of the material on the core, thereby reducing the extrusion concave deformation of the core surface, which is mainly aimed at the case where the core cross-section is small or thin.
[0026] Moreover, when the inward extrusion pressure of the material is too large, the inward extrusion force also forces the connecting rod to swing at a small angle through the cooperation of the wedge-shaped protrusion and the wedge-shaped block, that is, the inward extrusion force is converted into the elastic force of the steel strand, further improving the connection strength of the mold core, so as to reduce the compressive displacement of the mold core and stop the loss in time.
[0027] Optionally, a rotating ring is fixed to the end of the connecting rod, a second ring groove is formed on the outer circumference of the fixed rod, the rotating ring is rotatably sleeved on the second ring groove, and a rubber sleeve is provided on the inner circumference of the rotating ring.
[0028] Through the above technical solution, by providing the rubber sleeve, the deflection damping of the connecting rod can be increased, thereby reducing the occurrence of misalignment caused by the loosening and deviation of the connecting rod during the installation of the radial stress member into the third through hole.
[0029] Optionally, the diversion holes are provided in at least two groups, the modules and the modules are provided in at least two groups, and each group of diversion holes is provided in one-to-one correspondence with each of the mold cores and the modules.
[0030] Through the above technical solution, by utilizing the replaceable characteristics of mold cores and modules, different types of profiles can be processed in the same set of molds. In this way, according to the processing schedule of different profiles or temporary orders, molds that can process the corresponding batch quantity can be quickly assembled, which is extremely flexible and more applicable.
[0031] Optionally, the outer edges of the mating end faces of the first transition section and the second transition section are both provided with a third chamfer, and the first mounting assembly includes a third glass ring, and the third glass ring is embedded in the gap between two adjacent third chamfers.
[0032] Through the above technical solution, by setting the third glass ring, the matching gap between the first transition section and the second transition section can be filled, thereby reducing the occurrence of high-pressure material overflowing into the gap, and the glass ring has the characteristics of high temperature resistance and high hardness. The glass ring is difficult to be damaged by the high-pressure material and can maintain a strong gap filling effect.
[0033] Optionally, the cross section of the third glass ring is trapezoidal. When installing the third glass ring, the third glass ring is placed between the two third chamfers, and the two end faces of the third glass ring are respectively fitted on the inclined surfaces of the two third chamfers. At this time, there is a gap between the end face of the first transition section and the end face of the second transition section. Then, the third glass ring is heated and softened, and the upper mold body and the mold core are forced to approach each other to squeeze the softened third glass ring until the end face of the first transition section and the end face of the second transition section are fitted together. Finally, the third glass ring is cooled. When installing the second glass ring, the second glass ring is first placed on the end face of the module. , then tighten the fastening ring, the second chamfer of the fastening ring abuts against the second glass ring, at this time, there is a gap between the fastening ring and the module, then heat and soften the second glass ring, and continue to tighten the fastening ring to squeeze the softened second glass ring until the fastening ring and the module fit together, and finally cool the second glass ring; after installing the second glass ring, install the first glass ring, place the first glass ring at the first chamfer, then heat and soften the first glass ring, under the action of gravity, the liquefied part of the first glass ring flows into the gap between the outer circumference of the fastening ring and the inner circumference of the step block, and finally cool the first glass ring.
[0034] Through the above technical solution, the specific installation method of the first glass ring, the second glass ring and the third glass ring is limited, and the first glass ring, the second glass ring and the third glass ring are made to fit more tightly by heating and softening them and then applying corresponding pressure.
[0035] The beneficial effects of this application are:
[0036] 1. By setting a detachable mold core and module, when the mold core or the inner wall of the mold hole is damaged due to material extrusion, the mold core and the module can be replaced in time without replacing the entire mold, thereby reducing unnecessary waste; by setting the first transition section and the second transition section, during the movement of the material in the diversion hole, the component force of the extrusion force applied by the material to the first transition section and the second transition section will force the mold core and the diversion bridge to approach each other, thereby reducing the occurrence of the mold core being separated from the diversion bridge, that is, greatly improving the connection strength between the mold core and the diversion bridge;
[0037] 2. By providing the first glass ring, the second glass ring and the third glass ring, the gap can be filled, thereby reducing the occurrence of high-pressure material overflowing into the gap, and the specific installation method of the first glass ring, the second glass ring and the third glass ring is limited, and the first glass ring, the second glass ring and the third glass ring are made to fit more tightly by heating and softening and then applying pressure accordingly;
[0038] 3. By utilizing the replaceable features of mold cores and modules, different types of profiles can be processed in the same mold. In this way, according to the processing schedule of different profiles or the situation of temporary orders, molds that can process the corresponding batch quantity can be quickly assembled, which is highly flexible and more applicable;
[0039] 4. By setting prestressed steel strands, the prestress of the steel strands forces the mold core and the diversion bridge to be close to each other, which greatly improves the connection strength of the mold core and can also greatly improve the lateral pressure resistance of the mold core, thereby reducing the extrusion and displacement deformation of the mold core;
[0040] 5. By setting a radial stress piece, when the steel strand is tightened, the steel strand abuts against the connecting rod to force the connecting rod to swing relative to the fixed rod, so that the inclined surface of the wedge block presses on the inclined surface of the wedge-shaped protrusion, that is, the elastic force of the steel strand is converted into a radial outward force along the third through hole. This force can resist the inward extrusion force of the material on the mold core, thereby reducing the extrusion concave deformation of the surface of the mold core. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] Figure 1 It is a schematic diagram of the overall structure of Example 1.
[0042] Figure 2 yes Figure 1 Cross-sectional view along the AA direction.
[0043] Figure 3 yes Figure 1 Cross-sectional view along the BB direction.
[0044] Figure 4 yes Figure 2 A partial enlarged view of point C in the middle.
[0045] Figure 5 yes Figure 2 A partial enlarged view of point D in the middle.
[0046] Figure 6 It is a partial cross-sectional view of Example 2 for showing the coordination between the first transition section and the second transition section.
[0047] Figure 7 It is a partial cross-sectional view of Embodiment 2 for demonstrating the cooperation between the fastening ring and the module.
[0048] Figure 8 It is a schematic diagram of Example 3 for demonstrating the process of moving the mold core to fix the third glass ring.
[0049] Fig. 9 It is a top view of the mold core of Example 4.
[0050] Fig.10 It is a cross-sectional view of Example 4 for demonstrating the matching relationship between the mold core and the diverter bridge.
[0051] Fig.11 The fourth embodiment is a schematic diagram of three clips.
[0052] Fig.12 yes Fig.10 A partial enlarged view of point E in the middle.
[0053] Fig.13 Schematic diagram of the radial stress member of Example 5.
[0054] Fig.14 It is a schematic diagram of Example 5 for demonstrating the matching state between the radial stress member and the wedge-shaped protrusion.
[0055] Description of reference numerals: 10, upper mold; 101, diverter hole; 102, diverter bridge; 103, upper mold body; 105, mold core; 1051, second transition section; 1052, well-shaped protrusion; 106, first transition section; 1061, well-shaped hole; 11, fastening bolt; 111, countersunk hole; 112, first through hole; 113, first threaded hole; 12, third glass ring; 121, third chamfer; 13, steel strand; 14, first anchor seat; 15, second anchor seat; 16, clip; 161, friction protrusion; 17, sleeve; 171, prestressed protrusion; 18, end cover; 19, radial stress member; 191, fixing rod; 192, connecting rod; 193, Wedge block; 194, rotating ring; 195, second ring groove; 20, lower mold; 201, lower mold body; 202, module; 203, mold hole; 204, first tapered hole; 205, square block; 206, square hole; 207, welding chamber; 21, fastening ring; 211, screw thread; 212, second chamfer; 22, step block; 221, second threaded hole; 23, disc spring; 24, first ring groove; 25, second glass ring; 26, first glass ring; 261, first chamfer; 31, second through hole; 32, third through hole; 321, wedge-shaped protrusion; 33, second tapered hole; 34, third tapered hole; 35, fourth tapered hole; 36, fifth tapered hole. DETAILED DESCRIPTION
[0056] The embodiments of the present application are described in detail below, and examples of the embodiments are shown in the attached Figure 1-14 Shown in.
[0057] In the description of this specification, the description with reference to the terms "certain embodiments", "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials, or characteristics described in conjunction with the embodiments or examples are included in at least one embodiment or example of the present application. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.
[0058] Example 1
[0059] Example 1 discloses an aluminum extrusion splitter assembly die, such as Figure 1 , Figure 2 , Figure 3 As shown, the aluminum extrusion diversion combination die includes an upper die 10 and a lower die 20, the upper die 10 includes an upper die body 103, a die core 105 and a first mounting assembly, the upper die body 103 is penetrated by a plurality of diversion holes 101, and the portion of the upper die body 103 located between adjacent diversion holes 101 is set as a diversion bridge 102; the lower die 20 includes a lower die body 201, a module 202 and a second mounting assembly, the module 202 is penetrated by a die hole 203, the die core 105 passes through the die hole 203, and a die cavity for forming a profile is formed between the die core 105 and the inner wall of the die hole 203.
[0060] In the present embodiment, four diversion holes 101 are provided, and two diversion holes 101 form a group, that is, there are two groups of diversion holes 101, and two mold cores 105 and modules 202 are provided. One group of diversion holes 101 corresponds to one mold core 105 and one module 202, that is, the extrusion molding of two profiles can be realized in the same mold, and the two mold cores 105 and the two modules 202 can also be of different shapes, that is, the extrusion molding of two profiles can also be realized in the same mold. In other embodiments, the aluminum extrusion diversion combination mold can also have only one group of diversion holes 101, one mold core 105 and one module 202.
[0061] like Figure 4 As shown, one end of the diverter bridge 102 is set as a first transition section 106, the cross-section of the first transition section 106 is set as a rectangle, and the cross-sectional area of the first transition section 106 gradually decreases in the direction away from the lower mold 20, one end of the mold core 105 is set as a second transition section 1051, the cross-section of the second transition section 1051 is set as a rectangle, and the cross-sectional area of the second transition section 1051 gradually increases in the direction away from the lower mold 20, the end faces of the first transition section 106 and the second transition section 1051 are in contact with each other, and the first transition section 106 and the second transition section 1051 are detachably connected via a first mounting assembly.
[0062] like Figure 4 As shown, in this embodiment, the first mounting assembly includes two fastening bolts 11, and the core 105 is penetrated by first through holes 112 corresponding to the fastening bolts 11. The end of the core 105 away from the diversion bridge 102 is provided with a countersunk hole 111, and the countersunk hole 111 is connected to the first through hole 112. The end face of the first transition section 106 is provided with first threaded holes 113 corresponding to the fastening bolts 11.
[0063] The fastening bolt 11 passes through the first through hole 112 and is threadedly connected to the first threaded hole 113 , and the screw head of the fastening bolt 11 is located in the countersunk hole 111 , that is, the fastening bolt 11 is used to fix the core 105 and the diverter bridge 102 , and also facilitates subsequent disassembly.
[0064] Secondly, by setting the first transition section 106 and the second transition section 1051, when the material moves in the diversion hole 101, the component force of the extrusion force applied by the material to the first transition section 106 and the second transition section 1051 will force the core 105 and the diversion bridge 102 to approach each other, thereby reducing the occurrence of the core 105 detaching from the diversion bridge 102, that is, greatly improving the connection strength between the core 105 and the diversion bridge 102.
[0065] like Figure 2 , Figure 5 As shown, one end surface of the lower mold body 201 is recessed to form a welding chamber 207, and the bottom surface of the welding chamber 207 is penetrated by a first conical hole 204 extending axially along the lower mold body 201, the large end of the first conical hole 204 is arranged toward the upper mold body 103, and the small end of the first conical hole 204 is arranged away from the upper mold body 103, and the outer peripheral surface of the module 202 is set to be a conical surface adapted to the first conical hole 204.
[0066] Through the cooperation between the module 202 and the first tapered hole 204, when the material flows in the welding chamber 207, the material exerts an extrusion force on the surface of the module 202 along the axial direction of the lower mold body 201. The extrusion force will force the module 202 to be more embedded in the lower mold body 201 and also play a centering role, thereby greatly improving the connection strength and cooperation accuracy between the module 202 and the lower mold body 201.
[0067] In addition, a square block 205 is integrally formed at one end of the module 202 away from the upper mold body 103, and a square hole 206 adapted to the square block 205 is opened at the small end of the first tapered hole 204. The square block 205 and the square hole 206 cooperate to prevent the module 202 from rotating relative to the lower mold body 201.
[0068] like Figure 2 , Figure 5As shown, the module 202 is detachably connected to the lower mold body 201 through a second mounting assembly, specifically, the second mounting assembly includes a fastening ring 21 and a disc spring 23, the fastening ring 21 is coaxially arranged with the first tapered hole 204, the inner circumferential surface of the fastening ring 21 is set as a conical surface, the large end of the conical surface of the fastening ring 21 is set toward the upper mold body 103, and the outer circumferential surface of the fastening ring 21 is provided with a screw thread 211; the bottom of the welding chamber 207 is integrally formed with an annular step block 22, the step block 22 is coaxially arranged with the fastening ring 21, and the inner circumferential surface of the step block 22 is provided with a second threaded hole 221, the second threaded hole 221 is coaxially arranged with the fastening ring 21, and the second threaded hole 221 cooperates with the threaded hole 211, and the fastening ring 21 is tightened so that the end face of the fastening ring 21 is pressed against the end face of the module 202, thereby preventing the module 202 from detaching from the lower mold body 201, thereby completing the fixation between the module 202 and the lower mold body 201.
[0069] In addition, a first annular groove 24 is provided at one end of the outer peripheral surface of the fastening ring 21 away from the upper mold body 103. The first annular groove 24 is coaxially arranged with the fastening ring 21. The disc spring 23 is coaxially arranged with the fastening ring 21. The disc spring 23 is located in the first annular groove 24. When the fastening ring 21 is tightened, the fastening ring 21 will compress the module 202. At this time, the elastic force of the disc spring 23 forces the module 202 to move in a direction away from the upper mold body 103, so that the module 202 is pressed on the inner wall of the first conical hole 204, that is, the ability of the module 202 to resist separation from the lower mold body 201 is improved.
[0070] The implementation principle of Example 1 is: by setting a detachable core mold 105 and module 202, when the core mold 105 or the inner wall of the mold hole 203 is damaged due to material extrusion, the core mold 105 and module 202 can be replaced in time without replacing the entire set of molds, thereby reducing unnecessary waste.
[0071] Example 2
[0072] The difference between Example 2 and Example 1 is that Figure 6 As shown, the outer edges of the mating end faces of the first transition section 106 and the second transition section 1051 are both provided with a third chamfer 121, and the first mounting assembly also includes a third glass ring 12, which is a square ring and can withstand a high temperature of 600 degrees Celsius.
[0073] During installation, the third glass ring 12 is placed in the gap between two adjacent third chamfers 121 , and then the fastening bolts 11 are tightened to move the mold core 105 toward the diverter bridge 102 to embed the third glass ring 12 in the gap between two adjacent third chamfers 121 .
[0074] By providing the third glass ring 12, the matching gap between the edge of the first transition section 106 and the edge of the second transition section 1051 can be filled, thereby reducing the occurrence of high-pressure material overflowing into the gap. In addition, the third glass ring 12 has the characteristics of high temperature resistance and high hardness. The third glass ring 12 is difficult to be damaged by the high-pressure material and can maintain a strong gap filling effect.
[0075] like Figure 7 As shown, an end of the inner circumference of the fastening ring 21 away from the upper mold body 103 is provided with an annular second chamfer 212, and the annular second chamfer 212 is coaxially arranged with the fastening ring 21. An end of the outer circumference of the fastening ring 21 facing the upper mold body 103 is provided with an annular first chamfer 261, and the annular first chamfer 261 is coaxially arranged with the fastening ring 21.
[0076] The second mounting assembly also includes a first glass ring 26 and a second glass ring 25 . Both the first glass ring 26 and the second glass ring 25 are circular rings. Both the first glass ring 26 and the second glass ring 25 are coaxially arranged with the fastening ring 21 . Both the first glass ring 26 and the second glass ring 25 can withstand a high temperature of 600 degrees Celsius.
[0077] During installation, first place the second glass ring 25 on the upper end surface of the module 202, then screw on the fastening ring 21 so that the inclined surface of the second chamfer 212 of the fastening ring 21 embeds the second glass ring 25 on the module 202; then apply glue on the inclined surface of the first chamfer 261, and then place the first glass ring 26 on the inclined surface of the first chamfer 261.
[0078] The first glass ring 26 and the second glass ring 25 can fill the gaps between the fastening ring 21 and the step and the bottom surface of the welding chamber 207, respectively, thereby reducing the occurrence of high-pressure material overflowing into the gaps.
[0079] Example 3
[0080] The difference between Example 3 and Example 1 is that the installation methods of the first glass ring 26, the second glass ring 25 and the third glass are different, and the axial thickness of the first glass ring 26, the second glass ring 25 and the third glass in this embodiment is greater than the axial thickness of the first glass ring 26, the second glass ring 25 and the third glass in Example 2, and the cross-section of the third glass ring 12 is trapezoidal.
[0081] Specifically, when installing the third glass ring 12, first place the third glass ring 12 between the two third chamfers 121, and the two end surfaces of the third glass ring 12 are respectively attached to the inclined surfaces of the two third chamfers 121. At this time, there is a gap between the end surface of the first transition section 106 and the end surface of the second transition section 1051 (see Figure 8), then the third glass ring 12 is heated and softened, and the mold core 105 is forced to move close to the shunt bridge 102 by tightening the fastening bolts 11 to squeeze the softened third glass ring 12 until the end surface of the first transition section 106 and the end surface of the second transition section 1051 are in contact with each other, and finally the third glass ring 12 is cooled, that is, the third glass ring 12 is squeezed so that the gap between the third glass ring 12 and the third chamfer 121 is extremely small.
[0082] When installing the second glass ring 25, first place the second glass ring 25 on the end face of the module 202, then tighten the fastening ring 21, and the second chamfer 212 of the fastening ring 21 abuts against the second glass ring 25. At this time, there is a gap between the fastening ring 21 and the module 202. Then, heat and soften the second glass ring 25, and continue to tighten the fastening ring 21 to squeeze the softened second glass ring 25 until the fastening ring 21 fits the module 202. Finally, cool the second glass ring 25, that is, squeeze the second glass ring 25 to minimize the gap between the second glass ring 25 and the second chamfer 212. In other embodiments, when there is only one mold core 105 and only one module 202, and the module 202 is coaxial with the center line of the overall mold, the overall mold can be rotated while heating the second glass ring 25, and the centrifugal force can be used to force the second glass ring 25 to expand outward to further fit the second chamfer 212.
[0083] After the second glass ring 25 is installed, the first glass ring 26 is installed and placed at the first chamfer 261. The first glass ring 26 is then heated and softened. Under the action of gravity, the liquefied part of the first glass ring 26 flows into the gap between the outer circumference of the fastening ring 21 and the inner circumference of the step. Finally, the first glass ring 26 is cooled.
[0084] When the core mold 105 and the module 202 need to be disassembled, a sharp tool, such as a window-breaking hammer, can be used to break the first glass ring 26 , the second glass ring 25 and the third glass ring 12 , thereby facilitating the removal of the core mold 105 and the module 202 .
[0085] Example 4
[0086] The difference between Example 4 and Example 1 is that another first installation component is proposed, such as Fig. 9 , Fig.10As shown, the end surface of the first transition section 106 is provided with a tic-tac-toe hole 1061, and the end surface of the second transition section 1051 is integrally formed with a tic-tac-toe protrusion 1052, the protrusion direction of the tic-tac-toe protrusion 1052 is the axial direction of the mold core 105, and the tic-tac-toe protrusion 1052 is inserted and connected with the tic-tac-toe hole 1061. The shunt bridge 102 is penetrated by a second through hole 31, and the mold core 105 is penetrated by a third through hole 32, the third through hole 32 is located in the hollow area of the tic-tac-toe protrusion 1052, and the third through hole 32 is connected with the second through hole 31.
[0087] like Fig.10 , Fig.11 , Fig.12 As shown, the first installation assembly includes a steel strand 13, a first anchor seat 14, a second anchor seat 15, an end cover 18, a sleeve 17 and two sets of clips 16, wherein the sleeve 17 passes through the second through hole 31 and the third through hole 32 at the same time, and the outer diameter of the sleeve 17 is equal to the inner diameter of the second through hole 31 and the third through hole 32, and the inner circumference of the sleeve 17 is integrally formed with a plurality of prestressed protrusions 171 arranged axially staggered along the sleeve 17, and the steel strand 13 bypasses each prestressed protrusion 171 in turn, so that the shape of the steel strand 13 located in the sleeve 17 is wavy.
[0088] A second conical hole 33 is provided at the end of the second through hole 31 away from the mold core 105, and a third conical hole 34 is provided at the end of the third through hole 32 away from the diversion bridge 102, and the large end of the second conical hole 33 and the large end of the third conical hole 34 are arranged apart from each other; the outer peripheral surface of the first anchor seat 14 is set as a conical surface adapted to the second conical hole 33, and the outer peripheral surface of the second anchor seat 15 is set as a conical surface adapted to the third conical hole 34.
[0089] The first anchor seat 14 is penetrated by a fourth conical hole 35, and the second anchor seat 15 is penetrated by a fifth conical hole 36, and the large end of the fourth conical hole 35 and the large end of the fifth conical hole 36 are set apart, and the two groups of clips 16 are respectively located in the fourth conical hole 35 and the fifth conical hole 36, and the outer side surfaces of the clips 16 are set as conical surfaces, and the outer side surfaces of the two groups of clips 16 are respectively fitted on the inner walls of the fourth conical hole 35 and the fifth conical hole 36; a group of clips 16 includes three clips 16, and each clip 16 is evenly spaced and arranged around the circumference, that is, there is a gap between two adjacent clips 16, and the steel strand 13 passes through the central area enclosed by each clip 16, and the side of the clip 16 is provided with a friction protrusion 161, which bites into the surface of the steel strand 13.
[0090] When installing the mold core 105, first put the sleeve 17 with the steel strand 13 into the second through hole 31, and then complete the assembly of the first anchor seat 14, the second anchor seat 15 and the clip 16 in sequence, and then the mold core 105 and the diverter bridge 102 are positioned by the cooperation of the cross hole 1061 and the cross protrusion 1052. In this process, the two ends of the steel strand 13 pass through the second tapered hole 33 and the third tapered hole 34 respectively, and at the same time, the two ends of the steel strand 13 pass through the central area respectively surrounded by the two groups of clips 16, and then use the hydraulic jack to tension the two ends of the steel strand 13, forcing the steel strand 13 to stretch elastically, and during the elastic retraction of the steel strand 13, the steel strand 13 will drive The clip 16 is wedged more tightly into the fourth tapered hole 35 or the fifth tapered hole 36. During the wedging process, the three clips 16 of the same group will be guided by the conical surfaces of the fourth tapered hole 35 and the fifth tapered hole 36 to approach each other. The three clips 16 will tightly bite the steel strand 13, thereby preventing the steel strand 13 from further elastically shrinking, thereby fixing the steel strand 13 so that the steel strand 13 is in a taut state, and then the excess part of the steel strand 13 is cut off to avoid too much exposed structure of the steel strand 13 affecting the flow of materials. Finally, the end cover 18 is welded and fixed to the large port of the fourth tapered hole 35 to hide the steel strand 13, thereby reducing the occurrence of material flowing into the fourth tapered hole 35.
[0091] That is, by providing the prestressed steel strand 13, the prestress of the steel strand 13 forces the core 105 and the diversion bridge 102 to be close to each other, so as to greatly improve the connection strength of the core 105, and also greatly improve the lateral pressure resistance of the core 105, thereby reducing the extrusion and displacement deformation of the core 105.
[0092] When the core mold 105 needs to be replaced with a new one, a drill is used to drill through the end cover 18 and the clip 16 in sequence, so that the connection between one end of the steel strand 13 and the clip 16 fails, and then the steel strand 13 can be taken out from the end of the core mold 105.
[0093] Example 5
[0094] The difference between Example 5 and Example 4 is that Fig.13 , Fig.14As shown, the first mounting assembly also includes a radial stress member 19, which includes a fixed rod 191 and a plurality of connecting rods 192. In the present embodiment, there are three connecting rods 192, and the fixed rod 191 is coaxially arranged with the third through hole 32. The connecting rods 192 are arranged axially at intervals along the fixed rod 191, and the axis of each connecting rod 192 is located in a different radial plane of the fixed rod 191. A wedge block 193 is fixed to one end of the connecting rod 192, and a rotating ring 194 is fixed to the other end of the connecting rod 192. A second annular groove 195 is recessed on the outer circumference of the fixed rod 191, and the rotating ring 194 is rotatably sleeved on the second annular groove 195, so that the connecting rod 192 can swing relative to the fixed rod 191. In other embodiments, a rubber sleeve is provided on the inner circumference of the rotating ring 194 to increase the swing damping of the connecting rod 192.
[0095] The inner circumference of the third through hole 32 is integrally formed with a wedge-shaped protrusion 321 corresponding to each wedge block 193, and the wedge-shaped protrusion 321 is strip-shaped, and the length direction of the wedge-shaped protrusion 321 extends axially along the third through hole 32; the inclined surface of the wedge block 193 fits against the inclined surface of the wedge-shaped protrusion 321, and the steel strand 13 passes around each connecting rod 192 in turn.
[0096] When the steel strand 13 is tightened, the steel strand 13 abuts against the connecting rod 192 to force the connecting rod 192 to swing relative to the fixed rod 191 (the swing direction of the connecting rod 192 is shown in FIG. Fig.13 and Fig.14 The inclined surface of the wedge block 193 is pressed against the inclined surface of the wedge-shaped protrusion 321, that is, the elastic force of the steel strand 13 is converted into a radial outward force along the third through hole 32, which can resist the inward extrusion force of the material on the mold core 105, thereby reducing the extrusion and concave deformation of the surface of the mold core 105.
[0097] Although the embodiments of the present application have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations on the present application. Ordinary technicians in this field can change, modify, replace and modify the above embodiments within the scope of the present application.
Claims
1. An aluminum extrusion splitter assembly die, It is characterized in that The invention comprises an upper mold (10) and a lower mold (20), wherein the upper mold (10) comprises an upper mold body (103), a mold core (105) and a first mounting assembly, wherein the upper mold body (103) is provided with a plurality of diverter holes (101), a portion of the upper mold body (103) located between adjacent diverter holes (101) is provided as a diverter bridge (102), one end of the diverter bridge (102) is provided as a first transition section (106), the cross-sectional area of the first transition section (106) gradually decreases in a direction away from the lower mold (20), and one end of the mold core (105) is provided as a second transition section (1051), the cross-sectional area of the second transition section (1051) gradually increases in a direction away from the lower mold (20). The first transition section (106) and the second transition section (1051) are enlarged, and the end faces of the first transition section (106) and the second transition section (1051) are in contact with each other, and the first transition section (106) and the second transition section (1051) are detachably connected via a first mounting assembly; the lower mold (20) comprises a lower mold body (201), a module (202) and a second mounting assembly, wherein one end face of the lower mold body (201) is concavely formed with a welding chamber (207), the bottom face of the welding chamber (207) is penetrated by a first tapered hole (204) extending axially along the lower mold body (201), the large end of the first tapered hole (204) is arranged toward the upper mold body (103), the module (202) is penetrated by a mold hole (203), the module (202 ) is configured as a conical surface adapted to the first conical hole (204); the module (202) and the lower mold body (201) are detachably connected via a second mounting assembly; a tic-tac-toe hole (1061) is provided on the end surface of the first transition section (106); a tic-tac-toe protrusion (1052) is integrally formed on the end surface of the second transition section (1051); the tic-tac-toe protrusion (1052) and the tic-tac-toe hole (1061) are plug-connected; the diverter bridge (102) is penetrated by a second through hole (31); the mold core (105) is penetrated by a third through hole (32); the third through hole (32) is located in a hollow area of the tic-tac-toe protrusion (1052), and the third through hole (32) and the second through hole are connected. (31) connected; the first installation assembly includes a steel strand (13), a first anchor seat (14), a second anchor seat (15), an end cover (18), a sleeve (17) and two groups of clips (16); the sleeve (17) passes through the second through hole (31) and the third through hole (32) at the same time, and the outer diameter of the sleeve (17) is equal to the inner diameter of the second through hole (31) and the third through hole (32); the inner circumference of the sleeve (17) is integrally formed with a plurality of prestressed protrusions (171) arranged in an axially staggered manner along the sleeve (17); the steel strand (13) bypasses each prestressed protrusion (171) in turn, and the shape of the steel strand (13) located in the sleeve (17) is wavy;The second through hole (31) is provided with a second tapered hole (33) at one end away from the mold core (105), and the third through hole (32) is provided with a third tapered hole (34) at one end away from the diverter bridge (102). The large end of the second tapered hole (33) and the large end of the third tapered hole (34) are arranged apart from each other. The outer peripheral surface of the first anchor seat (14) is provided as a conical surface adapted to the second tapered hole (33), and the outer peripheral surface of the second anchor seat (15) is provided as a conical surface adapted to the third tapered hole (34). The first anchor seat (14) is penetrated by a fourth tapered hole (35 ), the second anchor seat (15) is penetrated by a fifth conical hole (36), the large end of the fourth conical hole (35) and the large end of the fifth conical hole (36) are arranged apart, two groups of clips (16) are respectively located in the fourth conical hole (35) and the fifth conical hole (36), one group of clips (16) includes three clips (16), each clip (16) is arranged evenly at intervals around the circumference, the steel strand (13) passes through the central area surrounded by each clip (16), the side of the clip (16) is provided with a friction protrusion (161), the friction protrusion (161) is engaged with the surface of the steel strand (13), the steel strand (13) is in a stretched and taut state; the end cover (18) is welded to block the large end of the fourth tapered hole (35) to hide the steel strand (13); the first mounting assembly also includes a radial stress member (19), the radial stress member (19) includes a fixed rod (191) and a plurality of connecting rods (192), the fixed rod (191) is coaxially arranged with the third through hole (32), the connecting rods (192) are axially spaced along the fixed rod (191), and the axis of each connecting rod (192) is located in a different radial plane of the fixed rod (191), and a wedge is fixed at one end of the connecting rod (192) The connecting rod (192) is hingedly connected to the fixing rod (191) around the axis of the fixing rod (191) by a connecting rod (192); the inner circumferential surface of the third through hole (32) is integrally formed with a wedge-shaped protrusion (321) corresponding to each wedge-shaped block (193); the steel strand (13) passes around each connecting rod (192) in sequence; when the steel strand (13) is tightened, the steel strand (13) abuts against the connecting rod (192) to force the connecting rod (192) to swing relative to the fixing rod (191), so that the inclined surface of the wedge-shaped block (193) presses against the inclined surface of the wedge-shaped protrusion (321).
2. The aluminum extrusion splitter assembly die according to claim 1, It is characterized in that The module (202) has a square block (205) integrally formed at one end away from the upper mold body (103), and the small end of the first conical hole (204) is provided with a square hole (206) adapted to the square block (205); the second mounting assembly includes a fastening ring (21) and a disc spring (23), the inner circumference of the fastening ring (21) is set as a conical surface, the large end of the conical surface of the fastening ring (21) is arranged toward the upper mold body (103), the outer circumference of the fastening ring (21) is provided with a screw thread (211), and the bottom of the welding chamber (207) is integrally formed with a square block (205); An annular step block (22) is formed, and a second threaded hole (221) is provided on the inner circumference of the step block (22), and the second threaded hole (221) cooperates with the thread (211), and the end face of the fastening ring (21) is pressed against the end face of the module (202); a first annular groove (24) is provided on the end of the outer circumference of the fastening ring (21) away from the upper mold body (103), and the disc spring (23) is located in the first annular groove (24), and the elastic force of the disc spring (23) forces the module (202) to move in a direction away from the upper mold body (103).
3. The aluminum extrusion splitter assembly die according to claim 2, It is characterized in that The second mounting assembly further comprises a first glass ring (26) and a second glass ring (25); an end of the outer circumferential surface of the fastening ring (21) facing the upper mold body (103) is provided with an annular first chamfer (261), and the first glass ring (26) is embedded in the first chamfer (261); an end of the inner circumferential surface of the fastening ring (21) away from the upper mold body (103) is provided with an annular second chamfer (212), and the second glass ring (25) is embedded in the second chamfer (212).
4. The aluminum extrusion splitter assembly die according to claim 1, It is characterized in that A rotating ring (194) is fixed at the end of the connecting rod (192), a second annular groove (195) is formed in a concave shape on the outer circumference of the fixed rod (191), the rotating ring (194) is rotatably sleeved on the second annular groove (195), and a rubber sleeve is provided on the inner circumference of the rotating ring (194).
5. The aluminum extrusion splitter assembly die according to claim 1, It is characterized in that The diversion holes (101) are provided in at least two groups, the mold cores (105) and the modules (202) are provided in at least two groups, and each group of diversion holes (101) is provided in a one-to-one correspondence with each mold core (105) and the module (202).
6. The aluminum extrusion splitter assembly die according to claim 3, It is characterized in that The outer edges of the mating end faces of the first transition section (106) and the second transition section (1051) are both provided with a third chamfer (121), and the first mounting assembly comprises a third glass ring (12), and the third glass ring (12) is embedded in the gap between two adjacent third chamfers (121).
7. The aluminum extrusion splitter assembly die according to claim 6, It is characterized in that The cross section of the third glass ring (12) is trapezoidal. When installing the third glass ring (12), the third glass ring (12) is placed between the two third chamfers (121), and the two end faces of the third glass ring (12) are respectively fitted on the inclined surfaces of the two third chamfers (121). At this time, there is a gap between the end face of the first transition section (106) and the end face of the second transition section (1051). Then, the third glass ring (12) is heated and softened, and the upper mold body (103) and the mold core (105) are forced to approach each other to squeeze the softened third glass ring (12) until the end face of the first transition section (106) and the end face of the second transition section (1051) are fitted together. Finally, the third glass ring (12) is cooled. When installing the second glass ring (25), the second glass ring (25) is first placed on the end face of the module (202), and then tightened. The fastening ring (21), the second chamfer (212) of the fastening ring (21) abuts against the second glass ring (25), at which time there is a gap between the fastening ring (21) and the module (202), then the second glass ring (25) is heated and softened, and the fastening ring (21) is continuously screwed to squeeze the second glass ring (25) in a softened state until the fastening ring (21) and the module (202) are in contact, and finally the second glass ring (25) is cooled; after the second glass ring (25) is installed, the first glass ring (26) is installed, the first glass ring (26) is placed at the first chamfer (261), and then the first glass ring (26) is heated and softened, and under the action of gravity, the liquefied part of the first glass ring (26) flows into the gap between the outer peripheral surface of the fastening ring (21) and the inner peripheral surface of the step block (22), and finally the first glass ring (26) is cooled.