Semiconductor device and method for manufacturing the same

By using a stacked structure of a diffusion barrier layer and an oxide layer to form a conductive channel on the substrate in the process of semiconductor devices, the metal wire bridging problem caused by the conductive channel is solved, the device yield is improved and the time cost is reduced.

CN118610162BActive Publication Date: 2024-11-12WUHAN XINXIN SEMICON MFG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411074484.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-07
Publication Date
2024-11-12
Estimated Expiration
2044-08-07

AI Technical Summary

Technical Problem

In the process of semiconductor devices, as the process nodes decrease, the spacing of the metal wiring layers decreases, and the conductive channels are prone to bridge adjacent metal wires, resulting in abnormal device circuit performance and reduced yield, and by reducing the design width of the conductive channel Avoiding bridging requires a lot of time to debug, which is expensive.

Method used

A metal wiring layer is formed on the substrate and covered with a diffusion barrier layer, an oxide layer and a nitride layer are stacked, and a dielectric hole is formed in the nitride layer, a second oxide layer is formed and an etched to form wiring trenches and through holes, filling The metal material forms conductive channels, and the width of the through-hole is limited by the laminated structure of the diffusion barrier layer and the oxide layer, avoiding metal wire bridging.

Benefits of technology

Effectively reduces the risk of conductive channels bridging adjacent metal wires, improves device yield, and does not need to change the design width of the through holes, reducing time costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118610162B_ABST
    Figure CN118610162B_ABST
Patent Text Reader

Abstract

The present invention relates to a semiconductor device and a manufacturing method thereof. In the manufacturing method, after forming an x-th metal wiring layer on a substrate and covering a diffusion barrier layer, a first oxide layer and a nitride layer are stacked, and a dielectric hole is formed in the nitride layer before forming a second oxide layer. In the process of etching the second oxide layer and the nitride layer, the first oxide layer in the dielectric hole region is exposed and then etched. The nitride layer can protect the covered first oxide layer, thereby reducing the risk of the first oxide layer being etched sideways and limiting the width of the hole formed in the first oxide layer. The diffusion barrier layer is exposed and etched, so that the width of the through hole formed corresponding to the dielectric hole is limited. After a conductive channel is formed in the through hole, the risk of the conductive channel bridging adjacent metal wires is reduced, and the risk of device failure caused by metal wire bridging is reduced, which helps to improve the device yield, and the manufacturing method has low time cost.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor device and a method for manufacturing the semiconductor device. Background Art

[0002] In the process of manufacturing semiconductor devices, one or more electronic components are usually formed on a substrate and covered with a dielectric layer, and then a metal interconnect structure is formed on the substrate. The metal interconnect structure includes multiple metal wiring layers isolated by dielectric materials and conductive channels connecting adjacent metal wiring layers.

[0003] However, as the semiconductor process node decreases, the spacing between metal wires in the metal wiring layer decreases. When forming a conductive channel connecting adjacent metal wiring layers, the conductive channel is likely to bridge adjacent metal wires in the lower metal wiring layer. That is, the conductive channel is not only connected to the metal wire to be contacted, but also to the surrounding metal wires, which can easily lead to abnormal device circuit performance or even device failure and reduced yield. If the metal wire bridging is avoided by reducing the design width of the conductive channel, it will take a lot of time to debug, and the time cost is high. Summary of the invention

[0004] In order to prevent the conductive channel in the metal interconnect structure from bridging adjacent metal wires, reduce the risk of device failure caused thereby, improve the device yield, and avoid increasing time cost, the present invention provides a method for manufacturing a semiconductor device and a semiconductor device.

[0005] In one aspect, the present invention provides a method for manufacturing a semiconductor device, the method comprising:

[0006] Forming an x-th metal wiring layer on the substrate and covering the diffusion barrier layer, where x is an integer greater than or equal to 1, the x-th metal wiring layer includes a metal line to be contacted for connecting the upper metal wiring layer;

[0007] Stacking a first oxide layer and a nitride layer on the diffusion barrier layer, and forming at least one dielectric hole in the nitride layer, wherein the orthographic projection of each dielectric hole on the plane of the x-th metal wiring layer only overlaps with a corresponding metal line to be contacted;

[0008] forming a second oxide layer, wherein the second oxide layer fills the dielectric hole and covers the nitride layer;

[0009] Etching the second oxide layer and the nitride layer to form a wiring groove, and etching the first oxide layer and the diffusion barrier layer below the dielectric hole at the same time, forming a through hole corresponding to the dielectric hole, which is connected to the wiring groove and exposes the metal line to be contacted, and the width of the wiring groove is greater than the width of the through hole; and

[0010] A metal material is filled in the through hole and the wiring groove, an (x+1)th metal wiring layer is formed in the wiring groove, and a conductive channel connecting the xth metal wiring layer and the (x+1)th metal wiring layer is formed in the through hole.

[0011] Optionally, the x-th metal wiring layer is embedded in a surface of a dielectric layer on the substrate, and the diffusion barrier layer covers the x-th metal wiring layer and the dielectric layer.

[0012] Optionally, etching the second oxide layer, the nitride layer, the first oxide layer and the diffusion barrier layer includes:

[0013] forming a patterned mask layer on the surface of the second oxide layer, wherein the mask layer is used to define the position of the wiring groove; and

[0014] Using the mask layer as a mask, a first etching process is used to etch the second oxide layer and the first oxide layer connected to the second oxide layer in the dielectric hole area to expose the nitride layer and the diffusion barrier layer, and then a second etching process is used to etch the nitride layer and the diffusion barrier layer to form the wiring groove and the through hole.

[0015] Optionally, the mask layer includes an anti-reflection layer stacked on the second oxide layer and a photoresist layer stacked on the second anti-reflection layer, and an opening for defining a position of the wiring groove is formed in the photoresist layer.

[0016] Optionally, the orthographic projection of the opening for defining the position of the wiring groove in the plane of the nitride layer covers at least one of the dielectric holes.

[0017] Optionally, the orthographic projection of each of the through holes on the plane of the x-th metal wiring layer falls within the range of the metal line to be contacted.

[0018] Optionally, the diffusion barrier layer includes at least one of nitrogen-doped silicon carbide (NDC) and silicon nitride.

[0019] Optionally, the width of the through hole is equal to the width of the corresponding medium hole.

[0020] In another aspect, the present invention provides a semiconductor device, comprising:

[0021] substrate;

[0022] An x-th metal wiring layer and an (x+1)-th metal wiring layer are provided on the substrate, where x is an integer greater than or equal to 1, and the x-th metal wiring layer includes a metal wire to be contacted for connecting the (x+1)-th metal wiring layer;

[0023] a diffusion barrier layer, a first oxide layer, a nitride layer, and a second oxide layer stacked in sequence from the xth metal wiring layer to the (x+1)th metal wiring layer, wherein at least one through hole exposing the corresponding metal line to be contacted is formed in the stack of the diffusion barrier layer and the first oxide layer, a wiring groove connected to the through hole is formed in the stack of the nitride layer and the second oxide layer, the (x+1)th metal wiring layer is arranged in the wiring groove, and the width of the wiring groove is greater than the width of the through hole; and

[0024] A conductive channel is provided in the through hole, wherein the conductive channel connects the xth metal wiring layer and the (x+1)th metal wiring layer.

[0025] Optionally, the diffusion barrier layer includes at least one of nitrogen-doped silicon carbide (NDC) and silicon nitride.

[0026] Optionally, at least two of the conductive paths are connected to the same metal line to be contacted.

[0027] In the manufacturing method of the semiconductor device provided by the present invention, after forming the xth metal wiring layer on the substrate and covering the diffusion barrier layer, a first oxide layer and a nitride layer are stacked, and a dielectric hole is formed in the nitride layer before forming the second oxide layer. In the process of etching the second oxide layer and the nitride layer, the first oxide layer in the dielectric hole area is also exposed and then etched. The nitride layer can protect the covered first oxide layer, thereby reducing the risk of the first oxide layer being etched sideways and limiting the width of the hole formed in the first oxide layer. After the diffusion barrier layer is exposed and etched, since the width of the hole in the first oxide layer is limited, the width of the hole formed in the diffusion barrier layer is also limited, so that the width of the through hole formed corresponding to the dielectric hole is limited, which helps to avoid the through hole exposing the metal wire around the corresponding metal wire to be contacted. After the conductive channel is formed in the through hole, the risk of the conductive channel bridging the adjacent metal wires is reduced, thereby reducing the risk of device failure caused by the bridging of the metal wires, which helps to improve the device yield. In addition, the manufacturing method does not need to change the design width of the through hole, and has low time cost.

[0028] The semiconductor device provided by the present invention comprises a diffusion barrier layer, a first oxide layer, a nitride layer and a second oxide layer which are stacked in sequence from the xth metal wiring layer to the (x+1)th metal wiring layer, wherein at least one through hole exposing a corresponding metal wire to be contacted is formed in the stack of the diffusion barrier layer and the first oxide layer, and a wiring groove connected to the through hole is formed in the stack of the nitride layer and the second oxide layer, and the nitride layer can limit the width of the through hole during the process of forming the through hole, so that the risk of the conductive channel bridging adjacent metal wires is low, the risk of device failure due to metal wire bridging is low, the device yield is high, and there is no need to change the design width of the through hole, and the time cost is low. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 It is a schematic diagram of the cross-sectional structure after the (x+1)th metal wiring layer is formed on the xth metal wiring layer using the existing process.

[0030] Figure 2 It is a schematic flow chart of a method for manufacturing a semiconductor device according to an embodiment of the present invention.

[0031] Figure 3 It is a partial plan view of a process after an x-th metal wiring layer is formed on a substrate in one embodiment of the present invention.

[0032] Figure 4 and Figure 5 Along Figure 3 Schematic diagram of the cross-sectional structure along line AA' and line BB'.

[0033] Figure 6 It is a local plan view schematically showing a dielectric hole formed in a nitride layer in one embodiment of the present invention.

[0034] Figure 7 and Figure 8 Along Figure 6 Schematic diagram of the cross-sectional structure along line AA' and line BB'.

[0035] Fig. 9 It is a partial plan view schematically showing a second mask layer formed on a substrate in one embodiment of the present invention.

[0036] Fig.10 and Fig.11 Along Fig. 9 Schematic diagram of the cross-sectional structure along line AA' and line BB'.

[0037] Fig.12 It is a partial plan view of a substrate after wiring grooves and through holes are formed in one embodiment of the present invention.

[0038] Fig.13 and Fig.14 Along Fig.12 Schematic diagram of the cross-sectional structure along line AA' and line BB'.

[0039] Fig.15 It is a partial plan view schematically showing a process after forming the (x+1)th metal wiring layer on the substrate in one embodiment of the present invention.

[0040] Fig.16 and Fig.17 Along Fig.15 Schematic diagram of the cross-sectional structure along line AA' and line BB'. DETAILED DESCRIPTION

[0041] The semiconductor device and the method for making the same of the present invention are further described in detail below in conjunction with the accompanying drawings and specific embodiments. According to the following description, the advantages and features of the present invention will be clearer. It should be understood that the drawings of the specification are all in a very simplified form and are all in non-precise proportions, which are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention. It should be noted that the order of the steps in the method presented herein is not necessarily the only order for performing these steps, some of the steps described may be omitted and / or some other steps not described herein may be added to the method. It should be understood that spatial relative terms are intended to include different orientations in use or operation in addition to the orientation of the device described in the figure. For example, if the structure in the figure is inverted or positioned in other different ways (such as rotation), the exemplary term "on..." may also include "under..." and other orientation relationships.

[0042] Reference Figure 1 In the conventional metal interconnection process, at the xth metal wiring layer M x After the oxide layer 101 is formed (x is an integer greater than or equal to 1), a diffusion barrier layer BL (such as NDC (Nitrogen doped Silicon Carbide)) is first covered, and then an oxide layer 101 is deposited. After that, a hole etching process is performed to form a through hole 10 in the oxide layer 101 corresponding to the area where the conductive channel is to be formed, exposing the diffusion barrier layer BL, and then a wiring groove for arranging a metal wiring and connecting to the through hole 10 is formed on the top of the oxide layer 101 (the extension direction of the wiring groove is parallel to Figure 1 The diffusion barrier layer BL is exposed by etching through the through hole 10, so that the through hole 10 is deepened and the xth metal wiring layer M is exposed. x The corresponding metal wire to be contacted is then filled with metal material in the through hole 10 and the wiring groove to form the (x+1)th metal wiring layer M located in the wiring groove. x+1 and the x-th metal wiring layer M formed in the through hole 10 xand the (x+1)th metal wiring layer M x+1 Conductive channel TV.

[0043] In the above-mentioned wiring groove etching process, the formation range of the wiring groove is larger than the formation range of the through hole 10 below, and the design width of the wiring groove is usually larger than the width of the through hole 10. During the etching process of forming the wiring groove, the side wall of the through hole 10 is exposed. Therefore, during the etching process of forming the wiring groove, the side wall of the through hole 10 will also be etched, resulting in that after the wiring groove is formed, the through hole 10 is widened compared to before the etching process of forming the wiring groove.

[0044] However, if Figure 1 As shown, as the process node decreases, the design spacing of the metal wires in the metal wiring layer decreases. Using the above process, the widened through hole formed not only exposes the xth metal wiring layer M x In addition to the metal wires to be exposed (i.e., the corresponding metal wires to be contacted), other metal wires are also easily exposed, resulting in that the conductive channel TV formed in the through hole 10 is easy to connect the xth metal wiring layer M x The adjacent metal wires are bridged, resulting in abnormal circuit performance of the corresponding conductive channel TV connection, which will cause device failure and reduced yield.

[0045] In the above process, although reducing the design width of the through hole 10 helps to obtain a through hole 10 with a smaller actual width, thereby reducing the conductive channel TV, the xth metal wiring layer M x However, if the actual width of the through hole 10 is too small, it will cause the xth metal wiring layer M x and the (x+1)th metal wiring layer M x+1 The resistance between them increases, affecting the device performance. If the design width of the through hole 10 is adjusted so that the actual through hole width does not cause metal wire bridging and satisfies the xth metal wiring layer M x and the (x+1)th metal wiring layer M x+1 The resistance requirement between 10 and 10 requires a lot of time for experimental debugging, which has a high time cost and affects the progress of research and development or production. In addition, if the design width of the through hole 10 is reduced, the difficulty of hole etching will increase and the yield rate will be reduced.

[0046] The method for manufacturing a semiconductor device and the semiconductor device provided by the embodiment of the present invention do not need to change the design width of the through hole, and compared with the above process, the etching process for forming the wiring groove has less influence on the width of the through hole, which can reduce the risk of device failure caused by the widening of the through hole and improve the device yield. Figures 2 to 17 A method for manufacturing a semiconductor device and a semiconductor device according to an embodiment of the present invention are described.

[0047] Reference Figure 2 In the method for manufacturing a semiconductor device according to an embodiment of the present invention, in step S1, an x-th metal wiring layer M is formed on a substrate. x and covers the diffusion barrier layer BL (refer to Figure 7 and Figure 8 ), x is an integer greater than or equal to 1, the x-th metal wiring layer M x Includes metal lines to be contacted for connecting to the upper metal wiring layer.

[0048] The substrate may be any base material used in the art for carrying semiconductor devices, such as a silicon substrate. One or more electronic components may be formed based on the substrate, and a dielectric layer may be covered on the electronic components. The electronic components may be, for example, MOS devices, sensors, memory devices, or passive devices. The connection end of the electronic component may be connected to the first metal wiring layer (i.e., the xth metal wiring layer M when x=1) through a contact plug penetrating the dielectric layer above the electronic component. x ), the first metal wiring layer may be covered by another dielectric layer and connected to the second metal wiring layer (i.e., the xth metal wiring layer M when x=2) formed on the surface of the other dielectric layer. x ) are connected by a conductive path passing through the other dielectric layer.

[0049] Forming the xth metal wiring layer M x As an example, the x-th metal wiring layer M may be formed by a dual damascene process. x and connecting the xth metal wiring layer M x The xth metal wiring layer M x The pattern can be set according to specific needs. x It may include at least one of Ti, TiN, Ta, TaN, Cu, Au, Ni, Al, Fe, Ti, Cr, Ag, Pd and Pt. In the following embodiments, the xth metal wiring layer M x For example, copper (Cu) is included. As an example, refer to Figure 3 , Figure 4 and Figure 5 , the xth metal wiring layer M x Embedded in a dielectric layer 102 formed on the substrate, the xth metal wiring layer M x It includes adjacent metal lines L1, L2 and L3 extending along a first direction OX. The metal lines L1, L2 and L3 are respectively planned to be connected to the upper metal wiring layer through different conductive channels. Therefore, the metal lines L1, L2 and L3 are all contact metal lines for connecting the upper metal wiring layer.

[0050] The diffusion barrier layer BL is used to prevent the xth metal wiring layer M x The metal to the xth metal wiring layer M x The diffusion barrier layer BL can be made of various suitable materials with this function and covered on the xth metal wiring layer M by using a suitable process. x and the surface of the dielectric layer 102. As an example, the diffusion barrier layer BL includes at least one of nitrogen-doped silicon carbide (NDC) and silicon nitride. In the following embodiments, as an example, the diffusion barrier layer BL adopts an NDC layer with a thickness ranging from 200Å to 1000Å.

[0051] Reference Figure 2 , Figure 6 , Figure 7 as well as Figure 8 In the method for manufacturing a semiconductor device according to an embodiment of the present invention, in step S2, a first oxide layer 110 and a nitride layer 120 are stacked on the diffusion barrier layer BL, and at least one dielectric hole 120a is formed in the nitride layer 120, each of the dielectric holes 120a is located in the xth metal wiring layer M x The orthographic projection of the plane only overlaps with a corresponding metal line to be contacted. Figure 7 as well as Figure 8 The dielectric hole 120a shown is located in the xth metal wiring layer M x The orthographic projection of the plane overlaps with the metal line L1, and the orthographic projection of the dielectric hole 120a may fall completely within the range of the metal line L1, or may fall partially within the range of the metal line L1 and partially outside the range of the metal line L1. It should be noted that in order to clearly distinguish the dielectric hole 120a in the xth metal wiring layer M x The position of the orthographic projection of the plane, Figure 6 The diffusion barrier layer BL and the first oxide layer 110 are not shown.

[0052] The first oxide layer 110 is, for example, silicon oxide, which can be prepared by a known process, for example, by decomposing tetraethyl orthosilicate (TEOS). The nitride layer 120 is, for example, silicon nitride. As an example, forming a dielectric hole 120a in the nitride layer 120 includes the following process: first, a patterned mask layer (i.e., a first mask layer) is formed on the surface of the nitride layer 120, and the mask layer is used to define the position of the dielectric hole 120a; then, the mask layer is used as a mask to etch the nitride layer 120 to form the dielectric hole 120a. In this embodiment, the mask layer is, for example, a patterned photoresist layer, but is not limited thereto. In one embodiment, the mask layer includes an anti-reflection layer stacked on the nitride layer 120 and a photoresist layer stacked on the anti-reflection layer, and an opening for defining the position of the dielectric hole 120a is formed in the photoresist layer. The dielectric hole 120a can be formed according to the position of the dielectric hole 120a to be formed in the x-th metal wiring layer M. x The designed dimensions of the conductive channel formed on the substrate are set.

[0053] Due to the difference in characteristics between oxide and nitride, the first oxide layer 110 and the nitride layer 120 have etching selectivity, so that in the etching process of the first oxide layer 110, the nitride layer 120 can be used as a protective layer for the first oxide layer 110. In this embodiment, the dielectric hole 120a formed in the nitride layer 120 is used to define the position of the conductive channel subsequently formed in the stack of the diffusion barrier layer BL and the first oxide layer 110, so that the orthographic projection of the dielectric hole 120a on the plane of the xth metal wiring layer Mx only overlaps with a corresponding metal line to be contacted, and when the first oxide layer 110 below is subsequently etched through the dielectric hole 120a, under the protection of the nitride layer 120, the width of the hole formed in the first oxide layer 110 is limited by the dielectric hole 120a, and the widening amount can be reduced.

[0054] Reference Figure 2 In the method for manufacturing a semiconductor device according to an embodiment of the present invention, in step S3, a second oxide layer 130 is formed (see Fig.10 as well as Fig.11 ), the second oxide layer 130 fills the dielectric hole 120a and covers the nitride layer 120. The second oxide layer 130 is, for example, silicon oxide, which can be prepared by a known process, for example, by decomposing tetraethyl orthosilicate (TEOS).

[0055] Reference Figure 2 In step S4, the second oxide layer 130 and the nitride layer 120 are etched to form a wiring groove, and the first oxide layer 110 and the diffusion barrier layer BL below the dielectric hole 120a are etched at the same time, and a through hole connected to the wiring groove and exposing the metal line to be contacted is formed corresponding to the dielectric hole 120a, and the width of the wiring groove is greater than the width of the through hole.

[0056] The wiring groove is used to set the (x+1)th metal wiring layer, and the pattern of the wiring groove can be set according to the design of the (x+1)th metal wiring layer. Fig. 9 , Fig.10 as well as Fig.11 , in step S4, first, a patterned mask layer (i.e., a second mask layer) is formed on the surface of the second oxide layer 130 to define the position of the wiring groove. As an example, the mask layer formed on the surface of the second oxide layer 130 includes an anti-reflection layer BARC stacked on the second oxide layer 130 and a photoresist layer PR stacked on the anti-reflection layer BARC, and an opening 20 for defining the position of the wiring groove is formed in the photoresist layer PR, and the orthographic projection of the opening 20 in the photoresist layer PR in the plane of the nitride layer 120 covers the range of the corresponding dielectric hole 120a. The opening 20, for example, extends along the second direction OY, and the second direction OY is, for example, perpendicular to the above-mentioned first direction OX, but is not limited thereto. In other embodiments, the second direction OY may also be the same as the first direction OX or have an angle other than 90 degrees. A plurality of the openings 20 may be formed in the photoresist layer PR, and each of the openings 20 may cover the range of one or more dielectric holes 120a. It should be noted that in order to clearly distinguish the relative positions of the openings 20 and the dielectric holes 120a, Fig. 9 The diffusion barrier layer BL, the first oxide layer 110 , the second oxide layer 130 , and the second anti-reflection layer BARC are not shown.

[0057] As an example, after a patterned mask layer is formed on the surface of the second oxide layer 130, the mask layer is used as a mask for etching. The second oxide layer 130 and the first oxide layer 110 connected to the second oxide layer 130 in the dielectric hole 120a region can be etched by a first etching process (such as an etching process suitable for etching silicon oxide) to expose the nitride layer 120 and the diffusion barrier layer BL, and then the nitride layer 120 and the diffusion barrier layer BL can be etched by a second etching process (such as an etching process suitable for etching silicon nitride and NDC) to form a Fig.12 , Fig.13 and Fig.14 The wiring trenches 30 and through-holes 40 are shown, and the mask layer is then removed.

[0058] By using the above etching process, a wiring trench is formed in the stack of the second oxide layer 130 and the nitride layer 120, and when the second oxide layer 130 and the first oxide layer 110 are etched by the first etching process, since the etching rate of the nitride layer 120 is lower than that of the second oxide layer 130 and the first oxide layer 110, the nitride layer 120 can protect the covered first oxide layer 110 to reduce the amount of side etching of the first oxide layer 110, thereby achieving control of the width of the hole formed in the first oxide layer 110. By setting a suitable thickness of the nitride layer 120, it can cover the first oxide layer 110 around the dielectric hole 120a before the diffusion barrier layer BL is exposed, so that the width of the hole formed in the first oxide layer 110 is substantially equal to the width of the dielectric hole 120a. After the diffusion barrier layer BL is exposed by the hole formed in the first oxide layer 110, the diffusion barrier layer BL and the nitride layer 120 are etched by a second etching process. Since the first oxide layer 110 and the diffusion barrier layer BL have etching selectivity, the first oxide layer 110 has a protective effect on the covered diffusion barrier layer BL, so that the width of the hole formed in the diffusion barrier layer BL can be controlled, so that the width of the hole formed in the diffusion barrier layer BL is substantially equal to the width of the dielectric hole 120a. The hole formed in the first oxide layer 110 is connected to the corresponding hole in the underlying diffusion barrier layer BL to form a through hole 40, and the through hole 40 is connected to the wiring trench 30 formed in the second oxide layer 130 and the nitride layer 120. The through hole 40 is formed in the xth metal wiring layer M x The orthographic projection of the plane falls on the corresponding metal line to be contacted (such as Fig.13 and Fig.14 The metal line L1 is shown in the figure.

[0059] In this embodiment, when etching the diffusion barrier layer BL, the nitride layer 120 is also etched. By selecting a suitable thickness and etching process, the hole formed in the diffusion barrier layer BL can expose the corresponding metal line to be contacted, and then the nitride layer 120 around the dielectric hole 120a is removed, so that the bottom surface of the wiring groove exposes the first oxide layer 110. Fig.13 and Fig.14 After the above process, a through hole 40 exposing the corresponding metal line to be contacted is formed in the stack of the diffusion barrier layer BL and the first oxide layer 110, and a wiring groove 30 connected to the corresponding through hole 40 is formed in the stack of the nitride layer 120 and the second oxide layer 130.

[0060] Reference Figure 2 , Fig.15 , Fig.16 and Fig.17 In the method for manufacturing a semiconductor device according to an embodiment of the present invention, in step S5, a metal material is filled in the through hole 40 and the wiring trench 30 to form the (x+1)th metal wiring layer M in the wiring trench 30.x+1 The through hole 40 is formed to connect the x-th metal wiring layer M x and the (x+1)th metal wiring layer M x+1 The metal material may be any suitable material, for example, at least one of Ti, TiN, Ta, TaN, Cu, Au, Ni, Al, Fe, Ti, Cr, Ag, Pd and Pt.

[0061] The metal material may be filled in the through hole 40 and the wiring groove 30 by electroplating, chemical plating or other suitable processes. As an example, in step S5, a seed layer (such as a copper seed layer) may be first formed on the inner surface of the through hole 40 and the wiring groove 30 and the surface of the second oxide layer 130, and then electroplating may be performed to deposit the metal material on the surface of the seed layer to fill the through hole 40 and the wiring groove 30 and cover the surface of the second oxide layer 130, and then a planarization process (such as chemical mechanical polishing) may be used to remove the metal material deposited on the surface of the second oxide layer 130, so that the remaining metal material is filled in the through hole 40 and the wiring groove 30.

[0062] In the method for manufacturing the semiconductor device described in the above embodiment, after forming the xth metal wiring layer Mx on the substrate and covering the diffusion barrier layer BL, the first oxide layer 110 and the nitride layer 120 are stacked, and the second oxide layer 130 is formed after forming the dielectric hole 120a in the nitride layer 120. In the process of etching the second oxide layer 130 and the nitride layer 120, the first oxide layer 110 in the dielectric hole 120a region is also exposed and etched. Since the nitride layer 120 and the first oxide layer 110 have etching selectivity, the nitride layer 120 can protect the covered first oxide layer 110, reduce the risk of the first oxide layer 110 being side-etched, and limit the width of the hole formed in the first oxide layer 110. The diffusion barrier layer BL is also etched after being exposed. Since the width of the hole in the first oxide layer 110 is limited, the width of the hole formed in the diffusion barrier layer BL is also limited to avoid being too large, so that the width of the through hole 40 formed in the first oxide layer 110 and the diffusion barrier layer BL is limited, which can reduce the risk of exposing the metal wires around the corresponding metal wires to be contacted due to widening. After the conductive channel TV is formed in the through hole 40, the risk of the conductive channel TV bridging the adjacent metal wires is reduced, thereby reducing the risk of device failure caused by metal wire bridging, which helps to improve the device yield. In addition, the manufacturing method does not need to change the design width of the through hole 40, thereby avoiding increasing the time cost.

[0063] The embodiment of the present invention also relates to a semiconductor device, which can be formed by using the method for manufacturing the semiconductor device described in the above embodiment. Fig.15 , Fig.16 and Fig.17The semiconductor device includes a substrate (not shown), an x-th metal wiring layer M disposed on the substrate x and the (x+1)th metal wiring layer M x+1 , from the xth metal wiring layer M x To the (x+1)th metal wiring layer M x+1 The diffusion barrier layer BL, the first oxide layer 110, the nitride layer 120 and the second oxide layer 130 are sequentially stacked, and the x-th metal wiring layer M is also connected. x and the (x+1)th metal wiring layer M x+1 The conductive channel TV, the xth metal wiring layer M x including a metal wiring layer M for connecting the (x+1)th metal wiring layer x+1 The metal lines to be contacted (such as metal lines L1, L2 and L3) are formed in the stack of the diffusion barrier layer BL and the first oxide layer 110, and a through hole 40 exposing the corresponding metal line to be contacted is formed, and the stack of the nitride layer 120 and the second oxide layer 130 is formed with a wiring groove 30 connected to the through hole 40, and the width of the wiring groove 30 is greater than the width of the through hole 40, wherein the (x+1)th metal wiring layer Mx+1 is formed in the wiring groove 40, and the conductive channel TV is formed in the through hole 40, and x is an integer greater than or equal to 1.

[0064] The diffusion barrier layer BL may include at least one of nitrogen-doped silicon carbide (NDC) and silicon nitride. x and the (x+1)th metal wiring layer M x+1 It may include at least one of Ti, TiN, Ta, TaN, Cu, Au, Ni, Al, Fe, Ti, Cr, Ag, Pd and Pt. Fig.17 Optionally, at least two of the conductive channels TV are connected to the same metal wire to be contacted.

[0065] In the semiconductor device of the above embodiment, the nitride layer 120 can control the width of the through hole 40 during the process of forming the through hole 40, so that the risk of the conductive channel TV bridging adjacent metal wires is low, the risk of device failure due to metal wire bridging is low, the device yield is high, and there is no need to change the design width of the through hole, so the time cost is low.

[0066] It should be noted that the embodiments in this specification are described in a progressive manner, and each part focuses on the differences from the previous part. The same and similar parts of each part can be understood by reference.

[0067] The above description is only a description of the preferred embodiment of the present invention, and is not any limitation on the scope of rights of the present invention. Any technical personnel in this field can make possible changes and modifications to the technical solution of the present invention by using the methods and technical contents disclosed above without departing from the spirit and scope of the present invention. Therefore, any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention shall fall within the protection scope of the technical solution of the present invention.

Claims

1. A method for manufacturing a semiconductor device, characterized in that: include: Forming an x-th metal wiring layer on the substrate and covering the diffusion barrier layer, where x is an integer greater than or equal to 1, the x-th metal wiring layer includes a metal wire to be contacted for connecting the upper metal wiring layer; Stacking a first oxide layer and a nitride layer on the diffusion barrier layer, and forming at least one dielectric hole in the nitride layer, wherein the orthographic projection of each dielectric hole on the plane of the x-th metal wiring layer only overlaps with a corresponding metal line to be contacted; forming a second oxide layer, wherein the second oxide layer fills the dielectric hole and covers the nitride layer; Etching the second oxide layer and the nitride layer to form a wiring groove, and etching the first oxide layer and the diffusion barrier layer below the dielectric hole at the same time, forming a through hole corresponding to the dielectric hole, which is connected to the wiring groove and exposes the metal line to be contacted, and the width of the wiring groove is greater than the width of the through hole; as well as Filling the through hole and the wiring groove with metal material, forming an (x+1)th metal wiring layer in the wiring groove, and forming a conductive channel connecting the xth metal wiring layer and the (x+1)th metal wiring layer in the through hole; Etching the second oxide layer, the nitride layer, the first oxide layer and the diffusion barrier layer comprises: forming a patterned mask layer on the surface of the second oxide layer, the mask layer being used to define the position of the wiring groove; And, using the mask layer as a mask, a first etching process is adopted to etch the second oxide layer and the first oxide layer connected to the second oxide layer in the dielectric hole area to expose the nitride layer and the diffusion barrier layer, and then a second etching process is adopted to etch the nitride layer and the diffusion barrier layer to form the wiring groove and the through hole.

2. The method according to claim 1, characterized in that: The x-th metal wiring layer is embedded in the surface of the dielectric layer on the substrate, and the diffusion barrier layer covers the x-th metal wiring layer and the dielectric layer.

3. The method according to claim 1, characterized in that: The mask layer includes an anti-reflection layer stacked on the second oxide layer and a photoresist layer stacked on the anti-reflection layer, and an opening for defining the position of the wiring groove is formed in the photoresist layer.

4. The method according to claim 3, characterized in that: The orthographic projection of the opening for defining the location of the wiring trench in the plane of the nitride layer covers at least one of the dielectric holes.

5. The method according to claim 1, characterized in that: The orthographic projection of each of the through holes on the plane of the x-th metal wiring layer falls within the range of the metal line to be contacted.

6. The method according to claim 1, characterized in that: The diffusion barrier layer includes at least one of nitrogen-doped silicon carbide and silicon nitride.

7. The method according to claim 1, characterized in that: The width of the through hole is equal to the width of the corresponding medium hole.

8. A semiconductor device, characterized in that: The semiconductor device is formed by the manufacturing method according to any one of claims 1 to 7, comprising: substrate; An x-th metal wiring layer and an (x+1)-th metal wiring layer are provided on the substrate, where x is an integer greater than or equal to 1, and the x-th metal wiring layer includes a metal wire to be contacted for connecting the (x+1)-th metal wiring layer; a diffusion barrier layer, a first oxide layer, a nitride layer, and a second oxide layer stacked in sequence from the xth metal wiring layer to the (x+1)th metal wiring layer, wherein at least one through hole exposing the corresponding metal line to be contacted is formed in the stack of the diffusion barrier layer and the first oxide layer, a wiring groove connected to the through hole is formed in the stack of the nitride layer and the second oxide layer, the (x+1)th metal wiring layer is arranged in the wiring groove, and the width of the wiring groove is greater than the width of the through hole; and A conductive channel is provided in the through hole, wherein the conductive channel connects the xth metal wiring layer and the (x+1)th metal wiring layer.

9. The semiconductor device according to claim 8, characterized in that The diffusion barrier layer includes at least one of nitrogen-doped silicon carbide and silicon nitride.

10. The semiconductor device according to claim 8, wherein At least two of the conductive paths are connected to the same metal line to be contacted.