NA anhydride modified coal tar and preparation method thereof
The preparation method of NA acid anhydride-modified coal tar solves the problem of insufficient density and calorific value caused by differences in coal tar components, improves the performance and yield of high-density fuel, and achieves efficient utilization of coal tar and resource conservation. .
Patent Information
- Application Number
- CN202411093395.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-10-01
AI Technical Summary
When coal tar is used to produce high-density fuels, due to the large differences in components, the density and volumetric calorific value cannot meet the demand, and traditional hydrotreating and distillation methods have problems of resource waste and insufficient performance.
NA acid anhydride is used as a modifier to increase the content of three-ring or higher components in coal tar through a ring-enhancing modification reaction. It combines extraction and rotary evaporation separation technology to prepare high-density fuel. Lewis acid catalyst and dichloromethane are used as solvents. and extraction agent, control the reaction temperature and time, and increase the density and calorific value of the fuel.
It significantly increases the density and volume calorific value of high-density fuel, reduces production costs, achieves efficient utilization of coal tar, simplifies the process, reduces the generation of impurities, and improves fuel performance and yield.
Smart Images

Figure BDA0004987198030000051 
Figure BDA0004987198030000081 
Figure BDA0004987198030000111
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of coal tar, and particularly relates to NA anhydride modified coal tar and a preparation method thereof. Background Art
[0002] At present, there are two main ways to utilize coal tar: one is to produce clean gasoline and diesel through hydrogenation to replace part of crude oil, which can also reduce the use of crude oil and reduce the dependence on crude oil to a certain extent; the other is to extract some special compounds in coal tar through various separation methods for use as basic chemical raw materials. However, with the increasingly severe environmental problems and the continuous development of new energy technologies in recent years, reprocessing to produce gasoline and diesel does not conform to the current development trend; and currently, the extraction of various chemical raw materials from coal tar is mainly carried out by distillation, which causes great waste of resources in the production process. Therefore, other methods should be developed to achieve efficient utilization of coal tar.
[0003] With the rapid development of the aerospace industry, the demand for high-density fuels has increased year by year, and higher requirements have been placed on their performance. Traditional petroleum-based high-density fuels are limited by raw materials, and their density and volume calorific value have gradually failed to meet the demand, while new biomass-based high-density fuels cannot be produced on a large scale industrially due to insufficient current technology.
[0004] Coal tar is a complex mixture of highly aromatic hydrocarbons, most of which are polycyclic and condensed ring compounds with or without side chains and heterocyclic compounds containing oxygen, sulfur and nitrogen. Its unique composition gives it the characteristics of high density and volume calorific value, making it very suitable for processing and producing high-density fuels. However, due to the large differences in its components, it should be modified before producing high-density fuels to make it more suitable for producing high-density fuels. Summary of the invention
[0005] In order to overcome the problem of large differences in components of high-density fuel produced from coal tar, the present invention provides a NA anhydride modified coal tar and a preparation method thereof.
[0006] In order to achieve the above object, the present invention adopts the following technical scheme:
[0007] A preparation method of NA anhydride modified coal tar comprises the following steps: coal tar, a modifier, a solvent and a catalyst are mixed to carry out a ring-increasing modification reaction to obtain a first crude product, the modifier adopts NA anhydride, and the mass ratio of coal tar to the modifier is 1:(1-2), the ring-increasing modification reaction of the first crude product is terminated to obtain a second crude product, the second crude product is mixed with an extractant to carry out extraction, and then impurities are separated by rotary evaporation to obtain modified coal tar, wherein the impurities include a catalyst and a solvent.
[0008] Furthermore, the catalyst is Lewis acid, the amount of the catalyst is 5% to 10% of the mass of the coal tar, the solvent is dichloromethane, and the volume ratio of the coal tar to the solvent is 1: (1 to 2).
[0009] Furthermore, the reaction temperature for the mixed ring-addition modification reaction is 80-120°C.
[0010] Furthermore, the extractant is dichloromethane, the volume ratio of the second crude product to the extractant is 1:1, and the extraction time is 5 to 10 minutes.
[0011] Furthermore, the first crude product is mixed with a hydrochloric acid solution to obtain a second crude product, and the mass percentage concentration of the hydrochloric acid solution is 10%.
[0012] Furthermore, coal tar is composed of 12% to 20% straight-chain alkanes, 20% to 26% monocyclic, 40% to 50% bicyclic and 10% to 20% tricyclic and above compounds.
[0013] Furthermore, the solvent is CH2Cl2, and the catalyst is anhydrous aluminum chloride, anhydrous ferric chloride, anhydrous tin tetrachloride or anhydrous boron trifluoride.
[0014] Furthermore, the reaction pressure of the mixing is 101.325 kPa, the reaction time of the mixing is 24 h, and the stirring rate of the mixing is 200-300 rpm / min.
[0015] Furthermore, the temperature of the rotary evaporation is 30-40° C., the speed of the rotary evaporation is set to 50-80 rpm / min, and the rotary evaporation is stopped after no bubbles are generated.
[0016] A NA anhydride modified coal tar is prepared by adopting the preparation method of the NA anhydride modified coal tar.
[0017] Compared with the prior art, the present invention has the following beneficial technical effects:
[0018] The invention provides a method for preparing NA anhydride modified coal tar, using coal tar as raw material, which has a wide range of sources and low production cost, and has high product added value and good economic benefits. The target product has high density, and can be subsequently treated simply to become an ideal high-density fuel blending component, and can also be applied to other fields. The process is simple, a large amount of impurities will not be generated during the reaction, and the product and the catalyst solvent are easy to separate.
[0019] The invention provides a method for preparing NA anhydride modified coal tar. For the first time, a modifier is used to perform ring-increasing modification on coal tar fraction oil, thereby increasing the content of components with three or more rings in the coal tar fraction oil by about 20%, significantly increasing the density and volume calorific value, and significantly alleviating the problem of density reduction caused by hydrogenation treatment, thereby producing high-density fuel with excellent performance; at the same time, the yield of high-density fuel can be greatly improved, thereby realizing high-value-added utilization of coal tar. DETAILED DESCRIPTION
[0020] The present invention is described in further detail below:
[0021] A method for preparing NA anhydride modified coal tar comprises the following steps:
[0022] Step 1: coal tar, a modifier, a solvent and a catalyst are put into a reactor and mixed evenly, and a Diels-Alder reaction is carried out under the action of the catalyst to perform ring-addition modification;
[0023] The Diels-Alder reaction, also known as the Diels-Alder reaction or diene synthesis reaction, is a very important cycloaddition reaction in organic chemistry.
[0024] Step 2: Refining the crude product after ring addition modification to separate impurities such as catalyst and solvent.
[0025] The composition of coal tar should be 12% to 20% straight-chain alkanes, 20% to 26% monocyclic, 40% to 50% bicyclic and 10% to 20% tricyclic and above compounds; the modifier is NA anhydride, the mass ratio of coal tar to modifier is 1:1 to 2, the reaction solvent is dichloromethane, and the volume ratio of solvent to coal tar is 1 to 2:1.
[0026] The reaction pressure of the ring-addition modification reaction in step 1 is 101.325 kPa, the reaction temperature is 80-120° C., the reaction time is 24 h, and the magnetic stirring rate during the reaction is 200-300 rpm / min.
[0027] The reaction catalyst is a Lewis acid catalyst, the preferred catalyst is AlCl3, and the amount of the catalyst used is 5-10% of the mass of the coal tar.
[0028] The separation and purification methods are extraction and rotary evaporation.
[0029] Before the extraction process, the reaction was terminated with 10% hydrochloric acid solution. This step was carried out in a pear-shaped flask and lasted for 10 minutes.
[0030] The extraction process is carried out in a separatory funnel, the extractant is dichloromethane, the volume ratio of the extractant to the product in the pear-shaped bottle is 1:1, and the extraction time is 5 to 10 minutes.
[0031] The rotary evaporation process was carried out in a rotary evaporator at a temperature of 30-40°C and a rotation speed of 50-80 rpm / min. The experiment was stopped when no bubbles were generated.
[0032] The present invention is further described in detail below in conjunction with embodiments:
[0033] Example 1
[0034] In this embodiment, toluene is used to simulate coal tar distillate oil for reaction, and the specific implementation method is as follows:
[0035] Weigh 10g toluene, 10g NA anhydride and 20ml dichloromethane into a 100ml Schlenk tube (reaction tube), add 0.5g anhydrous aluminum chloride catalyst and seal it. Fix the Schlenk tube with an iron stand, place it in a DF-101S thermal collector constant temperature heating magnetic stirrer, and heat it in an oil bath. Set the temperature of the DF-101S thermal collector constant temperature heating magnetic stirrer to 100°C, and the stirring speed to 250rpm / min. Start timing after the temperature reaches 100°C and is basically stable. End the reaction after 24 hours. After the reaction is completed, place the Schlenk tube above the DF-101S thermal collector constant temperature heating magnetic stirrer and cool it naturally for 1h.
[0036] Transfer the reaction product to a 250ml pear-shaped bottle, add 20ml 10% hydrochloric acid solution and wait for 10min to terminate the reaction. Transfer all the substances to a separatory funnel, add dichloromethane extractant three times, add 20ml each time, then let it stand for 10min to separate the solution, and collect the crude product after removing the catalyst. Place the collected crude product in a rotary evaporator for rotary evaporation, the rotary temperature is 39℃, the speed is set to 50rpm / min, and the experiment is terminated when no bubbles are generated.
[0037] The reaction that occurs during the modification process is shown below:
[0038]
[0039] Example 2
[0040] Different from Example 1, the modification reaction temperature is set to 80°C.
[0041] Example 3
[0042] Different from Example 1, the modification reaction temperature is set to 90°C.
[0043] Example 4
[0044] Different from Example 1, the modification reaction temperature is set to 110°C.
[0045] Example 5
[0046] Different from Example 1, the modification reaction temperature is set to 120°C.
[0047] The experimental results of the yield changes at different reaction temperatures in Examples 1 to 5 are shown in Table 1.
[0048] Table 1 Yield changes at different reaction temperatures
[0049] Example Modification temperature ℃ Yield % Example 1 100 58.87 Example 2 80 46.32 Example 3 90 51.52 Example 4 110 62.19 Example 5 120 64.67
[0050] Example 6
[0051] The difference from Example 1 is that the catalyst for the modification reaction is anhydrous ferric chloride.
[0052] Example 7
[0053] The difference from Example 1 is that the catalyst for the modification reaction is anhydrous tin tetrachloride.
[0054] Example 8
[0055] The difference from Example 1 is that the catalyst for the modification reaction is anhydrous boron trifluoride.
[0056] The reaction results under different catalyst conditions of Examples 1 and 6 to 8 are shown in Table 2.
[0057] Table 2 Yield changes under different catalysts
[0058] Example catalyst Yield % Example 1 <![CDATA[AlCl3]]> 58.87 Example 6 <![CDATA[FeCl3]]> 47.44 Example 7 <![CDATA[SnCl4]]> 45.92 Example 8 <![CDATA[BF3]]> 40.03
[0059] Example 9
[0060] The difference from Example 1 is that the amount of modifier used is 15 ml, and 22 ml of extractant is added each time.
[0061] Example 10
[0062] The difference from Example 1 is that the amount of modifier used is 20 ml, and 23 ml of extractant is added each time.
[0063] The experimental results of Examples 1, 9 and 10 under different agent-oil ratios are shown in Table 3.
[0064] Table 3 Yield changes under different agent-oil ratios
[0065] Example Agent to oil ratio Yield % Example 1 1:1 58.87 Example 9 1:1.5 59.03 Example 10 1:2 59.08
[0066] Embodiment 11
[0067] The difference from Example 1 is that the amount of catalyst used is 0.8 g.
[0068] Example 12
[0069] The difference from Example 1 is that the amount of catalyst used is 1.0 g.
[0070] The experimental results of Examples 1, 11 and 12 under different catalyst ratios are shown in Table 4.
[0071] Table 4 Yield changes under different catalyst dosages
[0072] Example Catalyst dosage Yield % Example 1 0.5 58.87 Embodiment 11 0.8 58.91 Example 12 1.0 58.92
[0073] Embodiment 13
[0074] The difference from Example 1 is that the amount of dichloromethane used as the reaction solvent is 10 ml, and 17 ml of the extractant is added each time.
[0075] Embodiment 14
[0076] The difference from Example 1 is that the amount of dichloromethane used as the reaction solvent is 15 ml, and 18 ml of the extractant is added each time.
[0077] The experimental results of Examples 1, 13 and 14 under different reaction solvent dosage conditions are shown in Table 5.
[0078] Table 5 Yield changes under different reaction solvent dosages
[0079] Example Dichloromethane dosage Yield % Example 1 20ml 58.87 Embodiment 13 10ml 58.65 Embodiment 14 15ml 58.78
[0080] Embodiment 15
[0081] Since the side chains on the benzene rings in coal tar have not only alkyl groups but also some hydroxyl groups, phenol is used as a raw material in this embodiment, and the remaining reaction conditions and reaction steps are the same as those in Example 1. The reaction that occurs is shown in the following formula:
[0082]
[0083] Example 16
[0084] Different from Example 15, the modification reaction temperature was set to 80°C.
[0085] Embodiment 17
[0086] Different from Example 15, the modification reaction temperature was set to 90°C.
[0087] Embodiment 18
[0088] Different from Example 15, the modification reaction temperature was set to 110°C.
[0089] Embodiment 19
[0090] Different from Example 15, the modification reaction temperature is set to 120°C.
[0091] The experimental results of the yield changes at different reaction temperatures in Examples 15 to 19 are shown in Table 6.
[0092] Table 6 Yield changes at different reaction temperatures
[0093] Example Modification temperature ℃ Yield % 15 100 50.68 16 80 41.32 17 90 47.17 18 110 57.54 19 120 63.79
[0094] Embodiment 20
[0095] The difference from Example 15 is that the catalyst for the modification reaction is anhydrous ferric chloride.
[0096] Embodiment 21
[0097] The difference from Example 15 is that the modification reaction catalyst is anhydrous tin tetrachloride.
[0098] Embodiment 22
[0099] The difference from Example 15 is that the catalyst for the modification reaction is anhydrous boron trifluoride.
[0100] The reaction results under different catalyst conditions of Example 15 and Example 20 to Example 22 are shown in Table 7.
[0101] Table 7 Yield changes under different catalysts
[0102] Example catalyst Yield % Embodiment 15 <![CDATA[AlCl3]]> 50.68 Embodiment 20 <![CDATA[FeCl3]]> 44.27 Embodiment 21 <![CDATA[SnCl4]]> 40.31 Embodiment 22 <![CDATA[BF3]]> 29.06
[0103] Embodiment 23
[0104] The difference from Example 15 is that the amount of modifier used is 15 ml, and 22 ml of extractant is added each time.
[0105] Embodiment 24
[0106] The difference from Example 15 is that the amount of modifier used is 20 ml, and 23 ml of extractant is added each time.
[0107] The experimental results of the yield changes under different agent-oil ratios of Examples 15, 23 and 24 are shown in Table 8.
[0108] Table 8 Yield changes under different agent-oil ratios
[0109] Example Agent to oil ratio Yield % Embodiment 15 1:1 50.68 Embodiment 23 1:1.5 50.73 Embodiment 24 1:2 50.76
[0110] Embodiment 25
[0111] The difference from Example 15 is that the amount of catalyst used is 0.8 g.
[0112] Embodiment 26
[0113] The difference from Example 15 is that the amount of catalyst used is 1.0 g.
[0114] The experimental results of yield changes under different catalyst dosage conditions of Examples 15, 25 and 26 are shown in Table 9.
[0115] Table 9 Yield changes under different catalyst dosages
[0116] Example Catalyst dosage g Yield % Embodiment 15 0.5 50.68 Embodiment 25 0.8 50.70 Embodiment 26 1.0 50.70
[0117] Embodiment 27
[0118] The difference from Example 15 is that the amount of dichloromethane used as the reaction solvent is 10 ml, and 17 ml of the extractant is added each time.
[0119] Embodiment 28
[0120] The difference from Example 15 is that the amount of dichloromethane used as the reaction solvent is 15 ml, and 18 ml of the extractant is added each time.
[0121] The experimental results of the yield changes under different solvent dosage conditions of Examples 15, 27 and 28 are shown in Table 10.
[0122] Table 10 Yield changes under different solvent dosages
[0123] Example Dichloromethane dosage Yield % Embodiment 15 20 50.68 Embodiment 27 10 50.33 Embodiment 28 15 50.51
[0124] Embodiment 29
[0125] Different from the above-mentioned embodiment, the raw material used in this embodiment is the distillate oil of 220-340° C. in medium-low temperature coal tar. The specific raw material properties are shown in Tables 11 and 12 below.
[0126] Table 11 Coal tar components
[0127] project content% Straight chain alkanes 14.74 Monocyclic compounds 24.13 Bicyclic compounds 46.22 Tricyclic and above compounds 14.91
[0128] Table 12 Coal tar carbon number distribution
[0129]
[0130]
[0131] The specific experimental steps include:
[0132] Weigh 10g coal tar, 10g NA anhydride and 20ml dichloromethane into a 100ml Schlenk tube, add 0.5g anhydrous aluminum chloride catalyst and seal. Fix the Schlenk tube with an iron stand and place it in a DF-101S collector constant temperature heating magnetic stirrer and heat it in an oil bath. Set the temperature of the DF-101S collector constant temperature heating magnetic stirrer to 100℃ and the stirring speed to 250rpm / min. Start timing when the temperature reaches 100℃ and is basically stable. End the reaction after 24 hours.
[0133] After the reaction is completed, place the Schlenk tube above the DF-101S collector-type constant temperature heating magnetic stirrer and cool it naturally for 1 hour. Transfer the reaction product to a 250ml pear-shaped bottle, add 20ml of 10% hydrochloric acid solution and wait for 10 minutes to terminate the reaction. Move all the substances to a separatory funnel, add dichloromethane extractant three times, add 20ml each time, then let it stand for 10 minutes to separate the solution, and collect the crude product after removing the catalyst. The collected crude product is placed in a rotary evaporator for rotary evaporation, the rotation temperature is 39°C, the speed is set to 50rpm / min, and the experiment is terminated after no bubbles are generated.
[0134] During the process of coal tar ring-increasing modification, the reaction that occurs is shown in the following formula:
[0135]
[0136] Wherein: R represents hydroxyl and various alkyl substituent groups, and the number of R on the same benzene ring is between 0 and 6.
[0137] Coal tar contains a variety of substances, and different substances undergo different reactions. The above four reactions represent the reactions occurring among the different types of substances.
[0138] After the products were collected and analyzed by GC-MS, it can be seen that after the ring-addition modification, the composition of the modified coal tar changed significantly compared with the coal tar raw material. The specific product composition and carbon number distribution of the modified coal tar are shown in Tables 13 and 14.
[0139] Table 13 Composition of modified coal tar products
[0140] project content% Straight chain alkanes 23.43 Monocyclic compounds 11.73 Bicyclic compounds 31.66 Tricyclic and above compounds 33.18
[0141] Table 14 Carbon number distribution of modified coal tar products
[0142] project content% C7 1.16 C8 3.47 C9 4.89 C10 6.97 C11 10.60 C12 11.67 C13 6.99 C14 4.01 C15 4.61 C16+ 45.63
[0143] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit its protection scope. Although the present invention has been described in detail with reference to the above embodiments, ordinary technicians in the field should understand that after reading the present invention, those skilled in the art can still make various changes, modifications or equivalent substitutions to the specific implementation methods of the invention, but these changes, modifications or equivalent substitutions are all within the protection scope of the pending claims of the invention.
Claims
1. A method for preparing NA anhydride modified coal tar, characterized in that: The method comprises the following steps: coal tar, a modifier, a solvent and a catalyst are mixed to carry out a ring-addition modification reaction to obtain a first crude product, wherein the modifier is NA anhydride, and the mass ratio of coal tar to the modifier is 1:(1-2); the ring-addition modification reaction of the first crude product is terminated to obtain a second crude product; the second crude product is mixed with an extractant to carry out extraction, and then impurities are separated by rotary evaporation to obtain modified coal tar, wherein the impurities include a catalyst and a solvent.
2. The method for preparing NA anhydride-modified coal tar according to claim 1, characterized in that: The catalyst adopts Lewis acid, the dosage of the catalyst is 5% to 10% of the mass of the coal tar, the solvent adopts dichloromethane, and the volume ratio of the coal tar to the solvent is 1: (1 to 2).
3. The method for preparing NA anhydride-modified coal tar according to claim 1, characterized in that: The reaction temperature for the mixed ring-addition modification reaction is 80-120°C.
4. The method for preparing NA anhydride-modified coal tar according to claim 1, characterized in that: The extractant is dichloromethane, the volume ratio of the second crude product to the extractant is 1:1, and the extraction time is 5 to 10 minutes.
5. The method for preparing NA anhydride-modified coal tar according to claim 1, characterized in that: The first crude product is mixed with a hydrochloric acid solution to obtain a second crude product, wherein the mass percentage concentration of the hydrochloric acid solution is 10%.
6. The method for preparing NA anhydride-modified coal tar according to claim 1, characterized in that: Coal tar is composed of 12% to 20% straight-chain alkanes, 20% to 26% monocyclic, 40% to 50% bicyclic and 10% to 20% tricyclic and above compounds.
7. The method for preparing NA anhydride-modified coal tar according to claim 6, characterized in that: The solvent is CH2Cl2, and the catalyst is anhydrous aluminum chloride, anhydrous ferric chloride, anhydrous tin tetrachloride or anhydrous boron trifluoride.
8. The method for preparing NA anhydride-modified coal tar according to claim 1, characterized in that: The reaction pressure of the mixture is 101.325 kPa, the reaction time of the mixture is 24 h, and the stirring rate of the mixture is 200-300 rpm / min.
9. The method for preparing NA anhydride-modified coal tar according to claim 1, characterized in that: The temperature of the rotary evaporation is 30-40° C., the speed of the rotary evaporation is set to 50-80 rpm / min, and the rotary evaporation is stopped when no bubbles are generated.
10. A NA anhydride modified coal tar, characterized in that: The product is prepared by the method for preparing NA anhydride-modified coal tar according to any one of claims 1 to 9.
Citation Information
Cited By
Catalyst for preparing high-density special fuel from high-temperature coal tar as well as grading method and application of catalyst
CN122006799A