Semiconductor structure and forming method thereof

By introducing a second isolation layer into the semiconductor structure and embedded in the middle fin, the source-drain doped layer is insulated from the bottom fin, which solves the problem of reduced leakage current and control capability after the size of the semiconductor device is reduced, and significantly improves performance.

CN118738083APending Publication Date: 2024-10-01SEMICON MFG INT (SHANGHAI) CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310318405.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-28
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The shrinking size of semiconductor devices leads to an increase in leakage current, making it difficult to control the channel and affecting performance.

Method used

Design a semiconductor structure, including a base, a channel protrusion structure, a first isolation layer, a gate structure, a source-drain doping layer and a second isolation layer. The second isolation layer is embedded in the middle fin, and the top and middle fins are The source and drain doped layers are flush with each other, and the source and drain doped layers are isolated from the bottom fin through the second isolation layer to improve the insulation effect.

Benefits of technology

The leakage current is effectively suppressed, the gate's ability to control the channel is enhanced, the short channel effect is reduced, and the performance of the semiconductor structure is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738083A_ABST
    Figure CN118738083A_ABST
Patent Text Reader

Abstract

The invention discloses a semiconductor structure and a forming method thereof, the semiconductor structure comprises a substrate, the substrate comprises a substrate and a channel protrusion structure protruding from the substrate, and the channel protrusion structure comprises a bottom fin part, a top fin part located above the bottom fin part and a middle fin part located between the bottom fin part and the top fin part in the normal direction of the top surface of the substrate; the first isolation layer is located on the substrate at the side part of the channel bulge structure, and the first isolation layer covers the side wall of the bottom fin part and the side wall of the middle fin part; the gate structure is located on the first isolation layer, crosses the channel bulge structure and covers part of the top and the side wall of the top fin part; the source-drain doping layer is located in the top fin parts on the two sides of the gate structure; the second isolation layer is located below the source-drain doping layer and embedded in the middle fin part, the top of the second isolation layer is flush with the top of the middle fin part, and the source-drain doping layer is isolated from the bottom fin part through the second isolation layer. According to the embodiment of the invention, the control capability of the gate to the channel is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present invention relate to the field of semiconductor manufacturing, and in particular to a semiconductor structure and a method for forming the same. Background Art

[0002] With the rapid development of the semiconductor integrated circuit (IC) industry, semiconductor technology continues to move towards smaller process nodes driven by Moore's Law, making integrated circuits develop in the direction of smaller size, higher circuit precision and higher circuit complexity.

[0003] In order to better adapt to the requirement of scaling down device size, semiconductor processes have gradually begun to transition from planar transistors to three-dimensional transistors with higher efficiency, such as fin field-effect transistors (FinFET) and gate-all-around (GAA) transistors, but this has also correspondingly increased the difficulty and complexity of integrated circuit manufacturing.

[0004] Therefore, the performance of semiconductor structures still needs to be improved. Summary of the invention

[0005] The problem solved by the embodiments of the present invention is to provide a semiconductor structure and a method for forming the same, so as to improve the performance of the semiconductor structure.

[0006] To solve the above problems, the present invention provides a semiconductor structure, including: a substrate, the substrate including a substrate and a channel protrusion structure protruding from the substrate, along the normal direction of the top surface of the substrate, the channel protrusion structure including a bottom fin, a top fin located above the bottom fin, and an intermediate fin located between the bottom fin and the top fin; a first isolation layer, located on the substrate at the side of the channel protrusion structure, the first isolation layer covers the sidewalls of the bottom fin and the sidewalls of the intermediate fin; a gate structure, located on the first isolation layer, the gate structure spans the channel protrusion structure and covers part of the top and sidewalls of the top fin; a source-drain doped layer, located in the top fin on both sides of the gate structure; a second isolation layer, located below the source-drain doped layer and embedded in the intermediate fin, the top of the second isolation layer is flush with the top of the intermediate fin, and the source-drain doped layer is isolated from the bottom fin by the second isolation layer.

[0007] Optionally, the semiconductor structure further includes: a gap located between the source-drain doped layer and the second isolation layer.

[0008] Optionally, the material of the second isolation layer includes oxide or nitride.

[0009] Optionally, the material of the middle fin includes silicon germanium.

[0010] Optionally, the material of the second isolation layer includes silicon oxide or silicon nitride; the semiconductor structure further includes: a reaction-generated layer, located at the bottom of the second isolation layer and in contact with the bottom of the second isolation layer, and the material of the reaction-generated layer is germanium.

[0011] Optionally, the molar concentration of germanium in the middle fin is greater than 20% and less than 50%.

[0012] Optionally, along a normal direction of the top surface of the substrate, a thickness of the middle fin ranges from 2 nanometers to 50 nanometers.

[0013] Correspondingly, an embodiment of the present invention also provides a method for forming a semiconductor structure, comprising: providing a substrate, the substrate comprising a substrate and a channel protrusion protruding from the substrate, wherein along the normal direction of the top surface of the substrate, the channel protrusion comprises a bottom fin, a top fin located above the bottom fin, and an intermediate fin located between the bottom fin and the top fin; forming a first isolation layer on the substrate on the side of the channel protrusion, the first isolation layer covering the sidewalls of the bottom fin and the sidewalls of the intermediate fin; forming a second isolation layer located in the intermediate fin in a preset area of ​​the intermediate fin along a direction parallel to the top surface of the substrate, the top of the second isolation layer is flush with the top of the intermediate fin, and a source-drain doped layer is formed above the preset area; forming a gate structure spanning the top fin on the first isolation layer, the gate structure covering a portion of the top and sidewalls of the top fin; forming source-drain doped layers in the top fins on both sides of the gate structure, the source-drain doped layers are isolated from the bottom fin by the second isolation layer.

[0014] Optionally, in a preset area of ​​the middle fin along a direction parallel to the top surface of the substrate, the step of forming a second isolation layer in the middle fin includes: performing a heat treatment process on the middle fin in the preset area under an oxygen-containing atmosphere or a nitrogen-containing atmosphere to convert the middle fin in the preset area into a second isolation layer.

[0015] Optionally, the parameters of the heat treatment process include: the gas in the oxygen-containing atmosphere includes one or more of oxygen and ozone, the gas in the nitrogen-containing atmosphere includes nitrogen, and the process temperature is less than or equal to 350°C.

[0016] Optionally, before performing a heat treatment process on the middle fin of the preset area in an oxygen-containing atmosphere or a nitrogen-containing atmosphere, the step of forming a second isolation layer located in the middle fin in a preset area of ​​the middle fin along a direction parallel to the top surface of the substrate also includes: performing an ion implantation process on the middle fin of the preset area, the implanted ions of the ion implantation process including oxygen ions or nitrogen ions.

[0017] Optionally, the parameters of the ion implantation process include: an implantation dose of 1E13 atoms / cm 2~9E17atoms / cm 2 The implantation energy is 3KeV~8KeV, and the process temperature is less than or equal to 350℃.

[0018] Optionally, after forming a gate structure spanning the top fin on the first isolation layer, and before forming source-drain doped layers in the top fins on both sides of the gate structure, it also includes: forming source-drain grooves in the top fins on both sides of the gate structure, the source-drain grooves exposing the top of the middle fin; in the area of ​​the middle fin along a direction parallel to the top surface of the substrate, the step of forming a second isolation layer located in the middle fin includes: forming a second isolation layer in the middle fin via the source-drain grooves, the second isolation layer being located at the bottom of the source-drain grooves; the step of forming source-drain doped layers in the top fins on both sides of the gate structure includes: after forming the second isolation layer, forming source-drain doped layers in the source-drain grooves.

[0019] Optionally, after forming the source and drain grooves and before forming the second isolation layer, it also includes: forming a protective layer covering the side walls and top of the gate structure and the side walls of the source and drain grooves; after forming the second isolation layer, it also includes: removing the protective layer; after removing the protective layer, forming a source and drain doping layer in the source and drain grooves.

[0020] Optionally, the step of forming a protective layer covering the side walls and top of the gate structure and the side walls of the source and drain grooves includes: forming a protective material layer covering the side walls and top of the gate structure and the side walls and bottom of the source and drain grooves; removing the protective material layer covering the bottom of the source and drain grooves, and the remaining protective material layer covering the side walls and top of the gate structure and the side walls of the source and drain grooves serves as a protective layer.

[0021] Optionally, the material of the protective layer includes a carbon-silicon based material.

[0022] Optionally, in the step of forming a second isolation layer located in the middle fin in a preset region of the middle fin along a direction parallel to the top surface of the substrate, a material of the second isolation layer includes oxide or nitride.

[0023] Optionally, the material of the middle fin includes silicon germanium.

[0024] Optionally, the molar concentration of germanium in the middle fin is greater than 20% and less than 50%.

[0025] Compared with the prior art, the technical solution of the embodiment of the present invention has the following advantages:

[0026] The semiconductor structure provided in this embodiment includes a second isolation layer located between the source-drain doped layer and the bottom fin. The top of the second isolation layer is flush with the top of the middle fin. Therefore, the source-drain doped layer is isolated from the bottom fin by the second isolation layer, which improves the insulation effect between the source-drain doped layer and the bottom fin. Correspondingly, it is less likely for leakage current to form under the source-drain doped layer, thereby improving the gate's control ability over the channel, suppressing the short channel effect, and further improving the performance of the semiconductor structure.

[0027] In an optional solution, there is a gap between the source-drain doped layer and the second isolation layer, so that the insulation effect between the source-drain doped layer and the bottom fin is better, and correspondingly, the effect of preventing leakage current from being formed under the source-drain doped layer is better, which can further improve the gate's control ability over the channel, suppress the short channel effect, and further improve the performance of the semiconductor structure.

[0028] In the method for forming a semiconductor structure provided by an embodiment of the present invention, a channel protrusion includes an intermediate fin located between a bottom fin and a top fin, and a second isolation layer is formed in the intermediate fin in a preset area. The top of the second isolation layer is flush with the top of the intermediate fin, and the area above the preset area is used to form a source-drain doping layer. Therefore, after the source-drain doping layer is formed, the source-drain doping layer is isolated from the bottom fin by the second isolation layer, which improves the insulation effect between the source-drain doping layer and the bottom fin, and correspondingly makes it difficult for leakage current to form below the source-drain doping layer, thereby improving the gate's control ability over the channel, suppressing the short channel effect, and further improving the performance of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 It is a structural schematic diagram of a semiconductor structure of the present invention;

[0030] Figures 2 to 8 It is a schematic structural diagram corresponding to each step in an embodiment of a method for forming a semiconductor structure of the present invention. DETAILED DESCRIPTION

[0031] As can be seen from the background art, as the size of semiconductor devices is gradually reduced, especially as the size of three-dimensional transistors is gradually reduced, how to reduce the leakage current of the device has become a problem that needs to be solved urgently.

[0032] In order to solve the above technical problems, an embodiment of the present invention provides a semiconductor structure, including: a substrate, the substrate including a substrate, and a channel protrusion structure protruding from the substrate, along the normal direction of the top surface of the substrate, the channel protrusion structure including a bottom fin, a top fin located above the bottom fin, and an intermediate fin located between the bottom fin and the top fin; a first isolation layer, located on the substrate on the side of the channel protrusion structure, the first isolation layer covers the sidewalls of the bottom fin and the sidewalls of the intermediate fin; a gate structure, located on the first isolation layer, the gate structure spans the channel protrusion structure and covers part of the top and sidewalls of the top fin; a source-drain doped layer, located in the top fin on both sides of the gate structure; a second isolation layer, located below the source-drain doped layer and embedded in the intermediate fin, the top of the second isolation layer is flush with the top of the intermediate fin, and the source-drain doped layer is isolated from the bottom fin by the second isolation layer.

[0033] The semiconductor structure provided by the embodiment of the present invention includes a second isolation layer located between the source-drain doped layer and the bottom fin. The top of the second isolation layer is flush with the top of the middle fin. Therefore, the source-drain doped layer is isolated from the bottom fin by the second isolation layer, which improves the insulation effect between the source-drain doped layer and the bottom fin. Correspondingly, it is less likely for leakage current to form under the source-drain doped layer, thereby improving the gate's control ability over the channel, suppressing the short channel effect, and further improving the performance of the semiconductor structure.

[0034] In order to make the above-mentioned purposes, features and advantages of the embodiments of the present invention more obvious and understandable, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0035] Figure 1 It is a schematic structural diagram of an embodiment of a semiconductor structure of the present invention.

[0036] refer to Figure 1In this embodiment, the semiconductor structure includes: a substrate (not shown), the substrate includes a substrate 100, and a channel protrusion structure 110 protruding from the substrate 100, along the normal direction of the top surface of the substrate 100, the channel protrusion structure 110 includes a bottom fin 111, a top fin 113 located above the bottom fin 111, and an intermediate fin 112 located between the bottom fin 111 and the top fin 113; a first isolation layer 120, located on the substrate 100 at the side of the channel protrusion structure 110, the first isolation layer 120 covers the sidewalls and The side wall of the middle fin 112; the gate structure 130, which is located on the first isolation layer 120, the gate structure 130 spans the channel protrusion structure 110 and covers part of the top and side wall of the top fin 113; the source-drain doped layer 141, which is located in the top fin 113 on both sides of the gate structure 130; the second isolation layer 115, which is located below the source-drain doped layer 141 and embedded in the middle fin 112, the top of the second isolation layer 115 is flush with the top of the middle fin 112, and the source-drain doped layer 141 is isolated from the bottom fin 111 by the second isolation layer 115.

[0037] The substrate is used to provide a process platform for the formation process of the semiconductor structure.

[0038] In this embodiment, the substrate is used to form a field effect transistor. As an example, the substrate is used to form a fin field effect transistor.

[0039] In this embodiment, the base includes a substrate 100, and the substrate 100 is a silicon substrate. In other embodiments, the material of the substrate may also be other materials such as germanium, silicon germanium, silicon carbide, gallium arsenide or indium gallium, and the substrate may also be other types of substrates such as a silicon substrate on an insulator or a germanium substrate on an insulator.

[0040] The channel protrusion structure 110 is protruded from the substrate 100 , so that the gate structure 130 can cross the channel protrusion structure 110 and cover a portion of the top and sidewall of the top fin 113 .

[0041] The channel protrusion structure 110 includes a bottom fin 111 , a top fin 113 located above the bottom fin 111 , and a middle fin 112 located between the bottom fin 111 and the top fin 113 .

[0042] As an example, the bottom fin 111 and the substrate 100 are an integral structure.

[0043] The middle fin 112 provides a process platform for forming the second isolation layer 115 , and the top fin 113 in the channel protrusion structure 110 is used to provide a conductive channel of the field effect transistor.

[0044] The material of the top fin 113 includes one or more of silicon, germanium, silicon germanium, silicon carbide, gallium nitride, gallium arsenide and indium gallium. In this embodiment, the material of the top fin 113 is silicon.

[0045] Along the normal direction of the top surface of the substrate 100, the thickness of the middle fin 112 should not be too large or too small. If the thickness of the middle fin 112 is too large, it is easy to cause lattice dislocation in the top fin 113 located above the middle fin 112, so that there are defect energy levels in the top fin 113, which correspondingly reduces the carrier concentration when the semiconductor device is working, thereby affecting the performance of the semiconductor device. If the thickness of the middle fin 112 is too small, it is easy to make the thickness of the second isolation layer 115 formed in the middle fin 112 correspondingly small, so that the source-drain doping layer 141 is isolated from the bottom fin 111 by the second isolation layer 115. The effect is also poor. Therefore, in this embodiment, along the normal direction of the top surface of the substrate 100, the thickness of the middle fin 112 ranges from 2 nanometers to 50 nanometers.

[0046] The middle fin 112 is used to define the formation position of the second isolation layer 115. The second isolation layer 115 is embedded in the middle fin 112, so the formation position of the second isolation layer 115 is easily controlled through the middle fin 112.

[0047] In this embodiment, after forming the material layer corresponding to the middle fin 112, a heat treatment process is performed on the material layer of the middle fin 112 in the preset area in an oxygen-containing atmosphere to oxidize the middle fin 112 in the preset area into the second isolation layer 115. In other words, the second isolation layer 115 is obtained after the middle fin 112 in the preset area is oxidized.

[0048] In other embodiments, after forming the material layer corresponding to the middle fin, the material layer of the middle fin in the preset area may be subjected to a heat treatment process in a nitrogen-containing atmosphere to convert the middle fin in the preset area into a second isolation layer. In other words, the second isolation layer is obtained after the middle fin in the preset area is nitrided.

[0049] As an example, the materials of the middle fin 112 and the bottom fin 111 are different, so that the middle fin 112 can be specifically processed and the second isolation layer 115 can be accurately formed in the middle fin.

[0050] In this embodiment, the material of the middle fin 112 includes silicon germanium.

[0051] By selecting silicon germanium, it is easy to epitaxially grow a material layer corresponding to the top fin 113 on the top of the middle fin 112. Moreover, silicon germanium is easy to oxidize, which is conducive to forming the second isolation layer 115 in the middle fin 112.

[0052] It should be noted that the molar concentration of germanium in the middle fin 112 should not be too large or too small. If the molar concentration of germanium in the middle fin 112 is too large, the thickness of the second isolation layer formed in the middle fin 112 will be difficult to meet the target thickness requirement; if the molar concentration of germanium in the middle fin 112 is too small, it will be difficult to oxidize silicon germanium, thereby making it more difficult to form the second isolation layer 115 in the middle fin 112. Therefore, in this embodiment, the molar concentration of germanium in the middle fin 112 is greater than 20% and less than 50%.

[0053] In this embodiment, along the normal direction of the top surface of the substrate 100, the thickness range of the top fin 113 is

[0054] The first isolation layer 120 is used to isolate each semiconductor device to prevent leakage current from occurring between the devices.

[0055] In this embodiment, the first isolation layer 120 is a shallow trench isolation (STI) structure.

[0056] The material of the first isolation layer 120 includes one or more of silicon oxide, silicon nitride and silicon oxynitride.

[0057] The first isolation layer 120 covers the side walls of the bottom fin 111 and the side walls of the middle fin 112, that is, the first isolation layer 120 exposes the top fin 113, so that the top fin 113 is used as an effective fin (Active Fin), while the middle fin 112 is not used as an effective fin. The effective fin covered by the gate structure 130 is used to provide a conductive channel when the device is working.

[0058] The second isolation layer 115 is located between the source-drain doped layer 141 and the bottom fin 111, and the top of the second isolation layer 115 is flush with the top of the middle fin 112. Therefore, the source-drain doped layer 141 is isolated from the bottom fin 111 by the second isolation layer 115, which improves the insulation effect between the source-drain doped layer 141 and the bottom fin 111, and accordingly makes it difficult for leakage current to form under the source-drain doped layer 141, thereby improving the control ability of the gate structure 130 over the channel, suppressing the short channel effect, and further improving the performance of the semiconductor structure.

[0059] In addition, compared with the solution of achieving insulation between the source-drain doped layer and the bottom fin by ion implantation into the channel protrusion structure below the source-drain doped layer to form a PN junction below the source-drain doped layer, the present embodiment achieves insulation between the source-drain doped layer 141 and the bottom fin 111 through the second isolation layer 115. There is no need to balance the PN junction leakage current in the substrate and the leakage current between the source-drain doped layer and the bottom fin. In other words, the limitation of the PN junction leakage current on the insulation effect can be avoided. Moreover, in the present embodiment, the insulation effect of the second isolation layer 115 obtained by oxidizing the middle fin 112 in a preset area is more significant than the insulation effect achieved by forming a PN junction below the source-drain doped layer.

[0060] Compared with the solution of forming the second isolation layer in the bottom fin, the second isolation layer 115 is embedded in the middle fin 112, which makes it easy to control the formation position of the second isolation layer 115 through the middle fin 112 and reduces the process complexity and difficulty.

[0061] The top of the second isolation layer 115 is flush with the top of the middle fin 112 , which reduces the longitudinal distance between the source-drain doped layer 141 and the second isolation layer 115 , thereby enhancing the suppression effect of the second isolation layer 115 on the leakage current below the source-drain doped layer 141 .

[0062] Moreover, after the middle fin 112 is formed, the second isolation layer 115 passes through the middle fin 112 to be formed in the middle fin 112 , thereby reducing the influence on the formation process of the material layer corresponding to the top fin 113 .

[0063] It should be noted that the second isolation layer 115 is embedded in the middle fin 112 , and the second isolation layer 115 may be located in a portion of the thickness of the middle fin 112 below the source / drain doped layer 141 , or may penetrate the middle fin 112 below the source / drain doped layer 141 .

[0064] In this embodiment, after forming the material layer corresponding to the middle fin 112, a heat treatment process is performed on the material layer of the middle fin 112 in a predetermined area in an oxygen-containing atmosphere to oxidize the middle fin 112 in the predetermined area into the second isolation layer 115. Therefore, in this embodiment, the material of the second isolation layer 115 includes oxide, that is, the second isolation layer 115 is formed by oxidizing the middle fin 112. Since in the present embodiment, the material of the middle fin 112 includes silicon germanium, that is, the silicon germanium in the preset area is subjected to a heat treatment process in an oxygen-containing atmosphere, so that the silicon germanium in the preset area is oxidized into a second isolation layer 115 whose material is silicon oxide, and the oxidation reaction of silicon germanium also generates volatile germanium. However, if germanium is generated at the bottom of the second isolation layer 115, since there are other film layers below the bottom of the second isolation layer 115, it is easy to affect the volatilization of germanium, so that a reaction generation layer (not marked) whose material is germanium is formed at the bottom of the second isolation layer 115. Therefore, in the present embodiment, the material of the second isolation layer 115 includes silicon oxide; the semiconductor structure also includes: a reaction generation layer (not marked), which is located at the bottom of the second isolation layer 115 and contacts with the bottom of the second isolation layer 115, and the material of the reaction generation layer is germanium.

[0065] Based on the above similar principles, in other embodiments, after forming the material layer corresponding to the middle fin, the material layer of the middle fin in the preset area is subjected to a heat treatment process in a nitrogen-containing atmosphere to convert the middle fin 112 in the preset area into a second isolation layer. Therefore, in other embodiments, the material of the second isolation layer may also include nitride. Correspondingly, in other embodiments, the material of the second isolation layer may also include silicon nitride.

[0066] The top fin 113 is used as an active fin. The active fin covered by the gate structure 130 is used to provide a conductive channel when the device is working.

[0067] In this embodiment, the gate structure 130 is a device gate structure, which is used to form a field effect transistor with the channel protrusion structure 110 and the source-drain doped layer 141 .

[0068] The gate structure 130 includes a gate dielectric layer (not shown) and a gate electrode layer (not shown) covering the gate dielectric layer.

[0069] The gate dielectric layer is used to isolate the gate electrode layer from the channel protrusion structure 110 .

[0070] The material of the gate dielectric layer includes one or more of HfO2, ZrO2, HfSiO, HfSiON, HfTaO, HfTiO, HfZrO, Al2O3, SiO2 and La2O3.

[0071] In this embodiment, the gate structure 130 is a metal gate structure, and therefore, the material of the gate electrode layer includes one or more of TiN, TaN, Ta, Ti, TiAl, W, Al, TiSiN and TiAlC. The gate electrode layer includes a work function layer and an electrode layer covering the work function layer, or may include only the work function layer.

[0072] Correspondingly, the gate dielectric layer includes a high-k gate dielectric layer. The material of the high-k gate dielectric layer is a high-k dielectric material, and the high-k dielectric material refers to a dielectric material having a relative dielectric constant greater than the relative dielectric constant of silicon oxide. Specifically, the material of the high-k gate dielectric layer can be selected from HfO2, ZrO2, HfSiO, HfSiON, HfTaO, HfTiO, HfZrO or Al2O3. As an example, the material of the high-k gate dielectric layer is HfO2.

[0073] In other embodiments, the gate structure may also be a polysilicon gate structure.

[0074] In this embodiment, the semiconductor structure further includes: a spacer structure (not shown) located on the sidewall of the gate structure 130 .

[0075] The sidewall spacer is used to protect the sidewall of the device gate structure. The sidewall spacer can be a single-layer structure or a stacked structure, and the material of the sidewall spacer includes one or more of silicon oxide, silicon nitride, silicon carbide, silicon carbonitride, silicon carbonitride oxide, silicon oxynitride, boron nitride and boron carbonitride.

[0076] The source-drain doped layer 141 is used as the source region and the drain region of the transistor. When the device is working, the source-drain doped layer 141 is used to provide a carrier source.

[0077] The source-drain doped layer 141 is isolated from the bottom fin 111 by the second isolation layer 115, which improves the insulation effect between the source-drain doped layer 141 and the bottom fin 111, and accordingly makes it difficult for leakage current to form under the source-drain doped layer 141, thereby improving the gate's control ability over the channel, suppressing the short channel effect, and further improving the performance of the semiconductor structure.

[0078] In this embodiment, the semiconductor structure further includes a gap 142 located between the source-drain doped layer 141 and the second isolation layer 115 .

[0079] There is a gap 142 between the source-drain doped layer 141 and the second isolation layer 115, so that the insulation effect between the source-drain doped layer 141 and the bottom fin 111 is better, and correspondingly, the effect of preventing leakage current from being formed under the source-drain doped layer 141 is better, which can further improve the gate's control ability over the channel, suppress the short channel effect, and further improve the performance of the semiconductor structure.

[0080] Specifically, the source-drain doped layer 141 is formed after the second isolation layer 115 is formed, and the source-drain doped layer 141 is formed at the ends of the top fin 113 on both sides of the gate structure 130 by an epitaxial growth process. Since the epitaxial growth process has the characteristic of selective growth, that is, the epitaxial growth is carried out with the surface of the top fin 113 as the growth basis, and the epitaxial growth cannot be carried out with the surface of the second isolation layer 115 as the growth basis. Therefore, after the source-drain doped layers 141 on the opposite ends of the top fin 113 contact each other, it is easy to form a gap 142 between the source-drain doped layer 141 and the second isolation layer 115.

[0081] Correspondingly, the gap 142 is surrounded by the source-drain doped layer 141 and the second isolation layer 115 , that is, the gap 142 exposes the source-drain doped layer 141 and the second isolation layer 115 .

[0082] In this embodiment, the semiconductor structure further includes: a source-drain doped interconnection layer 180 located above the source-drain doped layer 141 and electrically connected to the source-drain doped layer 141 ; and an interlayer dielectric layer 190 covering the source-drain doped interconnection layer 180 .

[0083] The description of the source-drain doped interconnect layer 180 and the interlayer dielectric layer 190 will not be repeated here.

[0084] Correspondingly, the present invention also provides a method for forming a semiconductor structure. Figures 2 to 8 It is a schematic structural diagram corresponding to each step in an embodiment of a method for forming a semiconductor structure of the present invention.

[0085] refer to Figures 2 to 3 , providing a substrate (not shown), the substrate comprising a substrate 500, and a channel protrusion 510 protruding from the substrate 500, along the normal direction of the top surface of the substrate 500, the channel protrusion 510 comprises a bottom fin 511, a top fin 513 located above the bottom fin 511, and a middle fin 512 located between the bottom fin 511 and the top fin 513;

[0086] The substrate provides a process platform for subsequent process steps.

[0087] In this embodiment, the substrate is used to form a field effect transistor. As an example, the substrate is used to form a fin field effect transistor.

[0088] In this embodiment, the base includes a substrate 500, and the substrate 500 is a silicon substrate 500. In other embodiments, the material of the substrate can also be other materials such as germanium, silicon germanium, silicon carbide, gallium arsenide or indium gallium, and the substrate can also be other types of substrates such as a silicon substrate on an insulator or a germanium substrate on an insulator.

[0089] The channel protrusion 510 protrudes from the substrate 500 , so that the gate structure formed subsequently can cross the channel protrusion 510 and cover a portion of the top and sidewall of the top fin 513 .

[0090] The channel protrusion 510 includes a bottom fin 511 , a top fin 513 located above the bottom fin 511 , and a middle fin 512 located between the bottom fin 511 and the top fin 513 .

[0091] As an example, the bottom fin 511 and the substrate 500 are an integral structure.

[0092] The middle fin 512 provides a process platform for subsequently forming a second isolation layer, and the top fin 513 in the channel protrusion 510 is used to provide a conductive channel of the field effect transistor.

[0093] The material of the top fin 513 includes one or more of silicon, germanium, silicon germanium, silicon carbide, gallium nitride, gallium arsenide and indium gallium. In this embodiment, the material of the top fin 513 is silicon.

[0094] Along the normal direction of the top surface of the substrate 500, the thickness of the middle fin 512 should not be too large or too small. If the thickness of the middle fin 512 is too large, it is easy to cause lattice dislocation in the top fin 513 located above the middle fin 512, so that there are defect energy levels in the top fin 513, which correspondingly reduces the carrier concentration when the semiconductor device is working, thereby affecting the performance of the semiconductor device. If the thickness of the middle fin 512 is too small, it is easy to make the thickness of the second isolation layer subsequently formed in the middle fin 512 also correspondingly small, so that the source and drain doping layer subsequently formed is isolated from the bottom fin 511 through the second isolation layer. Therefore, in this embodiment, along the normal direction of the top surface of the substrate 500, the thickness of the middle fin 512 ranges from 2 nanometers to 50 nanometers.

[0095] In this embodiment, the material of the middle fin 512 includes silicon germanium.

[0096] By selecting silicon germanium, it is easy to epitaxially grow a material layer corresponding to the top fin 513 on the top of the middle fin 512. In addition, silicon germanium is easy to oxidize, which is conducive to the subsequent formation of a second isolation layer in the middle fin 512.

[0097] It should be noted that the molar percentage concentration of germanium in the middle fin 512 should not be too large or too small. If the molar percentage concentration of germanium in the middle fin 512 is too large, the thickness of the second isolation layer formed in the middle fin 512 later will be difficult to meet the target thickness requirement; if the molar percentage concentration of germanium in the middle fin 512 is too small, it will be difficult for silicon germanium to be oxidized, thereby making it correspondingly difficult to form the second isolation layer in the middle fin 512 later; and if the molar percentage concentration of germanium in the middle fin 512 is too small, it will be difficult to use it as a stop position in the subsequent process of forming the source and drain grooves, thereby easily increasing the probability of the middle fin 512 being damaged in this process. Therefore, in this embodiment, the molar percentage concentration of germanium in the middle fin 512 is greater than 20% and less than 50%.

[0098] In this embodiment, along the normal direction of the top surface of the substrate 500, the thickness range of the top fin 513 is

[0099] In this embodiment, the steps of forming the substrate 500 and the channel protrusion 510 include: Figure 2 As shown, an initial substrate is provided, the initial substrate includes a substrate material layer 500', an intermediate fin material layer 512' and a top fin material layer 513' stacked sequentially from bottom to top; Figure 3 As shown, the initial substrate is patterned to pattern the top fin material layer 513 ′ into the top fin 513 , the middle fin material layer 512 ′ into the middle fin 512 , and a partial thickness of the substrate material layer 500 ′ is patterned into the bottom fin 511 , and the remaining thickness of the substrate material layer 500 ′ that has not been patterned serves as the substrate 500 .

[0100] Specifically, through an epitaxial growth process, a middle fin material layer 512 ′ is formed on the substrate material layer 500 ′, and a top fin material layer 513 ′ is formed on the middle fin material layer 512 ′.

[0101] Continue to refer Figure 3 A first isolation layer 520 is formed on the substrate 500 at the side of the channel protrusion 510 , and the first isolation layer 520 covers the sidewalls of the bottom fin 511 and the sidewalls of the middle fin 512 .

[0102] The first isolation layer 520 is used to isolate each semiconductor device to prevent leakage current from occurring between the devices.

[0103] In this embodiment, the first isolation layer 520 is a shallow trench isolation (STI) structure.

[0104] The material of the first isolation layer 520 includes one or more of silicon oxide, silicon nitride and silicon oxynitride.

[0105] The first isolation layer 520 covers the side walls of the bottom fin 511 and the side walls of the middle fin 512, that is, the first isolation layer 520 exposes the top fin 513, so that the top fin 513 is used as an effective fin (Active Fin), while the middle fin 512 is not used as an effective fin. The effective fin covered by the subsequently formed gate structure is used to provide a conductive channel when the device is working.

[0106] Continue to refer Figure 3 A gate structure 530 is formed on the first isolation layer 520 and crosses the top fin 513 . The gate structure 530 covers a portion of the top and sidewalls of the top fin 513 .

[0107] The top fin 513 is used as an active fin. The active fin covered by the gate structure 530 is used to provide a conductive channel when the device is working.

[0108] In this embodiment, the gate structure 530 is a dummy gate structure, which is used to reserve space for a device gate structure to be formed subsequently. For example, the gate structure 530 may be a polysilicon gate structure.

[0109] In this embodiment, after forming a gate structure 530 across the top fin 513 on the first isolation layer 520 , the method further includes: forming a spacer structure (not shown) on the sidewall of the gate structure 530 .

[0110] The sidewall spacer is used to protect the sidewall of the device gate structure formed subsequently. The sidewall spacer can be a single-layer structure or a stacked structure, and the material of the sidewall spacer includes one or more of silicon oxide, silicon nitride, silicon carbide, silicon carbonitride, silicon carbonitride oxide, silicon oxynitride, boron nitride and boron carbonitride.

[0111] refer to Figures 4 to 5 In a predetermined region (not shown) of the middle fin 512 along a direction parallel to the top surface of the substrate 500, a second isolation layer 515 (such as Figure 5 As shown), the top of the second isolation layer 515 is flush with the top of the middle fin 512, and the source and drain doping layers are formed above the preset area.

[0112] The channel protrusion 510 includes an intermediate fin 512 located between a bottom fin 511 and a top fin 513. A second isolation layer 515 is formed in the intermediate fin 512 in a preset area. The top of the second isolation layer 515 is flush with the top of the intermediate fin 512. The area above the preset area is used to form a source-drain doping layer, that is, the preset area is an area for forming a source-drain doping layer. Therefore, after the source-drain doping layer is formed, the source-drain doping layer is isolated from the bottom fin 511 by the second isolation layer 515, which improves the insulation effect between the source-drain doping layer and the bottom fin 511, and accordingly makes it difficult for leakage current to form below the source-drain doping layer, thereby improving the control ability of the device gate structure over the channel, suppressing the short channel effect, and further improving the performance of the semiconductor structure.

[0113] In addition, compared with the solution of achieving insulation between the source-drain doped layer and the bottom fin by ion implantation into the channel protrusion structure below the source-drain doped layer to form a PN junction below the source-drain doped layer, the present embodiment achieves insulation between the source-drain doped layer and the bottom fin 511 through the second isolation layer 515. There is no need to balance the PN junction leakage current in the substrate and the leakage current between the source-drain doped layer and the bottom fin. In other words, the limitation of the PN junction leakage current on the insulation effect can be avoided. Moreover, in the present embodiment, the insulation effect of the second isolation layer 515 obtained by oxidizing the middle fin 512 in the preset area is more significant than the insulation effect achieved by forming a PN junction below the source-drain doped layer.

[0114] The top of the second isolation layer 515 is flush with the top of the middle fin 512 , which reduces the longitudinal distance between the subsequently formed source-drain doped layer and the second isolation layer 515 , thereby enhancing the suppression effect of the second isolation layer 515 on the leakage current below the subsequently formed source-drain doped layer.

[0115] Furthermore, the second isolation layer 515 is formed in the middle fin 512 , thereby reducing the influence on the formation process of the material layer corresponding to the top fin 513 .

[0116] Compared with the solution of forming the second isolation layer in the bottom fin, the second isolation layer 515 is embedded in the middle fin 512, which makes it easy to control the formation position of the second isolation layer 515 through the middle fin 512 and reduces the process complexity and difficulty.

[0117] It should be noted that the second isolation layer 515 is embedded in the middle fin 512 , and the second isolation layer 515 may be located in a portion of the thickness of the middle fin 512 below the source and drain doping layer, or may penetrate the middle fin 512 below the source and drain doping layer.

[0118] In this embodiment, in a preset area of ​​the middle fin 512 along a direction parallel to the top surface of the substrate 500, the step of forming a second isolation layer 515 located in the middle fin 512 includes: performing a heat treatment process on the middle fin 512 in the preset area under an oxygen-containing atmosphere to convert the middle fin 512 in the preset area into a second isolation layer 515.

[0119] The middle fin 512 of the preset area is subjected to a heat treatment process in an oxygen-containing atmosphere so that the middle fin 512 of the preset area is oxidized into a second isolation layer 515. The second isolation layer 515 can be formed in the middle fin 512, which is beneficial for combining with the existing process flow, simplifying the process flow, and saving process costs.

[0120] In a specific embodiment, the heat treatment process is an annealing process.

[0121] It should be noted that since the middle fin 512 in the preset area is oxidized into the second isolation layer 515, accordingly, in this embodiment, in the step of forming the second isolation layer 515 located in the middle fin 512 in the preset area along the direction parallel to the top surface of the substrate 500, the material of the second isolation layer 515 includes oxide.

[0122] Since in the present embodiment, the material of the middle fin 512 includes silicon germanium, that is, the silicon germanium in the preset area is subjected to a heat treatment process in an oxygen-containing atmosphere, so that the silicon germanium in the preset area is oxidized into a second isolation layer 515 whose material is silicon oxide, and the oxidation reaction of silicon germanium also generates volatile germanium. However, if germanium is generated at the bottom of the second isolation layer 515, since there are other film layers below the bottom of the second isolation layer 515, it is easy to affect the volatilization of germanium, so that a reaction generation layer (not marked) whose material is germanium is formed at the bottom of the second isolation layer 515. Therefore, in the present embodiment, in the step of forming the second isolation layer 515 located in the middle fin 512 in the preset area of ​​the middle fin 512 along the direction parallel to the top surface of the substrate 500, the material of the second isolation layer 515 includes silicon oxide, and a reaction generation layer is also formed at the bottom of the second isolation layer 515, the reaction generation layer is in contact with the bottom of the second isolation layer 515, and the material of the reaction generation layer is germanium.

[0123] In other embodiments, in a predetermined region of the middle fin along a direction parallel to the top surface of the substrate, the step of forming a second isolation layer in the middle fin includes: performing a heat treatment process on the material layer of the middle fin in the predetermined region under a nitrogen-containing atmosphere to convert the middle fin in the predetermined region into the second isolation layer. Therefore, in other embodiments, the material of the second isolation layer may also include nitride.

[0124] Correspondingly, in other embodiments, the material of the second isolation layer may also include silicon nitride.

[0125] In this embodiment, the parameters of the heat treatment process include: the gas of the oxygen-containing atmosphere heat treatment process includes one or more of oxygen and ozone, and the process temperature is less than or equal to 350°C.

[0126] The middle fin 512 of the preset area is subjected to a heat treatment process in an oxygen and / or ozone atmosphere, so that the middle fin 512 of the preset area can be easily oxidized into a second isolation layer 515. In addition, it is convenient to obtain oxygen or ozone, which reduces the difficulty of the heat treatment process accordingly.

[0127] The process temperature of the heat treatment process is less than or equal to 350° C., which makes it difficult for the material of the middle fin 512 to diffuse into the effective fin, thereby reducing the probability of the effective fin being damaged.

[0128] In other embodiments, the heat treatment process may also be performed on the middle fin of the preset area in a nitrogen-containing atmosphere. Accordingly, the gas of the nitrogen-containing atmosphere may include nitrogen.

[0129] In the present embodiment, before performing a heat treatment process on the middle fin 512 in a preset area under an oxygen-containing atmosphere or a nitrogen-containing atmosphere, the step of forming a second isolation layer 515 located in the middle fin 512 in a preset area along a direction parallel to the top surface of the substrate 500 also includes: performing an ion implantation process on the middle fin 512 in the preset area, and the implanted ions in the ion implantation process include oxygen ions or nitrogen ions.

[0130] An ion implantation process is performed on the middle fin 512 in a preset area. The ion implantation process is used to convert the covalent bonds already formed in the middle fin 512 into dangling bonds, thereby facilitating the formation of new covalent bonds in the heat treatment process, thereby enhancing the conversion effect on the middle fin 512, which is correspondingly beneficial to increase the thickness of the second isolation layer 515 formed in the middle fin 512.

[0131] The implanted ions in the ion implantation process include oxygen ions or nitrogen ions, which convert the already formed covalent bonds into dangling bonds while reducing the probability of adverse effects.

[0132] In this embodiment, a heat treatment process is performed on the middle fin 512 of the predetermined area in an oxygen-containing atmosphere, and the implanted ions in the ion implantation process are oxygen ions, thereby further improving the oxidation effect.

[0133] In other embodiments, a heat treatment process is performed on the middle fin of the predetermined area in a nitrogen-containing atmosphere, and the implanted ions in the ion implantation process are nitrogen ions, thereby further improving the nitridation effect.

[0134] Specifically, the parameters of the ion implantation process include: the implantation dose is 1E13 atoms / cm 2 ~9E17atoms / cm 2The implantation energy is 3KeV~8KeV, and the process temperature is less than or equal to 350℃.

[0135] The parameters of the ion implantation process include: implantation dose of 1E13atoms / cm 2 ~9E17atoms / cm 2 The implantation energy is 3KeV to 8KeV, which can easily make the thickness of the second isolation layer 515 formed in the middle fin 512 meet the target thickness requirement, so that the second isolation layer 515 can better isolate the subsequently formed source and drain doping layer from the bottom fin 511.

[0136] The implantation dose should not be too large or too small. If the implantation dose is too large, the probability of the bottom fin 511 at the bottom of the middle fin 512 being damaged is likely to increase; if the implantation dose is too small, the enhanced heat treatment process may not be effective in the degree of material conversion along the thickness direction of the middle fin 512, which may easily lead to the second isolation layer 515 isolating the subsequently formed source and drain doping layer from the bottom fin 511. Therefore, in this embodiment, the implantation dose of the ion implantation process is 1E13atoms / cm 2 ~9E17atoms / cm 2 .

[0137] The injected energy should not be too large or too small. If the injected energy is too large, the probability of the bottom fin 511 at the bottom of the middle fin 512 being damaged is likely to increase; if the injected energy is too small, the enhanced heat treatment process is likely to have a poor effect on the degree of material conversion of the middle fin 512 along its thickness direction, which may easily lead to the second isolation layer 515 isolating the subsequently formed source and drain doping layer from the bottom fin 511. Therefore, in this embodiment, the injection energy of the ion implantation process is 3KeV to 8KeV.

[0138] The process temperature of the ion implantation process is less than or equal to 350° C., which makes it difficult for the material of the middle fin 512 to diffuse into the effective fin, thereby reducing the probability of the effective fin being damaged.

[0139] Combined with reference Figures 4 to 6 In this embodiment, after forming a gate structure 530 across the top fin 513 on the first isolation layer 520, and before forming a source-drain doping layer in the top fin 513 on both sides of the gate structure 530, it also includes: forming source-drain grooves 540 in the top fin 513 on both sides of the gate structure 530, and the source-drain grooves 540 expose the top of the middle fin 512.

[0140] Source-drain grooves 540 are formed in the top fins 513 on both sides of the gate structure 530, so as to facilitate the subsequent formation of source-drain doped layers in the source-drain grooves 540; moreover, the source-drain grooves 540 expose the top of the middle fin 512, so that a second isolation layer 515 can be formed in the middle fin 512 via the source-drain grooves 540, thereby reducing the process difficulty of forming the second isolation layer 515 in the middle fin 512, and is also conducive to compatibility with existing process steps, reducing changes to existing processes, simplifying the process flow, and saving process costs. Moreover, it is easy to define the position of the second isolation layer 515 through the source-drain grooves 540. In addition, it is easy to form a gap between the source-drain doped layer and the second isolation layer 515 in the subsequent process of forming the source-drain doped layer, thereby improving the insulation effect between the source-drain doped layer and the bottom fin 511.

[0141] Correspondingly, in the present embodiment, in the region of the middle fin 512 along a direction parallel to the top surface of the substrate 500, the step of forming a second isolation layer 515 located in the middle fin 512 includes: forming a second isolation layer 515 in the middle fin 512 via the source-drain groove 540, and the second isolation layer 515 is located at the bottom of the source-drain groove 540.

[0142] In this embodiment, after forming the source-drain groove 540 and before forming the second isolation layer 515, the protective layer 550 (such as a protective layer 550 for example) covering the sidewalls and top of the gate structure 530 and the sidewalls of the source-drain groove 540 is formed. Figure 4 shown).

[0143] The protection layer 550 is used to protect the gate structure 530 and the effective fins covered by the gate structure 530 , thereby reducing the probability that the gate structure 530 and the effective fins are damaged during the process of forming the second isolation layer 515 .

[0144] Specifically, the step of forming a protective layer 550 covering the sidewalls and top of the gate structure 530 and the sidewalls of the source and drain grooves 540 includes: forming a protective material layer (not marked) covering the sidewalls and top of the gate structure 530 and the sidewalls and bottom of the source and drain grooves 540; removing the protective material layer covering the bottom of the source and drain grooves 540, and the remaining protective material layer covering the sidewalls and top of the gate structure 530 and the sidewalls of the source and drain grooves 540 serves as the protective layer 550.

[0145] First, a protective material layer is formed to cover the sidewalls and top of the gate structure 530 and the sidewalls and bottom of the source-drain groove 540, and then the protective material layer at the bottom of the source-drain groove 540 is removed with the middle fin 512 as the stop position, and the remaining protective material layer is used as the protective layer 550, which is conducive to reducing the difficulty of forming the protective layer. In addition, the protective material layer covering the bottom of the source-drain groove 540 is removed, and the remaining protective material layer covering the sidewalls and top of the gate structure 530 and the sidewalls of the source-drain groove 540 is used as the protective layer 550 to expose the middle fin 512 at the bottom of the source-drain groove 540, thereby providing a process basis for the subsequent formation of the second isolation layer 515 in the middle fin 512.

[0146] It should be noted that the material of the protection layer 550 includes a carbon-silicon based material.

[0147] The material of the protection layer 550 includes a carbon-silicon based material which is difficult to be oxidized in an oxygen-containing atmosphere, so that the protection layer 550 has a better effect of preventing the gate structure 530 and the top fin 513 of the sidewall of the source / drain groove 540 from being oxidized.

[0148] Accordingly, after forming the second isolation layer 515, the process further includes: removing the protective layer 550 (eg Figure 6 shown).

[0149] The protection layer 550 is removed to expose the top fin 513 of the sidewall of the source / drain groove 540 , thereby providing a process basis for the subsequent formation of source / drain doping layers.

[0150] In this embodiment, the process for removing the protective layer 550 is a wet etching process, which has relatively low cost, simple operation steps, and can achieve a large etching selectivity ratio.

[0151] It should be noted that, in this embodiment, the source-drain grooves 540 are first formed in the top fins 513 on both sides of the gate structure 530, and then the second isolation layer 515 located in the middle fin 512 is formed in the preset area of ​​the middle fin 512 along the direction parallel to the top surface of the substrate 500 through the source-drain grooves 540. In other embodiments, the second isolation layer located in the middle fin may be first formed in the preset area of ​​the middle fin along the direction parallel to the top surface of the substrate, and then the source-drain grooves are formed in the top fins on both sides of the gate structure.

[0152] refer to Figure 7 , a source-drain doped layer 541 is formed in the top fin 513 on both sides of the gate structure 530 , and the source-drain doped layer 541 is isolated from the bottom fin 511 by the second isolation layer 515 .

[0153] The source-drain doped layer 541 is used as the source region and the drain region of the transistor. When the device is working, the source-drain doped layer 541 is used to provide a carrier source.

[0154] The source-drain doped layer 541 is isolated from the bottom fin 511 by the second isolation layer 515, which improves the insulation effect between the source-drain doped layer 541 and the bottom fin 511, and accordingly makes it difficult for leakage current to form under the source-drain doped layer 541, thereby improving the gate's control ability over the channel, suppressing the short channel effect, and further improving the performance of the semiconductor structure.

[0155] In this embodiment, during the process of forming the source-drain doped layer 541 , a gap 542 is provided between the source-drain doped layer 541 and the second isolation layer 515 .

[0156] There is a gap 542 between the source-drain doped layer 541 and the second isolation layer 515, so that the insulation effect between the source-drain doped layer 541 and the bottom fin 511 is better, and correspondingly, the effect of preventing leakage current from being formed under the source-drain doped layer 541 is better, which can further improve the gate's control ability over the channel, suppress the short channel effect, and further improve the performance of the semiconductor structure.

[0157] Specifically, the source-drain doped layer 541 is formed after the second isolation layer 515 is formed, and the source-drain doped layer 541 is formed at the ends of the top fin 513 on both sides of the gate structure 530 by an epitaxial growth process. Since the epitaxial growth process has the characteristic of selective growth, that is, the epitaxial growth is carried out with the surface of the top fin 513 as the growth basis, and the epitaxial growth cannot be carried out with the surface of the second isolation layer 515 as the growth basis. Therefore, after the source-drain doped layers 541 on the opposite ends of the top fin 513 contact each other, it is easy to form a gap 542 between the source-drain doped layer 541 and the second isolation layer 515.

[0158] Correspondingly, the gap 542 is surrounded by the source-drain doped layer 541 and the second isolation layer 515 , that is, the gap 542 exposes the source-drain doped layer 541 and the second isolation layer 515 .

[0159] In this embodiment, the step of forming source-drain doped layers 541 in the top fins 513 on both sides of the gate structure 530 includes: forming the source-drain doped layers 541 in the source-drain grooves 540 after forming the second isolation layer 515 .

[0160] The source-drain doped layer 541 is formed in the source-drain groove 540 , so that the quality of the source-drain doped layer 541 is better.

[0161] In this embodiment, after forming the source-drain groove 540 and before forming the second isolation layer 515, it also includes: forming a protective layer 550 covering the side walls and top of the gate structure 530 and the side walls of the source-drain groove 540; accordingly, after removing the protective layer 550, a source-drain doping layer 541 is formed in the source-drain groove 540.

[0162] refer to Figure 8 In this embodiment, after the source-drain doped layer 541 is formed, the formation method further includes: removing the gate structure 530 to form a gate opening (not shown); forming a device gate structure 570 in the gate opening; forming a source-drain doped interconnection layer 580 electrically connected to the source-drain doped layer 541 above the source-drain doped layer 541; forming an interlayer dielectric layer 590 located on the first isolation layer 520, and the interlayer dielectric layer 590 buries the source-drain doped layer 541, the device gate structure 570 and the source-drain doped interconnection layer 580 therein.

[0163] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

Claims

1. A semiconductor structure, It is characterized in that include: A substrate, the substrate comprising a substrate and a channel protrusion structure protruding from the substrate, wherein along a normal direction of a top surface of the substrate, the channel protrusion structure comprises a bottom fin, a top fin located above the bottom fin, and an intermediate fin located between the bottom fin and the top fin; A first isolation layer, located on the substrate at the side of the channel protrusion structure, the first isolation layer covering the sidewall of the bottom fin and the sidewall of the middle fin; A gate structure, located on the first isolation layer, the gate structure spanning the channel protrusion structure and covering a portion of the top and sidewalls of the top fin; Source and drain doped layers are located in the top fins on both sides of the gate structure; The second isolation layer is located below the source-drain doped layer and embedded in the middle fin. The top of the second isolation layer is flush with the top of the middle fin. The source-drain doped layer is isolated from the bottom fin by the second isolation layer.

2. The semiconductor structure according to claim 1, It is characterized in that The semiconductor structure further includes a gap located between the source-drain doped layer and the second isolation layer.

3. The semiconductor structure according to claim 1, It is characterized in that The material of the second isolation layer includes oxide or nitride.

4. The semiconductor structure according to claim 1, It is characterized in that The material of the middle fin includes silicon germanium.

5. The semiconductor structure according to claim 4, It is characterized in that The material of the second isolation layer includes silicon oxide or silicon nitride. The semiconductor structure further includes: a reaction-generated layer located at the bottom of the second isolation layer and in contact with the bottom of the second isolation layer. The material of the reaction-generated layer is germanium.

6. The semiconductor structure according to claim 4, It is characterized in that The molar concentration of germanium in the middle fin is greater than 20% and less than 50%.

7. The semiconductor structure according to claim 1, It is characterized in that Along the normal direction of the top surface of the substrate, the thickness of the middle fin is in a range of 2 nanometers to 50 nanometers.

8. A method for forming a semiconductor structure, It is characterized in that include: Providing a substrate, the substrate comprising a substrate and a channel protrusion protruding from the substrate, wherein along a normal direction of a top surface of the substrate, the channel protrusion comprises a bottom fin, a top fin located above the bottom fin, and an intermediate fin located between the bottom fin and the top fin; forming a first isolation layer on the substrate at the side of the channel protrusion, wherein the first isolation layer covers the sidewall of the bottom fin and the sidewall of the middle fin; In a preset region of the middle fin along a direction parallel to the top surface of the substrate, a second isolation layer is formed in the middle fin, the top of the second isolation layer is flush with the top of the middle fin, and a source-drain doping layer is formed above the preset region; forming a gate structure across the top fin on the first isolation layer, wherein the gate structure covers a portion of the top and sidewalls of the top fin; A source-drain doped layer is formed in the top fins on both sides of the gate structure, and the source-drain doped layer is isolated from the bottom fin by the second isolation layer.

9. The method for forming a semiconductor structure according to claim 8, It is characterized in that In a preset area of ​​the middle fin along a direction parallel to the top surface of the substrate, the step of forming a second isolation layer located in the middle fin includes: performing a heat treatment process on the middle fin in the preset area under an oxygen-containing atmosphere or a nitrogen-containing atmosphere to convert the middle fin in the preset area into a second isolation layer.

10. The method for forming a semiconductor structure according to claim 9, It is characterized in that The parameters of the heat treatment process include: the gas of the oxygen-containing atmosphere includes one or more of oxygen and ozone, the gas of the nitrogen-containing atmosphere includes nitrogen, and the process temperature is less than or equal to 350°C.

11. The method for forming a semiconductor structure according to claim 9, It is characterized in that Before performing a heat treatment process on the middle fin of the preset area in an oxygen-containing atmosphere or a nitrogen-containing atmosphere, the step of forming a second isolation layer located in the middle fin in a preset area of ​​the middle fin along a direction parallel to the top surface of the substrate also includes: performing an ion implantation process on the middle fin of the preset area, the implanted ions of the ion implantation process including oxygen ions or nitrogen ions.

12. The method for forming a semiconductor structure according to claim 11, It is characterized in that The parameters of the ion implantation process include: the implantation dose is 1E13 atoms / cm 2 ~9E17atoms / cm 2 The implantation energy is 3KeV~8KeV, and the process temperature is less than or equal to 350℃.

13. The method for forming a semiconductor structure according to claim 8 or 9, It is characterized in that After forming a gate structure across the top fin on the first isolation layer and before forming source-drain doping layers in the top fins on both sides of the gate structure, the method further includes: forming source-drain grooves in the top fins on both sides of the gate structure, wherein the source-drain grooves expose the top of the middle fin; The step of forming a second isolation layer in the middle fin in a region of the middle fin along a direction parallel to the top surface of the substrate comprises: forming a second isolation layer in the middle fin via the source-drain groove, wherein the second isolation layer is located at the bottom of the source-drain groove; The step of forming source-drain doped layers in the top fins on both sides of the gate structure includes: forming the source-drain doped layers in the source-drain grooves after forming the second isolation layer.

14. The method for forming a semiconductor structure according to claim 13, It is characterized in that After forming the source-drain grooves and before forming the second isolation layer, the method further includes: forming a protection layer covering the sidewalls and top of the gate structure and the sidewalls of the source-drain grooves; After forming the second isolation layer, the method further includes: removing the protective layer; After removing the protection layer, a source-drain doping layer is formed in the source-drain groove.

15. The method for forming a semiconductor structure according to claim 14, It is characterized in that The step of forming a protective layer covering the sidewalls and top of the gate structure and the sidewalls of the source / drain grooves comprises: forming a protective material layer covering the sidewalls and top of the gate structure, and the sidewalls and bottom of the source / drain grooves; The protective material layer covering the bottom of the source-drain groove is removed, and the remaining protective material layer covering the sidewall and top of the gate structure and the sidewall of the source-drain groove is used as a protective layer.

16. The method for forming a semiconductor structure according to claim 14, It is characterized in that The material of the protection layer includes a carbon-silicon based material.

17. The method for forming a semiconductor structure according to any one of claims 8 to 12, It is characterized in that In the step of forming a second isolation layer in the middle fin in a predetermined region of the middle fin along a direction parallel to the top surface of the substrate, a material of the second isolation layer includes oxide or nitride.

18. The method for forming a semiconductor structure according to any one of claims 8 to 12, It is characterized in that The material of the middle fin includes silicon germanium.

19. The method for forming a semiconductor structure according to claim 18, It is characterized in that The molar concentration of germanium in the middle fin is greater than 20% and less than 50%.