Visual inspection method and system for bonding shell membrane to substrate

Through visual detection methods, distinguishing the diaphragm and edge positioning areas ensure that the LOGO design is in the correct position and detecting surface defects, solving the problems of low efficiency and high cost of fitting products in the prior art, and achieving efficient fitting product quality control .

CN118706849BActive Publication Date: 2024-11-15SHENZHEN WANLI TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411196043.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-11-15
Estimated Expiration
2044-08-29

AI Technical Summary

Technical Problem

In the prior art, the mounting product detection of the housing diaphragm and the substrate is difficult to detect the alignment fitting defects and subtle appearance defects, the artificial visual efficiency is low, the cost is high, and the subjectivity is strong, making it difficult to control the overall fitting product. quality.

Method used

Using visual detection method, distinguish the diaphragm into a decorative area and an edge positioning area. Through image extraction and analysis, we ensure that the LOGO design is in the correct position, and the surface appearance defects are detected when the alignment is accurate. The edge positioning area is removed using CNC process to achieve Accurate inspection and improve the quality of fittings.

Benefits of technology

Accurate inspection of diaphragm and substrate bonding products is achieved, the detection efficiency and overall quality control level is improved, the detection cost is reduced, the production efficiency is systematically improved and image analysis resources are saved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118706849B_ABST
    Figure CN118706849B_ABST
Patent Text Reader

Abstract

The present invention relates to the technical fields of casing or structural parts of electrical equipment, machine vision inspection, etc., and provides a visual inspection method and system for bonding a shell diaphragm to a substrate. By distinguishing a shell diaphragm into a diaphragm decoration area and an edge positioning area, after the shell diaphragm is aligned and fixed on a diaphragm carrier, the shell diaphragm aligned and fixed on the diaphragm carrier of a vacuum bonding machine is controlled to bond with the shell substrate on the substrate carrier of the vacuum bonding machine to obtain a bonded product of the diaphragm and the substrate; an image of the bonded product of the diaphragm and the substrate is captured to obtain an image of the bonded product, and alignment state analysis, surface appearance defect analysis, and CNC process processing are successively performed to obtain a finished product in which the diaphragm decoration area and the shell substrate are bonded, so as to achieve accurate detection of alignment and bonding defects and subtle appearance defects of the bonded product of the diaphragm and the substrate, thereby improving inspection efficiency, reducing inspection costs, and improving the overall quality control level of the bonded product.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical fields of housing or structural parts of electrical equipment, machine vision detection and the like, and in particular to a visual detection method and system for the bonding of a housing diaphragm and a substrate. Background Art

[0002] In the shell appearance design of electronic devices such as mobile phones and tablets and automotive interior parts, in order to meet consumers' demand for shell appearance, the shell is usually designed to be transparent and combined with a decorative film layer to enhance the aesthetics of the device. In the prior art, the combination of the shell membrane and the substrate adopts vacuum bonding technology. The vacuum bonding machine controls the bonding of multiple decorative films fixed on the decorative film carrier with multiple shell substrates fixed on the substrate carrier to achieve batch bonding of membranes and substrates. In the specific bonding process, due to the lamination of the membrane and the substrate, heating, the material of the membrane and the substrate, etc., the bonded product after vacuum bonding may have surface appearance defects, such as bubbles, wrinkles and other appearance defects, and there may be alignment defects such as lamination offset, such as the pattern, text and other LOGO on the decorative film is not aligned to the correct position of the shell substrate. To solve these problems, the prior art mainly uses manual visual inspection, but manual visual inspection has a strong subjectivity, which is not conducive to the overall quality control of the bonded product, especially alignment defects and subtle appearance defects, which are difficult to detect by manual visual inspection. Moreover, manual visual inspection also has problems in terms of efficiency and cost, such as low efficiency and high cost.

[0003] In summary, in the prior art, the inspection technology for laminating products between diaphragms and substrates has technical problems such as alignment defects and subtle appearance defects that are difficult to detect with human eyes, low efficiency, high cost, and strong subjectivity of manual visual inspection, which is not conducive to the overall quality control of the laminated products. Summary of the invention

[0004] In view of the shortcomings of the above-mentioned prior art, the present invention provides a visual inspection method and system for the bonding of a shell diaphragm and a substrate, so as to accurately detect the alignment and bonding defects and subtle appearance defects of the bonded products of the diaphragm and the substrate, improve the inspection efficiency, reduce the inspection cost, and improve the overall quality control level of the bonded products.

[0005] In a first aspect, the present invention provides a method for visually inspecting the bonding between a shell membrane and a substrate, comprising:

[0006] The shell membrane is divided into a membrane decoration area and an edge positioning area, wherein the membrane decoration area is used for printing decorative effects, and the decorative effects include LOGO design; the edge positioning area is used for alignment and fixation with the membrane carrier, and when the edge positioning area is accurately aligned with the membrane carrier, the LOGO design is in the correct position required for lamination with the shell substrate;

[0007] After the shell film is aligned and fixed on the film carrier, the shell film aligned and fixed on the film carrier of the vacuum laminating machine is controlled to be laminated with the shell substrate on the substrate carrier of the vacuum laminating machine to obtain a laminated product of the film and the substrate;

[0008] The laminated product of the diaphragm and the substrate is imaged to obtain an image of the laminated product, the alignment status of the edge positioning area and the diaphragm carrier in the laminated product image is analyzed, and when the edge positioning area and the diaphragm carrier are accurately aligned, the surface appearance defects of the laminated product of the diaphragm and the substrate in the laminated product image are analyzed, and when the laminated product of the diaphragm and the substrate does not have surface appearance defects in the laminated product image, the laminated product of the diaphragm and the substrate without surface appearance defects is subjected to CNC process processing to remove the edge positioning area, so as to obtain a finished product in which the diaphragm decorative area is laminated to the shell substrate.

[0009] In a second aspect, the present invention provides a visual inspection system for bonding a shell membrane to a substrate, comprising:

[0010] A camera device is used to capture an image of the laminated product of the film and the substrate to obtain an image of the laminated product;

[0011] A control host is connected and communicated with the camera device to run the visual inspection method for the bonding between the shell membrane and the substrate;

[0012] A vacuum laminating machine is connected and communicated with the control host, and is used for laminating the shell substrate and the shell membrane under the control of the control host.

[0013] Compared with the prior art, the present invention has the following beneficial effects:

[0014] The present invention provides a visual inspection method and system for the bonding of a shell membrane to a substrate, wherein the shell membrane is distinguished into a membrane decoration area and an edge positioning area, wherein the membrane decoration area is used for printing a decorative effect, and the decorative effect includes a LOGO design; the edge positioning area is used for alignment and fixation with a membrane carrier, and when the edge positioning area and the membrane carrier are accurately aligned, the LOGO design is in the correct position required for bonding with the shell substrate; after the shell membrane is aligned and fixed to the membrane carrier, the shell membrane aligned and fixed on the membrane carrier of a vacuum bonding machine is controlled to bond with the shell substrate on the substrate carrier of the vacuum bonding machine to obtain a bonded product of the membrane and the substrate; an image of the bonded product of the membrane and the substrate is captured to obtain a To the image of the bonded product, analyze the alignment state of the edge positioning area and the diaphragm carrier in the image of the bonded product, and when the edge positioning area and the diaphragm carrier are accurately aligned, analyze the surface appearance defects of the bonded product of the diaphragm and the substrate in the image of the bonded product, and when there are no surface appearance defects of the bonded product of the diaphragm and the substrate in the image of the bonded product, perform CNC process on the bonded product of the diaphragm and the substrate without surface appearance defects to remove the edge positioning area, obtain the finished product in which the diaphragm decorative area is bonded to the shell substrate, and accurately detect the alignment and bonding defects and subtle appearance defects of the bonded product of the diaphragm and the substrate, improve the detection efficiency, reduce the detection cost, and improve the overall quality control level of the bonded product. At the same time, the present invention first analyzes the alignment state, and then analyzes the appearance defects of the bonded product when the alignment is accurate, and then enters the CNC process when the appearance of the bonded product is compliant, which not only systematically improves production efficiency, but also saves image analysis resources. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] The drawings described herein are used to provide a further understanding of the present invention and constitute a part of the present invention. The exemplary embodiments of the present invention and their description are used to explain the present invention and do not constitute an improper limitation of the present invention. Some specific embodiments of the present invention will be described in detail in an exemplary and non-restrictive manner with reference to the drawings. The same reference numerals in the drawings indicate the same or similar components or parts. It should be understood by those skilled in the art that these drawings are not necessarily drawn to scale. In the drawings:

[0016] Figure 1 It is a schematic flow chart of a method for visually inspecting the bonding between a shell diaphragm and a substrate according to an embodiment of the present invention;

[0017] Figure 2 This is a schematic diagram of the structure of a housing diaphragm according to an embodiment of the present invention;

[0018] Figure 3 It is a schematic diagram of the architecture of a visual inspection system for bonding a shell diaphragm to a substrate according to an embodiment of the present invention. DETAILED DESCRIPTION

[0019] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiment of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiment of the present invention. Obviously, the described embodiment is only an embodiment of a part of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work should fall within the scope of protection of the present invention.

[0020] Embodiment 1

[0021] See also Figure 1-Figure 3 This embodiment provides a visual inspection method for the bonding between a shell membrane and a substrate, including step S101, step S102 and step S103.

[0022] S101, the shell membrane is divided into a membrane decoration area and an edge positioning area, the membrane decoration area is used for printing decorative effects, and the decorative effects include LOGO design; the edge positioning area is used for alignment and fixation with the membrane carrier, and when the edge positioning area is accurately aligned with the membrane carrier, the LOGO design is in the correct position required for lamination with the shell substrate;

[0023] S102, after the shell film is aligned and fixed on the film carrier, controlling the shell film aligned and fixed on the film carrier of the vacuum laminating machine to be laminated with the shell substrate on the substrate carrier of the vacuum laminating machine to obtain a laminated product of the film and the substrate;

[0024] S103, capturing an image of the laminated product of the diaphragm and the substrate to obtain an image of the laminated product, analyzing the alignment state of the edge positioning area and the diaphragm carrier in the laminated product image, and when the edge positioning area and the diaphragm carrier are accurately aligned, analyzing the surface appearance defects of the laminated product of the diaphragm and the substrate in the laminated product image, and when there are no surface appearance defects in the laminated product of the diaphragm and the substrate in the laminated product image, performing CNC process on the laminated product of the diaphragm and the substrate without surface appearance defects to remove the edge positioning area, and obtain a finished product in which the diaphragm decoration area is laminated to the shell substrate. The surface appearance defects of the laminated product of the diaphragm and the substrate in the laminated product image include bubble appearance defects, wrinkle appearance defects, scratch appearance defects, and color difference appearance defects.

[0025] It should be noted that in step S101, by distinguishing between the diaphragm decoration area and the edge positioning area, it is clear which areas of the shell diaphragm are used for positioning and which areas are used for decoration, thereby reducing interference factors during image analysis, making the analysis of alignment status and appearance defects clearer and more focused, and saving computing resources for image analysis. In addition, the shell diaphragm is divided into a diaphragm decoration area and an edge positioning area. The former is used to display decorative effects such as LOGO, and the latter is used for precise alignment with the diaphragm carrier. Through this partition design, it is ensured that the LOGO is in the correct position during the alignment process, avoiding product appearance problems caused by misalignment between the diaphragm and the carrier or substrate.

[0026] In step S102, after the membrane and the carrier are aligned and fixed, the membrane and the substrate are bonded by controlling the vacuum bonding machine. Under the condition that the shell membrane is divided into a membrane decoration area and an edge positioning area, and the edge positioning area is used for alignment and fixing with the membrane carrier, the feeding process of the shell membrane will be limited by the edge positioning area, so that the edge positioning area of ​​the shell membrane and the membrane carrier are aligned as accurately as possible, so that the LOGO design is in the correct position required for bonding with the shell substrate, and the position deviation defect of the LOGO design bonding with the shell substrate is reduced.

[0027] It should be noted that although the shell diaphragm is aligned and fixed with the diaphragm carrier during loading, during the vacuum bonding process, due to factors such as pressure, temperature changes, material properties (such as the elasticity of the diaphragm, the surface roughness of the substrate), mechanical wear, and cumulative process errors, the diaphragm may be slightly displaced, causing the position deviation of the LOGO design. The position deviation defect of the LOGO design caused by this slight displacement is difficult to be found by manual visual inspection, resulting in a decrease in the quality of the bonded product between the diaphragm and the substrate. In step S103, the image of the bonded product of the diaphragm and the substrate is captured to obtain an image of the bonded product, and the alignment state of the edge positioning area and the diaphragm carrier in the bonded product image is analyzed, so as to find the position deviation defect of the edge positioning area and the diaphragm carrier through machine vision detection. Among them, the image analysis of the alignment state is relatively simple, and it is only necessary to judge the alignment of the edge positioning area and the carrier. The image processing algorithm involved in this analysis is less complex, and image processing algorithms such as edge detection, contour matching or template matching can be used to confirm whether the diaphragm is in the correct position. Since the analysis of the alignment state is less complex, this step can be completed quickly and provides a basis for the subsequent surface appearance defect analysis. It should also be noted that in step S103, the image analysis strategy is carried out in steps, that is, the alignment state analysis is performed first, and then the surface appearance defect analysis is performed. This step-by-step strategy ensures that more complex appearance defect analysis is performed only when the alignment is accurate, thereby reducing unnecessary computing burden, optimizing resource usage, and improving overall detection efficiency. The image analysis of surface appearance defects involves the detection of subtle defects in the image, such as the detection of surface appearance defects such as bubble appearance defects, wrinkle appearance defects, scratch appearance defects, and color difference appearance defects that appear on the surface of the laminated product of the diaphragm and the substrate. The detection of these surface appearance defects requires the application of more complex image processing algorithms, such as high-resolution image acquisition, color and texture analysis, machine learning classification, etc., which requires a large amount of computing resources. In step S103, by first ensuring that the alignment state is accurate and then performing surface appearance defects, the waste of image analysis resources can be avoided and the efficiency of visual inspection can be improved.

[0028] It should be noted that in step S103, the laminated product of the diaphragm and the substrate without surface appearance defects is processed by CNC process to remove the edge positioning area, and obtain the finished product in which the diaphragm decorative area is laminated with the shell substrate, thereby improving the overall quality level of the laminated finished product. Among them, the CNC (Computer Numerical Control) process is an automated processing technology controlled by a computer, which can be used for precise cutting, drilling, milling, engraving and other processing operations on materials. In this embodiment, during the early alignment and lamination process of the shell diaphragm, the edge positioning area is used to align and fix with the diaphragm carrier to ensure that the diaphragm decorative area can be accurately laminated to the predetermined position of the shell substrate. However, in the final product, the edge positioning area is not required and may affect the appearance or function of the product. Therefore, by removing the edge positioning area through the CNC process, a finished product can be obtained in which only the diaphragm decorative area is laminated with the shell substrate. This step ensures the consistency of the appearance and function of the finished product. In step S103, the CNC process is only used to process products that have been confirmed to have no surface appearance defects, which means that only qualified products will enter the CNC process, avoiding unnecessary processing of unqualified products, thereby saving production resources and reducing costs.

[0029] In some preferred embodiments, when the diaphragm decorative area is printed with a decorative effect including the LOGO design, the edge positioning area prints the LOGO positioning point; the diaphragm carrier is provided with a diaphragm carrier positioning point for aligning with the LOGO positioning point. Further, when the shell diaphragm is aligned and fixed to the diaphragm carrier, the LOGO positioning point is controlled to be aligned with the diaphragm carrier positioning point by plus or minus 2 wires. It should be noted that in this embodiment, by setting the LOGO positioning point in the edge positioning area and setting the corresponding positioning point on the diaphragm carrier, more precise alignment control can be achieved. The LOGO design is usually the most important part of the product appearance, and its position deviation may cause serious visual and quality problems. With the assistance of the LOGO positioning point, the position of the LOGO design can be fine-tuned to ensure the accuracy of its final position and reduce the position deviation of the LOGO on the substrate. In actual production, small alignment errors may accumulate and cause inaccurate LOGO position of the final product. By introducing an alignment mechanism between the LOGO positioning point and the diaphragm carrier positioning point, this error can be controlled within the range of plus or minus 2 silks (i.e. 0.02 mm). This high-precision requirement can significantly reduce the error in the alignment process and ensure the accuracy of the final fitting position of the LOGO on the shell substrate. It should be noted that the setting of the LOGO positioning point not only helps with mechanical alignment, but also provides a clear reference for subsequent image analysis. When performing image detection, the LOGO positioning point can be used as a standard reference to determine whether the relative position of the LOGO design and the substrate is accurate. If the LOGO positioning point and the diaphragm carrier positioning point are precisely aligned during the alignment process, it will be easier to detect and determine whether the final position of the LOGO is correct.

[0030] In some preferred embodiments, when the edge positioning area deviates from the film carrier, it is determined that the LOGO design is not in the correct position required for bonding with the shell substrate, the surface appearance defects of the bonded product of the film and the substrate in the bonded product image are stopped from being analyzed, and a LOGO design alignment deviation alarm is issued. It should be noted that alignment accuracy is a prerequisite for ensuring the correct bonding of the LOGO design. If the edge positioning area deviates from the alignment of the film carrier, the LOGO design will inevitably fail to align correctly. Therefore, when the alignment deviation is detected, it is necessary to first ensure that the LOGO design is in the correct position before performing subsequent appearance defect detection. This priority order can prevent the waste of resources on products that have already had alignment deviations. Image analysis of surface appearance defects involves complex image processing algorithms and a large amount of computing resources. If the surface appearance defect analysis is continued when the LOGO design has deviated, it will not only not help improve product quality, but also waste a large amount of computing resources. Therefore, stopping the appearance defect analysis immediately after detecting the alignment deviation can effectively save resources and improve system efficiency. Issuing a LOGO design alignment deviation alarm can promptly remind the operator that there are problems in the current production process. Such immediate feedback helps to quickly find and solve problems and prevent more defective products. Correcting deviations in production in a timely manner can reduce the production of defective products, thereby improving the quality and efficiency of the overall production line. If the deviation of the logo alignment is ignored and the surface appearance defect detection is continued, it may lead to misjudgment or more complicated problems. For example, a product with inaccurate logo alignment may be judged as a defective product due to alignment problems even if the surface appearance is flawless. Stopping the detection and issuing an alarm can avoid these misjudgments and reduce unnecessary rework or re-testing.

[0031] In some preferred embodiments, when the laminated product of the film and the substrate has a surface appearance defect in the laminated product image, the CNC process for the laminated product of the film and the substrate with the surface appearance defect is stopped, and a surface appearance defect alarm is issued. It should be noted that the CNC process is a precision machining process, which usually involves time-consuming and consumable cutting operations. If CNC machining is continued when surface appearance defects already exist, not only time and resources will be wasted, but the finished product after machining may still fail to meet quality requirements. By stopping the CNC process when surface appearance defects are detected, unnecessary processing of defective products can be avoided, saving costs and time. By promptly identifying and eliminating laminated products with surface appearance defects, the defective product processing time on the production line can be reduced. Stopping further processing of defective products can concentrate resources on processing qualified products and improve production efficiency.

[0032] In some preferred embodiments, the shell diaphragm fixed on the diaphragm carrier of the vacuum laminating machine is controlled to be laminated with the shell substrate on the substrate carrier of the vacuum laminating machine to obtain a laminated product of the diaphragm and the substrate, including: classifying the material type of the shell substrate to obtain shell substrates of different material types; classifying the material type of the shell diaphragm to obtain shell diaphragms of different material types; configuring vacuum laminating control parameters of the substrate and the diaphragm according to the shell substrates of different material types and the shell diaphragms of different material types, the vacuum laminating control parameters of the substrate and the diaphragm reflecting the corresponding selection of different types of substrates and different types of diaphragms during vacuum laminating; after applying adhesive between the shell substrates of different material types and the shell diaphragms, according to the vacuum laminating control parameters, the vacuum laminating machine is controlled to laminate the shell substrates of different material types and the shell diaphragms according to the vacuum laminating control parameters to obtain a laminated product of the diaphragm and the substrate. Among them, the shell substrates of different material types include polymer shell substrates, inorganic shell substrates and metal shell substrates. The inorganic material shell substrate includes a glass fiber shell substrate and a carbon fiber shell substrate; the metal material shell substrate includes an aluminum alloy shell substrate and a magnesium alloy shell substrate. Shell diaphragms of different material types include: polyolefin shell diaphragms, acrylonitrile-butadiene-styrene copolymer shell diaphragms, and polyethylene terephthalate copolymer shell diaphragms. It should be noted that different types of materials have significant differences in physical and chemical properties, such as thermal expansion coefficient, surface energy, flexibility, strength, etc. These differences will directly affect the bonding quality during the vacuum bonding process. For example, metal materials (such as aluminum alloys, magnesium alloys) and polymer materials (such as polyolefins) may exhibit different expansion or contraction characteristics during heating or cooling, resulting in defects such as uneven bonding, warping or bubbles. Therefore, by classifying the materials and adjusting the vacuum bonding control parameters according to the characteristics of different materials, the best bonding effect can be ensured under different material combinations. In addition, there are differences in adhesive selection and coating processes between different materials. For example, the bonding between polymers and inorganic materials requires specific adhesives and coating processes to ensure bonding strength and durability. Metal materials require different types of adhesives to prevent oxidation or corrosion. During the vacuum bonding process, the settings of parameters such as vacuum degree, temperature, pressure and time are crucial to the bonding quality. Different materials have different sensitivities to these parameters. For example, some polymer materials require higher temperatures and lower vacuum degrees, while metal materials require higher vacuum degrees and lower temperatures. By configuring the corresponding bonding control parameters according to the material type, it can ensure that each material combination can be bonded under optimal conditions, thereby improving the overall quality of the bonded product.

[0033] In some further preferred embodiments, when the vacuum laminating machine is laminating the shell substrate of different material types and the shell diaphragm of different material types, it includes: heating and softening the shell diaphragm according to the vacuum laminating control parameters to obtain a softened shell diaphragm; laminating and holding the softened shell diaphragm according to the vacuum laminating control parameters to obtain a shell diaphragm after pressure-holding lamination; baking the shell diaphragm after pressure-holding lamination according to the vacuum laminating control parameters to obtain a completed shell diaphragm. Wherein, when the material type of the shell substrate is a polymer shell substrate and the material type of the shell diaphragm is a polyolefin shell diaphragm, the vacuum laminating control parameters include a heating softening temperature of 80 degrees, a heating softening time of 30 seconds, a laminating holding temperature of 90-100 degrees, a laminating holding time of 90 seconds, a baking temperature of 90 degrees, and a baking time of 3 minutes. In addition, when the material type of the shell substrate is an inorganic shell substrate and the material type of the shell diaphragm is a polyolefin shell diaphragm, the vacuum lamination control parameters include a heating softening temperature of 120 degrees, a heating softening time of 30 seconds, a lamination holding temperature of 120 degrees, a lamination holding time of 90 seconds, a baking temperature of 130 degrees, and a baking time of 25-30 minutes. In addition, when the material type of the shell substrate is a metal shell substrate and the material type of the shell diaphragm is a polyolefin shell diaphragm, the vacuum lamination control parameters include a heating softening temperature of 120 degrees, a heating softening time of 30 seconds, a lamination holding temperature of 120 degrees, a lamination holding time of 90 seconds, a baking temperature of 130 degrees, and a baking time of 25-30 minutes. It should be noted that the physical and chemical behaviors of different materials during heat treatment vary greatly. For example, the thermal expansion coefficient, melting point, flexibility, thermal conductivity and other properties of polymers, inorganic materials and metal materials are different. In order to obtain the best bonding effect during the vacuum bonding process, precise temperature and time control is required according to the characteristics of different materials. Among them, the softening and bonding temperatures of high molecular polymers (such as polyolefins) are low, so they need to be heated, softened and held at a relatively low temperature (such as 80-100 degrees) to avoid excessive softening or decomposition of the material. Inorganic materials (such as glass fiber or carbon fiber) and metal materials (such as aluminum alloy or magnesium alloy) require higher bonding temperatures (such as 120 degrees and above) because these materials have higher heat capacity and different thermal conductivity, and higher temperatures are required to ensure good adhesion between the diaphragm and the substrate. By heating and softening the shell diaphragm, the molecular chains of the material can move under heating conditions, making it easier to form a strong bond with the substrate. The holding process further promotes the close fit of the softened diaphragm and the substrate by applying pressure, preventing air from remaining, and ensuring that the bonding is as bubble-free and warping-free as possible. It should be noted that different materials have different thermal expansion coefficients. If heated too quickly, thermal stress may be generated between the materials, which may lead to peeling or material damage at the interface.Therefore, when setting the temperature and time, it is necessary to ensure that the temperature gradient during heating and cooling is gentle to reduce the generation of thermal stress. For high molecular polymers, short heating and holding times, as well as relatively mild baking temperatures, are required to avoid thermal degradation of the material. For inorganic and metal materials, although they are more resistant to high temperatures, they still require a longer baking time to gradually release thermal stress and ensure the stability and long-term reliability of the bonding. It is also important to note that the optimization of processing parameters for different material combinations can ensure consistency and high-quality output under different production conditions. By setting specific vacuum bonding control parameters for each material combination, the production line can handle the bonding of different materials in a standardized manner, reduce human errors, improve production efficiency, and ensure the quality consistency of the finished product. It is also important to note that setting the appropriate baking temperature and time for different material combinations can fully cure the adhesive and release residual stress, thereby improving the durability and stability of the bonded product. For high molecular polymers, since their adhesives are usually cured at lower temperatures, relatively short baking times and temperatures are required. Inorganic and metal materials require longer times and higher temperatures to ensure that the adhesive is fully cured and achieves the best bonding effect.

[0034] In some further preferred embodiments, when the laminated product of the film and the substrate in the laminated product image has a surface appearance defect, the cause of the surface appearance defect is analyzed. If the surface appearance defect is caused by uneven softening of the film, the heating softening temperature is reduced or increased, or the heating time is extended / shortened to ensure that the film softens more evenly. For example, for a combination of a polymer substrate and a polyolefin film, the heating softening temperature can be adjusted from 80 degrees to 85 degrees to improve the flexibility of the film, thereby reducing surface defects. If the surface appearance defect is caused by uneven pressure or insufficient holding time, the holding temperature and time are adjusted. For example, for a metal substrate, the holding temperature can be appropriately increased to 125 degrees, or the holding time can be extended to 120 seconds to ensure better bonding. If the surface appearance defect is caused by insufficient curing of the adhesive, the baking temperature and time are adjusted. For example, for an inorganic material substrate, the baking time can be extended to 35 minutes to ensure that the adhesive is completely cured. If the surface appearance defect is caused by an adhesive, the type of adhesive is replaced or optimized. For example, for inorganic materials and polyolefin films, adhesives with stronger adhesion and better heat resistance can be selected to improve the bonding quality.

[0035] Embodiment 2

[0036] See also Figure 1-Figure 3This embodiment provides a visual inspection system for bonding a shell film to a substrate, comprising: a camera device, a control host, and a vacuum bonding machine. The camera device captures an image of a bonded product of the film and the substrate to obtain an image of the bonded product; the control host is connected to the camera device for communication and runs the visual inspection method for bonding a shell film to a substrate as described in any of the above embodiments; the vacuum bonding machine is connected to the control host for communication and is used to bond the shell substrate and the shell film under the control of the control host. It should be noted that, in the present embodiment, the shell membrane is divided into a membrane decoration area and an edge positioning area, the membrane decoration area is used for printing decorative effects, and the decorative effects include LOGO design; the edge positioning area is used for alignment and fixation with the membrane carrier, and when the edge positioning area and the membrane carrier are accurately aligned, the LOGO design is in the correct position required for bonding with the shell substrate; after the shell membrane is aligned and fixed to the membrane carrier, the shell membrane aligned and fixed on the membrane carrier of the vacuum bonding machine is controlled to bond with the shell substrate on the substrate carrier of the vacuum bonding machine to obtain a bonded product of the membrane and the substrate; an image of the bonded product of the membrane and the substrate is captured to obtain an image of the bonded product, Analyze the alignment state of the edge positioning area and the diaphragm carrier in the laminated product image, and when the edge positioning area and the diaphragm carrier are accurately aligned, analyze the surface appearance defects of the laminated product of the diaphragm and the substrate in the laminated product image, and when there are no surface appearance defects of the laminated product of the diaphragm and the substrate in the laminated product image, perform CNC process on the laminated product of the diaphragm and the substrate without surface appearance defects to remove the edge positioning area, obtain the finished product in which the diaphragm decorative area is bonded to the shell substrate, and accurately detect the alignment and bonding defects and subtle appearance defects of the laminated product of the diaphragm and the substrate, improve the detection efficiency, reduce the detection cost, and improve the overall quality control level of the laminated product. At the same time, the present invention first analyzes the alignment state, and then analyzes the appearance defects of the laminated product when the alignment is accurate, and then enters the CNC process when the appearance of the laminated product complies with the standards, which not only systematically improves production efficiency, but also saves image analysis resources.

[0037] It should be pointed out that the above embodiments are only preferred specific implementation modes of the present invention, and the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by any technician familiar with the technical field within the technical scope disclosed by the present invention should be covered within the protection scope of the present invention. The protection scope of the present invention should be based on the protection scope of the claims.

Claims

1. A visual inspection method for the adhesion between a shell membrane and a substrate, characterized in that: include: The shell membrane is divided into a membrane decoration area and an edge positioning area, wherein the membrane decoration area is used for printing decorative effects, and the decorative effects include LOGO design; the edge positioning area is used for alignment and fixation with the membrane carrier, and when the edge positioning area is accurately aligned with the membrane carrier, the LOGO design is in the correct position required for lamination with the shell substrate; After the shell film is aligned and fixed on the film carrier, the shell film aligned and fixed on the film carrier of the vacuum laminating machine is controlled to be laminated with the shell substrate on the substrate carrier of the vacuum laminating machine to obtain a laminated product of the film and the substrate; The laminated product of the diaphragm and the substrate is imaged to obtain an image of the laminated product, and the alignment state of the edge positioning area and the diaphragm carrier in the laminated product image is analyzed, so as to find the position deviation defect between the edge positioning area and the diaphragm carrier through machine vision detection; and when the edge positioning area and the diaphragm carrier are accurately aligned, the surface appearance defects of the laminated product of the diaphragm and the substrate in the laminated product image are analyzed, and when the laminated product of the diaphragm and the substrate does not have surface appearance defects in the laminated product image, the laminated product of the diaphragm and the substrate without surface appearance defects is subjected to CNC process processing to remove the edge positioning area, so as to obtain the alignment state of the diaphragm decorative area and the shell. The finished product after the substrate is bonded; when the decorative effect including the LOGO design is printed in the film decorative area, the LOGO positioning point is printed in the edge positioning area; the film carrier is provided with a film carrier positioning point for aligning with the LOGO positioning point; when performing image detection, the LOGO positioning point is used as a standard reference to determine whether the relative position of the LOGO design and the substrate is accurate; when the edge positioning area deviates from the alignment of the film carrier, it is determined that the LOGO design is not in the correct position required for bonding with the shell substrate, the surface appearance defects of the bonded product of the film and the substrate in the bonded product image are stopped to be analyzed, and a LOGO design alignment deviation alarm is issued; The shell diaphragm fixed on the diaphragm carrier of the vacuum laminating machine is controlled to be laminated with the shell substrate on the substrate carrier of the vacuum laminating machine to obtain a laminated product of the diaphragm and the substrate, including: classifying the material type of the shell substrate to obtain shell substrates of different material types; classifying the material type of the shell diaphragm to obtain shell diaphragms of different material types; configuring vacuum laminating control parameters of the substrate and the diaphragm according to the shell substrates of different material types and the shell diaphragms of different material types, the vacuum laminating control parameters of the substrate and the diaphragm reflecting the corresponding selection of different types of substrates and different types of diaphragms during vacuum laminating; After the adhesive is applied between the shell diaphragms, the vacuum laminating machine is controlled to laminate the shell substrate and the shell diaphragm of different material types according to the vacuum laminating control parameters to obtain a laminated product of the diaphragm and the substrate; the shell substrates of different material types include polymer shell substrates, inorganic material shell substrates and metal material shell substrates; the inorganic material shell substrates include glass fiber shell substrates and carbon fiber shell substrates; the metal material shell substrates include aluminum alloy shell substrates and magnesium alloy shell substrates; the shell diaphragms of different material types include: polyolefin shell diaphragms, acrylonitrile-butadiene-styrene copolymer shell diaphragms and polyethylene terephthalate copolymer shell diaphragms; When the vacuum laminating machine laminates the shell substrates of different material types and the shell diaphragms of different material types, the method includes: heating and softening the shell diaphragm according to the vacuum laminating control parameters to obtain a softened shell diaphragm; laminating and pressurizing the softened shell diaphragm according to the vacuum laminating control parameters to obtain a shell diaphragm after pressure-maintaining lamination; baking the shell diaphragm after pressure-maintaining lamination according to the vacuum laminating control parameters to obtain a laminating shell diaphragm; wherein, when the material type of the shell substrate is a polymer shell substrate and the material type of the shell diaphragm is a polyolefin shell diaphragm, the vacuum laminating control parameters include a heating softening temperature of 80 degrees, a heating softening time of 30 seconds, and a laminating pressure holding temperature of 90-100 degrees. The laminating holding time is 90 seconds, the baking temperature is 90 degrees, and the baking time is 3 minutes; when the material type of the shell substrate is an inorganic material shell substrate, and the material type of the shell diaphragm is a polyolefin shell diaphragm, the vacuum laminating control parameters include a heating softening temperature of 120 degrees, a heating softening time of 30 seconds, a laminating holding temperature of 120 degrees, a laminating holding time of 90 seconds, a baking temperature of 130 degrees, and a baking time of 25-30 minutes; when the material type of the shell substrate is a metal material shell substrate and the material type of the shell diaphragm is a polyolefin shell diaphragm, the vacuum laminating control parameters include a heating softening temperature of 120 degrees, a heating softening time of 30 seconds, a laminating holding temperature of 120 degrees, a laminating holding time of 90 seconds, a baking temperature of 130 degrees, and a baking time of 25-30 minutes.

2. The visual inspection method for bonding the shell membrane to the substrate according to claim 1, characterized in that: When the shell diaphragm is aligned and fixed to the diaphragm carrier, the LOGO positioning point is controlled to be aligned with the diaphragm carrier positioning point by plus or minus 2 wires.

3. The visual inspection method for bonding the shell membrane to the substrate according to claim 1, characterized in that: The surface appearance defects of the laminated product of the film and the substrate in the laminated product image include bubble appearance defects, wrinkle appearance defects, scratch appearance defects and color difference appearance defects.

4. The visual inspection method for bonding the shell membrane to the substrate according to any one of claims 1 to 3, characterized in that: When the laminated product of the film sheet and the substrate has a surface appearance defect in the laminated product image, the CNC process for the laminated product of the film sheet and the substrate with the surface appearance defect is stopped, and a surface appearance defect alarm is issued.

5. A visual inspection system for the bonding of a shell membrane and a substrate, characterized in that: include: A camera device is used to capture an image of the laminated product of the film and the substrate to obtain an image of the laminated product; A control host is connected and communicated with the camera device to run the visual inspection method for bonding the shell membrane to the substrate as described in any one of claims 1 to 4; A vacuum laminating machine is connected and communicated with the control host, and is used for laminating the shell substrate and the shell membrane under the control of the control host.