Electronic device with improved board-level reliability
Through cobalt-tin double-layer plating technology and the plated copper layer of the die bonding pad, the problems of material property degradation and insufficient heat dissipation at high temperatures of copper integrated circuit leads before welding are solved, improving the reliability of electronic systems. and thermal performance.
Patent Information
- Application Number
- CN202380021725.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-13
- Filing Date
- 2023-03-13
- Publication Date
- 2024-10-01
AI Technical Summary
Copper integrated circuit leads are prone to material property degradation and cracking before welding to printed circuit boards, which affects the board-level reliability of electronic systems. In addition, the heat dissipation performance of electronic devices at high temperatures is insufficient, affecting the stability of the equipment.
Double-layer plating technology of cobalt and tin is used to form a first plating layer and a second plating layer on the conductive leads. The first plating layer contains cobalt and the second plating layer contains tin, and is formed on the package structure. The bottom side is exposed to form a diffusion barrier layer that prevents the mutual diffusion of copper and tin, reduces the formation of intermetallic compounds, and improves fracture toughness and ductility, while a copper layer is plated on the die attachment pad to enhance heat dissipation.
It effectively extends the storage period of copper integrated circuit leads, improves the board-level reliability of electronic systems after welding, reduces the degradation of electronic devices at high temperatures, and enhances operating performance.
Smart Images

Figure CN118743016A_ABST
Abstract
Description
Background Art
[0001] Copper integrated circuit leads can be tinned to mitigate degradation of material properties and extend shelf life before soldering to a printed circuit board. However, tinning of bare copper leads can affect the board level reliability (BLR) of electronic systems due to cracking and material defects at the solder joints of the integrated circuit leads and pads of the printed circuit board. In addition, for compact and more highly integrated systems with smaller features and higher currents, heat dissipation through the die attach structure is important for degradation mitigation and enhanced operation of electronic devices at high temperatures. Summary of the invention
[0002] In one aspect, an electronic device includes a semiconductor die, a package structure enclosing the semiconductor die, and a conductive lead having a first surface and a second surface. The first surface has a double layer exposed along the bottom side of the package structure, and the second surface is exposed along the other side of the package structure. The double layer includes a first plating layer and a second plating layer, the first plating layer is on the first surface of the conductive lead and contacts the first surface of the conductive lead, and the second plating layer is on and contacts the first plating layer and exposed along the bottom side of the package structure, wherein the first plating layer includes cobalt and the second plating layer includes tin.
[0003] In another aspect, a method includes: forming a first plating layer on a first surface of a conductive lead in a panel array of intended electronic devices that is exposed along a bottom side of a molded structure, the first plating layer comprising cobalt; forming a second plating layer on the first plating layer, the second plating layer comprising tin; and separating the electronic device from the panel array, wherein the conductive lead is exposed along a bottom side of a corresponding packaging structure and the second surface of the conductive lead is exposed along a first side of the packaging structure.
[0004] In another aspect, an electronic device includes a semiconductor die, a die attach pad, a plated copper layer, and a packaging structure. The semiconductor die has a side and a metal layer, the metal layer is on the side of the semiconductor die, wherein the metal layer includes nickel. The die attach pad has an opening, and the semiconductor die is attached to the die attach pad, wherein the side of the semiconductor die faces the opening of the die attach pad. The plated copper layer extends over and contacts the metal layer, and the plated copper layer extends from the metal layer in the opening of the die attach pad in a direction away from the semiconductor die, and the packaging structure encloses a portion of the semiconductor die.
[0005] In another aspect, a method includes: attaching a semiconductor die to a die attach pad, wherein a metal layer along a side of the semiconductor die faces an opening of the die attach pad, the metal layer including nickel; and forming a package structure that encloses a portion of the semiconductor die and exposes the opening of the die attach pad. The method further includes: performing an electroless plating process that forms a plated copper layer on and in contact with the metal layer on the side of the semiconductor die, the plated copper layer extending from the metal layer in a direction away from the semiconductor die in the opening of the die attach pad; and performing a package separation process that separates the electronic device from the panel array. BRIEF DESCRIPTION OF THE DRAWINGS
[0006] Figure 1 A perspective view of an electronic device.
[0007] Figure 1A for Figure 1 A bottom view of an electronic device.
[0008] Figure 1B for Figure 1 and 1A A partial cross-sectional side view of an electronic device.
[0009] Figure 2 A flow chart of a method for manufacturing an electronic device.
[0010] Figure 3-8 Based on experience Figure 2 Method of manufacturing a process Figure 1-1B A partial cross-sectional side view of an electronic device.
[0011] Fig. 9 A perspective view of an electronic device.
[0012] Fig.9A for Fig. 9 A bottom view of an electronic device.
[0013] Fig. 9B for Fig. 9 and 9A Cross-sectional side view of an electronic device.
[0014] Fig.10 A flow chart of a method for manufacturing an electronic device.
[0015] Figure 11-18 Based on experience Fig.10 Method of manufacturing a process Figure 9-9B A partial cross-sectional side view of an electronic device. DETAILED DESCRIPTION
[0016] In the drawings, like reference numerals refer to like elements throughout, and the various features are not necessarily drawn to scale. Also, the term "couple" or "couples" includes indirect or direct electrical or mechanical connections, or a combination thereof. For example, if a first device is coupled to or coupled with a second device, the connection may be a direct electrical connection, or may be an indirect electrical connection via one or more intervening devices and connections.
[0017] Figure 1-1B An electronic device 100 is presented having copper leads plated after molding with cobalt and tin to improve BLR performance by electroplating cobalt with minimized defects and larger grain size, which provides a diffusion barrier layer that prevents interdiffusion of copper and tin. Since cobalt and copper have very low solubility in each other, the formation of intermetallic compounds (IMCs) such as Cu3Sn and Cu6Sn5 is slowed, resulting in higher BLR performance. In addition, the cobalt-tin intermetallic compound has high fracture toughness and high ductility, causing solder voiding at the interface and reducing the chance of cracking at the interface of the cobalt-copper IMC and the matte-tin plated interface. The described example enables tin plating of copper integrated circuit leads to mitigate degradation of material properties and extend shelf life before soldering to a printed circuit board, while improving the BLR of the electronic system once the electronic device is soldered to the main printed circuit board.
[0018] Figure 1-1B The electronic device 100 is shown as being located at an example position in a three-dimensional space, in which the corresponding first direction X, second direction Y, and third direction Z are mutually orthogonal. The electronic device 100 has a first side 101 and a second side 102 opposite to each other, which are spaced apart from each other along the first direction X and extend along the second direction Y. The electronic device 100 also includes a third side 103 and a fourth side 104 spaced apart from each other along the second direction Y, as well as a bottom side 105 and a top side 106 spaced apart from the bottom side 105 along the third direction Z. The electronic device 100 includes a molded package structure 108, which includes side surfaces 101-106. In the example shown, the bottom side 105 and the top side 106 are substantially planar and extend in corresponding XY planes of the first direction X and the second direction Y.
[0019] The electronic device 100 includes conductive leads 110 (e.g., copper) along lateral sides 101-104 to form a quad flat no-lead (QFN) package structure. In another embodiment, the device has conductive leads on two opposing sides to provide a dual flat no-lead (DFN) package structure (not shown). Figure 1BAs best shown in FIG. 1 , individual conductive leads 110 have a first surface 131 and a second surface 132. The first surface 131 has a double layer exposed outside the package structure 108 along the bottom side 105 of the package structure 108, and the second surface 132 is exposed outside the package structure 108 along the first side 101 of the package structure 108. The double layer includes a first plating layer 111 and a second plating layer 112. The first plating layer 111 is on and contacts the first surface 131 of the conductive lead 110. The first plating layer 111 includes cobalt. In one example, the first layer 111 has a thickness of approximately 0.5 μm or more and approximately 2.0 μm or less along the third direction Z. The second plating layer 112 is on and contacts the first plating layer 111, and the second plating layer 112 is exposed outside the package structure 108 along the bottom side 105 of the package structure 108. The second plating layer 112 includes tin, such as matte tin having a matte finish. Figure 1B A partial cross-sectional view of an example conductive lead 110 along a first side 101 of the electronic device 100 is shown. The conductive leads on the other lateral sides 102-104 of the electronic device 100 are similarly configured. Figure 1 As shown in FIG. 1 , the electronic device 100 also includes a semiconductor die 120 enclosed by a package structure 108 . The semiconductor die 120 has conductive bonding pads electrically connected to corresponding leads 110 by bonding wires 122 .
[0020] Figure 2 A method 200 of manufacturing an electronic device is presented, and Figure 3-8 An electronic device 100 is shown undergoing a manufacturing process according to method 200. Method 200 includes, at 202, a die attach process. Figure 3 An example is shown in which a die attach process 300 is performed to attach a semiconductor die 120 to a die attach pad 114 of a starting lead frame strip (e.g., copper) that also includes a desired lead 110. The die attach pad 114 has a lower surface 302, and the lead 110 has a lower first surface 131, such as Figure 3 In one example, the starting lead frame has a plurality of intended device sections arranged in a panel array 301 of rows and columns (not shown) of intended electronic devices 100. The die attach process 300 includes placing a plurality of semiconductor dies 120 simultaneously or sequentially to respective die attach pads 114 of the panel array 301.
[0021] Method 200 continues to 204, where the formation of electrical connections includes electrically coupling one or more conductive terminals (e.g., bonding pads) of die 120 to corresponding conductive leads 110, as well as any die-to-die connections required for a given electronic device design (e.g., die-to-die connections for a multi-chip module or MCM device, not shown). Figure 4 An example is shown in which a wire bonding process 400 is performed to form bond wires 122 between respective conductive bonding pads of semiconductor die 120 and associated ones of conductive leads 110 of a starting lead frame in panel array 301. Method 200 also includes performing a molding process at 206 that forms a molded package structure 108 enclosing semiconductor die 120 and bond wires 122. Figure 5 An example is shown in which a molding process 500 is performed that forms a molded package structure 108 enclosing the semiconductor die 120 and bond wires 122 .
[0022] At 208 , the method 200 includes performing a first plating process to plate the first surface 131 of the conductive lead 110 with a first plating layer 111 including cobalt. Figure 6 An example is shown in which a first plating process 600 is performed to form a first plating layer 111 on a first surface 131 of a conductive lead 110 exposed along a bottom side 105 of a molded structure 108 in a panel array 301 of an intended electronic device 100. In one example, the first plating process 600 is an electroplating process to form a first plating layer 111 having a thickness of approximately 0.5 μm or more and approximately 2.0 μm or less on the exposed first surface 131 of the conductive lead 110, wherein the first plating layer 111 contains cobalt. As described above, post-molding plating of the exposed first surface 131 of the conductive lead 110 with a bottom layer containing cobalt prior to plating of matte tin improves BLR performance by reducing defects and including a larger grain size that provides a diffusion barrier layer that prevents interdiffusion of copper and tin in subsequent tin plating.
[0023] The method 200 continues at 210 with matte tin plating. Figure 7An example is shown in which a second plating process 700 is performed, wherein the second plating process forms a second plating layer 112 on the first plating layer 111, wherein the second plating layer 112 contains tin. In one example, the second plating process 700 is an electroless plating process for forming the second plating layer 112 on the first plating layer 111. Since the solubility of cobalt and copper in each other is very low, the presence of cobalt in the first plating layer 111 slows down the formation of intermetallic compounds (IMCs) such as Cu3Sn and Cu6Sn5 that are prone to cracking in the double layer, thereby producing higher BLR performance. In addition, the cobalt-tin intermetallic compound has high fracture toughness and high ductility, thereby causing solder voiding at the interface and reducing the chance of cracking at the interface of the cobalt-copper IMC and the matte-tin plated. The described example enables tinning of copper integrated circuit leads to reduce the degradation of material properties and extend the shelf life before soldering to a printed circuit board, while improving the BLR of the electronic system once the electronic device is soldered to the main printed circuit board.
[0024] Method 200 continues Figure 2 The package is separated at 212. Figure 8 An example is shown in which a package separation process 800 is performed to separate the electronic devices 100 from the panel array 301, for example, by sawing, laser cutting, or other suitable processing along lines 802. The separation process 800 separates the individual semiconductor devices 100 from the cobalt and tin plated surfaces 131 of the conductive leads 110 exposed along the bottom side 105 of the corresponding package structure 108. The package separation process 800 exposes the second surfaces 132 of the conductive leads 110 along the sides 101-104 of the package structure 108.
[0025] Figure 9-9B An electronic device 900 with enhanced bottom side heat dissipation through plated copper structures in openings of die attach pads is shown. Good heat dissipation through die attach structures helps mitigate device degradation and enhance device operation at high temperatures. The electronic device 900 is shown as being located at an example position in a three-dimensional space in which respective first directions X, second directions Y, and third directions Z are mutually orthogonal. The electronic device 900 has opposing first and second sides 901 and 902 that are spaced apart from each other along the first direction X and extend along the second direction Y. The electronic device 900 also includes a third side 903 and a fourth side 904 that are spaced apart from each other along the second direction Y, as well as a bottom side 905 and a top side 906 that is spaced apart from the bottom side 905 along the third direction Z. The electronic device 900 includes a molded package structure 908 that includes side surfaces 901-906. In the illustrated example, the bottom side 905 and the top side 906 are substantially planar and extend in respective XY planes of the first direction X and the second direction Y.
[0026] The electronic device 900 includes conductive leads 910 (e.g., copper) along lateral sides 901-904 to form a quad flat no-lead (QFN) package structure. In another embodiment, the device has conductive leads on two opposing sides to provide a dual flat no-lead (DFN) package structure (not shown). Fig. 9B As best shown in , individual conductive leads 910 have bottom surfaces 931 exposed along bottom side 905 of package structure 908 , and conductive leads 910 on the other lateral sides 902 - 904 of electronic device 900 are similarly configured.
[0027] like Fig. 9 and 9B , the electronic device 900 also includes a plated copper layer 911 to facilitate heat transfer downward from a semiconductor die 920 enclosed by the package structure 908 and attached to a die attach pad 914. The die attach pad 914 has an opening 916 under a portion of the semiconductor die 920. Fig. 9B In the example of FIG. 9 , the die attach pad 914 has a recessed flange 918 surrounding the opening 916, and the semiconductor die 920 is attached to the flange 918 of the die attach pad 914. The semiconductor die 920 has a conductive bonding pad electrically connected to the corresponding lead 910 through a bonding wire 922. The package structure 908 encloses at least a portion of the semiconductor die 920.
[0028] like Fig. 9B, the semiconductor die 920 has a bottom side 921, and a metal layer 923 including nickel extends on the bottom side 921 of the semiconductor die 120. In one example, the metal layer 923 has a thickness of approximately 50 nm along the third direction Z. The semiconductor die 920 is attached to the die attach pad 914, wherein the side 921 of the semiconductor die 920 faces the opening 916 of the die attach pad 914. In this example, a second metal layer 919 (e.g., a pad) including nickel extends over and contacts the flange 918 of the die attach pad 914. The second metal layer 919 also contacts the metal layer 923 and the plated copper layer 911. In another embodiment, the flange 918 and the second metal layer 919 are omitted, and the semiconductor die 120 is attached to the top side of the die attach pad 914. The metal layer 923 facilitates electroless plating to form the plated copper layer 911 during manufacturing after the molding operation. The plated copper layer 911 extends downward from the metal layer 923 in the opening 916 of the die attach pad 914 along the third direction Z away from the semiconductor die 920. In one example, the plated copper layer 911 extends to the bottom side 905 of the electronic device 900 to allow soldering to a main printed circuit board (not shown). When a second metal layer 923 is included, electroless plating is also facilitated to form the plated copper layer 911. In the example shown, the plated copper layer 911 extends on and contacts the metal layer 923. The second metal layer 919 is thicker than the metal layer 923 along the third direction Z.
[0029] Also refer to Figure 10-18 , Fig.10 A method 1000 of manufacturing an electronic device is presented, and Figure 11-18 An electronic device 900 is shown undergoing a manufacturing process according to method 1000. Method 1000 includes spot printing a second metal layer 919 on flanges 918 of die attach pads 914 of a starting lead frame panel or strip. Fig.11 and 11A An example of a starting lead frame panel array 1101 is shown that includes a plurality of intended device areas arranged in an array of rows and columns (not shown). Each intended device area of the lead frame panel array 1101 includes a die attach pad structure 914 having an opening 916 and a recessed flange feature 918 that laterally surrounds the opening 916. Fig.12 and 12A In the process, a printing or other deposition process 1200 is performed to deposit nickel in selected portions on the flange 918 to form a second metal layer 919 thereon.
[0030] exist Fig.10At 1002 in the method 1000, the die attach process is continued. In the illustrated embodiment, the bottom side 921 of the semiconductor die 920 includes a nickel metal layer 923. In one example, the metal layer 923 has a thickness of approximately 50 nm along the third direction Z, and the second metal layer 919 is thicker than the metal layer 923. Fig.13 and 13A An example of processing at 1002 is shown in which an automated pick and place die attach process 1300 is performed that attaches a bottom side 921 of a semiconductor die 920 to a die attach pad 914, wherein a nickel metal layer 923 along the bottom side 921 of the semiconductor die 920 faces an opening 916 of the die attach pad 914. In the illustrated example having a die attach pad flange 918 and a second metal layer 919 thereon, the semiconductor die 920 is attached to the die attach pad 914, wherein a peripheral portion of the metal layer 923 along a side 921 of the semiconductor die 920 is on and in contact with the second metal layer 919 on the flange 918 of the die attach pad 914.
[0031] The method 1000 continues to 1004 where the formation of electrical connections includes electrically coupling one or more conductive terminals (eg, bond pads) of the die 920 to respective conductive leads 910, as well as any die-to-die connections required for a given electronic device design. Fig.14 and 14A An example is shown in which a wire bonding process 1400 is performed to form bond wires 922 between respective conductive bonding pads of semiconductor die 920 and associated ones of conductive leads 910 of a starting lead frame in panel array 1101. Method 1000 also includes performing a molding process at 1006 to form a molded package structure 908 enclosing at least a portion of semiconductor die 920 and bond wires 922. Fig.15 An example is shown in which a molding process 1500 is performed that forms a molded package structure 908 enclosing a semiconductor die 920 and bond wires 922 and exposing an opening 916 of a die attach pad 914 .
[0032] Method 100 further includes electroless plating at 1008 and 1010 to form a plated copper layer 911 on and in contact with the metal layer 923 on the side 921 of the semiconductor die 920, such that the plated copper layer 911 extends from the metal layer 923 in the opening 916 of the die attach pad 914 in a third direction Z away from the semiconductor die 920. Fig.16 and 17 Shown in Fig.16An example of a deposition process 1600 is performed in which a semi-solid gel 1602 is applied on the back side of semiconductor die 920 in opening 916. Gel 1602 in this example is impregnated with an electroless copper plating solution. Fig.17 In the embodiment, a thermal process 1700 is performed that applies heat to grow electroless copper from nickel metal layers 919 and 923 so as to form a plated copper layer 911 on and in contact with metal layer 923 on side 921 of semiconductor die 920 .
[0033] The method 1000 also includes performing a package separation process at 1012 to separate the manufactured electronic device 900 from the starting panel array 1101 . Fig.18 An example is shown in which a package separation process 1800 is performed to separate the electronic devices 900 from the panel array 1101, for example, by sawing, laser cutting, or other suitable processing along lines 1802. The separation process 1800 separates the individual semiconductor devices 900, wherein the bottom surfaces 931 of the conductive leads 910 are exposed along the bottom side 905 of the corresponding package structure 908, and the package separation process 1800 exposes the side surfaces of the conductive leads 910 along the sides 901-904 of the package structure 908, as described above. Figure 9-9B As shown in .
[0034] The above examples illustrate only several possible implementations of various aspects of the present specification, and other technical personnel in the field will conceive equivalent changes and / or modifications after reading and understanding the present specification and the accompanying drawings. Unless otherwise stated, "about," "roughly," or "substantially" in front of a value means + / -10% of the stated value. Modifications to the described examples are possible within the scope of the claims, and other implementations are possible.
Claims
1. An electronic device, comprising: Semiconductor die; a packaging structure enclosing the semiconductor die; as well as A conductive lead having a first surface and a second surface, the first surface having a double layer exposed outside the packaging structure along the bottom side of the packaging structure, and the second surface being exposed outside the packaging structure along the other side of the packaging structure, the double layer comprising a first plating layer and a second plating layer, the first plating layer being on the first surface of the conductive lead and contacting the first surface of the conductive lead, the second plating layer being on and contacting the first plating layer and exposed outside the packaging structure along the bottom side of the packaging structure, the first plating layer comprising cobalt, and the second plating layer comprising tin. 2 . The electronic device according to claim 1 , wherein the first plating layer has a thickness of approximately 0.5 μm or more and approximately 2.0 μm or less.
3. The electronic device according to claim 1 comprises a second conductive lead having a first surface and a second surface, the first surface of the second conductive lead having a second double layer exposed to the outside of the packaging structure along the bottom side of the packaging structure, and the second surface of the second conductive lead is exposed to the outside of the packaging structure along the other side of the packaging structure, the second double layer comprises a first layer and a second layer, the first layer of the second double layer is on the first surface of the second conductive lead and contacts the first surface of the second conductive lead, the second layer of the second double layer is on the first layer of the second double layer and contacts the first layer of the second double layer and is exposed to the outside of the packaging structure along the bottom side of the packaging structure, the first layer of the second double layer comprises cobalt, and the second layer of the second double layer comprises tin.
4. A method for manufacturing an electronic device, the method comprising: performing a first plating process that forms a first plating layer on a first surface of conductive leads in a panel array of an intended electronic device that is exposed along a bottom side of the molded structure, the first plating layer comprising cobalt; performing a second plating process, the second plating process forming a second plating layer on the first plating layer, the second plating layer comprising tin; as well as A package separation process is performed to separate the electronic devices from the panel array, wherein the conductive leads are exposed along the bottom side of the corresponding package structure, the package separation process exposing the second surface of the conductive leads along the first side of the package structure. 5 . The method according to claim 4 , wherein the first plating process is an electroplating process that forms the first plating layer having a thickness of approximately 0.5 μm or more and approximately 2.0 μm or less on the first surface of the conductive lead. 6 . The method of claim 5 , wherein the second plating process is an electroless plating process of forming the second plating layer on the first plating layer. 7 . The method of claim 4 , wherein the second plating process is an electroless plating process of forming the second plating layer on the first plating layer.
8. An electronic device comprising: a semiconductor die having a side and a metal layer on the side of the semiconductor die, the metal layer comprising nickel; a die attach pad having an opening, the semiconductor die being attached to the die attach pad, wherein the side surface of the semiconductor die faces the opening of the die attach pad; a plated copper layer on and contacting the metal layer, the plated copper layer extending from the metal layer in the opening of the die attach pad in a direction away from the semiconductor die; as well as A package structure encloses a portion of the semiconductor die.
9. The electronic device according to claim 8, wherein: The die attach pad has a flange and surrounds the opening; and The semiconductor die is attached to the flange of the die attach pad.
10. The electronic device of claim 9, further comprising a second metal layer on and contacting the flange of the die attach pad, the second metal layer contacting the metal layer and the plated copper layer, and the second metal layer comprising nickel. The electronic device of claim 10 , wherein the metal layer has a thickness of approximately 50 nm along the direction. The electronic device according to claim 10 , wherein the second metal layer is thicker than the metal layer along the direction.
13. The electronic device of claim 8, wherein the metal layer has a thickness of approximately 50 nm along the direction.
14. A method of manufacturing an electronic device, the method comprising: attaching a semiconductor die to a die attach pad, wherein a metal layer along a side of the semiconductor die faces an opening of the die attach pad, the metal layer comprising nickel; performing a molding process that forms a package structure enclosing a portion of the semiconductor die and exposing the opening of the die attach pad; performing an electroless plating process that forms a plated copper layer on and in contact with the metal layer on the side of the semiconductor die, the plated copper layer extending from the metal layer in the opening of the die attach pad in a direction away from the semiconductor die; as well as A package separation process is performed, which separates the electronic device from the panel array. 15 . The method of claim 15 , wherein attaching the semiconductor die to the die attach pad comprises attaching the semiconductor die to a flange of the die attach pad surrounding the opening.
16. The method of claim 15, wherein bonding the semiconductor die to the die bonding pad comprises bonding the semiconductor die to a peripheral portion of the metal layer along the side of the semiconductor die, the peripheral portion being on and contacting a second metal layer on the flange of the die bonding pad, the second metal layer comprising nickel. The method of claim 16 , wherein the metal layer has a thickness of approximately 50 nm. The method of claim 16 , wherein the second metal layer is thicker than the metal layer.
19. The method of claim 15, wherein the metal layer has a thickness of approximately 50 nm.
20. The method of claim 14, wherein the metal layer has a thickness of approximately 50 nm.