Method for manufacturing cell stack

By controlling the thickness variation of the storage units and applying restraint loads during the manufacturing process of the battery stack, the problems of thickness deviation and swelling caused by charging and discharging when stacking storage units in the battery stack are solved, and the stability and stability of the battery stack are achieved. Long life.

CN118738490APending Publication Date: 2024-10-01PRIME PLANET ENERGY & SOLUTIONS INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410282566.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-30
Filing Date
2024-03-13
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

During the manufacturing process of the battery stack, when multiple storage units are stacked along the thickness direction, the thickness deviation is large, making stacking difficult. At the same time, the storage units swell during the charging and discharging process, affecting the stability of the battery stack.

Method used

By applying a load to the storage unit in the preparation process, the thickness variation of the unit is controlled within the range of 0.051 to 0.055% to suppress thickness deviation, and a constraint load is applied along the thickness direction during the lamination process to ensure the stability of the storage unit.

Benefits of technology

It achieves easy stacking of storage units and stable thickness of the battery stack, suppresses swelling caused by charging and discharging, and improves the service life and performance of the battery stack.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738490A_ABST
    Figure CN118738490A_ABST
Patent Text Reader

Abstract

The invention relates to a method for manufacturing a cell stack. Provided is a method for manufacturing a cell stack in which both the suppression of variation in thickness of each power storage cell during assembly and the suppression of swelling of the power storage cells during use of the cell stack are achieved. The technology disclosed herein comprises: a preparation step for preparing an electricity storage cell comprising a wound electrode body, a non-aqueous electrolyte, and a case; and a stacking step for stacking a plurality of the power storage cells, in which, for the power storage cells prepared in the preparation step, a process in which a load is applied to 2.0 MPa at a speed of 0.1 mm / min in the thickness direction of the power storage cells and the load is reduced to 0.01 MPa after the application is performed as one cycle, and when the process is performed for three cycles, the load is reduced to 0.01 MPa after the load is applied to the power storage cells prepared in the preparation step. The amount of change ((X1-X3) / X1 * 100) in the thickness X3 of the electricity storage unit at the time of 2.0 MPa application in the third cycle relative to the thickness X1 of the electricity storage unit at the time of 2.0 MPa application in the first cycle is 0.051-0.055%.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a method of manufacturing a battery stack. Background Art

[0002] In recent years, a battery stack with multiple power storage units is suitable for use as a driving power source for vehicles such as hybrid electric vehicles (HEV), plug-in hybrid electric vehicles (PHEV), and electric vehicles (BEV). As a related prior art document, Japanese Patent Publication No. 2018-055806 can be cited. In Patent Document 1, a technology related to a non-aqueous electrolyte secondary battery (power storage unit) is disclosed, which includes an electrode body including a frame, a non-aqueous electrolyte (non-aqueous electrolyte) and a positive electrode, a negative electrode, and a separator, and the electrode body also includes a low spring constant film having a spring constant (second spring constant) lower than the spring constant (first spring constant) of the negative electrode, thereby suppressing the extrusion of the non-aqueous electrolyte inside the electrode body accompanied by the expansion and contraction of the electrode body.

[0003] Patent Literature

[0004] Patent Document 1: Japanese Patent Publication No. 2018-055806 Summary of the invention

[0005] Problems to be solved by the invention

[0006] In the manufacture of a battery stack, specifically, if the thickness deviation of each storage cell is large when a plurality of storage cells are stacked along the thickness direction of the storage cell, the stacking of the storage cells becomes difficult. On the other hand, in the case where a storage cell in which the extrusion of a non-aqueous electrolyte is excessively suppressed is used in a battery stack, the battery stack is repeatedly charged and discharged, so that the storage cells stacked on the battery stack swell (increase in thickness). In addition, according to the research of the present inventors, it is known that the easy extrusion of the non-aqueous electrolyte in the electrode body is not determined solely by the spring constant of the constituent components of the electrode body disclosed in Japanese Patent Publication No. 2018-055806. Therefore, in the manufacture of a battery stack including a plurality of storage cells, not only the thickness deviation of each storage cell when the storage cells are stacked, but also the suppression of the swelling of the storage cells mounted when the battery stack is used must be considered.

[0007] The technology disclosed herein has been developed in view of the above-mentioned actual situation, and its main purpose is to provide a method for manufacturing a battery stack that achieves both suppression of thickness variation among power storage cells during assembly and suppression of swelling of the power storage cells during use of the battery stack.

[0008] Means for solving problems

[0009] The technology disclosed herein is a method for manufacturing a battery stack including a plurality of square storage cells, characterized in that it comprises: a preparation step, in which the storage cells are prepared, the storage cells comprising a flat-shaped wound electrode body in which a positive electrode and a negative electrode are stacked and wound via a separator, a non-aqueous electrolyte, and a shell for accommodating the wound electrode body and the non-aqueous electrolyte; and a stacking step, in which a plurality of the storage cells are stacked along the thickness direction of the storage cells, wherein, for the storage cells prepared in the preparation step, A load of 2.0 MPa is applied in the thickness direction at a speed of 0.1 mm / min, and the load is reduced to 0.01 MPa after the application, which is regarded as one cycle. When the treatment is performed for 3 cycles, the change in thickness X3 of the power storage unit when 2.0 MPa is applied in the third cycle relative to the thickness X1 of the power storage unit when 2.0 MPa is applied in the first cycle ((X1-X3) / X1×100) (hereinafter also referred to as "unit thickness change") is 0.051 to 0.055%.

[0010] For the storage cell prepared in the above-mentioned preparation process, it is 0.051 to 0.055%. In the storage cell having this structure, the thickness deviation of each storage cell is suppressed at the stage of the preparation process. Therefore, the storage cells can be easily stacked (assembled) during the stacking process. On the other hand, the storage cell whose cell thickness variation is within the above-mentioned range suppresses the expansion of the storage cell caused by charging and discharging. Therefore, according to the manufacturing method disclosed herein, when the battery stack is constructed, the thickness deviation of the storage cell is also suppressed, and when the battery stack is used, a battery stack with a stable thickness of the storage cell is provided. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is a perspective view schematically showing a battery stack according to one embodiment.

[0012] Figure 2 A perspective view of a power storage unit.

[0013] Figure 3 For along Figure 2 Schematic longitudinal cross-sectional view along line III-III.

[0014] Figure 4 This is a perspective view schematically showing a wound electrode body attached to a sealing plate.

[0015] Figure 5 It is a perspective view schematically showing a wound electrode body.

[0016] Figure 6 Schematic diagram showing the structure of a wound electrode body.

[0017] Figure 7This is a flowchart showing a method for manufacturing a battery stack according to one embodiment.

[0018] Figure 8 Schematic diagrams for explaining the thickness change of a wound electrode body. (A) shows a wound electrode body with less non-aqueous electrolyte. (B) shows a wound electrode body with more non-aqueous electrolyte. (C) shows a wound electrode body with more non-aqueous electrolyte and a non-aqueous electrolyte layer.

[0019] Fig. 9 This is a schematic diagram for explaining the measurement of the cell thickness variation in the preparation step.

[0020] Fig.10 This is a flowchart showing a method for manufacturing a power storage unit according to an embodiment.

[0021] Fig.11 It is a graph showing the relationship between the cell thickness variation and the cell thickness deviation.

[0022] Fig.12 It is a graph showing the relationship between the cell thickness change and the cell expansion rate. DETAILED DESCRIPTION

[0023] Below, with appropriate reference to the attached Figure 1 Several preferred embodiments of the battery stack disclosed herein are described. Matters other than those specifically mentioned in this specification, i.e., matters required for the implementation of the present disclosure (e.g., the general structure and manufacturing process of the storage unit that are not the characteristics of the present invention) can be understood as design matters for those skilled in the art based on the prior art in this field. The battery stack disclosed herein can be implemented based on the contents disclosed in this specification and the technical common sense in this field.

[0024] In addition, in the following drawings, the same reference numerals are used for components and parts that play the same role, and repeated descriptions are sometimes omitted or simplified. In addition, the notation "A to B" showing a range in this specification includes the meaning of greater than A and less than B, and also includes the meaning of "preferably greater than A" and "preferably smaller than B".

[0025] Figure 1The figure is a three-dimensional diagram schematically showing a battery stack 500 according to an embodiment. The battery stack 500 includes a plurality of storage cells 100 and a restraint mechanism 300. In addition, for the convenience of explanation, although not shown in the figure, the plurality of storage cells 100 of the battery stack 500 are electrically connected by a busbar. It should be noted that in the following description, the marks L, R, F, Rr, U, and D in the drawings represent left, right, front, rear, top, and bottom, and the marks X, Y, and Z in the drawings represent the short side direction (thickness direction) of the storage cell 100, the long side direction (width direction) orthogonal to the short side direction, and the up and down direction. The short side direction X is also the arrangement direction of the storage cell 100. However, these are just directions for the convenience of explanation, and there is no limitation on the setting form of the battery stack 500.

[0026] The restraint mechanism 300 is configured to apply a predetermined restraint pressure to the plurality of power storage cells 100 in the thickness direction X. The restraint mechanism 300 is composed of a pair of end plates 310, a pair of side plates 320, and a plurality of screws 330. The pair of end plates 310 are arranged in a predetermined thickness direction X. The pair of end plates 310 are arranged at both ends of the battery stack 500 in the thickness direction X. The plurality of power storage cells 100 are arranged between the pair of end plates 310 along the thickness direction X. An insulating sheet, an inter-cell separator, etc. may be arranged between the plurality of power storage cells 100.

[0027] A pair of side plates 320 bridges a pair of end plates 310. The pair of side plates 320 are fixed to the end plates 310 by a plurality of screws 330, for example, in such a manner that the restraint load is about 5 to 20 kN. Thus, a restraint load is applied to the plurality of power storage cells 100 in the thickness direction X, and the battery stack 500 is held integrally. However, the restraint mechanism is not limited thereto. For example, the restraint mechanism 300 may be provided with a plurality of restraint belts, terminal strips, etc. instead of the side plates 320.

[0028] <Power Storage Unit 100>

[0029] In this specification, "power storage unit" refers to a device that can be repeatedly charged and discharged. In addition to batteries generally referred to as lithium-ion batteries and lithium secondary batteries, power storage units include lithium polymer batteries, lithium-ion capacitors, etc. Secondary batteries refer to all batteries that can be repeatedly charged and discharged with the movement of charge carriers between positive and negative electrodes. Here, as one form of power storage unit, a lithium-ion secondary battery can be exemplified.

[0030] Figure 2 1 is a perspective view of the power storage unit 100. Figure 1 , Figure 2 As shown, the plurality of power storage cells 100 are arranged in the thickness direction X so that first side walls 12 b described later face each other. Figure 3 For along Figure 2 A schematic longitudinal cross-sectional view of line III-III. Figure 3 As shown, the power storage unit 100 includes a case 10, a wound electrode body 20, a non-aqueous electrolyte (not shown), a positive electrode terminal 30, a negative electrode terminal 40, a positive electrode collector 50, and a negative electrode collector 60. The power storage unit 100 is a lithium ion secondary battery.

[0031] The housing 10 is a frame that accommodates the wound electrode body 20 and the non-aqueous electrolyte. Figure 2 As shown in FIG. 1 , the housing 10 has a flat rectangular parallelepiped (square) shape with a bottom. The material of the housing 10 can be the same as the material used in the past, and there is no particular limitation. The housing 10 is preferably made of metal, for example, more preferably made of aluminum, aluminum alloy, iron, iron alloy, etc. Figure 2 As shown, the housing 10 includes an outer body 12 having an opening 12h and a sealing plate (lid) 14 that seals the opening 12h. As in the present embodiment, the housing 10 preferably includes an outer body 12 having an opening 12h and a sealing plate 14 that seals the opening 12h.

[0032] like Figure 2 As shown, the outer body 12 includes: a bottom 12a, a pair of first side walls 12b extending from the bottom 12a and opposite to each other, and a pair of second side walls 12c extending from the bottom 12a and opposite to each other. The bottom 12a is roughly rectangular. The bottom 12a is opposite to the opening 12h. The first side wall 12b is flat. The first side wall 12b extends from the long side of the bottom 12a. The second side wall 12c extends from the short side of the bottom 12a. When viewed from above, the area of ​​the first side wall 12b is larger than the area of ​​the second side wall 12c.

[0033] The sealing plate 14 is mounted on the outer body 12 in a manner that plugs the opening 12h of the outer body 12. The sealing plate 14 is opposite to the bottom 12a of the outer body 12. The sealing plate 14 is substantially rectangular when viewed from above. The housing 10 is integrated by joining the sealing plate 14 to the periphery of the opening 12h of the outer body 12 (preferably by welding). The housing 10 is hermetically sealed (sealed).

[0034] like Figure 3 As shown, the sealing plate 14 is provided with an injection hole 15, a discharge valve 17 and two terminal lead holes 18, 19. The injection hole 15 is used to inject the non-aqueous electrolyte after the sealing plate 14 is installed on the outer body 12. The injection hole 15 is sealed with a sealing member 16. The discharge valve 17 is configured to break when the pressure in the housing 10 becomes above a specified value, and the gas in the housing 10 is discharged to the outside. The terminal lead holes 18, 19 penetrate the sealing plate 14 in the up and down direction Z. The terminal lead holes 18, 19 each have an inner diameter of a size that can be inserted through the positive terminal 30 and the negative terminal 40 before being installed on the sealing plate 14 (before riveting).

[0035] The non-aqueous electrolyte can be the same as before and is not particularly limited. The non-aqueous electrolyte contains a non-aqueous solvent and a supporting salt (electrolyte salt). The non-aqueous electrolyte may further contain additives as needed. The non-aqueous solvent, for example, contains carbonates such as ethylene carbonate, dimethyl carbonate, and ethyl methyl carbonate. The non-aqueous solvent preferably contains carbonates. In particular, it is preferred to contain cyclic carbonates and chain carbonates. The supporting salt is, for example, a fluorine-containing lithium salt such as lithium hexafluorophosphate (LiPF6). As additives that can be contained in the non-aqueous electrolyte, for example, a film former, a gas generator, a dispersant, a thickener, etc. can be used. As the film forming agent, for example, there can be listed carbonate compounds such as vinylene carbonate (VC), vinyl ethylene carbonate (VEC), fluoroethylene carbonate (FEC), chloroethylene carbonate, and methyl phenyl carbonate; lithium salts with oxalic acid complex as anion such as lithium bis(oxalato)borate (LiBOB), lithium difluoro(oxalato)borate (LiFOB), and lithium difluorobis(oxalato)phosphate (LPFO);

[0036] The positive electrode terminal 30 is disposed at an end portion ( Figure 2 , Figure 3 The negative terminal 40 is arranged at the end of the sealing plate 14 on the other side in the longitudinal direction Y ( Figure 2 , Figure 3 The right end of Figure 3 As shown, the positive terminal 30 and the negative terminal 40 are inserted through the terminal lead holes 18 and 19 and extend from the inside of the sealing plate 14 to the outside. The positive terminal 30 and the negative terminal 40 are fixed to the sealing plate 14. The positive terminal 30 and the negative terminal 40 are riveted to the peripheral portion of the sealing plate 14 surrounding the terminal lead holes 18 and 19 by riveting. At the end ( Figure 3 The lower end portion of the rivet portion 30c, 40c is formed.

[0037] like Figure 3 As shown, the positive electrode terminal 30 is inside the outer casing 12 and is connected to the positive electrode 22 (see Figure 6 The negative electrode terminal 40 is electrically connected to the negative electrode 24 (see Figure 6 The positive terminal 30 is insulated from the sealing plate 14 by an internal insulating member 80 and a gasket 90. The negative terminal 40 is insulated from the sealing plate 14 by an internal insulating member 80 and a gasket 90.

[0038] On the outer surface of the sealing plate 14, a plate-shaped positive electrode external conductive member 32 and a negative electrode external conductive member 42 are installed. The positive electrode external conductive member 32 is electrically connected to the positive electrode terminal 30. The negative electrode external conductive member 42 is electrically connected to the negative electrode terminal 40. The positive electrode external conductive member 32 and the negative electrode external conductive member 42 are components with busbars etc. that electrically connect the plurality of storage cells 100 to each other. The positive electrode external conductive member 32 and the negative electrode external conductive member 42 are insulated from the sealing plate 14 by an external insulating member 92. In addition, in Figure 1 Although not shown in the figure, when the battery stack 500 is used, the adjacent storage cells 100 are electrically connected. For example, among the adjacent storage cells 100, the positive electrode external conductive member 32 of one storage cell 100 is electrically connected to the negative electrode external conductive member 42 of another storage cell 100 by a bus bar or the like. Thus, the battery stack 500 is electrically connected. The connection of the battery stack 500 may be a series connection or a parallel connection, and may also be a so-called multi-series multi-parallel connection that combines series and parallel connections.

[0039] Figure 4 The three-dimensional diagram schematically shows the wound electrode bodies 20 mounted on the sealing plate 14. The wound electrode bodies 20 include three wound electrode bodies 20. However, the number of electrode bodies arranged inside one outer body 12 is not particularly limited, and may be one or more (two or more). The wound electrode bodies 20 are electrically connected in parallel. The wound electrode bodies 20 are arranged on the winding axis WL (see Figure 6 ) is arranged inside the outer casing 12 in a direction roughly parallel to the long side direction Y. The wound electrode bodies 20 are arranged side by side in a direction (short side direction X) that coincides with the thickness direction of the wound electrode bodies 20 in the thickness direction of the storage cell 100 (in other words, a direction roughly perpendicular to the first side wall 12b of the casing 10). The wound electrode bodies 20 preferably have a flat outer shape. The end surface of the wound electrode body 20 that is orthogonal to the winding axis WL (in other words, the stacking surface where the positive electrode 22 and the negative electrode 24 are stacked) is opposite to the second side wall 12c. In addition, although not shown in the figure, an insulating sheet is arranged between the wound electrode body 20 and the outer casing 12.

[0040] Figure 5 Schematically showing a three-dimensional view of the wound electrode body 20. In addition, the wound electrode body 20 contained in the case 10 can have the same structure. The wound electrode body 20 has a pair of curved portions (R portions) 20r and a flat portion 20f connecting the pair of curved portions 20r. Figure 5 The bent portion 20r of the upper side of the sealing plate 14 is opposite to the other side ( Figure 5The bent portion 20r (lower side) is opposite to the bottom 12a of the outer casing 12. The flat portion 20f is opposite to the first side wall 12b of the outer casing 12. The flat portions 20f of the plurality of wound electrode bodies 20 adjacent to each other in the short side direction X are opposite to each other.

[0041] Figure 6 Schematic diagram showing the structure of the wound electrode body 20. The wound electrode body 20 includes a positive electrode 22, a negative electrode 24, and a separator 26. The wound electrode body 20 is formed by stacking a strip-shaped positive electrode 22 and a strip-shaped negative electrode 24 via a strip-shaped separator 26, and winding in the longitudinal direction with a winding axis WL as the center. The winding axis WL direction is a direction substantially parallel to the longitudinal direction Y.

[0042] like Figure 6 As shown, the positive electrode 22 has a positive electrode core 22c, and a positive electrode active material layer 22a and a positive electrode protective layer 22p fixed on the surface of at least one of the positive electrode cores 22c. However, the positive electrode protective layer 22p is not necessary and can be omitted in other embodiments. The positive electrode core 22c is strip-shaped. The positive electrode core 22c is preferably a metal foil, more preferably composed of aluminum foil or aluminum alloy foil. The positive electrode core 22c is aluminum foil here. The number of layers of the positive electrode 22 is preferably 30 or more.

[0043] At one end portion ( Figure 6 A plurality of positive electrode tabs 22t are provided at the left end portion of the longitudinal direction Y. Figure 6 The plurality of positive electrode tabs 22t protrude in the longitudinal direction Y relative to the separator 26. The positive electrode tab 22t is a part of the positive electrode core 22c and is made of metal foil (aluminum foil). The thickness of the positive electrode core 22c is not particularly limited, but is preferably 5 to 30 μm, and more preferably 10 to 25 μm. Figure 3 to Figure 6 As shown, a plurality of positive electrode sheets 22t are arranged at one end portion ( Figure 3 to Figure 6 The positive electrode sheet group 23 is stacked at the left end of the positive electrode sheet 50 to form the positive electrode sheet group 23. The positive electrode sheet group 23 is electrically connected to the positive electrode terminal 30 via the positive electrode collector 50.

[0044] like Figure 6As shown, the positive electrode active material layer 22a is arranged in a strip shape along the length direction of the positive electrode core 22c. The positive electrode active material layer 22a contains a positive electrode active material that can reversibly absorb and release charge carriers. As a positive electrode active material, for example, a lithium transition metal composite oxide can be listed. The positive electrode active material layer 22a may contain any component other than the positive electrode active material, such as various additives such as a binder and a conductive material. As an additive, it is preferred to include a conductive material and a binder. As a binder for the positive electrode active material layer 22a, for example, polyvinylidene fluoride (PVdF) and the like can be listed. As a conductive material used in the positive electrode active material layer 22a, there is no particular limitation, and a carbon material is preferably used. The density of the positive electrode active material layer 22a is preferably 3.0 g / cc or more, preferably 3.5 g / cc or more. On the other hand, the density of the positive electrode active material layer 22a is preferably 3.7 g / cc or less.

[0045] like Figure 6 As shown, the positive electrode protection layer 22p is provided at the boundary portion between the positive electrode core 22c and the positive electrode active material layer 22a in the long side direction Y. The positive electrode protection layer 22p is provided in a strip shape along the positive electrode active material layer 22a. The positive electrode protection layer 22p includes an inorganic filler (e.g., alumina). The positive electrode protection layer 22p may include any component other than the inorganic filler, such as a conductive material, a binder, various additives, etc.

[0046] like Figure 6 As shown, the negative electrode 24 has a negative electrode core 24c and a negative electrode active material layer 24a fixed on the surface of at least one of the negative electrode cores 24c. The negative electrode core 24c is in a strip shape. The negative electrode core 24c is preferably a metal foil, more preferably a copper foil or a copper alloy foil. The negative electrode core 24c is a copper foil.

[0047] At one end portion ( Figure 6 A plurality of negative electrode tabs 24t are provided at the right end of the long side direction Y. Figure 6 The plurality of negative electrode tabs 24t protrude in the longitudinal direction Y relative to the separator 26. The negative electrode tab 24t is a part of the negative electrode core 24c and is made of metal foil (copper foil). The thickness of the negative electrode core 24c is not particularly limited, but is preferably 5 to 30 μm, and more preferably 5 to 15 μm. Figure 3 to Figure 6 As shown, a plurality of negative electrode tabs 24t are arranged at one end portion ( Figure 3 to Figure 6 The negative electrode sheet group 25 is stacked at the right end of the positive electrode sheet group 23 to form the negative electrode sheet group 25. The negative electrode sheet group 25 is arranged at a position symmetrical to the positive electrode sheet group 23 in the long side direction Y. The negative electrode sheet group 25 is electrically connected to the negative terminal 40 via the negative electrode collector 60.

[0048] like Figure 6As shown, the negative electrode active material layer 24a is arranged in a strip shape along the length direction of the negative electrode core 24c. The negative electrode active material layer 24a contains a negative electrode active material that can reversibly absorb and release charge carriers. As the negative electrode active material, for example, graphite, silicon-based materials (materials containing silicon) and their mixed oxides are preferably used. The negative electrode active material layer 24a may contain any component other than the negative electrode active material, such as various additives such as binders, thickeners, and dispersants. As a binder for the negative electrode active material layer 24a, for example, styrene butadiene rubber (SBR), carboxymethyl cellulose (CMC), etc. can be listed. As a conductive material for the negative electrode active material layer 24a, there is no particular limitation, and carbon materials are preferably used. The density of the negative electrode active material layer 24a is preferably 1.3g / cc or more, and more preferably 1.4g / cc or more. On the other hand, the density of the negative electrode active material layer 24a is preferably 1.7g / cc or less.

[0049] The length Ln of the width direction Y of the negative electrode active material layer 24a is the same as or longer than the length La of the width direction Y of the positive electrode active material layer 22a. Among them, the length Ln of the width direction Y of the negative electrode active material layer 24a is preferably 20 cm or more. Specifically, as will be described later, according to this configuration, it is possible to appropriately control the extrusion of the non-aqueous electrolyte in the wound electrode body 20 to the outside of the wound electrode body 20. In addition, when the length of the direction perpendicular to the winding axis WL direction of the wound electrode body 20 and perpendicular to the thickness direction X of the wound electrode body 20 (here, the Z direction) is set as the height T of the wound electrode body 20, the ratio (Ln / T) of the length Ln of the width direction of the negative electrode active material layer 24a to the height T of the wound electrode body 20 (hereinafter also referred to as the "electrode body aspect ratio") is preferably 2.8 to 3.2. According to this configuration, it is possible to appropriately control the extrusion of the non-aqueous electrolyte in the wound electrode body 20 to the outside of the wound electrode body 20. In the specification, “the height T of the wound electrode body 20” refers to the height T of the wound electrode body 20 from one side ( Figure 5 The uppermost end of the bent portion 20r of the U side) is connected to the other ( Figure 5 The distance from the lowermost end of the curved portion 20r on the D side).

[0050] The separator 26 is a member that insulates the positive electrode active material layer 22a of the positive electrode 22 from the negative electrode active material layer 24a of the negative electrode 24. The separator 26 constitutes the outer surface of the wound electrode body 20. The length Ls of the long side direction Y of the separator 26 is the same as or longer than the length Ln of the long side direction Y of the negative electrode active material layer 24a. As for the separator 26, a heat-resistant layer containing ceramic particles and a binder may be formed on at least one surface. In addition, an adhesive layer containing a binder may be formed on at least one surface of the separator 26. When viewed from above, the adhesive layer may be formed in a shape such as dots, stripes, corrugations, bands (stripes), dotted lines, or a combination thereof.

[0051] The separator 26 is preferably a sheet-like member of a microporous film. The separator 26 is preferably made of a polyolefin resin. As the polyolefin resin, for example, polyethylene (PE), polypropylene (PP), or a mixture thereof can be used.

[0052] There is no particular limitation on the thickness of the separator 26. When the separator 26 does not contain a non-aqueous electrolyte, the thickness of the separator 26 is preferably about 10 to 30 μm. In addition, the "thickness of the separator 26" in this specification means the thickness including the adhesive layer and the heat-resistant layer when the separator 26 has an adhesive layer and a heat-resistant layer, and unless otherwise specified, it means the thickness before the press molding process.

[0053] like Figure 3 As shown, the positive electrode collector 50 constitutes a conductive path that electrically connects the positive electrode sheet group 23 composed of a plurality of positive electrode sheets 22t to the positive electrode terminal 30. The positive electrode collector 50 includes a positive electrode first collector 51 and a positive electrode second collector 52. The positive electrode first collector 51 is installed on the inner surface of the sealing plate 14. The positive electrode second collector 52 extends along the second side wall 12c of the outer body 12. Figure 3 to Figure 5 As shown, the positive electrode second current collecting portion 52 is attached to the wound electrode body 20 .

[0054] like Figure 3 As shown, the negative electrode collector 60 constitutes a conductive path that electrically connects the negative electrode sheet group 25 composed of a plurality of negative electrode sheets 24t to the negative electrode terminal 40. The negative electrode collector 60 includes a negative electrode first collector 61 and a negative electrode second collector 62. The configuration of the negative electrode first collector 61 and the negative electrode second collector 62 may be the same as the positive electrode first collector 51 and the positive electrode second collector 52 of the positive electrode collector 50.

[0055] <Method of Manufacturing Battery Stack 500>

[0056] Figure 71 is a flowchart showing a manufacturing method of a battery stack 500 according to an embodiment. The battery stack 500 disclosed herein can be manufactured by a manufacturing method including a preparation step S10 and a stacking step S20, and is characterized in that the preparation step S10 is performed. In addition, in the manufacturing method of the battery stack 500 disclosed herein, in addition to the above-mentioned steps, other steps may be included at any stage, and the manufacturing process other than the steps may be the same as before.

[0057] (Preparation Step S10)

[0058] In the preparation step S10, the electricity storage cell 100 including the wound electrode body 20, the nonaqueous electrolyte, and the case 10 is prepared. In the preparation step S10, the electricity storage cell 100 may be purchased and prepared, or the electricity storage cell 100 may be manufactured and prepared.

[0059] The storage cell 100 prepared in the preparation step S10 is characterized in that the storage cell 100 is provided with a plurality of layers in the thickness direction ( Figure 1 A load is applied to the storage unit 100 at a speed of 0.1 mm / min until 2.0 MPa is applied, and the load is reduced to 0.01 MPa after the application as one cycle. When the treatment is performed for three cycles, the change in the thickness X3 of the storage unit 100 when 2.0 MPa is applied in the third cycle relative to the thickness X1 of the storage unit 100 when 2.0 MPa is applied in the first cycle ((X1-X3) / X1×100) (hereinafter also referred to as "cell thickness change") is 0.051 to 0.055%. In addition, the "cell thickness change" in this specification is obtained by measurement using Autograph (precision universal testing instrument).

[0060] For example, when each storage cell 100 has a deviation in the ease of extrusion of the non-aqueous electrolyte in the wound electrode body 20 (i.e., when the cell thickness variation is large), in other words, when the thickness (thickness in the X direction) of the storage cell 100 has a deviation, the stacking (assembly) of the storage cell 100 becomes difficult in the subsequent stacking step S20. The thickness of the storage cell 100 varies, for example, depending on the thickness of the wound electrode body 20. Specifically, the thickness of the wound electrode body 20 is determined by the ease of extrusion of the non-aqueous electrolyte present in the wound electrode body 20 when the wound electrode body 20 is squeezed in the thickness direction X of the wound electrode body. In other words, it is determined by the amount of the non-aqueous electrolyte in the wound electrode body 20 after the above squeezing.

[0061] Figure 8 It is a schematic diagram for explaining the change in thickness of the wound electrode body 20 . Figure 8 In FIG. 1 , a portion of the wound electrode body 20 is partially enlarged. Figure 8 (A) shows a wound electrode body 20 containing less non-aqueous electrolyte. Figure 8 (B) shows a wound electrode body 20 containing a large amount of non-aqueous electrolyte. Figure 8 (C) shows a wound electrode body 20 having a large amount of non-aqueous electrolyte and a non-aqueous electrolyte layer 28. The non-aqueous electrolyte in the wound electrode body 20 may be present, for example, inside the separator 26. When the non-aqueous electrolyte is present inside the separator 26, the thickness of the separator 26 becomes thicker due to the presence of the non-aqueous electrolyte, and the thickness of the wound electrode body 20 changes. Figure 8 As shown in FIG. 1 , the thickness of the separator 26 is different when the nonaqueous electrolyte is high or low, and the thickness of the wound electrode body 20 is different accordingly. Figure 8 As shown in (C), the nonaqueous electrolyte layer 28 may be present between the separator 26 and the positive electrode active material layer 22a, or between the separator 26 and the negative electrode active material layer 24a. Figure 8 As shown in (C), when the nonaqueous electrolyte layer 28 is present in the wound electrode body 20 , the thickness of the wound electrode body 20 is further increased.

[0062] On the other hand, in order to make the thickness of the storage cell 100 constant (suppress the variation), it is considered to make it difficult for the non-aqueous electrolyte to be squeezed out of the wound electrode body 20 (that is, to reduce the variation of the cell thickness). In other words, it is considered to make the thickness of the storage cell 100 constant by leaving a large amount of non-aqueous electrolyte inside the wound electrode body 20. However, when a large amount of non-aqueous electrolyte remains excessively inside the wound electrode body 20, when the battery stack 500 is used, the expansion of the storage cells 100 stacked in the battery stack 500 due to charge and discharge becomes large.

[0063] Therefore, the technology disclosed herein is characterized in that a storage cell 100 having a cell thickness variation of 0.051 to 0.055% is prepared. In the storage cell 100 having this structure, the thickness variation of each storage cell 100 is suppressed in the stage of the preparation step S10, so the storage cell 100 can be easily stacked (assembled) in the stacking step S20. On the other hand, the storage cell 100 having a cell thickness variation within the above range suppresses the expansion of the storage cell 100 caused by charging and discharging. Therefore, when the battery stack 500 is constructed, the thickness variation of the storage cell 100 is suppressed, and when the battery stack 500 is used, it is possible to provide a battery stack 500 with a stable thickness of the storage cell 100.

[0064] Fig. 9 Schematic diagram for explaining the measurement of the cell thickness variation in the preparation step S10. Fig. 9In FIG. 1 , the direction in which the load is applied by Autograph 600 in the thickness direction of the storage cell 100 is indicated by a white arrow. Fig. 9 As shown in FIG. 1 , first, the power storage cell 100 is placed on the Autograph 600 in such a manner that a load is applied in the thickness direction (the direction of the white arrow). Fig. 9 As shown, the pair of first side walls 12b of the storage cell 100 are arranged in abutment with the Autograph 600. When the storage cell 100 is viewed in the horizontal direction, the load generated by the Autograph 600 is applied to the flat portion 20f of the wound electrode body 20. Figure 3 The storage cell 100 is set in Autograph600 in a manner that a load is applied to the portion represented by the imaginary line. Furthermore, a load is applied to the storage cell 100 at a speed of 0.1 mm / min in the thickness direction of the storage cell 100 (illustrated by a white arrow). When the load reaches 2 MPa, the thickness of the storage cell 100 is measured using a displacement meter (not shown), and the thickness is set to X1. Then, the load on the storage cell 100 is reduced to 0.01 MPa. The above-mentioned cycle is regarded as 1 cycle, and this treatment is performed for 3 cycles. Then, the thickness of the storage cell 100 when the load reaches 2 MPa in the third cycle is set to X3. Then, according to the following formula (i), the change in cell thickness (%) is calculated.

[0065] Unit thickness change (%) = (X1-X3) / X1×100···Formula (i)

[0066] There is no particular limitation on the means for measuring the thickness displacement of the storage cell 100. For example, a laser displacement meter (e.g., manufactured by KEYENCE Co., Ltd., product name IL-S025) or the like can be used. In addition, the thickness of the storage cell 100 may be measured at one location or at multiple locations (two or more). When the thickness of the storage cell 100 is measured at multiple locations, X1 and X3 can be obtained by calculating the average value from the measured values ​​at the multiple locations.

[0067] In the preparation step S10, the storage cell 100 having a cell thickness variation value ranging from 0.051 to 0.055% can be prepared. By measuring the cell thickness variation value using the method described in the preparation step S10, it can be confirmed that the cell thickness variation value of the storage cell 100 is within the range of 0.051 to 0.055%.

[0068] (Lamination Step S20)

[0069] In the stacking step S20, a plurality of storage cells 100 are stacked along the thickness direction X of the storage cells 100. The stacking step S20 may be the same as a conventionally known method for manufacturing a battery stack. The plurality of storage cells 100 are clamped in the arrangement direction X by a pair of end plates 310 and restrained by side plates 320 and a plurality of screws 330. In this way, the battery stack 500 of this embodiment is manufactured.

[0070] <Method of Manufacturing Power Storage Cell 100>

[0071] Although not particularly limited, the electric storage cell 100 in the preparation step S10 can be prepared by, for example, the manufacturing method described below. The manufacturing method of the electric storage cell 100 described below is an example of the preparation step S10 in this specification. Fig.10 FIG. 1 is a flowchart showing a method for manufacturing the power storage unit 100 according to one embodiment. Fig.10 As shown, although not particularly limited, the storage cell 100 can be manufactured by a manufacturing method that typically includes, in sequence, an assembling step S101, a drying step S102, a liquid injection step S103, an exhaust charging step S104, a decompression step S105, a liquid injection hole sealing step S106, an activation step S107, and an aging step S108. In addition, in the manufacturing method of the storage cell 100 disclosed herein, in addition to the above-mentioned steps, other steps may be included in any stage, and the manufacturing process other than the above steps may be the same as in the past.

[0072] (Assembly process S101)

[0073] In the assembly step S101, the wound electrode body 20 is placed in the case 10 (external body 12) to prepare an assembly. In this specification, the "assembly" refers to the power storage unit assembled in a state before the injection hole sealing step described later is performed.

[0074] In the assembly process S101, the positive second collector 52 is installed on the positive electrode sheet group 23 of the wound electrode body 20, and the negative second collector 62 of the negative collector 60 is installed on the negative electrode sheet group 25. Next, the positive terminal 30 and the negative terminal 40 are installed on the sealing plate 14. Next, the positive terminal 30 and the positive first collector 51 and the negative terminal 40 and the negative first collector 61 are respectively joined by a conventionally known method (such as ultrasonic joining, resistance welding, laser welding, etc.). Next, the insulating sheet is accommodated in the wound electrode body 20. The insulating sheet can be prepared, for example, by folding an insulating resin sheet composed of a resin material such as polyethylene (PE) into a bag or box shape. Then, the wound electrode body 20 covered with the insulating sheet is preferably accommodated (inserted) in the internal space of the outer body 12. Then, the outer body 12 of the shell 10 is joined to the sealing plate 14 to make an assembly. The joining can be performed by welding such as laser welding, for example. In the assembly step S101 , the liquid injection hole 15 is not sealed.

[0075] In the assembly step S101, the wound electrode bodies 20 are preferably arranged in parallel in the thickness direction of the storage battery cell 100 (in other words, in the direction substantially perpendicular to the first side wall 12b of the case 10) and in the direction (short side direction X) that coincides with the thickness direction of the wound electrode bodies 20. In other words, the wound electrode bodies 20 are preferably arranged inside the outer casing 12 in such a manner that the winding axis WL is parallel to the bottom 12a of the outer casing 12.

[0076] (Drying process S102)

[0077] In the drying step S102, the assembly is dried to remove moisture contained in the assembly (e.g., the interior of the wound electrode body 20). The drying method can be performed by a known method. For example, the drying step S102 can be performed by transporting the assembly (the case 10 containing the wound electrode body 20) to a drying furnace (not shown) and heating it.

[0078] The drying temperature and drying time in the drying step S102 can be appropriately adjusted according to the amount of water contained in the wound electrode body 20, etc. The drying temperature is not particularly limited as long as it is within the range that can remove the water, and it is preferably dried at a temperature at which the separator 26 of the wound electrode body 20 is not damaged. In addition, the drying step S102 is preferably carried out in a reduced pressure atmosphere. Thereby, the drying time in the drying step S102 can be shortened. However, it is not limited to this, and the drying step S102 can be carried out in an atmospheric pressure atmosphere. Furthermore, in the technology disclosed herein, the drying step S102 is not a necessary step. In several preferred embodiments, the drying step S102 can also be omitted.

[0079] (Liquid injection step S103)

[0080] In the injection process S103, a non-aqueous electrolyte is injected into the shell 10 accommodating the wound electrode body 20 from the injection hole 15 provided in the sealing plate 14. The injection process S103 can be implemented under an atmospheric pressure atmosphere or under a reduced pressure atmosphere. Preferably, it is preferably implemented under a reduced pressure atmosphere. As a result, the impregnation of the non-aqueous electrolyte in the wound electrode body 20 is improved, and the injection process S103 can be performed in a shorter time. In the injection process S103, the non-aqueous electrolyte is injected in an amount that the non-aqueous electrolyte becomes the entirety of the wound electrode body 20. The injection process S103 can appropriately utilize a non-aqueous electrolyte injection device that is previously known. Furthermore, at this time, as a pressurized gas that can be used to pressurize the non-aqueous electrolyte, as in the past, inert gases such as nitrogen (N2), dry air, etc. can be listed. After the injection process S103 is completed, it is preferred to appropriately pressurize and depressurize the shell 10.

[0081] (Exhaust Charging Step S104)

[0082] In the exhaust charging step S104, the assembly is charged. As a result, a film can be formed on the surface of the negative electrode active material layer 24a. Furthermore, by discharging the gas generated during charging and discharging to the outside of the shell 10, the amount of gas generated inside the shell 10 after the injection hole 15 is sealed is reduced, and the gas accumulation in the wound electrode body 20 after the injection hole 15 is sealed can be suppressed. There is no particular limitation on the charging conditions in this step, and it can be the same as the previous manufacturing method. Although there is no particular limitation, for example, the exhaust charging step S104 can be implemented by charging with a current of about 0.05C to 1C at a normal temperature environment (for example, 25°C) until the SOC (State of Charge) becomes about 5% to 20%.

[0083] (Decompression Step S105)

[0084] In the decompression step S105, the gas existing inside the shell 10 (such as air, gas generated in the exhaust charging step S104, etc.) is further discharged to the outside of the shell 10 by decompressing the inside of the shell 10. The decompression step S105 can be the same as the means used in the decompression step in the previous manufacturing method of this type, and the technology disclosed herein is not particularly characterized, and an excessively detailed description is omitted. In addition, in the technology disclosed herein, the decompression step S105 is not a necessary step. In some preferred embodiments, the decompression step S105 can also be omitted.

[0085] (Liquid injection hole sealing step S106)

[0086] In the injection hole sealing step S106, the injection hole 15 of the assembly is sealed. The injection hole sealing step S106 can be the same as the manufacturing method of the previously known storage battery unit 100, and is not particularly limited. Here, the injection hole 15 is sealed by using a metal sealing member 16, and the metal part of the sealing member 16 is welded to the sealing plate 14 (the peripheral portion of the injection hole 15) to seal it. However, the sealing method of the injection hole 15 is not limited to this. Although the illustration is omitted, for example, the injection hole 15 can be sealed with rivets such as blind rivets.

[0087] (Activation Step S107)

[0088] In the activation step S107, the storage cell 100 whose injection hole 15 is sealed in the injection hole sealing step S106 is charged while applying a load in the thickness direction of the storage cell 100. Thus, a film is formed on the surface of the negative electrode active material layer 24a. The activation step S107 is included as an example of the "preparation step S10" in this specification.

[0089] The charging conditions in the activation step S107 are not particularly limited and can be the same as those in the conventional manufacturing method. Although not particularly limited, for example, the activation step S107 can be performed by charging at a current of about 0.05C to 10C at a normal temperature environment (e.g., 25°C) until the SOC (State of Charge) reaches about 20% to 100%.

[0090] In the activation step S107, the load applied to the storage cell 100 is preferably 0.5 to 0.7 MPa. According to this configuration, the cell thickness variation can be further made within a preferred range (0.051 to 0.055%). The method of applying a load to the storage cell 100 is not particularly limited, and a general method that can be used in a conventional method of manufacturing a storage cell can be used. For example, a pair of first side walls 12b of the storage cell 100 are clamped by a restraining plate, and the restraining plate is connected by a bridging member, so that a load can be applied to the storage cell 100.

[0091] (Aging process S108)

[0092] In the aging step S108, the storage cell 100 that has passed the activation step S107 is stored for a predetermined time in a predetermined temperature environment while maintaining the charged state. In this way, a film can be formed more appropriately on the surface of the negative electrode active material layer 24a. In addition, in the technology disclosed herein, the aging step S108 is not a necessary step. In some preferred embodiments, the aging step S108 can also be omitted.

[0093] Furthermore, the conditions of the aging process S108 can be appropriately adjusted according to the desired method of film formation, and are not particularly limited. For example, the unit temperature (aging temperature) in the aging process S108 can be set to above 30°C, preferably above 40°C, for example, above 50°C, and further above 60°C. There is no particular restriction on the upper limit of the aging temperature, for example, about 80°C or less can be used as an indicator. The temperature management in the aging process S108 can use a constant temperature bath, for example. The implementation time (aging time) of the aging process S108 can be appropriately changed according to the aging temperature, for example, and is not particularly limited. For example, when the aging temperature is about 45 to 70°C, the aging time is preferably about 5 to 20 hours. In addition, when the aging temperature is about 70 to 75°C, the aging time is preferably about 5 to 15 hours.

[0094] In the aging step S108, it is preferred to perform aging while applying a load in the thickness direction X of the power storage cell 100. The amount of load applied to the power storage cell in the aging step S108 is not particularly limited, but is preferably 0.5 to 0.7 MPa. In addition, the aging step S108 may be performed while maintaining the load applied in the activation step S107.

[0095] The battery stack 500 can be used for various purposes, for example, it can be suitably used as a power source (driving power source) for a motor mounted on a car, truck, etc. The type of vehicle is not particularly limited, and examples thereof include a plug-in hybrid electric vehicle (PHEV), a hybrid electric vehicle (HEV), and a battery electric vehicle (BEV).

[0096] Hereinafter, examples related to the technology disclosed herein will be described, but these examples are not intended to limit the technology disclosed herein.

[0097] <Preparation of power storage unit>

[0098] First, 100 storage cells for constructing the battery stack according to Example 1 were prepared. The wound electrode bodies contained in the storage cells according to Example 1 were made of Figure 5 The wound electrode body shown has a pair of curved portions, a strip-shaped positive electrode and a strip-shaped negative electrode stacked via a strip-shaped separator and wound in the length direction. In addition, the width (Ln) of the negative electrode active material layer formation region of the storage unit involved in the embodiment is 28 cm, and the electrode body aspect ratio (the ratio of the length Ln of the width direction of the negative electrode active material layer to the height T of the wound electrode body (Ln / T)) is 3.0. In addition, the number of stacked positive electrodes involved in the wound electrode body is 100 layers.

[0099] In addition, as Comparative Example 1, 100 storage cells involved in Comparative Example 1 were prepared in the same manner as the storage cells involved in Example 1, except that the electrode bodies of the so-called stacked structure (i.e., the electrode bodies that are not wound electrode bodies) were stacked in the thickness direction X of the storage cells, the aspect ratio of the electrode bodies was 1.6, the shape of the shell was changed according to the aspect ratio of the electrode bodies, and a load of 0.2 MPa was applied in the thickness direction of the storage cells during the activation process while charging and discharging was performed. Similarly, as Comparative Example 2, 100 storage cells involved in Comparative Example 2 were prepared in the same manner as the storage cells involved in Example 1, except that a load of 0.4 MPa was applied in the thickness direction of the storage cells during the activation process while charging and discharging was performed.

[0100] <Evaluation of cell thickness variation>

[0101] For Example 1, Comparative Example 1 and Comparative Example 2, an average of 3 (i.e., n=3) storage cells were randomly selected for each example. The above-mentioned method was used to evaluate the change in cell thickness. In addition, Autograph used AG-X Plus (Shimadzu Corporation), and two displacement meters for measuring the thickness of the storage cells were set in Autograph. First, as Fig. 9 As shown, the storage cell is set in Autograph. Then, a load is applied in the thickness direction of the storage cell (illustrated by a white arrow) at a speed of 0.1 mm / min. The thickness of the storage cell when the load reaches 2 MPa is measured at 2 points. From the measured values, the average value is calculated and set as X1. Then, the load is reduced to 0.01 MPa. Set as 1 cycle, and perform this treatment for 3 cycles. Then, using the obtained X1 and X3, the change in cell thickness (%) is calculated according to formula (i). The results are shown in Table 1.

[0102] Unit thickness change (%) = (X1-X3) / X1×100···Formula (i)

[0103] [Table 1]

[0104]

[0105] <Evaluation of cell thickness variation>

[0106] Using Autograph, for the storage cells involved in Example 1, Comparative Example 1 and Comparative Example 2, the thickness of the storage cell when a load of 0.2 MPa is applied in the thickness direction of the storage cell is measured. This measurement is performed for every 100 storage cells prepared in each example. The device used in the measurement is the same as that used in the evaluation of the cell thickness change described above. Using the obtained storage cell thickness, the deviation of the storage cell thickness is evaluated according to formula (ii). The results are shown in Table 1. In addition, a coordinate diagram showing the relationship between the cell thickness change and the cell thickness deviation is shown in Table 1. Fig.11 . In addition, Fig.11 For the cell thickness change amount related to each example, the average value of the cell thickness change amount for each power storage cell is plotted.

[0107] Unit thickness deviation δ (%) = standard deviation / average thickness × 100 ···Formula (ii)

[0108] <Evaluation of cell expansion rate caused by charge and discharge>

[0109] Here, the cell expansion rate caused by charging and discharging was evaluated for the storage cells involved in Example 1 and Comparative Examples 1 to 2. Specifically, first, for the three storage cells involved in Example 1 and Comparative Examples 1 to 2 that were used for the evaluation of the cell thickness change, the thickness of the storage cell when a load of 0.2 MPa was applied in the thickness direction of the storage cell was measured, and this was set as the cell thickness before the test. The storage cells involved in Example 1 and Comparative Examples 1 to 2 were placed in a temperature environment of 40°C, and charged and discharged at a current rate of 1 / 5C in the range of SOC of 0 to 100%. This operation was regarded as one cycle, and this operation was repeated 1000 times. Then, for the storage cells that were charged and discharged for 1000 cycles, the thickness of the storage cell after the test when a load of 0.2 MPa was applied in the thickness direction of the storage cell was measured, and this was set as the cell thickness after the test. Then, the cell expansion rate caused by charging and discharging was evaluated using the following formula (iii). The results are shown in Table 1. In addition, a coordinate diagram showing the relationship between the cell thickness change and the cell expansion rate is shown in Fig.12 . In addition, Fig.12 For the cell thickness change amount related to each example, the average value of the cell thickness change amount for each power storage cell is plotted.

[0110] Cell expansion rate due to charge and discharge (%) = (cell thickness after test - cell thickness before test) / cell thickness before test × 100 ... Formula (iii)

[0111] <Results>

[0112] As can be seen from Table 1, in the storage cell in which the cell thickness variation is within the range of 0.051 to 0.055% as in Example 1, the thickness variation of the storage cell is suppressed and the cell expansion rate after 1000 cycles of charge and discharge is suppressed compared with Comparative Examples 1 and 2. Therefore, in the battery stack in which the storage cells of Example 1 are stacked, since the thickness variation of the storage cells is small, the stacking process can be easily performed, and the thickness variation (expansion) caused by charge and discharge can be suppressed after the battery stack is constructed.

[0113] The preferred embodiment of the present disclosure is described above, and the above embodiment is only an example. The present disclosure can be implemented in various other ways. The present disclosure can be implemented based on the contents disclosed in this specification and the technical common sense in the field. The technology described in the claims includes the technology of variously deforming and changing the above-mentioned exemplified embodiments. For example, part of the above-mentioned embodiment can be replaced by other variations, and other variations can be added to the above-mentioned embodiment. In addition, as long as it is not described as a necessary feature of the technology, it can be appropriately deleted.

[0114] As described above, specific aspects of the technology disclosed herein include aspects described in the following items.

[0115] Item 1: A method for manufacturing a battery stack, a method for manufacturing a battery stack including a plurality of square storage cells, comprising: a preparation step, wherein the storage cells are prepared, wherein the storage cells include: a flat wound electrode body in which a positive electrode and a negative electrode are stacked and wound via a separator, a non-aqueous electrolyte, and a shell for accommodating the wound electrode body and the non-aqueous electrolyte; and a stacking step, wherein a plurality of the storage cells are stacked along a thickness direction of the storage cells, wherein the storage cells prepared in the preparation step are stacked A process in which a load of 2.0 MPa is applied in the thickness direction of the power storage unit at a speed of 0.1 mm / min and then the load is reduced to 0.01 MPa is defined as one cycle. When this process is performed for three cycles, a change ((X1-X3) / X1×100) in the thickness X3 of the power storage unit when 2.0 MPa is applied in the third cycle relative to the thickness X1 of the power storage unit when 2.0 MPa is applied in the first cycle is 0.051 to 0.055%.

[0116] Item 2: A method for manufacturing a battery stack according to Item 1, wherein the negative electrode includes a negative electrode core and a negative electrode active material layer formed on the negative electrode core, and the length Ln of the negative electrode active material layer in the width direction orthogonal to the length direction of the wound electrode body is greater than 20 cm.

[0117] Item 3: A method for manufacturing a battery stack according to Item 2, wherein, when the length in a direction perpendicular to the winding axis direction of the wound electrode body and perpendicular to the thickness direction of the wound electrode body is set as the height T of the wound electrode body, the ratio of the length Ln in the width direction of the negative electrode active material layer to the height T of the wound electrode body (Ln / T) is 2.8 to 3.2.

[0118] Item 4: A method for manufacturing a battery stack according to any one of Items 1 to 3, wherein the preparation step includes: an activation step of charging the power storage unit while applying a load in the thickness direction of the power storage unit, wherein in the activation step, the load applied to the power storage unit is 0.5 to 0.7 MPa.

[0119] Item 5: The method for manufacturing a battery stack according to any one of Items 1 to 4, wherein the number of stacked layers of the positive electrode is 30 or more.

Claims

1. A method for manufacturing a battery stack, which is a method for manufacturing a battery stack including a plurality of square power storage units, comprising: Preparation process, including preparing the electricity storage unit including: a flat-shaped wound electrode body in which a positive electrode and a negative electrode are stacked and wound via a separator, a nonaqueous electrolyte, and a case accommodating the wound electrode body and the nonaqueous electrolyte; and a stacking step, wherein a plurality of the power storage cells are stacked along a thickness direction of the power storage cells; Among them, for the storage battery unit prepared in the preparation process, a load is applied to the thickness direction of the storage battery unit at a speed of 0.1 mm / min until it reaches 2.0 MPa, and the load is reduced to 0.01 MPa after the application as one cycle. When this treatment is performed for 3 cycles, the change in the thickness X3 of the storage battery unit when 2.0 MPa is applied in the third cycle relative to the thickness X1 of the storage battery unit when 2.0 MPa is applied in the first cycle ((X1-X3) / X1×100) is 0.051~0.055%.

2. The method for manufacturing a battery stack according to claim 1, wherein: The negative electrode includes a negative electrode core and a negative electrode active material layer formed on the negative electrode core, and a length Ln of the negative electrode active material layer in a width direction perpendicular to a length direction of the wound electrode body is 20 cm or more.

3. The method for manufacturing a battery stack according to claim 2, wherein: When the length in a direction perpendicular to the winding axis direction of the wound electrode body and perpendicular to the thickness direction of the wound electrode body is defined as the height T of the wound electrode body, the ratio (Ln / T) of the length Ln in the width direction of the negative electrode active material layer to the height T of the wound electrode body is 2.8 to 3.

2.

4. The method for manufacturing a battery stack according to claim 1 or 2, wherein: The preparation step includes an activation step of charging the power storage cell while applying a load in a thickness direction of the power storage cell, wherein the load applied to the power storage cell in the activation step is 0.5 to 0.7 MPa.

5. The method for manufacturing a battery stack according to claim 1 or 2, wherein: The positive electrode has 30 or more layers stacked.