Pole piece coating method based on single-layer double-coating die head coating device
Through the alternating coating and blank area optimization of the single-layer dual-coating die coating device, the problems of low energy density and uneven edge thickness in lithium-ion battery pole piece coating are solved, and the cell performance and production efficiency are improved.
Patent Information
- Application Number
- CN202410925795.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-11
- Publication Date
- 2024-10-01
AI Technical Summary
There are large blank areas during the coating process of lithium-ion battery pole pieces, resulting in reduced energy density and uneven edge thickness, which affects battery performance and life. Moreover, the existing single-die coating process is affected by edge effects and gasket structural deformation. , reducing production efficiency and product yield.
It adopts a coating device based on a single-layer double coating die head, controlled by a servo motor-driven feeding structure and coating valve, to achieve alternating coating of the pole pieces and optimization of the blank area, reduce the area of the tab area, and improve the uniformity of the electrode material. degree and reduce processing accuracy requirements.
It effectively increases the energy density of the battery core, avoids the problem of uneven edge thickness, improves production efficiency and product yield, and reduces processing accuracy requirements.
Smart Images

Figure CN118719456A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of lithium ion battery production equipment, and in particular to a pole piece coating method based on a single-layer double-coating die head coating device. Background Art
[0002] Compared with traditional batteries, lithium-ion batteries have the advantages of higher energy, stronger discharge capacity and longer cycle life. In addition, their energy storage efficiency can exceed 90% and their safety performance is good. Therefore, lithium-ion batteries have great development prospects in electric vehicles and storage power sources.
[0003] When the pole piece is coated in the production process of lithium-ion batteries, a pole ear area is reserved at the head of the battery cell pole piece for welding the pole ear. The general coating method is to install the gasket in the die head, and control the coating of the die head to reach the two areas of the coating area and the blank area. In order to reduce the internal resistance of the battery cell and improve the performance and safety of the battery cell, the pole ear area is generally set in the middle of the pole piece. However, in the prior art, there is a large blank area in the middle of the pole piece. This large blank area cannot be fully utilized, which leads to a decrease in the energy density of the battery cell and affects the performance of the battery. Therefore, in order to reduce the area of the pole ear area and make full use of the pole piece area, a pole piece coating method that can improve the energy density is needed.
[0004] In addition, since the general coating device is affected by the edge effect, the coating thickness at the edge and the head and tail of the pole piece is uneven. The coating edge effect refers to the phenomenon that the thickness of the electrode material is uneven at the edge during the coating process of the positive and negative electrode materials of the lithium battery due to the limitations of the coating mechanical structure and the coating process. This uneven thickness distribution will cause local overcharge or over-discharge of the electrode material during use, thereby affecting the performance and life of the lithium battery. The existing single-die coating process will be more affected by the edge effect, and the existing gasket structure is also prone to deformation due to the pressure difference between the upper and lower coating chambers, which leads to greater reliance on the processing accuracy of the gasket, which affects the production efficiency and product yield to a certain extent, and requires high processing accuracy. Summary of the invention
[0005] The technical problem to be solved by the present invention is to provide a pole piece coating method based on a single-layer double-coating die head coating device, aiming to effectively reduce the area of the pole ear region and make full use of the pole piece area to improve the energy density of the battery cell; on this basis, it further prevents the gasket structure from deforming, improves the uniformity of the electrode material at the edge, so as to improve production efficiency and product yield, and reduce the precision requirements of processing.
[0006] In this regard, the present invention provides a pole piece coating method based on a single-layer double-die coating device, which adopts a single-layer double-die coating device, wherein the single-layer double-die coating device comprises a single-layer double-die coating structure, a coating roller assembly and a feeding structure, wherein the single-layer double-die coating structure is connected to the feeding structure and is arranged on one side of the coating roller assembly; the single-layer double-die coating structure comprises an upper die, a gasket and a lower die, wherein the gasket comprises a first gasket, a second gasket and a third gasket stacked in sequence, or the gasket comprises a fourth gasket, a second gasket and a third gasket stacked in sequence; the stacked gasket is arranged in the middle of the upper die and the lower die, and the first gasket or the fourth gasket is arranged near the upper die. On one side of the upper die head, the third gasket is arranged on a side close to the lower die head, the second gasket is arranged between the first gasket and the third gasket, or the second gasket is arranged between the fourth gasket and the third gasket; the feeding structure comprises an upper feeding device and a lower feeding device, the upper feeding device is connected to the upper die head, the lower feeding device is connected to the lower die head, the feeding structure feeds the slurry into the single-layer double-coating die head structure through a coating valve, when the upper die head is coated alone, a pole piece with a complete coating area is obtained; when the lower die head is coated alone, a pole piece with a coating area and a blank area alternating in the middle position is obtained; When the first gasket is used among the gaskets, the pole piece coating process based on the single-layer double-coating die head coating device includes the following steps: Step S1, driving the upper layer feeding device through a servo motor, opening the upper layer feeding valve of the upper layer feeding device, feeding the slurry to the upper die head through the feeding cylinder assembly, and the upper die head coats the electrode piece to obtain a complete first coating area on the electrode piece; in the step S, the lower die head stops coating; Step S2, the upper die head stops coating, the lower layer feeding device is driven by a servo motor, the lower layer feeding valve of the lower layer feeding device is opened, the slurry is sent to the lower die head through the feeding cylinder assembly, the lower die head coats the gap part in the middle of the first coating area, and under the action of the extrusion die head, the coating flows out from the coating area of the third gasket, and a second coating area is obtained on the pole piece, and the second coating area is the pole ear coating area; Step S3, the lower die head stops coating, the upper layer feeding device is driven by a servo motor, the upper layer feeding valve of the upper layer feeding device is opened, the slurry is delivered to the upper die head through the feeding cylinder assembly, and the upper die head coats the electrode piece to obtain a first coating area on the electrode piece that is continuously coated with the step S1; Step S4, the upper die head and the lower die head both stop coating to form a blank area, until the length of the blank area reaches the preset gap of the pole piece, then jump back to step S1, and cycle until the pole piece coating process is completed; the blank area is used for welding the pole lug; When the fourth gasket is used among the gaskets, the pole piece coating process based on the single-layer double-coating die head coating device includes the following steps: Step S1', driving the upper layer feeding device through a servo motor, opening the upper layer feeding valve of the upper layer feeding device, feeding the slurry to the upper die head through the feeding cylinder assembly, the upper die head coats the electrode piece, the slurry flows out from the fourth gasket coating area of the fourth gasket, and a third coating area is obtained on the electrode piece; Step S2', while the upper die head is coating, the lower layer feeding device is driven by a servo motor, the lower layer feeding valve of the lower layer feeding device is opened, and the slurry is sent to the lower die head through the feeding cylinder assembly, and the lower die head coats the gap between two adjacent third coating areas. Under the action of the extrusion die head, the coating flows out from the coating area of the third gasket, and a fourth coating area is obtained on the pole piece, and the fourth coating area is the pole ear coating area; Step S3', the upper die head continues coating, and the lower die head stops coating to form a first blank area, until the length of the first blank area reaches the preset gap of the electrode piece, and then jumps back to step S2' to obtain a fourth coating area coated in step S2' on the electrode piece, and the first blank area is used for welding the electrode lug; In step S4', the upper die head and the lower die head stop coating to form a second blank area until the length of the second blank area reaches the preset gap of the electrode, then jump back to step S1', and cycle until the electrode coating process is completed; the second blank area is used for cutting each battery electrode.
[0007] A further improvement of the present invention is that a first gasket fixing hole, a first gasket reinforcement rib and a first square hole are provided on the first gasket, the first gasket fixing hole is arranged on the side of the gasket away from the coating roller assembly, the first gasket reinforcement rib is evenly arranged in the first gasket coating area of the first gasket; the first square hole is arranged on the inner side of the bottom of the first gasket coating area.
[0008] A further improvement of the present invention is that the fourth gasket also includes a fourth gasket blank area, the blank area is arranged in the middle position of the fourth gasket coating area, and the third gasket coating area of the third gasket completely intersects with the fourth gasket coating area of the fourth gasket.
[0009] A further improvement of the present invention is that a second gasket fixing hole is provided on the second gasket, and the position of the second gasket fixing hole corresponds to the position of the first gasket fixing hole.
[0010] A further improvement of the present invention is that the third gasket includes a third gasket fixing hole, a third gasket coating area, a third gasket blank area and a third gasket reinforcement rib, the position of the third gasket fixing hole corresponds to the position of the first gasket fixing hole, the third gasket coating area and the third gasket blank area are alternately arranged on the third gasket in sequence, and the width of the third gasket coating area is greater than the width of the third gasket blank area, and the third gasket reinforcement ribs are evenly arranged in the third gasket coating area.
[0011] A further improvement of the present invention is that a third rectangular hole is provided on the third gasket, the third rectangular hole is provided on the inner side of the bottom of the coating area of the third gasket, and the length and width of the third rectangular hole are smaller than the length and width of the first square hole.
[0012] A further improvement of the present invention is that, according to the width requirement of the pole lug area, the width of the blank area of the third gasket is set accordingly to realize a pole piece in which the second coating area and the blank area alternate in the middle position, and the blank area serves as the pole lug area for welding the pole lug.
[0013] A further improvement of the present invention is that the feeding structure also includes a first extrusion head feeding elbow, a second extrusion head feeding elbow, a third extrusion head feeding elbow, a fourth extrusion head feeding elbow, a feeding cylinder assembly, a return pipe elbow, a return collection pipe, a return cylinder assembly and a servo motor; the upper die head and the upper layer feeding device are connected via the first extrusion head feeding elbow, the third extrusion head feeding elbow and the clamp fixing structure; the lower die head and the lower layer feeding device are connected via the second extrusion head feeding elbow, the fourth extrusion head feeding elbow and the clamp fixing structure to realize two sets of independently controlled feeding structures; a first material cavity is provided at the bottom of the upper die head, and the first The material cavity is connected to the first extrusion head feed elbow; the top of the lower die head is provided with a second material cavity, the second material cavity is connected to the second extrusion head feed elbow, the positions of the first material cavity and the second material cavity correspond to each other, so as to realize a double material cavity structure; the feeding structure feeds the slurry into the single-layer double-coating die head structure through the coating valve, the upper feeding device in the feeding structure is driven by a servo motor, the upper feeding valve is opened, and the slurry is fed to the upper die head through the feeding cylinder assembly, the lower feeding device in the feeding structure is driven by a servo motor, the lower feeding valve is opened, and the slurry is fed to the lower die head through the feeding cylinder assembly; When the single-layer double-coating die head structure needs to coat the ear area, the lower die head stops coating while the upper die head is coating, and the upper die head stops coating according to the preset gap. At the same time, the servo motor of the upper layer feed valve stops working, and the servo motor corresponding to the upper layer return valve of the upper layer feeding device starts working, and the excess slurry is returned to the return material collection pipe through the return cylinder assembly and the return pipe elbow, the servo motor of the lower layer feed valve starts working, and the lower die head performs coating alone to fill the gap part in the middle of the first coating area, and performs alternating coating.
[0014] A further improvement of the present invention is that the coating speed in steps S1 to S3 is controlled by a coating valve.
[0015] A further improvement of the present invention is that before the step S1, it also includes a pre-coating step, first coating at the same coating speed, and respectively detecting and recording the thickness of the pole piece head, the pole piece middle area and the pole piece tail at the same coating speed, and establishing a corresponding relationship between the coating speed and the thickness in each area for the pole piece head, the pole piece middle area and the pole piece tail; through the corresponding relationship between the coating speed and the thickness in each area, the coating valve is used to adjust and control the coating speed.
[0016] Compared with the prior art, the beneficial effects of the present invention are: providing a single-layer double-coating die head coating device including a gasket with an optimized structure, and providing a matching pole piece coating process based on the single-layer double-coating die head coating device, thereby greatly reducing the area of the blank area in the pole ear, making full use of the pole piece area, so as to improve the energy density of the battery cell; on this basis, by optimizing the design of the first gasket, the second gasket and the third gasket, the gasket structure can be further prevented from being deformed; the coating speed is optimized and controlled by the coating valve, so as to improve the uniformity of the electrode material at the edge and avoid the disadvantages caused by uneven thickness. The present invention can effectively improve production efficiency and product yield, and reduce the precision requirements of processing. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 A schematic diagram of the structure of an embodiment of the present invention; Figure 2 A schematic diagram of a three-dimensional structure of an embodiment of the present invention; Figure 3 A composition diagram of a feeding structure according to an embodiment of the present invention; Figure 4 This is a schematic structural diagram of a first gasket according to an embodiment of the present invention; Figure 5 A schematic structural diagram of a second gasket according to an embodiment of the present invention; Figure 6A schematic structural diagram of a third gasket according to an embodiment of the present invention; Figure 7 A schematic diagram of the structure of a pole piece obtained by processing in one embodiment of the present invention; Figure 8 A gasket position installation diagram of an embodiment of the present invention; Fig. 9 for Figure 8 A is a schematic diagram of the partially enlarged structure of the middle part; Fig.10 A schematic structural diagram of a fourth gasket according to another embodiment of the present invention; Fig.11 A schematic diagram of the structure of a pole piece obtained by processing in another embodiment of the present invention; Fig.12 This is a schematic diagram of single-sided thickness test data of a negative electrode sheet after coating and drying applied to an embodiment of the present invention; Fig.13 This is a schematic diagram of single-sided thickness test data of a positive electrode sheet after coating and drying applied to an embodiment of the present invention; Fig.14 It is a schematic diagram of the structure of a pole piece in the prior art. DETAILED DESCRIPTION
[0018] In the description of the present invention, if it involves a description of orientation, for example, the orientation or position relationship indicated by "upper", "lower", "front", "back", "left", "right", etc. is based on the orientation or position relationship shown in the drawings, which is only for the convenience of describing the present invention and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. If a certain technical feature is referred to as "set", "fixed", "connected", or "installed" on another technical feature, it can be directly set, fixed, or connected to the other technical feature, or it can be indirectly set, fixed, connected, or installed on the other technical feature.
[0019] In the description of the present invention, if "several" is involved, it means more than one; if "multiple" is involved, it means more than two; if "greater than", "less than", or "exceed" is involved, it should be understood as not including the number itself; if "above", "below", or "within" is involved, it should be understood as including the number itself. If "first", "second", etc. are involved, they should be understood as being used only to distinguish the names of the same or similar technical features, and should not be understood as implying / indicating the relative importance of the technical features, the number of the technical features, or the order of the technical features.
[0020] The preferred embodiments of the present invention will be further described in detail below in conjunction with the accompanying drawings.
[0021] Embodiment 1: like Figures 1 to 11 As shown, this embodiment provides a pole piece coating method based on a single-layer double-coating die head coating device, which adopts a single-layer double-coating die head coating device, wherein the single-layer double-coating die head coating device comprises a single-layer double-coating die head structure 1, a coating roller assembly 5 and a feeding structure 6, wherein the single-layer double-coating die head structure 1 is connected to the feeding structure 6 and is arranged on one side of the coating roller assembly 5; the single-layer double-coating die head structure 1 comprises an upper die head 2, a gasket 3 and a lower die head 4, as shown in FIG. Figure 8 and Fig. 9 As shown, the gasket 3 includes a first gasket 31, a second gasket 42 and a third gasket 35 which are stacked in sequence, the stacked gasket 3 is arranged in the middle of the upper die head 2 and the lower die head 4, the first gasket 31 is arranged on the side close to the upper die head 2, the third gasket 35 is arranged on the side close to the lower die head 4, and the second gasket 42 is arranged in the middle of the first gasket 31 and the third gasket 35; the feeding structure 6 includes an upper feeding device 7 and a lower feeding device 8, the upper feeding device 7 is connected to the upper die head 2, the lower feeding device 8 is connected to the lower die head 4, the feeding structure 6 feeds the slurry into the single-layer double-coating die head structure 1 through a coating valve, when the upper die head 2 is coated alone, a pole piece with a complete coating area is obtained; when the lower die head 4 is coated alone, a pole piece with a coating area and a blank area alternating in the middle position is obtained; In this embodiment, a fourth gasket 51 is used in the gasket 3, and the pole piece coating process based on the single-layer double-coating die head coating device includes the following steps: Step S1, driving the upper layer feeding device 7 by a servo motor, opening the upper layer feeding valve 71 of the upper layer feeding device 7, feeding the slurry to the upper die head 2 through the feeding cylinder assembly, and the upper die head 2 coats the electrode piece to obtain a complete first coating area 30 on the electrode piece; in the step S1, the lower die head 4 stops coating; Step S2, the upper die head 2 stops coating, the lower layer feeding device 8 is driven by a servo motor, the lower layer feeding valve 81 of the lower layer feeding device 8 is opened, and the slurry is sent to the lower die head 4 through the feeding cylinder assembly, and the lower die head 4 coats the gap part in the middle of the first coating area 30. Under the action of the extrusion die head, the coating flows out from the coating area 37 of the third gasket 35, and a second coating area 312 is obtained on the electrode piece, and the second coating area 312 is the electrode ear coating area; Step S3, the lower die head 4 stops coating, the upper layer feeding device 7 is driven by a servo motor, the upper layer feeding valve 71 of the upper layer feeding device 7 is opened, the slurry is sent to the upper die head 2 through the feeding cylinder assembly, and the upper die head 2 coats the electrode piece, and a first coating area 30 which is continuously coated with the step S1 is obtained on the electrode piece; In step S4, the upper die head 2 and the lower die head 4 stop coating to form a blank area 313 until the length of the blank area 313 reaches the preset gap of the electrode, then jump back to step S1, and cycle until the electrode coating process is completed. The effect is shown in FIG. Figure 7 As shown; the blank area 313 is used for welding the electrode lug.
[0022] It should be noted that since the electrode coating involves at least two coating processes, and the widths of the two coating processes are different, the required spraying pressures are also different. If the single feed port and single material cavity form of the existing technology is directly adopted, it will inevitably fail to meet the actual application requirements of such different spraying pressures, which will lead to uneven coating thickness at the edge and head and tail of the electrode, resulting in edge effect.
[0023] In order to overcome this practical technical problem, this embodiment adopts a double feed and double material chamber structure. Figure 1 As shown, the feeding structure 6 includes two feeding structures, namely, a first extrusion head feeding elbow 9 and a second extrusion head feeding elbow 10. A first material cavity 18 is arranged at the bottom of the upper die head 2, and the first material cavity 18 is connected to the first extrusion head feeding elbow 9; a second material cavity 19 is arranged at the top of the lower die head 4, and the second material cavity 19 is connected to the second extrusion head feeding elbow 10, thereby realizing a double material cavity structure. The positions of the first material cavity 18 and the second material cavity 19 correspond to each other to form an integral material cavity, and a buffer cavity 20 is arranged at one end of the integral material cavity close to the coating roller assembly 5, so as to share the same buffer cavity 20 and adopt a mutually independent double feed and double material cavity structure, thereby realizing two sets of independently controlled feeding structures, so as to meet the actual application requirements of spraying different pressures, avoid edge effects, and make the coating thickness of the edge and the head and tail of the pole piece more uniform and controllable.
[0024] In the prior art, in addition to the edge effect, the coating adopts a simple zebra coating, such as Fig.14 As shown, this simple zebra coating structure realizes a simple distribution of material area 21 and blank area 22. The blank area 22 occupies a larger area, while in actual applications, an area as wide as the material area 21 is not required to weld the tabs, which not only causes a waste of raw materials such as foil, but also affects the energy density of the battery.
[0025] In this regard, it is also worth noting that, unlike the prior art, on the basis of the structure of independent double feeds and double material chambers, this embodiment uses a first gasket 31, a second gasket 42 and a third gasket 35 which are stacked in sequence in a combined manner, and the battery slurry is coated through the first gasket 31 and the third gasket 35 respectively. When one of the gaskets and its feeding system is working, the other set of gaskets and its feeding system stops, and the coating process is performed alternately. Specifically, see the above-mentioned steps S1 to S4 for details, so that the first gasket 31 and the third gasket 35 each have a set of adapted and independently controlled feeding and loading systems, and the middle second gasket 42 is used as a separation plate to achieve the following. Figure 7 The final coating effect shown reasonably and fully utilizes a small portion of the area in the third gasket coating area 37 as the blank area 313 .
[0026] Therefore, through the technical solution provided in this embodiment, in addition to meeting the requirements of the electrode ear welding, only less than half of the area of the gap part is used as the blank area 313, so as to better ensure the energy density of the battery cell and greatly reduce the waste of raw materials such as foil. This is very meaningful for manufacturing companies in this field.
[0027] like Figure 4 As shown, in the first embodiment of the present embodiment, the second gasket 42 is used to separate the first gasket 31 and the third gasket 35, so as to cooperate with the single-layer double-coating die head coating device to realize the corresponding electrode coating process, that is, alternate coating, alternate coating, and finally obtain the overall first coating area 30 and the blank area 313 alternately forming the electrode, as shown in FIG. Figure 7 As shown, a small portion of the blank area 313 is used as the pole lug area for welding the pole lug, and the other area is the coating area, thereby obtaining a pole piece with significantly increased energy density.
[0028] like Figure 4 As shown, in this embodiment, the first gasket 31 is provided with a first gasket fixing hole 32 and a first gasket reinforcement rib 33. The first gasket fixing hole 32 is arranged on the side of the gasket 3 away from the coating roller assembly 5 to utilize the rear end position to achieve rapid fixation and assembly; the first gasket reinforcement rib 33 is evenly arranged in the first gasket coating area 314 of the first gasket 31 to ensure its strength and prevent deformation.
[0029] In actual applications, during high-speed automated coating work, if there is air during the coating process, it will affect the production yield of the product. Therefore, in this embodiment, the first gasket 31 is preferably provided with a first square hole 315, and the first square hole 315 is provided at the bottom inner side of the first gasket coating area 314 to exhaust air, thereby avoiding the problem of air affecting the product yield during the coating process through a simple and efficient structure.
[0030] like Figure 5 As shown, a second gasket fixing hole 41 is provided on the second gasket 42 of this embodiment, and the position of the second gasket fixing hole 41 corresponds to the position of the first gasket fixing hole 32, so as to facilitate the rapid fixation and assembly of the gasket structure and prevent misalignment between the first gasket 31 and the second gasket 42.
[0031] like Figure 6 As shown, the third gasket 35 described in this embodiment includes a third gasket fixing hole 36, a third gasket coating area 37, a third gasket blank area 38 and a third gasket reinforcing rib 39. The position of the third gasket fixing hole 36 corresponds to the position of the first gasket fixing hole 32. The third gasket coating area 37 and the third gasket blank area 38 are alternately arranged on the third gasket 35 in sequence, and the width of the third gasket coating area 37 is greater than the width of the third gasket blank area 38, so as to make full use of a small part of the area in the third gasket coating area 37 as the blank area 313. That is to say, even in the gap part in the middle of the first coating area 30, this embodiment only uses less than half of the area of the gap part as the blank area 313, so as to better ensure the energy density of the battery cell; the third gasket reinforcing rib 39 is evenly arranged in the third gasket coating area 37 to ensure its strength and prevent deformation.
[0032] The third gasket 35 of this embodiment is provided with a third rectangular hole 316, which is provided at the inner side of the bottom of the third gasket coating area 37, and the length and width of the third rectangular hole 316 are both smaller than the length and width of the first square hole 315. Similarly, the provision of the third rectangular hole 316 can be conducive to exhausting air, thereby avoiding the problem of the coating process being affected by air due to air through a simple and efficient structure. On this basis, the length and width of the third rectangular hole 316 are both smaller than the length and width of the first square hole 315, that is, the size of the third rectangular hole 316 is smaller than the size of the first square hole 315, so that while ensuring the exhaust of air, different forces are formed between the first square hole 315 and the second gasket 42 and between the third rectangular hole 316 and the second gasket 42, and the difference in forces can further ensure the coating effect of the gasket structure and improve the production yield of the product, which is not disclosed in the prior art.
[0033] Preferably, in this embodiment, the width of the blank area 38 of the third gasket is set according to the width requirement of the pole lug area, so as to realize a pole piece in which the second coating area 312 and the blank area 313 alternate, and the blank area 313 is used as the pole lug area for welding the pole lug. In other words, in this embodiment, the width of the pole lug area can be changed by the width of the middle strip of the third gasket 35 to meet different processing requirements.
[0034] like Figures 1 to 3 As shown, the feeding structure 6 of this embodiment includes a first extrusion head feeding elbow 9, a second extrusion head feeding elbow 10, a third extrusion head feeding elbow 11, a fourth extrusion head feeding elbow 12, a feeding cylinder assembly 13, a return pipe elbow 14, a return collection pipe 15, a return cylinder assembly 16 and a servo motor 17. The upper die head 2 and the upper layer feeding device 7 are connected through the first extrusion head feeding elbow 9, the third extrusion head feeding elbow 11 and the clamp fixing structure, and the lower die head 4 and the lower layer feeding device 8 are connected through the second extrusion head feeding elbow The head 10, the fourth extrusion head feed elbow 12 and the clamp fixing structure are connected, the feeding structure 6 feeds the slurry into the single-layer double-coating die head structure 1 through the coating valve, the upper feeding device 7 in the feeding structure 6 is driven by the servo motor 17, the upper feeding valve 71 is opened, and the slurry is fed to the upper die head 2 through the feeding cylinder assembly 13, the lower feeding device 8 in the feeding structure 6 is driven by the servo motor 17, the lower feeding valve 81 is opened, and the slurry is fed to the lower die head 4 through the feeding cylinder assembly 13.
[0035] The upper layer return valve 72 and the lower layer return valve 82 of this embodiment are used to return the excess slurry to the return collection pipe 15 through the reflux pipe when the upper layer feed valve 71 and the lower layer feed valve 81 stop feeding; when the single-layer double coating die head structure 1 needs to coat the ear area, the lower die head 4 stops coating while the upper die head 2 is coating, and the upper die head 2 stops coating according to the preset gap. At the same time, the servo motor of the upper layer feed valve 71 stops working, and the servo motor corresponding to the upper layer return valve 72 of the upper layer feeding device 7 starts working, and the excess slurry is returned to the return collection pipe 15 through the return cylinder assembly 16 and the return pipe elbow 14, and the servo motor of the lower layer feed valve 81 starts working, and the lower die head 4 is coated alone to fill the gap part in the middle of the first coating area 30, and the coating is performed alternately.
[0036] More preferably, the coating speed is controlled by the coating valve in steps S1 to S3 of this embodiment. The electrode is significantly less affected by the edge effect during coating, and the thickness of the electrode head and the electrode tail can be consistent with the middle area of the electrode. The coating speed is controlled by the coating valve so that the thickness of the electrode head and the electrode tail is consistent with the middle area of the electrode. The faster the coating valve is opened, the faster the coating speed is, the smaller the thickness of the electrode head and the electrode tail is, and vice versa.
[0037] More preferably, the present embodiment may further include a pre-coating step before the step S1, in which coating is first performed at the same coating speed, and the thickness of the pole piece head, the pole piece middle area and the pole piece tail at the same coating speed are respectively detected and recorded, and a corresponding relationship between the coating speed and the thickness in each area is established for the pole piece head, the pole piece middle area and the pole piece tail; therefore, in the actual pole piece coating process, the coating speed can be adjusted and controlled by using the coating valve according to the corresponding relationship between the coating speed and the thickness in each area. For example, if the thickness of the pole piece head is greater than the thickness of the middle area at the same coating speed, then, in the actual pole piece coating process, the coating speed of the pole piece head is increased proportionally according to the ratio between the thickness of the pole piece head and the thickness of the middle area, so that its thickness becomes smaller, so as to be consistent with the middle area of the pole piece; conversely, if the thickness of the pole piece head is smaller than the thickness of the middle area at the same coating speed, then, in the actual pole piece coating process, the coating speed of the pole piece head is reduced proportionally according to the ratio between the thickness of the pole piece head and the thickness of the middle area, so that its thickness becomes larger, so as to be consistent with the middle area of the pole piece. The same is true for the process of adjusting and controlling the coating speed of the pole piece tail. Therefore, this embodiment can make the thickness of the pole piece head and the pole piece tail as consistent as possible with the middle area of the pole piece, more effectively reduce the influence of the edge effect, no longer need a better gasket structure to improve efficiency, and effectively reduce the precision requirements of processing. The pole piece head and the pole piece tail are also called the pole piece edge.
[0038] Compared with the prior art, the area of the blank area 313 of the present application is greatly reduced. In the blank area 313, there is also a key point to handle the coating size of each joint. Therefore, the present application realizes the control of the joint by designing a new combined gasket 3 and adjusting the servo valve, and realizes the matching electrode coating process based on the single-layer double coating die head coating device. The data of the actual measured size of the product will be sorted and analyzed below.
[0039] like Fig.12 As shown, this embodiment is applied to the negative electrode sheet, and the single-side thickness is tested after coating and drying to obtain the test data of the single-side thickness. The unit of each test data is um, and the product thickness dimension requirement is 92±5um. It can be seen from the test that the data applied to the negative electrode sheet can be maintained within the required range. Fig.13 As shown, this embodiment is applied to the positive electrode sheet, and the single-sided thickness is tested after coating and drying to obtain the test data of the single-sided thickness. The unit of each test data is um, and the product thickness dimension requirement is 117±5um. It can be seen from the test that the data applied to the positive electrode sheet can also be maintained within the required range. Therefore, after the area of the blank area 313 is greatly reduced in this embodiment, the coating size at each joint is also well guaranteed.
[0040] In summary, this embodiment provides a single-layer double-coating die head coating device including a gasket 3 with an optimized structure, and provides a matching electrode coating process based on the single-layer double-coating die head coating device, thereby greatly reducing the area of the blank area 313 in the pole ear, making full use of the electrode area to improve the energy density of the battery cell; on this basis, through the optimized design of the first gasket 31, the second gasket 42 and the third gasket 35, the gasket structure can be further prevented from being deformed; the coating speed is optimized and controlled by the coating valve, thereby improving the uniformity of the electrode material at the edge. This embodiment can effectively improve production efficiency and product yield, and reduce the precision requirements of processing.
[0041] Embodiment 2: In another embodiment of the present application, a single-layer double-coating die head coating device substantially the same as that of embodiment 1 is used. Similarly, the single-layer double-coating die head coating device comprises a single-layer double-coating die head structure 1, a coating roller assembly 5 and a feeding structure 6. The single-layer double-coating die head structure 1 is connected to the feeding structure 6 and is arranged on one side of the coating roller assembly 5; the single-layer double-coating die head structure 1 comprises an upper die head 2, a gasket 3 and a lower die head 4, as shown in FIG. Figure 8 and Fig. 9 As shown, the gasket 3 includes a fourth gasket 51, a second gasket 42 and a third gasket 35 which are stacked in sequence, the stacked gasket 3 is arranged in the middle of the upper die head 2 and the lower die head 4, the fourth gasket 51 is arranged on the side close to the upper die head 2, the third gasket 35 is arranged on the side close to the lower die head 4, and the second gasket 42 is arranged in the middle of the fourth gasket 51 and the third gasket 35; the feeding structure 6 includes an upper feeding device 7 and a lower feeding device 8, the upper feeding device 7 is connected to the upper die head 2, and the lower feeding device 8 is connected to the lower die head 4.
[0042] In the second embodiment of the present embodiment, the second gasket 42 is used to separate the fourth gasket 51 and the third gasket 35 so as to cooperate with the single-layer double-coating die head coating device to realize the corresponding electrode coating process, that is, alternate coating, alternate coating, and finally obtain a fourth coating area 55 and a first blank area 56 alternately, and the whole is placed in the gap between the left and right third coating areas 54. Fig.11 As shown, a small portion of the first blank area 56 is used as the pole lug area for welding the pole lug, and the other area is the coating area, thereby obtaining a pole piece with significantly increased energy density. On this basis, a second blank area 57 is formed between the upper and lower integral pole pieces to realize the cutting of each battery pole piece.
[0043] The difference from Example 1 is that this embodiment is Fig.10The fourth gasket 51 shown replaces the first gasket 31. That is, in this embodiment, the first gasket 31 of embodiment 1 is replaced by the fourth gasket 51 shown in FIG. Fig.10 The fourth gasket 51 shown in the figure is used to adaptively modify the electrode coating process. In this embodiment, the upper die head 2 is continuously coated, and the lower die head 4 is intermittently coated, so as to obtain a first blank area 56 for realizing the electrode tab welding with a smaller area; and when both the upper die head 2 and the lower die head 4 stop coating, a second blank area 57 is formed to realize the cutting of each battery electrode. Compared with Example 1, this embodiment can be more conducive to large-scale electrode coating processing and production on the basis of retaining its technical effect.
[0044] When the fourth gasket 51 is used in the gasket 3, the pole piece coating process based on the single-layer double-coating die head coating device includes the following steps: Step S1', driving the upper layer feeding device 7 by a servo motor, opening the upper layer feeding valve 71 of the upper layer feeding device 7, feeding the slurry to the upper die head 2 through the feeding cylinder assembly, the upper die head 2 coats the electrode piece, the slurry flows out from the fourth gasket coating area 52 of the fourth gasket 51, and a third coating area 54 is obtained on the electrode piece; Step S2', while the upper die head 2 is coating, the lower layer feeding device 8 is driven by a servo motor, the lower layer feeding valve 81 of the lower layer feeding device 8 is opened, and the slurry is sent to the lower die head 4 through the feeding cylinder assembly, and the lower die head 4 coats the gap between two adjacent third coating areas 54. Under the action of the extrusion die head, the coating flows out from the coating area 37 of the third gasket 35, and a fourth coating area 55 is obtained on the electrode piece, and the fourth coating area 55 is the electrode lug coating area; Step S3', the upper die head 2 continues coating, and the lower die head 4 stops coating to form a first blank area 56, until the length of the first blank area 56 reaches the preset gap of the electrode piece, and then jumps back to step S2' to obtain a fourth coating area 55 coated in step S2' on the electrode piece, and the first blank area 56 is used for welding the electrode lug; In step S4', the upper die head 2 and the lower die head 4 stop coating to form a second blank area 57 until the length of the second blank area 57 reaches the preset gap of the electrode, then jump back to step S1', and cycle until the electrode coating process is completed; the second blank area 57 is used for cutting each battery electrode.
[0045] In this embodiment, if Figure 5 , Figure 6 , Fig.10 and Fig.11As shown, the fourth gasket 51 also includes a fourth gasket blank area 53, and the blank area 53 is arranged in the middle position of the fourth gasket coating area 52, and the third gasket coating area 37 of the third gasket 35 completely intersects with the fourth gasket coating area 52 of the fourth gasket 51, so as to meet the coating processing requirements of the first blank area 56 and the second blank area 57.
[0046] In summary, this embodiment provides a single-layer double-coating die head coating device including a gasket 3 with an optimized structure, and provides a matching pole piece coating process based on the single-layer double-coating die head coating device, thereby greatly reducing the area of the first blank area 56 in the pole ear, making full use of the pole piece area to improve the energy density of the battery cell; on this basis, the gasket structure can be further prevented from being deformed by optimizing the design of the fourth gasket 51, the second gasket 42 and the third gasket 35; the coating speed is optimized and controlled by the coating valve, thereby improving the uniformity of the electrode material at the edge. It is also possible to form a second blank area 57 when both the upper die head 2 and the lower die head 4 stop coating, so as to be used for cutting each battery pole piece, which is more conducive to large-scale pole piece coating processing and production, so as to further improve production efficiency.
[0047] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the protection scope of the present invention.
Claims
1. A pole piece coating method based on a single-layer double-coating die head coating device, characterized in that: A single-layer double-die coating device is used, the single-layer double-die coating device comprising a single-layer double-die structure (1), a coating roller assembly (5) and a feeding structure (6), the single-layer double-die structure (1) being connected to the feeding structure (6) and arranged on one side of the coating roller assembly (5); the single-layer double-die structure (1) comprising an upper die (2), a gasket (3) and a lower die (4), the gasket (3) comprising a first gasket (31), a second gasket (42) and a third gasket (35) stacked in sequence, or the gasket (3) comprising a fourth gasket (51), a second gasket (42) and a third gasket (35) stacked in sequence; the stacked gasket (3) is arranged in the middle of the upper die (2) and the lower die (4), the first gasket (31) or the fourth gasket (51) being arranged near the upper die (2). On one side, the third gasket (35) is arranged on a side close to the lower die head (4), and the second gasket (42) is arranged between the first gasket (31) and the third gasket (35), or the second gasket (42) is arranged between the fourth gasket (51) and the third gasket (35); the feeding structure (6) comprises an upper feeding device (7) and a lower feeding device (8), the upper feeding device (7) is connected to the upper die head (2), and the lower feeding device (8) is connected to the lower die head (4); the feeding structure (6) feeds the slurry into the single-layer double-coating die head structure (1) through a coating valve, and when the upper die head (2) is coated alone, a pole piece with a complete coating area is obtained; when the lower die head (4) is coated alone, a pole piece with a coating area and a blank area alternating in the middle position is obtained; When the first gasket (31) is used among the gaskets (3), the pole piece coating process based on the single-layer double-coating die head coating device comprises the following steps: Step S1, driving the upper layer feeding device (7) by a servo motor, opening the upper layer feeding valve (71) of the upper layer feeding device (7), feeding the slurry to the upper die head (2) through the feeding cylinder assembly, and the upper die head (2) coating the electrode piece to obtain a complete first coating area (30) on the electrode piece; in step S1, the lower die head (4) stops coating; Step S2, the upper die head (2) stops coating, the lower layer feeding device (8) is driven by a servo motor, the lower layer feeding valve (81) of the lower layer feeding device (8) is opened, and the slurry is sent to the lower die head (4) through the feeding cylinder assembly, and the lower die head (4) coats the gap portion in the middle of the first coating area (30). Under the action of the extrusion die head, the coating flows out from the coating area (37) of the third gasket (35), and a second coating area (312) is obtained on the electrode piece, and the second coating area (312) is the electrode lug coating area; Step S3, the lower die head (4) stops coating, the upper layer feeding device (7) is driven by a servo motor, the upper layer feeding valve (71) of the upper layer feeding device (7) is opened, the slurry is sent to the upper die head (2) through the feeding cylinder assembly, and the upper die head (2) coats the electrode piece, thereby obtaining a first coating area (30) on the electrode piece that is continuously coated with step S1; Step S4, the upper die head (2) and the lower die head (4) both stop coating to form a blank area (313), until the length of the blank area (313) reaches the preset gap of the electrode piece, then jump back to step S1, and cycle until the electrode piece coating process is completed; the blank area (313) is used for welding the electrode lug; When the fourth gasket (51) is used among the gaskets (3), the pole piece coating process based on the single-layer double-coating die head coating device comprises the following steps: Step S1', driving the upper layer feeding device (7) by a servo motor, opening the upper layer feeding valve (71) of the upper layer feeding device (7), feeding the slurry to the upper die head (2) through the feeding cylinder assembly, the upper die head (2) coating the electrode piece, the slurry flowing out from the fourth gasket coating area (52) of the fourth gasket (51), and obtaining a third coating area (54) on the electrode piece; Step S2', while the upper die head (2) is coating, the lower layer feeding device (8) is driven by a servo motor, the lower layer feeding valve (81) of the lower layer feeding device (8) is opened, and the slurry is sent to the lower die head (4) through the feeding cylinder assembly, and the lower die head (4) coats the gap between two adjacent third coating areas (54), and under the action of the extrusion die head, the coating flows out from the coating area (37) of the third gasket (35), and a fourth coating area (55) is obtained on the electrode piece, and the fourth coating area (55) is the electrode lug coating area; Step S3', the upper die head (2) continues coating, and the lower die head (4) stops coating, forming a first blank area (56), until the length of the first blank area (56) reaches a preset gap of the pole piece, and then jumping back to step S2', obtaining a fourth coating area (55) coated in step S2' on the pole piece, and the first blank area (56) is used for welding the pole lug; In step S4', the upper die head (2) and the lower die head (4) both stop coating to form a second blank area (57), until the length of the second blank area (57) reaches the preset gap of the electrode sheet, then jump back to step S1', and repeat this cycle until the electrode sheet coating process is completed; the second blank area (57) is used for cutting each battery electrode sheet.
2. The pole piece coating method based on the single-layer double-coating die head coating device according to claim 1 is characterized in that: The first gasket (31) is provided with a first gasket fixing hole (32), a first gasket reinforcing rib (33) and a first square hole (315); the first gasket fixing hole (32) is arranged on the side of the gasket (3) away from the coating roller assembly (5); the first gasket reinforcing rib (33) is evenly arranged on the first gasket coating area (314) of the first gasket (31); and the first square hole (315) is arranged on the inner side of the bottom of the first gasket coating area (314).
3. The electrode coating method based on the single-layer double-coating die head coating device according to claim 2 is characterized in that: The fourth gasket (51) further comprises a fourth gasket blank area (53), wherein the blank area (53) is arranged in the middle of the fourth gasket coating area (52), and the third gasket coating area (37) of the third gasket (35) completely intersects with the fourth gasket coating area (52) of the fourth gasket (51).
4. The pole piece coating method based on the single-layer double-coating die head coating device according to claim 2 or 3, characterized in that: The second gasket (42) is provided with a second gasket fixing hole (41), and the position of the second gasket fixing hole (41) corresponds to the position of the first gasket fixing hole (32).
5. The pole piece coating method based on the single-layer double-coating die head coating device according to claim 2 or 3, characterized in that: The third gasket (35) comprises a third gasket fixing hole (36), a third gasket coating area (37), a third gasket blank area (38) and a third gasket reinforcing rib (39); the position of the third gasket fixing hole (36) corresponds to the position of the first gasket fixing hole (32); the third gasket coating area (37) and the third gasket blank area (38) are alternately arranged on the third gasket (35); the width of the third gasket coating area (37) is greater than the width of the third gasket blank area (38); and the third gasket reinforcing rib (39) is evenly arranged in the third gasket coating area (37).
6. The pole piece coating method based on the single-layer double-coating die head coating device according to claim 5 is characterized in that: The third gasket (35) is provided with a third rectangular hole (316), the third rectangular hole (316) is arranged on the inner side of the bottom of the third gasket coating area (37), and the length and width of the third rectangular hole (316) are both smaller than the length and width of the first square hole (315).
7. The pole piece coating method based on the single-layer double-coating die head coating device according to claim 5 is characterized in that: The width of the third gasket blank area (38) is set accordingly according to the width requirement of the pole lug area, so as to realize a pole piece in which the second coating area (312) and the blank area (313) alternate in the middle position, and the blank area (313) serves as a pole lug area for welding the pole lug.
8. The pole piece coating method based on a single-layer double-coating die head coating device according to any one of claims 1 to 3, characterized in that: The feeding structure (6) further comprises a first extrusion head feeding elbow (9), a second extrusion head feeding elbow (10), a third extrusion head feeding elbow (11), a fourth extrusion head feeding elbow (12), a feeding cylinder assembly (13), a return pipe elbow (14), a return collection pipe (15), a return cylinder assembly (16) and a servo motor (17); the upper die head (2) and the upper layer feeding device (7) are connected via the first extrusion head feeding elbow (9), the third extrusion head feeding elbow (11) and the clamp fixing structure; the lower die head (4) and the lower layer feeding device (8) are connected via the second extrusion head feeding elbow (10), the fourth extrusion head feeding elbow (12) and the clamp fixing structure, so as to realize two sets of independently controlled feeding structures; a first material cavity (18) is arranged at the bottom of the upper die head (2); the first material cavity (18) is connected to the The first extrusion head feed elbow (9) is connected to the first extrusion head feed elbow (9); the top of the lower die head (4) is provided with a second material cavity (19), the second material cavity (19) is connected to the second extrusion head feed elbow (10), and the positions of the first material cavity (18) and the second material cavity (19) correspond to each other, so as to realize a double material cavity structure; the feeding structure (6) feeds the slurry into the single-layer double coating die head structure (1) through the coating valve, the upper feeding device (7) in the feeding structure (6) is driven by the servo motor (17), the upper feeding valve (71) is opened, and the slurry is fed to the upper die head (2) through the feeding cylinder assembly (13); the lower feeding device (8) in the feeding structure (6) is driven by the servo motor (17), the lower feeding valve (81) is opened, and the slurry is fed to the lower die head (4) through the feeding cylinder assembly (13); When the single-layer double coating die head structure (1) needs to coat the lug area, the lower die head (4) stops coating while the upper die head (2) is coating. The upper die head (2) stops coating according to a preset gap. At the same time, the servo motor of the upper layer feed valve (71) stops working, and the servo motor corresponding to the upper layer return valve (72) of the upper layer feeding device (7) starts working, and the excess slurry is returned to the return collection pipe (15) through the return cylinder assembly (16) and the return pipe elbow (14). The servo motor of the lower layer feed valve (81) starts working, and the lower die head (4) performs coating alone to fill the gap in the middle of the first coating area (30), and performs alternating coating.
9. The pole piece coating method based on a single-layer double-coating die head coating device according to any one of claims 1 to 3, characterized in that: The coating speed in steps S1 to S3 is controlled by a coating valve.
10. The pole piece coating method based on the single-layer double-coating die head coating device according to claim 9, characterized in that: Before the step S1, a pre-coating step is also included, in which coating is first performed at the same coating speed, and the thickness of the pole piece head, the pole piece middle area and the pole piece tail at the same coating speed are respectively detected and recorded, and the corresponding relationship between the coating speed and the thickness in each area is established for the pole piece head, the pole piece middle area and the pole piece tail; through the corresponding relationship between the coating speed and the thickness in each area, the coating valve is used to adjust and control the coating speed.
Citation Information
Cited By