Magnetic control hollow tungsten electrode global negative pressure arc design method

Through numerical simulation and external longitudinal magnetic field control, a magnetically controlled hollow tungsten pole full-area negative pressure arc is designed, which solves the problem of the lack of effective design methods in the existing technology and achieves the formation of negative pressure on the workpiece surface and the uniform stability of the molten pool. , promoting the development of negative pressure arc welding and additive manufacturing technology.

CN118720331AActive Publication Date: 2024-10-01SHANGHAI UNIV OF ENG SCI

Patent Information

Application Number
CN202410790491.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-19
Publication Date
2024-10-01
Estimated Expiration
2044-06-19

AI Technical Summary

Technical Problem

The existing technology lacks an economical and effective magnetically controlled hollow tungsten pole full-range negative pressure arc design method, which limits the development and engineering application of negative pressure arc welding technology and additive manufacturing technology.

Method used

Through numerical simulation, the mass conservation equation, momentum conservation equation and energy conservation equation are established, combined with the external longitudinal magnetic field, the arc shape and physical characteristics of the hollow tungsten electrode are calculated, the initial process parameters and boundary conditions are adjusted, and the full-area negative pressure of the magnetically controlled hollow tungsten electrode is realized Arc design.

Benefits of technology

It achieves the formation of negative pressure on the workpiece surface, improves the uniformity and stability of the molten pool, provides new ideas for numerical simulation-assisted design, and promotes the development of negative pressure arc welding and additive manufacturing technology.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118720331A_ABST
    Figure CN118720331A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of hollow tungsten electrode welding, and discloses a magnetic control hollow tungsten electrode negative pressure electric arc welding design method. The method includes: calculating a hollow tungsten electrode arc form; calculating a hollow tungsten electrode arc under the external longitudinal magnetic field; the influence rule of an external magnetic field on the arc temperature, pressure, speed and current density is researched by changing the initial condition and boundary condition of the hollow tungsten electrode arc, and then the dominant effect on the arc physical characteristics and the change rule of the workpiece surface pressure under different parameters are summarized; through the steps, the method has the advantages that the molten pool is more uniform and stable, and the numerical simulation result better conforms to the actual situation, a complete new numerical simulation thought is provided, and follow-up personnel can continue to conduct negative pressure arc research conveniently.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to negative pressure arc welding technology and negative pressure arc additive manufacturing technology, and more specifically, to a design method for a magnetically controlled hollow tungsten pole full-domain negative pressure arc. Background Art

[0002] Negative pressure arc means that in the conventional horizontal standard position, the arc pressure is in a negative pressure state, and a reverse pressure gradient is formed in the arc with increasing pressure from the center to the periphery, so that the arc temperature distribution in the central area drops evenly and rapidly, thereby enhancing the process characteristics of the arc, improving the physical properties and energy distribution of the traditional positive pressure arc, effectively regulating the adverse effects of the positive pressure arc, and improving the efficiency, forming accuracy and quality of additive manufacturing. Negative pressure arc welding refers to the horizontal welding position, which is also the commonly used standard position for arc additive manufacturing. Relative to the welding pool, the welding arc pressure is negative, that is, the arc negative pressure (attraction), and the arc has an attraction (adsorption) effect, which is called a negative pressure arc. To distinguish it from conventional positive pressure arc welding, it is newly defined as negative pressure arc welding. Negative pressure arc welding is generated by controlling the arc welding method with an external longitudinal magnetic field, so it is defined as magnetic control negative pressure arc welding to distinguish it from conventional magnetic control positive pressure arc welding. Obviously, negative pressure arc welding is essentially different from hollow tungsten electrode "micro-negative pressure" arc welding, because the "overall arc pressure of hollow tungsten electrode "micro-negative pressure" arc welding is still positive, but the pressure in the local area is lower than that of the conventional arc", and it still has the characteristics of positive pressure arc, not the characteristics of global negative pressure. It completely belongs to the category of positive pressure arc welding science and technology, and does not belong to the true negative pressure arc welding and negative pressure arc additive manufacturing technology system. Compared with the conventional solid tungsten electrode arc, the pressure of the hollow tungsten electrode arc is reduced, and the energy distribution and thermal output of the hollow tungsten electrode arc are changed, and they decrease as the local pressure decreases. The characteristics and regulation of the hollow tungsten electrode arc are flexible, and there is potential for the application of hollow tungsten electrode in coaxial wire feeding arc welding, arc-laser hybrid welding, surface cladding and arc additive manufacturing. The inner hole of the hollow tungsten electrode is in a "slightly negative pressure" state, which reduces the pressure value in the arc area and has characteristics different from those of a conventional arc. However, the hollow tungsten electrode welding arc is still a positive pressure welding arc, but the arc pressure is lower than that of a conventional arc, and no arc negative pressure is generated, and it still exhibits a positive pressure arc welding mechanism. The magnetic field control method can easily cause the GTAW welding arc to form a variety of arc characteristics from positive pressure to negative pressure, and from positive pressure gradient to negative pressure gradient, and can achieve flexible regulation of arc additive manufacturing (or welding) technology. At present, external field technology provides a variety of control means and technical references for negative pressure arc welding technology, and can innovatively construct magnetically controlled hollow tungsten electrode global negative pressure arc welding technology and magnetically controlled hollow tungsten electrode global negative pressure arc additive manufacturing technology.

[0003] Through experimental observation, numerical simulation and theoretical analysis, the formation mechanism, ionization process and energy transfer characteristics of the negative pressure arc can be revealed, providing a scientific basis for optimizing and applying negative pressure arc welding and additive manufacturing. The design method of the negative pressure arc adopts experimental methods, measures its laws, and designs its characteristics. The process is very complicated and unsatisfactory. Therefore, the negative pressure arc is designed by numerical simulation assisted design. However, so far, there is no economical, effective and reliable method for designing the full-domain negative pressure arc of the magnetron hollow tungsten pole to promote the development and engineering application of negative pressure arc welding technology and negative pressure arc additive manufacturing technology.

[0004] In view of this, the present invention proposes a design method for a magnetically controlled hollow tungsten pole full-area negative pressure arc to solve the above problems. Summary of the invention

[0005] In order to overcome the above-mentioned defects of the prior art, an embodiment of the present invention provides a method for designing a magnetically controlled hollow tungsten pole full-area negative pressure arc.

[0006] To achieve the above object, the present invention provides the following technical solution: a method for designing a magnetically controlled hollow tungsten pole full-domain negative pressure arc, characterized in that it comprises the following steps:

[0007] Step 1: Calculate the hollow tungsten electrode arc shape; Step 1 comprises the following steps:

[0008] (1) Establish the mass conservation equation and momentum conservation equation under negative pressure arc to determine the velocity and pressure distribution of arc plasma:

[0009]

[0010] Where ρ is density; v is velocity vector; P is pressure; μ is viscosity; I is the unit matrix; F is momentum source term;

[0011] Solve the arc temperature T according to the energy conservation equation:

[0012]

[0013] In the formula, k is the thermal conductivity; T is the temperature; Cp is the specific heat capacity; Q is the source term of the energy conservation equation;

[0014] The electric potential and magnetic vector potential distribution are calculated based on the current continuity equation and Ohm's law:

[0015]

[0016] Where V is the electric potential, A is the magnetic vector potential, and σ is the conductivity;

[0017] According to V and A, the current density J and magnetic induction intensity B are obtained:

[0018]

[0019] The arc energy source term consists of three parts: Joule heat, electron enthalpy transfer and arc radiation loss:

[0020]

[0021] Where KB is the Boltzmann constant; e is the electron charge; T is the temperature field of the arc shape; Q is the heat source term; Q rad is the arc radiation loss;

[0022] According to the arc self-induced magnetic field intensity B, current density J and momentum conservation equation, the momentum source term in the momentum conservation equation is solved:

[0023] F=J×B

[0024] (2) Define the initial process parameters of the hollow tungsten arc, material thermophysical parameters, and boundary conditions;

[0025] (3) Obtain the physical characteristics of the hollow tungsten electrode arc based on the temperature field T, pressure p, velocity v and current density J of the arc morphology;

[0026] Step 2: Calculate the hollow tungsten pole arc under an applied longitudinal magnetic field; Step 2 comprises the following steps:

[0027] (1) Add external electromagnetic force by changing the momentum source term:

[0028] F=J×(B+B0)

[0029] Where, B0 is the magnetic induction intensity of the external longitudinal magnetic field;

[0030] (2) Based on the changes in the physical characteristics of the arc under the external magnetic field, the influence of the external longitudinal magnetic field on the arc temperature, pressure, velocity and current density is studied, and then the changing law of the arc pressure and the negative pressure on the workpiece surface under the external magnetic field is obtained;

[0031] Step 3: By comparing the calculated results with the experimental results under the same conditions, verify whether the calculated results are consistent with the experimental results under the same conditions. If they are consistent, proceed to the next step; otherwise, return to step 1, adjust the model or boundary conditions or initial conditions, and re-perform the cycle of modeling and numerical simulation calculations until the calculated results are consistent with the experimental results under the same conditions, completing the model accuracy verification; fix the model, change other conditions or parameters, and solve the arc results under various conditions and situations.

[0032] Step 4: Study the influence of the external magnetic field on the arc temperature, pressure, speed and current density by changing other conditions or parameters of the hollow tungsten pole arc; then obtain and analyze and summarize the dominant role of the arc physical characteristics and the change of the workpiece surface pressure under different parameters; complete the design of the magnetically controlled hollow tungsten pole full-domain negative pressure arc.

[0033] The present invention discloses a design method for a magnetron hollow tungsten pole full-area negative pressure arc. When there is no exhaust and only the external magnetic field is changed, the existence of the tungsten pole hollow cavity promotes the generation of arc plasma reflux. The external longitudinal magnetic field always reduces the surface pressure of the hollow tungsten pole arc welding workpiece and forms a negative pressure on the workpiece surface, thereby realizing the construction of a magnetron hollow tungsten pole negative pressure arc.

[0034] The present invention discloses a method for designing a magnetically controlled hollow tungsten pole global negative pressure arc. When the exhaust pressure and the external magnetic field change, when the exhaust pressure is close to -20 kPa, the pressure change value is small when the magnetic induction intensity is less than 0.03 T, and when the magnetic induction intensity is greater than 0.04 T, the pressure drops rapidly. When the magnetic induction intensity is less than 0.03 T, the exhaust pressure plays a major role in the pressure at the center of the arc, and when the magnetic induction intensity is greater than 0.04 T, the external magnetic field plays a major role in the pressure at the center of the arc.

[0035] The technical effects and advantages of the method for designing a magnetically controlled hollow tungsten pole full-domain negative pressure arc in the present invention are as follows: by simulating magnetic field control through numerical simulation and changing the exhaust pressure, the surface temperature of the workpiece is controlled, making the molten pool more uniform and stable; by increasing the volume force method to load the external electromagnetic force, the arc is controlled by the external magnetic field; and by adding the cathode anode heat source boundary conditions, the simulation of the cathode anode sheath region is realized, making the numerical simulation results more consistent with the actual situation, providing a new idea for the design of a complete numerical simulation-assisted negative pressure arc, which is beneficial to the development of negative pressure arc welding technology and negative pressure arc additive manufacturing technology.

[0036] The present invention is applicable to negative pressure arc welding technology, or negative pressure arc additive manufacturing technology, or negative pressure arc-laser coaxial composite welding technology, or negative pressure arc-laser paraxial composite welding technology, or negative pressure arc-laser composite cladding technology, or negative pressure arc-laser composite additive manufacturing technology, or negative pressure arc-high energy beam composite welding technology, or negative pressure arc-high energy beam composite cladding technology, or negative pressure arc-high energy beam composite additive manufacturing technology. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 It is a schematic diagram of the process of the present invention;

[0038] Figure 2 It is a geometric model diagram of the hollow tungsten pole of the present invention;

[0039] Figure 3It is a pressure diagram of a hollow tungsten pole negative pressure arc under the action of an external magnetic field alone according to the present invention;

[0040] Figure 4 It is a design parameter diagram of a hollow tungsten pole negative pressure arc with the combined effect of air extraction and external magnetic field of the present invention. DETAILED DESCRIPTION

[0041] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0042] Example 1

[0043] See also Figure 1 As shown, the method for designing a magnetically controlled hollow tungsten pole full-domain negative pressure arc in this embodiment includes:

[0044] A method for designing a magnetically controlled hollow tungsten pole global negative pressure arc, characterized in that it comprises the following steps:

[0045] Step 1: Calculate the hollow tungsten electrode arc shape; Step 1 comprises the following steps:

[0046] (1) Establish the mass conservation equation and momentum conservation equation under negative pressure arc to determine the velocity and pressure distribution of arc plasma:

[0047]

[0048] Where ρ is density; v is velocity vector; P is pressure; μ is viscosity; I is the unit matrix; F is momentum source term;

[0049] Solve the arc temperature T according to the energy conservation equation:

[0050]

[0051] In the formula, k is the thermal conductivity; T is the temperature; Cp is the specific heat capacity; Q is the source term of the energy conservation equation;

[0052] The electric potential and magnetic vector potential distribution are calculated based on the current continuity equation and Ohm's law:

[0053]

[0054] Where V is the electric potential, A is the magnetic vector potential, and σ is the conductivity;

[0055] According to V and A, the current density J and magnetic induction intensity B are obtained:

[0056]

[0057] The arc energy source term consists of three parts: Joule heat, electron enthalpy transfer and arc radiation loss:

[0058]

[0059] Where KB is the Boltzmann constant; e is the electron charge; T is the temperature field of the arc shape; Q is the heat source term; Q rad is the arc radiation loss;

[0060] According to the arc self-induced magnetic field intensity B, current density J and momentum conservation equation, the momentum source term in the momentum conservation equation is solved:

[0061] F=J×B

[0062] (2) Define the initial process parameters of the hollow tungsten arc, material thermophysical parameters, and boundary conditions;

[0063] (3) Obtain the physical characteristics of the hollow tungsten electrode arc based on the temperature field T, pressure p, velocity v and current density J of the arc morphology;

[0064] Step 2: Calculate the hollow tungsten pole arc under an applied longitudinal magnetic field; Step 2 comprises the following steps:

[0065] (1) Add external electromagnetic force by changing the momentum source term:

[0066] F=J×(B+B0)

[0067] Where, B0 is the magnetic induction intensity of the external longitudinal magnetic field;

[0068] (2) Based on the changes in the physical characteristics of the arc under the external magnetic field, the influence of the external longitudinal magnetic field on the arc temperature, pressure, velocity and current density is studied, and then the changing laws of the arc pressure and the negative pressure on the workpiece surface under the external magnetic field are obtained.

[0069] Step 3: By comparing the calculated results with the experimental results under the same conditions, verify whether the calculated results are consistent with the experimental results under the same conditions. If they are consistent, proceed to the next step; otherwise, return to step 1, adjust the model or boundary conditions or initial conditions, and re-perform the cycle of modeling and numerical simulation calculations until the calculated results are consistent with the experimental results under the same conditions, completing the model accuracy verification; fix the model, change other conditions or parameters, and solve the arc results under various conditions and situations.

[0070] Step 4: Study the influence of the external magnetic field on the arc temperature, pressure, speed and current density by changing other conditions or parameters of the hollow tungsten pole arc; then obtain and analyze and summarize the dominant role of the arc physical characteristics and the change of the workpiece surface pressure under different parameters; complete the design of the magnetically controlled hollow tungsten pole full-domain negative pressure arc.

[0071] Preferably, the step 1 comprises the following steps:

[0072] (1) Construct a welding arc geometry model based on the actual welding gun geometry;

[0073] (2) Meshing the welding arc geometry model; the meshing process includes:

[0074] Define the mesh size: Use free quadrilateral mesh and adjust the distribution; complete meshing through mapping and sweeping operations.

[0075] (3) Verification of models and calculation results;

[0076] (4) Change the conditions and solve the negative pressure arc characteristics under various conditions or situations.

[0077] Preferably, the step 1 further comprises the following steps:

[0078] (1) Initial conditions of negative pressure arc model;

[0079] (2) Define the boundary conditions of the welding arc model; the boundary conditions include:

[0080] Current density input:

[0081]

[0082] Shielding gas flow rate:

[0083]

[0084] Cathode boundary conditions:

[0085]

[0086] J e =J r [(|J·n|-J r )>0]+|J·n|[(|J·n|-J r )<0]

[0087] J i =|J·n|-J e

[0088]

[0089] Anode boundary conditions:

[0090]

[0091] In the formula, |J i |V i is cathode ion heat, It is the electronic heat that plays a cooling role; is the surface work function; V i is the ionization potential of argon; A r is the Richardson constant, is the cathode effective work function, e is the elementary charge, k b is the Boltzmann constant.

[0092] Preferably, step 2 comprises the following steps:

[0093] (1) Reload the momentum source term of the negative pressure arc model;

[0094] (2) Performing parametric scanning by changing the magnetic induction intensity;

[0095] Preferably, step 3 comprises the following steps:

[0096] (1) Redefine the boundary conditions of the welding arc model;

[0097] (2) Perform parametric sweeps by changing boundary conditions;

[0098] (3) Reload the momentum source term of the negative pressure arc model;

[0099] Preferably, the presence of the exhaust pressure changes the flow pattern of the arc plasma. As the exhaust pressure decreases, part of the reflux plasma flows along the axis from the workpiece to the hollow cavity. When the exhaust pressure is -12 kPa, the arc plasma is completely composed of the reflux plasma, which will make the welding more stable.

[0100] As the exhaust pressure decreases, the pressure on the workpiece surface does not always show a downward trend. When the arc plasma acts on the workpiece surface, the pressure at the center of the workpiece decreases as the exhaust pressure decreases. When the arc plasma flow is entirely composed of reflux, the impact force does not play a major role. At this time, the arc contraction caused by the decrease in exhaust pressure increases the pressure at the center of the workpiece, which is convenient for simultaneous control with the external magnetic field to achieve better welding results.

[0101] Example 2

[0102] See also Figure 2As shown, the geometric model diagram of the hollow tungsten pole negative pressure arc of the present invention, according to the geometric model, the boundary conditions and initial conditions are set in the numerical simulation, and the mathematical model of the magnetically controlled hollow tungsten pole negative pressure arc is established. The part not described in detail in this embodiment is described in the description of embodiment 1, and a magnetically controlled hollow tungsten pole global negative pressure arc design method is provided, the method comprising: when only the external magnetic field acts on the hollow tungsten pole negative pressure arc welding, the hollow tungsten pole is not evacuated and is in a natural state. The tungsten pole radius of the hollow tungsten pole center negative pressure arc is 1.6mm, the hollow cavity radius is 0.5mm, the arc length is 3mm, the welding current is 80A, the magnetic induction intensity is 0-0.05T, the exhaust pressure is 0kPa, the shielding gas is 99.99% argon, and the shielding gas flow rate is 20-30L / min.

[0103] like Figure 3As shown, a pressure diagram of a hollow tungsten pole negative pressure arc under the action of an external magnetic field alone is shown in the figure. From the calculation results of the temperature field, velocity field and pressure field of the magnetron arc when the external longitudinal magnetic field is 0 and the external longitudinal magnetic field is 0.05T, it can be seen that the peak temperature of the arc appears below the tungsten pole. Under the action of the external longitudinal magnetic field, the arc near the tungsten pole shrinks, and the arc near the workpiece expands outward. There are two low-temperature zones in the magnetron state: the arc temperature near the workpiece appears a "low-temperature zone", and the arc temperature below the hollow cavity of the tungsten pole also appears a "low-temperature zone". The peak temperature of the arc increases with the increase of the external magnetic field strength. When the external magnetic field strength is 0.01T, a reflux plasma is generated in the center of the arc. At the same time, the pressure formed in the center of the arc is greater than 0Pa, and an upward flow is formed in the hollow cavity. Compared with the reflux phenomenon of the solid tungsten pole arc when the external magnetic field strength is 0.02T, the existence of the tungsten pole hollow cavity promotes the generation of plasma reflux. When the applied magnetic field strength is 0.02T, the plasma flows from the hollow cavity of the tungsten pole to the center of the arc, and negative pressure has been formed under the tungsten pole. As the applied magnetic field strength is further increased, the arc plasma flow speed changes from being concentrated under the tungsten pole to being concentrated on both sides of the axis. As the applied magnetic field strength increases, the arc plasma rotation speed near the tungsten pole continues to increase, causing the pressure in the arc center to continue to decrease. When the applied magnetic field strength is 0.01T, the arc peak pressure appears at the workpiece. When the applied magnetic field strength is 0.02T, a negative pressure concentration area appears in the arc center. As the magnetic induction strength continues to rise, the negative pressure area continues to expand and eventually forms a negative pressure on the workpiece surface, and the negative pressure arc design is realized. Due to the existence of the hollow tungsten pole, when the applied magnetic field strength is 0-0.01T, the workpiece surface pressure distribution is Gaussian distribution; when the applied magnetic field strength is 0.02T, the workpiece surface pressure is neither Gaussian distribution nor bimodal distribution; when the applied magnetic field strength is greater than 0.03T, the workpiece surface pressure is bimodal distribution, and the peak pressure appears at the bimodal position. When the strength of the applied magnetic field is 0.01T, reflux plasma appears in the arc, but the workpiece surface does not form a double peak distribution, the arc plasma impact on the workpiece surface is reduced, and the pressure in the center of the workpiece continues to decrease. In short, when there is no exhaust and only the external magnetic field changes, the existence of the tungsten pole hollow cavity promotes the generation of arc plasma reflux, and the applied longitudinal magnetic field always reduces the surface pressure of the hollow tungsten pole arc welding workpiece, and forms a negative pressure on the workpiece surface, realizing the construction of a magnetically controlled hollow tungsten pole negative pressure arc.

[0104] Example 3

[0105] See also Figure 4 As shown, the parts not described in detail in this embodiment can be found in the description of Embodiment 1, which provides a design method for a magnetically controlled hollow tungsten pole full-range negative pressure arc, the method comprising: the exhaust pressure and the external magnetic field act simultaneously on the hollow tungsten pole negative pressure arc welding, which is richer and more flexible than the single external magnetic field control method, and the arc characteristics are more stable and effective.

[0106] like Figure 4 The figure shows a design parameter diagram of a hollow tungsten pole negative pressure arc with the combined effect of exhaust and external magnetic field of the present invention. The tungsten pole radius of the hollow tungsten pole center negative pressure arc is 1.6mm, the hollow cavity radius is 0.5mm, the arc length is 3mm, the welding current is 80A, the magnetic induction intensity is 0-0.05T, the exhaust pressure is from 0kPa to -20kPa, the shielding gas is 99.99% argon, and the shielding gas flow rate is 20-30L / min. The pressure change caused by reducing the exhaust pressure is less than the pressure change value of increasing the magnetic induction intensity. The effect of the external magnetic field on the center pressure of the workpiece is greater than the effect of the exhaust pressure. When the exhaust pressure is close to -20kPa, the pressure change value is small when the magnetic induction intensity is less than 0.03T, and the pressure drops rapidly when the magnetic induction intensity is greater than 0.04T. When the magnetic induction intensity is less than 0.03T, the exhaust pressure plays a major role in the pressure at the center of the arc. When the magnetic induction intensity is greater than 0.04T, the external magnetic field plays a major role in the pressure at the center of the arc.

[0107] Example 4

[0108] For the parts not described in detail in this embodiment, please refer to the description of embodiment 1, which provides a method for designing a magnetically controlled hollow tungsten pole full-domain negative pressure arc, the method comprising: welding current 80A, arc length 3mm, 100% pure argon protection, arc center pressure of 61.5 Pa without external magnetic field and exhaust pressure. When the external magnetic field acts alone on the hollow tungsten pole arc, negative pressure is formed at a magnetic induction intensity of 0.025T.

[0109] Example 5

[0110] For the part not described in detail in this embodiment, please refer to the description of embodiment 1, which provides a method for designing a magnetically controlled hollow tungsten pole full-domain negative pressure arc, the method comprising: welding current 80A, arc length 3mm, 100% pure argon protection, weak exhaust pressure (-1kPa to -3kPa), when the external magnetic field acts on the hollow tungsten pole arc, a negative pressure is formed between 0.0225T and 0.0245T. Compared with the 0.025T required for the external magnetic field to act alone on the hollow tungsten pole arc, it is lower. The weak exhaust pressure can promote the formation of negative pressure.

[0111] Example 6

[0112] For the part not described in detail in this embodiment, please refer to the description of embodiment 1, which provides a method for designing a magnetically controlled hollow tungsten pole full-domain negative pressure arc, the method comprising: welding current 80A, arc length 3mm, 100% pure argon protection, and strong exhaust pressure (-4kPa to -20kPa), when an external magnetic field acts on the hollow tungsten pole arc, a negative pressure is formed between 0.0259T and 0.036T. Compared with the 0.025T required for the external magnetic field to act alone on the hollow tungsten pole arc, it is increased. Strong exhaust pressure has an inhibitory effect on the formation of negative pressure.

[0113] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the purpose and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.

Claims

1. A method for designing a magnetically controlled hollow tungsten pole global negative pressure arc, characterized in that: include: Follow these steps: Step 1: Calculate the hollow tungsten electrode arc shape; Step 1 comprises the following steps: (1) Establish the mass conservation equation and momentum conservation equation under negative pressure arc to determine the velocity and pressure distribution of arc plasma: Where ρ is density; v is velocity vector; P is pressure; μ is viscosity; I is the unit matrix; F is momentum source term; Solve the arc temperature T according to the energy conservation equation: In the formula, k is the thermal conductivity; T is the temperature; Cp is the specific heat capacity; Q is the source term of the energy conservation equation; The electric potential and magnetic vector potential distribution are calculated based on the current continuity equation and Ohm's law: Where V is the electric potential, A is the magnetic vector potential, and σ is the conductivity; According to V and A, the current density J and magnetic induction intensity B are obtained: The arc energy source term consists of three parts: Joule heat, electron enthalpy transfer and arc radiation loss: Where KB is the Boltzmann constant; e is the electron charge; T is the temperature field of the arc shape; Q is the heat source term; Q rad is the arc radiation loss; According to the arc self-induced magnetic field intensity B, current density J and momentum conservation equation, the momentum source term in the momentum conservation equation is solved: F=J×B (2) Define the initial process parameters of the hollow tungsten arc, material thermophysical parameters, and boundary conditions; (3) Obtain the physical characteristics of the hollow tungsten electrode arc based on the temperature field T, pressure p, velocity v and current density J of the arc morphology; Step 2: Calculate the hollow tungsten pole arc under an applied longitudinal magnetic field; Step 2 comprises the following steps: (1) Add external electromagnetic force by changing the momentum source term: F=J×(B+B0) Wherein, B0 is the magnetic induction intensity of the external longitudinal magnetic field; (2) Based on the changes in the physical characteristics of the arc under the external magnetic field, the influence of the external longitudinal magnetic field on the arc temperature, pressure, velocity and current density is studied, and then the changing law of the arc pressure and the negative pressure on the workpiece surface under the external magnetic field is obtained; Step 3: By comparing the calculated results with the experimental results under the same conditions, verify whether the calculated results are consistent with the experimental results under the same conditions. If they are consistent, proceed to the next step; otherwise, return to step 1, adjust the model or boundary conditions or initial conditions, and re-perform the cycle of modeling and numerical simulation calculations until the calculated results are consistent with the experimental results under the same conditions, completing the model accuracy verification; fix the model, change other conditions or parameters, and solve the arc results under various conditions and situations. Step 4: Study the influence of the external magnetic field on the arc temperature, pressure, speed and current density by changing other conditions or parameters of the hollow tungsten pole arc; then obtain and analyze and summarize the dominant role of the arc physical characteristics and the change of the workpiece surface pressure under different parameters; complete the design of the magnetically controlled hollow tungsten pole full-domain negative pressure arc.

2. A method for designing a magnetically controlled hollow tungsten pole full-range negative pressure arc according to claim 1, characterized in that: The step 1 comprises the following steps: (1) Construct a welding arc geometry model based on the actual welding gun geometry; (2) Meshing the welding arc geometry model; the meshing process includes: Define the mesh size: Use free quadrilateral mesh and adjust the distribution; complete meshing through mapping and sweeping operations. (3) Verification of models and calculation results; (4) Change the conditions and solve the negative pressure arc characteristics under various conditions or situations.

3. A method for designing a magnetically controlled hollow tungsten pole full-range negative pressure arc according to claim 2, characterized in that: The step 1 also includes the following steps: (1) Initial conditions of negative pressure arc model; (2) Define the boundary conditions of the welding arc model; the boundary conditions include: Current density input: Shielding gas flow rate: Cathode boundary conditions: I e =J r [(|J·n|-J r )>0]+|J·n|[(|J·n|-J r )<0] I i =|J·n|-J e Anode boundary conditions: In the formula, |J i |V i is cathode ion heat, It is the electronic heat that plays a cooling role; is the surface work function; V i is the ionization potential of argon; A r is the Richardson constant, is the cathode effective work function, e is the elementary charge, k b is the Boltzmann constant.

4. The negative pressure arc finite element modeling method according to claim 1, characterized in that: The step 2 comprises the following steps: (1) Reload the momentum source term of the negative pressure arc model; (2) Parametric scanning is performed by changing the magnetic induction intensity.

5. The method for designing a magnetically controlled hollow tungsten pole full-range negative pressure arc according to claim 1, characterized in that: The step 3 comprises the following steps: (1) Redefine the boundary conditions of the welding arc model; (2) Perform parametric sweeps by changing boundary conditions; (3) Reload the momentum source term of the negative pressure arc model.

6. A method for designing a magnetically controlled hollow tungsten pole global negative pressure arc according to claim 1, characterized in that: When there is no exhaust and only the external magnetic field changes, the existence of the tungsten pole hollow cavity promotes the generation of arc plasma reflux. The external longitudinal magnetic field will always reduce the surface pressure of the hollow tungsten pole arc welding workpiece and form a negative pressure on the workpiece surface, thus realizing the construction of a magnetically controlled hollow tungsten pole negative pressure arc.

7. A method for designing a magnetically controlled hollow tungsten pole global negative pressure arc according to claim 1, characterized in that: When the exhaust pressure and the external magnetic field change, when the exhaust pressure is close to -20kPa, the pressure change value is small when the magnetic induction intensity is less than 0.03T, and the pressure drops rapidly when the magnetic induction intensity is greater than 0.04T. When the magnetic induction intensity is less than 0.03T, the exhaust pressure plays a major role in the arc center pressure, and when the magnetic induction intensity is greater than 0.04T, the external magnetic field plays a major role in the arc center pressure.

8. A method for designing a magnetically controlled hollow tungsten pole global negative pressure arc according to claim 1, characterized in that: Applicable to negative pressure arc welding technology, or negative pressure arc additive manufacturing technology, or negative pressure arc-laser coaxial composite welding technology, or negative pressure arc-laser paraxial composite welding technology, or negative pressure arc-laser composite cladding technology, or negative pressure arc-laser composite additive manufacturing technology, or negative pressure arc-high energy beam composite welding technology, or negative pressure arc-high energy beam composite cladding technology, or negative pressure arc-high energy beam composite additive manufacturing technology.

Citation Information

Patent Citations

  • Fe-based bulk amorphous alloy and method for preparing same

    CN101012531A

  • Multifunctional vacuum melting furnace

    CN101745625A

  • Piston with Ti-doping diamond multi-layer thick heat-insulating film on top face and preparation method and application of piston

    CN106978593A

  • Air-magnetic combined adjusting control hollow tungsten pole TOPTIG weld welding method

    CN109365958A

  • Tungsten electrode argon arc additive manufacturing method with arc negative pressure constraint

    CN114713942A

Cited By

  • Hollow tungsten electrode negative pressure arc plasma beam cleaning and processing method

    CN120571821A

  • Hollow tungsten electrode positive and negative voltage pulse arc coaxial wire feeding fusion welding and additive manufacturing method

    CN120715343A