Comfortable woven shirt fabric and production method thereof
By combining a combination of microdenier fiber, modal fiber and Lycra fiber in the shirt fabric, combined with intelligent temperature control technology and specific processing technology, it solves the problem that existing fabrics have difficulty in providing comfortable temperature regulation and smooth and soft touch in different scenarios. It solves the problem of fabric softness, smoothness and intelligent temperature regulation, improving the wearing experience and comfort.
Patent Information
- Application Number
- CN202411027097.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-10-01
AI Technical Summary
It is difficult for existing shirt fabrics to provide comfortable temperature regulation and smooth and soft touch in different scenarios, and cannot meet consumers' high requirements for versatility and comfort.
Using a combination of 60-75% ultra-fine denier polyester fiber, 25-30% Lenzing Modal fiber and 5% Lycra fiber, it is spun through compact siro spinning to form a 55-count yarn, combined with HEIQ SMART TEMP intelligent temperature control technology weaves woven fabrics with 2/1 bias or 2/2 bias, using specific dyeing and finishing processes, including singeing, weight reduction, fiber opening and tank steaming processes to enhance the fabric of softness and temperature regulating properties.
It achieves the fabric's soft and waxy feel, skin-friendly touch and intelligent temperature adjustment function, which significantly improves the wearing experience, meets consumers' needs for comfort and functionality, and provides a suitable microclimate environment.
Smart Images

Figure CN118727239A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a comfortable woven shirt fabric, in particular to a smooth, soft, delicate, skin-friendly, intelligent temperature-controlled woven fabric and a production method thereof, belonging to the field of functional fabrics. Specifically, it relates to a comfortable woven shirt fabric and a production method thereof. Background Art
[0002] With the development of the times, the improvement of people's consumption level and the change of work scenes, the functionality and types of clothing are increasing, and people's requirements for fabrics, which are the basis of clothing, are becoming more and more diverse. In the 21st century, market products have developed explosively, and consumer demand has been greatly met. As a traditional business attribute product, consumers hope that shirts have multiple scenes and a more comfortable wearing experience. People have higher requirements for the intrinsic quality and comfort of clothing fabrics. To this end, comfortable fabrics that can maintain temperature regulation, release a cool touch when the body is hot, lock in temperature and reduce heat loss at low temperatures, and feel smooth, soft, and skin-friendly have become the focus of people's attention. The research and development of this product can bring consumers a more comfortable product experience, effectively improve the comfort of fabrics in the field of men's shirts, and enable consumers to always stay in a suitable body environment, which is in line with consumers' pursuit of quality of life.
[0003] Ultrafine denier fiber is more fluffy and softer than ordinary fiber, with elegant silk-like luster and good air permeability. Ultrafine denier fiber has fine fiber density and small bending stiffness, so its fabric is fine and delicate, with many excellent characteristics such as wrinkle-resistant, warm, light, comfortable, breathable, good drape and fullness.
[0004] Modal fiber is a high wet modulus regenerated cellulose fiber. The raw material of the fiber is wood pulp made from European spruce and beech, which is then processed into fiber through a special spinning process. There is no pollution in the entire production process of the fiber. The raw materials are all natural materials, harmless to the human body, and can be naturally decomposed, which is friendly to the environment. Fabrics woven with modal fibers have a silky luster, the fabric is elegant and luxurious, with a comfortable soft touch and drape and excellent moisture absorption.
[0005] Lycra is a spandex elastic fiber, a block molecular segment polyurethane composed of flexible segments and rigid segments. It has better performance than ordinary spandex. Lycra's stretchability can reach 500%, which is far superior to traditional elastic fibers. It can be stretched very easily and can still adhere to the surface of human skin after recovery, with little restraint on the human body. The appropriate recovery and retention of Lycra fabrics give clothing comfortable elasticity, shape retention, fit and formability.
[0006] HEIQ SMART TEMP intelligent temperature control technology applies HEIQ functional polymer particles on the surface of fabrics, giving fabrics the ability to dynamically respond to changes in body temperature. When the human body feels hot, the cooling function is immediately activated, and the cooling effect is achieved by expanding and increasing moisture dissipation, and it automatically stops when the human body reaches a suitable temperature. When the human body feels cold, the heat preservation function is immediately activated, and the heat preservation effect is achieved by contracting and reducing heat loss. Summary of the invention
[0007] The purpose of the present invention is to overcome the defects in the prior art and provide a comfortable woven shirt fabric, a soft, comfortable, fine velvety and comfortable shirt fabric with intelligent temperature control performance.
[0008] To achieve the above purpose, the technical solution of the present invention is to design a comfortable woven shirt fabric, which is woven from warp yarn and weft yarn. The warp yarn is 60-75% superfine denier polyester fiber and 25-30% Lenzing modal fiber, which are spun by compact siro spinning to form a yarn with a yarn count of 55. The weft yarn is 60-75% superfine denier polyester fiber and 25-30% Lenzing modal fiber, which are spun by compact siro spinning to form a yarn with a yarn count of 55 and then coated with 5% Lycra fiber of 30 denier.
[0009] A further technical solution is that the fabric has a 2 / 1 bias weave, a 2 / 2 bias weave, a 3 / 1 bias weave, a width of 152 cm, and a gram weight of 140 grams per square meter.
[0010] The present invention also provides a technical solution, which is a method for producing comfortable woven shirt fabrics, which is made from 60-75% superfine polyester fiber, 25-30% Lenzing Modal fiber and 5% Lycra fiber through spinning, weaving, dyeing and finishing processes.
[0011] A further technical solution is that in the spinning process: a compact siro spinning process is used, the yarn count is 55, the Z twist, and the twist coefficient is 8200;
[0012] In the dyeing process, the process of first dyeing ultrafine denier polyester fiber and then dyeing modal is adopted; the ultrafine denier polyester fiber has a dyeing temperature of 80°C, acetic acid and leveling agent are added, the dyeing temperature is 130°C, and the heat preservation time is 40 minutes; modal fiber is chemically treated at 40°C, sodium sulfate and soda ash are added, the temperature is increased by 1°C / min to 60°C, and the heat preservation time is 40 minutes for dyeing;
[0013] The dyeing and finishing process includes the following processes which are carried out in sequence: enzyme stacking, washing, pre-shrinking, pre-setting, singeing, weight reduction, fiber opening, dyeing, drying, shaping, tank steaming and pre-shrinking.
[0014] The further technical scheme is that the singeing process adopts LTYM01 singeing machine, natural gas as fuel, the burner is tangent to the fabric, the speed is 120m / min, medium fire, one positive and one negative; the reduction process adopts overflow cylinder machine cylinder reduction, caustic soda 25g / L, treatment temperature 120℃, insulation time 30min; the fiber opening process adopts sulfuric acid to open modal fiber, temperature 110℃, insulation for 120 minutes; the shaping process adopts Rixin W-type stenter shaping machine, temperature 180℃, speed 40m / min, overfeed 3%, and HEIQ additive; the can steaming process adopts Italian TMT PF2000 can steaming machine, hot pack light can steaming process, pressure 0.2MPA, temperature 100 degrees, steaming 8min. In the post-finishing process, through many practices, considering the different characteristics of various raw materials of this product, the process is finally optimized, which not only pays attention to the style and feel characteristics of the product, but also gives full play to the performance characteristics of each material. In the production process, the above processes are focused on, and the expected design effect has been achieved. Considering the effect of singeing, strength and feel of the fabric, a gas singeing machine is used. During the alkali reduction treatment, the surface of polyester is eroded, the fiber diameter becomes thinner, pits are formed on the surface, and the stiffness of the fiber decreases, making the fabric soft and luster soft. This product uses the peeling effect of alkali reduction treatment on polyester to improve the softness and flexibility of the fabric, and keep the product soft and soft. The above optimal process conditions are obtained through experiments. The fiber opening effect with uniform effect, full flesh, soft and glutinous feel, and clean cloth surface can be obtained, ensuring the delicate velvet feel and soft comfort of the fabric. The various process parameters of shaping ensure the shaping effect and physical and chemical properties of the fabric. Adding the tank steaming process can further improve the stiffness of the fabric, enhance the skin-friendly and smooth effect of the fabric, and ensure that the fabric feels plump and has a soft appearance.
[0015] A further technical solution is to use the remaining caustic soda after the treatment in the reduction process for the alkali in the post-acid washing and alkali neutralization process in the fiber opening process.
[0016] A further technical solution is that the can steaming process uses a can steamer; a flexible shaft is fixedly connected to the roller shaft of the steaming roller on the star frame of the can steamer, the flexible shaft is fixedly connected to the wheel shaft of the exhaust fan impeller, the exhaust fan impeller is arranged inside the inner wall of the body of the can steamer, a condensate guide channel is arranged inside the inner wall of the body of the can steamer, and an opening connected to the guide channel is arranged on the inner wall of the body. The purpose of exhaustion is achieved by the principle of generating air flow through the rotation of the impeller, and the opening and condensate guide channel arranged on the inner wall of the body can be used to remove the condensate formed on the inner wall of the body as soon as possible, and avoid falling on the cloth surface due to gravity after being formed in the wall to contaminate the cloth surface.
[0017] The advantages and beneficial effects of the present invention are:
[0018] After conducting research on domestic market consumption trends and consumer pain points, as well as continuous R&D experiments, the applicant has successfully developed a shirt fabric that meets the comfort function of consumers. The fabric of the present invention has a soft and smooth feel and intelligent temperature regulation function, which greatly improves the wearing experience of consumers in different scenarios and meets the consumer's requirements for comfortable products.
[0019] The polyester fiber uses ultra-fine fibers with a fineness of 0.89D, giving the fabric a soft, smooth, light, elastic and skin-friendly touch. At the same time, the excellent natural wrinkle-resistant and iron-free properties of polyester fiber are retained. The fabric is wide and easy to care for, meeting the requirements of human comfort.
[0020] Modal fiber is a high wet modulus regenerated cellulose fiber made by Lenzing Group from beech wood in sustainably managed forests in Austria and its neighboring countries. Modal fiber has good softness and excellent moisture absorption. Its skin-friendly and soft touch provides the material basis for comfortable fabrics. At the same time, the silky luster of the fiber gives the fabric a high-quality feel and provides visual comfort for consumers. The Modal Air fiber used in this product is Lenzing's most slender and lightest wood fiber. The use of this 0.8 dtex fiber fully demonstrates the luxurious texture of the product;
[0021] Lycra stretch fiber has better elasticity than general spandex, maintaining excellent recovery and minimal restraint. DuPont Lycra fiber is used to give the fabric comfortable elasticity and shape retention;
[0022] The present invention is a woven shirt fabric made by blending the above three fibers in proportion, combining Swiss intelligent temperature control HEI Q technology, and adopting a specific processing method. It has a smooth and soft skin-friendly touch while maintaining the comfortable temperature regulation function of human clothing. The fabric has the characteristic of natural temperature regulation, creates a microclimate environment inside the clothing, and helps consumers always stay in a comfortable environment. It is a fabric that meets the human visual, tactile, and body comfort requirements. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 It is a schematic diagram of a third embodiment of a comfortable woven shirt fabric of the present invention;
[0024] Figure 2 yes Figure 1 A perspective view of the central exhaust fan body;
[0025] Figure 3 is a schematic diagram of a fourth embodiment of the present invention;
[0026] Figure 4 is a schematic diagram of Embodiment 5 of the present invention;
[0027] Figure 5 yes Figure 4An enlarged schematic diagram of the middle cam mechanism and the ear suction ball;
[0028] Figure 6 yes Figure 5 A schematic diagram of another working state of;
[0029] Figure 7 yes Figure 6 Schematic diagram of the cam mechanism;
[0030] Figure 8 yes Figure 7 Side view of.
[0031] In the figure: 1. steaming roller; 2. flexible shaft; 3. exhaust fan impeller; 4. condensate diversion channel; 5. opening; 6. exhaust body; 7. cam; 8. bottom plate; 9. top block; 10. intermediate wheel; 11. ear suction ball; 12. suction port. DETAILED DESCRIPTION
[0032] The specific implementation of the present invention is further described below in conjunction with the accompanying drawings and embodiments. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and cannot be used to limit the protection scope of the present invention.
[0033] Embodiment 1: The present invention is a comfortable woven shirt fabric, the raw materials of which are 55-count 71% ultra-fine polyester fiber, 25% Lenzing Modal fiber and 4% Lycra fiber. The product specifications are fabric structure 2 / 2 twill, width 152cm, and weight per square meter 140g.
[0034] Embodiment 2: A method for producing the intelligent temperature-controlled comfortable shirt woven fabric of Embodiment 1, the main process flow is:
[0035] (1) Spinning: Raw cotton --- Opening and cleaning --- Combing --- Preparation before combing --- Combing ---
[0036] Polyester---opening and cleaning cotton---carding cotton---pre-bundling---first-bundling---second-bundling---third-bundling---roving---spinning---winding
[0037] (2) Weaving: warping --- sizing --- drawing in --- reeding --- weaving --- blank inspection --- blank repair
[0038] (3) Dyeing and finishing: enzyme pile---washing---pre-shrinking---pre-singling---singing---reduction---fiber opening---dyeing---drying---setting---tank steaming---pre-shrinking
[0039] in:
[0040] (1) Spinning technology
[0041] Adopt compact siro spinning process, special yarn 55S, twist coefficient 8200, weft yarn covered with 30D Lycra yarn. Produced according to conventional compact siro spinning process;
[0042] (2) Weaving technology
[0043] Weaving is done on a Toyota air-jet loom. The heald frame opening adopts a symmetrical shed, with a 2 / 2 weave, 1, 3, 2, 4 patterns, and the height of the heald frame decreases. The warp stop frame has a height of 2 grids and a depth of 3. The back beam has a height of 0 and a depth of 4. The warp stop line is in a balanced state.
[0044] (3) Dyeing technology
[0045] Adjusted process conditions: high temperature and high pressure overflow dyeing tank two-bath dyeing. Disperse dyeing, 45℃ loading material gradually heated up, add dispersant, leveling agent and HAC (i.e. acetic acid), dye at 130℃ and keep warm for 40min, cool down to 90℃ for reduction and cleaning; after the color is qualified, active dyeing; medium temperature active dyeing, 40℃ chemical material, add sodium sulfate and soda ash, heat up to 60℃ at 1℃ / min, keep warm for 40min.
[0046] (4) Finishing technology
[0047] In the post-processing process, the applicant has optimized the process through repeated practice, taking into account the different characteristics of various raw materials of this product, focusing on the style and feel of the product, and giving full play to the performance characteristics of each material. In the production process, the following processes are focused on, and the expected design effect has been achieved:
[0048] 4.1 Singeing. Considering the effect, strength and feel of fabric singeing, this project uses a gas singeing machine; the fuel is natural gas, the flame is blue and in the tangential direction; the burner is one front and one back, double-sided singeing process; the machine speed is 120m / min; the distance between the fabric and the flame is 1.0cm.
[0049] 4.2 Weight reduction. During the alkali weight reduction treatment, the surface of polyester is eroded, the fiber diameter becomes thinner, pits are formed on the surface, and the stiffness of the fiber decreases, making the fabric soft and luster soft. This product uses the peeling effect of alkali weight reduction treatment on polyester to improve the softness and flexibility of the fabric and keep the product soft and gentle. The best process conditions were obtained through experiments: 25g / L caustic soda, treatment temperature 120℃, insulation time 30min, and the process parameters during neutralization were: using HAC and temperature 65℃.
[0050] 4.3 Fiber opening. The modal sulfuric acid fiber opening process is adopted. The temperature is raised to 90℃, 0.8g / l sulfuric acid is added to the cylinder, the temperature is raised to 110℃ at 1℃ / min and kept at this temperature for 120 minutes, the temperature is lowered to 70℃ at 2℃ / min, and then acid-washed and alkali is added for neutralization. This process can obtain a fiber opening effect with uniform effect, full flesh, soft and glutinous feel, and clean fabric surface, ensuring the fine velvety feeling and soft comfort of the fabric.
[0051] 4.4 Shaping. In order to ensure the shaping effect and physical and chemical properties of the fabric, this process adopts a shaping temperature of 180°C, a speed of 40m / min, and an overfeed of 3%. Functional HEIQ auxiliary AC-06 is added to the shaping process, with a dosage of 30g / L and a liquid rolling rate of 60%. At the same time, 30g / L of hydrophilic amino silicone softener is used.
[0052] 4.5 Can steaming. In order to further improve the stiffness of the fabric, enhance the skin-friendly and smooth effect of the fabric, and ensure that the fabric feels full and has a soft glossy appearance, this product adds a can steaming process. Light can steaming process, pressure 0.2MPA, temperature 100 degrees, time 40 minutes.
[0053] Embodiment 3: The difference from Embodiment 1 is that Figure 1 , Figure 2 As shown (for ease of illustration, Figure 1 Only the condensate diversion channel connected to the exhaust fan body located above is shown, and only two openings are shown), a flexible shaft 2 is fixedly connected to the roller shaft of the steaming roller 1 on the star frame of the tank steamer, the flexible shaft is fixedly connected to the wheel shaft of the exhaust fan impeller, the exhaust fan impeller 3 is arranged inside the inner wall of the body of the tank steamer (the exhaust fan impeller 3 is located in the exhaust fan body 6, and the exhaust fan body is located inside the wall of the inner wall of the body of the tank steamer), both ends of the wheel shaft of the exhaust fan impeller extend beyond the inner wall of the body to facilitate connection with the flexible shaft, a condensate diversion channel 4 is arranged inside the wall of the inner wall of the body of the tank steamer, and an opening 5 connected to the diversion channel is arranged on the inner wall of the body.
[0054] For example, Wang Yong mentioned in his paper "Development of a New Tank Steaming Equipment" published in the second issue of "Modern Textile Technology" in 2016: Since the tank steamer is a wet heat setting machine, steam can act as a heat carrier. It is both a plasticizer and a lubricant. Due to the existence of pressure, water vapor molecules quickly penetrate the fiber structure to destroy the interpolymerization bonds between molecules. The steamed fabric is permanently set, the physical indicators are significantly improved, the quality is further improved, and the added value is increased. It also mentioned: a timely step-by-step control function is designed. The machine consists of a cloth feeding unit, a star frame unit, a steaming tank unit, and a cloth discharging unit. The timely step-by-step function can start the action of the unit in time according to the running position of the cloth, and the other non-working units do not work. The steaming roller has a multi-station parallel function. The three-station parallel function means that the three steaming rollers realize "cloth feeding, cloth steaming, and cloth discharging" at three positions at the same time, which is highly efficient. It also mentioned: the steaming tank has a reliable condensate discharge measure to ensure that the fabric will not be contaminated by condensate during the tank steaming process. However, it is well known that even with a condensate discharge structure, condensate will condense on the inner wall of the machine body. If only relying on diversion and discharge structures, it cannot guarantee that the condensate will not fall on the decatizing cloth during the diversion process. Therefore, this method of the prior art still has the possibility of condensate contaminating the fabric. The present application uses the principle of generating air flow through the rotation of the impeller to achieve the purpose of exhaust. With the openings and condensate diversion channels provided on the inner wall of the machine body, the condensate formed on the inner wall of the machine body can be extracted as soon as possible to avoid falling on the cloth due to gravity after being formed in the wall and contaminating the cloth. In addition, the present embodiment utilizes the characteristic that the steaming roller needs to be driven to rotate, and utilizes the rotation of the steaming roller to drive the impeller to rotate to form exhaust, so that the impeller for exhaust does not need an additional power device, saving the cost of the entire device and reducing the structural complexity of the entire device.
[0055] Embodiment 4: The difference from Embodiment 3 is that Figure 3 As shown, the vertical side walls in the inner wall of the body of the pot steamer are inclined and the inclination direction is gradually inclined outward from top to bottom. The top wall in the inner wall of the body of the pot steamer is a "dome", that is, a curved inner top wall. After such an arrangement, the inner wall of the body can also play a role in diversion, and the formed condensed water is not easy to fall on the cloth surface, but is diverted along the inner wall of the body to both sides and the lower end, so as to avoid the condensed water from contaminating the cloth surface as much as possible.
[0056] A rubber sheet one-way valve can also be provided at the opening 5. The rubber sheet serving as the one-way valve is hinged at the opening of the tank steamer body. In this way, even if condensed water drawn to the condensed water guide channel 4 flows back, it will be blocked by the one-way valve, thereby ensuring that the condensed water is drawn away as much as possible to avoid falling on the cloth surface.
[0057] Embodiment 5: The difference from Embodiment 3 is that Figures 4 to 8As shown, a flexible shaft 2 is fixedly connected to the roller shaft of the steaming roller 1 on the star frame of the pot steamer, and the flexible shaft is connected to a cam mechanism, specifically, the flexible shaft 2 is fixedly connected to the wheel shaft of the cam 7 of the cam mechanism, so that when the steaming roller rotates, the cam mechanism is driven to operate, and the cam mechanism is arranged inside the inner wall of the body of the pot steamer, and both ends of the wheel shaft of the cam extend beyond the inner wall of the body to facilitate connection with the flexible shaft, a condensate diversion channel 4 is arranged inside the inner wall of the body of the pot steamer, an opening 5 connected with the diversion channel is arranged on the inner wall of the body, a rubber sheet one-way valve is arranged at the opening 5, and the rubber sheet serving as a one-way valve is hinged at the opening of the body of the pot steamer. The cam mechanism includes a base plate 8, one end of the cam wheel shaft is connected to the flexible shaft, and the other end is rotatably set on the base plate, a top block 9 is slidably set on the base plate 8, and the top block 9 is connected to the base plate 8 by a spring so that the top block always has a tendency to approach the cam 7, an intermediate wheel is rotatably set on the end of the top block 9 close to the cam, and the intermediate wheel 10 is set against the cam 7, an ear suction ball 11 is fixedly set inside the inner wall of the body of the tank steamer, the top block 9 is against the outer surface of the ear suction ball, and the suction port of the ear suction ball 11 is connected to the condensate diversion channel 4.
[0058] After such arrangement, even if the condensed water sucked into the condensed water guide channel 4 by the expansion of the ear suction ball reappears due to the rotation of the cam and the ear suction ball is pressed against and squeezed by the top block and flows back, it will be blocked by the one-way valve, so as to ensure the extraction of condensed water as much as possible and avoid falling on the cloth surface. Compared with the exhaust method of the previous embodiment, the effect of absorbing condensed water is better. When the steaming roller 1 rotates, the cam is driven to rotate by the flexible shaft, and the initial state is that the top block 9 presses against and squeezes the ear suction ball 11, so the ear suction ball is initially in a contracted state. After the cam rotates, the top block moves away from the ear suction ball due to the action of the spring, and the ear suction ball relaxes and expands, forming a state of absorbing condensed water. The cam continues to rotate, and the top block squeezes the ear suction ball again, forming a state of pushing out the condensed water, but due to the action of the one-way valve, the condensed water cannot be sprayed out. An observation window can be provided on the inner wall of the tank steamer, the observation window is located at the ear suction ball, the observation window is detachably provided on the inner wall of the tank steamer, an opening is provided on the ear suction ball, a rubber plug is provided at the opening, and the ear suction ball is usually blocked. Through the observation window, it is observed that the tail of the ear suction ball obviously drops, indicating that a lot of condensed water has accumulated (to facilitate the implementation of this solution, the ear suction ball is fixedly connected to the inner wall of the tank steamer in the middle, and the tail of the ear suction ball is at a lower position relative to the suction port 12, that is, the rotation axis of the ear suction ball is inclined relative to the horizontal line). Before the next work starts, the accumulated condensed water can be collected by removing the observation window and pulling out the plug, and it can be reused.
[0059] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A comfortable woven shirt fabric, characterized in that: The fabric is woven from warp yarn and weft yarn, the warp yarn is 60-75% superfine denier polyester fiber and 25-30% Lenzing modal fiber, which are spun by compact siro spinning to form 55 yarn count ply, and the weft yarn is 60-75% superfine denier polyester fiber and 25-30% Lenzing modal fiber, which are spun by compact siro spinning to form 55 yarn count and then coated with 30 denier 5% Lycra fiber to form yarn.
2. A comfortable woven shirt fabric according to claim 1, characterized in that: The fabric has a weave of 2 / 1 bias weave, 2 / 2 bias weave, and 3 / 1 bias weave, a width of 152 cm, and a weight of 140 grams per square meter.
3. A method for producing the comfortable woven shirt fabric according to claim 1 or 2, characterized in that: It is made of 60-75% superfine polyester fiber, 25-30% Lenzing Modal fiber and 5% Lycra fiber through spinning, weaving, dyeing and finishing processes.
4. The method for producing a comfortable woven shirt fabric according to claim 3, characterized in that: In the spinning process: a compact siro spinning process is adopted, the yarn count is 55, the Z twist is used, and the twist coefficient is 8200; In the dyeing process, the process of first dyeing ultrafine denier polyester fiber and then dyeing modal is adopted; the ultrafine denier polyester fiber has a dyeing temperature of 80°C, acetic acid and leveling agent are added, the dyeing temperature is 130°C, and the heat preservation time is 40 minutes; modal fiber is chemically treated at 40°C, sodium sulfate and soda ash are added, the temperature is increased by 1°C / min to 60°C, and the heat preservation time is 40 minutes for dyeing; The dyeing and finishing process includes the following steps which are carried out in sequence: enzyme piling, washing, pre-shrinking, pre-setting, singeing, reduction, fiber opening, dyeing, drying, shaping, and pre-shrinking.
5. The method for producing a comfortable woven shirt fabric according to claim 4, characterized in that: The singeing process adopts LTYM01 singeing machine, natural gas as fuel, the burner is tangent to the fabric, the speed is 120m / min, medium fire, one positive and one negative; the reduction process adopts overflow cylinder reduction, caustic soda 25g / L, treatment temperature 120℃, insulation time 30min; the fiber opening process adopts modal sulfuric acid fiber opening, temperature 110℃, insulation time 120min; the shaping process adopts Risin W-type tank steaming stenter setting machine, temperature 180℃, speed 40m / min, overfeed 3%, and HEIQ additive; the tank steaming process adopts Italian TMT PF2000 tank steaming machine, hot bag light tank steaming process, pressure 0.2MPA, temperature 100 degrees, steaming for 8min.
6. The method for producing a comfortable woven shirt fabric according to claim 5, characterized in that: The remaining caustic soda after the treatment in the weight reduction step is used as alkali in the post-acid washing and alkali neutralization step in the fiber opening step.
7. The method for producing a comfortable woven shirt fabric according to claim 6, characterized in that: The pot steaming process adopts a pot steamer; a flexible shaft is fixedly connected to the roller shaft of the steaming roller on the star frame of the pot steamer, the flexible shaft is fixedly connected to the wheel shaft of the exhaust fan impeller, the exhaust fan impeller is arranged inside the inner wall of the body of the pot steamer, a condensate diversion channel is arranged inside the inner wall of the body of the pot steamer, and an opening connected to the diversion channel is arranged on the inner wall of the body.
Citation Information
Patent Citations
Ultrafine denier fiber super-high-count sirospun compact yarn spinning technology
CN105002609A
Compact siro spinning air conditioning / modal fiber blended knitted fabric and producing method thereof
CN106012261A
Fiber splitting and dyeing process for modal polyester peach skin
CN108442146A
Production process of intelligent dynamic moisture absorption and sweat releasing fabric
CN111074416A
Super-soft heating red-bean-velvet underwear fabric and suit
CN111455538A
Cited By
Moisture-absorbing breathable chemical fiber fabric containing fine denier polyester filament yarn and production process thereof
CN119932788A
Real-silk cotton brocade shuttle-imitating fine-texture cool-feeling fabric and preparation method thereof
CN121047027A