Groove type semiconductor bridge chip and preparation method thereof

By designing a sharp edge gap and a honeycomb trench structure in the bridge area of ​​the semiconductor bridge chip, the current density and plasma discharge efficiency are improved, the problem of ignition time and energy of the existing semiconductor bridge pyrotechnics is solved, and a higher Accuracy and reliability.

CN118729871APending Publication Date: 2024-10-01CHINA ZHENHUA GRP YONGGUANG ELECTRONICS CO LTD STATE OWNED NO 873 FACTORY
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202410956445.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-17
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The ignition time of existing semiconductor bridge pyrotechnics is difficult to be faster and the ignition energy is difficult to be lower, resulting in insufficient accuracy and rapidity of the system, making it difficult to meet the high requirements of modern aerospace technology for pyrotechnics.

Method used

A sharp edge gap is made on both sides of the bridge area of ​​the semiconductor bridge chip, and a honeycomb trench structure is formed in the outer area to increase the current density and quickly form Joule heat and plasma discharge, thus reducing the ignition time and energy.

Benefits of technology

It achieves faster firing time and lower firing energy, improves the accuracy and reliability of semiconductor bridge pyrotechnics, and is suitable for smart or smart weapons, satellites, ammunition and blasting engineering.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118729871A_ABST
    Figure CN118729871A_ABST
Patent Text Reader

Abstract

The invention discloses a groove type semiconductor bridge chip and a preparation method thereof, and belongs to the technical field of initiating explosive devices. Comprising an N-type silicon substrate, a silicon dioxide layer, a front pattern polycrystalline silicon layer and a front pattern metal electrode layer. The thickness of the silicon dioxide layer ranges from 2000 angstroms to 20000 angstroms, the thickness of the front pattern polycrystalline silicon layer ranges from 10000 angstroms to 50000 angstroms, and the thickness of the front pattern metal electrode layer ranges from 10000 angstroms to 50000 angstroms. The sharp-corner-shaped edge notches are formed in the two side edges of the bridge area, the honeycomb groove structures are formed in the areas, except the sharp-corner-shaped edge notches, of the two side edges of the bridge area, the current density of the sharp-corner-shaped edge notches and the honeycomb groove structures is greatly improved after electrification, Joule heat is rapidly formed, and plasma discharge is rapidly formed. The problems that the ignition time and the ignition energy of the semiconductor bridge initiating explosive device are difficult to further reduce, and the accuracy and the rapidness of a semiconductor bridge initiating explosive device system are difficult to improve are solved. The semiconductor bridge chip is widely applied to the technical field of SCB initiating explosive device semiconductor bridge chips.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of pyrotechnics, and further relates to the technical field of semiconductor bridge pyrotechnics, and specifically, to a groove-type semiconductor bridge chip and a preparation method thereof. Background Art

[0002] Initiators are components or devices that provide ignition, detonation or power sources. They are the first and most sensitive components in weapons and ammunition, rockets, satellites, spacecraft, pilot life-saving, civil engineering blasting, gunpowder power and other devices. In recent years, with the development of science and technology, the requirements for the precision, accuracy and consistency of blasting and explosive ignition have become increasingly higher. The development of ammunition systems and the strengthening of the harshness of the electromagnetic environment require that the ignition system has the ability to resist static electricity, electromagnetic radiation, power supply transients, stray currents and lightning, and the ignition system should have good electromagnetic compatibility with other systems. Modern aerospace technology requires that initiators have the following characteristics: high anti-interference, including anti-electromagnetic interference, anti-mechanical stress and high safety insensitivity; low ignition energy and fast ignition; low-cost mass production with good consistency; miniaturization and intelligence of ignition devices. Traditional initiators can no longer meet these requirements, and it is necessary to study and develop advanced initiator technologies. Semiconductor Bridge (SCB) pyrotechnics is a high-tech pyrotechnic product that has been developed at home and abroad in recent years and is a typical representative of modern advanced pyrotechnic products.

[0003] The mechanism of action of SCB explosives is different from the heat conduction mechanism of traditional bridgewire explosives. It is generally believed to be a micro-convection mechanism. That is, when a pulse current is passed through the SCB, the silicon bridge material is rapidly vaporized due to Joule heat and forms a 4100K~6000K plasma discharge under the action of the electric field. This high-temperature, high-pressure fluid quickly diffuses into the explosive, causing the explosive to heat up to the ignition temperature and ignite. In addition, the shock wave generated by the rapid diffusion of the plasma also acts on the explosive.

[0004] When current passes through SCB, energy is dissipated through many channels and methods, mainly heat conduction from the bridge to the substrate; consumption of heating bridge materials; melting heat and vaporization heat of bridge materials; thermal radiation; circuit losses outside the bridge. The distribution of these energies depends on the electrical characteristics of the ignition device and the geometric shape and structure of the bridge. At present, the bridge area structure of semiconductor bridge chips is long and narrow, and it is difficult to reduce the ignition time and ignition energy. For semiconductor bridge pyrotechnics used in smart or intelligent weapons, satellites, ammunition, civilian anti-collision airbags and blasting engineering, the requirements for ignition time and ignition energy are extremely high. Having faster ignition time and lower ignition energy is a new development direction for semiconductor bridge pyrotechnics. At present, the ignition time and ignition energy of the bridge area structure of semiconductor bridge chips are difficult to reduce.

[0005] Therefore, a semiconductor bridge chip with a new bridge region structure is urgently needed to solve the above problems.

[0006] The purpose of the present invention is to provide a semiconductor bridge chip with faster ignition time and lower ignition energy and a preparation method thereof, which can greatly improve the ignition time and ignition energy of the semiconductor bridge, realize the accuracy and rapidity of the semiconductor bridge pyrotechnics, and realize micro-difference blasting.

[0007] In view of this, the present invention is proposed. Summary of the invention

[0008] The technical problem to be solved by the present invention is to solve the problem that the ignition time of the existing semiconductor bridge pyrotechnics is difficult to be further faster and the ignition energy is difficult to be further lower, and it is difficult to improve the accuracy and speed of the semiconductor bridge pyrotechnics system.

[0009] The inventive concept of the present invention is: sharp-angled edge notches are made on both sides of the bridge area, and honeycomb groove structures are made in the areas other than the sharp-angled edge notches on both sides of the bridge area, so that the current density at the sharp-angled edge notches and the honeycomb groove structure is greatly improved after power is turned on, Joule heat is quickly generated here, the temperature rises rapidly, the ignition energy is small, and a vaporization point is quickly formed to form plasma discharge, thereby reducing the ignition time and ignition energy of the semiconductor bridge chip.

[0010] To this end, the present invention provides a trench-type semiconductor bridge chip, such as Figure 1-2 As shown. The chip structure includes: N-type silicon substrate 1, silicon dioxide layer 2, front pattern polysilicon layer 3, front pattern metal electrode layer 4.

[0011] A silicon dioxide layer 2 is formed on the N-type silicon substrate 1 .

[0012] A front pattern polysilicon layer is formed on the silicon dioxide layer 2.

[0013] A front pattern metal electrode layer 4 is formed on the front pattern polysilicon layer 3.

[0014] The thickness of the silicon dioxide layer 2 is 2000 angstroms to 20000 angstroms.

[0015] The thickness of the front pattern polysilicon layer 3 is 10000 angstroms to 50000 angstroms.

[0016] The thickness of the front pattern metal electrode layer 4 is 10000 angstroms to 50000 angstroms.

[0017] The two sides of the polysilicon bridge area are made with sharp-angled edge notches, and the two sides of the bridge area except the sharp-angled edge notches are made with honeycomb groove structures.

[0018] The present invention provides a method for preparing a trench-type semiconductor bridge chip, comprising the following steps: (1) growing a silicon dioxide layer (2000 angstroms to 20000 angstroms) on the N-type silicon substrate; (2) forming a polysilicon layer (10,000 angstroms to 50,000 angstroms) on the silicon dioxide layer; (3) heavily doping the polysilicon layer; (4) forming a polysilicon bridge region and a bridge region groove on the polysilicon layer; (5) forming an ultra-thick metal layer (10,000 angstroms to 50,000 angstroms) on the polysilicon bridge region; (6) making the metal layer into a semiconductor bridge chip electrode; (7) performing annealing to form an ohmic contact between the metal layer and silicon; (8) The wafer is diced to form individual semiconductor bridge chips.

[0019] For semiconductor bridge pyrotechnics, lower ignition voltage and faster ignition time are important manifestations of better performance of semiconductor bridge pyrotechnics.

[0020] The bridge area structure of the pointed edge notch + honeycomb groove structure provided by the present invention has a greater edge effect than other semiconductor bridge products, and the ignition time and ignition energy of the product are greatly improved; at the same time, during the charging period, the groove provides more area for the explosive contact, and the product reliability is greatly improved.

[0021] Therefore, the semiconductor bridge chip with a pointed edge notch + honeycomb groove structure has a better edge effect, the ignition time required for the semiconductor bridge area is faster, and the ignition energy is lower; at the same time, the honeycomb groove structure on the surface of the bridge area also greatly widens the contact area with the explosive, and the ignition reliability has been steadily improved.

[0022] The beneficial effects of the present invention are: Due to the adoption of semiconductor bridge chips with a bridge area structure of pointed edge notch + honeycomb groove structure, the performance and reliability of semiconductor bridge products have been greatly improved, providing a new direction for the development of semiconductor bridge chips with lower ignition time, lower ignition energy and greater reliability.

[0023] The technical solution of the present invention can be widely used in the technical field of SCB pyrotechnic semiconductor bridge chips. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a schematic diagram of the longitudinal structure of a semiconductor bridge chip with a V-shaped + honeycomb groove bridge area structure.

[0025] Figure 2This is a schematic diagram of the structure of the polysilicon trench bridge area.

[0026] In the figure: 1 is an N-type silicon substrate, 2 is a silicon dioxide layer, 3 is a front pattern polysilicon layer, and 4 is a front pattern metal electrode layer. DETAILED DESCRIPTION

[0027] like Figure 1-2 As shown, the trench-type semiconductor bridge chip and the preparation method thereof are specifically implemented as follows: The N-type silicon substrate 1 is single crystal silicon, with a thickness of 500±25 μm and a resistivity of (55-65) ohm.cm.

[0028] The shape of the pointed edge notch is single V-shape, double V-shape or multiple V-shape (at least 3), and is symmetrically distributed on both sides of the bridge area.

[0029] The honeycomb grooves are circular, elliptical, groove-shaped or other grooves, and are distributed in the bridge area.

[0030] The silicon dioxide layer is grown on an N-type silicon substrate by thermal oxidation. The thickness of the silicon dioxide layer 2 is 12000 angstroms.

[0031] The polysilicon layer is deposited on the silicon dioxide layer by LPCVD or PECVD. The thickness of the polysilicon layer 3 is 25000 angstroms.

[0032] The heavy doping is to heavily dope the polysilicon layer with phosphorus. The doping concentration of the heavily doped phosphorus is 5E20.

[0033] The polysilicon bridge region and the bridge region groove are formed by etching the polysilicon bridge region and the bridge region groove on the polysilicon layer through a photolithography process.

[0034] The metal layer is a gold layer, which is formed on the polysilicon bridge region by evaporation or sputtering process (gold electrode layer). The thickness of the gold electrode layer 4 is 40000 angstroms.

[0035] The semiconductor bridge chip electrode is formed by photolithography of an ultra-thick gold layer through a photolithography process.

[0036] The metal layer-silicon ohmic contact is formed by an annealing process.

[0037] The scribing is laser scribing, grinding wheel scribing or diamond knife scribing.

[0038] Finally, it should be noted that the above embodiments are merely examples for the purpose of clear explanation. The present invention includes but is not limited to the above embodiments. It is not necessary and impossible to list all implementation methods exhaustively. For ordinary technicians in the relevant field, other different forms of changes or modifications can be made based on the above description. All implementation methods that meet the requirements of the present invention belong to the protection scope of the present invention.

Claims

1. A trench-type semiconductor bridge chip, Features ,The chip structure includes: N-type silicon substrate, silicon dioxide layer, front pattern polysilicon layer, front pattern metal electrode layer; A silicon dioxide layer formed on the N-type silicon substrate; a front patterned polysilicon layer formed on the silicon dioxide layer; A front pattern metal electrode layer formed on the front pattern polysilicon layer; The thickness of the silicon dioxide layer is 2000 angstroms to 20000 angstroms; The thickness of the front pattern polysilicon layer is 10000 angstroms to 50000 angstroms; The thickness of the front pattern metal electrode layer is 10000 angstroms to 50000 angstroms; The two sides of the polysilicon bridge area are made with sharp-angled edge notches, and the two sides of the bridge area except the sharp-angled edge notches are made with honeycomb groove structures.

2. A trench-type semiconductor bridge chip as claimed in claim 1, Features: The N-type silicon substrate is single crystal silicon with a thickness of 500±25 μm and a resistivity of (55-65) ohm.cm.

3. A trench-type semiconductor bridge chip as claimed in claim 1, Features: The shape of the pointed edge notch is a single V-shape, a double V-shape, or three or more V-shapes, and is symmetrically distributed on both sides of the bridge area.

4. A method for preparing a trench-type semiconductor bridge chip as claimed in claim 1, It is characterized in that The following steps are involved: (1) growing a silicon dioxide layer on the N-type silicon substrate; (2) forming a polysilicon layer on the silicon dioxide layer; (3) heavily doping the polysilicon layer; (4) forming a polysilicon bridge region and a bridge region groove on the polysilicon layer; (5) forming a metal layer on the polysilicon bridge region; (6) making the metal layer into a semiconductor bridge chip electrode; (7) performing annealing to form an ohmic contact between the metal layer and silicon; (8) The wafer is diced to form individual semiconductor bridge chips.

5. A method for preparing a trench-type semiconductor bridge chip as claimed in claim 1, Features: The silicon dioxide layer is grown on an N-type silicon substrate by thermal oxidation, and the thickness of the silicon dioxide layer is 12000 angstroms.

6. A method for preparing a trench-type semiconductor bridge chip as claimed in claim 1, Features: The polysilicon layer is deposited on the silicon dioxide layer by LPCVD or PECVD, and the thickness of the polysilicon layer is 25000 angstroms.

7. A method for preparing a trench-type semiconductor bridge chip as claimed in claim 1, Features: The heavy doping is to heavily dope the polysilicon layer with phosphorus, and the doping concentration of the heavily doped phosphorus is 5E20.

8. A method for preparing a trench-type semiconductor bridge chip as claimed in claim 1, Features: The metal layer is a gold layer. A gold electrode layer is formed on the polysilicon bridge region by evaporation or sputtering process. The thickness of the gold electrode layer is 40,000 angstroms.

9. A method for preparing a trench-type semiconductor bridge chip as claimed in claim 1, Features: The polysilicon bridge region and the bridge region groove are formed by etching the polysilicon bridge region and the bridge region groove on the polysilicon layer through a photolithography process; the semiconductor bridge chip electrode is formed by photolithography of an ultra-thick gold layer through a photolithography process.

10. A method for preparing a trench-type semiconductor bridge chip as claimed in claim 1, Features: The metal layer-silicon ohmic contact is formed by an annealing process; and the scribing is laser scribing, grinding wheel scribing or diamond knife scribing.

Citation Information

Patent Citations

  • Integrated semiconductor bridge transduction element

    CN107218852A

  • Semiconductor bridge chip and packing structure thereof

    CN108426489A

  • Semiconductor bridge chip and preparation method thereof

    CN110137090A

  • Self-destruction chip based on porous silicon composite energetic film-energetic semiconductor bridge binary structure