Forming mold filling simulation experiment platform and experiment method

Through the mold filling simulation experiment platform and experimental methods, the problems of air hole defects and cold material wrapping during the die-casting process have been solved, effective verification and performance evaluation of the mold design have been achieved, and product quality and production continuity have been improved.

CN118720091APending Publication Date: 2024-10-01CHONGQING RUITONG IND
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410797565.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-20
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

During the die-casting process, existing technology cannot effectively prevent air hole defects and cold material wrapping during the mold cavity filling process, resulting in a low product quality rate, seriously affecting production continuity and increasing manufacturing costs.

Method used

A mold filling simulation experimental platform and corresponding experimental methods were designed. Through the combination of the mold body, container, piston and air inlet pipeline, air pressure was used to simulate the die-casting process, and the solidification distribution of liquid wax in the cavity was observed and verified. Factors such as smooth transition of R angle and wall thickness provide means of experimental verification.

Benefits of technology

This method provides a low-cost verification method, which can visually observe the design results during the mold design stage, evaluate the mold performance, help improve the mold structure, reduce the number of trial production improvements, and improve production continuity and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118720091A_ABST
    Figure CN118720091A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of metal and plastic molding simulation, in particular to a molding mold filling simulation experiment platform and an experiment method, which can be used for molding mold filling simulation experiments. On one hand, the mold filling simulation experiment platform for the forming mold comprises a mold body provided with a first cavity, a second cavity, a third cavity and a sprue gate which are different in structure, and the sprue gate is provided with a first pouring channel, a second pouring channel and a third pouring channel which correspondingly communicate with the first cavity, the second cavity and the third cavity; the cavity I, the cavity II and the cavity III are respectively provided with an air outlet; one end of the containing cup is connected to the sprue gate, a plugging device for plugging the opening is arranged at the other end of the containing cup, and an air inlet communicated to the interior of the containing cup is formed in the plugging device; the piston is arranged in the containing cup; one end of the air inlet pipeline is connected with the air inlet, and a flow control valve is arranged on the air inlet pipeline. On the other hand, the invention provides a mold filling simulation experiment method for the forming mold.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of metal and plastic molding simulation, in particular to a molding die filling simulation experimental platform and an experimental method. Background Art

[0002] During the die-casting process, in order to prevent the occurrence of pore defects and cold material wrapping during the filling process of the mold cavity, it is necessary to fully consider the turning points of each forming part of the mold cavity during the filling stage, the smooth transition of the R angle, and the wall thickness, so as to discharge as much gas and cold material in the liquid as possible from the mold cavity in an orderly manner, so as to obtain high-quality qualified products.

[0003] However, in actual production, different products often have complex structures, large differences in wall thickness, and many filling defects, resulting in low product quality qualification rates, which seriously affect product delivery schedules. Existing solutions usually use mold flow design software to simulate and verify the feasibility of the solution in the early stage. The disadvantage is that it relies too much on the personal experience of engineering technicians. Once the solution is not appropriate, frequent trial production and improvement are required during the production process, which will affect production continuity and cause product quality fluctuations. At the same time, it will increase product quality losses and manufacturing costs.

[0004] Therefore, for mold products with complex structures and large differences in wall thickness, it is very necessary to design experimental equipment to experimentally verify the molds designed based on experience. At the same time, it is beneficial for later staff to evaluate the mold performance based on the experimental results and provide a reference for mold structure improvement. Summary of the invention

[0005] The purpose of the present invention is to propose a forming mold filling simulation experimental platform and experimental method, which solves the problem that the R angle smooth transition of each forming part and the wall thickness and other factors need to be experimentally verified in the mold design stage.

[0006] In order to achieve the above object, the present invention adopts the following technical solutions:

[0007] On the one hand, the present invention provides a molding mold filling simulation experiment platform, comprising: a mold body, wherein the mold body is provided with a cavity one, a cavity two and a cavity three with different structures, the mold body is provided with a pouring port, and the side of the pouring port is provided with a pouring channel one, a pouring channel two and a pouring channel three correspondingly connected to the cavity one, the cavity two and the cavity three, and the ends of the cavity one, the cavity two and the cavity three away from the pouring port are respectively provided with air outlets extending to the outside of the mold body; a container cup, one end of the container cup is connected to the pouring port, and the other end is provided with a blocking device for blocking the opening, and the blocking device is provided with an air inlet connected to the interior of the container cup; a piston, the piston is movably arranged in the container cup, and the peripheral side of the piston is sealed with the inner wall of the container cup; an air inlet pipeline, one end of the air inlet pipeline is connected to the air inlet, and a flow control valve is provided on the air inlet pipeline.

[0008] On the basis of the above solution and as a preferred solution of the above solution: a cooling water channel for cooling is also provided on the mold body.

[0009] On the basis of the above scheme and as a preferred scheme of the above scheme: the overall length direction of cavity one, cavity two and cavity three extends along the length direction of the mold body, the pouring gate is arranged at one end of the length direction of the mold body, the opening direction of the pouring gate is perpendicular to the length direction of the mold body, the container is perpendicular to the length direction of the mold body and docked with the opening of the pouring gate, the pouring gate is provided with a cavity deviated from the opening direction side toward the air outlet direction side, and the pouring channel one, pouring channel two and pouring channel three are all connected to the cavity.

[0010] On the basis of the above scheme and as a preferred scheme of the above scheme: an internal thread is provided at the opening of the pouring port, an external thread is provided at the end of the container close to one end of the pouring port, and the external thread is threadably connected to the internal thread.

[0011] On the basis of the above solution and as a preferred solution of the above solution: the mold body and the container are both made of transparent materials.

[0012] On the other hand, based on the same inventive technical concept of the above scheme, the present invention provides a forming mold filling simulation experiment method, including the forming mold filling simulation experiment platform described above; and also including the following steps:

[0013] (1) Prepare markers;

[0014] (2) Prepare the filling medium, prepare a sufficient amount of wax and heat it to ≥100°C to melt;

[0015] (3) preparing an air source and connecting the air inlet pipeline to a pressurized air source;

[0016] (4) preparing the experiment, placing the marker in the container, then quickly injecting liquid wax with a temperature of ≥100° C. into the container, and connecting the container to the pouring port;

[0017] (5) Conducting an experiment, manually opening the flow control valve, and outputting air pressure from a pressurized air source to push the piston toward the pouring port, so that the moving piston injects the liquid wax containing the marker into the first, second, and third cavities;

[0018] (6) Observe the results, and observe the distribution of the liquid wax after solidification in the first cavity, the second cavity, and the third cavity.

[0019] On the basis of the above scheme and as a preferred scheme of the above scheme: the marker includes one or more of black granules, colloidal ribbon debris, and colored flaky wax.

[0020] On the basis of the above scheme and as a preferred scheme of the above scheme: the output air pressure of the pressurized air source is 6 bar, and the flow rate of the flow control valve is controlled to be 45-65 L / min.

[0021] On the basis of the above scheme and as a preferred scheme of the above scheme: for the same marker, it is necessary to carry out the experiment twice in order according to step (1) to step (6);

[0022] One of the steps is that in the experiment of step (5), before the flow control valve is manually opened, the container is placed horizontally, the gas outlet is facing upward, and the marker is distributed in the container along the length direction of the container;

[0023] In another experiment of step (5), before manually opening the flow control valve, the container is placed vertically, the mold body is at the lower side of the container, and the markers are concentrated at the pouring port.

[0024] On the basis of the above scheme and as a preferred scheme of the above scheme: the observation result of step (6) also includes observing the activity of the marker during the process of injecting the liquid wax into the cavity one, cavity two and cavity three.

[0025] In order to solve the problem that the R angle smooth transition of each forming part and factors such as wall thickness need to be experimentally verified during the mold design stage, the present invention has the following advantages:

[0026] The molding die filling simulation experimental platform and experimental method of the present invention provide a low-cost verification means that can be used to experimentally verify factors such as the smooth transition of the R angle of each molding part and the wall thickness during the mold design stage. The design results can be intuitively observed through experimental verification, which is beneficial for later staff to evaluate the mold performance according to the experimental results and provide a reference basis for improving the mold structure.

[0027] On the one hand, the molding mold filling simulation experimental platform of the present invention can simulate the injection molding process of the die-casting machine by pushing the piston through the container and the air pressure after the air intake line is connected to the air pressure. One of the cavities 1, 2 and 3 with different structures arranged inside the mold body is used to reflect the current design structure, and the other two are used to form comparative experimental examples of the current design structure. In this way, the platform can not only verify the current design structure, but also observe and compare the comparative experimental examples designed based on the current design structure to evaluate the performance of the mold of the current design.

[0028] On the other hand, the molding die filling simulation experiment method of the present invention is based on the molding die filling simulation experiment platform of the present invention for experimental operation, and can simulate the degree to which the condensation layer, oxides, etc. that may exist in the filling medium during die casting are affected by the smooth transition of the R angle of the mold design structure, and the wall thickness during the injection molding process through markers.

[0029] In addition to the above-described objects, features and advantages, the present invention has other objects, features and advantages. The present invention will be further described in detail with reference to the drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 It is a structural schematic diagram of a molding die filling simulation experimental platform of the present invention;

[0031] Figure 2 It is a schematic diagram of the exploded mold body of the present invention;

[0032] Figure 3 It is an exploded schematic diagram of the connection between the pouring spout and the container of the present invention;

[0033] Figure 4 It is a schematic diagram of the distribution of cavity one, cavity two and cavity three of the present invention;

[0034] Figure 5 It is a schematic cross-sectional view of cavity one, cavity two and cavity three of the present invention;

[0035] Figure 6 It is a flowchart of the steps of the molding die filling simulation experiment method of the present invention;

[0036] Figure 7 This is a schematic diagram of the slow filling stage of the black granules of the present invention;

[0037] Figure 8 This is a schematic diagram of the distribution of black particles of the present invention;

[0038] Fig. 9 The colloidal ribbon distribution of the colloidal ribbon debris at the low speed stage of the present invention;

[0039] Fig.10 The colloidal ribbon distribution of the colloidal ribbon debris at the high-speed stage of the present invention;

[0040] Fig.11 It is a schematic diagram of the process of filling the colored flaky wax and the colloid ribbon debris of the present invention;

[0041] Fig.12 It is a schematic diagram of the finished body of the colored flaky wax and the colloid ribbon debris filled with molds of the present invention. DETAILED DESCRIPTION

[0042] The technical solutions in the embodiments of the present invention are described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0043] See also Figure 1-12 The molding die filling simulation experimental platform and experimental method of the present invention provide a low-cost verification means that can be used to experimentally verify the smooth transition of the R angle of each molding part, as well as factors such as wall thickness during the mold design stage. The design results can be intuitively observed through experimental verification, which is conducive to the later staff to evaluate the mold performance according to the experimental results and provide a reference basis for the improvement of the mold structure.

[0044] First, as Figure 1-5 As shown, the present invention discloses a molding mold filling simulation experiment platform, including a mold body 100, a container 200, a piston 300, and an air intake pipe 400. The mold body 100 is provided with a cavity 101, a cavity 202, and a cavity 303 with different structures (see Figure 4-5), a pouring port 105 is provided on the mold body 100, and a pouring channel 1 108, a pouring channel 2 109 and a pouring channel 3 110 are provided on the side of the pouring port 105, which are connected to the cavity 1 101, the cavity 2 102 and the cavity 3 103 respectively, and an air outlet 104 extending to the outside of the mold body 100 is provided at one end of the cavity 101, the cavity 2 102 and the cavity 3 103 away from the pouring port 105; a container cup One end of 200 is connected to the pouring port 105, and the other end is provided with a sealing device 201 for sealing the opening, and the sealing device 201 is provided with an air inlet 202 connected to the interior of the container 200; the piston 300 is movably arranged inside the container 200, and the peripheral side of the piston 300 is sealed with the inner wall of the container 200; one end of the air inlet pipeline 400 is connected to the air inlet 202, and the air inlet pipeline 400 is provided with a flow control valve 401.

[0045] Among them, the overall length direction of cavity one 101, cavity two 102 and cavity three 103 extends along the length direction of the mold body 100, the pouring gate 105 is arranged at one end of the length direction of the mold body 100, the opening direction of the pouring gate 105 is perpendicular to the length direction of the mold body 100, the container 200 is connected to the opening of the pouring gate 105 perpendicular to the length direction of the mold body 100, the pouring gate 105 is provided with a chamber 106 which deviates from the opening direction side toward the air outlet 104 side, and the pouring channel one 108, the pouring channel two 109 and the pouring channel three 110 are all connected to the chamber 106.

[0046] This molding mold filling simulation experimental platform can simulate the injection molding process of the die-casting machine by pushing the piston 300 through the container 200 in coordination with the air pressure after the air inlet line 400 is connected to the air pressure. One of the cavities 1 101, 102 and 103 with different structures arranged inside the mold body 100 is used to reflect the current design structure, and the other two are used to form comparative experimental examples of the current design structure. In this way, this experimental platform can not only verify the current design structure, but also observe and compare the comparative experimental examples designed based on the current design structure, and evaluate the performance of the mold of the current design.

[0047] Among them, Figure 1 and Figure 2 As shown, the mold body 100 can be designed to be a body 112 and a body 2 115 that are assembled from top to bottom. The body 112 is provided with an inwardly concave cavity groove 114, and the body 2 115 is provided with an outwardly convex core 117. Figure 4 As shown, cavity one 101 , cavity two 102 , cavity three 103 and an air outlet 104 are formed between the top of the core 117 and the bottom of the cavity groove 114 , and a pouring port 105 can be provided on the body one 112 .

[0048] In order to ensure the simplicity of the assembly operation, the first body 112 is provided with a through hole 113, and the second body 115 is provided with a threaded hole 116 corresponding to the through hole 113. When assembling, a screw can be set to pass through the through hole 113 and then locked with the threaded hole 116. After forming, the first body 112 and the second body 115 can be separated to observe the effect.

[0049] Furthermore, a cooling water channel 111 is provided on the mold body 100 for cooling the mold and the product.

[0050] In order to visually observe the flow of the filling medium during the molding process, the mold body 100 and the container 200 are both made of transparent materials.

[0051] Generally, the end of the container 200 is detachably connected to the pouring port 105. During the experiment, in order to reduce the cost while meeting the experimental requirements, as shown in FIG. Figure 3 As shown, the opening of the pouring port 105 is provided with an internal thread 107, and the end of the container 200 close to the pouring port 105 is provided with an external thread 203, and the external thread 203 is threadedly connected with the internal thread 107. Then, the filling medium used for the experiment can be injected from the end where the external thread 203 of the container 200 is provided and then docked with the pouring port 105.

[0052] Some designs, such as Figure 4 As shown, an injection port 204 may be provided at the upper end of the container 200 , and when the piston 300 is moved upward to above the injection port 204 , the filling medium may be injected into the container 200 from the injection port 204 .

[0053] In general experimental scheme design, there are many ways to express the different structures of cavity 101, cavity 2 102 and cavity 3 103, such as Figure 5 As shown, the overall length of cavity 1 101, cavity 2 102 and cavity 3 103 is L, the overall thickness is W, the cavity wall thickness is T, the cavity structure is a wave-shaped structure that bends in the thickness direction, and the bending angle is R. In order to observe the impact of different cavity structures on the filling medium, the data of cavity wall thickness T and bending angle R can be designed and changed as a reference for punching experiments when the other parameters are the same. One of cavity 1 101, cavity 2 102 and cavity 3 103 is the current design, and the other two are the assumed upper and lower limits of the current design. In this way, the cause of the defect can be analyzed intuitively, so that the solution can be adjusted quickly and accurately to improve the defect.

[0054] In the second aspect, based on the same technical concept of the present invention, the present invention also discloses a molding die filling simulation experiment method, the molding die filling simulation experiment method includes the above molding die filling simulation experiment platform, such as Figure 6 As shown, the following steps are also included:

[0055] (1) Prepare markers;

[0056] (2) Prepare the filling medium, prepare a sufficient amount of wax and heat it to ≥100°C to melt;

[0057] (3) Prepare the gas source and connect the air inlet pipeline 400 to the pressurized gas source;

[0058] (4) Prepare the experiment, place the marker in the container 200, then quickly inject liquid wax with a temperature ≥100° C. into the container 200, and connect the container 200 to the pouring port 105;

[0059] (5) Conducting an experiment, manually opening the flow control valve 401, and the compressed air source outputting air pressure pushes the piston 300 to move toward the pouring port 105, and the moving piston 300 injects the liquid wax containing the marker into the cavity 1 101, the cavity 2 102, and the cavity 3 103;

[0060] (6) Observe the results, and observe the distribution of the liquid wax after solidification in cavity 1 101 , cavity 2 102 , and cavity 3 103 .

[0061] In some experimental design, the observation results of step (6) also include observing the activity of the marker during the process of injecting liquid wax into cavity one 101, cavity two 102 and cavity three 103.

[0062] The molding die filling simulation experiment method of the present invention is based on the molding die filling simulation experiment platform of the present invention to perform experimental operations, and uses markers to simulate the condensation layer or oxide. The markers can be used to simulate the condensation layer, oxides, etc. that may exist in the filling medium (wax) during die casting, and the degree to which they are affected by factors such as the smooth transition of the R angle of the mold design structure and the wall thickness during the injection molding process.

[0063] The advantage of choosing wax as the filling medium is that considering the physical characteristics of aluminum alloy liquid that the viscosity increases and the fluidity decreases as the temperature decreases and the existing experimental conditions, wax is selected as the filling medium. The density of wax is 0.9g / cm3, and the liquid viscosity is 130-160mPa.s at 100℃. It has similar properties to aluminum alloy, and more importantly, it has a low melting point and is easy to handle.

[0064] The marker can be selected from one or more of black granules, colloidal ribbon fragments, and colored flaky wax (colored with red lead powder).

[0065] When designing the experiment, for the same marker, two experiments can be carried out in order according to steps (1) to (6); one of the experiments is performed in step (5), before the flow control valve 401 is manually opened, the container 200 is placed horizontally, the air outlet 104 is facing upward, and the markers are distributed in the container 200 along the length direction of the container 200; the other experiment is performed in step (5), before the flow control valve 401 is manually opened, the container 200 is placed vertically, the mold body 100 is on the lower side of the container 200, and the markers are concentrated at the pouring port 105.

[0066] Experiment 1: Filling experiment

[0067] like Figure 4 The volume of the designed cavity (including cavity one 101, cavity two 102 and cavity three 103) is about 241500 mm3.

[0068] (1) Prepare a marker, about 5 g of black granules with a particle size of less than 1.5 mm.

[0069] (2) Prepare the filling medium, prepare 265g of wax liquid, and heat it to ≥100℃ to melt.

[0070] (3) Prepare the air source. Connect the air inlet line 400 to a pressurized air source. The air pressure is 6 bar and the maximum air flow rate is set to 65 L / min.

[0071] (4) Prepare the experiment, place the marker in the container 200, then quickly inject liquid wax with a temperature of ≥100°C into the container 200, and connect the container 200 to the pouring port 105, as shown in FIG. Figure 7 shown.

[0072] (5) Conducting an experiment, manually opening the flow control valve 401 to achieve constant speed filling of the cavity, the compressed air source outputs air pressure to push the piston 300 toward the pouring port 105, and the moving piston 300 injects the liquid wax containing the marker into the cavity 1 101, the cavity 2 102, and the cavity 3 103;

[0073] (6) Observation results: observe the activity of the marker during the process of injecting liquid wax into cavity 1 101, cavity 2 102 and cavity 3 103; observe the distribution of the liquid wax after solidification in cavity 1 101, cavity 2 102 and cavity 3 103.

[0074] Through experimental observation, air enters the container 200 and pushes the piston 300 to run slowly, the liquid wax flows slowly, and the black granules in the container 200 gather at the front end of the piston 300. As the opening of the flow control valve 401 increases, the running speed of the piston 300 increases sharply, and the cavity filling is completed instantly. After the high-speed filling is completed, the black granules are roughly distributed in three parts (see Figure 8 ):

[0075] 1. A large number of sprues (diverter nozzles) are gathered;

[0076] 2. Horizontal runner;

[0077] 3. Ingate and 1 / 4 cavity close to the ingate side.

[0078] Experiment 2: Oxide filling experiment

[0079] like Figure 4 The volume of the designed cavity (including cavity one 101, cavity two 102 and cavity three 103) is about 241500 mm3.

[0080] (1) Prepare markers and a certain amount of colloid ribbon debris to simulate oxides. In order to facilitate the later decomposition of the video and observe the recognition and flow state of the oxides during the cavity filling process, the amount of colloid ribbon can be deliberately increased during the experiment.

[0081] (2) Prepare the filling medium, prepare 265g of wax liquid, and heat it to ≥100℃ to melt.

[0082] (3) Prepare the air source. Connect the air inlet line 400 to a pressurized air source. The air pressure is 6 bar and the maximum air flow rate is set to 55 L / min.

[0083] (4) Prepare the experiment, place the marker in the container 200, spread it evenly along the round bottom of the container 200, then quickly inject liquid wax with a temperature ≥100° C. into the container 200, and connect the container 200 to the pouring port 105.

[0084] (5) Conducting an experiment, manually opening the flow control valve 401 to achieve constant speed filling of the cavity, the compressed air source outputs air pressure to push the piston 300 toward the pouring port 105, and the moving piston 300 injects the liquid wax containing the marker into the cavity 1 101, the cavity 2 102, and the cavity 3 103;

[0085] (6) Observation results: observe the activity of the marker during the process of injecting liquid wax into cavity 1 101, cavity 2 102 and cavity 3 103; observe the distribution of the liquid wax after solidification in cavity 1 101, cavity 2 102 and cavity 3 103.

[0086] Through experimental observation, after the liquid wax is injected into the container 200, the colloid ribbon mostly floats on the wax liquid surface, and a small part is mixed in the liquid wax (which is consistent with the state of oxides in the aluminum alloy liquid in the container 200). When air enters the container 200 and pushes the piston 300 to run slowly, the liquid wax flows slowly, the filling degree of the container 200 increases, and the colloid ribbon gathers and enters the runner (such as Fig. 9 ).

[0087] As the opening of the regulating flow valve increases, the speed of the piston 300 increases sharply, and the cavity filling is completed instantly. The distribution of the colloid ribbon in the cross runner, cavity, and exhaust overflow channel during the high-speed filling stage can be viewed through video analysis (such as Fig.10 , the order of change is ABCD).

[0088] Experiment 3: Condensation layer and oxide filling experiment

[0089] like Figure 4 The volume of the designed cavity (including cavity one 101, cavity two 102 and cavity three 103) is about 241500 mm3.

[0090] (1) preparing a marker, preparing a certain amount of colloid ribbon debris to simulate oxides, and preparing a certain amount of colored flaky wax to simulate a condensation layer, and mixing the colloid ribbon debris and the colored flaky wax to simulate the coexistence of a mixture of the two.

[0091] (2) Prepare the filling medium, prepare 265g of wax liquid, and heat it to ≥100℃ to melt.

[0092] (3) Prepare the air source. Connect the air inlet line 400 to a pressurized air source. The air pressure is 6 bar and the maximum air flow rate is set to 45 L / min.

[0093] (4) Prepare the experiment. Place the marker in the container 200 and spread it evenly along the round bottom of the container 200. Fig.11 As shown, liquid wax with a temperature of ≥100° C. is then quickly injected into the container 200 , and the container 200 is connected to the pouring port 105 .

[0094] (5) Conducting an experiment, manually opening the flow control valve 401 to achieve constant speed filling of the cavity, the compressed air source outputs air pressure to push the piston 300 toward the pouring port 105, and the moving piston 300 injects the liquid wax containing the marker into the cavity 1 101, the cavity 2 102, and the cavity 3 103;

[0095] (6) Observation results: observe the activity of the marker during the process of injecting liquid wax into cavity 1 101, cavity 2 102 and cavity 3 103; observe the distribution of the liquid wax after solidification in cavity 1 101, cavity 2 102 and cavity 3 103.

[0096] Through experimental observation, after the liquid wax is injected into the container 200, the colored flaky wax is distributed at the round bottom of the container 200, the colloid color ribbon mostly floats on the wax liquid surface, and a small part is mixed in the liquid wax (which is consistent with the state of the condensation layer and the oxide in the aluminum alloy liquid in the container 200). When air enters the container 200 and pushes the piston 300 to run slowly, the liquid wax flows slowly, the filling degree of the container 200 increases, and the colored flaky wax and the colloid color ribbon gather and enter the runner.

[0097] like Figure 11-12 (The order of changes in the diagram is Fig.11 ABCD, then Fig.12 ), as air enters the container 200, the piston 300 is pushed to run at a rapid speed, and the cavity is filled instantly. The video is broken down to see the distribution of colored flake wax and colloid ribbons in the runner, cavity, and exhaust overflow channel during the high-speed filling stage.

[0098] The following conclusions were obtained through three visual simulation filling experiments: Experiment 1, Experiment 2, and Experiment 3:

[0099] 1. Due to poor fluidity, the condensation layer in the container 200 is distributed in the sprue, runner, and 1 / 3 area of ​​the product cavity near the inner gate after filling.

[0100] 2. The oxide cannot be completely discharged from the cavity during the cavity filling process, and a small amount of oxide remains in the gate and inside the product;

[0101] Experiments reveal that the condensation layer and oxides will inevitably remain inside the product or at the gate, which may be exposed during the machining process and cause the product to be scrapped. Therefore, in the die-casting production process, the generation of condensation layer and oxides should be minimized and controlled. When designing the gating system, try to avoid the condensation layer and oxides from entering the product to reduce product scrapping and improve the pass rate.

[0102] The pouring system and overflow system of the present invention make the whole process of the filling stage visible, so that the causes of defects can be analyzed intuitively, so that the plan can be adjusted quickly and accurately to improve the defects, saving manpower, material resources, time and trial and error costs. It solves the problem of excessive reliance on the personal experience of engineering technicians, and being unable to intuitively identify the flow direction of the filling medium liquid, gas and cold material wrapping during the filling stage. Once the plan is not appropriate, it will affect the continuity of production, cause product quality fluctuations, and increase product quality losses and manufacturing costs.

[0103] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. Forming mold filling simulation experimental platform, It is characterized in that include: A mold body, wherein a cavity 1, a cavity 2 and a cavity 3 having different structures are arranged inside the mold body, a pouring port is arranged on the mold body, a pouring channel 1, a pouring channel 2 and a pouring channel 3 correspondingly connected to the cavity 1, the cavity 2 and the cavity 3 are arranged on the side of the pouring port, and an air outlet extending to the outside of the mold body is respectively arranged at one end of the cavity 1, the cavity 2 and the cavity 3 away from the pouring port; A container, one end of which is connected to the pouring port, and the other end of which is provided with a blocking device for blocking the opening, wherein the blocking device is provided with an air inlet connected to the interior of the container; A piston, the piston is movably disposed inside the container, and the peripheral side of the piston is sealed with the inner wall of the container; An air intake pipeline, one end of which is connected to the air inlet, and a flow control valve is arranged on the air intake pipeline.

2. The forming mold filling simulation experimental platform according to claim 1, It is characterized in that The mold body is also provided with a cooling water channel for cooling.

3. The molding die filling simulation experimental platform according to claim 1, It is characterized in that The overall length direction of cavity one, cavity two and cavity three extends along the length direction of the mold body, the pouring gate is arranged at one end of the length direction of the mold body, the opening direction of the pouring gate is perpendicular to the length direction of the mold body, the container is perpendicular to the length direction of the mold body and docked with the opening of the pouring gate, the pouring gate is provided with a cavity deviated from the opening direction side toward the air outlet direction side, and the pouring channel one, pouring channel two and pouring channel three are all connected to the cavity.

4. The forming mold filling simulation experimental platform according to claim 3, It is characterized in that An internal thread is arranged at the opening of the pouring port, and an external thread is arranged at the end of the container close to one end of the pouring port, and the external thread is threadably connected with the internal thread.

5. The molding die filling simulation experimental platform according to claim 1, It is characterized in that The mold body and the container are both made of transparent materials.

6. Forming mold filling simulation experimental method, It is characterized in that The molding die filling simulation experimental platform comprises the molding die filling simulation experimental platform according to any one of claims 1 to 4; and further comprises the following steps: (1) Prepare markers; (2) Prepare the filling medium, prepare a sufficient amount of wax and heat it to ≥100°C to melt; (3) preparing an air source and connecting the air inlet pipeline to a pressurized air source; (4) preparing the experiment, placing the marker in the container, then quickly injecting liquid wax with a temperature of ≥100° C. into the container, and connecting the container to the pouring port; (5) Conducting an experiment, manually opening the flow control valve, and outputting air pressure from a pressurized air source to push the piston toward the pouring port, so that the moving piston injects the liquid wax containing the marker into the first, second, and third cavities; (6) Observe the results, and observe the distribution of the liquid wax after solidification in the first cavity, the second cavity, and the third cavity.

7. The molding die filling simulation experimental method according to claim 6, It is characterized in that The marker includes one or more of black granules, colloidal ribbon fragments, and colored flaky wax.

8. The molding die filling simulation experimental method according to claim 6, It is characterized in that The output air pressure of the pressurized air source is 6 bar, and the flow rate of the flow control valve is controlled to be 45-65 L / min.

9. The molding die filling simulation experimental method according to claim 6, It is characterized in that For the same marker, the experiment needs to be carried out twice in order according to step (1) to step (6); One of the steps is that in the experiment of step (5), before the flow control valve is manually opened, the container is placed horizontally, the gas outlet is facing upward, and the marker is distributed in the container along the length direction of the container; In another experiment of step (5), before manually opening the flow control valve, the container is placed vertically, the mold body is at the lower side of the container, and the markers are concentrated at the pouring port.

10. The molding die filling simulation experimental method according to claim 6, It is characterized in that The observation results of step (6) also include observing the activity of the marker during the process of injecting the liquid wax into the first, second and third cavities.