Organic semiconductor film detection method and device

Through soft plasma etching technology and optimized optical systems, combined with two-dimensional spectroscopy technology, the problem of low detection accuracy and efficiency of organic semiconductor thin films has been solved, and high-precision internal structure detection and in-situ non-destructive etching have been achieved, significantly improving detection. Precision and efficiency.

CN118730934APending Publication Date: 2024-10-01NINGBO UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310332297.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Existing organic semiconductor film detection technology cannot comprehensively and accurately obtain the internal structure information of the film, and the existing equipment is high-cost and low-precision, making it difficult to detect internal components and analyze micro-defects.

Method used

Using soft plasma etching technology and optimized optical systems, through layer-by-layer etching and sealed vacuum chamber design, the internal structure detection and in-situ non-destructive etching of organic semiconductor films are achieved, combined with two-dimensional spectroscopy technology and transfer matrix optics model to improve detection accuracy and efficiency.

Benefits of technology

It achieves precise detection of the internal structure of organic semiconductor films with a vertical resolution of less than 2 nm, an optical resolution of up to 0.1 nm, and a time resolution of less than 1 ms. It significantly improves detection accuracy and efficiency and overcomes the problems of single function and insufficient accuracy of traditional technology. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118730934A_ABST
    Figure CN118730934A_ABST
Patent Text Reader

Abstract

The invention provides an organic semiconductor film detection method and equipment, which can be used for accurately and effectively detecting an organic semiconductor and accurately and effectively detecting the interior of the organic semiconductor, and particularly, the equipment can be arranged as integrated equipment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of spectral analysis, and in particular to an organic semiconductor film detection method and equipment. Background Art

[0002] Nowadays, organic semiconductor materials have become a booming emerging science and technology field in China and a new focus of global material research and development due to their high flexibility, high biocompatibility, and easy material processing. However, since organic semiconductor films use organic doping solutions and their structures change after chemical reactions, the internal structure detection of organic semiconductor films is particularly critical. With the rapid development of the organic semiconductor industry, a number of technologies have been applied to the internal detection of organic semiconductor films in recent years. Limited by technical bottlenecks, most of the existing detection methods are difficult to fully and accurately grasp the structural properties of semiconductor film materials.

[0003] At present, the existing organic semiconductor thin film detection technology is still unable to fully and accurately obtain the internal structural information of the film, and there is still a lot of room for improvement. The existing problems are summarized as follows:

[0004] 1. X-ray diffraction technology and near-infrared spectroscopy technology are widely used in semiconductor testing. They can only analyze the overall average performance of bulk materials and cannot directly obtain information about micro-defects themselves.

[0005] 2. Transmission electron microscopy can only be used for surface morphology and structure analysis, and cannot detect the internal structure of semiconductors. It has the limitations of long R&D cycle and high cost, and due to the small analysis scale, it can only be used within the microscopic range.

[0006] 3. Neutron scattering analysis can detect and identify thickness, but cannot detect internal components. At the same time, secondary ion mass spectrometry equipment is expensive, and the sub-layer parameters obtained by ellipsometry are of low accuracy. Summary of the invention

[0007] An advantage of the present invention is to provide an organic semiconductor thin film detection method and device, wherein the organic semiconductor thin film detection method can be used to perform internal detection on the organic semiconductor thin film.

[0008] An advantage of the present invention is to provide an organic semiconductor thin film detection method and device, wherein the organic semiconductor thin film detection method can be used to perform in-situ non-destructive etching on the organic semiconductor thin film.

[0009] One advantage of the present invention is that it provides an organic semiconductor film detection method and device, wherein the organic semiconductor film detection device is an integrated device that can integrate etching detection and analysis of the organic semiconductor film.

[0010] An advantage of the present invention is that it provides an organic semiconductor thin film detection method and device, wherein the organic semiconductor thin film detection device is an integrated device that can perform in-situ detection of the organic semiconductor thin film.

[0011] Other advantages and features of the present invention will become more apparent from the following detailed description and may be realized by means of the instrumentalities and combinations particularly pointed out in the appended claims.

[0012] Further objects and advantages of the present invention will be fully apparent from an understanding of the following description and the accompanying drawings.

[0013] These and other objects, features and advantages of the present invention will be more fully understood from the following detailed description, accompanying drawings and claims. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a schematic diagram of a preferred embodiment according to the present invention.

[0015] Figure 2 It is a schematic diagram of a preferred embodiment according to the present invention. DETAILED DESCRIPTION

[0016] The following description is used to disclose the present invention so that those skilled in the art can implement the present invention. The preferred embodiments described below are only examples, and those skilled in the art can think of other obvious variations. The basic principles of the present invention defined in the following description can be applied to other embodiments, variations, improvements, equivalents, and other technical solutions that do not deviate from the spirit and scope of the present invention.

[0017] Those skilled in the art should understand that, in the disclosure of the present invention, the terms "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicating the orientation or position relationship are based on the orientation or position relationship shown in the drawings, which are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation. Therefore, the above terms should not be understood as limiting the present invention.

[0018] It is to be understood that the term "one" should be understood as "at least one" or "one or more", that is, in one embodiment, the number of an element may be one, while in another embodiment, the number of the element may be multiple, and the term "one" should not be understood as a limitation on the quantity.

[0019] Our design concept is as follows:

[0020] First, in order to solve the problem of how to get into the material, we developed a "soft plasma etching" process, which uses soft plasma to etch the sample layer by layer, and gradually expose the internal sublayers. Using the capacitively coupled discharge mode, the light path directly passes through the holes above and below the cavity to form an optical circuit, realizing the simultaneous measurement of reflectivity, transmittance and absorptivity.

[0021] Secondly, in order to solve the problem of how to characterize materials, the optical system was optimized and a sealed vacuum cavity was designed, so that the entire optical path inspection realized a closed vacuum circuit. Then a high-brightness xenon lamp was used as the excitation light source. The light emitted by the xenon lamp was converted into parallel light by a hemispherical lens, and then entered the optical fiber after focusing. The light was irradiated to the device under test through the optical fiber above the plasma etcher cavity, and then entered the spectrometer through the optical fiber below the cavity. The spectrometer converted the light of the optical fiber circuit into an electrical signal, thereby obtaining a series of spectra to characterize the material. Finally, the etching system and the spectral system were integrated, and the etching inspection and analysis were integrated and connected to the software terminal to achieve real-time detection.

[0022] At least one embodiment of the present application innovatively uses soft plasma etching technology based on previous detection technologies, and can perform internal depth inspection of materials through non-destructive etching. In terms of optical system devices, at least one embodiment of the present application optimizes the optical system and achieves breakthrough innovations in optical accuracy and optical resolution detection accuracy. At the same time, at least one embodiment of the present application has a high degree of system integration, and through the "three-in-one" - etching, inspection and analysis integrated design, in-situ etching is achieved, which improves detection efficiency.

[0023] In semiconductor films, due to the presence of dopants or structural defects, the material will have free electrons or holes distributed to varying degrees, so that charge injection, transmission, photon generation, propagation and other effects often occur in different sublayers. Therefore, measuring the structural properties of the film at different depths can provide a more comprehensive understanding of the overall material performance. The organic layer in the organic semiconductor film is thinned layer by layer by high-pressure plasma, and the internal sublayer is gradually exposed by etching the surface of the film layer by layer. The mapping between the optical spectrum and the fault depth is established by using ultraviolet, infrared and Raman spectroscopy techniques, and the sublayer absorption spectrum of the organic (including polymer) film can be obtained, and then the accurate data of the material structure properties can be obtained. Therefore, soft plasma detection technology can deeply detect the internal structure of organic semiconductor films and obtain more accurate and comprehensive data.

[0024] The optical system of the instrument uses a high-brightness xenon lamp, which is three times brighter than an ordinary light bulb, but consumes only two-thirds of the energy. At the same time, its spectrum ranges from ultraviolet to near-infrared, which enhances the measurement breadth. The light it emits is transformed by a hemispherical lens into parallel light, which is focused and enters the optical fiber. The light is irradiated to the device under test through the optical fiber on the plasma etcher cavity, and then enters the spectrometer through the optical fiber under the cavity. The spectrometer converts the received optical signal into an electrical signal, that is, obtains a series of spectra. Therefore, this instrument system enhances the measurement breadth and accuracy by optimizing the xenon lamp parameters.

[0025] In terms of energy supply to the optical system, the DC power supply is used to provide stable voltage and current for the light source to ensure continuous and stable operation of the light source. In order to ensure that the light intensity is adjustable, the output voltage of the power supply is controlled between 0-25V, the output current is between 7-9A, the current instability is limited to 0.05%, and the accuracy is within 0.1%. The enhanced stability of the power supply system has greatly improved the stability of the inspection process and inspection results.

[0026] Innovation point 1: Develop soft plasma etching technology to etch the sample film layer by layer to achieve non-destructive etching.

[0027] At least one embodiment of the present application is developed using soft plasma etching technology to etch samples layer by layer to deeply detect the internal structure information of the samples. During the detection process, the chemical and physical parameters of the plasma generator are adjusted so that the inspection of this layer during the etching process will not affect the chemical and physical properties of the underlying sublayer. The gentle layer-by-layer etching ensures the information restoration and stability, greatly improving the inspection accuracy, making the vertical resolution less than 2nm, which is about one fifty-thousandth of the diameter of a hair.

[0028] Innovation 2: Optimize the optical system to improve optical accuracy and resolution

[0029] The team designed a sealed vacuum chamber, which enables the entire optical path inspection to achieve a closed vacuum circuit, which is minimally affected by the external environment. Based on optoelectronic devices, the team constructed six basic angle-resolved spectral measurement modes, which can more specifically measure the different characteristics of organic semiconductor films, greatly improving the accuracy and resolution of optical inspections. The optical accuracy was increased by 57%, and the optical resolution was as high as 0.1nm, achieving a breakthrough in detection accuracy.

[0030] Innovation point 3: "Three-in-one" - integrated design of etching inspection and analysis to improve detection efficiency. By obtaining the dynamic changes of absorption spectrum, fluorescence spectrum and reflection spectrum in the etching process in situ, the vertical dimension is added on the basis of the traditional one-dimensional spectrum to expand the spectrum into a two-dimensional spectrum. Each time the etcher etches a layer, the spectrometer synchronously inspects the layer and transmits the data of the layer. The optical parameter distribution and charge transport characteristics in photovoltaic devices and thin-film transistors can be solved by using the Fermi-Dirac statistics of the transfer matrix optical model and Poisson's equation. Ultimately, the detection accuracy is improved to achieve a breakthrough innovation, so that the time resolution is less than 1ms and the spatial resolution is as high as 1nm.

[0031] Technical effect:

[0032] (1) Two-dimensional spectral detection technology has greatly improved the spatial resolution of optical inspection, making the vertical spatial resolution less than 2nm.

[0033] (2) The integrated organic semiconductor film internal detection spectrometer produced can achieve a detection accuracy of 1nm, which is about one fifty thousandth of the diameter of a hair, with an optical resolution of up to 0.1nm and a time resolution of 1ms.

[0034] (3) Realize internal detection of organic semiconductor films by using soft plasma etching technology combined with an optimized optical system and an integrated design of etching detection and analysis to achieve in-situ non-destructive etching.

[0035] Technical advantages:

[0036] (1) Organic semiconductors refer to organic materials with semiconductor properties. Compared with traditional inorganic semiconductors, organic semiconductor films have the advantages of low synthesis cost, superior performance and greater safety for the human body, making them a new focus of global material research and development. Our team's products have been developed by building and debugging a spectral testing platform based on an in-situ etching spectrometer, testing the homemade PTB7 to calculate the fluctuation of vertical optical constants, calculate the photoelectric field distribution, energy distribution, exciton generation rate distribution and short-circuit current density, and producing and developing a "plasma in-situ etching spectrometer", which truly realizes in-situ etching and in-situ spectral analysis of polymer films, greatly improves the accuracy of the spectrum, and achieves a new breakthrough in my country's semiconductor technology industry.

[0037] (2) The semiconductor thin film tomography absorption spectrometer developed by this research team uses a breakthrough soft plasma source etching technology. Compared with the existing detection technology on the market, it expands "one dimension" to "two dimensions", and the qualitative change of the detection dimension greatly improves the detection accuracy. At the same time, the spectrum analysis software adapted to at least one embodiment involved in this application has a background parameter debugging function compared to similar products, which improves the accuracy of measurement and identification to a certain extent. In terms of function implementation, user needs are fully taken into consideration, and the measured spectral data can be directly exported in txt format, which is convenient for realizing the algorithm analysis of the optical electric field.

[0038] (3) At least one embodiment of the present application uses the Fermi-Dirac statistics of the transfer matrix optical model and Poisson's equation to solve the optical parameter distribution and charge transport characteristics in photovoltaic devices and thin film transistors. Combined with the experimentally obtained sub-layer optical and electrical properties, the photoelectric properties of the thin film can be studied more accurately. This project provides a basis for improving the performance of the thin film by analyzing the aggregated structure and photoelectric properties of the thin film sub-layer, making the detection technology more mature and stable.

[0039] This project overcomes the shortcomings of most traditional domestic absorption spectrometers, such as single function and insufficient measurement accuracy. Its tomographic resolution can reach 1nm, optical resolution can reach 0.13nm, and time resolution can reach 1ms, which can effectively replace and supplement the traditional spectrometer market. Specific implementation method:

[0041] 1. Soft plasma etching process

[0042] 1.1 Etching Principle

[0043] Plasma etching technology is a technology that uses plasma for thin film micromachining. Under low pressure, the reaction gas is ionized and forms plasma under the excitation of radio frequency power. Plasma is mainly composed of electrons, ions and active reaction groups (such as active free radicals), which is used to describe the material form in the gas discharge tube. The active reaction groups react chemically with the surface of the etched material to form volatile reaction products, which are separated from the surface of the etched material and are extracted from the cavity by the vacuum system. During the etching process, the etched material is placed on the bias electrode. A DC bias is formed between the plasma and the bias electrode, and the positively charged reaction gas ions are accelerated to hit the surface of the etched material. This ion bombardment can greatly accelerate the chemical reaction on the surface and accelerate the desorption of the reaction products, resulting in a very high etching rate. It is precisely because of the existence of ion bombardment that anisotropic etching can be achieved.

[0044] 1.2 Technical Implementation

[0045] This instrument uses soft plasma etching technology, and uses high-voltage plasma to thin the organic layer in the organic semiconductor film layer by layer. It etches layer by layer, and uses a special process to suppress micro-scale filament discharge. By etching the surface of the film layer by layer, its internal sublayers are gradually exposed, and the transmission spectrum and reflection spectrum can be obtained in situ at the same time. The physical and chemical parameters inside the device are precisely controlled. Compared with the chemical etching of traditional inspections, non-chemically doped physical etching is truly realized. When the organic semiconductor film is thinned layer by layer, the underlying sample to be tested will not be corroded due to chemical reactions. The method is gentle, highly safe, and can reduce sample loss. Principle of soft plasma etching (a) Capacitive coupled discharge, air ionization; (b) Plasma bombardment of the surface of the organic sample; (c) Physical and chemical reactions occur on the surface of the organic sample; (d) By-products are extracted from the cavity;

[0046] 1.3 Internal design of etching device

[0047] Etching device structure of the spectrometer: The touch screen at the front end can display all the etching information of the machine, including controlling the etching process with the start or stop button, adjusting the etching power, etching time, gas selection and other parameters. There are two air inlets A and B at the rear of the machine, connected to the gas tank containing the gas used. The gas used can be modulated through the touch screen to set the gas mixing ratio, and the specific flow of the gas can be monitored through the pressure reducing valve of the gas tank and the flow meter on the lower left of the machine. The air outlet at the tail of the machine is connected to the vacuum pump to remove the air in the cavity. When in use, turn on the machine, first use the vacuum pump to vacuum the cavity, set the etching parameters on the touch screen, open the gas pressure reducing valve, pass the gas, and then etch. After the etching is completed, close the pressure reducing valve, open the balance valve, and pass the gas into the cavity.

[0048] At least one embodiment involved in the present application uses "soft plasma etching technology", which is simple and efficient to operate, and can accurately adjust various parameters to meet different detection needs. Soft plasma etching uses physical and chemical reactions to achieve non-destructive etching to a large extent, greatly improving the detection accuracy and raising the detection accuracy to the nanometer level.

[0049] 2. Optical Devices

[0050] 2.1 Factors associated with optical inspection

[0051] Organic polymer photovoltaic films based on donor-acceptor phase heterogeneous structures often have different optical absorption characteristics at different positions in the vertical direction of the film. The optical absorption peak position and intensity of the polymer are related to the following factors: (1) The polymer molecules are relatively long and can be regarded as composed of different molecular segments. The HOMO and LUMO energy levels between different segments are different, which leads to the dispersion of the film energy gap; (2) The polymer molecular weight is polydisperse; (3) Crystalline polymers are generally semi-crystalline, and there are both amorphous and crystalline phases in the film. Their respective molecular conformations are quite different, and the corresponding optical absorption characteristics are also significantly different; (4) The molecular orientation in the film is different on the surface and inside the film; (5) The two components of the donor and acceptor have vertical phase separation due to chemical incompatibility. The above factors indicate that in polymer semiconductor film materials, the optical absorption characteristics of the film are different at different depths inside the film. This uneven distribution has a great influence on the device performance. We use continuous plasma etching technology and in situ test the optical absorption spectrum of the material. The continuous Beer-Lambert law and appropriate optical models are used to achieve depth-resolved optical absorption spectroscopy of thin films, providing support for thin film structure analysis, light-matter interaction, and optoelectronic device performance optimization.

[0052] 2.2 Sealed vacuum chamber

[0053] In order to realize in-situ etching spectrum analysis, our team designed a sealed vacuum chamber, fixed a discharge plate in the cavity, and polished the cavity wall smoothly. The discharge process adopts the capacitive coupled discharge mode. One end of the symmetrical probe is connected to the collimator, and the other end is connected to the optical fiber. The sample to be tested is placed on the tray, and the light path directly passes through the holes above and below the cavity to form an optical circuit. A closed vacuum circuit is realized for the entire optical path inspection, which is minimally affected by the external environment, and the inspection accuracy is greatly improved. The fully encapsulated structure will not directly touch any dangerous items during operation, and there are no items inside the instrument that may cause explosions, fires, and other accidents, ensuring the personal and property safety of the operator.

[0054] 2.3 Optoelectronic devices

[0055] The plasma in-situ etching spectrometer is composed of a DC power supply, an in-situ plasma etcher, a vacuum pump, a light source, a spectrometer and a measuring terminal. The DC power supply is used to provide stable voltage and current to the light source to ensure that the light source works continuously and stably. In order to ensure that the light intensity is adjustable, the output voltage of the power supply is controlled at 0-25V, the output current is 7-9A, the current instability is limited to 0.05%, and the accuracy is within 0.1%. In terms of the optical system of the instrument, a high-brightness 150W xenon lamp is used. The brightness of the xenon lamp is three times that of an ordinary bulb, but the energy consumption is only two-thirds. The spectral range of the light it emits is from ultraviolet to near-infrared, which increases the breadth of organic semiconductor film inspection. The light of the xenon lamp is transformed by a hemispherical lens into parallel light, which enters the optical fiber after focusing. The light is irradiated to the device under test through the optical fiber on the plasma etcher cavity, and then enters the spectrometer through the optical fiber under the cavity. The spectrometer converts the received optical signal into an electrical signal, that is, a series of spectra are obtained.

[0056] Based on optoelectronic devices, at least one embodiment involved in the present application can realize six basic angularly resolved spectral measurement modes, including: reflection mode, transmission mode, scattering mode, radiation mode, free mode and programming mode. The six modes can be switched freely and flexibly, and can measure the different characteristics of organic semiconductor films more specifically, making full use of the advantages of optical detection and achieving a significant improvement in the accuracy of optical resolution to 0.13nm.

[0057] 2.4 Summary

[0058] At least one embodiment of the present application can use an optical path device to optically inspect an organic semiconductor thin film sample to be tested in real time, using a transfer moment

[0059] The Fermi-Dirac statistical method based on the array optical model and Poisson's equation is used to solve the optical parameter distribution and charge transport characteristics in photovoltaic devices and thin film transistors. Combined with the experimentally obtained sublayer optical and electrical properties, the photoelectric properties of thin films can be studied more accurately. This project provides a basis for improving the performance of thin films by analyzing the aggregated structure and photoelectric properties of thin film sublayers.

[0060] 3. Etching, Spectroscopy and Analysis Integration Technology

[0061] 3.1 “Three-in-one technology integration”

[0062] This optical inspection instrument is well integrated with plasma etching technology, two-dimensional "spectral" detection technology and the matching new spectral analysis software Morpho. Soft plasma etching uses the discharge mode of capacitive coupling to make the light path directly pass through the holes above and below the cavity to form an optical circuit, which can realize the function of measuring reflectivity, transmittance and absorptivity at the same time. In-situ etching spectrum detection technology can simultaneously capture the transmittance, reflectivity, absorptivity of the test sample and the vertical resolution of the research polymer. The captured detection data can quickly enter the Morpho tomographic spectrum software for intuitive display and multi-dimensional analysis, so that the time resolution reaches 1ms.

[0063] 3.2 Two-dimensional spectral inspection

[0064] At least one embodiment involved in the present application adopts spectral "two-dimensional" analysis technology. Based on the etching technology, the spectral data of each layer is collected by an ultraviolet spectrometer, which can analyze the performance of organic semiconductor films at different depths, better unfold the relevant information of the sample to be tested, break through the information dimension, and obtain the internal information of the fault of the inspection sample.

[0065] This technology can realize spectral analysis such as reflection spectrum, transmission spectrum, fluorescence spectrum, Raman spectrum, etc. of micron-level samples, accurately collect spatially resolved spectral information, and greatly improve the spatial resolution of optical inspection, making the vertical spatial resolution less than 2nm.

[0066] At the same time, this two-dimensional spectral inspection technology has strong graftability and can be applied to a variety of spectral technologies. In addition to traditional ultraviolet light, it can also better adapt to a variety of light sources such as near-infrared light and laser.

[0067] 3.2 Integrated detection device

[0068] The spectrometer consists of a DC power supply, an in-situ soft plasma etcher, a vacuum pump, a light source, a spectrometer, and a measurement terminal. During the etching process, the thickness of the sample decreases with the plasma etching, and the computer terminal monitors the changes in the spectrum in real time. The whole process is intuitive and clear. In the whole experiment, "in-situ" in a dual sense is achieved, that is, the organic semiconductor film sample to be tested will be fixed in the same position to achieve in-situ etching and in-situ detection.

[0069] In the internal structure of the etcher, the sample on the tray is cleverly arranged so that it is in the optical path. Slight changes in thickness are evident in the spectrum. This allows the sample to remain in place during the etching process, reducing errors and improving optical accuracy by 57%.

[0070] 3.3 Spectral analysis software

[0071] At least one embodiment of the present application may be directly connected to a computer terminal, so that the terminal may directly obtain spectral data from the spectrometer.

[0072] The optical inspection instrument is equipped with the self-developed Morpho spectrum analysis software, which can directly measure the reflection spectrum, transmission spectrum, absorption spectrum of the sample, and also has the functions of measuring plasma emission spectrum, Raman spectrum, chromatography, etc.

[0073] Performance Comparison

[0074] Organic semiconductor thin film internal detection technology involves many complex processes such as material etching and spectral analysis.

[0075] In the severe context of technological blockade, we have addressed the actual needs and difficulties encountered in the testing process through independent research and development, overcome difficulties, and achieved overtaking in products and technology, turning "bottlenecks" into "trump cards."

[0076] At present, the main semiconductor thin film analysis technologies at home and abroad are electron microscopy, X-ray diffraction and micro-fiber spectroscopy. Electron microscopy can be used to study the surface morphology of solids and obtain three-dimensional images of solid surfaces. Material scientists can use electron microscopes to obtain information on the microstructure and chemical composition of materials from the atomic scale. X-ray diffraction (XRD) is a research method that obtains information such as the composition of materials, the structure or morphology of atoms or molecules inside materials by performing X-ray diffraction on materials and analyzing their diffraction patterns. Micro-fiber spectroscopy can directly reflect the spectral information of materials, obtain the existence status and material composition of the target, and is one of the most important technologies in the fields of material characterization and chemical analysis. For example, Shimadzu Corporation of Japan uses electron microscopy, Thermo of the United States uses X-ray diffraction, and Ocean Optics of the United States uses micro-fiber spectroscopy. The performance of the internal detection of semiconductor thin films of these three technologies is summarized and compared with our products as shown in the following table.

[0077] Through multi-dimensional comparison with international products, our team innovatively adopted tomographic absorption spectroscopy technology to avoid many pain points of traditional spectroscopy technology, and achieved the improvement of comprehensive performance and the reduction of preparation costs. Limited by the constraints of the original internal detection technology, tomographic inspection has never been realized. Our team took the lead in achieving a breakthrough in spectral two-dimensionalization and achieved a great leap from "point to surface". The product has excellent performance, and while exceeding the data volume of the same product by at least three times, it also raises the data accuracy to a high standard of 99%. In addition, in the field of high-tech, a small mistake can lead to a big mistake. When semiconductor research was trapped in the dilemma of substandard resolution, we kept improving, and the optical resolution of the instrument took the lead in reaching the 0.15nm mark, which was a huge breakthrough in the detection process. Improving quality, increasing efficiency and reducing costs are the essential requirements of high-quality development. Our team has also improved in cost control, basically achieving the lowest price for products of the same grade.

[0078] Table 1 Product comparison table

[0079]

[0080] It should be understood by those skilled in the art that the embodiments of the present invention described above and shown in the accompanying drawings are only examples and do not limit the present invention. The purpose of the present invention has been fully and effectively achieved. The functional and structural principles of the present invention have been demonstrated and explained in the embodiments, and the embodiments of the present invention may be deformed or modified in any way without departing from the principles.

Claims

1. A method for detecting an organic semiconductor thin film, characterized in that: The steps include: Soft plasma etching of an organic semiconductor thin film sample: and In situ spectral detection.

2. An organic semiconductor thin film detection device, suitable for detecting an organic semiconductor thin film, characterized in that: include: A direct current power supply, an in-situ soft plasma etcher, a vacuum pump, a light source and a spectrometer, wherein the organic semiconductor film is suitable for being placed in the soft plasma etcher for etching to gradually expose its internal sublayers, wherein the soft plasma etcher has a closed cavity and is respectively connected to the light source and the spectrometer to form an optical circuit, the light source is suitable for emitting light and the light enters the cavity to irradiate the sample, and then enters the spectrometer through the optical path, and the spectrometer converts the optical signal into an electrical signal to realize the detection of the sample.