Forming method of phase change memory
By forming an initial mask structure of different materials on the composite storage layer of the phase change memory and controlling the etching process, the problem of poor uniformity of memory cell size is solved, the uniformity of electrical performance and leakage current density is improved, and the phase change is improved. Overall memory performance.
Patent Information
- Application Number
- CN202411012627.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-10-01
AI Technical Summary
The memory cell feature size of existing phase change memory has poor uniformity, resulting in poor leakage current density uniformity, affecting performance and yield.
By forming an initial mask structure on the composite storage layer, using first and second mask layers of different materials, the etching rate of the first etching process is controlled so that the mask structure is maintained in a direction parallel to the substrate surface. Uniform size, thereby improving the uniformity of size and spacing of memory cells when they are subsequently formed.
The electrical performance uniformity and leakage current density uniformity of the memory cell are improved, and the performance and yield of the phase change memory are improved.
Smart Images

Figure CN118737814A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to a method for forming a phase change memory. Background Art
[0002] Phase Change Random Access Memory (PCRAM or PCM) has higher capacity than Dynamic Random Access Memory (DRAM) and lower latency and byte-level addressing capability than Flash memory, making PCRAM one of the most promising and promising technologies in the field of Non-Volatile Memory (NVM).
[0003] The storage unit of the existing phase change memory is usually composed of a phase change storage layer, a gate layer and an electrode layer, and the storage unit is selected, read, written, programmed, etc. in combination with a word line and a bit line.
[0004] However, since the memory cell of the phase change memory has the above-mentioned complex multi-layer structure, it brings great challenges to the manufacture of the memory cell. The critical dimension (CD) uniformity of the memory cell formed by the prior art is not good, which easily causes the leakage current density uniformity (LCDU) to deteriorate, thereby deteriorating the performance and yield of the phase change memory. Summary of the invention
[0005] The purpose of the present application is to provide a method for forming a memory, aiming to improve the uniformity of feature sizes between memory cells of the formed phase change memory, thereby improving the uniformity of leakage current density of the phase change memory.
[0006] To solve the above technical problems, the technical solution of the present application provides a method for forming a phase change memory, comprising: providing a substrate; forming a composite storage layer on the substrate; forming a plurality of initial mask structures on the composite storage layer, wherein the initial mask structure exposes a portion of the composite storage layer, the initial mask structure comprises a first mask layer and a second mask layer located on the first mask layer, the material of the second mask layer is different from the material of the first mask layer; using the initial mask structure as a mask, etching the composite storage layer by a first etching process to form a first groove in the composite storage layer, the etching rate of the first etching process on the second mask layer is lower than the etching rate of the first mask layer.
[0007] In some embodiments, in the first etching process, the ratio of the etching rate of the second mask layer to the etching rate of the first mask layer is in a range of 1:3 to 1:4.
[0008] In some embodiments, the etching gas of the first etching process includes a hydrogen-containing gas and a fluorine-containing gas; the material of the first mask layer includes silicon nitride; and the material of the second mask layer includes silicon oxide.
[0009] In some embodiments, the composite storage layer includes: a gating layer located on a substrate, a phase change layer located on the gating layer, a third electrode layer located on the phase change layer, and a conductive layer located on the third electrode layer; the first groove penetrates the conductive layer, the third electrode layer and the phase change layer.
[0010] In some embodiments, the thickness of the second mask layer is greater than the thickness of the first mask layer.
[0011] In some embodiments, the ratio of the thickness of the first mask layer to the thickness of the second mask layer is in a range of 1:4 to 1:5.
[0012] In some embodiments, the method for forming the initial mask structure includes: forming a first mask material layer on the composite storage layer; hardening the first mask material layer to increase the density of the first mask material layer; forming a second mask material layer on the first mask material layer; and patterning the second mask material layer and the first mask material layer to form the first mask layer and a second mask layer located on the first mask layer.
[0013] In some embodiments, the hardening treatment includes a plasma treatment process, and a gas of the plasma treatment process includes an inert gas.
[0014] In some embodiments, it also includes: after the first etching process, the initial mask structure forms a transition mask structure; using the transition mask structure as a mask, a second etching process is used to etch the composite storage layer at the bottom of the first trench to form a plurality of discrete storage unit structures on the substrate.
[0015] In some embodiments, the method further includes: after the second etching, forming an interlayer dielectric layer on the substrate and the surface of the memory cell; performing a planarization process on the interlayer dielectric layer until the top of the memory cell is exposed, wherein the planarization process obtains a stop position according to the first mask layer; and the planarization process includes a chemical mechanical polishing process or an etch-back process. Compared with the prior art, the technical solution of the present invention has the following beneficial effects:
[0016] In the method for forming a phase change memory provided by the technical solution of the present application, by making the material of the formed second mask layer different from the material of the first mask layer, and making the thickness of the second mask layer greater than the thickness of the first mask layer, the etching rate of the second mask layer in the first etching process is smaller than the etching rate of the first mask layer, so that in the direction parallel to the substrate surface, the etching amount of the second mask layer in the first etching process is smaller than the etching amount of the first mask layer. Thus, in the first etching process, the mask structure can maintain a relatively uniform size in the direction parallel to the substrate surface, and then when the memory cell is subsequently formed by the initial composite memory layer, the memory cell has a relatively uniform size and spacing in the direction parallel to the substrate surface. The formed memory cell has a relatively uniform size and spacing in the direction parallel to the substrate surface, so that the electrical properties of the formed memory cells are uniform and stable, and the uniformity of the leakage current density is improved.
[0017] In some embodiments, before forming the second mask material layer, the first mask material layer is hardened to increase the density of the first mask material layer. On the one hand, the increase in the density of the first mask layer is beneficial to reducing the etching amount of the first mask layer in the direction parallel to the substrate surface in the first etching process, thereby further improving the morphological stability of the initial mask structure in the first etching process. On the other hand, in subsequent processes, the first mask layer can also be retained as a protective layer, avoiding the step of additionally forming a protective layer, which is beneficial to saving costs and improving process efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] The technical solution and other beneficial effects of the present application will be made apparent by describing in detail the specific implementation methods of the present application in conjunction with the accompanying drawings.
[0019] Figure 1 and Figure 2 It is a cross-sectional structural schematic diagram of an embodiment of a phase change memory formation process;
[0020] Figure 3 is a flow chart of a method for forming a phase change memory according to an embodiment of the present application;
[0021] Figures 4 to 8 is a schematic cross-sectional structure diagram of a formation process of a phase change memory according to an embodiment of the present application;
[0022] Figures 9 to 11 It is a cross-sectional structural schematic diagram of another formation process of a phase change memory according to an embodiment of the present application. DETAILED DESCRIPTION
[0023] As described in the background art, the memory cells formed by the prior art have poor uniformity of characteristic dimensions and poor uniformity of leakage current density, and the performance and yield of the phase change memory are poor.
[0024] The following is a detailed description with reference to the accompanying drawings.
[0025] Figure 1 and Figure 2 The present invention is a schematic cross-sectional structure diagram of an embodiment of a phase change memory formation process.
[0026] Please refer to Figure 1 , providing a substrate 100; forming an initial composite storage layer 110 on the substrate 100, the composite storage layer 110 comprising a first electrode layer 101 on the substrate 100, a gating layer 102 on the first electrode layer 101, a second electrode layer 103 on the gating layer 102, a phase change layer 104 on the second electrode layer 103, a third electrode layer 105 on the phase change layer 104, and a word line layer 106 on the third electrode layer 105; forming a mask structure 120 on the composite storage layer 110, the mask structure 120 exposing a portion of the composite storage layer 110.
[0027] Please refer to Figure 2 , using the mask structure 120 as a mask, etching the composite storage layer 110 to form a first trench 130 in the composite storage layer 110 to expose the second electrode layer 103 .
[0028] In the above embodiment, the material of the word line layer 106 includes tungsten, and the process gas for etching the composite storage layer 110 needs to include hydrogen-containing gas and fluorine-containing gas, so as to achieve effective etching of the word line layer 106, the first electrode layer 101 and the gate layer 102. However, since the material of the mask structure 120 in the above embodiment is silicon nitride, and silicon nitride has poor corrosion resistance in hydrogen-containing gas and fluorine-containing gas, it is easy to cause the mask structure 120 to be consumed during the etching process.
[0029] On the one hand, the etching process may cause loss of the mask structure 120 in the direction parallel to the surface of the substrate 100 and in the direction perpendicular to the surface of the substrate 100, resulting in the mask structure 120 being reduced in size in the direction parallel to the surface of the substrate 100 and also in the direction perpendicular to the surface of the substrate 100. This may not only easily lead to uneven size and morphology of the memory cells formed subsequently, but also easily lead to excessive consumption of the mask structure 120 during the etching process, and thus fail to complete the function as a mask. The uneven size and morphology of the memory cells may easily lead to degradation and differentiation of the electrical performance of the memory cells, and further lead to the problem of poor uniformity of the leakage current density.
[0030] On the other hand, since the mask structure 120 is easily consumed excessively during the etching process, after forming the first trench 130, a protective layer is usually formed on the inner wall surface of the first trench 130 and the surface of the mask structure 120, and the composite storage layer 110 is further etched under the protection of the protective layer to form a plurality of discrete storage units. The material of the protective layer usually includes silicon oxide, which is easy to leave byproducts on the surface of the formed storage unit in the subsequent process, resulting in defects on the surface of the formed storage unit.
[0031] In order to solve the above problems, the present application embodiment proposes a method for forming a phase change memory, please refer to Figure 3 , Figure 3 : is a flow chart of a method for forming a phase change memory according to an embodiment of the present application, comprising:
[0032] Step S10, providing a substrate;
[0033] Step S20, forming an initial composite storage layer on the substrate;
[0034] Step S30, forming an initial mask structure on the composite storage layer, wherein the initial mask structure exposes a portion of the composite storage layer, the initial mask structure comprises a first mask layer and a second mask layer located on the first mask layer, the material of the second mask layer is different from the material of the first mask layer, and the thickness of the second mask layer is greater than the thickness of the first mask layer;
[0035] Step S40, using the initial mask structure as a mask, adopting a first etching process to etch the composite storage layer to form a first trench in the composite storage layer, wherein the etching rate of the first etching process on the second mask layer is lower than the etching rate on the first mask layer.
[0036] The technical solution of the present application adjusts the material and thickness of the second mask layer so that the etching rate of the second mask layer in the first etching process is less than the etching rate of the first mask layer, so that the etching amount of the second mask layer in the first etching process is less than the etching amount of the first mask layer, thereby, the mask structure can maintain a relatively uniform size and morphology in the first etching process. Furthermore, when a memory cell is subsequently formed from the initial composite memory layer, the memory cell has a relatively uniform size and spacing in a direction parallel to the substrate surface, and the electrical properties of the formed memory cells are uniform and stable, and the uniformity of the leakage current density is improved.
[0037] The technical solutions in the embodiments of the present application will be described clearly and completely below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present application.
[0038] It should be understood that although the terms first, second, etc. may be used herein to describe various components, these components should not be limited to these terms. These terms are used to distinguish one component from another component. For example, a first component may be referred to as a second component, and similarly, a second component may be referred to as a first component without departing from the scope of the present application.
[0039] It should be understood that when a component is said to be "on" or "connected" another component, it can be directly on or connected to another component, or there may be an intervening component. Other words used to describe the relationship between components should be interpreted in a similar manner.
[0040] As used herein, the term "layer" refers to a portion of a material including an area having a thickness. A layer may extend over the entire underlying or superstructure, or may have an extent that is less than the extent of the underlying or superstructure. In addition, a layer may be an area of a uniform or non-uniform continuous structure having a thickness that is less than the thickness of a continuous structure. For example, a layer may be located between the top and bottom surfaces of a continuous structure or between any set of horizontal planes at the top and bottom surfaces. A layer may extend horizontally, vertically and / or along a tapered surface. A substrate may be a layer, which may include one or more layers, and / or may have one or more layers on, above and / or below it. A layer may include multiple layers. For example, an interconnect layer may include one or more conductive layers and a contact layer and one or more dielectric layers.
[0041] It should be noted that, in the embodiments of the present invention, a feature is recorded as being on the "surface" of another feature. The "surface" is only used to express the relative positional relationship between the features, and is not used to limit whether the features are in direct contact with each other.
[0042] It should be noted that the illustrations provided in the embodiments of the present application are only used to illustrate the basic concept of the present application in a schematic manner. Although the illustrations only show components related to the present application and are not drawn according to the number, shape and size of components in actual implementation, the type, quantity and proportion of each component in actual implementation may be changed arbitrarily, and the component layout may also be more complicated.
[0043] Figures 4 to 8 It is a schematic cross-sectional structure diagram of a formation process of a phase change memory according to an embodiment of the present application.
[0044] Please refer to Figure 4 , providing a substrate 200; forming a device layer 210 on the substrate 200, wherein the device layer 210 has a first conductive structure 201.
[0045] In this embodiment, the substrate 200 is a planar substrate; the planar substrate is a bulk substrate, and the bulk substrate is a silicon substrate, a silicon germanium substrate, a silicon carbide substrate, a silicon on insulator (SOI) substrate, a germanium on insulator (GOI) substrate, a glass substrate or a III-V compound substrate (such as silicon nitride or gallium arsenide, etc.).
[0046] In some other embodiments, the substrate includes: a base, a fin located on the surface of the base, and an insulating layer located on the surface of the base and covering a portion of the sidewall of the fin. In one embodiment, the fin is a single body structure; in another embodiment, the fin includes a plurality of stacked and mutually separated nanowires.
[0047] In this embodiment, the device layer 210 includes a dielectric layer located on the substrate 200 and an electrical interconnection structure located in the dielectric layer. The material of the dielectric layer includes one or more stacks of silicon oxide, silicon nitride, silicon oxynitride, low-k dielectric materials and ultra-low-k dielectric materials. The electrical interconnection structure includes at least one electrical interconnection layer, and a plurality of conductive plugs located between two electrical interconnection layers or between an electrical interconnection layer and a substrate; the material of the electrical interconnection structure includes one or more combinations of copper, tungsten, aluminum, silver, titanium, tantalum, titanium nitride, and tantalum nitride.
[0048] In another embodiment, the device layer further includes a device structure located in the dielectric layer, the device structure being electrically connected to the electrical interconnect structure; the device structure includes one or more of a transistor, a capacitor structure, a resistor structure, and an inductor structure.
[0049] In other embodiments, the device layer may also be only a dielectric layer.
[0050] In this embodiment, the first conductive structure 201 is a bit line structure. In other embodiments, the first conductive structure can also be a word line structure.
[0051] The first conductive structure 201 is used to connect the memory cells formed subsequently. In this embodiment, there are multiple first conductive structures 201 in the device layer, and the multiple first conductive structures 201 are parallel to the first direction and arranged along the second direction. The first direction and the second direction are parallel to the surface of the substrate 200, and the first direction is perpendicular to the second direction. In other embodiments, the angle between the second direction and the first direction is an acute angle.
[0052] The first conductive structure 201 is exposed on the surface of the device layer 200 , and the top surface of the first conductive structure 201 is higher, lower or flush with the surface of the device layer 200 .
[0053] The material of the first conductive structure 201 includes one or more of copper, tungsten, aluminum, silver, titanium, tantalum, titanium nitride, and tantalum nitride. In this embodiment, the material of the first conductive structure 201 includes tungsten.
[0054] In this embodiment, the surface of the first conductive structure 201 further has a first adhesion layer, which is used to enhance the bonding strength between the first conductive structure 201 and the subsequently formed composite storage layer, and improve the interface performance between the first conductive structure 201 and the composite storage layer. The material of the first adhesion layer includes tungsten silicon nitride (WSiN).
[0055] Please refer to Figure 5 , a composite storage layer 220 is formed on the substrate 200 , and the composite storage layer 220 is located on the first conductive structure 210 .
[0056] The composite memory layer 220 is subsequently used to form a memory cell located on the first conductive structure 201 ; in this embodiment, the memory cell formed subsequently is a memory cell of a phase change memory.
[0057] The composite storage layer 220 includes: a gating layer 222 located on the substrate 200 , a second electrode layer 223 located on the gating layer 222 , a phase change layer 224 located on the second electrode layer 223 , a third electrode layer 225 located on the phase change layer 224 , and a conductive layer 226 located on the third electrode layer 225 .
[0058] The phase change layer 224 is used to realize the data storage function based on the resistance difference in different phases. The material of the phase change layer 224 is a phase change material, and the phase change material includes a chalcogenide, and the chalcogenide includes a germanium antimony telluride compound (Ge-Sb-Te, referred to as GST). In this embodiment, the material of the phase change layer 224 is a germanium antimony telluride compound, and the germanium antimony telluride compound is in a high resistance state in an amorphous state, and the germanium antimony telluride compound is in a low resistance state in a crystalline state. The germanium antimony telluride compound can be switched between the crystalline state and the amorphous state under the drive of different electrical signals, thereby realizing data storage and erasure operations.
[0059] The gating layer 222 is used as a switch to control the current flowing through the phase change layer 224. The material of the gating layer 222 includes an Ovonic threshold switching (OTS) material, and the Ovonic threshold switching material includes a chalcogenide, and the chalcogenide includes GeSeAs, GeTeAs, GeSeTeSe, GeSe, SeAs, GeTe and SiTe. The Ovonic threshold switching material can realize the switching between a high resistance state and a low resistance state under the control of an electrical signal, thereby realizing the switching control of the current.
[0060] The material of the third electrode layer 225 includes amorphous carbon. In one embodiment, the amorphous carbon is further doped with modified particles, and the modified particles include one or more of nitrogen, boron and silicon, which are used to adjust the etching rate of the third electrode layer 225 .
[0061] In this embodiment, the conductive layer 226 is subsequently used to form a word line. In other embodiments, when the first conductive structure is a word line structure, the conductive layer 226 is subsequently used to form a bit line.
[0062] The material of the conductive layer 226 includes one or more of copper, tungsten, aluminum, silver, titanium, tantalum, titanium nitride, and tantalum nitride. In this embodiment, the material of the conductive layer 226 includes tungsten.
[0063] In this embodiment, the surface of the conductive layer 226 also has a second adhesion layer, which is used to enhance the bonding strength between the conductive layer 226 and the initial mask structure formed subsequently, and improve the interface performance between the first conductive structure 201 and the initial mask structure. The material of the first adhesion layer includes tungsten silicon nitride (WSiN).
[0064] Since the composite storage layer 220 is a multi-layer structure with a large number of layers and complex materials, when the composite storage layer 220 is subsequently etched to form a storage unit, it is necessary to precisely control the gas and process parameters of the etching process to meet the requirements of etching a variety of materials while being able to form a groove with a higher aspect ratio.
[0065] In this embodiment, the composite storage layer further includes: a first electrode layer 221, and the gating layer 222 is located on the first electrode layer 221; the composite storage layer further includes: a second electrode layer 223 located on the gating layer 222, and the phase change layer is located on the second electrode layer.
[0066] In some other embodiments, the composite storage layer may further include one of a first electrode layer and a second electrode layer. In other embodiments, the composite storage layer may also not include the first electrode layer and the second electrode layer.
[0067] The material of the first electrode layer 221 includes amorphous carbon. In one embodiment, the amorphous carbon is further doped with modified particles, and the modified particles include one or more of nitrogen, boron and silicon, which are used to adjust the etching rate of the first electrode layer 221 .
[0068] The material of the second electrode layer 223 includes amorphous carbon. In one embodiment, the amorphous carbon is further doped with modified particles, and the modified particles include one or more of nitrogen, boron and silicon, which are used to adjust the etching rate of the second electrode layer 223 .
[0069] Please refer to Figure 6 , a plurality of initial mask structures 230 are formed on the composite storage layer 220, wherein the initial mask structures 230 expose a portion of the composite storage layer 220, and the initial mask structures 230 include a first mask layer 231 and a second mask layer 232 located on the first mask layer 231, wherein the material of the second mask layer 232 is different from that of the first mask layer 231.
[0070] The initial mask structure 230 is used to etch the composite storage layer 220 to form a plurality of discrete storage units located on the first conductive structure. Since the composite storage layer 220 is a multi-layer structure, the multi-layer structure has a large number of layers, a large thickness, and complex materials. Therefore, the initial mask 230 structure needs to be able to maintain a stable morphology in the subsequent etching process to improve the uniformity of the characteristic storage of the formed storage unit, thereby ensuring the stable performance of the formed memory.
[0071] The initial mask structure 230 includes a second mask layer 232 located on the first mask layer 231, and the material of the second mask layer 232 is different from the material of the first mask layer 231. By adjusting the material relationship between the second mask layer 232 and the first mask layer 231, the etching selectivity between the second mask layer 232 and the first mask layer 231 in the subsequent first etching process can be adjusted, thereby improving the stability of the morphology and feature size of the second mask layer 232 in the subsequent first etching process and the second etching process.
[0072] Moreover, the initial mask structure 230 includes a double-layer structure, so that the initial mask structure 230 can not only serve as a mask for the subsequent first etching process and the second etching process, but also enable the first mask layer 231 to serve as a stop layer for subsequent planarization processes or etching processes, or as a protective layer to protect the top of the storage unit in subsequent processes.
[0073] The material of the first mask layer 231 includes one or a combination of silicon nitride and silicon oxynitride; the material of the second mask layer 232 includes silicon oxide. In this embodiment, the material of the first mask layer 231 is silicon nitride, and the material of the second mask layer 232 is silicon oxide.
[0074] Since the etching gas of the subsequent first etching process includes fluorine-containing gas and hydrogen-containing gas, and the etching rate of the fluorine-containing gas and the hydrogen-containing gas on silicon oxide is lower than the etching rate on silicon nitride, therefore, when the material of the second mask layer 232 is silicon oxide, it can be ensured that after the subsequent first etching process, the side wall and the top of the second mask layer 232 are not excessively consumed.
[0075] On the one hand, since the side walls of the second mask layer 232 are not transitionally lost, the second mask layer 232 has stable and uniform dimensions in a direction parallel to the surface of the substrate 200. Furthermore, the first mask layer 231 at the bottom of the second mask layer 232 has stable and uniform dimensions in a direction parallel to the surface of the substrate 200. Therefore, after the first etching process, the transition mask structure formed by the initial mask structure 230 can still be used as a mask for subsequent etching of the composite storage layer 220.
[0076] On the other hand, since the top of the second mask layer 232 is not transitionally consumed, the thickness of the second mask layer 232 in the direction perpendicular to the surface of the substrate 200 can be maintained stable and uniform, that is, after the first etching process, the thickness of the formed transition mask structure can still meet the requirements of subsequent etching of the composite storage layer 220, and there is no need to form an additional protective layer on the surface of the transition mask structure.
[0077] In some embodiments, the thickness of the second mask layer 232 is greater than the thickness of the first mask layer 231. Since the etching rate of the second mask layer 232 in the subsequent first etching process is slower than that of the first mask layer 231, when the thickness of the second mask layer 232 is thicker, the second mask layer 232 after the first etching process can retain a greater thickness, thereby ensuring that the formed transition mask structure is sufficient to directly serve as a mask for the subsequent etching of the composite storage layer 220, and there is no need to form an additional protective layer on the surface of the transition mask structure.
[0078] In this embodiment, the ratio of the thickness of the first mask layer 231 to the thickness of the second mask layer 232 is in the range of 1:4 to 1:5. Within the ratio range, the first mask layer 231 and the second mask layer 232 can be used as masks for the first etching process and the second etching process, while not excessively increasing the distance from the surface of the first conductive structure to the top of the initial mask structure 230, which is beneficial to reducing the depth-to-width ratio of the trenches between the storage units, reducing the difficulty of the etching process, reducing etching byproducts, and thus improving device performance. In some embodiments, the thickness of the first mask layer 231 ranges from 250 angstroms to 350 angstroms; the thickness of the second mask layer 232 ranges from 1400 angstroms to 1500 angstroms. In this embodiment, the thickness of the first mask layer 231 is 300 angstroms, and the thickness of the second mask layer 232 is 1450 angstroms.
[0079] The method for forming the initial mask structure 230 includes: forming a first mask material layer (not shown) on the composite storage layer 220; forming a second mask material layer (not shown) on the first mask material layer; and patterning the second mask material layer and the first mask material layer to form the first mask layer 231 and a second mask layer 232 located on the first mask layer 231.
[0080] The formation process of the first mask material layer includes a deposition process, which includes a chemical vapor deposition process, a physical vapor deposition process, or an atomic layer deposition process. The formation process of the second mask material layer includes a deposition process, which includes a chemical vapor deposition process, a physical vapor deposition process, or an atomic layer deposition process.
[0081] The patterning method includes: forming a plurality of mutually separate patterning layers on the surfaces of the second mask material layer and the first mask material layer; using the patterning layers as masks, etching the second mask material layer and the first mask material layer until the composite storage layer 220 is exposed. The patterning layer includes a patterned photoresist layer. The process of etching the second mask material layer and the first mask material layer includes an anisotropic dry etching process.
[0082] Please refer to Figure 7 , using the initial mask structure 230 as a mask, the composite storage layer 220 is etched by a first etching process to form a first trench 240 in the composite storage layer 220, and the first etching process is performed on the second mask layer 232 (such as Figure 6 The etching rate of the first mask layer 231 (as shown) is less than that of the first mask layer 231 (as shown Figure 6 The etching rate is shown in FIG.
[0083] The first etching process is used to etch the conductive layer 226, the third electrode layer 225 and the phase change layer 224. In this embodiment, the first trench 240 penetrates the conductive layer 226, the third electrode layer 225 and the phase change layer 224, and exposes the surface of the second electrode layer 223. In other embodiments, the bottom surface of the first trench can be lower or higher than the top surface of the second electrode.
[0084] The first etching process is an anisotropic dry etching process. In some embodiments, the first etching process is a plasma dry etching process.
[0085] The etching gas of the first etching process includes a hydrogen-containing gas and a fluorine-containing gas. Since the material of the second electrode layer 223 includes amorphous carbon, the material of the conductive layer 226 includes tungsten, and the material of the phase change layer 224 includes a chalcogenide, when the hydrogen-containing gas and the fluorine-containing gas are used as etching gases, a high etching rate can be achieved for the conductive layer 226, the third electrode layer 225, and the phase change layer 224 to meet the etching requirements.
[0086] After the composite storage layer 220 is etched by the first etching process, the initial mask structure 230 forms a transition mask structure 250; and the thickness of the transition mask structure 250 is less than the thickness of the initial mask structure.
[0087] In the first etching process, the etching rate of the second mask layer 232 is lower than the etching rate of the first mask layer 231. After the first etching process, the loss of the sidewall and the top of the second mask layer 232 is limited. On the one hand, the size of the second mask layer 232 in the direction parallel to the surface of the substrate 200 is stable and uniform, so the transition mask structure has a uniform characteristic size in the direction parallel to the surface of the substrate 200. On the other hand, since the top of the second mask layer 232 is not consumed by the transition, the thickness of the transition mask structure can still meet the requirements of the subsequent etching of the composite storage layer 220. Therefore, the transition mask structure can still serve as a mask for the subsequent etching of the composite storage layer 220.
[0088] In this embodiment, the material of the second mask layer 232 includes silicon oxide, and the material of the first mask layer 231 includes silicon nitride. In the first etching process, the ratio of the etching rate of the second mask layer 232 to the etching rate of the first mask layer 231 is in the range of 1:3 to 1:4.
[0089] When within the said ratio range, the etching amount of the second mask layer 232 in the direction parallel to the surface of the substrate 200 can be small, so that the said transition mask structure 250 has a uniform morphology and a stable characteristic size in the direction parallel to the surface of the substrate 200; at the same time, the thickness of the said initial mask structure 230 can be reduced, so that the distance from the top surface of the said transition mask structure 250 to the surface of the first conductive structure 201 is appropriate, which is beneficial to reduce the aspect ratio of the grooves between the subsequently formed storage units, thereby reducing the difficulty of the etching process, reducing the residual by-products of the etching process, and improving the performance of the formed storage unit.
[0090] When the ratio of the etching rate of the second mask layer 232 to the etching rate of the first mask layer 231 is less than 1:3, the first etching process tends to cause a large amount of lateral etching (parallel to the surface direction of the substrate 200) of the second mask layer 232, and it is difficult for the transition mask structure 250 to maintain a uniform morphology and stable feature size.
[0091] When the etching rate ratio of the second mask layer 232 to the first mask layer 231 is greater than 1:4, it is easy to make the distance from the top surface of the transition mask structure 250 to the first conductive surface larger, thereby increasing the aspect ratio of the groove between the storage cells and increasing the difficulty of the etching process.
[0092] The thickness of the transition mask structure 250 ranges from 10 nanometers to 20 nanometers. The distance from the top surface of the transition mask structure 250 to the surface of the first conductive structure 201 is appropriate, which is conducive to reducing the depth-to-width ratio of the grooves between the memory cells formed subsequently, thereby reducing the difficulty of the etching process. When the thickness of the transition mask structure 250 is less than 10 nanometers, it is difficult for the transition mask structure 250 to maintain a stable morphology in the subsequent second etching process, which is likely to cause the morphology of the memory cells formed subsequently to deteriorate. When the thickness of the transition mask structure 250 is greater than 20 nanometers, it is easy to make the distance from the top surface of the transition mask structure 250 to the first conductive surface larger, thereby increasing the depth-to-width ratio of the grooves between the memory cells and increasing the difficulty of the etching process. In this embodiment, the thickness of the transition mask structure 250 is 15 nanometers.
[0093] Please refer to Figure 8After the first etching process, the composite storage layer 220 (eg, Figure 7 As shown in FIG. 2 , a plurality of separate memory cell structures 260 are formed on the substrate 200 .
[0094] The second etching process is used to etch the second electrode layer 223 , the gating layer 222 and the first electrode layer 221 until the first conductive structure 201 is exposed.
[0095] The second etching process is an anisotropic dry etching process. In some embodiments, the second etching process is a plasma dry etching process. The process parameters of the second etching process are the same as or different from those of the first etching process, and the process gas of the second etching process is the same as or different from that of the first etching process. In one embodiment, the etching gas of the second etching process includes a hydrogen-containing gas and a fluorine-containing gas.
[0096] Since the thickness of the transition mask structure 250 is in the range of 10 nanometers to 20 nanometers, on the one hand, the thickness of the transition mask structure 250 is sufficient to meet the requirements of being a mask in the second etching process; on the other hand, the thickness of the transition mask structure 250 is not too thick, so that the depth-width ratio of the trenches between the storage units is small, reducing the difficulty of the second etching process.
[0097] In some embodiments, after forming the memory cell structure 260, an interlayer dielectric layer is formed on the substrate 200 and on the surface of the memory cell 260; the interlayer dielectric layer is planarized until the top of the memory cell 260 is exposed, and the planarization process obtains a stop position according to the first mask layer 231; the planarization process includes a chemical mechanical polishing process or an etching back process.
[0098] In summary, by making the material of the formed second mask layer different from the material of the first mask layer, and making the thickness of the second mask layer greater than the thickness of the first mask layer, the etching rate of the second mask layer in the first etching process is smaller than the etching rate of the first mask layer, so that in the direction parallel to the substrate surface, the etching amount of the second mask layer in the first etching process is smaller than the etching amount of the first mask layer. Therefore, in the first etching process, the mask structure can maintain a relatively uniform size in the direction parallel to the substrate surface, and then when the storage unit is subsequently formed by the initial composite storage layer, the storage unit has a relatively uniform size and spacing in the direction parallel to the substrate surface. The formed storage unit has a relatively uniform size and spacing in the direction parallel to the substrate surface, so the electrical properties of the formed storage units are uniform and stable, and the uniformity of the leakage current density is improved.
[0099] Accordingly, the present application also provides a method for forming a storage system, including: Figures 4 to 8 The related method forms a phase change memory; a logic device is formed on the substrate 200, and the logic device is coupled to the phase change memory.
[0100] In summary, since the formed storage cells have relatively uniform size and spacing in the direction parallel to the substrate surface, the electrical properties of the formed storage cells are uniform and stable, and the uniformity of the leakage current density is improved, so the performance and yield of the formed storage system are improved.
[0101] Figures 9 to 11 FIG. 1 is a cross-sectional structural diagram of another phase change memory forming process of an embodiment of the present application. Figures 4 to 8 The difference between the related embodiments is that before forming the second mask material layer, the first mask material layer is hardened to increase the density of the first mask material layer.
[0102] exist Figure 5 Please continue to refer to Fig. 9 , a first mask material layer 301 is formed on the composite storage layer 220 .
[0103] The material of the first mask material layer 301 includes one or a combination of silicon nitride and silicon oxynitride. In this embodiment, the material of the first mask material layer 301 is silicon nitride.
[0104] The formation process of the first mask material layer 301 includes a deposition process, and the deposition process includes a chemical vapor deposition process, a physical vapor deposition process or an atomic layer deposition process.
[0105] Please refer to Fig.10 , performing a hardening treatment 320 on the first mask material layer 301 to increase the density of the first mask material layer 301 .
[0106] On the one hand, the increased density of the first mask material layer 301 is beneficial to reducing the etching amount of the first mask layer in a direction parallel to the substrate surface in the subsequent first etching process, thereby further improving the morphology stability of the initial mask structure in the first etching process.
[0107] On the other hand, after the memory cell is subsequently formed, the first mask layer can be retained as a protective layer for subsequent processes, thereby avoiding the step of additionally forming a protective layer, which is beneficial to saving costs and improving process efficiency.
[0108] In some embodiments, the hardening treatment 320 includes a plasma treatment process; the gas of the plasma treatment process includes an inert gas; the inert gas includes one or a mixture of helium and argon. Using the inert gas for plasma treatment, on the one hand, it is difficult to cause changes in the first mask material layer 301 and the composite storage layer 220, and on the other hand, the first mask material layer 301 can be densified through the mechanism of physical bombardment.
[0109] Please refer to Fig.11 After the hardening treatment, the first mask material layer 300 (such as Fig.10 A second mask material layer (not shown) is formed on the first mask material layer 301; the second mask material layer and the first mask material layer 301 are patterned to form an initial mask structure 310, wherein the initial mask structure 310 includes a first mask layer 311 and a second mask layer 312 located on the first mask layer 311.
[0110] The material of the second mask material layer includes silicon oxide. In this embodiment, the material of the first mask material layer 301 is silicon oxide.
[0111] The thickness of the second mask material layer is greater than the thickness of the first mask material layer 300. In this embodiment, the ratio of the thickness of the first mask material layer 300 to the thickness of the second mask material layer is in a range of 1:4 to 1:5.
[0112] The formation process of the second mask material layer includes a deposition process, and the deposition process includes a chemical vapor deposition process, a physical vapor deposition process or an atomic layer deposition process.
[0113] The patterning method includes: forming a plurality of mutually separate patterning layers on the surface of the second mask material layer and the first mask material layer 300; using the patterning layers as masks, etching the second mask material layer and the first mask material layer 300 until the composite storage layer 220 is exposed. The patterning layer includes a patterned photoresist layer. The process of etching the second mask material layer and the first mask material layer 300 includes an anisotropic dry etching process.
[0114] The initial mask structure 310 includes a double-layer structure, so that the initial mask structure 310 can serve as a mask for the subsequent first etching process and the second etching process, and can also make the first mask layer 311 serve as a stop layer for subsequent planarization process or etching process, or as a protective layer for protecting the top of the storage unit in subsequent processes.
[0115] In this embodiment, the material of the first mask layer 311 is hardened, so that the first mask layer 311 has stronger protection capability when used as a stop layer in subsequent planarization process or etching process after the memory unit is subsequently formed.
[0116] Please continue to refer to Fig.11 , using the initial mask structure 310 as a mask, the composite storage layer 220 is etched by a first etching process to form a first groove 320 in the composite storage layer 220, and the initial mask structure 310 forms a transition mask structure 330, and the etching rate of the second mask layer 312 by the first etching process is lower than the etching rate of the first mask layer 311; after the first etching process, using the transition mask structure 330 as a mask, the composite storage layer 220 at the bottom of the first groove 320 is etched by a second etching process to form a plurality of discrete storage unit structures on the substrate 200.
[0117] The first etching process, the second etching process, and the structure, material, size, etc. of the storage unit are the same as those in the above-mentioned embodiment and are not described in detail here.
[0118] Accordingly, the present application also provides a method for forming a storage system, including: Figures 9 to 11 The related method forms a phase change memory; a logic device is formed on the substrate 200, and the logic device is coupled to the phase change memory.
[0119] In summary, by hardening the first mask material layer before forming the second mask material layer, the density of the first mask material layer is increased. On the one hand, the increase in the density of the first mask layer is beneficial to reducing the etching amount of the first mask layer in the direction parallel to the substrate surface in the first etching process, thereby further improving the morphological stability of the initial mask structure in the first etching process. On the other hand, in the subsequent process, the first mask layer can also be retained as a protective layer, avoiding the step of additionally forming a protective layer, which is beneficial to saving costs and improving process efficiency.
[0120] The description of the above embodiments is only used to help understand the technical solutions and core ideas of the present application. Ordinary technical personnel in this field should understand that they can still modify the technical solutions recorded in the aforementioned embodiments, or replace some of the technical features therein with equivalents. However, these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the embodiments of the present application.
Claims
1. A method for forming a phase change memory, characterized in that: include: providing a substrate; forming a composite storage layer on the substrate; forming a plurality of initial mask structures on the composite storage layer, wherein the initial mask structures expose a portion of the composite storage layer, the initial mask structures comprising a first mask layer and a second mask layer located on the first mask layer, wherein a material of the second mask layer is different from a material of the first mask layer; The composite storage layer is etched by a first etching process using the initial mask structure as a mask to form a first trench in the composite storage layer. The etching rate of the first etching process on the second mask layer is lower than the etching rate on the first mask layer.
2. The method for forming a phase change memory according to claim 1, characterized in that: In the first etching process, a ratio of an etching rate of the second mask layer to an etching rate of the first mask layer is in a range of 1:3 to 1:
4.
3. The method for forming a phase change memory according to claim 2, characterized in that: The etching gas of the first etching process includes hydrogen-containing gas and fluorine-containing gas; the material of the first mask layer includes silicon nitride; and the material of the second mask layer includes silicon oxide.
4. The method for forming a phase change memory according to claim 1, characterized in that: The composite storage layer includes: a gating layer located on a substrate, a phase change layer located on the gating layer, a third electrode layer located on the phase change layer, and a conductive layer located on the third electrode layer; the first groove penetrates the conductive layer, the third electrode layer and the phase change layer.
5. The method for forming a phase change memory according to claim 1, characterized in that: The thickness of the second mask layer is greater than the thickness of the first mask layer.
6. The method for forming a phase change memory according to claim 5, characterized in that: The ratio of the thickness of the first mask layer to the thickness of the second mask layer is in a range of 1:4 to 1:
5.
7. The method for forming a phase change memory according to claim 1, characterized in that: The method for forming the initial mask structure includes: forming a first mask material layer on the composite storage layer; hardening the first mask material layer to increase the density of the first mask material layer; forming a second mask material layer on the first mask material layer; and patterning the second mask material layer and the first mask material layer to form the first mask layer and a second mask layer located on the first mask layer.
8. The method for forming a phase change memory according to claim 7, characterized in that: The hardening treatment includes a plasma treatment process, and a gas of the plasma treatment process includes an inert gas.
9. The method for forming a phase change memory according to claim 8, characterized in that: Also includes: After the first etching process, the initial mask structure forms a transition mask structure; The composite storage layer at the bottom of the first trench is etched using the transition mask structure as a mask by a second etching process to form a plurality of discrete storage unit structures on the substrate.
10. The method for forming a phase change memory according to claim 9, characterized in that: Also includes: After the second etching, an interlayer dielectric layer is formed on the substrate and on the surface of the storage unit; The interlayer dielectric layer is planarized until the top of the storage unit is exposed, and the planarization process obtains a stop position according to the first mask layer; the planarization process includes a chemical mechanical polishing process or an etch-back process.