Electrolyte and secondary lithium battery containing same

By using electrolytes with fluorine-free solvents as the main solvent, the problem of matching lithium-ion batteries with high specific capacity cathode materials at high voltages and the environmental pollution of polyfluorinated solvents are solved, achieving high energy density, high power density and long-term operation. Cycle life of lithium batteries.

CN118738566APending Publication Date: 2024-10-01TSINGHUA UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411017161.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Existing lithium-ion batteries are difficult to match the next generation of high-voltage, high-specific-capacity cathode materials at high voltages, and the high production costs and environmental pollution of polyfluorinated solvents limit their applications.

Method used

The electrolyte uses a fluorine-free solvent as the main solvent, including methyl pivalate, ethyl pivalate, etc., combined with lithium salt, co-solvent, and film-forming additives, with a volume fraction of 70% to 100% to reduce the corrosion resistance of the cathode material. Reactive and build stable solid electrolyte membrane.

Benefits of technology

It significantly reduces the decomposition of organic solvents under high voltage conditions, improves the energy density, power density and cycle life of lithium batteries, and reduces the risk of environmental pollution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738566A_ABST
    Figure CN118738566A_ABST
Patent Text Reader

Abstract

The invention provides an electrolyte and a secondary lithium battery containing the same. The electrolyte comprises a fluorine-free solvent as a main solvent. According to the present application, the fluorine-free solvent may be at gt; obvious oxidation does not occur under the high voltage of 5V (vs. Li / Li < + >). Therefore, the electrolyte using the fluoride-free solvent can be matched with a high-voltage high-nickel ternary positive electrode (4.3 V) or a lithium-rich manganese-based positive electrode (4.7 V), and a lithium battery with high energy density and long cycle stability is assembled.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field The present application relates to the field of battery technology, and in particular to an electrolyte and a secondary lithium battery containing the electrolyte. Background Art Secondary batteries represented by lithium-ion batteries are widely used in digital electronic products, energy storage systems, drones, electric vehicles, etc. due to their high energy density, high power density and long cycle life. However, if the "range anxiety" problem of electric vehicles is to be completely solved and further applied to electric ships and electric aircraft, the energy density of lithium batteries must be further developed. However, due to the voltage and specific capacity limitations of the positive electrode, the energy density of traditional lithium batteries has reached a development bottleneck period. Conventional lithium-ion battery solvents do not contain fluorine, such as ethylene carbonate and dimethyl carbonate. Because they have a higher HOMO energy level, they are easily oxidized and decomposed at a voltage higher than 4.3V (vs. Li / Li+), making it difficult to match the next generation of high-voltage, high-specific-capacity high-nickel ternary positive electrode materials or lithium-rich manganese-based positive electrode materials. At present, polyfluorinated solvent molecules have excellent antioxidant ability because of their lower HOMO energy level, and can be well matched with high-voltage positive electrode materials. However, due to the high production cost of polyfluorinated solvents and the large environmental pollution, the practical application of polyfluorinated solvents in high-voltage electrolytes is seriously hindered. Therefore, in order to meet the demand for practical application, it is urgent to propose an electrolyte that includes a cheap, environmentally friendly, and high-voltage stable fluorine-free solvent as the main solvent. Summary of the invention Problem that the invention aims to solve The present application aims to solve the problems of high production cost and serious environmental pollution of existing polyfluorinated solvents by providing an electrolyte comprising a fluorine-free solvent as a main solvent. Solutions for solving problems

[0001] , an electrolyte comprising a lithium salt, a fluorine-free solvent as a main solvent, an optional co-solvent and an optional film-forming additive, wherein the fluorine-free solvent comprises at least one selected from methyl pivalate, ethyl pivalate, methyl 2,2'-dimethylbutyrate, ethyl 2,2'-dimethylbutyrate, α,α'-dimethyl-γ-butyrolactone, α,α'-dimethyl-γ-valerolactone, α,α'-dimethyl-δ-valerolactone, dimethyl 2,2'-dimethylmalonate, and diethyl 2,2'-dimethylmalonate.

[0002] , The electrolyte according to [1], wherein the volume fraction of the fluorine-free solvent in the electrolyte is 70% to 100%, the volume fraction of the co-solvent in the electrolyte is 0% to 30%, and the volume fraction of the film-forming additive in the electrolyte is 0% to 30%.

[0003] , The electrolyte according to [1] or [2], wherein the lithium salt is selected from one or more of lithium bis(trifluoromethanesulfonyl imide), lithium bis(fluorosulfonyl imide), lithium trifluoromethanesulfonate, lithium nitrate, lithium tetrafluoroborate, lithium perchlorate, lithium hexafluorophosphate, lithium difluorooxalatoborate, and lithium dioxalatoborate; and the concentration of the lithium salt in the electrolyte is 0.01 mol / L to 3.0 mol / L.

[0004] , The electrolyte according to [1] or [2], wherein the co-solvent is selected from at least one of dimethyl carbonate, diethyl carbonate, ethyl methyl carbonate, ethylene carbonate, propylene carbonate, trimethyl phosphate, triethyl phosphate, tris(2,2,2-trifluoroethyl) phosphate, cyclopentane sulfone, 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether, bis(2,2,2-trifluoroethyl) ether, 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, and tris(2,2,2-trifluoroethyl)orthoformate.

[0005] , The electrolyte according to [1] or [2], wherein the film-forming additive is selected from at least one of fluoroethylene carbonate, vinylene carbonate, propylene sulfite, trimethyl borate, triethyl borate, tris(trimethylsilyl)borate, trimethyl phosphite, triethyl phosphite, tris(trimethylsilyl)phosphite, tris(trimethylsilyl)phosphate, and triallyl phosphate.

[0006] , a secondary lithium battery comprising: a positive electrode plate, a negative electrode plate, and an electrolyte according to any one of [1] to [5].

[0007] , The secondary lithium battery according to [6], wherein the secondary battery is any one of a lithium metal battery and a lithium ion battery.

[0008] , A secondary lithium battery according to [6] or [7], wherein the active electrode material in the positive electrode plate is any one of lithium iron phosphate, nickel-cobalt-manganese ternary material, nickel-cobalt-aluminum ternary material, lithium cobalt oxide, and lithium-rich manganese-based material.

[0009] , A secondary lithium battery according to [6] or [7], wherein the active electrode material in the negative electrode plate is any one of graphite, metal lithium foil, and silicon / carbon. Effects of the Invention 1. The fluorine-free solvent of the present application exhibits extremely low reactivity to the positive electrode material under high voltage conditions. 2. The use of the fluorine-free solvent electrolyte of the present application can significantly reduce the decomposition of the organic solvent on the surface of the high-voltage positive electrode. 3. The secondary lithium battery containing the electrolyte of the present application has high energy density, high power density and long cycle life. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 1 is a graph showing the LSV test results of the lithium||carbon-coated aluminum foil button cells obtained in Example 1 and Comparative Example 1. Figure 2 This is a graph showing the LSV test results of the lithium||carbon-coated aluminum foil button cells obtained in Example 2 and Comparative Example 2. Figure 3 It is a long cycle performance diagram of a full battery of lithium||lithium-rich manganese-based materials including the electrolytes in Examples 3 and 4 under 1.0C current density conditions. Figure 4 It is a long cycle performance diagram of a full battery of lithium||lithium-rich manganese-based materials including the electrolyte in Example 5 under 1.0C current density conditions. Figure 5 It is a long cycle performance diagram of a full battery of lithium||lithium-rich manganese-based materials including the electrolyte in Example 6 under 1.0C current density conditions. Figure 6 It is a long cycle performance diagram of a full battery of lithium||lithium-rich manganese-based materials including the electrolyte in Example 7 under 1.0C current density conditions. DETAILED DESCRIPTION The various embodiments or implementation schemes in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials, or characteristics described in conjunction with the implementation or examples are included in at least one implementation or example of the present application. In this specification, the schematic representation of the above terms does not necessarily refer to the same implementation or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in any one or more implementations or examples in a suitable manner. In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of this application, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined. As described in the background technology above, the existing commercial lithium-ion batteries are limited by the low operating voltage and low discharge specific capacity of the positive electrode materials. The development of their energy density has reached a bottleneck period and it is difficult to break through 300Wh / kg. In order to match the next generation of high-voltage positive electrode materials, such as high-nickel ternary positive electrode materials and lithium-rich manganese-based positive electrode materials, the development of a new generation of stable electrolytes that can be charged and discharged at high voltage has become a research focus. At present, the strategy to improve the stability of electrolytes to high voltages is often based on polyfluorinated solvents. The reason is that the high electronegativity of fluorine can significantly reduce the HOMO energy level of organic solvent molecules and improve the antioxidant capacity of the molecules. However, the production cost of fluorinated solvents is high, and the environmental pollution problem during the production process is serious. At the same time, fluorinated solvents are difficult to degrade, resulting in fluorinated electrolytes in discarded lithium batteries being potential sources of environmental pollution. Therefore, fluorinated solvents still face many difficult-to-solve problems in terms of practicality and commercialization. Based on the above problems, the present application provides an electrolyte containing a fluorine-free solvent as a main solvent. The fluorine-free solvent can avoid the introduction of fluorine element while ensuring stability at high voltage, thereby effectively solving the above technical problems. The technical solution provided by the present application is described in detail below. In a first aspect, the present application provides an electrolyte comprising a lithium salt, a fluorine-free solvent as a main solvent, an optional co-solvent, and an optional film-forming additive. In some embodiments of the present application, the fluorine-free solvent includes at least one selected from methyl pivalate, ethyl pivalate, methyl 2,2'-dimethylbutyrate, ethyl 2,2'-dimethylbutyrate, α,α'-dimethyl-γ-butyrolactone, α,α'-dimethyl-γ-valerolactone, α,α'-dimethyl-δ-valerolactone, dimethyl 2,2'-dimethylmalonate, and diethyl 2,2'-dimethylmalonate. The present application is based on low-viscosity, low-freezing-point carboxylates for molecular design. The α-oxidation of carboxylic acid derivatives is a common oxidation reaction in organic chemistry, and a key step in the reaction process is the departure of the carbonyl α-H as a proton. Based on this, the fluorine-free solvent provided in the present application has a chemical composition of fluorine-free, α-H-free carboxylates. The fluorine-free solvent uses a hydrocarbon group to replace all carbonyl α positions of the carboxylate. This modification strategy blocks the path of the α-oxidation of ordinary carboxylates to generate more stable oxidation products, thereby eliminating the need to introduce strong electron-withdrawing substituents (such as fluorine, cyano, etc.), and has little effect on the HOMO energy level of the molecule, but greatly increases the oxidation potential of the molecule. Therefore, this type of fluorine-free solvent exhibits extremely low reactivity to positive electrode materials under high voltage conditions. The construction of the positive electrode solid electrolyte membrane (CEI membrane) is crucial to the stability of the high-voltage positive electrode. The high-valent transition metal ions and peroxide and superoxide species in the high-nickel ternary positive electrode material and the lithium-rich manganese-based positive electrode material often undergo an uncontrollable oxidation reaction with the organic solvent in the electrolyte, thereby obtaining a loose CEI membrane rich in organic components. The CEI membrane rich in organic components cannot further inhibit the continuous oxidation and decomposition of organic matter in the electrolyte on the high-voltage positive electrode, resulting in low coulombic efficiency and short cycle life of the lithium battery. Based on this, the use of this type of fluorine-free solvent electrolyte can greatly reduce the decomposition of organic solvents on the surface of high-voltage positive electrodes. The fluorine-free solvent has extremely low reactivity to oxidation reactions, which helps the inorganic salts in the electrolyte to preferentially decompose on the surface of the positive electrode and construct a CEI membrane rich in inorganic components. The CEI membrane rich in inorganic components is tougher and more stable, and can exist stably during the battery cycle, so it can significantly improve the coulombic efficiency and cycle life of lithium batteries. In some embodiments, the volume fraction of the fluorine-free solvent in the electrolyte is 70% to 100%, preferably 90% to 100%; the volume fraction of the co-solvent in the electrolyte is 0% to 30%, preferably 0% to 10%; the volume fraction of the film-forming additive in the electrolyte is 0% to 30%, preferably 0% to 10%. In the present application, the electrolyte may contain only the fluorine-free solvent, or may contain the fluorine-free solvent as the main solvent and other auxiliary solvents at the same time. As long as the fluorine-free solvent is present in the electrolyte as the main solvent in the above-mentioned proportion, it will not affect the technical effect of the present application. In the present application, the main solvent refers to the solvent that accounts for the majority proportion. As mentioned above, the volume fraction of the main solvent in the electrolyte is 70% to 100%. In some embodiments, the lithium salt is selected from one or more of lithium bis(trifluoromethanesulfonyl imide), lithium bis(fluorosulfonyl imide), lithium trifluoromethanesulfonate, lithium nitrate, lithium tetrafluoroborate, lithium perchlorate, lithium hexafluorophosphate, lithium difluorooxalatoborate, and lithium dioxalatoborate; the concentration of the lithium salt in the electrolyte is 0.01 mol / L to 3.0 mol / L, preferably 0.1 mol / L to 2.0 mol / L. It is understandable that the higher the concentration of lithium salt, the more ions can be used for conduction in the obtained electrolyte, the better the ion transport performance, and the higher the degree of anion-cation bonding, the more inclined to form anion-derived inorganic component-rich solid electrolyte membrane on the electrode surface. However, if the concentration of lithium salt is too high, the viscosity of the electrolyte will be too high, which will hinder the conduction of ions and cause the ion transport performance of the obtained electrolyte to deteriorate. Therefore, the concentration of lithium salt in the electrolyte described in the present application is within the above range. In some embodiments, the co-solvent is selected from at least one of dimethyl carbonate, diethyl carbonate, ethyl methyl carbonate, ethylene carbonate, propylene carbonate, trimethyl phosphate, triethyl phosphate, tris(2,2,2-trifluoroethyl) phosphate, cyclopentane, 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether, bis(2,2,2-trifluoroethyl) ether, 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, and tris(2,2,2-trifluoroethyl)orthoformate. In some embodiments, the film-forming additive is selected from at least one of fluoroethylene carbonate, vinylene carbonate, propylene sulfite, trimethyl borate, triethyl borate, tris(trimethylsilyl)borate, trimethyl phosphite, triethyl phosphite, tris(trimethylsilyl)phosphite, tris(trimethylsilyl)phosphate, and triallyl phosphate. Film-forming additives can form a layer of solid electrolyte film on the negative electrode or positive electrode, reduce the energy barrier for lithium ions to cross the electrode-electrolyte interface phase, and reduce the interface impedance. Therefore, polarization can be reduced, the formation of dendrites and huge volume expansion can be inhibited, and the coulombic efficiency and cycle life of the battery can be improved. However, too much film-forming additive will induce uncontrollable interfacial side reactions and may reduce the ionic conductivity of the electrolyte, thereby reducing the coulombic efficiency and cycle life of the battery. Therefore, the volume fraction of the film-forming additive in the electrolyte described in the present application is within the above range. The electrolyte provided in the present application has simple components, and each component can be produced commercially on a large scale. The electrolyte can be prepared by simply mixing each component evenly, so it is very cost-effective for commercial applications and suitable for large-scale production applications. In a second aspect, the present application provides a secondary lithium battery, which includes: a positive electrode plate, a negative electrode plate, and an electrolyte according to the present application. According to the present application, since the secondary lithium battery includes the electrolyte containing a fluorine-free solvent as a main solvent according to any embodiment of the first aspect, it has the beneficial effects of the first aspect. In some embodiments, the secondary battery is any one of a lithium metal battery and a lithium ion battery. In some embodiments, the active electrode material in the positive electrode plate is any one of lithium iron phosphate, nickel cobalt manganese ternary material, nickel cobalt aluminum ternary material, lithium cobaltate, and lithium-rich manganese-based materials. It is understandable that, represented by lithium-rich manganese-based positive electrode active materials, lithium-rich manganese-based positive electrodes have the advantages of high charging voltage (>4.6V), high discharge specific capacity (>250mAh / g), and low cost, and are expected to achieve a breakthrough in the energy density of practical lithium batteries. However, the working potential of the lithium-rich manganese-based positive electrode is too high, and the conventional electrolyte has poor antioxidant capacity, and oxidation side reactions are prone to occur, which significantly reduces the coulombic efficiency and life of the battery. In the present application, the electrolyte of any embodiment of the first aspect has excellent antioxidant capacity and has extremely low reactivity to high-voltage lithium-rich manganese-based positive electrode materials. Therefore, the use of this electrolyte and matching with lithium-rich manganese-based positive electrode materials is expected to achieve the next generation of practical high-specific energy (>500Wh / kg) lithium batteries. In some embodiments, the active electrode material in the negative electrode plate is any one of graphite, metal lithium foil, and silicon / carbon. Hereinafter, the embodiments of the present application will be described. The embodiments described below are exemplary and are only used to explain the present application, and should not be construed as limiting the present application. If no specific techniques or conditions are indicated in the embodiments, the techniques or conditions described in the literature in this area or the product specifications are used. If the manufacturer is not indicated in the reagents or instruments used, they are all conventional products that can be obtained commercially. Example 1 The specific steps for preparing the electrolyte for assembling secondary lithium batteries in an argon glove box (O2, H2O <1ppm) are as follows: (1) Weigh 1.519 g of lithium hexafluorophosphate and dissolve it in 10 mL of methyl pivalate to obtain an electrolyte solution. (2) Take 100 μL of the electrolyte and drip it into a lithium||carbon-coated aluminum foil button cell. The positive electrode shell is a stainless steel shell. The LSV test is performed at a scan rate of 0.1 mV / s in the voltage range of 0 to 7 V. The results are as follows: Figure 1 shown. Example 2 The specific steps for preparing the electrolyte for assembling secondary lithium batteries in an argon glove box (O2, H2O <1ppm) are as follows: (1) Weigh 1.519 g of lithium hexafluorophosphate and dissolve it in 10 mL of ethyl pivalate to obtain an electrolyte solution. (2) Take 100 μL of the electrolyte and drip it into a lithium||carbon-coated aluminum foil button cell. The positive electrode shell is a stainless steel shell. The LSV test is performed at a scan rate of 0.1 mV / s in the voltage range of 0 to 7 V. The results are as follows: Figure 2 shown. Comparative Example 1 The specific steps for preparing the electrolyte for assembling secondary lithium batteries in an argon glove box (O2, H2O <1ppm) are as follows: (1) 1.519 g of lithium hexafluorophosphate was weighed and dissolved in 10 mL of methyl acetate to obtain an electrolyte solution. (2) Take 100 μL of the electrolyte and drip it into a lithium||carbon-coated aluminum foil button cell. The positive electrode shell is a stainless steel shell. The LSV test is performed at a scan rate of 0.1 mV / s in the voltage range of 0 to 7 V. The results are as follows: Figure 1 shown. Comparative Example 2 The specific steps for preparing the electrolyte for assembling secondary lithium batteries in an argon glove box (O2, H2O <1ppm) are as follows: (1) Weigh 1.519 g of lithium hexafluorophosphate and dissolve it in 10 mL of ethyl acetate to obtain an electrolyte solution. (2) Take 100 μL of the electrolyte and drip it into a lithium||carbon-coated aluminum foil button cell. The positive electrode shell is a stainless steel shell. The LSV test is performed at a scan rate of 0.1 mV / s in the voltage range of 0 to 7 V. The results are as follows: Figure 2 shown. according to Figure 1 , 2 The results show that in Comparative Examples 1 and 2, carboxylates containing α-H are used as solvents, and their withstand voltage values ​​are methyl acetate: 3.62V, ethyl acetate: 3.50V, indicating that they are easily decomposed under high voltage and cannot match the high-voltage positive electrode; while after using carboxylates without α-H in Examples 1 and 2, their withstand voltage values ​​can be increased to methyl pivalate: 5.94V, ethyl pivalate: 5.92V, which have the potential to match the high-voltage positive electrode. Example 3 The specific steps for preparing the electrolyte for assembling secondary lithium batteries in an argon glove box (O2, H2O <1ppm) are as follows: (1) Weigh 2.244 g of lithium bis(fluorosulfonyl)imide and 0.576 g of lithium difluorooxalatoborate, and dissolve them in 10 mL of methyl pivalate to obtain an electrolyte solution. (2) Take 100 μL of the above electrolyte and add it dropwise to a lithium||lithium-rich manganese-based positive electrode material full-cell button cell. The positive electrode shell is an aluminum-plated stainless steel shell. After standing at room temperature for 1 hour, the charge and discharge voltage range is controlled to be 2.0-4.6V. The formation is carried out under the conditions of 0.1C, 0.2C, and 0.5C current density. Then, a long cycle test is carried out under the condition of 1.0C current density. The results are as follows: Figure 3 shown. Example 4 The specific steps for preparing the electrolyte for assembling secondary lithium batteries in an argon glove box (O2, H2O <1ppm) are as follows: (1) Weigh 2.244 g of lithium bis(fluorosulfonyl)imide and 0.576 g of lithium difluorooxalatoborate, and dissolve them in 10 mL of methyl pivalate to obtain an electrolyte solution. (2) Take 100 μL of the above electrolyte and drip it into a lithium||lithium-rich manganese-based positive electrode material full-cell button cell. The positive electrode shell is an aluminum-plated stainless steel shell. After standing at room temperature for 1 hour, the charge and discharge voltage range is controlled to be 2.0-4.7V. The formation is carried out under the conditions of 0.1C, 0.2C, and 0.5C current density. Then, a long cycle test is carried out under the condition of 1.0C current density. The results are as follows: Figure 3 shown. Example 5 The specific steps for preparing the electrolyte for assembling secondary lithium batteries in an argon glove box (O2, H2O <1ppm) are as follows: (1) Weigh 2.244 g of lithium bis(fluorosulfonyl)imide and 0.576 g of lithium difluorooxalatoborate, and dissolve them in 10 mL of ethyl pivalate to obtain an electrolyte solution. (2) Take 100 μL of the above electrolyte and add it dropwise to a lithium||lithium-rich manganese-based positive electrode material full-cell button cell. The positive electrode shell is an aluminum-plated stainless steel shell. After standing at room temperature for 1 hour, the charge and discharge voltage range is controlled to be 2.0-4.6V. The formation is carried out under the conditions of 0.1C, 0.2C, and 0.5C current density. Then, a long cycle test is carried out under the condition of 1.0C current density. The results are as follows: Figure 4 shown. according to Figure 3 and Figure 4 It can be seen that Examples 3, 4 and 5 all have good long cycle stability in lithium-rich manganese-metal lithium full batteries with charge cut-off voltages of 4.6V and 4.7V, especially in Examples 3 and 5, when the charge cut-off voltage is selected as 4.6V, the full battery exhibits good stability with almost zero attenuation for more than 300 cycles. This indicates that the fluorine-free solvent-based electrolyte provided in the present application has good antioxidant ability and good stability at high voltage, and can significantly improve the long cycle stability of high-voltage lithium-rich manganese full batteries. Example 6 The specific steps for preparing the electrolyte for assembling secondary lithium batteries in an argon glove box (O2, H2O <1ppm) are as follows: (1) 1.512 g of lithium hexafluorophosphate and 0.288 g of lithium difluorooxalatoborate were weighed and dissolved in a mixed solvent of 7 mL of methyl pivalate and 3 mL of fluoroethylene carbonate to obtain an electrolyte solution. (2) Take 100 μL of the above electrolyte and drip it into a lithium||lithium-rich manganese-based positive electrode material full-cell button cell. The positive electrode shell is a stainless steel shell. After standing at room temperature for 1 hour, the charge and discharge voltage range is controlled to be 2.0-4.6V. The formation is carried out under the conditions of 0.1C, 0.2C, and 0.5C current density. Then, a long cycle test is carried out under the condition of 1.0C current density. The results are as follows: Figure 5 shown. Example 7 The specific steps for preparing the electrolyte for assembling secondary lithium batteries in an argon glove box (O2, H2O <1ppm) are as follows: (1) 0.151 g of lithium hexafluorophosphate, 1.723 g of lithium bis(trifluoromethanesulfonyl)imide and 0.576 g of lithium difluorooxalatoborate were weighed and dissolved in a mixed solvent of 9 mL of methyl pivalate and 1 mL of fluoroethylene carbonate to obtain an electrolyte solution. (2) Take 100 μL of the above electrolyte and add it dropwise to a lithium||lithium-rich manganese-based positive electrode material full-cell button cell. The positive electrode shell is an aluminum-plated stainless steel shell. After standing at room temperature for 1 hour, the charge and discharge voltage range is controlled to be 2.0-4.6V. The formation is carried out under the conditions of 0.1C, 0.2C, and 0.5C current density. Then, a long cycle test is carried out under the condition of 1.0C current density. The results are as follows: Figure 6 shown. Figures 3 to 6 It is shown that, since the fluorine-free solvent of the present application exhibits extremely low reactivity to the positive electrode material under high voltage conditions, the electrolyte using the fluorine-free solvent of the present application can greatly reduce the decomposition of the organic solvent therein on the surface of the high-voltage positive electrode, so that the secondary lithium battery containing the electrolyte of the present application has high energy density, high power density and long cycle life. Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit it. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present application.

Claims

1. An electrolyte comprising a lithium salt, a fluorine-free solvent as a main solvent, an optional co-solvent and an optional film-forming additive, characterized in that The fluorine-free solvent includes at least one selected from methyl pivalate, ethyl pivalate, methyl 2,2'-dimethylbutyrate, ethyl 2,2'-dimethylbutyrate, α,α'-dimethyl-γ-butyrolactone, α,α'-dimethyl-γ-valerolactone, α,α'-dimethyl-δ-valerolactone, dimethyl 2,2'-dimethylmalonate, and diethyl 2,2'-dimethylmalonate.

2. The electrolyte according to claim 1, characterized in that The volume fraction of the fluorine-free solvent in the electrolyte is 70% to 100%, the volume fraction of the auxiliary solvent in the electrolyte is 0% to 30%, and the volume fraction of the film-forming additive in the electrolyte is 0% to 30%.

3. The electrolyte according to claim 1 or 2, characterized in that The lithium salt is selected from one or more of lithium bis(trifluoromethanesulfonyl imide), lithium bis(fluorosulfonyl imide), lithium trifluoromethanesulfonate, lithium nitrate, lithium tetrafluoroborate, lithium perchlorate, lithium hexafluorophosphate, lithium difluorooxalatoborate, and lithium dioxalatoborate; the concentration of the lithium salt in the electrolyte is 0.01 mol / L to 3.0 mol / L.

4. The electrolyte according to claim 1 or 2, characterized in that The cosolvent is selected from at least one of dimethyl carbonate, diethyl carbonate, ethyl methyl carbonate, ethylene carbonate, propylene carbonate, trimethyl phosphate, triethyl phosphate, tris(2,2,2-trifluoroethyl) phosphate, cyclopentane, 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether, bis(2,2,2-trifluoroethyl) ether, 1,1,2,2-tetrafluoroethyl-2,2,2-trifluoroethyl ether, and tris(2,2,2-trifluoroethyl) orthoformate.

5. The electrolyte according to claim 1 or 2, characterized in that: The film-forming additive is selected from at least one of fluoroethylene carbonate, vinylene carbonate, propylene sulfite, trimethyl borate, triethyl borate, tris(trimethylsilyl)borate, trimethyl phosphite, triethyl phosphite, tris(trimethylsilyl)phosphite, tris(trimethylsilyl)phosphate, and triallyl phosphate.

6. A secondary lithium battery, characterized in that: include: A positive electrode sheet, a negative electrode sheet, and an electrolyte according to any one of claims 1 to 5.

7. The secondary lithium battery according to claim 6, characterized in that: The secondary battery is any one of a lithium metal battery and a lithium ion battery.

8. The secondary lithium battery according to claim 6 or 7, characterized in that: The active electrode material in the positive electrode plate is any one of lithium iron phosphate, nickel-cobalt-manganese ternary material, nickel-cobalt-aluminum ternary material, lithium cobalt oxide, and lithium-rich manganese-based material.

9. The secondary lithium battery according to claim 6 or 7, characterized in that: The active electrode material in the negative electrode plate is any one of graphite, metal lithium foil, and silicon / carbon.