Resin film, laminated film, and method for producing resin film

By rationally adding anti-adhesive agents to the resin film and adopting specific manufacturing methods, the problems of adhesion and optical properties of the resin film during the winding process are solved, and a resin film with both excellent anti-adhesion and high optical properties is achieved.

CN118721931APending Publication Date: 2024-10-01NITTO DENKO CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410253113.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-31
Filing Date
2024-03-06
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Resin films are prone to dents due to the release liner attached during the winding process, and are prone to sticking without a release liner, making it difficult to achieve both excellent blocking resistance and optical properties.

Method used

A resin film containing 350 ppm to 3000 ppm of anti-adhesive agent is used. The absolute value of the refractive index difference of the anti-adhesive agent is less than 0.10 and the average particle size is 0.1 μm to 1.3 μm. The resin material in the molten state and the anti-adhesive agent are mixed, filtered and The resin film is prepared by an extrusion manufacturing method to ensure the anti-blocking and optical properties of the resin film.

Benefits of technology

It achieves stable winding and excellent anti-blocking properties of the resin film without peeling the liner, while maintaining high total light transmittance and low haze value, making it suitable for applications such as optical films.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118721931A_ABST
    Figure CN118721931A_ABST
Patent Text Reader

Abstract

Provided are a resin film, a laminated film, and a method for producing the resin film, which can achieve both excellent blocking resistance and optical characteristics. A resin film according to an embodiment of the present invention comprises a resin material as a matrix and an anti-blocking agent dispersed in the resin material. The content ratio of the anti-blocking agent is 350 ppm to 3000 ppm. The absolute value of the refractive index difference between the resin material and the anti-blocking agent is 0.10 or less.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field The present invention relates to a resin film, a laminated film, and a method for producing the resin film. Background Art Resin films are widely used in various industrial products. For example, it is known that a resin film is used as a surface protection film for protecting the surface of an adherend (see, for example, Patent Document 1). Such resin films are generally rolled up and recycled with a release liner attached to the surface of the resin film. However, when the resin film with the release liner attached is rolled up, the unevenness of the release liner may be transferred to the resin film, forming dents on the resin film. Therefore, the method of winding a resin film without attaching a release liner has been studied. However, when a resin film is wound into a roll without a release liner (release liner-free), there is a risk that the resin films will stick to each other and cause adhesion. In this regard, the resin film can be given anti-blocking properties by including an anti-blocking agent (hereinafter referred to as AB agent) in the resin film, but the optical properties of the resin film may be deteriorated. Therefore, it is desired that the resin film has both excellent anti-blocking properties and optical properties. Prior art literature Patent Literature Patent Document 1: Japanese Patent Application Publication No. 2017-32768 Summary of the invention Technical problem to be solved by the invention The present invention has been made to solve the above-mentioned problems of the prior art, and a main object of the present invention is to provide a resin film, a laminated film, and a method for producing a resin film that can have both excellent anti-blocking properties and optical properties. Means for solving technical problems

[0001] A resin film according to one embodiment includes a resin material as a matrix and an anti-blocking agent dispersed in the resin material. In the resin film, the anti-blocking agent is contained in an amount of 350 ppm to 3000 ppm. The absolute value of the difference in refractive index between the resin material and the anti-blocking agent is 0.10 or less.

[0002] The resin film according to the above [1], wherein the refractive index of the anti-blocking agent may be lower than the refractive index of the resin material.

[0003] In the resin film described in [1] or [2] above, the anti-blocking agent may have an average primary particle size of 0.1 μm to 1.3 μm.

[0004] The resin film according to any one of [1] to [3] above may have an indentation elastic modulus of 2.0N to 6.5N at 25°C.

[0005] The resin film according to any one of [1] to [4] above may have a dynamic friction coefficient of 1.0 or less.

[0006] The resin film according to any one of [1] to [5] may have a total light transmittance of 90% or more and a haze value of 1.0% or less.

[0007] The resin film according to any one of [1] to [6] may have an in-plane retardation Re (550) of 10 nm or less.

[0008] The resin film according to any one of [1] to [7], wherein the resin material may include a polycarbonate-based resin.

[0009] A laminated film according to another aspect of the present invention comprises the resin film according to any one of [1] to [8] above and a pressure-sensitive adhesive layer laminated on the resin film.

[0010] A method for manufacturing a resin film according to another aspect of the present invention comprises the following steps: a step of mixing a molten resin material and an anti-blocking agent to prepare a resin composition; a step of passing the resin composition through a filter; and a step of extruding the resin composition after passing through the filter. The content ratio of the anti-blocking agent in the resin composition is 350 ppm to 3000 ppm. The refractive index difference between the resin material and the anti-blocking agent is 0.10 or less.

[0011] The method for producing a resin film according to the above

[10] , wherein the filter may be a mesh having a mesh size of 0.035 mm to 0.070 mm.

[0012] The method for producing a resin film according to

[10] or

[11] may further include a step of winding up the resin film with a winding member. Effects of the Invention According to the embodiment of the present invention, a resin film and a laminated film having both excellent anti-blocking properties and excellent optical properties can be realized. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 This is a schematic cross-sectional view of a resin film according to one embodiment of the present invention. Figure 2 This is a schematic cross-sectional view of a laminated film according to another embodiment of the present invention. Figure 3 To include Figure 2 A schematic cross-sectional view of a laminated film optical component with a laminated film. Explanation of symbols 1. Resin film 2 adhesive layers 100 layers of laminated film DETAILED DESCRIPTION Representative embodiments of the present invention are described below, but the present invention is not limited to these embodiments. In addition, in order to make the description clearer, the accompanying drawings sometimes schematically represent the width, thickness, shape, etc. of each part compared with the embodiments, but this is only an example and does not limit the interpretation of the present invention. (Definition of Terms and Symbols) The definitions of terms and symbols in this specification are as follows. (1) Refractive index (nx, ny, nz) “nx” is the refractive index in the direction where the refractive index in the plane is maximum (ie, the slow axis direction), “ny” is the refractive index in the direction orthogonal to the slow axis in the plane (ie, the fast axis direction), and “nz” is the refractive index in the thickness direction. (2) In-plane phase difference (Re) "Re(λ)" is the in-plane phase difference measured at 23°C using light of wavelength λnm. For example, "Re(550)" is the in-plane phase difference measured at 23°C using light of wavelength 550nm. Re(λ) is obtained by using the formula: Re(λ) = (nx-ny) × d, when the thickness of the layer (film) is set to d (nm). (3) Retardation in the thickness direction (Rth) "Rth(λ)" is the phase difference in the thickness direction measured by light of wavelength λnm at 23°C. For example, "Rth(550)" is the phase difference in the thickness direction measured by light of wavelength 550nm at 23°C. Rth(λ) is obtained by the formula: Rth(λ) = (nx-nz) × d, when the thickness of the layer (film) is set to d (nm). A. Overall structure of resin film Figure 1 This is a schematic cross-sectional view of a resin film according to one embodiment of the present invention. The resin film 1 shown in the figure includes a resin material as a matrix and an anti-blocking agent (hereinafter referred to as AB agent) dispersed in the resin material. The content ratio (mass basis) of the AB agent in the resin film 1 is 350 ppm to 3000 ppm. The absolute value of the refractive index difference between the resin material and the AB agent is less than 0.10. When the content ratio of the AB agent and the absolute value of the refractive index difference between the resin material and the AB agent are within such a range, the resin film can be provided with excellent anti-blocking properties, and light diffusion caused by the AB agent can be suppressed. Therefore, in the resin film, the total light transmittance can be increased and the haze can be reduced. That is, a resin film having both excellent anti-blocking properties and optical properties can be realized. The content ratio (mass basis) of the AB agent in the resin film 1 is preferably 500 ppm to 3000 ppm, more preferably 500 ppm to 2000 ppm, and even more preferably 500 ppm to 1500 ppm. When the content ratio of the AB agent is within such a range, sufficient anti-blocking properties can be imparted to the resin film. The absolute value of the refractive index difference between the resin material and the AB agent is preferably 0.08 or less, more preferably 0.06 or less, and even more preferably 0.04 or less. The lower limit of the absolute value of the refractive index difference between the resin material and the AB agent is typically 0. When the absolute value of the refractive index difference between the resin material and the AB agent is within such a range, the total light transmittance can be further increased and the haze can be further reduced in the resin film. In one embodiment, the refractive index of the AB agent is lower than that of the resin material. When the refractive index of the AB agent is lower than that of the resin material and the refractive index difference between the resin material and the AB agent is within the above range, the total light transmittance in the resin film can be further increased and the haze can be further reduced. The refractive index of the AB agent is, for example, 1.35 or more, preferably 1.40 or more, and more preferably 1.45 or more. On the other hand, the refractive index of the AB agent is, for example, 1.65 or less, preferably 1.60 or less, and more preferably 1.55 or less. In addition, the refractive index of the AB agent can be measured at 25° C. using light with a wavelength of 590 nm, for example, according to JIS K7142. The refractive index of the resin material is, for example, 1.40 or more, preferably 1.45 or more, and more preferably 1.48 or more. On the other hand, the refractive index of the resin material is, for example, 1.70 or less, preferably 1.65 or less, and more preferably 1.60 or less. In addition, the refractive index of the resin material can be measured at 25° C. using light with a wavelength of 590 nm, for example, according to JIS K7142. The dynamic friction coefficient of the resin film 1 is, for example, 1.2 or less, and preferably 1.0 or less. On the other hand, the lower limit of the dynamic friction coefficient of the resin film 1 is typically 0.2. The dynamic friction coefficient of the resin film is measured, for example, in accordance with JIS K7142. When the dynamic friction coefficient of the resin film is within such a range, excellent anti-blocking properties can be stably imparted to the resin film. The resin film 1 has excellent anti-blocking properties as described above. Therefore, the resin film 1 can be wound into a roll without a release liner, typically. Thus, even when the resin film is wound into a roll, the formation of dents on the resin film can be suppressed. The indentation elastic modulus of the resin film 1 at 25° C. is, for example, 2.0 N to 6.5 N, or, for example, 2.5 N to 6.0 N. The indentation elastic modulus of the resin film can be measured by a nanoindentation method. Even if the resin film has an indentation elastic modulus within such a range, by winding the film without a release liner, it is possible to sufficiently suppress indentations in the resin film. The total light transmittance of the resin film 1 is, for example, 90.0% or more, more preferably 91.0% or more, and further preferably 92.0% or more. The upper limit of the total light transmittance of the resin film 1 is typically 100%. In addition, the total light transmittance of the resin film can be measured according to JIS R 3106-2019. The haze value of the resin film 1 is, for example, 1.0% or less, preferably 0.90% or less, more preferably 0.80% or less, and further preferably 0.70% or less. The lower limit of the haze value of the resin film 1 is typically 0%. The haze value of the resin film can be measured according to JIS K7136. The resin film 1 can be applied to any appropriate purpose, and can be preferably used as an optical film requiring excellent optical properties. Examples of the optical film include a protective layer attached to a polarizer, a blank film used in the manufacture of a phase difference film, and a base film of a laminated film requiring optical properties. B. Overall composition of laminated film like Figure 2 As shown, in one embodiment, a laminated film 100 includes a resin film 1 as a base film. The laminated film 100 shown in the figure is a film with an adhesive layer, and includes an adhesive layer 2 in addition to the resin film 1. The adhesive layer 2 is laminated on the resin film 1. The laminated film 100 may further include a release liner 3 in addition to the resin film 1 and the adhesive layer 2. The release liner 3 is typically temporarily attached to the adhesive layer 2 until the laminated film is attached to the adherend, and is peeled off from the adhesive layer 2 when the laminated film is attached. The release liner 3 is formed of any appropriate resin film that can be used as a release liner. A release treatment layer may also be provided on the contact surface of the release liner 3 with the adhesive layer 2. The laminated film 100 including the release liner 3 can be wound into a roll typically. Since the resin film has excellent anti-blocking properties, when the laminated film including the release liner is wound into a roll, even if the resin film and the release liner come into contact, they are prevented from sticking to each other and causing blocking. like Figure 3 As shown, the laminated film 100 can be preferably used as a surface protective film. At this time, the laminated film 100 is pasted on the surface of various adherends 5 to protect the surface of the adherends during inspection, processing and / or transportation of the adherends. The laminated film 100 is typically pasted on the surface of the adherend 5 using the adhesive layer 2. The details will be described later. There is a case where the adherend is subjected to optical inspection while the laminate film is attached to the adherend. In this case, since the resin film has excellent optical properties as described above, even if the laminate film is attached to the adherend and subjected to optical inspection, false inspections due to the resin film can be suppressed, and as a result, the adherend can be inspected with good accuracy. In other words, the results of inspecting the adherend with the laminate film attached can be integrated with the results of inspecting only the adherend. The resin film and the adhesive layer will be described in detail below. C. Resin film The resin film 1 is typically optically isotropic. In this specification, the term "optically isotropic" means that the in-plane retardation Re(550) and the retardation Rth(550) in the thickness direction are within the following ranges. The in-plane retardation Re(550) of the resin film 1 is, for example, 10 nm or less, preferably 5 nm or less, and more preferably 3 nm or less. On the other hand, the lower limit of the in-plane retardation Re(550) of the resin film 1 is typically 0 nm. When the in-plane retardation Re (550) of the resin film is within such a range, rainbow fringes of the resin film in optical inspection can be well suppressed, and as a result, the inspection accuracy of the adherend can be improved. The retardation Rth(550) in the thickness direction of the resin film 1 is in the range of, for example, -10 nm to +10 nm, or preferably -5 nm to +5 nm. The resin film 1 has a unit area of ​​10 cm 2 The number of defects with a maximum Feret diameter of 30 μm or more (hereinafter referred to as D30 / 10 cm of the resin film) 2 ) is, for example, 5 or less, preferably 3 or less. D30 / 10cm of the resin film 2 The lower limit of is typically 0. In addition, the number of defects can be measured using an optical microscope. If the D30 / 10cm of the resin film 2 When the thickness is within such a range, in the optical inspection of the adherend, erroneous inspection due to the resin film can be stably suppressed, and as a result, the inspection accuracy of the adherend can be improved. In addition, the resin film 1 has a thickness of 10 cm per unit area. 2 The number of defects having a maximum Feret diameter of less than 30 μm is not particularly limited. Examples of defects in the resin film 1 include aggregates of the AB agent; foreign matter such as fibers mixed in the resin material; gel-like matter generated by thermal crosslinking of the resin material; and bubbles caused by moisture in the resin. The thickness of the resin film 1 is, for example, 30 μm or more, preferably 40 μm or more. On the other hand, the thickness of the resin film 1 is, for example, 130 μm or less, preferably 120 μm or less. If the thickness of the resin film is in this range, the stiffness (elasticity) suitable for the peeling of the laminated film can be imparted to the resin film. Therefore, the resin film can be peeled off smoothly from the adherend. In addition, the in-plane phase difference of the resin film can be stably adjusted to the above range. The trouser-type tear strength of the resin film 1 is, for example, 0.09 N or more, preferably 0.10 N or more. The trouser-type tear strength of the resin film 1 is, for example, 0.4 N or less, preferably 0.3 N or less. If the trouser-type tear strength of the resin film is within this range, the laminated film can be smoothly peeled off from the adherend, and when the laminated film is peeled off from the adherend, the occurrence of rupture (cracking) in the laminated film can be suppressed. The trouser-type tear strength can be measured, for example, according to JIS K7128-1. C-1. Resin material The resin film 1 includes a resin material as a main component. Specific examples of the resin material include cycloolefin (COP) systems such as polynorbornene systems; polyester systems such as polyethylene terephthalate (PET) systems; cellulose resins such as triacetyl cellulose (TAC); polycarbonate (PC); (meth) acrylic acid systems; polyvinyl alcohol systems; polyamide systems; polyimide systems; polyether sulfone systems; polysulfone systems; polystyrene systems; polyolefin systems; transparent resins such as acetate systems. In addition, thermosetting resins or ultraviolet curing resins such as (meth) acrylic acid systems, urethane systems, (meth) acrylic urethane systems, epoxy systems, and silicone systems can also be cited. In addition, "(meth) acrylic acid resin" refers to acrylic resins and / or methacrylic resins. In addition, for example, glassy polymers such as siloxane polymers can also be cited. In addition, polymers described in Japanese Patent Publication No. 2001-343529 (WO01 / 37007) can also be used. As the material of the polymer, for example, a resin composition containing a thermoplastic resin having a substituted or unsubstituted imide group in a side chain, a thermoplastic resin having a substituted or unsubstituted phenyl and nitrile group in a side chain, and for example, a resin composition containing an alternating copolymer formed of isobutylene and N-methylmaleimide and an acrylonitrile-styrene copolymer can be used. The materials of the resin film can be used alone or in combination. In one embodiment, the resin material of the resin film 1 is amorphous. When the resin film is composed of an amorphous resin material, excellent transparency can be imparted to the resin film. Among these resin materials, preferably, PC-based resins and COP-based resins are used, and more preferably, PC-based resins are used. In one embodiment, the PC-based resin comprises at least a structural unit derived from a dihydroxy compound having a bonding structure represented by the following structural formula (1), and is produced by reacting a dihydroxy compound comprising at least a dihydroxy compound having at least one bonding structure -CH2-O- in the molecule with a carbonic acid diester in the presence of a polymerization catalyst. In other words, the PC-based resin comprises a structural unit derived from a dihydroxy compound and a carbonate group derived from a carbonic acid diester. [Chemical structure 1] Here, as the dihydroxy compound having a bonding structure represented by structural formula (1), any compound of any structure can be used, and multiple compounds can be used in combination, as long as it contains a structure having two alcoholic hydroxyl groups and a connecting group -CH2-O- in the molecule, and can react with a carbonic acid diester in the presence of a polymerization catalyst to produce a polycarbonate. In addition, as the dihydroxy compound used in the PC-based resin, a dihydroxy compound without the bonding structure shown in the above structural formula (1) can also be used in combination. Hereinafter, the dihydroxy compound having the bonding structure shown in the structural formula (1) is sometimes abbreviated as a dihydroxy compound (A), and the dihydroxy compound without the bonding structure shown in the structural formula (1) is sometimes abbreviated as a dihydroxy compound (B). (Dihydroxy compound (A)) The "linking group -CH2-O-" in the dihydroxy compound (A) refers to a structure in which atoms other than hydrogen atoms are bonded to each other to form a molecule. In the linking group, the atom to which at least an oxygen atom can be bonded or the atom to which a carbon atom and an oxygen atom can be bonded at the same time is preferably a carbon atom. The number of "linking groups -CH2-O-" in the dihydroxy compound (A) is preferably 1 or more, more preferably 2 to 4. Specific examples of the dihydroxy compound (A) include 9,9-bis(4-(2-hydroxyethoxy)phenyl)fluorene, 9,9-bis(4-(2-hydroxyethoxy)-3-methylphenyl)fluorene, 9,9-bis(4-(2-hydroxyethoxy)-3-isopropylphenyl)fluorene, 9,9-bis(4-(2-hydroxyethoxy)-3-isobutylphenyl)fluorene, 9,9-bis(4-(2-hydroxyethoxy)-3-tert-butylphenyl)fluorene, 9,9-bis(4-(2-hydroxyethoxy)-3-cyclohexylphenyl)fluorene, 9,9-bis(4-(2-hydroxyethoxy)-3-phenylphenyl)fluorene, 9,9-bis(4-(2-hydroxyethoxy)-3,5-dimethylphenyl)fluorene, 9,9 - Compounds having an aromatic group in the side chain and an ether group bonded to the aromatic group in the main chain, such as bis(4-(2-hydroxyethoxy)-3-tert-butyl-6-methylphenyl)fluorene and 9,9-bis(4-(3-hydroxy-2,2-dimethylpropoxy)phenyl)fluorene; compounds having bis[4-(2-hydroxyethoxy)phenyl]methane, bis[4-(2-hydroxyethoxy)phenyl]diphenylmethane, 1,1-bis[4-(2-hydroxyethoxy)phenyl]ethane, 1,1-bis[4-(2-hydroxyethoxy)phenyl]-1-phenylethane, 2,2-bis[4-(2-hydroxyethoxy)phenyl]propane, 2,2-bis[4-(2-hydroxyethoxy)-3-methylphenyl]propane, 2,2-bis[ 3,5-dimethyl-4-(2-hydroxyethoxy)phenyl]propane, 1,1-bis[4-(2-hydroxyethoxy)phenyl]-3,3,5-trimethylcyclohexane, 1,1-bis[4-(2-hydroxyethoxy)phenyl]cyclohexane, 1,4-bis[4-(2-hydroxyethoxy)phenyl]cyclohexane, 1,3-bis[4-(2-hydroxyethoxy)phenyl]cyclohexane, 2,2-bis[4-(2-hydroxyethoxy)-3-phenylphenyl]propane, 2,2-bis[(2-hydroxyethoxy)-3-isopropylphenyl]propane, 2,2-bis[3-tert-butyl-4-(2-hydroxyethoxy)phenyl]propane, 2,2-bis[4-(2-hydroxyethoxy)phenyl]butane, 2,2 - bis(hydroxyalkoxyaryl)alkanes such as bis[4-(2-hydroxyethoxy)phenyl]-4-methylpentane, 2,2-bis[4-(2-hydroxyethoxy)phenyl]octane, 1,1-bis[4-(2-hydroxyethoxy)phenyl]decane, 2,2-bis[3-bromo-4-(2-hydroxyethoxy)phenyl]propane, and 2,2-bis[3-cyclohexyl-4-(2-hydroxyethoxy)phenyl]propane; bis(hydroxyalkoxyaryl)cycloalkanes such as 1,1-bis[4-(2-hydroxyethoxy)phenyl]cyclohexane, 1,1-bis[3-cyclohexyl-4-(2-hydroxyethoxy)phenyl]cyclohexane, and 1,1-bis[4-(2-hydroxyethoxy)phenyl]cyclopentane;Dihydroxyalkoxydiaryl ethers such as 4,4'-bis(2-hydroxyethoxy)diphenyl ether and 4,4'-bis(2-hydroxyethoxy)-3,3'-dimethyldiphenyl ether; bishydroxyalkoxyaryl sulfides such as 4,4'-bis(2-hydroxyethoxyphenyl) sulfide and 4,4'-bis[4-(2-dihydroxyethoxy)-3-methylphenyl] sulfide; bishydroxyalkoxyaryl sulfoxides such as 4,4'-bis(2-hydroxyethoxyphenyl) sulfoxide and 4,4'-bis[4-(2-dihydroxyethoxy)-3-methylphenyl] sulfoxide; bishydroxyalkoxyaryl sulfoxides such as 4,4'-bis(2-hydroxyethoxyphenyl) sulfone and 4,4'-bis[4-(2-dihydroxyethoxy)-3-methylphenyl] sulfoxide; Bishydroxyalkoxyaryl sulfones exemplified by bis[4-(2-dihydroxyethoxy)-3-methylphenyl]sulfone; bishydroxyalkoxybenzenes exemplified by 1,4-bishydroxyethoxybenzene; 1,3-bis[2-[4-(2-hydroxyethoxy)phenyl]propyl]benzene; 1,4-bis[2-[4-(2-hydroxyethoxy)phenyl]propyl]benzene; 4,4'-bis(2-hydroxyethoxy)biphenyl; 1,3-bis[4-(2-hydroxyethoxy)phenyl]-5,7-dimethyladamantane; anhydrous sugar alcohols exemplified by dihydroxy compounds represented by the following formula (2); and compounds having a cyclic ether structure exemplified by spiroglycols represented by the following general formula (3). The dihydroxy compound (A) may be used alone or in combination. ; [Chemical structure 2] [Chemical structure 3] Among these dihydroxy compounds (A), the dihydroxy compounds represented by the above formula (2) are preferred. As the dihydroxy compounds represented by the above formula (2), isosorbide, isomannide and isoidide, which are in a stereoisomer relationship, can be mentioned. These substances can be used alone or in combination of two or more. Among the dihydroxy compounds (A), isosorbide obtained by dehydration condensation of sorbitol produced from various starches that are abundant in resources and easily available is most preferred from the viewpoints of easy availability and production, optical properties, and moldability. The proportion of the structural units derived from the dihydroxy compound (A) relative to all the structural units derived from the dihydroxy compound contained in the PC-based resin is, for example, 10 mol% or more, preferably 40 mol% or more, and more preferably 60 mol% or more. On the other hand, the proportion of the structural units derived from the dihydroxy compound (A) is, for example, 100 mol% or less, preferably 90 mol% or less, more preferably 80 mol% or less, and further preferably 70 mol% or less. When the proportion of the dihydroxy compound (A) is within the above range, the rainbow stripes of the resin film in the optical inspection can be stably suppressed. (Dihydroxy compound (B)) As a dihydroxy compound that becomes a structural unit of the PC-based resin, a dihydroxy compound (B) may be used together with the dihydroxy compound (A). When the dihydroxy compounds (A) and (B) are used in combination, rainbow fringes of the resin film in optical inspection can be more stably suppressed. The dihydroxy compound (B) is typically a dihydroxy compound other than the dihydroxy compound (A). Examples of the dihydroxy compound (B) include alicyclic dihydroxy compounds, aliphatic dihydroxy compounds, oxyalkylene glycols, aromatic dihydroxy compounds, and diols having a cyclic ether structure. The dihydroxy compound (B) may be used alone or in combination. Among the dihydroxy compounds (B), preferably, an alicyclic dihydroxy compound is used. The alicyclic dihydroxy compound is not particularly limited, and preferably includes compounds generally containing a 5-membered ring structure or a 6-membered ring structure. In addition, the 6-membered ring structure can be fixed to a chair shape or a boat shape by a covalent bond. When the alicyclic dihydroxy compound is a 5-membered ring or a 6-membered ring structure, the heat resistance of the obtained PC-based resin can be improved. The number of carbon atoms contained in the alicyclic dihydroxy compound is, for example, 70 or less, preferably 50 or less, and more preferably 30 or less. Specific examples of the alicyclic dihydroxy compound containing a 5-membered ring structure or a 6-membered ring structure include alicyclic dihydroxy compounds represented by the following general formula (I) or (II). HOCH2-R 1 -CH2OH (I) HO-R 2 -OH (II) (In formula (I) and (II), R 1 and R 2 They represent cycloalkylene groups having 4 to 20 carbon atoms. Cyclohexanedimethanol as the alicyclic dihydroxy compound represented by the general formula (I) includes R 1 The following general formula (Ia) (wherein R 3 represents an alkyl group having 1 to 12 carbon atoms or a hydrogen atom) and specifically includes 1,2-cyclohexanedimethanol, 1,3-cyclohexanedimethanol and 1,4-cyclohexanedimethanol. [Chemical structure 4] The tricyclodecane dimethanol or pentacyclopentadecanedimethanol as the alicyclic dihydroxy compound represented by the general formula (I) comprises R 1 These are various isomers represented by the following general formula (Ib) (wherein n represents 0 or 1). [Chemical structure 5] The alicyclic dihydroxy compound represented by the general formula (I) is decalinedimethanol or tricyclotetradecane dimethanol, which contains R 1 It is various isomers represented by the following general formula (Ic) (wherein m represents 0 or 1). Specific examples of such substances include 2,6-decalinedimethanol, 1,5-decalinedimethanol, and 2,3-decalinedimethanol. [Chemical structure 6] The alicyclic dihydroxy compound represented by the general formula (I) is a norbornane dimethanol comprising: 1 It is various isomers represented by the following general formula (Id). Specific examples of such substances include 2,3-norbornane dimethanol and 2,5-norbornane dimethanol. [Chemical structure 7] The alicyclic dihydroxy compound represented by the general formula (I) includes: 1 It is various isomers represented by the following general formula (Ie). Specific examples of such a substance include 1,3-adamantanedimethanol. [Chemical structure 8] Cyclohexanediol as the alicyclic dihydroxy compound represented by the general formula (II) includes R 2 The following general formula (IIa) (wherein R 3 represents an alkyl group having 1 to 12 carbon atoms or a hydrogen atom). Specific examples of such substances include 1,2-cyclohexanediol, 1,3-cyclohexanediol, 1,4-cyclohexanediol, and 2-methyl-1,4-cyclohexanediol. [Chemical structure 9] The tricyclodecanediol or pentacyclopentadecanediol as the alicyclic dihydroxy compound represented by the general formula (II) comprises R 2 These are various isomers represented by the following general formula (IIb) (wherein n represents 0 or 1). [Chemical structure 10] The alicyclic dihydroxy compound represented by the general formula (II) is decalindiol or tricyclotetradecanediol, which contains R2 These are various isomers represented by the following general formula (IIc) (wherein m represents 0 or 1). Specific examples of such substances include 2,6-decalin, 1,5-decalin, and 2,3-decalin. [Chemical structure 11] The norbornanediol as the alicyclic dihydroxy compound represented by the general formula (II) includes R 2 It is various isomers represented by the following general formula (IId). Specific examples of such substances include 2,3-norbornanediol and 2,5-norbornanediol. [Chemical structure 12] The alicyclic dihydroxy compound represented by the general formula (II) includes: 2 It is various isomers represented by the following general formula (IIe). Specific examples of such substances include 1,3-adamantanediol. [Chemical structure 13] Specific examples of the alicyclic dihydroxy compounds include preferably cyclohexanedimethanols, tricyclodecanedimethanols, adamantanediols, and pentacyclopentadecanedimethanols. From the viewpoint of easy availability and easy handling, more preferably 1,4-cyclohexanedimethanol, 1,3-cyclohexanedimethanol, 1,2-cyclohexanedimethanol, and tricyclodecanedimethanol. Still more preferably, tricyclodecanedimethanol is used. The proportion of the structural units derived from the dihydroxy compound (B) relative to all the structural units derived from the dihydroxy compound contained in the PC-based resin is, for example, 0 mol% or more, preferably 10 mol% or more, more preferably 20 mol% or more, and further preferably 30 mol% or more. On the other hand, the proportion of the structural units derived from the dihydroxy compound (B) is, for example, 90 mol% or less, preferably 60 mol% or less, and more preferably 40 mol% or less. The details of these PC-based resins are described in, for example, Japanese Patent Application Laid-Open No. 2012-31370 (Japanese Patent No. 5448264), and the description of the patent document is incorporated herein by reference. In one embodiment, the PC-based resin includes a structural unit derived from a dihydroxy compound (A) represented by the above formula (2), a structural unit derived from an alicyclic dihydroxy compound (B) represented by the above general formula (I), and a carbonate group connecting them. When the PC-based resin including these structural units is applied to a resin film, rainbow fringes of the resin film in optical inspection can be further stably suppressed. In such a PC-based resin, the molar ratio (A:B) of the structural unit derived from the dihydroxy compound (A) represented by the above formula (2) to the structural unit derived from the alicyclic dihydroxy compound (B) represented by the above general formula (I) is, for example, 5:5 to 9:1, preferably 6:4 to 8:2. In such a PC-based resin, the combination of the dihydroxy compound (A) represented by the above formula (2) and the alicyclic dihydroxy compound (B) represented by the above general formula (I) is preferably a combination of isosorbide and tricyclodecane dimethanol. C-2. Anti-adhesive agent The resin film 1 contains an AB agent in addition to the resin material. The AB agent is typically in a particle form, and is dispersed in the resin material as an aggregate in which a plurality of AB agent particles are aggregated. The average primary particle size of the AB agent is, for example, 0.1 μm to 1.3 μm, or preferably 0.1 μm to 1.0 μm. The average primary particle size of the AB agent can be measured by a laser diffraction method. When the average primary particle size of the AB agent is within such a range, it is possible to stably suppress erroneous detection of the AB agent (particularly, aggregates of the AB agent) in optical inspection of an adherend. The AB agent preferably has transparency. As materials constituting the AB agent, for example, metal oxides and resins can be cited. As metal oxides, for example, silicon dioxide, aluminum oxide, titanium oxide, zirconium oxide, and calcium oxide can be cited. As resins, for example, polymethyl methacrylate, polystyrene, polyurethane, (meth) acrylic resin, (meth) acrylic acid-styrene copolymer, benzoguanamine, melamine, polycarbonate, and silicone can be cited. The surface of the AB agent may be subjected to any appropriate surface modification. Examples of the surface modification include chemical modification, and preferably alkyl modification. The AB agents may be used alone or in combination of two or more. Among such AB agents, preferably, resins and metal oxides are used, more preferably, resins are used, and further preferably, (meth)acrylic acid-styrene copolymers are used. In addition to the above-mentioned resin material and AB agent, the resin film 1 may also contain any appropriate additives. Examples of additives include antioxidants, ultraviolet absorbers, light stabilizers, nucleating agents, fillers, pigments, surfactants, and antistatic agents. Any appropriate surface treatment layer may also be provided on the surface of the resin film 1 (the surface on the opposite side of the adhesive layer 2). Examples of surface treatment layers include easy-adhesion layers, easy-slip layers, antistatic layers, antireflection layers, and oligomer prevention layers. D. Method for producing resin film The resin film 1 can be manufactured by any appropriate method. In one embodiment, the method for manufacturing the resin film includes: a step of preparing a resin composition (preparation step); a step of passing the resin composition through a filter (filter passing step); and a step of extruding the resin composition after passing through the filter (extrusion molding step). In the preparation step, typically, the resin material is melted, and then the molten resin material is mixed with the AB agent to prepare the resin composition. The resin material before melting may have any appropriate shape. In one embodiment, the resin material is pelletized in advance. The method for pelletizing the resin material is not particularly limited, and may be a strand cutting method or a thermal cutting method. The details of the pellet preparation process are described, for example, in Japanese Patent Publication No. 2013-181105. The description of the patent document is cited as a reference in this specification. Next, the resin material (representatively, pellets) is heated to melt. The heating temperature can be any appropriate value corresponding to the resin material. In addition, the molten resin material is mixed with the AB agent. Thus, a molten resin composition is prepared. The range of the content ratio of the AB agent in the resin composition is, for example, the same as the range of the content ratio of the AB agent in the above-mentioned resin film 1. In the filter passing step, the molten resin composition is passed through a filter, thereby removing foreign matter and / or aggregates of the AB agent contained in the resin composition from the resin composition. The filter may have any appropriate structure. Examples of the filter include a mesh and a disc filter, and a mesh is preferred. The mesh size of the screen is, for example, 0.080 mm or less, preferably 0.070 mm or less, and more preferably 0.055 mm or less. When the screen has such a mesh size, it is possible to suppress the mixing of foreign matter and / or agglomerates of the AB agent having a maximum Feret diameter of 30 μm or more into the produced resin film. Therefore, defects in the resin film (specifically, agglomerates of foreign matter and / or the AB agent) can be reduced, and the D30 / 10 cm of the resin film can be increased. 2 Stably adjust to the above range. On the other hand, the mesh size of the screen is, for example, 0.025 mm or more, preferably 0.035 mm or more. When the screen has such a mesh size, the resin composition can pass through the screen smoothly. Therefore, the retention of the resin composition can be suppressed, and the resin composition can be suppressed from being overheated. Thus, the generation of gel-like substances caused by thermal crosslinking of the resin material can be suppressed. As a result, defects in the resin film (specifically gel substances) can be reduced, and the D30 / 10cm of the resin film can be reduced. 2 More stable adjustment to the above range. In the extrusion molding step, the molten resin after passing through the filter is typically extruded into a film shape using a die head, thereby preparing the resin film 1. The above-mentioned preparation step, filter passing step and extrusion molding step can be carried out by any appropriate film forming device. The method for manufacturing the resin film 1 may further include a step (winding step) of winding the resin film with a winding member in addition to the above-mentioned preparation step and the above-mentioned film-making step. In the winding step, the winding member winds the resin film 1 into a roll. The winding member typically has a cylindrical shape and can rotate around a bobbin. Since the resin film 1 has excellent anti-blocking properties, even if the resin film 1 is wound into a roll, it is possible to fully suppress the resin films 1 from sticking to each other. Through the above, the resin film 1 is manufactured. E. Adhesive layer The adhesive layer 2 is provided on the surface of the resin film 1 in order to attach the laminated film 100 to the surface of an adherend. The adhesive layer 2 is composed of an adhesive (pressure-sensitive adhesive). As the adhesive constituting the adhesive layer 2, for example, (meth) acrylic adhesives, rubber adhesives, silicone adhesives, polyester adhesives, urethane adhesives, epoxy adhesives, and polyether adhesives can be cited. By adjusting the type, quantity, combination and proportion of monomers forming the base resin of the adhesive, as well as the amount of the cross-linking agent, the reaction temperature, the reaction time, etc., an adhesive having desired properties corresponding to the purpose can be prepared. The base resin of the adhesive can be used alone or in combination of two or more. In one embodiment, the adhesive layer 2 is composed of a (meth)acrylic adhesive (a (meth)acrylic adhesive composition). When the adhesive layer is composed of a (meth)acrylic adhesive, the peeling force of the laminated film can be preferably adjusted. The (meth)acrylic adhesive composition typically contains a (meth)acrylic polymer as a main component. The content of the (meth)acrylic polymer in the solid content of the adhesive composition is, for example, 50% by mass or more, preferably 70% by mass or more, and more preferably 90% by mass or more. On the other hand, the upper limit of the content of the (meth)acrylic polymer is typically 100% by mass. The (meth)acrylic acid polymer contains a structural unit derived from an alkyl (meth)acrylate. In the (meth)acrylic acid polymer, the content of the structural unit derived from the alkyl (meth)acrylate is, for example, 70% by mass or more, preferably 80% by mass or more. On the other hand, the upper limit of the content of the structural unit derived from the alkyl (meth)acrylate is typically 90% by mass. As the alkyl group of the (meth)acrylic acid alkyl ester, for example, a linear or branched alkyl group having 1 to 18 carbon atoms can be mentioned. The average number of carbon atoms of the alkyl group is preferably 3 to 12, more preferably 3 to 8. Among the (meth)acrylic acid alkyl esters, butyl acrylate and 2-ethylhexyl acrylate can be preferably mentioned, and 2-ethylhexyl acrylate can be more preferably mentioned. In addition to the structural units derived from the alkyl (meth)acrylate, the (meth)acrylic polymer may also contain structural units derived from comonomers that can polymerize with the alkyl (meth)acrylate. Examples of the comonomers include carboxyl group-containing monomers, hydroxyl group-containing monomers, amide group-containing monomers, aromatic ring-containing (meth)acrylates, and heterocyclic vinyl monomers. The comonomers may be used alone or in combination. Among the comonomers, preferably, a carboxyl group-containing monomer and a hydroxyl group-containing monomer are mentioned. In one embodiment, the (meth)acrylic polymer includes a structural unit derived from an alkyl (meth)acrylate, a structural unit derived from a carboxyl group-containing monomer, and a structural unit derived from a hydroxyl group-containing monomer. The carboxyl group-containing monomer is a compound containing a carboxyl group and a polymerizable unsaturated double bond such as a (meth)acryloyl group and a vinyl group in its structure. Examples of the carboxyl group-containing monomer include (meth)acrylic acid, carboxyethyl (meth)acrylate, maleic acid, fumaric acid, and crotonic acid, and preferably (meth)acrylic acid. When a (meth)acrylic acid polymer includes a structural unit derived from a carboxyl group-containing monomer, the adhesive properties of the adhesive layer can be improved. When the (meth) acrylic acid polymer includes a structural unit derived from a carboxyl group-containing monomer, the content of the structural unit derived from the carboxyl group-containing monomer is, for example, 0.01% by mass or more, preferably 0.10% by mass or more. On the other hand, the content of the structural unit derived from the carboxyl group-containing monomer is, for example, 10% by mass or less, preferably 5.0% by mass or less, more preferably 1.0% by mass or less, and further preferably 0.5% by mass or less. The hydroxyl-containing monomer is a compound containing a hydroxyl group and a polymerizable unsaturated double bond such as a (meth)acryloyl group and a vinyl group in its structure. As the hydroxyl-containing monomer, for example, 2-hydroxyethyl (meth)acrylate, 3-hydroxypropyl (meth)acrylate, 8-hydroxyoctyl (meth)acrylate, 12-hydroxylauryl (meth)acrylate, (meth)acrylate (4-hydroxymethylcyclohexyl) ester can be cited, preferably 2-hydroxyethyl (meth)acrylate and 4-hydroxybutyl (meth)acrylate can be cited, and more preferably 4-hydroxybutyl (meth)acrylate can be cited. When the (meth)acrylic polymer contains a structural unit derived from a hydroxyl-containing monomer, the durability of the adhesive layer can be improved. When the (meth)acrylic acid polymer contains a structural unit derived from a hydroxyl-containing monomer, the content of the structural unit derived from the hydroxyl-containing monomer is, for example, 0.01% by mass or more, preferably 1.0% by mass or more, more preferably 5.0% by mass or more, and further preferably 8.0% by mass or more. The upper limit of the content of the structural unit derived from the hydroxyl-containing monomer is typically 10% by mass. The weight average molecular weight Mw of the (meth)acrylic polymer is, for example, 100,000 to 2,000,000, and preferably 200,000 to 1,000,000. The weight average molecular weight Mw can be calculated from the result of GPC measurement in terms of styrene. In addition, the (meth)acrylic adhesive may further contain a crosslinking agent. Representative examples of the crosslinking agent include organic crosslinking agents and functional metal chelates, and preferably organic crosslinking agents. Examples of the organic crosslinking agent include isocyanate crosslinking agents, peroxide crosslinking agents, epoxy crosslinking agents, and imine crosslinking agents, and more preferably isocyanate crosslinking agents. The content of the crosslinking agent is, for example, 0.01 parts by mass or more, preferably 0.5 parts by mass or more, more preferably 0.8 parts by mass or more, and further preferably 1.2 parts by mass or more, relative to 100 parts by mass of the (meth)acrylic polymer. On the other hand, the content of the crosslinking agent is, for example, 10 parts by mass or less, preferably 5 parts by mass or less, more preferably 2.5 parts by mass or less, and further preferably 2.0 parts by mass or less. When the content of the crosslinking agent is within this range, the peeling force of the laminated film can be preferably adjusted. Furthermore, the (meth)acrylic pressure-sensitive adhesive may contain various additives (for example, a silane coupling agent, a polymerization initiator, a solvent, and a cross-linking catalyst) at appropriate ratios. The details of these adhesives are described in, for example, Japanese Patent Application Publication No. 2006-183022, Japanese Patent Application Publication No. 2015-199942, Japanese Patent Application Publication No. 2018-053114, Japanese Patent Application Publication No. 2016-190996, and International Publication No. 2018 / 008712, and the descriptions of these publications are incorporated herein by reference. The thickness of the adhesive layer 2 is typically 1 μm or more, preferably 5 μm or more. On the other hand, the thickness of the adhesive layer 2 is, for example, 30 μm or less, preferably 15 μm or less. The storage elastic modulus of the adhesive layer 2 at 25° C. is, for example, 5.0×10 4 Pa~5.0×10 6 Pa, preferably 7.5×10 4 Pa~2.5×10 6 When the storage elastic modulus of the pressure-sensitive adhesive layer is within such a range, wettability to an adherend is good and adhesive strength can be sufficient. The adhesive layer 2 is formed on the resin film 1 by any appropriate means. To form the adhesive layer 2 on the resin film 1, for example, the adhesive may be directly applied to the resin film 1 or applied to another substrate to form an adhesive layer and then transferred to the resin film 1. F. Application of laminated films like Figure 2 and Figure 3 As shown, in one embodiment, the laminated film 100 is attached to the surface of the adherend 5 by the adhesive layer 2 after the release liner 3 is peeled off from the adhesive layer 2 . The adherend 5 includes, for example, optical components and electronic components, preferably optical components. Representative optical components include polarizing plates, phase difference films, optical laminates including polarizing plates and / or phase difference films, displays, imaging devices, lenses, and (half) mirrors. Figure 3 To include Figure 2 Schematic cross-sectional view of an optical component with a laminated film. The optical component with a laminated film 200 shown in the figure includes an optical component 5a as an adherend and a laminated film 100 as a surface protective film. The laminated film 100 is attached to the surface of the optical component 5a via an adhesive layer 2. In one embodiment, the optical component 5a included in the optical component with a laminated film 200 is a polarizing plate. The thickness of the polarizing plate is, for example, 5 μm to 200 μm. The thickness of the resin film 1 of the laminated film 100 is, for example, 0.1 to 1.05, preferably 0.15 to 1.0, relative to the thickness of the adherend (optical component). If the thickness ratio of the resin film to the adherend is within this range, the adherend (optical component) can be inspected with greater accuracy even when the laminated film is attached to the adherend and subjected to optical inspection. Such an optical component 200 with a laminated film is typically subjected to optical inspection. The optical inspection is not particularly limited, and an example thereof may be an automatic optical inspection (AOI). Examples of the automatic optical inspection include a foreign matter inspection for inspecting foreign matter contained in an optical component and a bubble inspection for inspecting bubbles contained in an optical component. In such an optical inspection, since false detection caused by the resin film can be sufficiently suppressed, the optical component can be inspected with good accuracy even when the laminated film is attached to the optical component. Thereafter, the laminate film 100 can be peeled off from the surface of the optical component 5 a (adherend) at a desired timing. The peeling force of the laminated film 100 with respect to the acrylic plate is, for example, 3.5 N / 25 mm or less, preferably 3.0 N / 25 mm or less, more preferably 2.5 N / 25 mm or less, and further preferably 2.0 N / 25 mm or less at a pulling speed of 30 m / min and a peeling angle of 180°. If the laminated film has such a peeling force, the laminated film can be smoothly peeled off from the adherend after optical inspection. On the other hand, the peeling force of the laminated film 100 to the acrylic plate is, for example, 0.5N / 25mm or more, preferably 1.0N / 25mm or more, preferably 1.2N / 25mm or more. If the laminated film has such a peeling force, the laminated film can stably follow the surface of the adherend when the laminated film is attached to the adherend. In addition, the above-mentioned peeling force can be measured according to JIS Z0237, and more specifically, it can be measured using the following peeling force test. (Peel force test) The laminated film was cut into strips of 25 mm × 100 mm to prepare a sample; the sample was pressed onto the surface of an acrylic plate using an adhesive layer with a roller at a pressure of 0.25 MPa and a conveying speed of 0.3 m / min; the sample attached to the acrylic plate was left to stand at a temperature of 23°C and a relative humidity of 50% for 30 minutes, and then peeled off at a peeling angle of 180° and a pulling speed of 30 m / min under the same environment to measure the peeling force. [Example] Hereinafter, the present invention will be specifically described using examples, but the present invention is not limited to these examples. In addition, the measuring methods of each characteristic are as follows. (1) Optical properties (1-1) Total light transmittance The total light transmittance of the resin films of Examples and Comparative Examples was measured using a spectrophotometer (trade name: U-4100, manufactured by Hitachi High-Tech Science Co., Ltd.) in accordance with JISR 3106-2019. (1-2) Haze value The haze values ​​of the resin films of Examples and Comparative Examples were measured using a haze meter (trade name: HAZE METER HM-150, manufactured by Murakami Color Research Laboratory Co., Ltd.) in accordance with JIS K7136. In addition, the optical properties of the resin film were evaluated according to the following criteria, and the results are shown in Table 1. ○: The total light transmittance of the resin film is 90% or more and the haze value is 1.0% or less ×: The total light transmittance of the resin film is less than 90% and / or the haze value exceeds 1.0% (2) Sliding properties (anti-adhesion properties) The base films of the resin films obtained in Examples and Comparative Examples were rubbed against each other, and the sliding property (anti-blocking property) was evaluated according to the following criteria. The results are shown in Table 1. Furthermore, if the slidability is sufficient, even if the resin film is simply wound into a roll, the blocking of the resin films can be sufficiently suppressed. ◎: The substrate films do not stick to each other and slide well ○: The base films do not stick to each other, but they are slightly slippery compared to ◎ ×: The base films stick to each other and do not slide <<Preparation Example 1: PC-based resin film>> Relative to 81.98 parts by mass of isosorbide (ISB), 47.19 parts by mass of tricyclodecane dimethanol (TCDDMA), 175.1 parts by mass of diphenyl carbonate (DPC), and 0.979 parts by mass of 0.2% aqueous solution of cesium carbonate as a catalyst are put into a reaction vessel, and under a nitrogen environment, the heating tank temperature is heated to 150°C as the first stage of the reaction and stirred as needed, while the raw materials are dissolved (about 15 minutes). Then, the pressure is changed from normal pressure to 13.3kPa, and the heating tank temperature is raised to 190°C in 1 hour, and the generated phenol is discharged out of the reaction vessel. After the entire reaction vessel is kept at 190°C for 15 minutes, as the second stage of the process, the pressure in the reaction vessel is 6.67kPa, and the heating tank temperature is raised to 230°C in 15 minutes, and the generated phenol is discharged out of the reaction vessel. Since the stirring torque of the stirrer increases, the pressure in the reaction vessel is reduced to 0.200 kPa or less in order to raise the temperature to 250° C. in 8 minutes and remove the generated phenol. After reaching the specified stirring torque, the reaction is terminated and the generated reactant is extruded into water to obtain PC resin pellets. [Example 1, Comparative Examples 1 and 3] The pellets of the PC resin obtained in Preparation Example 1 were vacuum dried at 100°C for 12 hours. Then, the pellets of the PC resin and an AB agent (polymer particles, average primary particle size: 0.5 μm, refractive index: 1.5, manufactured by Sekisui Chemicals Co., Ltd., trade name: Techpolymer) were supplied to a film forming apparatus. The addition ratio of the AB agent to the total amount of the pellets and the AB agent and the average primary particle size of the AB agent are shown in Table 1. The film forming apparatus includes a single screw extruder (manufactured by Toshiba Machine Co., Ltd., cylinder setting temperature: 250°C), a screen with a mesh size of 0.045 mm, a T-die (width 1700 mm, setting temperature: 250°C), a casting roll (setting temperature: 60°C), and a winding member. More specifically, the pellets and the AB agent are supplied to a single screw extruder and heated. Thus, the pellets are melted, and the molten PC resin and the AB agent are mixed to prepare a resin composition. Thereafter, the resin composition is extruded from the single screw extruder and sequentially passes through a screen and a T die. Thus, a PC resin film having a thickness of 40 μm is prepared. After passing through a casting roll, the PC resin film is wound using a winding member. Through the above, a PC-based resin film (resin film) was obtained. [Example 2] A PC-based resin film (resin film) was obtained in the same manner as in Example 1, except that the AB agent (polymer particles, average primary particle size: 0.5 μm, refractive index: 1.5, manufactured by Sekisui Chemicals, trade name: Techpolymer) was replaced with AB agent (average primary particle size: 1.0 μm, refractive index: 1.5, manufactured by Sekisui Chemicals, trade name: Techpolymer) and the addition ratio of the AB agent relative to the total amount of the pellets and the AB agent was changed to 500 ppm. [Example 3] A PC-based resin film (resin film) was obtained in the same manner as in Example 1, except that the AB agent (polymer particles, average primary particle size: 0.5 μm, refractive index: 1.5, manufactured by Sekisui Chemicals Co., Ltd., trade name: Techpolymer) was replaced with methyl-modified silica particles (average primary particle size: 0.5 μm, refractive index: 1.43, manufactured by Nippon Shokubai Co., Ltd., trade name: Seahostar KE). [Comparative Example 2] A PC-based resin film (resin film) was obtained in the same manner as in Example 1 except that the AB agent (polymer particles, average primary particle size: 0.5 μm, refractive index: 1.5, manufactured by Sekisui Chemicals Co., Ltd., trade name: Techpolymer) was replaced with magnesium fluoride nanoparticles (average primary particle size: 0.5 μm, refractive index: 1.38, manufactured by Stella-Chemifa). Table 1 [evaluate] As can be seen from Table 1, when the content of the AB agent in the resin film is 350 ppm or more, the resin film has excellent anti-blocking properties. In addition, when the content of the AB agent in the resin film is 3000 ppm or less and the absolute value of the refractive index difference between the resin material and the AB agent is 0.10 or less, the total light transmittance can be improved and the haze value can be reduced in the resin film. Industrial Applicability The resin film of the present invention can be applied to various industrial products, and can be particularly preferably used as an optical film (for example, a protective layer of a polarizer, a raw material of a phase difference film, and a base film of a surface protection film).

Claims

1. A resin film comprising a resin material as a matrix and an anti-blocking agent dispersed in the resin material, in, The content of the anti-adhesive agent is 350ppm to 3000ppm. An absolute value of a refractive index difference between the resin material and the anti-blocking agent is 0.10 or less.

2. The resin film according to claim 1, in, The refractive index of the anti-blocking agent is lower than the refractive index of the resin material.

3. The resin film according to claim 1, in, The average primary particle size of the anti-blocking agent is 0.1 μm to 1.3 μm. The resin film according to claim 1 , which has an indentation elastic modulus of 2.0 N to 6.5 N at 25° C. The resin film according to claim 1 , which has a dynamic friction coefficient of 1.0 or less. 6 . The resin film according to claim 1 , which has a total light transmittance of 90% or more and a haze value of 1.0% or less. The resin film according to claim 1 , wherein the in-plane retardation Re (550) is 10 nm or less.

8. The resin film according to claim 1, in, The resin material includes a polycarbonate-based resin. 9 . A laminated film comprising the resin film according to claim 1 and a pressure-sensitive adhesive layer laminated on the resin film.

10. A method for producing a resin film, comprising the following steps: A step of mixing a molten resin material and an anti-blocking agent to prepare a resin composition; a step of passing the resin composition through a filter; and The resin composition after passing through the filter is extruded and molded. in, The content ratio of the anti-blocking agent in the resin composition is 350 ppm to 3000 ppm, and the refractive index difference between the resin material and the anti-blocking agent is 0.10 or less.

11. The method for producing a resin film according to claim 10, in, The filter is a sieve, and the mesh size of the sieve is 0.035 mm to 0.070 mm. 12 . The method for producing a resin film according to claim 10 , further comprising a step of winding the resin film with a winding member.