Prestressed double-layer hose preparation method and device and double-layer hose

Through the preparation method of prestressed double-layer hose, the problem that the double-layer glue model in the existing technology cannot truly simulate vascular tissue is solved. A double-layer hose with prestress is prepared, which improves the reliability of research data and is used for analysis. Soft tubular structures and mechanisms of vasculopathy.

CN118721818AActive Publication Date: 2024-10-01CHANGSHA UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410610694.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-05-16
Publication Date
2024-10-01
Estimated Expiration
2044-05-16

AI Technical Summary

Technical Problem

The existing double-layer glue model cannot truly simulate the multi-layer structure and characteristics of tubular biological tissues such as blood vessels, resulting in large errors between research data and actual conditions.

Method used

The prestressed double-layer hose preparation method is adopted. The inner hose is first formed, and then stretched along the axial direction to elastically deform to form a second form. Then the outer hose is formed on the outer circumferential surface, and finally the stretching and deformation are released. Demold and prepare a prestressed double-layer hose.

Benefits of technology

It achieves a realistic simulation of animal or human tubular tissue, improves the reliability of research data, can better analyze the impact mechanism of prestress on soft tubular structures and vascular lesions, and guides the design of soft robots and vascular diagnosis and treatment technology.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118721818A_ABST
    Figure CN118721818A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of soft material structure manufacturing, and discloses a prestressed double-layer hose preparation method and device and a double-layer hose. The preparation method of the prestressed double-layer hose comprises the following steps: firstly forming an inner-layer hose in a first form, then axially stretching the inner-layer hose in the first form to a second form, then forming an outer-layer hose on the peripheral surface of the inner-layer hose in the second form, and finally releasing stretching of the inner-layer hose and demolding to obtain the double-layer hose. And the inner-layer hose of the double-layer hose reforms the outer-layer hose in the stretched second form, so that axial prestress exists between the inner layer and the outer layer of the double-layer hose, and the double-layer hose meeting the requirements and having the prestress is manufactured. The prestressed double-layer hose prepared by the preparation method of the prestressed double-layer hose can simulate more real animal tubular tissues, and better technical reference is provided for subsequent research and disease treatment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of soft material structure manufacturing, and in particular, to a method for preparing a prestressed double-layer hose, a preparation device and a double-layer hose. Background Art

[0002] Hydrogel is a type of hydrophilic polymer material with a three-dimensional (3D) network structure. It is a slippery soft material with a large amount of bound water, interfacial water and free water medium in its three-dimensional polymer network. Hydrogel has physiological properties similar to those of animal tissues and organs and is also widely used in biomedical research.

[0003] Among them, for example, tubular tissues such as human blood vessels are multi-layer structures. In order to simulate tubular biological tissues such as blood vessels and complex soft structures, a simple double-layer rubber model tube is provided as a simulation model in the prior art. However, in actual operation, there are still certain differences between the existing double-layer rubber tube model and the tubular tissues of animals, resulting in a large error between the research data and the actual situation, and it is not possible to provide good guidance for research and surgical operations. Summary of the invention

[0004] The purpose of the present application is to provide a prestressed double-layer hose preparation method, preparation device and double-layer hose, so as to solve the problem that the existing double-layer glue model cannot truly simulate the multi-layer structure and corresponding characteristics of tubular biological tissues such as blood vessels, resulting in a large error between the research data and the actual situation.

[0005] To achieve the above objectives, in a first aspect, the present application provides a method for preparing a prestressed double-layer hose, comprising:

[0006] S100: Injection molding of the first form of the inner hose;

[0007] S200: stretching the inner layer hose in the first form in the axial direction by a preset length and maintaining the stretching, so that the inner layer hose (11) in the first form undergoes elastic deformation to obtain an inner layer hose in the second form;

[0008] S300: injecting glue on the outer peripheral surface of the inner hose in the second state to prepare an outer hose;

[0009] S400: After the outer layer hose is solidified and formed, the inner layer hose is stretched and demoulded to obtain a double-layer hose with prestress.

[0010] As a further improvement of the above technical solution:

[0011] In a possible implementation, the step S100 includes:

[0012] S110: preparing an elastic inner core in advance;

[0013] S120: using a radially split first mold to close the mold outside the inner core;

[0014] S130: injecting a colloid stock solution for preparing the inner layer hose into the first mold;

[0015] S140: after the colloid stock solution solidifies to form the inner hose in the first form, opening the first mold;

[0016] S150: axially stretching the inner core and the inner layer hose in the first form to obtain and maintain the inner layer hose in the second form.

[0017] In a possible implementation manner, the inner core is an elastic rubber tube or an elastic rubber stick.

[0018] In a possible implementation manner, the preset length by which the inner hose in the first form is stretched is 15%-30% of the original length.

[0019] In a possible implementation, the colloid stock solution for preparing the inner hose is a hydrogel stock solution;

[0020] Wherein, before step S100, the method further includes:

[0021] S90: preparing the hydrogel stock solution.

[0022] In a possible implementation manner, the step S90 includes:

[0023] S91: preparing deionized water, polyvinyl alcohol, acrylamide, NN methylenebisacrylamide, ammonium persulfate and a catalyst;

[0024] S92: mixing deionized water with polyvinyl alcohol, acrylamide, NN methylenebisacrylamide and ammonium persulfate in a certain proportion, heating and stirring the solution, and cooling the solution to obtain the hydrogel stock solution;

[0025] Wherein, the step S130 includes adding a certain amount of the catalyst solution with a concentration of 0.55% to the hydrogel stock solution prepared in step S92, stirring the mixture evenly, and then injecting the mixture into the first mold.

[0026] In a possible implementation manner, the step S92 further includes:

[0027] S920: adding polyvinyl alcohol into a container containing deionized water to prepare a polyvinyl alcohol solution with a concentration of 5%, setting a first heating temperature, and stirring for a first preset time to obtain a polyvinyl alcohol aqueous solution;

[0028] S921: Add the prepared acrylamide into the container so that the ratio of the concentration of acrylamide particles to the concentration of the polyvinyl alcohol aqueous solution is 17.5%, and stir at room temperature for a second preset time until the solution is free of impurities and bubbles;

[0029] S922: Add the prepared NN methylenebisacrylamide into the container so that the concentration ratio of NN methylenebisacrylamide to acrylamide is 0.066%, and stir at room temperature for a third preset time until the solution is free of impurities and bubbles;

[0030] S923: Add the prepared ammonium persulfate into the container so that the concentration ratio of ammonium persulfate to acrylamide is 0.66%, thereby obtaining the hydrogel stock solution.

[0031] In a possible implementation, an exhaust operation is performed when the inner hose of the first form is formed in step S100 and / or when the outer hose is prepared in step S300.

[0032] To achieve the above-mentioned purpose, in a second aspect, the present application further provides a prestressed double-layer hose preparation device, which applies the prestressed double-layer hose preparation method provided in the above-mentioned first aspect, and the prestressed double-layer hose preparation device comprises:

[0033] Base;

[0034] A first mold, detachably disposed on the base, for forming an inner hose of a first form;

[0035] A second mold is detachably disposed on the base and is used to be nested outside the inner hose after demoulding, the inner diameter of the second mold is larger than the inner diameter of the first mold, and the second mold is used to mold the outer hose;

[0036] a stretching mechanism, arranged on the base or on one side of the base; and

[0037] An inner core, one end of which is connected to the base, and the other end of which is connected to the stretching end of the stretching mechanism, wherein when the inner hose of the first form is formed, the inner core is coaxially arranged with the first mold;

[0038] Wherein, both the first mold and the second mold adopt a split-type demoulding structure.

[0039] To achieve the above objectives, in a third aspect, the present application further provides a double-layer hose, comprising a prestressed double-layer hose preparation method according to the above first aspect or a prestressed double-layer hose preparation device according to the above second aspect.

[0040] Compared with the prior art, the present invention has the following beneficial effects:

[0041] The present application provides a method for preparing a prestressed double-layer hose, a preparation device and a double-layer hose, wherein the method for preparing a prestressed double-layer hose first forms an inner hose of a first form, then stretches the inner hose of the first form axially to elastically deform the inner hose to obtain an inner hose of a second form, then forms an outer hose on the outer peripheral surface of the inner hose of the second form, and finally releases the stretching of the inner hose and demolds to obtain a double-layer hose. Since the inner hose of the double-layer hose is reshaped into an outer hose in the second form after being stretched and elastically deformed, the inner and outer layers of the double-layer hose have axial prestress, so as to obtain a double-layer hose that meets the requirements and has prestress. The prestressed double-layer hose prepared by the prestressed double-layer hose preparation method of the present application can truly simulate the tubular tissue of an animal or human body (such as tubular tissue such as human blood vessels), and the data obtained by using the prestressed double-layer hose for research is more real and reliable, so as to better analyze the influence mechanism of prestress on soft tubular structures and vascular lesions, so as to better guide the design of soft robots and vascular diagnosis and treatment technology.

[0042] Other features and advantages of the present application will be described in detail in the subsequent detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] The accompanying drawings are used to provide a further understanding of the present application and constitute a part of the specification. Together with the following specific embodiments, they are used to explain the present application. It should be understood that the following drawings only show certain embodiments of the present application and should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work. In the drawings:

[0044] Figure 1 A flow chart showing a method for preparing a prestressed double-layer hose provided in an embodiment of the present application is shown;

[0045] Figure 2 An axial cross-sectional view of a double-layer hose produced by the method for producing a prestressed double-layer hose provided in an embodiment of the present application is shown;

[0046] Figure 3 An axial schematic diagram of a partial structure of a double-layer hose preparation device provided in an embodiment of the present application is shown;

[0047] Figure 4 An exploded schematic diagram of a first mold provided by an embodiment of the present application is shown;

[0048] Figure 5 A schematic diagram of the axial side of a double-layer hose preparation device provided in an embodiment of the present application when a first mold is installed is shown;

[0049] Figure 6An exploded schematic diagram of a second mold provided by an embodiment of the present application is shown;

[0050] Figure 7 A schematic diagram of the axial side of a double-layer hose preparation device provided in an embodiment of the present application when a second mold is installed is shown;

[0051] Figure 8 A schematic diagram showing the dimensional changes of an incompressible superelastic double-layer cylindrical structure provided in an embodiment of the present application before (a) and after (b) uniaxial stretching is shown.

[0052] Description of reference numerals:

[0053] 10. Double-layer hose; 11. Inner hose; 12. Outer hose;

[0054] 100, base; 110, positioning groove;

[0055] 200, first mold; 210, first half mold;

[0056] 300, second mold; 310, second half mold;

[0057] 400, stretching mechanism; 410, column; 420, stretching head; 430, driving assembly; 431, screw module;

[0058] 500, inner core. DETAILED DESCRIPTION

[0059] The specific implementation of the embodiment of the present application is described in detail below in conjunction with the accompanying drawings. It should be understood that the specific implementation described here is only used to illustrate and explain the embodiment of the present application, and is not used to limit the embodiment of the present application.

[0060] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application may be combined with each other.

[0061] In the embodiments of the present application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0062] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0063] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0064] The present application will be described in detail below with reference to the accompanying drawings and in conjunction with exemplary embodiments.

[0065] Embodiment 1

[0066] See also Figure 1 and Figure 2 This embodiment provides a method for preparing a prestressed double-layer hose, which can prepare a double-layer hose 10 with prestress.

[0067] In this embodiment, the method for preparing a prestressed double-layer hose includes the following steps:

[0068] S100: injecting and molding the inner hose 11 in a first form. The inner hose 11 in a first form is defined as the inner hose 11 in an original state, and the inner hose 11 has no stress at this time.

[0069] S200: The inner hose 11 in the first form is stretched axially by a preset length and maintained, so that the inner hose 11 in the first form is elastically deformed to obtain the inner hose 11 in the second form. It should be noted that the inner wall of the inner hose 11 in the second form is intact and cannot be torn.

[0070] S300: Injecting glue onto the outer peripheral surface of the inner layer hose 11 in the second state to prepare the outer layer hose 12.

[0071] S400: After the outer layer hose 12 is solidified and formed, the inner layer hose 11 is stretched and demoulded to obtain a double-layer hose 10 with prestress.

[0072] It should be noted that tubular tissues such as human blood vessels are multi-layer structures and have prestress. In order to conduct research on the pathological mechanisms of tubular biological tissues such as blood vessels from a mechanical perspective, it is not only necessary to use a hyperelastic model containing prestress to describe them, but also to provide a method and experimental model for simulating tubular biological tissues such as blood vessels and complex soft structures, so as to better analyze the influence mechanism of prestress on soft tubular structures and vascular lesions, and to better guide soft robot design and vascular diagnosis and treatment technology.

[0073] In this way, the prestressed double-layer hose 10 prepared by the prestressed double-layer hose preparation method of the present application can truly simulate the tubular tissues of animals or human bodies (for example, tubular tissues such as human blood vessels, which are multi-layer structures and have prestress), so that the data obtained by using the prestressed double-layer hose 10 for research is more real and reliable, so as to provide better guidance for subsequent research and surgical operations.

[0074] In order to more clearly describe the technical solution of this embodiment, the following describes each step in the above-mentioned prestressed double-layer hose preparation method, as follows:

[0075] Please also read Figure 3 , Figure 4 , Figure 5 , Figure 6 and Figure 7 , the above step S100 includes:

[0076] S110: Prepare an elastic inner core 500 in advance. It is understandable that, since the inner core 500 is elastic, it has axial elastic deformation capability, so that it can be stretched axially with the inner hose 11 prepared later, so as to ensure that the wall thickness of the inner hose 11 changes evenly during the stretching process.

[0077] S120: Using a radially split first mold 200 to close the mold outside the inner core 500. The radially split first mold 200 is easy to demould and will not interfere with the stretching of the inner hose 11.

[0078] S130: injecting the colloid stock solution for preparing the inner layer hose 11 into the first mold 200. During the injection process, the first mold 200 may be knocked or vibrated at a certain frequency to discharge bubbles in the injected colloid stock solution and gas in the first mold 200, so as to ensure that the colloid stock solution can occupy and fill the entire first mold 200, and at the same time ensure that no bubbles are mixed in the prepared inner layer hose 11, thereby ensuring the preparation quality.

[0079] S140: After the colloid stock solution solidifies to form the first form of the inner hose 11, the first mold 200 is opened. Since the first mold 200 is a radially split mold structure, the first mold 200 can be removed along the radial direction of the inner hose 11 to achieve mold opening, which greatly reduces the impact of the first mold 200 on the inner hose 11.

[0080] S150: axially stretch the inner core 500 and the inner hose 11 in the first form to obtain and maintain the inner hose 11 in the second form. The inner hose 11 is elastic and will deform elastically during the stretching process, so that prestress can be ensured between the inner and outer layers after the double-layer hose is manufactured.

[0081] Optionally, the inner core 500 can be an elastic hose or an elastic rubber stick. The inner diameter of the elastic hose should be as small as possible so that the elastic hose has a thicker wall thickness, thereby ensuring that the wall thickness of the inner hose 11 changes evenly during the stretching process and ensuring uniform thickness.

[0082] Optionally, the inner core 500 is made of rubber, silicone or latex.

[0083] In some embodiments, the preset length of the inner hose 11 in the first form stretched is 15%-30% of the original length, so as to ensure that the inner hose 11 has corresponding internal stress after being stretched.

[0084] It should also be noted that the wall thickness of the inner hose 11 will change during the stretching process. If the stretching length is too long, plastic deformation will easily occur, and in severe cases, the hose will break. Therefore, the relationship between the stretching length and the wall thickness of the inner hose 11 needs to be considered.

[0085] Please also read Figure 8 Specifically, the inner core 500 and the inner hose 11 formed outside the inner core 500 are regarded as an incompressible hyperelastic double-layer cylindrical structure subjected to unidirectional tension. The length of the inner hose 11 in the initial state without being stretched is defined as L, the radius of the inner core 500 is A, the radius of the inner hose 11 is B, and the initial wall thickness of the inner hose is C=BA; the length of the inner hose 11 after stretching is l, the radius of the inner core 500 is a, and the radius of the inner hose 11 is b; the axial elongation ratio is According to the incompressible condition, the hoop stretch ratio is λ -1 / 2 ,Right now

[0086] a=λ -1 / 2 A, b = λ -1 / 2 B

[0087] The wall thickness of the inner hose 11 after stretching is c, and satisfies Thus, KE can achieve precise control of the thickness of the double-layer hose and accurate matching of the thickness of the prestressed and inner hose 11 .

[0088] Furthermore, the maximum stretching length l of the inner layer hose 11 that satisfies the elastic deformation can be obtained by performing a tensile test on the inner layer hose 11 with different corresponding thicknesses. max Substituting into the above formula, the minimum wall thickness c of the inner hose 11 corresponding to the corresponding thickness and maximum stretch length can be calculated. min , the maximum stretch is Δl max =Ll max . Then the thickness C and the maximum stretching amount Δl can be constructed max The relationship curve diagram is used to determine the maximum stretching amount Δl of the inner hose 11 of the corresponding thickness. max Therefore, before stretching, the thickness of the inner hose 11 after forming is determined first, and then the maximum stretching amount Δl is calculated based on the thickness C. max The maximum stretching amount of the inner hose 11 is determined by the relationship curve, and the stretching amount of the inner hose 11 during the stretching process does not exceed the maximum stretching amount.

[0089] In this embodiment, the colloid stock solution for preparing the inner hose 11 is a hydrogel stock solution.

[0090] In some embodiments, the colloid stock solution for preparing the outer hose 12 can also be a hydrogel stock solution, so that a double-layer hydrogel tube with prestress can be prepared. Of course, in other embodiments, the colloid stock solution of the outer hose 12 can be prepared using colloid stock solutions of other materials.

[0091] It should be noted that hydrogel materials are considered to be the biological functional materials closest to living tissues due to their high water content, good water retention, excellent biocompatibility and microstructure similar to the extracellular matrix. Therefore, tubular hydrogel materials can cooperate with the human body to a certain extent and are used in wound healing and bone diseases. In this way, the double-layer hydrogel tube prepared with hydrogel stock solution can better simulate the tubular tissue of the human body (such as tubular tissues such as human blood vessels) as an anatomical model for surgical simulation, so as to better analyze the influence mechanism of prestress on soft tubular structures and vascular lesions, so as to better guide the design of soft robots and vascular diagnosis and treatment technology.

[0092] The method further includes step S90 before step S100, wherein step S90 is to prepare a hydrogel stock solution.

[0093] Specifically, the preparation of the hydrogel stock solution in the above step S90 includes the following steps:

[0094] S91: Deionized water, polyvinyl alcohol (PVA), acrylamide (PAM), NN methylenebisacrylamide (BIS), ammonium persulfate (APS) and a catalyst (TEMED) are prepared.

[0095] S92: Deionized water is mixed with polyvinyl alcohol, acrylamide, NN methylenebisacrylamide and ammonium persulfate in a certain proportion, and the solution is heated and stirred, and the temperature is lowered to obtain a hydrogel stock solution. The stirring can be performed with a stirrer to ensure that the above components are fully integrated. The hydrogel stock solution is formed through corresponding physical or chemical cross-linking.

[0096] The step S130 includes adding a certain amount of catalyst solution with a concentration of 0.55% to the hydrogel stock solution prepared in the step S92, stirring the mixture evenly, and then injecting the mixture into the first mold 200. The catalyst can accelerate the formation of the hydrogel.

[0097] It should be noted that if the outer hose 12 is also prepared using a hydrogel stock solution, the method of step S90 is also applicable.

[0098] Furthermore, step S92 further includes:

[0099] S920: Add polyvinyl alcohol to a container containing deionized water to prepare a polyvinyl alcohol solution with a concentration of 5%, set a first heating temperature, and stir for a first preset time to obtain a polyvinyl alcohol aqueous solution; wherein the first heating temperature can be set to 90°C ± 5°C, and the first preset stirring time is at least 3 hours. Optionally, the first heating temperature can be set to 86°C, 87.4°C, 88°C, 89°C, 90°C, 91°C, 93.5°C, or 94.2°C.

[0100] S921: Add the prepared acrylamide into the container so that the ratio of the concentration of acrylamide particles to the concentration of the polyvinyl alcohol aqueous solution is 17.5%, and stir at room temperature for a second preset time until the solution is free of impurities and bubbles; wherein the second preset time for stirring at room temperature is at least 15 minutes.

[0101] S922: Add the prepared NN methylenebisacrylamide into the container so that the concentration ratio of NN methylenebisacrylamide to acrylamide is 0.066%, and stir at room temperature for a third preset time until the solution is free of impurities and bubbles; wherein the third preset time for stirring at room temperature is at least 15 minutes.

[0102] S923: Add the prepared ammonium persulfate into the container so that the concentration ratio of ammonium persulfate to acrylamide is 0.66%, thereby obtaining a hydrogel stock solution.

[0103] In the above step S100, exhaust operations are performed when the inner hose 11 of the first form is formed and in the step S300, the outer hose 12 is prepared. For example, the preparation mold is knocked or vibrated at a certain frequency to exhaust the bubbles in the injected hydrogel stock solution and the gas in the mold, so as to ensure that the hydrogel stock solution can occupy and fill the entire mold, thereby ensuring that there are no bubbles in the prepared inner hose 11 and the outer hose 12, and ensuring the preparation quality.

[0104] Please also read Figure 6 and Figure 7 Furthermore, vent holes can be provided on the first mold 200 for preparing the inner hose 11 and the second mold 300 for preparing the outer hose (described in detail below) to facilitate the exhaust of gas in the mold. After the exhaust is completed, a sealant is used to block the vent holes to prevent glue from overflowing.

[0105] Embodiment 2

[0106] See also Figure 2 , Figure 3 , Figure 5 and Figure 7 This embodiment provides a prestressed double-layer hose preparation device, and the prestressed double-layer hose preparation device applies the prestressed double-layer hose preparation method provided according to the above-mentioned embodiment 1.

[0107] In this embodiment, the prestressed double-layer hose preparation device includes a base 100, a first mold 200, a second mold 300, a stretching mechanism 400 and an inner core 500. The first mold 200 and the second mold 300 are both detachably arranged on the base 100, but the first mold 200 and the second mold 300 are used in sequence according to the molding sequence of the inner layer hose 11 and the outer layer hose 12. The base 100 is provided with positioning grooves 110 for positioning the first mold 200 and the second mold 300 respectively.

[0108] It can be understood that the first mold 200 is used to form the inner layer hose 11 of the first form; the second mold 300 is used to be nested outside the inner layer hose 11 after demolding, and the inner diameter of the second mold 300 is larger than the inner diameter of the first mold 200, and the second mold 300 is used to form the outer layer hose 12.

[0109] The stretching mechanism 400 is arranged on one side of the base 100 and connected to the base 100. One end of the inner core 500 is connected to the base 100, and the other end is connected to the stretching end of the stretching mechanism 400. When forming the inner hose 11 of the first form, the inner core 500 is coaxially arranged with the first mold 200. The inner core 500 has elasticity, as described in the above embodiment 1, which will not be repeated here.

[0110] Please also read Figure 4 and Figure 6In this embodiment, the first mold 200 and the second mold 300 both adopt a radially open demoulding structure. The first mold 200 includes two radially aligned first half molds 210. When assembled, the two first half molds 210 are molded together and fixed on the base 100. The first injection cavity for molding the inner layer hose 11 is formed between the two first half molds 210. The axis of the inner core 500 coincides with the axis of the first injection cavity (see Figure 5 The second mold 300 includes two second half molds 310 arranged radially opposite to each other. After the first mold 200 is opened, the second mold 300 is assembled. When the second mold 300 is assembled, the two second half molds 310 are molded and fixed on the base 100. At this time, a second injection cavity is formed between the second mold 300 and the formed inner hose 11, and the axis of the second injection cavity coincides with the axis of the inner core 500 (see Figure 7 ).

[0111] It should be noted that when injecting glue into the second injection cavity, the inner core 500 and the inner hose 11 should be stretched to a preset length and maintained by the stretching mechanism 400 (see Figure 7 ). This stretching step can be performed before or after the second mold 300 is closed. During the stretching, both ends of the inner hose 11 are fixedly connected to the inner core 500, for example, positioning pins or circumferential mounting clamps can be inserted to fix the inner hose 11 to the inner core 500.

[0112] In some embodiments, the two first half molds 210 and the two second half molds 310 can be fixed by snapping after being molded together, for example, a concave-convex structure can be used to achieve snap-fit.

[0113] In some other embodiments, the two first half molds 210 and the two second half molds 310 may be fixed by bolts or screws after being molded together, for example, by quick-release screws.

[0114] In some other embodiments, the two first half molds 210 and the two second half molds 310 may be fixed by means of a clamp after being molded together.

[0115] See also Figure 3 The stretching mechanism 400 includes a column 410, a stretching head 420 disposed on the column 410, and a driving assembly 430. The stretching head 420 is sleeved on the column 410 and connected to the inner core 500. The stretching head 420 and the column 410 are slidably matched up and down, and the driving assembly 430 can drive the stretching head 420 to move up and down along the column 410.

[0116] Optionally, the drive assembly 430 may use a screw module 431, wherein the screw module nut seat is disposed on the stretching head 420, and the vertical rod of the screw shaft in the screw module passes through the nut seat in the vertical direction and is connected to the column 410. In this way, the stretching head 420 is driven to move in the vertical direction by rotating the screw shaft and utilizing the thread pair of the screw shaft and the nut seat.

[0117] Optionally, the driving assembly 430 may be a pneumatic cylinder, an oil cylinder, an electric cylinder, a linear motor or a screw motor. It should be understood that the above is only an example and is not intended to limit the scope of protection of this application.

[0118] Optionally, the column 410 may be replaced by a slide rail, and the stretching head 420 may be provided with a slide seat that slidably cooperates with the slide rail.

[0119] Optionally, a scale mark may be provided on the column 410 for judging the stretching length to ensure the stretching accuracy. Of course, a scale may also be provided separately or the stretching length may be measured by a laser displacement sensor.

[0120] Furthermore, this embodiment also provides a double-layer hose 10. The double-layer hose 10 is made according to the method for making a prestressed double-layer hose provided in the first embodiment or the device for making a prestressed double-layer hose provided in the second embodiment.

[0121] In this way, the double-layer hose 10 includes an inner hose 11 and an outer hose 12 which are sequentially distributed along the radial direction, wherein the inner hose 11 is elastic and has axial prestress.

[0122] Optionally, the inner hose 11 and the outer hose 12 are made of the same material.

[0123] Optionally, the double-layer hose 10 may be a double-layer hydrogel hose.

[0124] The prestressed double-layer hose preparation device provided in this embodiment also has the following advantages:

[0125] 1. Prepare a hydrogel stock solution and make it into a double-layer hydrogel hose. The thickness of the inner and outer layers can be controlled by the first mold 200 and the second mold 300.

[0126] 2. The inner core 500 is elastic, and the stretching length of the inner hose 11 can be precisely controlled through the screw module, thereby precisely controlling the prestress of the inner hose 11 after stretching.

[0127] 3. The inner core 500 may be a super elastic solid cylindrical latex tube as the inner core 500 of the mold. This material can be stretched 6-7 times.

[0128] 4. The first mold 200 and the second mold 300 adopt a radially split half-mold structure, which is convenient for assembly and demoulding and improves demoulding efficiency.

[0129] The above describes in detail the optional implementation methods of the embodiments of the present application in combination with the accompanying drawings. However, the embodiments of the present application are not limited to the specific details in the above implementation methods. Within the technical concept of the embodiments of the present application, various simple modifications can be made to the technical scheme of the embodiments of the present application, and these simple modifications all belong to the protection scope of the embodiments of the present application.

[0130] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any suitable manner without contradiction. In order to avoid unnecessary repetition, the embodiments of the present application will not further describe various possible combinations.

[0131] In addition, the various implementation methods of the embodiments of the present application may be arbitrarily combined, and as long as they do not violate the ideas of the embodiments of the present application, they should also be regarded as the contents disclosed in the embodiments of the present application.

Claims

1. A method for preparing a prestressed double-layer hose, characterized in that: include: S100: injecting and molding the first form of the inner hose (11); S200: stretching the inner layer hose (11) in the first form in the axial direction by a preset length and maintaining the stretching, so that the inner layer hose (11) in the first form undergoes elastic deformation to obtain the inner layer hose (11) in the second form; S300: injecting glue on the outer peripheral surface of the inner hose (11) in the second state to prepare the outer hose (12); S400: After the outer layer hose (12) is solidified and formed, the stretching of the inner layer hose (11) is released, and the inner layer hose (11) is demoulded to obtain a double-layer hose (10) with prestress.

2. The method for preparing a prestressed double-layer hose according to claim 1, characterized in that: The step S100 includes: S110: Preparing an elastic inner core (500) in advance; S120: using a radially split first mold (200) to close the mold outside the inner core (500); S130: injecting a colloid stock solution for preparing the inner layer hose (11) into the first mold (200); S140: after the colloid stock solution solidifies to form the inner hose (11) in the first form, the first mold (200) is opened; S150: axially stretching the inner core (500) and the inner layer hose (11) in the first form to obtain and maintain the inner layer hose (11) in the second form.

3. The method for preparing a prestressed double-layer hose according to claim 2, characterized in that: The inner core (500) is an elastic rubber tube or an elastic rubber stick.

4. The method for preparing a prestressed double-layer hose according to claim 1 or 2, characterized in that: The preset length of the inner hose (11) in the first form stretched is 15%-30% of the original length.

5. The method for preparing a prestressed double-layer hose according to claim 1 or 2, characterized in that: The colloid stock solution for preparing the inner hose (11) is a hydrogel stock solution; Wherein, before step S100, the method further includes: S90: preparing the hydrogel stock solution.

6. The method for preparing a prestressed double-layer hose according to claim 5, characterized in that: The step S90 includes: S91: preparing deionized water, polyvinyl alcohol, acrylamide, NN methylenebisacrylamide, ammonium persulfate and a catalyst; S92: mixing deionized water with polyvinyl alcohol, acrylamide, NN methylenebisacrylamide and ammonium persulfate in a certain proportion, heating and stirring the solution, and cooling the solution to obtain the hydrogel stock solution; Wherein, the step S130 includes adding a certain amount of the catalyst solution with a concentration of 0.55% to the hydrogel stock solution prepared in step S92, stirring the mixture evenly, and then injecting the mixture into the first mold (200).

7. The method for preparing a prestressed double-layer hose according to claim 5, characterized in that: The step S92 further includes: S920: adding polyvinyl alcohol into a container containing deionized water to prepare a polyvinyl alcohol solution with a concentration of 5%, setting a first heating temperature, and stirring for a first preset time to obtain a polyvinyl alcohol aqueous solution; S921: Add the prepared acrylamide into the container so that the ratio of the concentration of acrylamide particles to the concentration of the polyvinyl alcohol aqueous solution is 17.5%, and stir at room temperature for a second preset time until the solution is free of impurities and bubbles; S922: Add the prepared NN methylenebisacrylamide into the container so that the concentration ratio of NN methylenebisacrylamide to acrylamide is 0.066%, and stir at room temperature for a third preset time until the solution is free of impurities and bubbles; S923: Add the prepared ammonium persulfate into the container so that the concentration ratio of ammonium persulfate to acrylamide is 0.66%, thereby obtaining the hydrogel stock solution.

8. The method for preparing a prestressed double-layer hose according to claim 1, characterized in that: In the step S100, when the inner hose (11) of the first form is formed and / or in the step S300, when the outer hose (12) is prepared, an exhaust operation is performed.

9. A prestressed double-layer hose preparation device, characterized in that: The method for preparing a prestressed double-layer hose according to any one of claims 1 to 8 is applied, and the prestressed double-layer hose preparation device comprises: Base (100); A first mold (200) is detachably disposed on the base (100) and is used to mold an inner hose (11) of a first form; a second mold (300) detachably disposed on the base (100) and used to be nested outside the inner hose (11) after demoulding, the inner diameter of the second mold (300) being larger than the inner diameter of the first mold (200), and the second mold (300) being used to mold the outer hose (12); A stretching mechanism (400) is arranged on the base (100) or on one side of the base (100); and an inner core (500), one end of which is connected to the base (100), and the other end of which is connected to the stretching end of the stretching mechanism (400); when forming the inner hose (11) in the first form, the inner core (500) is coaxially arranged with the first mold (200); Wherein, both the first mold (200) and the second mold (300) adopt a split-type demoulding structure.

10. A double-layer hose, characterized in that: The method for preparing a prestressed double-layer hose according to any one of claims 1 to 8 or the device for preparing a prestressed double-layer hose according to claim 9 is used for preparing the prestressed double-layer hose.