SLR optical sensor and preparation method and application thereof
By adopting a hexagonal close-packed gold and silver array structure in the optical sensor and using the surface lattice resonance phenomenon to measure the wavelength shift, the problem of low sensitivity of refractive index measurement in the existing technology is solved, and high-precision and efficient environmental refractive index detection is achieved. .
Patent Information
- Application Number
- CN202410773876.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-14
- Publication Date
- 2024-10-01
AI Technical Summary
Existing refractive index measurement methods based on surface plasmon resonance (SPR) peaks have the problem of low sensitivity, making it difficult to efficiently measure refractive index changes in the environment.
A hexagonal close-packed gold and silver array optical sensor based on the surface lattice resonance phenomenon is used to measure the environmental refractive index by measuring the wavelength shift. The sensor is composed of a metal alloy supersurface layer and a transparent substrate layer, and the metal alloy hemispheres are packed according to the hexagonal close-packing The arrangement is arranged to form a periodic array structure, which is prepared by liquid surface transfer method and coating process.
The sensitivity and accuracy of refractive index measurement are improved, and the sensitivity reaches 396.95 (nm/RIU), which expands the measurement range, reduces measurement costs, and improves measurement efficiency.
Smart Images

Figure CN118730973A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to an SLR optical sensor and a preparation method and application thereof, belonging to the technical field of plasma photoelectric devices and material preparation. Background Art
[0002] Noble metal (e.g., gold, silver, platinum, palladium, etc.) nanoparticles have attracted extensive attention in the past few decades due to their unique optical properties, catalytic performance, and localized surface plasmon resonance (LSPR). In particular, the characteristics of the surface plasmon resonance (SPR) peaks of these nanoparticles depend on their composition, size, shape, and local dielectric environment, making them widely used in biochemical sensors and surface-enhanced Raman spectroscopy.
[0003] Among them, spherical Au nanoparticles have been widely studied due to their chemical stability and precise surface plasmon resonance peaks. In most LSPR sensors, the size of spherical Au nanoparticles is fixed, and the interaction between the probe molecules and the sensor causes a change in the refractive index around it, which causes a sensitive shift of the SPR peak. However, this SPR peak shift is still relatively small, resulting in relatively low sensitivity.
[0004] The measurement of refractive index is crucial in fields such as chemistry, industry, biosensing and environmental monitoring. However, the current measurement method based on surface plasmon resonance (SPR) peak has the problem of low sensitivity. Therefore, how to improve the sensitivity of refractive index measurement has become a key issue. Summary of the invention
[0005] In order to solve the above problems, the present application proposes a hexagonal close-packed gold-silver array optical sensor based on surface lattice resonance phenomenon and a preparation method thereof, which can measure the ambient refractive index by measuring wavelength shift.
[0006] In one aspect of the present application, a SLR optical sensor is provided, wherein the SLR optical sensor comprises, from top to bottom, a metal alloy super surface layer and a transparent substrate layer;
[0007] The metal alloy super surface layer is composed of a periodic array structure formed by metal alloy hemispheres arranged in a hexagonal close-packed manner.
[0008] Optionally, the dielectric constant of the transparent substrate layer is 1.1-3.0.
[0009] Optionally, the light transmittance of the transparent substrate layer is 50% to 99.9%.
[0010] Optionally, in the array structure on the metal alloy super surface layer, the lattice spacing is d, 300nm≤d≤800nm;
[0011] The diameter of the metal alloy hemisphere is D, 100nm≤D≤d.
[0012] Optionally, the metal alloy in the metal alloy hemisphere includes at least two metal elements of gold, silver, copper and aluminum.
[0013] Optionally, the effective working spectrum of the SLR optical sensor is 300-800 nm.
[0014] Optionally, in the SLR optical sensor, the thickness of the metal alloy super surface layer is 20 to 300 nm.
[0015] Another aspect of the present application provides a method for preparing the above-mentioned SLR optical sensor, the preparation method comprising:
[0016] (1) mixing polystyrene microspheres with water to obtain a self-assembled polystyrene microsphere solution;
[0017] (2) preparing a polystyrene microsphere layer having a two-dimensional array structure of hexagonal close-packed shapes on the transparent substrate layer by a liquid surface transfer method;
[0018] (3) depositing metal films of the same thickness and different metal elements on the polystyrene microsphere layer in steps;
[0019] wherein, in each step, a metal film containing one of the metal elements is deposited;
[0020] (4) Annealing is performed under inert atmosphere conditions to obtain the SLR optical sensor.
[0021] Optionally, in the polystyrene microsphere solution, the mass fraction of the polystyrene microspheres is 0.1% to 10%;
[0022] The diameter of the polystyrene microspheres is 10nm to 1000nm.
[0023] Optionally, the metal film has a thickness of 1 to 50 nm.
[0024] Optionally, the inert atmosphere is selected from at least one of argon and nitrogen;
[0025] The annealing temperature is 500° C. to 1200° C.;
[0026] The annealing time is 2h to 12h.
[0027] As a specific implementation, the method for preparing the SLR optical sensor includes:
[0028] 1. First prepare a transparent medium with an appropriate dielectric constant. Theoretical calculations must be performed in advance to determine its parameters.
[0029] 2. Prepare a polystyrene microsphere solution of appropriate size and concentration.
[0030] 3. Distribute the polystyrene microspheres on the substrate surface in the form of hexagonal close packing.
[0031] 4. Use high-precision coating technology to deposit gold and silver films of equal thickness on the sample surface.
[0032] 5. Perform high temperature annealing in an argon atmosphere.
[0033] As a specific implementation, the present application relates to a gold-silver array metal supersurface structure optical sensor chip based on a strontium titanate single crystal substrate, wherein the sensor can be subdivided from top to bottom into a gold-silver array metal supersurface and a strontium titanate substrate layer. The gold-silver array is composed of gold-silver hemispheres, forming a hexagonal close-packed periodic structure. The strontium titanate substrate needs to have an appropriate dielectric constant and light transmittance. When the detection light is vertically incident on the optical chip, by measuring the extinction spectrum of the optical chip, the peak displacement related to the ambient refractive index on the extinction spectrum can be obtained, thereby measuring the change in the ambient refractive index.
[0034] The specific parameters of the optical chip proposed by the present invention are as follows: the size of the strontium titanate single crystal is 5×5×0.1mm, and it is a double-polished single crystal. The gold-silver array is composed of gold-silver alloy hemispheres with a diameter of 120nm, which are evenly distributed on the surface of the strontium titanate single crystal in a hexagonal close-packed periodic structure. The effective working spectrum range of the optical chip is 400nm-800nm.
[0035] In another aspect of the present application, there is provided an application of the above-mentioned SLR optical sensor in detecting the refractive index of an environment.
[0036] Another aspect of the present application provides a method for detecting an environmental refractive index, using the above-mentioned SLR optical sensor;
[0037] The method comprises:
[0038] (1) placing the SLR optical sensor in environments with different refractive indices respectively, and measuring different diffraction peaks λ after being irradiated by an incident light source;
[0039] (2) According to the Rayleigh anomaly formula, the ambient refractive index under different diffraction peaks λ is calculated, and the linear relationship between the ambient refractive index and the peak offset is obtained by fitting;
[0040] Among them, the formula for Rayleigh anomaly is:
[0041]
[0042] Where D is the lattice spacing, n1 is the ambient refractive index, n2 is the substrate refractive index, m and l are different diffraction mode orders, θ is the incident angle, and C is a constant;
[0043] (3) placing the SLR optical sensor in a test environment, and after being irradiated by an incident light source, measuring the peak shift, and obtaining the refractive index of the test environment according to the linear relationship obtained in step (2);
[0044] Wherein, the incident light is linearly polarized light, and the polarization direction of the incident light is the same as the direction in which the metal alloy hemispheres are arranged.
[0045] The beneficial effects of this application include:
[0046] Compared with the traditional plasmon-based refractive index measurement method, the detection method provided in this application has the following beneficial effects:
[0047] (1) Improved measurement accuracy, with a sensitivity of 396.95 (nm / RIU);
[0048] (2) The measurement range has been expanded, and the specific environmental refractive index can be detected from 1.0-2.0;
[0049] (3) The measurement efficiency is improved. It only needs to put the sample to be tested into the sample cell and measure the change of the diffraction peak. Then, the specific value of the refractive index can be quickly obtained by comparing with the standard parameters.
[0050] (4) Cost savings: Due to the improved measurement efficiency and accuracy, the optical device may be able to save resources required in the measurement process, thereby reducing the measurement cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] Figure 1 This is a schematic diagram of the gold-silver array structure that produces the surface lattice resonance phenomenon in Example 1 of the present application.
[0052] Figure 2 for Figure 1 Diagram of the basic optical principle of the structure's surface lattice resonance.
[0053] Figure 3 This is the extinction spectrum of the gold-silver array at different lattice spacings in Example 2.
[0054] Figure 4 This is the extinction spectrum of the gold-silver array under different environmental refractive indices in test example 2.
[0055] Figure 5 This is the linear fitting of the relationship curve between the change in the ambient refractive index and the wavelength shift in test example 2.
[0056] Figure 6It is a flow chart of a method for preparing an optical sensor according to an embodiment of the present invention. DETAILED DESCRIPTION
[0057] The present application is described in detail below with reference to embodiments, but the present application is not limited to these embodiments.
[0058] Unless otherwise specified, the raw materials in the examples of this application were purchased through commercial channels.
[0059] The analysis method in the examples of this application is as follows:
[0060] The instruments required for the test mainly include:
[0061] Light source: A device that can provide a stable, continuous light source, such as a laser, a high-pressure mercury lamp or a xenon lamp.
[0062] Monochromator: Separates the incident light beam into different wavelengths for subsequent measurement. Using a high-quality monochromator can achieve more accurate results.
[0063] Sample cell: also called absorption cell, used to load the sample to be tested.
[0064] Optical sensor: For solid samples, the sample to be tested needs to be evenly covered on the optical sensor. For liquids and gases, no additional operation is required.
[0065] Detector: Usually a phototube or photomultiplier tube, used to detect the intensity of light after passing through the sample.
[0066] The steps are as follows:
[0067] Sample processing: Choose appropriate samples and sample processing methods according to experimental requirements. For example, liquids and gases need to be diluted when the concentration is too high, and solid materials need to be ground.
[0068] Loading samples: Place the processed samples and optical sensors into the sample cell and install them into the experimental device.
[0069] Connect equipment: Connect the experimental device to equipment such as a power source or computer.
[0070] Adjustment parameters: Adjust the parameters of the light source and detector, such as the brightness and wavelength of the light source, the gain of the detector, etc.
[0071] Example 1
[0072] according to Figure 6 The optical sensor is prepared by the process.
[0073] (1) Prepare a double-polished strontium titanate transparent substrate:
[0074] The size of the strontium titanate single crystal is 5×5×0.1 mm, and it is a double-polished single crystal sheet.
[0075] (2) Preparation of polystyrene microsphere suspension: First, prepare a polystyrene microsphere suspension 1 with a polystyrene microsphere mass fraction of 0.5% and a water to ethanol volume ratio of 1:1. The size of the polystyrene microsphere is 420 nm.
[0076] (3) Preparation of hexagonal close-packed two-dimensional film: Wet one side of the Si substrate with a polystyrene microsphere suspension. Then place the Si substrate with the wetted side facing up in an inclined position underwater. The polystyrene microspheres on the Si substrate diffuse on the water surface and spontaneously assemble into a single-layer polystyrene microsphere film under the action of the water surface tension. Then place the double-polished strontium titanate substrate in an inclined position under the polystyrene microsphere film, lift up the double-polished strontium titanate substrate to transfer the polystyrene microsphere film to the double-polished strontium titanate substrate. Dry the double-polished strontium titanate with the polystyrene microsphere film at room temperature to form a polystyrene microsphere template.
[0077] (4) A 7nm thick silver film and a 7nm thick gold film are deposited step by step on the polystyrene microsphere template obtained in step (3), that is, a 7nm thick silver film is first deposited, and then a 7nm thick gold film is deposited. The specific steps of deposition are to prepare all necessary equipment and materials, including Leica high vacuum coater, gold target, argon gas, silver target, polystyrene microsphere template, etc. Install the gold target or silver target into the Leica high vacuum coater, and place the polystyrene template into the sputtering chamber. Start the vacuum pump and evacuate the sputtering chamber to a high vacuum state. Introduce argon gas into the sputtering chamber, generate plasma through power supply, and cause argon ions to sputter the gold / silver target. By adjusting and setting the parameter thickness, the desired film thickness can be achieved. The coating is set to 7nm this time. After the sputtering is completed, turn off the power supply and let the equipment cool naturally.
[0078] (5) The sample obtained in step (4) was annealed at 1000°C for 4 h in an argon atmosphere.
[0079] Test Example 1
[0080] The optical sensor obtained in Example 1 was placed in different refractive index medium solutions, and the incident light was Figure 2 The light is irradiated into the optical sensor obtained in Example 1 and the diffraction peak λ is measured.
[0081] in, Figure 2 This shows the requirements of optical sensors for incident light. The incident light must be linearly polarized, and the polarization direction must be the same as the direction in which the gold and silver particles are arranged. After theoretical calculations in advance, if the lattice spacing, surface material, and substrate dielectric constant are within the appropriate range, surface lattice resonance will occur. The absorption peaks of surface lattice resonance will become very sharp, and secondary diffraction peaks that are extremely sensitive to the refractive index will also be generated. These peaks are also called Rayleigh anomalies. The effect of detecting the ambient refractive index can be achieved by monitoring the diffraction peaks.
[0082] Example 2
[0083] An optical sensor was prepared according to the preparation method of Example 1, wherein the difference from Example 1 lies in that different lattice spacings of 300, 340, 380, 420, 460, and 500 nm were used.
[0084] The extinction spectra of the obtained optical sensors with different lattice spacings are measured. The measurement results are as follows: Figure 3 shown.
[0085] Figure 3 In the figure, (a) is the three-dimensional extinction spectrum of this optical sensor when the lattice spacing is changed, and the white line is the area of Rayleigh anomaly. (b) is the two-dimensional extinction spectrum of a part of the lattice spacing in (a). The first thing is to observe that as the lattice spacing increases, the extinction peak gradually becomes sharper, and a new extinction peak appears at the same time. The first phenomenon is because as the lattice spacing gradually approaches the optimal spacing, the excitation mode of the gold and silver array slowly changes from the original surface plasmon resonance (SPR) to the surface lattice resonance (SLR). The second phenomenon can be considered as a Rayleigh anomaly. The periodic structure will produce secondary diffraction modes, and each different mode will produce a new extinction peak. The formula for Rayleigh anomaly is:
[0086]
[0087] Among them, D is the lattice spacing, n1 is the ambient refractive index, n2 is the substrate refractive index, m, l are different diffraction mode orders, and θ is the incident angle. Therefore, by substituting the relevant parameters, we can find that the diffraction peak λ generated by the Rayleigh anomaly is a linear function of the ambient refractive index n, so we can use the diffraction peak λ to detect the change of the ambient refractive index.
[0088] Test Example 2
[0089] The diffraction peak λ was measured according to the method of Test Example 1, except that the refractive index of the test environment was changed to 1.0-2.0 with an interval of 0.05. The test results are shown in Figure 4 a. Figure 4 b is Figure 4 The extinction spectrum of 1.0-1.35 was extracted in a.
[0090] Figure 4 This is the extinction spectrum of the optical sensor after changing the refractive index after selecting a 420nm lattice spacing. It can be observed that within the response range of 400-800nm of the present invention, the diffraction peak generated by the Rayleigh anomaly shown by the white line shows a linear relationship with the change of the ambient refractive index, which is completely consistent with the previous theoretical formula prediction. Observing the extinction spectrum in the range of 1.0-1.35, the change of the diffraction peak is very clear.
[0091] Figure 5 It is the refractive index change, the deviation of the diffraction peak. It can be found that as the ambient refractive index increases, the peak wavelength moves toward the long-wave direction. Linear fitting of the peak shifts corresponding to different refractive indices can be obtained, and the sensitivity of the diffraction peak to the refractive index change is 396.95 (nm / RIU), which is much higher than the traditional refractive index detection method.
[0092] Although the best examples of the present invention are shown above, they are not intended to limit the present invention. By changing the substrate, the metal metasurface material and period, and the structure size, the resolution of the ambient refractive index can be achieved.
[0093] The above are only a few embodiments of the present application and do not constitute any form of limitation to the present application. Although the present application is disclosed as above with preferred embodiments, it is not intended to limit the present application. Any technician familiar with the profession, without departing from the scope of the technical solution of the present application, using the technical content disclosed above to make slight changes or modifications are equivalent to equivalent implementation cases and fall within the scope of the technical solution.
Claims
1. A SLR optical sensor, characterized in that: The SLR optical sensor comprises, from top to bottom, a metal alloy super surface layer and a transparent substrate layer; The metal alloy super surface layer is composed of a periodic array structure formed by metal alloy hemispheres arranged in a hexagonal close-packed manner.
2. The SLR optical sensor according to claim 1, characterized in that: The dielectric constant of the transparent substrate layer is 1.1 to 3.0; The light transmittance of the transparent substrate layer is 50% to 99.9%.
3. The SLR optical sensor according to claim 1, characterized in that: In the array structure on the metal alloy super surface layer, the lattice spacing is d, 300nm≤d≤800nm; The diameter of the metal alloy hemisphere is D, 100nm≤D≤d; Preferably, the metal alloy in the metal alloy hemisphere includes at least two metal elements of gold, silver, copper and aluminum.
4. The SLR optical sensor according to claim 1, characterized in that: The effective working spectrum of the SLR optical sensor is 300-800nm; Preferably, in the SLR optical sensor, the thickness of the metal alloy super surface layer is 20 to 300 nm.
5. A method for preparing the SLR optical sensor according to any one of claims 1 to 4, characterized in that: The preparation method comprises: (1) mixing polystyrene microspheres with water to obtain a self-assembled polystyrene microsphere solution; (2) preparing a polystyrene microsphere layer having a two-dimensional array structure of hexagonal close-packed shapes on the transparent substrate layer by a liquid surface transfer method; (3) depositing metal films of the same thickness and different metal elements on the polystyrene microsphere layer in steps; wherein, in each step, a metal film containing one of the metal elements is deposited; (4) Annealing is performed under inert atmosphere conditions to obtain the SLR optical sensor.
6. The preparation method according to claim 5, characterized in that: In the polystyrene microsphere solution, the mass fraction of the polystyrene microspheres is 0.1% to 10%; The diameter of the polystyrene microspheres is 10nm to 1000nm.
7. The preparation method according to claim 5, characterized in that: The thickness of the metal film is 1-50 nm.
8. The preparation method according to claim 5, characterized in that: The inert atmosphere is selected from at least one of argon and nitrogen; The annealing temperature is 500° C. to 1200° C.; The annealing time is 2h to 12h.
9. Use of the SLR optical sensor according to any one of claims 1 to 4 in detecting environmental refractive index.
10. A method for detecting an environmental refractive index, characterized in that: Use the SLR optical sensor according to any one of claims 1 to 4; The method comprises: (1) placing the SLR optical sensor in environments with different refractive indices respectively, and measuring different diffraction peaks λ after being irradiated by an incident light source; (2) According to the Rayleigh anomaly formula, the ambient refractive index under different diffraction peaks λ is calculated, and the linear relationship between the ambient refractive index and the peak offset is obtained by fitting; Among them, the formula for Rayleigh anomaly is: Where D is the lattice spacing, n1 is the ambient refractive index, n2 is the substrate refractive index, m and l are different diffraction mode orders, θ is the incident angle, and C is a constant; (3) placing the SLR optical sensor in a test environment, and after being irradiated by an incident light source, measuring the peak shift, and obtaining the refractive index of the test environment according to the linear relationship obtained in step (2); Wherein, the incident light is linearly polarized light, and the polarization direction of the incident light is the same as the direction in which the metal alloy hemispheres are arranged.